Improved welding die for electric ignition head
Through the improved welding mold, the use of heating resistors and automated solder ball implanting devices has solved the problems of false soldering and poor consistency in the welding mold of electric starters, achieved a high-quality and efficient welding process, and improved the product qualification rate. and consistency.
Patent Information
- Application Number
- CN202323654388.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-31
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2033-12-31
AI Technical Summary
Existing electric starter welding molds are prone to false welding and false welding during the welding process, and the length of the bridge wire is difficult to accurately control, resulting in poor product consistency and low qualification rate.
An improved welding mold is used, including a lower mold and an upper mold. A receiving groove is provided in the longitudinal groove of the lower mold and a non-thermal conductive layer is coated. The solder ball is in the receiving groove and a heating resistor is used to weld between the bridge wire and the copper wire. , and realize automated welding through the solder ball planting device and the wire walking mechanism, combining the advantages of soldering and resistance welding, and using high-temperature resistant and non-thermal conductive ceramic materials and flux to ensure welding quality.
It improves the quality of electric starter welding and product qualification rate, avoids the problems of false welding and strength reduction, and ensures product consistency and production efficiency.
Smart Images

Figure CN221817689U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of production of automatic welding and forming of pyrotechnic products, and is mainly suitable for improved welding moulds of electric ignition heads of military enterprises in aerospace, aviation and weapon systems and civilian blasting equipment. Background Art
[0002] The electric ignition head is a common pyrotechnic product. It is a small-scale detonation / detonation transmission element or device that is relatively sensitive to explosives. It can cause chemical reactions such as combustion and explosion under the action of a small initial impulse energy (electric energy) from the outside world, and use the energy released to ignite the gunpowder and detonate the explosives. The characteristics of the electric ignition head are high energy density, high reliability, small size, and large instantaneous release of electricity. It is widely used in the ignition or detonation of various conventional weapons, nuclear weapons, missiles and other spacecraft. Many systems in spacecraft also use it to complete specific functions (such as control, emergency, interstage separation, fairing release and recovery and landing, safety insurance and self-destruction systems). In the civilian field, the electric ignition head is widely used in mining, blasting, explosive forming, lifesaving, exploration and other fields.
[0003] The ignition head is composed of two parallel copper wires and a bridge wire connecting the two wires at one end of the copper wires. The function of the bridge wire is that when the two wires are energized, the bridge wire heats up, heats the heating agent, and ignites it, thereby achieving the purpose of detonating other explosives.
[0004] Since the diameter of the bridge wire (nickel-chromium alloy wire) is very thin (usually a few to dozens of wires) and it is not easy to tin, the welding process is completed by tinning soldering, which can easily cause cold welding and false welding. In addition, the welding bridge wire is short (usually about 2 mm), and the length of the welding bridge wire determines the final heating resistance value of the electric ignition head. It is difficult for the human eye to accurately judge the welding length of the bridge wire, resulting in poor product consistency and low product qualification rate.
[0005] To this end, the patent applicant has applied for a utility model patent with patent number ZL202322339962.7 and patent name "A kind of electric ignition head welding mold". However, during the welding process, it was found that after the tin ball C was heated and melted by the laser above, a tin ingot was often formed at the connection between the hot wire A and the bridge wire B, which led to defects such as poor welding quality and easy falling off of the welding point. Summary of the invention
[0006] The utility model aims to overcome the defects of the prior art and provide an improved welding die for an electric ignition head with good welding and electrical connectivity.
[0007] The utility model adopts the following technical solutions:
[0008] An improved welding mold for an electric ignition head comprises a lower mold and an upper mold, wherein the lower mold is provided with a longitudinal groove for placing a copper wire A, the upper mold is provided with a through groove penetrating and corresponding to the longitudinal groove, a through hole larger than the transverse through groove is provided in the middle of the through groove, and the through hole is located above the position where the copper wire A and the bridge wire B in the longitudinal groove need to be welded; the longitudinal groove of the lower mold is provided with a receiving groove at the position of the through hole, the surface of the receiving groove is coated with a non-heat-conducting layer, the solder ball C is located in the receiving groove, the bridge wire B is located between the solder ball C and the exposed layer at the front end of the copper wire A, and a heating resistor is provided at the rear end of the exposed layer at the front end of the copper wire A;
[0009] The non-heat-conductive layer coated on the surface of the receiving groove of the lower mold 1 is ceramic;
[0010] The heating resistor is a heating resistor extending from the positive and negative electrodes of the resistance welding machine to the rear end of the exposed layer of the front end of the copper wire A;
[0011] The solder ball C described above is automatically pushed into the through hole of the upper mold by the solder ball implanting device with a diameter of 0.5-0.6 mm;
[0012] The bridge wire B is moved to the corresponding position of the solder ball C through the wire moving mechanism.
[0013] The electric ignition head welding of the resistance welding machine plus tin ball welding combines the advantages of tin soldering and resistance welding. The heating resistor is made of special materials that are completely non-tin-sticky, and high-temperature resistant and non-heat-conductive ceramic materials are coated near the welding point to ensure that the same specifications of electric ignition head skeleton welding have the same heat generation. Since the same size of tin balls are used for the welding of electric ignition head skeletons of the same specifications, it is convenient to control the relevant parameters of the resistance welding machine and ensure the consistency of the product. It avoids the problems of false welding and reduced strength of nickel-chromium alloy wire in the previous production method, and greatly improves the quality and product qualification rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Attached Figure 1 This is a three-dimensional exploded view of the utility model;
[0015] Attached Figure 2 This is a cross-sectional view of the utility model;
[0016] Attached Figure 3 This is a diagram of the utility model in use with the upper mold removed. DETAILED DESCRIPTION
[0017] See attached Figures 1 to 3The improved welding mold for electric ignition head comprises a lower mold 1 and an upper mold 2. The lower mold 1 is provided with a longitudinal groove 11 for placing a copper wire A. The upper mold 2 is provided with a through groove 21 that penetrates and corresponds to the longitudinal groove. A through hole 22 larger than the transverse through groove is provided in the middle of the through groove 21. The through hole 22 is located above the position where the copper wire A and the bridge wire B in the longitudinal groove 11 need to be welded. The longitudinal groove 11 of the lower mold 1 is provided with a receiving groove 111 at the position of the through hole 22. The surface of the receiving groove 111 is coated with a non-conductive layer. The solder ball C is located in the receiving groove 111. The bridge wire B is located between the solder ball C and the exposed layer at the front end of the copper wire A. A heating resistor 3 is provided at the rear end of the exposed layer at the front end of the copper wire A.
[0018] The non-heat-conductive layer coated on the surface of the receiving groove 111 of the lower mold 1 is ceramic;
[0019] The heating resistor 3 is a heating resistor 3 extending from the positive and negative electrodes of the resistance welding machine to the rear of the exposed layer at the front end of the copper wire A;
[0020] The solder ball C with a diameter of 0.5-0.6 mm is automatically pushed into the through hole 22 of the upper mold 2 by the solder ball implantation device;
[0021] The bridge wire B is moved to the corresponding position of the solder ball C through the wire moving mechanism.
[0022] When the utility model is applied, the solder ball C with a diameter of 0.5-0.6 mm is driven by a servo motor through the solder ball implanting device 4, and visually assisted positioning is performed, and the solder balls at multiple positions are automatically placed into the receiving groove 111 of the lower mold 1 in sequence;
[0023] The bridge wire B is fed to the corresponding position of the receiving groove 111 of the lower mold 1 through the wire feeding mechanism. After reaching the position, the front and rear ends of the bridge wire B are pressed and fixed by the upper mold 2;
[0024] In order to ensure the control of the welding quality of the electric ignition head, it is necessary to add the function of flux dripping on the basis of removing the oxide layer on the surface of the bridge wire B. The purpose is to use the fluxing effect of the flux in the welding process to better wet the bridge wire and the solder ball C below. After the solder ball melts, the bridge wire wrapping performance will be better.
[0025] The exposed layer at the front end of the shaped copper conductor A is manually installed to the designated position through the longitudinal groove 11 on the lower die 1. Multiple skeleton copper core wires can be installed each time (determined by the combined tooling) to improve production efficiency.
[0026] Since a heating resistor 3 made of a special non-tin-sticking material is connected between the positive and negative electrodes of the resistance welding machine, a tin ball C is added to the intersection of the exposed layer at the front end of the copper wire A of the electric ignition head skeleton and the bridge wire B, and then the heating resistor 3 between the two electrodes of the resistance welding machine pre-applies a certain pressure to the tin ball C, the copper wire A and the bridge wire B, and then a large current is applied to the two electrodes for an instant, and the heating resistor 3 between the two electrodes is used to generate heat, and the exposed layer at the front end of the copper wire A and the bridge wire B are covered and welded together through the tin ball C to complete the welding process of the electric ignition head skeleton.
Claims
1. An improved welding mold for an electric ignition head, comprising a lower mold and an upper mold, wherein the lower mold is provided with a longitudinal groove for placing a copper wire A, and the upper mold is provided with a through groove that penetrates and corresponds to the longitudinal groove, and a through hole larger than the transverse through groove is provided in the middle of the through groove, and the through hole is located above the position where the copper wire A and the bridge wire B in the longitudinal groove need to be welded; characterized in that: The longitudinal groove of the lower mold is provided with a receiving groove at the position of the through hole, the surface of the receiving groove is coated with a non-heat-conductive layer, the solder ball C is located in the receiving groove, the bridge wire B is located between the solder ball C and the exposed layer at the front end of the copper wire A, and a heating resistor is provided at the rear end of the exposed layer at the front end of the copper wire A.
2. The improved welding mold for electric ignition head according to claim 1, characterized in that: The non-heat-conductive layer coated on the surface of the receiving groove of the lower mold is ceramic.
3. The improved welding mold for electric ignition head according to claim 1, characterized in that: The heating resistor is a heating resistor extending from the positive and negative electrodes of the resistance welding machine to the rear end of the exposed layer of the front end of the copper wire A.
4. The improved welding mold for electric ignition head according to claim 1, characterized in that: The solder ball C with a diameter of 0.5-0.6 mm is automatically pushed into the through hole of the upper mold by the solder ball implanting device.
5. The improved welding mold for electric ignition head according to claim 1 is characterized in that: The bridge wire B is moved to the corresponding position of the solder ball C through the wire moving mechanism.