Outer sizing device for plastic pipe production

By adopting an external sizing device in the production of PPR pipes and using negative pressure fans and spiral water-cooled pipe technology, the problem of uneven pipe wall thickness caused by the internal sizing cylinder has been solved, improving pipe diameter uniformity and production quality, and simplifying maintenance process.

CN221819452UActive Publication Date: 2024-10-11SHANXI JIN EXECUTIVE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420057690.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-10
Publication Date
2024-10-11
Estimated Expiration
2034-01-10

AI Technical Summary

Technical Problem

In the prior art, when an internal sizing cylinder is used to produce PPR pipes, due to the effect of gravity, the thickness of the pipe wall is uneven, resulting in uneven pipe diameters and reducing product quality.

Method used

Design an external sizing device for plastic pipe production, which uses a sizing cylinder, an adsorption mechanism and a cooling mechanism. It uses a negative pressure fan and a spiral water-cooling pipe to ensure that the plastic pipe is evenly adsorbed and cooled on the inner wall of the sizing cylinder to avoid the influence of gravity.

Benefits of technology

The PPR pipe outer wall diameter error is small and the overall pipe diameter is uniform, which improves production quality and simplifies maintenance and parts replacement through the detachable design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221819452U_ABST
    Figure CN221819452U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of plastic pipe processing, in particular to an external sizing device for plastic pipe production, which comprises a sizing cylinder, an adsorption mechanism and a cooling mechanism for cooling and forming a plastic pipe, the sizing cylinder comprises an adsorption section and a cooling section, and fixing rings are arranged on two sides of the adsorption section. The adsorption mechanism comprises a plurality of circles of uniformly arranged adsorption holes formed in the adsorption section and an adsorption cylinder detachably connected to the fixing ring, the adsorption cylinder and the fixing ring are sealed, a cavity chamber is formed between the adsorption cylinder and the adsorption section, the adsorption cylinder is connected with an adsorption pipe, and the adsorption pipe is connected with a negative pressure fan. According to the design, the adsorption barrel and the adsorption pipe are arranged, so that adsorption force is generated on the inner wall of the sizing barrel, it is ensured that the error of the pipe diameter of the outer wall of the cooled PPR pipe is small, and the problem that the wall thickness of the PPR pipe is not uniform due to the fact that an inner sizing barrel is used for producing the PPR pipe in the prior art is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of plastic pipe processing, in particular to an external sizing device for plastic pipe production. Background Art

[0002] Compared with traditional cast iron pipes, galvanized steel pipes, cement pipes and other pipes, PPR pipes have the advantages of energy saving and material saving, environmental protection, light weight and high strength, corrosion resistance, smooth inner wall and no scaling, easy construction and maintenance, and long service life. They are widely used in building water supply and drainage, urban and rural water supply and drainage, city gas, electricity and optical cable sheathing, industrial fluid transportation, agricultural irrigation and other construction, municipal, industrial and agricultural fields.

[0003] PPR pipe production is to use an extruder to heat-melt the plastic raw materials and then extrude them into shape. During the extrusion process, the diameter of the extruded molten plastic pipe needs to be fixed. The usual method is to use an internal sizing cylinder to attach the extruded plastic to the sizing cylinder, cool it, and then remove it from the internal sizing cylinder for final molding. However, when processing PPR pipes using an internal sizing cylinder, when the plastic is attached to the sizing cylinder, it falls downward due to gravity, making the lower part of the PPR pipe thicker and the upper part thinner, making the diameter of the PPR pipe uneven, and reducing the product quality of the PPR pipe. Utility Model Content

[0004] The utility model aims to provide an external sizing device for producing plastic pipes, so as to solve the problem that the wall thickness of PPR pipes is uneven when the internal sizing cylinder is used to produce PPR pipes in the prior art.

[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a plastic pipe production external sizing device, comprising a sizing cylinder, an adsorption mechanism and a cooling mechanism for cooling the plastic pipe into shape, the sizing cylinder comprising an adsorption section and a cooling section, fixing rings are arranged on both sides of the adsorption section, the adsorption mechanism comprises a plurality of circles of evenly arranged adsorption holes opened on the adsorption section and an adsorption cylinder detachably connected to the fixing ring, the adsorption cylinder and the fixing ring are sealed, a cavity is formed between the adsorption cylinder and the adsorption section, the adsorption cylinder is connected to an adsorption tube, and the adsorption tube is connected to a negative pressure fan.

[0006] The working principle of this scheme is as follows: the sizing cylinder is fixed at the outlet of the extruder. After the extruder extrude the plastic tube, when the extruded plastic tube passes through the adsorption cylinder, the negative pressure fan draws out the air in the cavity to generate negative pressure, and the plastic tube is adsorbed on the inner wall of the sizing cylinder through the adsorption hole. After the plastic tube passes through the adsorption section, it is cooled and hardened under the cooling of the cooling mechanism, and gradually cooled and formed. When leaving the cooling section, it is completely cooled and formed.

[0007] Preferably, the cooling mechanism includes a primary cooling component, a full cooling component and a water supply tank for providing cooling water to the primary cooling component and the full cooling component, the water supply tank is connected to a water pump, and a heat exchanger is arranged inside the water supply tank.

[0008] Preferably, the full cooling component includes a flange plate arranged on the outside of the sizing cylinder between the adsorption section and the cooling section, and a cooling cylinder sleeved on the cooling section. The cooling cylinder and the flange plate are detachably connected. A spiral water-cooling pipe is fixed to the inner wall of the cooling cylinder. The lower part of the spiral water-cooling pipe is connected to a second water inlet pipe, and the second water inlet pipe is connected to a water pump. The upper part of the spiral water-cooling pipe is connected to a second water outlet pipe, and the second water outlet pipe is connected to a water supply tank.

[0009] Preferably, the pre-cooling assembly includes a plurality of pre-cooling tubes fixed on the inner wall of one side of the adsorption cylinder, each of the pre-cooling tubes is located between two adjacent circles of adsorption holes, the lower part of each pre-cooling tube is connected to a first water inlet pipe, and the upper part of each pre-cooling tube is connected to a first water outlet pipe, the first water inlet pipe is detachably connected to the second water inlet pipe, and the first water outlet pipe is detachably connected to the second water outlet pipe.

[0010] Preferably, the adsorption tube is connected to the upper part and both sides of the adsorption cylinder, the negative pressure fan is fixed on the outer wall of the adsorption cylinder, a pressure regulating tube is provided on the right side of the adsorption cylinder, and a pressure compensation valve is installed on the pressure regulating tube.

[0011] Compared with the known public technology, the technical solution provided by the utility model has the following beneficial effects:

[0012] 1. The utility model generates an adsorption force on the inner wall of the sizing cylinder by arranging an adsorption cylinder, an adsorption hole, an adsorption tube, and a negative pressure fan, so that the PPR tube extruded by the extruder is adsorbed on the inner wall of the sizing cylinder, and a spiral water-cooling pipe, a cooling cylinder, and a cooling PPR tube are arranged to ensure that the error of the outer wall diameter of the PPR tube after cooling is small, the overall tube diameter is uniform, and the production quality of the PPR tube is improved.

[0013] 2. The utility model installs the adsorption cylinder and the cooling cylinder on the sizing cylinder in a detachable manner, which facilitates the disassembly of parts and facilitates maintenance when the adsorption hole is blocked or the spiral water cooling tube is damaged. If some parts are damaged, the damaged parts can be directly replaced without replacing the entire equipment.

[0014] 3. The utility model arranges a pressure regulating pipe and a pressure-replenishing valve on the adsorption cylinder. When the negative pressure fan is working all the time, the air in the cavity is continuously extracted. When the PPR tube moves forward until it completely blocks the adsorption hole, the negative pressure fan continues to extract the air in the cavity. When the negative pressure in the cavity is large, the pressure-replenishing valve is pushed open by the air to maintain the air pressure in the cavity, thereby preventing the PPR tube plastic from being sucked into the adsorption hole, causing blockage of the adsorption hole and uneven surface of the PPR tube. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the structure of the utility model;

[0016] Figure 2 For this utility model Figure 1 longitudinal cross-sectional view;

[0017] Figure 3 For this utility model Figure 1 Schematic diagram of the AA section structure;

[0018] Figure 4 For this utility model Figure 2 A partial enlarged schematic diagram of point B in the middle.

[0019] In the figure: sizing cylinder 101, fixing ring 102, adsorption section 103, cooling section 104, flange 105, adsorption hole 201, adsorption cylinder 202, adsorption tube 203, cavity chamber 204, negative pressure fan 205, pressure regulating pipe 206, pressure compensation valve 207, water supply tank 301, water pump 302, primary cooling pipe 303, first water inlet pipe 304, first water outlet pipe 305, cooling cylinder 306, spiral water cooling pipe 307, second water inlet pipe 308, second water outlet pipe 309. DETAILED DESCRIPTION

[0020] In order to make the purpose, technical solution and advantages of the embodiment of the utility model clearer, the technical solution in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is a part of the embodiment of the utility model, not all of the embodiments. Based on the embodiment of the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.

[0021] The present invention will be further described below in conjunction with the embodiments.

[0022] like Figure 1 - Figure 4 As shown, the utility model provides an external sizing device for plastic pipe production, comprising a sizing cylinder 101, an adsorption mechanism for adsorbing the plastic pipe of the extruder base onto the sizing cylinder 101, and a cooling mechanism for cooling the plastic pipe into shape.

[0023] The sizing cylinder 101 is divided into two sections, a left adsorption section 103 and a right cooling section 104. A flange 105 is provided on the outer side of the sizing cylinder 101 between the adsorption section 103 and the cooling section 104. Both left and right ends of the adsorption section 103 are provided with fixing rings 102, and the fixing rings 102 are provided with threaded holes evenly distributed circumferentially.

[0024] The adsorption mechanism includes a circle of adsorption holes 201 axially distributed at a certain interval on the adsorption section 103, and each circle of adsorption holes 201 is evenly distributed in the circumferential direction. An adsorption cylinder 202 is fixed to the outside of the adsorption section 103, and the left and right ends of the adsorption cylinder 202 are fixed in the threaded holes by bolts. A sealing gasket is provided between the left and right ends of the adsorption cylinder 202 and the fixing ring 102, so that a cavity chamber 204 is formed between the adsorption cylinder 202 and the adsorption section 103.

[0025] Adsorption tubes 203 are provided on the upper left side and on both sides of the adsorption tube 202. The adsorption tubes 203 penetrate the adsorption tube 202 and communicate with the cavity chamber 204. The three adsorption tubes 203 are connected to the same pipeline and are connected to a negative pressure fan 205. The negative pressure fan 205 is fixed on the upper outer wall of the adsorption tube 202. Since the nozzles of the adsorption tubes 203 are closer to the upper part and the left and right sides, the adsorption force generated on the plastic tube through the adsorption holes 201 is greater than that on the lower part far from the nozzles of the adsorption tubes 203, thereby offsetting part of the influence of gravity. As for the lower part, since the plastic tube itself is affected by gravity, it will fall down and can fit completely on the inner wall of the adsorption section 103.

[0026] A pressure regulating pipe 206 is provided on the right side of the adsorption cylinder 202, and a pressure-boosting valve 207 is installed on the pressure-boosting pipe 206. The pressure-boosting valve 207 is a reverse structure of a pressure relief valve. When the atmospheric pressure is greater than a certain pressure of the air pressure in the cavity chamber 204, the pressure-boosting valve 207 opens to adjust the negative pressure in the cavity chamber 204 to avoid that after all the adsorption holes 201 are blocked by plastic tubes, a large adsorption force is generated in the cavity chamber 204, and the plastic that has not yet solidified is sucked into the adsorption holes 201, which on the one hand causes the adsorption holes 201 to be blocked, and on the other hand causes poor surface quality of the material tube.

[0027] The required negative pressure in the cavity chamber 204 can be easily obtained through debugging, and the uncooled molded plastic tube can be adsorbed while maintaining the adsorption force, and a large adsorption force will not be generated to suck the cooled plastic into the adsorption hole 201.

[0028] The cooling mechanism includes a primary cooling component, a full cooling component and a water supply tank 301 for providing cooling water for the primary cooling component and the full cooling component. The water supply tank 301 is connected to a water pump 302. A heat exchanger is provided in the water supply tank 301 for cooling the water in the water supply tank 301.

[0029] The primary cooling component includes a plurality of primary cooling tubes 303 fixed on the right inner wall of the adsorption cylinder 202 between two adjacent circles of adsorption holes 201. The primary cooling tubes 303 are fixed to the inner wall of the adsorption cylinder 202 by welding. The lower part of each primary cooling tube 303 is connected to a first water inlet pipe 304, which passes through the cylinder wall of the adsorption cylinder 202 and is connected to the primary cooling tube 303. The first water inlet pipe 304 is fixed to the adsorption cylinder 202 by welding. The upper part of each primary cooling tube 303 is connected to a first water outlet pipe 305, which passes through the cylinder wall of the adsorption cylinder 202 and is connected to the primary cooling tube 303. The first water outlet pipe 305 is fixed to the adsorption cylinder 202 by welding. All first water outlet pipes 305 are connected, and all first water inlet pipes 304 are connected.

[0030] The full cooling component includes a cooling cylinder 306 which is sleeved on the cooling section 104. A flange 105 is provided at the left end of the cooling cylinder 306. The cooling cylinder 306 is connected and fixed to the sizing cylinder 101 through the flange 105. A spiral water-cooling pipe 307 is fixed to the inner wall of the cooling cylinder 306. The lower left end of the spiral water-cooling pipe 307 is connected to a second water inlet pipe 308. The second water inlet pipe 308 passes through the cooling cylinder 306. The second water inlet pipe 308 is connected to the water pump 302. The second water inlet pipe 308 is connected to the first water inlet pipe 304 through a sealing flange. The upper right end of the spiral water-cooling pipe 307 is connected to a second water outlet pipe 309. The second water outlet pipe 309 is connected to the first water outlet pipe 305 through a sealing flange. The second water outlet pipe 309 is connected to the water supply tank 301.

[0031] The water pump 302 pumps the water in the water supply tank 301 into the second water inlet pipe 308. The first water inlet pipe 304 is connected to the second water inlet pipe 308. The cooling water enters the first water inlet pipe 304 together, and then enters the spiral water cooling pipe 307 and the primary cooling pipe 303 respectively, and then flows out from the first water outlet pipe 305 and merges with the cooling water in the spiral water cooling pipe 307 into the second water outlet pipe 309 and then returns to the water supply tank 301. The temperature of the cooling water in the water supply tank 301 is reduced by a heat exchanger.

[0032] When the utility model is used, the sizing cylinder 101 is fixed at the outlet of the extruder. After the extruder extrude the plastic tube, when the extruded plastic tube passes through the adsorption cylinder 202, the negative pressure fan 205 extracts the air in the cavity chamber 204 to generate negative pressure, and the plastic tube is adsorbed on the inner wall of the sizing cylinder 101 through the adsorption hole 201. When the plastic tube passes through the rear section of the adsorption section 103, it is initially cooled and hardened under the initial cooling of the primary cooling tube 303, so as to avoid deformation of the plastic tube due to disappearance of the adsorption force when passing between the adsorption section 103 and the cooling section 104. When the plastic tube passes through the cooling section 104, it is gradually cooled and formed under the cooling of the spiral water-cooling tube 307, and is completely cooled and formed when leaving the cooling section 104.

[0033] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some of the technical features therein by equivalents. These modifications or replacements will not cause the essence of the corresponding technical solutions to deviate from the protection scope of the technical solutions of the embodiments of the present invention.

Claims

1. A plastic pipe production external sizing device, characterized in that: The invention comprises a sizing cylinder (101), an adsorption mechanism and a cooling mechanism for cooling and forming a plastic tube. The sizing cylinder (101) comprises an adsorption section (103) and a cooling section (104). A fixing ring (102) is arranged on both sides of the adsorption section (103). The adsorption mechanism comprises a plurality of circles of evenly arranged adsorption holes (201) opened on the adsorption section (103) and an adsorption cylinder (202) detachably connected to the fixing ring (102). The adsorption cylinder (202) and the fixing ring (102) are sealed. A cavity chamber (204) is formed between the adsorption cylinder (202) and the adsorption section (103). The adsorption cylinder (202) is connected to an adsorption tube (203), and the adsorption tube (203) is connected to a negative pressure fan (205).

2. The external sizing device for plastic pipe production according to claim 1, characterized in that: The cooling mechanism comprises a primary cooling component, a full cooling component and a water supply tank (301) for providing cooling water to the primary cooling component and the full cooling component. The water supply tank (301) is connected to a water pump (302) and a heat exchanger is arranged inside the water supply tank (301).

3. The external sizing device for plastic pipe production according to claim 2, characterized in that: The full cooling component comprises a flange (105) arranged on the outside of a sizing cylinder (101) between an adsorption section (103) and a cooling section (104), and a cooling cylinder (306) sleeved on the cooling section (104); the cooling cylinder (306) and the flange (105) are detachably connected; a spiral water cooling pipe (307) is fixed to the inner wall of the cooling cylinder (306); a second water inlet pipe (308) is connected to the lower part of the spiral water cooling pipe (307); the second water inlet pipe (308) is connected to a water pump (302); a second water outlet pipe (309) is connected to the upper part of the spiral water cooling pipe (307); the second water outlet pipe (309) is connected to a water supply tank (301).

4. The external sizing device for plastic pipe production according to claim 3, characterized in that: The primary cooling component comprises a plurality of primary cooling tubes (303) fixed to the inner wall of one side of the adsorption cylinder (202), each of the primary cooling tubes (303) being located between two adjacent circles of adsorption holes (201), the lower portion of each primary cooling tube (303) being connected to a first water inlet pipe (304), the upper portion of each primary cooling tube (303) being connected to a first water outlet pipe (305), the first water inlet pipe (304) being detachably connected to the second water inlet pipe (308), and the first water outlet pipe (305) being detachably connected to the second water outlet pipe (309).

5. The external sizing device for plastic pipe production according to any one of claims 1 to 4, characterized in that: The adsorption tube (203) is connected to the upper part and both sides of the adsorption cylinder (202), the negative pressure fan (205) is fixed on the outer wall of the adsorption cylinder (202), and a pressure regulating tube (206) is provided on the right side of the adsorption cylinder (202), and a pressure compensation valve (207) is installed on the pressure regulating tube (206).