Antibacterial composite pipe
By using stainless steel reinforcement and recovery layer structures in antibacterial composite pipes, the problem of poor sealing after hot melt treatment is solved and a more stable and sealed pipe connection is achieved.
Patent Information
- Application Number
- CN202420595267.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2034-03-26
AI Technical Summary
The existing antibacterial composite pipes have poor sealing performance after hot melt treatment, mainly because the outside of the pipe cannot fully contact the inner wall of the joint, resulting in unstable connections.
The first reinforcement layer, restoration layer and second reinforcement layer made of stainless steel are used to form an integrated structure. Antibacterial plastic is wrapped on the outside to increase the support capacity and strength of the pipe. After hot-melt connection, it is restored to close contact with the joint to improve sealing. .
It improves the connection stability and sealing of pipes and joints, ensuring the quality and long-term effectiveness of hot-melt connections.
Smart Images

Figure CN221824709U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of composite pipes, in particular to an antibacterial composite pipe. Background Art
[0002] At present, the building pipes used for water supply and drainage are generally galvanized steel pipes, but this type of pipe is facing elimination due to many disadvantages. Therefore, it is necessary to find a new type of pipe to replace the traditional galvanized steel pipe. In order to solve the above problems, people have developed a stainless steel-plastic composite pipe, which has solved the above problems to a certain extent. However, the existing stainless steel-plastic composite pipe has a big disadvantage, that is, since its inner layer only uses ordinary plastic, it can neither inhibit the growth of bacteria in the water nor kill them. Therefore, this pipe cannot meet the needs of pure water supply projects, differentiated water supply projects and water supply occasions with high requirements for sanitary performance.
[0003] The prior art antibacterial composite tube and its preparation method are as follows: its raw material components include, by weight, 1.6 parts of antibacterial active ingredients, 83.4 parts of linear polyethylene and 15 parts of epoxy resin; a mold is prepared according to the size of the plastic antibacterial inner tube; the antibacterial active ingredients, linear polyethylene and epoxy resin are mixed by a mixer at 30°C for 30 minutes; a coupling agent and a dispersant are added during the mixing for modification treatment; the molding main machine and the molding auxiliary machine are heated to 80°C, and extrusion molding is performed under a vacuum state; after the extrusion is completed, the tube is drawn, and after cooling and molding, an antibacterial test is performed by an antibacterial machine to test the antibacterial ingredients. After the antibacterial test results meet the national standards, the tube is put into storage for the next step of preparation; by adding coupling agents and dispersants, the antibacterial active ingredients can be dispersed more evenly in the linear resin, the antibacterial active ingredients and the linear resin are combined more thoroughly, the antibacterial effect is better and the compressive strength is higher.
[0004] The current connection of composite pipes is to use a hot melt gun to hot-melt the outer wall of the composite pipe and the inner wall of the connecting head, and then connect the pipe and the connecting head in a hot-melt state. After cooling, the two are connected together and stability can be guaranteed; however, the current antibacterial composite pipe has a shortcoming that there is no good stable support inside it. When the outer wall of the pipe is hot-melt treated, it is necessary to apply a force perpendicular to the hot melt to the pipe to ensure the quality of the pipe during hot-melt treatment. However, the hot-melt treated pipe has a poor sealing problem after hot-melt treatment, mainly because the outside of the pipe cannot fully contact the inner wall of the pipe joint after hot-melt treatment, which leads to poor sealing; for this reason, the present application proposes an antibacterial composite pipe with higher strength and convenient hot-melt connection. Utility Model Content
[0005] In view of the deficiencies in the prior art, the utility model provides an antibacterial composite pipe to solve the problem that the outside of the pipe cannot fully contact the inner wall of the pipe joint after hot-melt treatment, thereby causing poor sealing.
[0006] The embodiment of the utility model provides an antibacterial composite tube, comprising:
[0007] pipeline;
[0008] The pipeline includes antibacterial plastic, a first reinforcement layer, a recovery layer and a second reinforcement layer, the first reinforcement layer is located inside the second reinforcement layer, the recovery layer is located between the first reinforcement layer and the second reinforcement layer, and the first reinforcement layer, the recovery layer and the second reinforcement layer are integrally arranged, and the antibacterial plastic is coated on the outside of the first reinforcement layer, the recovery layer and the second reinforcement layer to form a pipeline.
[0009] Furthermore, the antibacterial plastic comprises an antibacterial layer and plastic.
[0010] Furthermore, the first reinforcement layer is made of a stainless steel mesh, and the first reinforcement layer is arranged in a cylindrical shape.
[0011] Furthermore, the second reinforcement layer is two arc-shaped stainless steel meshes, and the two arc-shaped stainless steel meshes are symmetrically arranged outside the first reinforcement layer.
[0012] Furthermore, the recovery layer is a connecting rod made of stainless steel, and the recovery layer is fixedly connected to the first reinforcement layer and the second reinforcement layer.
[0013] Compared with the prior art, the utility model has the following beneficial effects:
[0014] The utility model can increase the supporting capacity and strength of the pipeline by arranging a first reinforcement layer, a recovery layer and a second reinforcement layer made of stainless steel. After hot-melt connection, the second reinforcement layer and the recovery layer are gradually restored without pressure and tightly adhere to the pipe joint, so that the stability and sealing of the connection between the pipeline and the pipe joint are better. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic structural diagram of an antibacterial composite tube described in an embodiment of the utility model.
[0016] Figure 2 1 is a schematic diagram of a first reinforcement layer, a recovery layer, and a second reinforcement layer 14 in an antibacterial composite tube described in an embodiment of the utility model.
[0017] Figure 3 It is a schematic diagram of the first reinforcement layer in an antibacterial composite tube described in an embodiment of the utility model.
[0018] In the above drawings: 1 is a pipe, 11 is bacterial plastic, 12 is a first reinforcement layer, 13 is a recovery layer, and 14 is a second reinforcement layer. DETAILED DESCRIPTION
[0019] The technical solution of the present utility model is further described below in conjunction with the accompanying drawings and embodiments.
[0020] like Figure 1-Figure 3 As shown, the embodiment of the utility model provides an antibacterial composite tube, comprising:
[0021] Pipeline 1;
[0022] The pipeline 1 includes an antibacterial plastic 11, a first reinforcement layer 12, a recovery layer 13 and a second reinforcement layer 14, wherein the first reinforcement layer 12 is located inside the second reinforcement layer 14, and the first reinforcement layer 12 is made of a stainless steel mesh, and the first reinforcement layer 12 is arranged in a cylindrical shape; wherein the second reinforcement layer 14 is two arc-shaped stainless steel meshes, and the two arc-shaped stainless steel meshes are symmetrically arranged outside the first reinforcement layer 12;
[0023] The recovery layer 13 is located between the first reinforcement layer 12 and the second reinforcement layer 14. The recovery layer 13 is a connecting rod made of stainless steel. The recovery layer 13 is fixedly connected to the first reinforcement layer 12 and the second reinforcement layer 14. The first reinforcement layer 12, the recovery layer 13 and the second reinforcement layer 14 are integrally arranged, and the antibacterial plastic 11 is coated on the outside of the first reinforcement layer 12, the recovery layer 13 and the second reinforcement layer 14.
[0024] Among them, the antibacterial plastic 11 includes an antibacterial layer and plastic, that is, an antibacterial agent is mixed with a plastic material, which is a prior art; wherein, the antibacterial plastic 11 is further explained: the use of antibacterial plastics must first meet the necessary requirements for the physical, chemical, mechanical and other properties of plastics when used as basic materials, and at the same time, the requirements for the special function of antibacterial and the additional factors arising therefrom must be considered. Therefore, the antibacterial plastic must have good mechanical strength appearance, chemical stability, and good processability. In terms of antibacterial properties, the antibacterial plastic is required to be able to adapt to the use environment and should have high-efficiency, broad-spectrum, and long-lasting antibacterial properties. Since the antibacterial plastic contains a small amount of antibacterial agent, the antibacterial agent used is required to meet the specified sanitary safety, and the ultimate antibacterial plastic product must meet the requirements of being non-toxic, odorless, and harmless to the environment;
[0025] By providing a first reinforcement layer 12, a recovery layer 13 and a second reinforcement layer 14 made of stainless steel, the supporting capacity and strength of the pipeline 1 can be increased. When the pipeline 1 is subjected to a heat-melting treatment using a heat melter, the pipeline 1 is heated and melted, and after entering the heat melter, the second reinforcement layer 14 and the recovery layer 13 are squeezed, causing them to shrink toward the first reinforcement layer 12. After the pipeline 1 is connected to the pipe joint, as the temperature of the pipeline 1 decreases and the second reinforcement layer 14 and the recovery layer 13 are not under pressure, they gradually recover and fit tightly against the pipe joint, thereby improving the stability and sealing of the connection between the pipeline 1 and the pipe joint.
[0026] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the utility model rather than to limit it. Although the utility model has been described in detail with reference to the preferred embodiments, ordinary technicians in the field should understand that the technical solution of the utility model can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution of the utility model, which should be included in the scope of the claims of the utility model.
Claims
1. An antibacterial composite tube, characterized in that: include: Pipeline (1); The pipeline (1) comprises an antibacterial plastic (11), a first reinforcement layer (12), a recovery layer (13) and a second reinforcement layer (14); the first reinforcement layer (12) is located inside the second reinforcement layer (14); the recovery layer (13) is located between the first reinforcement layer (12) and the second reinforcement layer (14); the first reinforcement layer (12), the recovery layer (13) and the second reinforcement layer (14) are integrally arranged; and the antibacterial plastic (11) is coated on the outside of the first reinforcement layer (12), the recovery layer (13) and the second reinforcement layer (14).
2. The antibacterial composite tube according to claim 1, characterized in that: in: The antibacterial plastic (11) comprises an antibacterial layer and plastic.
3. The antibacterial composite tube according to claim 1, characterized in that: in: The first reinforcement layer (12) is made of a stainless steel mesh, and the first reinforcement layer (12) is arranged in a cylindrical shape.
4. The antibacterial composite tube according to claim 1, characterized in that: in: The second reinforcement layer (14) is two arc-shaped stainless steel meshes, and the two arc-shaped stainless steel meshes are symmetrically arranged outside the first reinforcement layer (12).
5. The antibacterial composite tube according to claim 1, characterized in that: in: The recovery layer (13) is a connecting rod made of stainless steel, and the recovery layer (13) is fixedly connected to the first reinforcement layer (12) and the second reinforcement layer (14).