Manganese zinc ferrite magnetic core with high insulation and voltage resistance
By introducing snap-in components and a multi-layer coating structure into the manganese-zinc ferrite core, the problem of unfixed core splicing is solved, more stable splicing is achieved, and the core's voltage resistance and insulation performance are improved.
Patent Information
- Application Number
- CN202420010283.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-03
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing E-type magnetic core cannot be fixed during splicing and is easily scattered due to shaking or touching, resulting in poor splicing effect and affecting use.
A manganese-zinc ferrite core with high insulation and voltage resistance is designed, which is fixedly connected using snap-in components (including snap-in grooves, grooves, telescopic rods, clips, springs, sliders, moving plates and connecting plates). , and provide zinc-nickel alloy coating, carbon fiber layer, galvanized stainless steel coating and insulating coating layer on the surface to improve the overall strength and insulation performance.
It effectively prevents the magnetic core from being scattered due to shaking or touching, improves splicing stability, and meets the needs of use in special environments through enhanced high temperature resistance and insulation performance.
Smart Images

Figure CN221827708U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of manganese-zinc ferrite cores, in particular to a manganese-zinc ferrite core with high insulation and withstand voltage. Background Art
[0002] A magnetic core is a sintered magnetic metal oxide used in coils and transformers of various electronic devices. The shapes of magnetic cores vary, and the E-type magnetic core is the most common one. The E-type magnetic core includes a core body, a winding column, and a side column. Usually, two E-type magnetic cores are installed together in a corresponding manner.
[0003] According to the application number 201821063326.9, a spliced ferrite core is disclosed, which solves the problem of the frame hindering the winding process and facilitates winding.
[0004] The following problems still exist in actual use:
[0005] The splicing method of the above-mentioned device is to align and plug it directly. The magnetic core cannot be fixed when splicing. It is easy to scatter and get out of the splicing state due to shaking or touching when moving before the next step is carried out. The splicing effect is poor and it is not conducive to people's use. Utility Model Content
[0006] In view of the deficiencies in the prior art, the utility model provides a manganese-zinc ferrite core with high insulation and withstand voltage, which has the advantages of good splicing effect and can avoid the core from scattering due to shaking or touching, and solves the problems raised in the background technology.
[0007] The utility model provides the following technical scheme: a manganese-zinc ferrite core with high insulation and withstand voltage, comprising a first core body, both ends of the first core body are fixedly connected with side columns, a clamping assembly is arranged inside the side column, the clamping assembly is composed of a clamping groove, a groove, a telescopic rod, a clamping block, a spring, a slider, a movable plate and a connecting plate, a clamping groove is provided on the upper surface of the side column, grooves are provided on both side walls of the clamping groove, a telescopic rod is fixedly connected to one side wall of the groove, a clamping block is fixedly connected to one end of the telescopic rod, a spring is sleeved on the surface of the telescopic rod, a slider is fixedly connected to one side surface of the clamping block, a movable plate is slidably inserted into one side surface of the side column, and a connecting plate is fixedly connected to one side surface of the movable plate.
[0008] Preferably, the surface of the first core is provided with a zinc-nickel alloy coating layer, the surface of the zinc-nickel alloy coating layer is provided with a carbon fiber layer, the surface of the carbon fiber layer is provided with a galvanized stainless steel coating layer, the surface of the galvanized stainless steel coating layer is provided with an insulating paint layer, and the surface of the insulating paint layer is provided with an antistatic coating.
[0009] Preferably, one end of the spring is fixedly connected to a groove wall on one side of the groove, and the other end of the spring is fixedly connected to a surface on one side of the block.
[0010] Preferably, a second core is mounted on the upper surface of the first core, and both ends of the second core are fixedly connected with clamping blocks, and both side surfaces of the clamping blocks are provided with clamping grooves.
[0011] Preferably, a winding post is fixedly connected to one side surface of the first core body, and a positioning rod is fixedly connected to one end of the winding post.
[0012] Preferably, the zinc-nickel alloy coating layer and the first core body are connected via a conductive adhesive, and the carbon fiber layer and the galvanized stainless steel coating layer are connected via a conductive adhesive.
[0013] Compared with the prior art, the utility model has the following beneficial effects:
[0014] 1. The manganese-zinc ferrite core with high insulation and voltage resistance can be clamped with the second core body by providing a clamping assembly to limit the second core body to prevent it from being scattered or out of the splicing state when it is moved due to shaking or touching. The clamping block enters the clamping groove for clamping, and vice versa, the connecting plates at both ends can be pressed to disassemble, which is convenient for personnel to operate and understand and increases practicality.
[0015] 2. The high insulation and voltage-resistant manganese-zinc ferrite core can increase the overall strength of the core through the zinc-nickel alloy plating layer, the carbon fiber layer and the galvanized stainless steel coating, and improve the overall high temperature resistance of the core, thereby improving the voltage resistance of the core. The insulating coating layer can increase the insulation performance of the core, and it also has the effects of anti-corrosion and anti-ultraviolet. It can have anti-static properties when combined with the anti-static coating to prevent dust from adhering to its surface, and can meet the use requirements in special environments. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a schematic diagram of the overall structure of the utility model device;
[0017] Figure 2 This is a schematic diagram of the second core splicing structure of the utility model;
[0018] Figure 3 This is a schematic diagram of the internal structure of the side column of the utility model;
[0019] Figure 4 This is a schematic diagram of the structure of the clamping block of the utility model;
[0020] Figure 5 It is a schematic diagram of the core surface composition structure of the utility model.
[0021] In the figure: 1. first core body; 2. side column; 3. snap-on assembly; 301. snap-on groove; 302. groove; 303. telescopic rod; 304. snap block; 305. spring; 306. slider; 307. moving plate; 308. connecting plate; 4. second core body; 5. snap-on block; 6. snap groove; 7. winding column; 8. positioning rod; 9. zinc-nickel alloy plating layer; 10. carbon fiber layer; 11. galvanized stainless steel coating; 12. insulating paint layer; 13. antistatic coating. DETAILED DESCRIPTION
[0022] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0023] See also Figure 1 - Figure 4 A manganese-zinc ferrite core with high insulation and withstand voltage comprises a first core body 1, both ends of the first core body 1 are fixedly connected with side columns 2, a clamping assembly 3 is arranged inside the side column 2, the clamping assembly 3 is composed of a clamping groove 301, a groove 302, a telescopic rod 303, a clamping block 304, a spring 305, a slider 306, a moving plate 307 and a connecting plate 308, a clamping groove 301 is opened on the upper surface of the side column 2, grooves 302 are opened on both sides of the groove wall of the clamping groove 301, a telescopic rod 303 is fixedly connected to one side of the groove wall of the groove 302, a clamping block 304 is fixedly connected to one end of the telescopic rod 303, and the telescopic rod 303 is fixedly connected to the clamping block 304. A spring 305 is sleeved on the surface of 03, a slider 306 is fixedly connected to one side surface of the block 304, a movable plate 307 is slidably inserted into one side surface of the side column 2, and a connecting plate 308 is fixedly connected to one side surface of the movable plate 307. One end of the spring 305 is fixedly connected to one side groove wall of the groove 302, and the other end of the spring 305 is fixedly connected to one side surface of the block 304. The second core 4 can be clamped by providing a clamping component 3 to limit the second core 4 to prevent it from scattering and being out of the splicing state due to shaking or touching when moving. At the same time, installation and disassembly are convenient for personnel to operate.
[0024] See also Figure 5The surface of the first core body 1 is provided with a zinc-nickel alloy plating layer 9, the surface of the zinc-nickel alloy plating layer 9 is provided with a carbon fiber layer 10, the surface of the carbon fiber layer 10 is provided with a galvanized stainless steel coating 11, the surface of the galvanized stainless steel coating 11 is provided with an insulating coating layer 12, the surface of the insulating coating layer 12 is provided with an antistatic coating 13, the zinc-nickel alloy plating layer 9 and the first core body 1 are connected by a conductive adhesive, and the carbon fiber layer 10 and the galvanized stainless steel coating 11 are connected by a conductive adhesive. The zinc-nickel alloy plating layer 9, the carbon fiber layer 10 and the galvanized stainless steel coating 11 can improve the pressure resistance of the magnetic core, and the insulating coating layer 12 can increase the insulation performance of the magnetic core, and it also has the effects of corrosion resistance and UV protection.
[0025] See also Figure 2 A second core body 4 is installed on the upper surface of the first core body 1, and both ends of the second core body 4 are fixedly connected with a clamping block 5. Both side surfaces of the clamping block 5 are provided with a clamping groove 6. A winding column 7 is fixedly connected to one side surface of the first core body 1, and one end of the winding column 7 is fixedly connected to a positioning rod 8. When splicing, the positioning rod 8 enters the interior of the second core body 4, which can play a positioning effect and increase stability.
[0026] In the utility model, the working principle of the device is as follows:
[0027] Step 1: When splicing, align the clamping blocks 5 on both ends of the second core 4 with the clamping groove 301 and insert them, so that the clamping blocks 5 enter the clamping groove 301 and squeeze the clamping blocks 304. Since one side surface of the clamping block 304 is arc-shaped, the clamping block 304 is forced to shrink into the groove 302, so that the clamping block 5 enters the inside of the clamping groove 301. When the clamping groove 6 and the clamping block 304 are located on the same horizontal line, the spring 305 is reset due to the force, driving the clamping block 304 to move into the inside of the clamping groove 6, and the clamping is completed, and the splicing is completed. The second core 4 can be limited to prevent it from being scattered and out of the splicing state due to shaking or touching when it moves;
[0028] Step 2: When the magnetic core needs to be disassembled, the connecting plates 308 at both ends are pressed to drive the movable plate 307 to move, so that the movable plate 307 squeezes the slider 306, and the slider 306 is forced to move toward both ends, thereby driving the clamping block 304 to move toward both ends and retract into the groove 302, so that the distance between the clamping block 304 and the clamping slot 6 is increased, and the clamping relationship is disconnected, and the second core body 4 can be lifted upward for disassembly;
[0029] The third step: the zinc-nickel alloy coating 9, the carbon fiber layer 10 and the galvanized stainless steel coating 11 can increase the overall strength of the magnetic core, improve the overall high temperature resistance of the magnetic core, and thus improve the pressure resistance of the magnetic core. The insulating coating layer 12 can increase the insulation performance of the magnetic core, and at the same time has anti-corrosion and anti-ultraviolet effects. In combination with the antistatic coating 13, it can have anti-static properties to prevent dust from adhering to its surface, and can meet the use requirements in special environments.
[0030] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0031] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A manganese-zinc ferrite core with high insulation withstand voltage, comprising a first core body (1), It is characterized in that Both ends of the first core body (1) are fixedly connected to side columns (2), and a clamping assembly (3) is arranged inside the side column (2). The clamping assembly (3) consists of a clamping groove (301), a groove (302), a telescopic rod (303), a clamping block (304), a spring (305), a slider (306), a movable plate (307) and a connecting plate (308). The upper surface of the side column (2) is provided with a clamping groove (301), and groove walls on both sides of the clamping groove (301) are provided with recesses. A groove (302) is provided, a groove wall on one side of the groove (302) is fixedly connected to a telescopic rod (303), one end of the telescopic rod (303) is fixedly connected to a clamping block (304), a spring (305) is sleeved on the surface of the telescopic rod (303), a sliding block (306) is fixedly connected to a surface of one side of the clamping block (304), a moving plate (307) is slidably inserted on a surface of one side of the side column (2), and a connecting plate (308) is fixedly connected to a surface of one side of the moving plate (307).
2. A manganese-zinc ferrite core with high insulation withstand voltage according to claim 1, Features: The surface of the first core (1) is provided with a zinc-nickel alloy coating layer (9), the surface of the zinc-nickel alloy coating layer (9) is provided with a carbon fiber layer (10), the surface of the carbon fiber layer (10) is provided with a galvanized stainless steel coating layer (11), the surface of the galvanized stainless steel coating layer (11) is provided with an insulating coating layer (12), and the surface of the insulating coating layer (12) is provided with an antistatic coating (13).
3. A manganese-zinc ferrite core with high insulation withstand voltage according to claim 1, Features: One end of the spring (305) is fixedly connected to a groove wall on one side of the groove (302), and the other end of the spring (305) is fixedly connected to a surface on one side of the clamping block (304).
4. A manganese-zinc ferrite core with high insulation withstand voltage according to claim 1, Features: A second core (4) is mounted on the upper surface of the first core (1), and both ends of the second core (4) are fixedly connected to a clamping block (5), and both side surfaces of the clamping block (5) are provided with a clamping groove (6).
5. A manganese-zinc ferrite core with high insulation withstand voltage according to claim 1, Features: A winding post (7) is fixedly connected to one side surface of the first core body (1), and a positioning rod (8) is fixedly connected to one end of the winding post (7).
6. A manganese-zinc ferrite core with high insulation withstand voltage according to claim 2, Features: The zinc-nickel alloy coating layer (9) and the first core body (1) are connected via a conductive adhesive, and the carbon fiber layer (10) and the galvanized stainless steel coating layer (11) are connected via a conductive adhesive.