Flat drill welding device
By combining the spark ablation and pulsed direct current of the flat drill welding device with rotating friction welding, the problems of uneven friction welding and materials with different hardness are solved, the equipment cost and energy consumption are reduced, and the welding quality and efficiency are improved.
Patent Information
- Application Number
- CN202323642163.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-29
AI Technical Summary
Friction welding has problems such as vibration, deformation, high equipment cost, low energy utilization efficiency and weld metal fatigue when welding materials that are uneven or have large hardness differences.
A flat drill welding device is used to smooth the welding surface through electric spark ablation, combined with pulsed direct current and rotating friction welding, to reduce the upsetting pressure and rotation speed, use electric sparks to provide heat, increase flash turning tool processing, and control the current to achieve annealing treatment.
It achieves a smooth welding surface, reduces equipment costs and energy consumption, improves welding quality and efficiency, and avoids weld deformation and metal fatigue.
Smart Images

Figure CN221848937U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of welding equipment, and in particular relates to a flat drill welding device and a welding method thereof. Background Art
[0002] Friction welding is a solid phase pressure welding method that uses the heat generated by the friction between the contacting end faces of the weldment to make the end faces reach a thermoplastic state. Subsequently, the upsetting force is quickly applied to achieve welding. Friction welding has the following significant advantages:
[0003] (1) The welding quality is stable, the weldment size accuracy is high, and the joint scrap rate is significantly lower than resistance butt welding and flash butt welding;
[0004] (2) The weld itself has low stress and the welded parts have high straightness;
[0005] (3) It can weld different types of metals, such as the connection between carbon steel and stainless steel, high-speed steel, and the connection between copper and stainless steel, copper and aluminum, aluminum and steel, steel and zirconium, etc.;
[0006] (4) No special cleaning is required for weldments;
[0007] (5) It is easy to realize mechanization and automation, simple to operate, and there is no spark, arc or harmful gas in the welding workplace;
[0008] Although friction welding has many advantages, it also has the following limitations and problems in practical applications:
[0009] (1) When the head of the welded part is uneven or convex in the middle, a turning process must be performed first. Otherwise, the part may vibrate violently, or the linear speed of the middle contact surface may be insufficient, resulting in insufficient friction heat and thus failure to weld.
[0010] (2) Disk-mounted parts and thin-walled parts are prone to deformation because they cannot withstand large upsetting pressure;
[0011] (3) Due to the limitation of the spindle motor power of the welding machine, the maximum cross-section that can be welded by friction welding is currently 20,000 square millimeters, and the one-time investment cost of a high-power friction welding machine is relatively high;
[0012] (4) Due to the limitation of spindle speed, when welding bars with a diameter of less than 6 mm, in order to achieve the required friction line speed, the spindle speed may be as high as 60,000 rpm, which exceeds the upper limit of the speed of ordinary bearings, resulting in a significant increase in costs;
[0013] (5) When welding large-mass parts, most of the motor power is used to accelerate the workpiece rotation. After welding is completed, this part of the kinetic energy needs to be consumed through braking, resulting in reduced energy utilization efficiency;
[0014] (6) When welding materials with large hardness differences, the softer material may have been over-extended by the harder material when the welding temperature is reached, resulting in the formation of larger flash, thereby reducing the material utilization rate;
[0015] (7) When the welding material is hardened steel, the weld seam of friction welding may be a very narrow soft steel area in the annealed state. During transportation and processing, stress may be concentrated in the weld area, resulting in metal fatigue of the weld;
[0016] For this reason, we propose a flat drill welding device and a welding method thereof. Utility Model Content
[0017] The utility model aims to provide a flat drill welding device and a welding method thereof to solve the problems raised in the above background technology.
[0018] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0019] A flat drill welding device comprises a box body, on which a flat drill workpiece clamping mechanism, a flat drill workpiece abutting mechanism, a driving rotating mechanism and a flash turning tool mechanism are arranged, the flat drill workpiece clamping mechanism is arranged between the flat drill workpiece abutting mechanism and the driving rotating mechanism, the flash turning tool mechanism is arranged above the flat drill workpiece clamping mechanism, the driving rotating mechanism is connected to a positive lead, the flat drill workpiece clamping mechanism is connected to a negative lead, and the positive lead and the negative lead are externally connected to a DC power supply;
[0020] The flat drill workpiece clamping mechanism is used to clamp the flat drill workpiece;
[0021] The flat drill workpiece abutment mechanism is used to assist in moving the flat drill workpiece clamping mechanism so that the flat drill workpiece clamping mechanism moves toward the driving rotation mechanism;
[0022] The driving rotation mechanism is used to clamp the workpiece to be welded and drive the workpiece to be welded to rotate;
[0023] A low-voltage pulse direct current is formed between the flat drill workpiece and the workpiece to be welded through a positive wire and a negative wire, and the workpiece to be welded is rotationally friction welded to the flat drill workpiece through the driving rotation mechanism;
[0024] The flash cutting tool mechanism is used for cutting the welding flash of the flat drill workpiece and the workpiece to be welded.
[0025] Preferably, the flat drill workpiece comprises a flat drill portion and a round rod segment, the flat drill portion and the round rod segment are an integrated structure, the flat drill portion is arranged on the flat drill workpiece abutment mechanism, and the round rod segment is arranged on the flat drill workpiece clamping mechanism.
[0026] Preferably, the flat drill workpiece abutment mechanism comprises a cylinder support, an abutment cylinder, a guide rail, an abutment slide seat and a positioning abutment seat;
[0027] The cylinder bracket is arranged on one side of the box body, the abutting cylinder is arranged on the cylinder bracket, the guide slide rail is arranged on the box body, the abutting slide seat is arranged on the guide slide rail, the positioning abutting seat is arranged on the abutting slide seat, the output end of the abutting cylinder is connected to the abutting slide seat, a positioning placement groove is provided on the positioning abutting seat, and the flat drill part is positioned and placed in the positioning placement groove.
[0028] Preferably, the flat drill workpiece clamping mechanism is arranged on the abutting slide, and the flat drill workpiece clamping mechanism comprises a base plate, a clamping seat, a clamping cylinder and a clamping block;
[0029] The bottom plate is arranged on the box body, the clamping seat and the clamping cylinder are symmetrically arranged on the bottom plate, the clamping block is arranged at the output end of the clamping cylinder, and the clamping block and the clamping seat clamp and fix the round rod segment;
[0030] The bottom plate is connected to the negative electrode lead.
[0031] Preferably, the driving rotating mechanism comprises a motor mounting plate, a driving motor, a transmission belt, a driving spindle, a supporting seat and a rotating shaft seat;
[0032] The driving motor is installed in the box body through the motor mounting plate, the rotating shaft seat is installed on the box body through the supporting seat, the driving spindle is installed on the rotating shaft seat, and the output end of the driving motor and the driving spindle are connected through the transmission belt.
[0033] Preferably, the driving spindle clamps the workpiece to be welded via a spring chuck, and the round rod segments on the workpiece to be welded and the flat drill workpiece are aligned.
[0034] Preferably, an insulating spacer is provided between the support seat and the rotating shaft seat, a conductive live wire is connected to the rotating shaft seat via a carbon brush, and a conductive disk connected to the carbon brush is provided on the driving main shaft.
[0035] Preferably, the flash turning tool mechanism comprises a transverse guide rail, a transverse adjustment plate, a transverse adjustment cylinder, a longitudinal guide rail, a longitudinal adjustment plate, a longitudinal adjustment cylinder and a turning tool;
[0036] The transverse adjustment plate is mounted on the box body through the transverse guide rail, the transverse adjustment cylinder is mounted on the box body, and the output end of the transverse adjustment cylinder is connected to the transverse adjustment plate;
[0037] The longitudinal adjustment plate is mounted on the transverse adjustment plate through the longitudinal guide rail, the longitudinal adjustment cylinder is mounted on the box body, and the output end of the longitudinal adjustment cylinder is connected to the longitudinal adjustment plate;
[0038] The turning tool is arranged on the longitudinal adjustment plate.
[0039] Compared with the prior art, the beneficial effects of the utility model are:
[0040] 1. Welding starts with electric spark ablation of the welding surface to make the welding surface flat, eliminating two pre-processing steps on the welding surfaces of the two workpieces;
[0041] 2. During welding, electric sparks are used to share the heating, and the pressure of the workpiece forging can be reduced to less than one tenth, so weak workpieces can also be welded;
[0042] 3. The welding heat is mainly provided by the electric spark arc, and the power of the large welding spindle can be reduced to only one percent, reducing the equipment cost;
[0043] 4. The welding heat is mainly provided by the electric spark arc. The welding speed of small diameter bars is reduced from 60,000 rpm to 3,000 rpm, and ordinary ball bearings can bear the load.
[0044] 5. The welding heat is mainly provided by the electric spark arc. The welding speed is reduced, the energy to drive the large mass workpiece is reduced exponentially, and the energy utilization rate is improved;
[0045] 6. When welding materials with a large difference in hardness, the workpieces on both sides are preheated by electric sparks. The upsetting force on the workpieces is small and they will not be excessively squeezed out of the welding area during preheating.
[0046] 7. The heating annealing treatment of the utility model can be achieved by simply controlling the current, which can also solve the welding problem of the quenched material;
[0047] 8. As the welding surface of the workpiece is flat, the speed of the driving spindle 404 is reduced, the top forging pressure is reduced, and the rigidity of the entire equipment can also be reduced. An open structure can be used to save costs and facilitate operation. BRIEF DESCRIPTION OF THE DRAWINGS
[0048] Figure 1 It is a three-dimensional structural schematic diagram of the utility model;
[0049] Figure 2 It is a three-dimensional structural schematic diagram of the utility model;
[0050] Figure 3 It is a three-dimensional structural schematic diagram of the utility model;
[0051] Figure 4 It is a three-dimensional structural schematic diagram of the utility model;
[0052] Figure 5 It is a three-dimensional structural schematic diagram of the utility model.
[0053] In the figure: 1, box; 2, flat drill workpiece clamping mechanism; 201, bottom plate; 202, clamping seat; 203, clamping cylinder; 204, clamping block; 3, flat drill workpiece abutment mechanism; 301, cylinder bracket; 302, abutment cylinder; 303, guide slide rail; 304, abutment slide seat; 305, positioning abutment seat; 306, positioning placement groove; 4, driving rotary machine; 401, motor mounting plate; 402, driving motor; 403, transmission belt; 4 04. Driving spindle; 405. Support seat; 406. Rotating shaft seat; 407. Insulating spacer; 408. Carbon brush; 409. Conductive disk; 5. Flash turning tool mechanism; 501. Transverse guide rail; 502. Transverse adjustment plate; 503. Transverse adjustment cylinder; 504. Longitudinal guide rail; 505. Longitudinal adjustment plate; 506. Longitudinal adjustment cylinder; 507. Turning tool; 6. Flat drill workpiece; 601. Flat drill part; 602. Round rod segment; 7. Workpiece to be welded. DETAILED DESCRIPTION
[0054] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0055] See also Figure 1-Figure 5 The utility model provides
[0056] A flat drill welding device comprises a box body 1, on which a flat drill workpiece clamping mechanism 2, a flat drill workpiece abutting mechanism 3, a driving rotating mechanism 4 and a flash turning tool mechanism 5 are arranged, the flat drill workpiece clamping mechanism 2 is arranged between the flat drill workpiece abutting mechanism 3 and the driving rotating mechanism 4, the flash turning tool mechanism 5 is arranged above the flat drill workpiece clamping mechanism 2, the driving rotating mechanism 4 is connected to a positive wire, the flat drill workpiece clamping mechanism 2 is connected to a negative wire, and the positive wire and the negative wire are externally connected to a DC power supply;
[0057] The flat drill workpiece clamping mechanism 2 is used to clamp the flat drill workpiece 6, which includes a flat drill portion 601 and a round rod segment 602. The flat drill portion 601 and the round rod segment 602 are an integrated structure. The flat drill portion 601 is arranged on the flat drill workpiece abutment mechanism 3, and the round rod segment 602 is arranged on the flat drill workpiece clamping mechanism 2. The flat drill workpiece clamping mechanism 2 is arranged on the abutment slide 304. The flat drill workpiece clamping mechanism 2 includes a base plate 201, a clamping seat 202, a clamping cylinder 203 and a clamping block 204; the base plate 201 is arranged on the box body 1, the clamping seat 202 and the clamping cylinder 203 are symmetrically arranged on the base plate 201, the clamping block 204 is arranged at the output end of the clamping cylinder 203, and the clamping block 204 and the clamping seat 202 clamp and fix the round rod segment 602; the base plate 201 is connected to the negative electrode wire;
[0058] The flat drill workpiece abutment mechanism 3 is used for assisting the movement of the flat drill workpiece clamping mechanism 2, so that the flat drill workpiece clamping mechanism 2 moves toward the driving rotation mechanism 4. The flat drill workpiece abutment mechanism 3 includes a cylinder support 301, an abutment cylinder 302, a guide rail 303, an abutment slide 304 and a positioning abutment seat 305; the cylinder support 301 is arranged on one side of the box body 1, the abutment cylinder 302 is arranged on the cylinder support 301, the guide rail 303 is arranged on the box body 1, the abutment slide 304 is arranged on the guide rail 303, the positioning abutment seat 305 is arranged on the abutment slide 304, the output end of the abutment cylinder 302 is connected to the abutment slide 304, and a positioning placement groove 306 is provided on the positioning abutment seat 305, and the flat drill part 601 is positioned and placed in the positioning placement groove 306;
[0059] The driving rotating mechanism 4 is used to clamp the workpiece 7 to be welded, and drive the workpiece 7 to be welded to rotate. The driving rotating mechanism 4 includes a motor mounting plate 401, a driving motor 402, a transmission belt 403, a driving spindle 404, a support seat 405 and a rotating shaft seat 406; the driving motor 402 is installed in the box body 1 through the motor mounting plate 401, the rotating shaft seat 406 is installed on the box body 1 through the support seat 405, the driving spindle 404 is installed on the rotating shaft seat 406, the output end of the driving motor 402 and the driving spindle 404 are connected by transmission through the transmission belt 403, the driving spindle 404 clamps the workpiece 7 to be welded through a spring chuck, and the round rod segment 602 on the workpiece 7 to be welded and the flat drill workpiece 6 are aligned, an insulating spacer 407 is arranged between the support seat 405 and the rotating shaft seat 406, the rotating shaft seat 406 is connected to a conductive live wire through a carbon brush 408, and a conductive disk 409 connected to the carbon brush 408 is arranged on the driving spindle 404;
[0060] A low-voltage pulse direct current is formed between the flat drill workpiece 6 and the workpiece to be welded 7 through the positive and negative wires, and the workpiece to be welded 7 is rotationally friction welded to the flat drill workpiece 6 by driving the rotating mechanism 4;
[0061] The flash cutting tool mechanism 5 is used for cutting the welding flash of the flat drill workpiece 6 and the workpiece to be welded 7. The flash cutting tool mechanism 5 includes a transverse guide rail 501, a transverse adjustment plate 502, a transverse adjustment cylinder 503, a longitudinal guide rail 504, a longitudinal adjustment plate 505, a longitudinal adjustment cylinder 506 and a cutting tool 507; the transverse adjustment plate 502 is installed on the box body 1 through the transverse guide rail 501, the transverse adjustment cylinder 503 is installed on the box body 1, and the output end of the transverse adjustment cylinder 503 is connected to the transverse adjustment plate 502; the longitudinal adjustment plate 505 is installed on the transverse adjustment plate 502 through the longitudinal guide rail 504, the longitudinal adjustment cylinder 506 is installed on the box body 1, and the output end of the longitudinal adjustment cylinder 506 is connected to the longitudinal adjustment plate 505; the cutting tool 507 is arranged on the longitudinal adjustment plate 505.
[0062] The utility model adopts a method of applying pulse voltage between two workpieces to assist friction welding, solves the problem of insufficient heat source by single friction heating, reduces welding process requirements, improves welding quality, and reduces welding equipment cost and welding use cost.
[0063] The utility model provides a welding method for a flat drill welding device, comprising the following steps:
[0064] A. Workpiece clamping and fixing:
[0065] First, the workpiece 7 to be welded is mounted on the driving spindle 404 through a spring chuck, and then the flat drill portion 601 of the flat drill workpiece 6 is positioned and placed in the positioning groove 306, and the round rod segment 602 is placed on the clamping seat 202, and the clamping cylinder 203 is started, and the clamping cylinder 203 drives the clamping block 204 to clamp and fix the round rod segment 602 on the clamping seat 202, so that the flat drill workpiece 6 is clamped and fixed;
[0066] B. Pulse voltage heating:
[0067] Then, the abutting cylinder 302 is started, and the abutting cylinder 302 pushes the abutting slide 304 to move along the guide rail 303, so that the round rod segment 602 of the flat drill workpiece 6 moves toward the workpiece 7 to be welded, and then the external DC power supply applies low-voltage pulse DC to the two workpieces through the positive wire and the negative wire, so that a small arc is generated between the flat drill workpiece 6 and the workpiece 7 to be welded, so that the facing surfaces of the flat drill workpiece 6 and the workpiece 7 to be welded begin to heat and melt;
[0068] In the initial stage of welding, due to the manufacturing and processing of the workpieces, the contact surface may not be completely flat, which means that there will be some local protrusions on the contact surface of the two workpieces. These protrusions are called "high spots";
[0069] When the two workpieces are in contact, the uneven high points of the workpieces are instantly blown out of the welding surface by the pressure of the large current vaporization. The uneven high points of the welding surface are first burned and vaporized. After the original high points disappear, new high points are continuously burned until the other parts of the welding surface begin to gradually contact. As the contact area increases, the average current of the contact surface is reduced to the critical current, and the gasification phenomenon with sparks no longer occurs. The current can be adjusted by the voltage. In this process, the welding surface absorbs part of the heat input by the electric spark, arc, and resistance. When the welding surface is fully in contact, the rotational friction of the workpiece becomes the main energy input, and the welding surface continues to be heated. When the weld metal softens, the materials of the two workpieces are fully fused together by rotating left and right, and the impurity oxide layer on the weld surface is squeezed out of the weld.
[0070] As the welding process progresses, these high points gradually melt and disappear, allowing the other parts of the welding surface to gradually contact. In this process, since the original high points have melted, they form a layer of hot metal in the molten state. This layer of hot metal acts as a "medium" to help the contact surfaces of the two workpieces merge better;
[0071] When the workpieces soften and begin to fuse, the softened metal will squeeze out of the welding surface, and the total length of the two workpieces will be significantly shortened by 2-3 mm compared to the friction heating stage. By measuring this displacement, it can be determined that the welding fusion stage is completed;
[0072] As time goes by, as more high points melt and more contact surfaces come into contact, eventually the contact surfaces of the two workpieces will be completely in contact, forming a uniform, continuous weld surface. At this time, the above-mentioned hot metal covers the weld surface, and this layer of hot metal will form a solid weld after cooling, thus ensuring the quality and strength of the weld.
[0073] When the fusion is detected, the spindle will brake and stop within 0.1-0.3 seconds, and the 302 cylinder will continue to maintain pressure. After about 1 second, the weld will solidify and the welding is completed;
[0074] This step ensures that the welding surfaces of the two workpieces are in full contact, and the heat generated by the arc achieves metal fusion, thus forming a strong weld;
[0075] Due to the flow of current and the contact resistance, small arcs will occur at these high points, specifically:
[0076] 1. Contact resistance: When two metal objects come into contact, since their surfaces are not completely smooth, only some tiny contact points (i.e. high points) are actually in contact. The contact resistance between these tiny contact points is relatively high, and the current that can pass through is small;
[0077] 2. Current flow: When current flows through these high-resistance contact points, a lot of heat is generated at the contact points because the greater the resistance, the greater the heat generated by the current passing through it (according to Joule's law, Q=I^2Rt, where Q is heat, I is current, R is resistance, and t is time);
[0078] 3. Arc generation: When the temperature of these contact points rises to a level high enough to vaporize the metal, the metal vapor forms a conductive path, which is the arc. The arc is a high-temperature ionized gas that can transfer current between the two electrodes.
[0079] 4. Continuation of the arc: Once the arc is formed, its own temperature will further heat the surrounding metal, vaporizing more metal and maintaining the existence of the arc. In this case, the arc is maintained not only by the heat generated by the contact resistance, but also by the heat generated by the arc itself.
[0080] 5. Effect of the arc: The high temperature generated by the arc can melt the metal quickly, which is beneficial in the welding process because it can help melt the high points and make the weld surface smoother;
[0081] To summarize, due to the flow of current and contact resistance, a lot of heat is generated at the high points. When this heat is high enough, an arc is formed. This arc can quickly melt the metal and help the welding process;
[0082] C. Rotary friction welding:
[0083] While the pulse voltage is heating, the driving motor 402 is started, and the driving motor 402 drives the driving spindle 404 to rotate through the transmission belt 403, so that the workpiece 7 to be welded follows the driving spindle 404 to rotate, so that the round rod segment 602 and the rotating workpiece 7 to be welded are in contact and friction, and the contact pressure between the flat drill workpiece 6 and the workpiece 7 to be welded is maintained, so that the workpiece 7 to be welded and the flat drill workpiece 6 are frictionally welded to form a welded workpiece;
[0084] In this step, the rotation of the workpieces generates friction heat, so that the contact surface of the workpieces reaches a thermoplastic state. When the materials of the two workpieces are fully mixed on the contact surface, the rotation of the workpieces is stopped to avoid excessive friction heat from continuing to be generated, thereby avoiding excessive thermal effects on the welding area;
[0085] Although the workpieces have stopped rotating, a certain amount of pressure must still be maintained on the workpieces to ensure that the two workpieces remain in close contact during the cooling and solidification process, thereby ensuring the integrity and strength of the weld. In addition, maintaining pressure can also help to exclude any residual air or gas in the welding area, thereby avoiding porosity or other defects in the weld;
[0086] While maintaining the pressure, the workpiece begins to cool naturally. During the cooling process, the high-temperature metal in the welding area gradually solidifies to form a solid weld.
[0087] As the temperature drops, the metal in the welding area begins to change from a thermoplastic state to a solid state, and eventually the two workpieces are stably bonded together;
[0088] D. Welding flash turning process:
[0089] After the cooling of the welding area is completed, the clamping cylinder 203 contracts, so that the clamping block 204 releases the flat drill workpiece 6, and then the abutment cylinder 302 begins to contract, so that the flat drill part 601 of the flat drill workpiece 6 leaves the positioning placement groove 306 on the positioning abutment seat 305, and the lateral adjustment cylinder 503 is started, and the lateral adjustment cylinder 503 pushes the lateral adjustment plate 502 to move along the lateral guide rail 501 for lateral adjustment, and the longitudinal adjustment cylinder 506 is started, and the longitudinal adjustment cylinder 506 pushes the longitudinal adjustment plate 505 to move along the longitudinal guide rail 504 for longitudinal adjustment, so that the turning tool 507 follows the longitudinal adjustment plate 505 to align the welding area of the welding workpiece, and then the driving motor 402 is started, and the driving motor 402 drives the driving spindle 404 to rotate through the transmission belt 403, so that the welding workpiece follows the driving spindle 404 to rotate, so that the turning tool 507 turns the welding flash of the welding workpiece to obtain a finished welded workpiece.
[0090] In this embodiment, if Figure 1 As shown, after the flat drill workpiece 6 and the workpiece to be welded 7 are welded, if the flat drill workpiece 6 and the workpiece to be welded 7 are hardened steel, low-voltage direct current is applied again between the flat drill workpiece 6 and the workpiece to be welded 7 to make the flat drill workpiece 6 and the workpiece to be welded 7 generate heat through resistance, thereby expanding the heating range, making the welding annealing area larger, and preventing excessive stretching and deformation of the weld area caused by the hardness difference of the material.
[0091] The utility model has the following beneficial effects:
[0092] 1. Welding starts with electric spark ablation of the welding surface to make the welding surface flat, eliminating two pre-processing steps on the welding surfaces of the two workpieces;
[0093] 2. Electric sparks share the heating during welding, which can reduce friction and pressure. The pressure of workpiece upsetting can be reduced to less than one tenth, and weak workpieces can also be welded;
[0094] 3. The welding heat is mainly provided by the electric spark arc, and the power of the large welding spindle can be reduced to only one percent, reducing the equipment cost;
[0095] 4. The welding heat is mainly provided by the electric spark arc. The welding speed of small diameter bars is reduced from 60,000 rpm to 3,000 rpm, and ordinary ball bearings can bear the load.
[0096] 5. The welding heat is mainly provided by the electric spark arc. The welding speed is reduced, the energy to drive the large mass workpiece is reduced exponentially, and the energy utilization rate is improved;
[0097] 6. When welding materials with a large difference in hardness, the workpieces on both sides are preheated by electric sparks. The upsetting force on the workpieces is small and they will not be excessively squeezed out of the welding area during preheating.
[0098] 7. The heating annealing treatment of the utility model can be achieved by simply controlling the current, which can also solve the welding problem of the quenched material;
[0099] 8. As the welding surface of the workpiece is flat, the speed of the driving spindle 404 is reduced, the upsetting pressure is reduced, and the rigidity of the entire equipment can also be reduced. An open structure can be used, which saves costs and facilitates operation;
[0100] 9. Compared with the single flash welding equipment, it is convenient to add the flash turning tool mechanism and improve the integration of the equipment;
[0101] 10. The rotation speed of the driving spindle 404 is reduced, so that workpieces with large eccentricity can be welded.
[0102] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A flat drill welding device, It is characterized in that The invention comprises a box body (1), wherein the box body (1) is provided with a flat drill workpiece clamping mechanism (2), a flat drill workpiece abutting mechanism (3), a driving rotating mechanism (4) and a flash turning tool mechanism (5), wherein the flat drill workpiece clamping mechanism (2) is arranged between the flat drill workpiece abutting mechanism (3) and the driving rotating mechanism (4), and the flash turning tool mechanism (5) is arranged above the flat drill workpiece clamping mechanism (2), the driving rotating mechanism (4) is connected to a positive lead, and the flat drill workpiece clamping mechanism (2) is connected to a negative lead, and the positive lead and the negative lead are externally connected to a DC power supply; The flat drill workpiece clamping mechanism (2) is used to clamp the flat drill workpiece (6); The flat drill workpiece abutment mechanism (3) is used to assist in moving the flat drill workpiece clamping mechanism (2) so that the flat drill workpiece clamping mechanism (2) moves toward the driving rotation mechanism (4); The driving rotation mechanism (4) is used to clamp the workpiece to be welded (7) and drive the workpiece to be welded (7) to rotate; A low-voltage pulse direct current is formed between the flat drill workpiece (6) and the workpiece to be welded (7) via a positive wire and a negative wire, and the workpiece to be welded (7) is rotationally friction welded onto the flat drill workpiece (6) via the driving rotation mechanism (4); The flash cutting tool mechanism (5) is used to cut the welding flash of the flat drill workpiece (6) and the workpiece to be welded (7).
2. A flat drill welding device according to claim 1, Features: The flat drill workpiece (6) comprises a flat drill portion (601) and a round rod segment (602); the flat drill portion (601) and the round rod segment (602) are an integrated structure; the flat drill portion (601) is arranged on the flat drill workpiece abutment mechanism (3), and the round rod segment (602) is arranged on the flat drill workpiece clamping mechanism (2).
3. A flat drill welding device according to claim 2, Features: The flat drill workpiece abutment mechanism (3) comprises a cylinder support (301), an abutment cylinder (302), a guide slide rail (303), an abutment slide seat (304) and a positioning abutment seat (305); The cylinder support (301) is arranged on one side of the box body (1), the abutting cylinder (302) is arranged on the cylinder support (301), the guide rail (303) is arranged on the box body (1), the abutting slide seat (304) is arranged on the guide rail (303), the positioning abutting seat (305) is arranged on the abutting slide seat (304), the output end of the abutting cylinder (302) is connected to the abutting slide seat (304), and a positioning placement groove (306) is provided on the positioning abutting seat (305), and the flat drill portion (601) is positioned and placed in the positioning placement groove (306).
4. A flat drill welding device according to claim 3, Features: The flat drill workpiece clamping mechanism (2) is arranged on the abutting slide seat (304), and the flat drill workpiece clamping mechanism (2) comprises a base plate (201), a clamping seat (202), a clamping cylinder (203) and a clamping block (204); The bottom plate (201) is arranged on the box body (1), the clamping seat (202) and the clamping cylinder (203) are symmetrically arranged on the bottom plate (201), the clamping block (204) is arranged at the output end of the clamping cylinder (203), and the clamping block (204) and the clamping seat (202) clamp and fix the round rod segment (602); The bottom plate (201) is connected to a negative electrode lead.
5. A flat drill welding device according to claim 4, Features: The driving rotation mechanism (4) comprises a motor mounting plate (401), a driving motor (402), a driving belt (403), a driving main shaft (404), a supporting seat (405) and a rotating shaft seat (406); The drive motor (402) is installed in the housing (1) via the motor mounting plate (401); the rotating shaft seat (406) is installed on the housing (1) via the support seat (405); the drive spindle (404) is installed on the rotating shaft seat (406); and the output end of the drive motor (402) and the drive spindle (404) are connected in transmission via the transmission belt (403).
6. A flat drill welding device according to claim 5, Features: The driving spindle (404) clamps the workpiece (7) to be welded via a spring chuck, and the workpiece (7) to be welded and the round rod segment (602) on the flat drill workpiece (6) are aligned.
7. A flat drill welding device according to claim 6, Features: An insulating spacer (407) is provided between the support seat (405) and the rotating shaft seat (406); a conductive live wire is connected to the rotating shaft seat (406) via a carbon brush (408); and a conductive disk (409) connected to the carbon brush (408) is provided on the driving main shaft (404).
8. A flat drill welding device according to claim 1, Features: The flash cutting tool mechanism (5) comprises a transverse guide rail (501), a transverse adjustment plate (502), a transverse adjustment cylinder (503), a longitudinal guide rail (504), a longitudinal adjustment plate (505), a longitudinal adjustment cylinder (506) and a cutting tool (507); The transverse adjustment plate (502) is mounted on the box body (1) via the transverse guide rail (501), the transverse adjustment cylinder (503) is mounted on the box body (1), and the output end of the transverse adjustment cylinder (503) is connected to the transverse adjustment plate (502); The longitudinal adjustment plate (505) is mounted on the transverse adjustment plate (502) via the longitudinal guide rail (504); the longitudinal adjustment cylinder (506) is mounted on the box body (1); and the output end of the longitudinal adjustment cylinder (506) is connected to the longitudinal adjustment plate (505); The turning tool (507) is arranged on the longitudinal adjustment plate (505).
Citation Information
Cited By
Flat drill welding device and welding method thereof
CN117548885A