Charging system for producing blanks with different section diameters by serially connecting graphitization furnaces

By designing a multi-layer insulation and stacking structure in the series graphitization furnace, the problem of loading blanks with different cross-sectional diameters is solved, the output is increased and the energy consumption is reduced, the graphitization degree and resistivity are ensured, and a better Safe and efficient power delivery processing.

CN221859218UActive Publication Date: 2024-10-18BAOFANG CARBON MATERIALS&TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323567096.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-26
Publication Date
2024-10-18
Estimated Expiration
2033-12-26

AI Technical Summary

Technical Problem

Existing series-connected graphitization furnaces cannot meet the furnace installation needs of electrodes of all specifications, resulting in low production capacity, high cost, and resistivity that cannot meet user needs, especially in the processing of billets with different cross-sectional diameters, resulting in low output and energy consumption per ton. high.

Method used

A furnace loading system for serially connecting graphitization furnaces to produce billets with different cross-section diameters is designed, including a laying module, a stacking module, a unloading module and a connecting module. Through the multi-layer insulation of the calcined petroleum coke layer and the semi-graphitized petroleum coke layer The connection between the structure and the conductive copper plate enables effective stacking and power transmission of multi-diameter blanks.

Benefits of technology

It increases output, reduces energy consumption, ensures satisfactory graphitization degree and resistivity, limits the position of conductive electrodes through multi-level insulation and stacking, and ensures the safety and efficiency of power transmission.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221859218U_ABST
    Figure CN221859218U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of internal serial graphitization furnaces, in particular to a furnace charging system for producing blanks with different section diameters by serial graphitization furnaces. Comprising a laying module, a stacking module, a discharging module and a connecting module. The laying module is used for laying heat-insulating materials at the bottom in the furnace to form a heat-insulating layer; the stacking module is used for stacking blanks on the heat preservation layer to form a blank layer; the discharging module is used for covering the surface of the stacking module with a heat preservation material; the connecting module is used for connecting the stacking module. The technical problem that multiple batches of blanks can only be independently treated in batches is solved, the furnace temperature can reach 2600 DEG C or above through multiple power transmission temperature rise tests, ideal graphite structure materials can be obtained, the charging mode is more reasonable, the yield is increased, energy consumption is reduced, the positions of conductive electrodes are limited through multi-layer heat preservation and stacking, and the production efficiency is improved. Power supply loading is more stable, and power transmission safety is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of internally connected graphitization furnaces, in particular to a furnace loading system for serially connected graphitization furnaces to produce blanks with different cross-sectional diameters. Background Art

[0002] With the continuous development of the carbon industry and technological progress, the internal graphitization process technology has been widely used. The internal graphitization process technology has the advantages of low power consumption in the production process, good graphitization homogeneity of the product, short production cycle, low pollution, and single materials. It is used by many domestic graphite electrode manufacturers;

[0003] At present, due to the different furnace chamber designs, the series graphitization furnace cannot meet the requirements of loading electrodes of all specifications. Some specifications of electrodes are not loaded in combination, and the production capacity cannot reach the optimal loading capacity, the energy consumption remains high, and the resistivity is difficult to meet the needs of users. The internal series graphitization furnace uses the same specification of electrodes to load the furnace, which has low output and high cost and can no longer fully meet the market demand. The use of series graphitization furnaces to load multiple specifications of electrodes is increasing.

[0004] When loading billets of different diameters in a series graphitization furnace, it is necessary to first connect the billets with larger cross-sectional area and larger diameter into 1 or 2 columns and stack them on the lower layer, and stack the billets with smaller cross-sectional area and smaller diameter into 1 or 2 columns on the upper layer. Fill the material according to the process requirements, and heat it up to above 2600℃ after power supply, so as to achieve the heat treatment effect. Different ways of loading the furnace may lead to low billet output, high energy consumption per ton, failure to achieve the ideal graphitization degree, and resistivity that cannot meet the needs of users. For this reason, we design a loading system for the production of billets of different cross-sectional diameters in a series graphitization furnace to provide another technical solution to the above technical problems. Utility Model Content

[0005] Based on this, it is necessary to provide a furnace loading system for producing billets with different cross-sectional diameters in series with graphitization furnaces to solve the above technical problems, which is used to solve the technical problems raised in the above background technology.

[0006] In order to solve the above technical problems, the utility model adopts the following technical solutions:

[0007] A furnace loading system for connecting graphitization furnaces in series to produce billets with different cross-sectional diameters.

[0008] A laying module, a stacking module, a material discharging module and a connection module are arranged in the graphitization furnace;

[0009] The laying module is divided into a calcined petroleum coke layer IV and a calcined petroleum coke layer V, and the calcined petroleum coke layer IV and the calcined petroleum coke layer V are used to lay a thermal insulation layer at the bottom of the furnace;

[0010] The stacking module is divided into a calcined petroleum coke layer I and a calcined petroleum coke layer II, the calcined petroleum coke layer II wraps the crucible and fills the gap between the crucibles, the calcined petroleum coke layer I is arranged on both sides of the calcined petroleum coke layer II, the crucible is filled with materials to be graphitized to form a blank column, and the calcined petroleum coke layer I and the calcined petroleum coke layer II are used to stack on the upper part of the insulation layer to form a blank layer;

[0011] The discharge module is divided into a semi-graphitized petroleum coke layer and a calcined petroleum coke layer III, and the calcined petroleum coke layer III and the semi-graphitized petroleum coke layer are arranged layer by layer on the upper part of the blank layer, and the calcined petroleum coke layer III and the semi-graphitized petroleum coke layer are used to cover the surface of the stacking module with insulation material to form an upper insulation layer;

[0012] The connection module is divided into a conductive copper plate and a conductive electrode. The conductive electrodes are arranged at both ends of the blank layer. The conductive copper plate clamps the conductive electrode and is energized for operation. The conductive copper plate and the conductive electrode are used to connect the stacking module.

[0013] The crucible is arranged in a horizontal direction, and the crucible is arranged parallel to an axis from a furnace head to a furnace tail of the graphitization furnace.

[0014] The calcined petroleum coke layer I is composed of petroleum coke with a particle size of 0-2mm, the calcined petroleum coke layer II is composed of petroleum coke with a particle size of 8-25mm, the semi-graphitized petroleum coke layer is composed of semi-graphitized petroleum coke with a particle size of 0-2mm, the calcined petroleum coke layer III is composed of calcined petroleum coke with a particle size of 3-8mm, the calcined petroleum coke layer IV is composed of petroleum coke with a particle size of 8-25mm, and the calcined petroleum coke layer V is composed of petroleum coke with a particle size of 0-2mm.

[0015] The thickness of the thermal insulation layer of the laying module and the upper thermal insulation layer of the discharge module is ≥550mm.

[0016] The crucibles of the blank column are spliced ​​in series end to end, and a flexible graphite pad with a thickness of 20 mm is arranged at the splicing position between the crucibles.

[0017] The distance between the blank columns is 80 mm.

[0018] The blank columns are stacked layer by layer, the diameter of the blank column in the lower layer is larger than the diameter of the blank column in the lower layer, and 1 or 2 blank columns are arranged in the same layer.

[0019] The connection module is used to connect the conductive electrodes in the stacking module to form a graphitized power transmission area, and the conductive electrodes are pressed and contacted through the conductive copper plate to connect the circuit.

[0020] It can be seen without a doubt that the above-mentioned technical solution of the present application can definitely solve the technical problem to be solved by the present application.

[0021] At the same time, through the above technical solutions, the utility model has at least the following beneficial effects:

[0022] The utility model provides a furnace loading system for producing billets with different cross-sectional diameters by connecting graphitizing furnaces in series. By adopting the graphitizing furnaces in series, the technical requirements for stacking and graphitizing billets with different diameters are achieved. The structure effectively guarantees the process requirements for the conductive electrodes in the furnace. The billets with multiple diameters can be processed at one time through the stacking of single-layer and multi-layer billet columns and the use of the equipment, thereby solving the technical problem that multiple batches of billets can only be processed separately in batches. The furnace temperature can reach above 2600°C after multiple power supply and temperature rise tests, and ideal graphite structural materials can be obtained. The loading method is more reasonable, which not only improves the output and reduces the energy consumption, but also limits the conductive electrode position through multi-level insulation and stacking, and the power supply loading is more stable to ensure the safety of power supply. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0024] Figure 1 It is a partial cross-sectional view of the furnace loading of the utility model from top view;

[0025] Figure 2 It is a partial cross-sectional view of the furnace loading side of the utility model;

[0026] Figure 3 This is a schematic diagram of the first embodiment of the utility model stacking layer by layer;

[0027] Figure 4 This is a schematic diagram of a second embodiment of the utility model stacking layer by layer;

[0028] In the figure: calcined petroleum coke layer Ⅰ1; calcined petroleum coke layer Ⅱ2; crucible 3; semi-graphitized petroleum coke layer 4; calcined petroleum coke layer Ⅲ5; calcined petroleum coke layer Ⅳ6; calcined petroleum coke layer Ⅴ7; conductive copper plate 8; conductive electrode 9. DETAILED DESCRIPTION

[0029] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described here are only used to explain the utility model and are not used to limit the utility model.

[0030] In order to enable those skilled in the art to better understand the solution of the utility model, the technical solution in the embodiments of the utility model will be clearly and completely described below in conjunction with the accompanying drawings.

[0031] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features and technical solutions in the embodiments may be combined with each other.

[0032] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0033] Reference Figure 1 , a furnace loading system for connecting graphitization furnaces in series to produce billets with different cross-sectional diameters,

[0034] A laying module, a stacking module, a material discharging module and a connection module are arranged in the graphitization furnace;

[0035] The laying module is divided into a calcined petroleum coke layer IV6 and a calcined petroleum coke layer V7, and the calcined petroleum coke layer IV6 and the calcined petroleum coke layer V7 are used to lay a heat-insulating layer at the bottom of the furnace;

[0036] The stacking module is divided into a calcined petroleum coke layer I1 and a calcined petroleum coke layer II2, the calcined petroleum coke layer II2 wraps the crucible 3 and fills the gap between the crucibles, the calcined petroleum coke layer I1 is arranged on both sides of the calcined petroleum coke layer II2, the crucible 3 is filled with the material to be graphitized to form a blank column, and the calcined petroleum coke layer I1 and the calcined petroleum coke layer II2 are used to stack on the upper part of the insulation layer to form a blank layer;

[0037] The discharge module is divided into a semi-graphitized petroleum coke layer 4 and a calcined petroleum coke layer III5. The calcined petroleum coke layer III5 and the semi-graphitized petroleum coke layer 4 are arranged layer by layer on the upper part of the blank layer. The calcined petroleum coke layer III5 and the semi-graphitized petroleum coke layer 4 are used to cover the surface of the stacking module with insulation material to form an upper insulation layer.

[0038] The connection module is divided into a conductive copper plate 8 and a conductive electrode 9. The conductive electrode 9 is arranged at both ends of the blank layer. The conductive copper plate 8 clamps the conductive electrode 9 and is energized. The conductive copper plate 8 and the conductive electrode 9 are used to connect the stacking module.

[0039] The crucible 3 is arranged in the horizontal direction, and the crucible 3 is arranged parallel to the axis from the furnace head to the furnace tail of the graphitization furnace. The above structure and furnace loading method realizes multiple, multi-layer, and multi-diameter mixed furnace loading, which greatly increases the furnace loading capacity.

[0040] The calcined petroleum coke layer Ⅰ1 is composed of petroleum coke with a particle size of 0-2mm, the calcined petroleum coke layer Ⅱ2 is composed of petroleum coke with a particle size of 8-25mm, the semi-graphitized petroleum coke layer 4 is composed of semi-graphitized petroleum coke with a particle size of 0-2mm, the calcined petroleum coke layer Ⅲ5 is composed of calcined petroleum coke with a particle size of 3-8mm, the calcined petroleum coke layer Ⅳ6 is composed of petroleum coke with a particle size of 8-25mm, and the calcined petroleum coke layer Ⅴ7 is composed of petroleum coke with a particle size of 0-2mm. It not only effectively improves the utilization efficiency of petroleum coke of various particle sizes, but also effectively meets the heating effect of multiple multi-layer furnace loading, ensuring the effective graphitization production of each billet column.

[0041] The thickness of the thermal insulation layer of the laying module and the upper thermal insulation layer of the discharge module is ≥550mm.

[0042] The crucibles 3 of the blank column are connected in series end to end, and a flexible graphite pad with a thickness of 20 mm is set at the joint between the crucibles 3. The blank columns are 80 mm apart. The blank columns are stacked layer by layer, and the diameter of the lower blank column is larger than that of the lower blank column. One or two blank columns are set in the same layer. The connection module is used to connect the conductive electrodes in the stacking module to form a graphitized power transmission area, and the conductive copper plate 8 is used to press the conductive electrode 9 to contact the circuit.

[0043] When using, combine with Figure 3 and 4 According to the transformer parameters and the cross section of the conductive electrode, set up 1 or 2 columns of billets with different diameters for upper and lower layers of furnace loading. The electrodes of the same layer of billets have the same cross section and the distance between the billet columns in the same layer is 80mm. Figure 1 and 2 Schematic diagram, gradually set up laying module, stacking module, discharge module and connection module, specifically, the laying module is divided into calcined petroleum coke layer IV6 and calcined petroleum coke layer V7, calcined petroleum coke layer IV6 and calcined petroleum coke layer V7 are used to lay on the bottom of the furnace to form a thermal insulation layer; the stacking module is divided into calcined petroleum coke layer I1 and calcined petroleum coke layer II2, calcined petroleum coke layer II2 wraps the crucible 3 and fills the gap between the crucibles, calcined petroleum coke layer I1 is arranged on both sides of the calcined petroleum coke layer II2, the crucible 3 is filled with the material to be graphitized to form a blank column, the calcined petroleum coke layer I1 and the calcined petroleum coke layer II2 are used to stack on the upper part of the thermal insulation layer to form a blank column. The blank layer is formed; the discharge module is divided into a semi-graphitized petroleum coke layer 4 and a calcined petroleum coke layer III5, and the calcined petroleum coke layer III5 and the semi-graphitized petroleum coke layer 4 are arranged layer by layer on the upper part of the blank layer. The calcined petroleum coke layer III5 and the semi-graphitized petroleum coke layer 4 are used to cover the surface of the stacking module with insulation material to form an upper insulation layer; the connection module is divided into a conductive copper plate 8 and a conductive electrode 9, and the conductive electrode 9 is arranged at both ends of the blank layer. The conductive copper plate 8 clamps the conductive electrode 9 and is energized for operation. The conductive copper plate 8 and the conductive electrode 9 are used to connect the stacking module; the conductive electrode and the conductive copper plate are in contact with each other by applying pressure, and the contact pressure is maintained to turn on the power supply for operation.

[0044] The preferred embodiments of the utility model disclosed above are only used to help explain the utility model. The preferred embodiments do not describe all the details in detail, nor do they limit the utility model to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the utility model, so that technicians in the relevant technical field can well understand and use the utility model. The utility model is limited only by the claims and their full scope and equivalents.

Claims

1. A furnace loading system for connecting graphitization furnaces in series to produce billets with different cross-sectional diameters. It is characterized in that A laying module, a stacking module, a material discharging module and a connection module are arranged in the graphitization furnace; The laying module is divided into a calcined petroleum coke layer IV (6) and a calcined petroleum coke layer V (7), and the calcined petroleum coke layer IV (6) and the calcined petroleum coke layer V (7) are used to lay a thermal insulation layer at the bottom of the furnace; The stacking module is divided into a calcined petroleum coke layer I (1) and a calcined petroleum coke layer II (2), the calcined petroleum coke layer II (2) wraps the crucible (3) and fills the gap between the crucibles, the calcined petroleum coke layer I (1) is arranged on both sides of the calcined petroleum coke layer II (2), the crucible (3) is filled with a material to be graphitized to form a blank column, and the calcined petroleum coke layer I (1) and the calcined petroleum coke layer II (2) are used to stack on the upper part of the insulation layer to form a blank layer; The material discharging module is divided into a semi-graphitized petroleum coke layer (4) and a calcined petroleum coke layer III (5); the calcined petroleum coke layer III (5) and the semi-graphitized petroleum coke layer (4) are arranged layer by layer on the upper part of the blank layer; the calcined petroleum coke layer III (5) and the semi-graphitized petroleum coke layer (4) are used to cover the surface of the stacking module with a thermal insulation material to form an upper thermal insulation layer; The connection module is divided into a conductive copper plate (8) and a conductive electrode (9), the conductive electrode (9) is arranged at both ends of the blank layer, the conductive copper plate (8) clamps the conductive electrode (9) and is energized for operation, and the conductive copper plate (8) and the conductive electrode (9) are used to connect the stacking module; The crucible (3) is arranged in a horizontal direction, and the crucible (3) is arranged parallel to an axis from the furnace head to the furnace tail of the graphitization furnace.

2. A furnace loading system for producing billets with different cross-sectional diameters by connecting graphitization furnaces in series according to claim 1, characterized in that: The calcined petroleum coke layer I (1) is composed of petroleum coke with a particle size of 0-2 mm, the calcined petroleum coke layer II (2) is composed of petroleum coke with a particle size of 8-25 mm, the semi-graphitized petroleum coke layer (4) is composed of semi-graphitized petroleum coke with a particle size of 0-2 mm, the calcined petroleum coke layer III (5) is composed of calcined petroleum coke with a particle size of 3-8 mm, the calcined petroleum coke layer IV (6) is composed of petroleum coke with a particle size of 8-25 mm, and the calcined petroleum coke layer V (7) is composed of petroleum coke with a particle size of 0-2 mm.

3. The furnace loading system for producing billets with different cross-sectional diameters by connecting graphitization furnaces in series according to claim 1, characterized in that: The thickness of the thermal insulation layer of the laying module and the upper thermal insulation layer of the discharge module is ≥550mm.

4. The furnace loading system for producing billets with different cross-sectional diameters by connecting graphitization furnaces in series according to claim 1, characterized in that: The crucibles (3) of the blank column are spliced ​​in series end to end, and a flexible graphite pad with a thickness of 20 mm is provided at the splicing position between the crucibles (3).

5. A furnace loading system for producing billets with different cross-sectional diameters by connecting graphitization furnaces in series according to claim 4, characterized in that: The distance between the blank columns is 80 mm.

6. A furnace loading system for producing billets with different cross-sectional diameters by connecting graphitization furnaces in series according to claim 5, characterized in that: The blank columns are stacked layer by layer, the diameter of the blank column in the lower layer is larger than the diameter of the blank column in the lower layer, and 1 or 2 blank columns are arranged in the same layer.

7. A furnace loading system for producing billets with different cross-sectional diameters by connecting graphitization furnaces in series according to claim 5, characterized in that: The connection module is used to connect the conductive electrodes in the stacking module to form a graphitized power transmission area, and the conductive electrodes (9) are pressed and contacted through the conductive copper plate (8) to connect the circuit.