SiC MOSFET device structure

By using doped fillers and annealing activation technology in SiC MOSFET devices, an ion region is formed to wrap the bottom of the trench, which solves the problem of electric field concentration at the corners of the gate oxide layer and improves the reliability and stability of the device.

CN221861667UActive Publication Date: 2024-10-18XIAMEN XINERGY MICROELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323453786.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-18
Publication Date
2024-10-18
Estimated Expiration
2033-12-18

AI Technical Summary

Technical Problem

The corners of the gate oxide layer of SiC MOSFET devices tend to concentrate electric fields, causing reliability problems. It is difficult to effectively protect the bottom gate oxide layer with existing technology.

Method used

In SiC MOSFET devices, the trench filler doped with ions of the second doping type is filled at the bottom of the trench, and the ions are activated through annealing so that they diffuse into the drift region to form an ion region, wrapping the bottom of the trench and reducing the electric field. Concentrated to protect the gate oxide layer.

Benefits of technology

It effectively improves the reliability of the device, reduces the risk of breakdown of the gate oxide layer, improves the electric field distribution at the corners of the gate oxide layer, and enhances the stability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221861667U_ABST
    Figure CN221861667U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of semiconductor devices, in particular to a SiC MOSFET (Metal-Oxide-Semiconductor Field Effect Transistor) device structure, which comprises a substrate, a drift region, a base region, a groove filler, a gate oxide layer and a gate. Wherein the groove filler is deposited from the upper surface of the source region to the bottom of a groove formed in the drift region, and the groove filler is doped with second doping type ions; a gate oxide layer is arranged above the groove filler along the inner wall of the groove, at least one ion region is formed by extending from the joint of the groove filler and the drift region to the corner of the bottom end of the gate oxide layer, second doping type ions are arranged in the ion region and wrap the bottom of the groove, and the second doping type ions are arranged in the ion region. The electric field concentration at the bottom of the trench gate is reduced, the gate oxide at the bottom is effectively protected, and the reliability of the device is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of semiconductor devices, in particular to a SiC MOSFET device structure. Background Art

[0002] The third generation semiconductor material silicon carbide (SiC) has superior properties such as wide bandgap, high thermal conductivity, high carrier saturation mobility and high critical breakdown electric field, which gives it unique advantages and broad prospects in the fields of high power, high frequency and high voltage. At present, SiC MOSFET has been widely used in automotive electronics, photovoltaics and energy storage.

[0003] SiC MOSFET has become one of the research hotspots of SiC power devices due to its advantages of low on-resistance and high cell density. However, the critical breakdown field strength of SiC is extremely high and the quality of gate oxide is poor, which will easily lead to the concentration of a large electric field at the corner of the gate oxide layer, causing the gate oxide layer to be broken down, and there are serious reliability issues. Therefore, this field is in urgent need of a new SiC MOSFET structure that can effectively protect the bottom gate oxide layer and improve the reliability of the device. Utility Model Content

[0004] In order to solve the problem in the prior art that the electric field is easily concentrated at the corner of the gate oxide layer, causing the gate oxide layer to be broken down, the utility model provides a SiC MOSFET device structure, including:

[0005] a substrate, the substrate being of a first doping type and having a first surface and a second surface opposite to each other;

[0006] A drift region is formed on the first surface of the substrate, and the drift region is of a first doping type;

[0007] A base region, formed above the drift region, the base region being of a second doping type;

[0008] A source region is formed on the upper surface of the base region, and the source region is of a first doping type; a trench is formed from the upper surface of the source region to the inside of the drift region;

[0009] A trench filler, the trench filler is deposited at the bottom of the trench; the trench filler is doped with ions of a second doping type; a gate oxide layer is arranged above the trench filler along the inner wall of the trench, and at least one ion region extending to a corner of the bottom end of the gate oxide layer is formed by the connection between the trench filler and the drift region, and the ion region contains ions of the second doping type;

[0010] A gate is disposed inside the trench and is separated from the trench filler, the drift region, the base region and the source region by the gate oxide layer.

[0011] In one embodiment, it further includes:

[0012] an interlayer dielectric layer covering the base region, the source region and an upper surface of the gate oxide layer located on the top of the gate, wherein a contact hole is formed in a portion of the interlayer dielectric layer located above the source region, and a contact region is formed in the contact hole;

[0013] A source electrode, covering the upper surface of the interlayer dielectric layer and electrically connected to the source region through the contact region;

[0014] A drain electrode is disposed on the second surface of the substrate.

[0015] In one embodiment, the first doping type is N-type, and the second doping type is P-type; or, the first doping type is P-type, and the second doping type is N-type.

[0016] In one embodiment, the second doping type ion is one of boron, aluminum, gallium, indium or thallium.

[0017] In one embodiment, the trench filler is polysilicon.

[0018] In one embodiment, the ion region is formed by diffusing the second doping type ions in the trench filler into the drift region and wrapping the bottom of the trench.

[0019] In one embodiment, the thickness of the trench filler is 0.1 μm to 0.3 μm.

[0020] In one embodiment, the doping concentration of the second doping type ions in the trench fill is 1*10 18 cm -3 ~1*10 21 cm -3 .

[0021] In one embodiment, the thickness of the trench filler is smaller than the depth of the trench extending into the drift region.

[0022] In one embodiment, the thickness of the interlayer dielectric layer is 0.8 μm to 1.2 μm.

[0023] Based on the above, compared with the prior art, the SiC MOSFET device structure provided by the utility model fills the bottom of the trench with a trench filler doped with ions of the second doping type, and then uses certain conditions to anneal and activate the ions, so that the second doping type ions diffuse into the drift region to form an ion region, so that the bottom of the trench is wrapped by the second doping type ions, which reduces the electric field concentration at the bottom of the trench gate, effectively protects the bottom gate oxide, and improves the reliability of the device.

[0024] Other features and beneficial effects of the utility model will be described in the subsequent description, and partly become apparent from the description, or understood by practicing the utility model. The purpose and other beneficial effects of the utility model can be achieved and obtained by the structures specifically pointed out in the description, claims and drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the following is a brief introduction to the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. The positional relationships described in the drawings in the following description are based on the directions of the components shown in the diagrams unless otherwise specified.

[0026] Figure 1 A cross-sectional structure diagram of a SiC MOSFET device in the prior art;

[0027] Figure 2 , Figure 3 A cross-sectional structure diagram of a SiC MOSFET device preparation process provided by the utility model;

[0028] Figure 4 A cross-sectional structure diagram of a SiC MOSFET device provided by the utility model;

[0029] Figure 5 A cross-sectional structural diagram of another SiC MOSFET device provided by the utility model.

[0030] Reference numerals:

[0031] 1 substrate 2 drift region 3 base region

[0032] 4 source region 5 trench 6 trench filling

[0033] 7 ion region 8 gate 9 gate oxide layer

[0034] 10 source 11 drain 12 interlayer dielectric layer

[0035] 13 Contact Area DETAILED DESCRIPTION

[0036] In order to make the purpose, technical solutions and advantages of the embodiments of the utility model clearer, the technical solutions in the embodiments of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. Obviously, the described embodiments are part of the embodiments of the utility model, rather than all of the embodiments; the technical features designed in different implementation modes of the utility model described below can be combined with each other as long as they do not conflict with each other; based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.

[0037] In the description of the present invention, it should be noted that all terms (including technical terms and scientific terms) used in the present invention have the same meanings as those generally understood by ordinary technicians in the field to which the present invention belongs, and cannot be understood as limitations on the present invention; it should be further understood that the terms used in the present invention should be understood to have meanings consistent with the meanings of these terms in the context of this specification and in the relevant fields, and should not be understood in an idealized or overly formal sense, unless explicitly defined in this utility model.

[0038] Figure 1 It is a cross-sectional structure diagram of a SiC MOSFET device in the prior art, comprising: a substrate 1; a drift region 2 formed above the substrate 1; a base region 3 formed above the drift region 2; a source region 4 formed on the upper surface of the base region 3; and a trench gate structure opened from the surface of the source region 4 to the inside of the drift region 2, wherein a source electrode 10 is in contact with the trench gate structure and covers the base region 3, the source region 4 and the upper surface of the trench gate structure, and a drain electrode 11 is formed on the lower surface of the substrate 1.

[0039] The first embodiment of the utility model relates to a SiC MOSFE device structure, see Figure 4 , at least includes a substrate 1, a drift region 2, a base region 3, a source region 4, a trench filler 6 and a gate 8.

[0040] The substrate 1 is of the first doping type and has a first surface and a second surface relative to each other; a drift region 2 is formed on the first surface of the substrate 1, and the drift region 2 is of the first doping type; a base region 3 is formed above the drift region 2, and the base region 3 is of the second doping type; a source region 4 is formed on the upper surface of the base region 3, and the source region 4 is of the first doping type.

[0041] A trench filler 6 is provided, wherein a trench 5 is provided from the upper surface of the source region 4 to the inside of the drift region 2, and a trench filler 6 is deposited at the bottom of the trench 5, and the trench filler 6 is doped with ions of the second doping type; a gate oxide layer 9 is provided above the trench filler 6 and along the inner wall of the trench 5, and at least one ion region 7 is formed extending from the connection between the trench filler 6 and the drift region 2 to the bottom corner of the gate oxide layer 9, and the ion region 7 contains ions of the second doping type;

[0042] The gate 8 is arranged inside the trench 5 and is separated from the trench filler 6, the drift region 2, the base region 3 and the source region 4 by a gate oxide layer 9.

[0043] When implementing it, Figure 4 As shown, a drift region is formed on the first surface of the SiC substrate 1 in this embodiment. Preferably, the ion doping amount of the drift region is 7*10 15 cm -3 ~1.1*10 16 cm -3 A base region 3 is formed above the drift region, a source region 4 is formed in a preset area on the upper surface of the base region 3, a trench 5 is opened from the upper surface of the source region 4 to the inside of the drift region 2, and a trench filler 6 doped with the second doping type ions is filled at the bottom of the trench 5. In this embodiment, the thickness of the trench filler 6 is less than the depth of the trench 5 that penetrates into the drift region 2. Preferably, the thickness of the trench filler 6 is 0.1μm to 0.3μm, and the doping concentration of the trench filler 6 is 1*10 18 cm -3 ~1*10 21 cm -3 . A gate oxide layer 9 is formed above the trench filler 6 along the exposed sidewalls of the trench 5, and at least one ion region 7 is formed extending from the connection between the trench filler 6 and the drift region 2 to the bottom corner of the gate oxide layer 9. A conductive structure, such as a gate polysilicon structure, is formed between the gate oxide layers 9 on the inner wall of the trench 5. This gate polysilicon structure is separated from the trench filler 6 by the gate oxide layer 9 to form a gate 8. The gate 8 is separated from the trench filler 6, the drift region 2, the base region 3 and the source region 4 by a gate oxide layer 9.

[0044] Preferably, it also includes: an interlayer dielectric layer 12, covering the upper surface of the base region 3, the source region 4 and the gate oxide layer 9 located on the top of the gate 8, and a contact hole is opened in the part of the interlayer dielectric layer 12 located above the source region 4, and a contact region 13 is formed in the contact hole; a source electrode 10, covering the upper surface of the interlayer dielectric layer 12, and electrically connected to the source region 4 through the contact region 13; a drain electrode 11, and the drain electrode 11 is arranged on the second surface of the substrate 1.

[0045] When implementing it, Figure 5 As shown, the interlayer dielectric layer 12 (ILD layer) is an integral structure covering the upper surface of the base region 3, the source region 4 and the gate oxide layer 9 located on the top of the gate 8. Preferably, the thickness of the interlayer dielectric layer 12 is 0.8μm to 1.2μm. In this embodiment, the thickness of the interlayer dielectric layer 12 can be 1μm. Preferably, the material of the interlayer dielectric layer 12 is silicon oxide. The interlayer dielectric layer 12 can form electrical isolation between the transistor and the first layer of metal. Further, a contact hole is opened in the part of the interlayer dielectric layer 12 located above the source region 4, and ions of the first conductive type or the second conductive type are injected into the contact hole, and then a high-temperature annealing treatment is performed to form a contact area 13 in the contact hole. The source 10 is arranged above the interlayer dielectric layer 12 and is electrically connected to the source region 4 through the contact area 13; the drain 11 is arranged on the second surface of the substrate 1.

[0046] Preferably, the ion region 7 is formed by diffusing the second doping type ions in the trench filler 6 into the drift region 2 and wrapping around the bottom of the trench 5 .

[0047] When implementing it, Figure 3 , 4 As shown, preferably, at least one side of the trench filler 6 directly contacts the drift region 2. Annealing under certain conditions is used to activate the second doping type ions in the trench filler 6, and then the second doping type ions are diffused from the trench filler 6 to the drift region 2 to wrap the bottom of the trench 5, forming the ion region 7. In this embodiment, the trench filler 6 is P-type doped, so a P-type ion region 7 is formed around the bottom of the trench 5. The ion region 7 wraps around the bottom of the trench 5, forming an effective electron isolation layer, reducing the electric field concentration at the bottom of the trench 5, effectively protecting the bottom gate oxide, and improving the reliability of the device.

[0048] Preferably, the first doping type is N-type and the second doping type is P-type; or, the first doping type is P-type and the second doping type is N-type. When the second doping type is P-type, the second doping type ion is one of boron, aluminum, gallium, indium or thallium.

[0049] The second embodiment of the present utility model relates to a method for manufacturing a novel SiC MOSFET device. This embodiment takes the manufacture of a 1200V withstand voltage device as an example, and the steps are as follows:

[0050] S100, epitaxially grow a silicon carbide (SiC) substrate 1 with a thickness of 10 μm and a doping concentration of 7*10 15 cm -3 ~1.1*10 16 cm -3 N-type drift region 2;

[0051] S200, depositing a first hard mask layer on the surface of the drift region 2, forming the required P-type base region 3 pattern by photolithography and etching, and the implantation dose is 9*10 16 cm -3 ~5*10 17 cm -3 After Al ions are formed into a P-type base region 3, the first hard mask layer is removed, and then high-concentration N ions are injected into the surface of the P-type base region 3 to form an N+ type source region 4;

[0052] S300, depositing a second hard mask layer on the surface of the base region 3 and the source region 4, forming a trench 5 of a certain depth into the drift region 2 by photolithography and etching, and then filling the trench filler 6 with a thickness of 0.1 μm to 0.3 μm, wherein the trench filler 6 has a doping concentration of 1*10 18 cm -3 ~1*10 21 cm -3 P-type polysilicon, the SiC MOSFET device structure screenshot is as follows Figure 2 As shown. Next, a carbon film is first coated on the surface of the SiC MOSFET device as a protective layer to reduce surface degradation caused by Si desorption and surface atomic migration. Specifically, a carbon film can be coated on the surface of the base region 3, the source region 4 and the trench filler 6. A high-temperature annealing treatment is performed at a temperature of 1800 to 2000°C for 10 minutes to 30 minutes. After the annealing is completed, the carbon film is removed by oxidation or corrosion. At this time, the SiC MOSFET device structure screenshot is as follows Figure 3 As shown, an ion region 7 is formed around the trench fill 6 .

[0053] S400, growing a gate oxide layer 9, depositing polysilicon, and photolithographically etching the gate 8 to form a gate 8. The thickness of the gate oxide layer 9 may be 500 Å.

[0054] S500, depositing metal and photolithography etching to form metal source 10 and depositing passivation layer and photolithography etching to form passivation. After completing the front process, the back is ground to the required thickness, and then polished, cleaned, evaporated, and alloyed to form back metal as drain 11. The final structure of the SiC MOSFET device is as follows: Figure 4 shown.

[0055] In another optional embodiment, when executing step S300, N continuous trenches 5 (N is an integer greater than or equal to 2) are formed from the surface of the source region 4 to the inside of the drift region 2 by photolithography and etching, and then a layer with a thickness of 0.1 μm to 0.3 μm and a doping concentration of 1*10 18 cm -3 ~1*10 21 cm -3 The trench filler 6 is then subjected to high temperature annealing at a temperature of 1800-2000° C. for 10-30 minutes. The high temperature annealing step simultaneously causes the doping in the N trench fillers 6 to diffuse outward, thereby forming N ion regions 7 (N is an integer greater than or equal to 2), respectively wrapping the bottom of the corresponding trench 5. Furthermore, the N ion regions 7 are interconnected.

[0056] In another optional embodiment, when performing step S400, the formation of the gate oxide layer 9 is divided into two steps, firstly forming a thicker gate oxide layer 9 on the upper surface of the trench filler 6, and then forming a thinner gate oxide layer 9 on the sidewall of the trench 5. The thicker gate oxide layer 9 helps to reduce the capacitance value (Vgd) between the gate 8 and the drain 11.

[0057] In another optional embodiment, before executing step S500, it also includes: growing an ILD layer on the upper surface of the base region 3, the source region 4 and the gate oxide layer 9 located on the top of the gate 8, and the dielectric material of the ILD is silicon oxide. The portion of the ILD layer located above the N+ source region 4 is etched downward and Ni is deposited, and a contact region is formed after high-temperature annealing. The thickness of the ILD layer is in the range of 0.8μm to 1.2μm. The ILD layer forms electrical isolation between the upper surface of the base region 3, the source region 4 and the gate oxide layer 9 located on the top of the gate 8 and the source 10 metal. The ILD layer can effectively reduce the parasitic capacitance between the metal and the substrate 1, and improve the parasitic field effect transistor formed by the metal crossing different regions.

[0058] In summary, compared with the prior art, the SiC MOSFET device structure and manufacturing method provided by the present invention have the following advantages:

[0059] 1. A trench filler is provided at the bottom of the trench to focus on protecting the bottom gate oxide layer to reduce the risk of gate oxide layer breakdown, thereby improving the reliability of the device.

[0060] 2. Activate the second doping type ions in the trench filler to diffuse them into the drift region to form an ion region that wraps around the bottom of the trench, improve the electric field distribution at the corner of the gate oxide layer, reduce the electric field concentration, and help reduce the risk of breakdown.

[0061] In addition, those skilled in the art should understand that, although there are many problems in the prior art, each embodiment or technical solution of the utility model can be improved in only one or several aspects, without having to solve all the technical problems listed in the prior art or background technology at the same time. Those skilled in the art should understand that the content not mentioned in a claim should not be used as a limitation on the claim.

[0062] Although the terms such as substrate, drift region, base region, source region, trench, trench filling, gate oxide layer, gate, source, first doping type, second doping type, second doping type ion, etc. are used more frequently in this article, the possibility of using other terms is not excluded. The use of these terms is only to more conveniently describe and explain the essence of the utility model; interpreting them as any additional restrictions is contrary to the spirit of the utility model; the terms "first", "second", etc. (if any) in the description and claims of the embodiments of the utility model and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence.

[0063] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solution deviate from the scope of the technical solution of the embodiments of the utility model.

Claims

1. A SiC MOSFET device structure, It is characterized in that include: a substrate, the substrate being of a first doping type and having a first surface and a second surface opposite to each other; A drift region is formed on the first surface of the substrate, and the drift region is of a first doping type; A base region, formed above the drift region, the base region being of a second doping type; A source region, formed on the upper surface of the base region, the source region being of a first doping type; A groove is formed from the upper surface of the source region to the interior of the drift region; A trench filler, the trench filler being deposited at the bottom of the trench; the trench filler being doped with ions of a second doping type; A gate oxide layer is arranged above the trench filler along the inner wall of the trench, and at least one ion region extending to the bottom corner of the gate oxide layer is formed by the connection between the trench filler and the drift region, and the ion region contains ions of the second doping type; A gate is disposed inside the trench and is separated from the trench filler, the drift region, the base region and the source region by the gate oxide layer.

2. The SiC MOSFET device structure according to claim 1, It is characterized in that Also includes: an interlayer dielectric layer covering the base region, the source region and an upper surface of the gate oxide layer located on the top of the gate, wherein a contact hole is formed in a portion of the interlayer dielectric layer located above the source region, and a contact region is formed in the contact hole; A source electrode, covering the upper surface of the interlayer dielectric layer and electrically connected to the source region through the contact region; A drain electrode is disposed on the second surface of the substrate.

3. The SiC MOSFET device structure according to claim 1, Features: The first doping type is N-type, and the second doping type is P-type; or, the first doping type is P-type, and the second doping type is N-type.

4. The SiC MOSFET device structure according to claim 1, Features: The second doping type ion is one of boron, aluminum, gallium, indium or thallium.

5. The SiC MOSFET device structure according to claim 1, Features: The trench filler is polysilicon.

6. The SiC MOSFET device structure according to claim 1, Features: The ion region is formed by diffusing the second doping type ions in the trench filler into the drift region and wrapping the bottom of the trench.

7. The SiC MOSFET device structure according to claim 1, Features: The thickness of the trench filler is 0.1 μm to 0.3 μm.

8. The SiC MOSFET device structure according to claim 1, Features: The doping concentration of the second doping type ions in the trench filler is 1*10 18 cm -3 ~1*10 21 cm -3 .

9. The SiC MOSFET device structure according to claim 1, Features: The thickness of the trench filler is smaller than the trench depth of the trench extending into the drift region.

10. The SiC MOSFET device structure according to claim 2, Features: The thickness of the interlayer dielectric layer is 0.8 μm to 1.2 μm.