Zinc-aluminum alloy die-casting die

By using a fan and demoulding mechanism in the zinc-aluminum alloy die-casting mold to achieve automatic demoulding, combined with the rapid cooling technology of the suction pump and nozzle, the problems of low demoulding efficiency and deformation of molded parts in the existing technology are solved, and the efficiency is improved Demold efficiency and cooling speed.

CN221870220UActive Publication Date: 2024-10-22DONGTAI HEJINGCHENG HARDWARE PROD CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420404538.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-04
Publication Date
2024-10-22
Estimated Expiration
2034-03-04

AI Technical Summary

Technical Problem

The existing zinc-aluminum alloy die-casting mold has low efficiency and uneven manual operation during the demoulding process, which can easily lead to deformation and wear of molded parts and affect the quality of die-casting.

Method used

A zinc-aluminum alloy die-casting mold is designed, which uses a combination of a fan, a conveyor pipe, a demoulding mechanism, a groove, a limit plate, a sinking groove, a limit rod, a top plate and an air hole to achieve automatic demoulding, and through partitions, The suction pump, connecting pipe, ring pipe and nozzle are set up for rapid cooling and heat dissipation.

Benefits of technology

It realizes automatic demoulding, improves the demoulding efficiency, prevents the top plate from tilting and getting stuck, ensures the stability of pushing, and makes the die castings cool faster and finalize faster through rapid cooling and heat dissipation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221870220U_ABST
    Figure CN221870220U_ABST
Patent Text Reader

Abstract

The utility model discloses a zinc-aluminum alloy die-casting die, which relates to the technical field of zinc-aluminum alloy production and processing and comprises a base, a lower die seat is arranged in the base, a fan is fixedly mounted on the front side of the outer surface of the base, and the upper end of the fan is connected with two delivery pipes through a three-way pipe. A demolding mechanism is arranged below the inner surface of the lower mold base and comprises grooves formed in the two sides of the lower portion of the inner surface of the lower mold base, limiting plates are fixedly installed on the left side and the right side of the inner surface of each groove, and sinking grooves are formed in the positions, located on the surface of the lower mold base, of the two sides of each groove. Compared with an existing common zinc-aluminum alloy die-casting die, the zinc-aluminum alloy die-casting die can stably and automatically demould a die-casting formed part, manual demoulding is not needed, the wind pressure pushing demoulding mode can enable force applied to all point positions to be consistent, and the situation that the formed part is deformed and damaged due to uneven force application is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of zinc-aluminum alloy production and processing, in particular to a zinc-aluminum alloy die-casting mold. Background Art

[0002] Die casting is a method of casting liquid die forging, a process completed on a dedicated die casting forging machine. Its basic process is: the molten metal is first cast at a low speed or high speed to fill the mold cavity of the mold. The mold has a movable cavity surface. It is pressurized forged with the cooling process of the molten metal, which not only eliminates the shrinkage and porosity defects of the blank, but also makes the internal structure of the blank reach the broken grains of the forged state. The comprehensive mechanical properties of the blank are significantly improved. In the production and processing of zinc-aluminum alloy, in order to make the alloy be processed into the required shape and appearance, it needs to be pressurized through a die casting mold.

[0003] For example, the public document with application number 201821084090.7 discloses a zinc-aluminum alloy die-casting mold. The utility model places the zinc-aluminum alloy in the installation groove, and the pad and the damping shock absorber can play a certain shock-absorbing and buffering role on the mold. Then, the hydraulic cylinder is used to squeeze the buffer plate to drive the upper die seat to move downward. At the same time, the first spring can play a certain elastic supporting role. At the same time, the slide rod and the guide rod can effectively prevent the shaking of the upper die seat. The steel ball can reduce the friction between the slide rod and the inner wall of the slide. The second spring can play a certain elastic buffering role on the upper die seat, and the block can prevent the guide rod from falling off from the cavity. The utility model improves the stability of the device through the setting of the guide rod and the slide rod, thereby ensuring the die-casting effect of the zinc-aluminum alloy. However, after the zinc-aluminum alloy die-casting mold is die-cast, it needs to be manually demoulded, the demoulding efficiency is low, and the manual demoulding force is uneven, which is very easy to cause deformation and wear of the molded parts, affecting the die-casting quality.

[0004] Therefore, in view of this, the existing structural deficiencies are studied and improved, and a zinc-aluminum alloy die-casting mold is proposed. Utility Model Content

[0005] The purpose of the utility model is to provide a zinc-aluminum alloy die-casting mold to solve the problems raised in the above background technology.

[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a zinc-aluminum alloy die-casting mold, comprising a base, a lower mold seat is arranged inside the base, a fan is fixedly installed on the front side of the outer surface of the base, the upper end of the fan is connected to two conveying pipes through a three-way pipe, and a demolding mechanism is arranged below the inner surface of the lower mold seat.

[0007] Preferably, the demolding mechanism includes grooves opened on both sides below the inner surface of the lower mold seat, and limit plates are fixedly installed on the left and right sides of the inner surface of the groove. The surface of the lower mold seat on both sides of the groove is provided with sink grooves, and a limit rod is slidably arranged inside the sink groove. A top plate is fixedly installed on the upper end of the limit rod, and the top plate is located inside the groove. The conveying pipe passes through the base and the lower mold seat and is located below the inside of the groove. An air hole is opened in a section above the surface of the conveying pipe located inside the groove.

[0008] Preferably, edges are protruding around the inner surface of the base, and the lower mold seat is fixedly installed above the surface of the edge by bolts, and a partition is fixedly installed below the inner surface of the base.

[0009] Preferably, a suction pump is fixedly installed on the bottom of the inner surface of the base below the partition, and the suction end of the suction pump is connected to the top of the partition through a pipeline penetrating the partition, and a connecting pipe is fixedly provided at the output end of the suction pump.

[0010] Preferably, a ring tube is fixedly mounted on the inner wall of the edge, and the connecting tube passes through the partition and the edge to communicate with the ring tube, and a nozzle is fixedly arranged on the surface of the ring tube, and the nozzle passes through the edge.

[0011] Preferably, guide columns are fixedly installed at the four corners above the outer surface of the base, and an upper mold die-casting block is slidably provided on the surface of the guide column.

[0012] Preferably, a fixing plate is fixedly mounted on the top of the guide column, and a hydraulic cylinder is fixedly arranged in the middle above the surface of the fixing plate, and the movable end of the hydraulic cylinder passes through the fixing plate and is connected to the upper mold die-casting block.

[0013] Compared with the prior art, the beneficial effects of the utility model are:

[0014] 1. The utility model is provided with a fan, a conveying pipe, a demoulding mechanism, a groove, a limiting plate, a sink, a limiting rod, a top plate and air holes. After the die-casting of the zinc-aluminum alloy parts is completed, the fan inhales air, inputs it into the conveying pipe, and then blows it to the inside of the groove through the air holes. The continuously input wind pressure will push the top plate upward, and then push the die-casting part upward through the top plate to complete automatic demoulding, without the need for manual demoulding, thereby improving the demoulding efficiency. After the top plate is moved up, the gap between the top plate and the groove will allow the wind to flow out, so that the die-casting part can be cooled. The upward movement of the top plate is limited by the sink and the limiting rod to prevent the top plate from tilting and getting stuck when it moves up, thereby ensuring the stability of the top plate push. The limiting plate uses the shape of the top plate itself to limit the maximum upward movement distance of the top plate, thereby preventing the top plate from falling off due to excessive movement.

[0015] 2. The utility model adds water to the upper layer of the partition through the arrangement of a partition, a suction pump, a connecting pipe, a ring pipe and a nozzle. The upper space can contact the bottom end of the lower mold seat. The water can directly soak the outer bottom end of the lower mold seat to cool the bottom end of the lower mold seat. The suction pump can suck the upper layer of water, transport it to the ring pipe through the connecting pipe, and spray it out through the nozzle to cool the edges around the lower mold seat. It can further quickly and effectively cool and dissipate heat on all surfaces of the lower mold seat as a whole, so that the die-casting can be cooled and formed more quickly. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic diagram of the overall structure of the utility model;

[0017] Figure 2 This is a schematic diagram of the cross-sectional structure of the base and the lower mold base of the utility model;

[0018] Figure 3 This is a schematic diagram of the cross-sectional structure of the lower mold base of the utility model;

[0019] Figure 4 For this utility model Figure 3 The enlarged structural diagram at A in the middle;

[0020] Figure 5 It is a schematic diagram of the cross-sectional structure of the base and the partition of the utility model.

[0021] In the figure: 1. base; 2. lower mold base; 3. fan; 4. conveying pipe; 5. demoulding mechanism; 501. groove; 502. limit plate; 503. sink; 504. limit rod; 505. top plate; 506. air hole; 6. edge; 7. partition; 8. suction pump; 9. connecting pipe; 10. ring pipe; 11. nozzle; 12. guide column; 13. upper mold die-casting block; 14. fixing plate; 15. hydraulic cylinder. DETAILED DESCRIPTION

[0022] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0023] like Figure 1-Figure 4As shown, a zinc-aluminum alloy die-casting mold comprises a base 1, a lower mold base 2 is arranged inside the base 1, a fan 3 is fixedly installed on the front side of the outer surface of the base 1, and two conveying pipes 4 are connected to the upper end of the fan 3 through a tee pipe. A demoulding mechanism 5 is arranged below the inner surface of the lower mold base 2, and the demoulding mechanism 5 comprises grooves 501 opened on both sides of the lower inner surface of the lower mold base 2, and limit plates 502 are fixedly installed on the left and right sides of the inner surface of the groove 501. The surface of the lower mold base 2 is provided with sink grooves 503 on both sides of the groove 501, and a limit rod 504 is slidably arranged inside the sink groove 503. A top plate 505 is fixedly installed on the upper end of the limit rod 504, and the top plate 505 is located inside the groove 501. The conveying pipe 4 passes through the base 1 and the lower mold base 2 and is located inside the groove 501. The conveying pipe 4 is located below the inner surface of the groove 501, and an air hole 506 is opened at a section inside the groove 501 above the surface of the conveying pipe 4.

[0024] Furthermore, the top plate 505 is shaped like a "π" so that the two protruding blocks at the lower end of the top plate 505 can effectively limit the upward movement distance with the limiting plate 502 to prevent the top plate 505 from falling off.

[0025] Furthermore, the upper end of the top plate 505 fits tightly against the inner surface of the groove 501 and can slide, thereby preventing the air blown out of the air hole 506 from leaking and failing to increase pressure to push the top plate 505 .

[0026] Furthermore, the limiting rod 504 is slidably fitted inside the sink 503, and the upper end is connected to the top plate 505. When the top plate 505 moves upward, the limiting rod 504 can also move upward, and is limited by the sink 503, so that the top plate 505 can move stably to prevent displacement and jamming.

[0027] like Figure 1 and Figure 5 As shown, the inner surface of the base 1 is provided with a rim 6 protruding around the periphery, and the lower mold base 2 is fixedly installed on the surface of the rim 6 by bolts, and a partition 7 is fixedly installed below the inner surface of the base 1, and a suction pump 8 is fixedly installed at the bottom of the inner surface of the base 1 below the partition 7, and the suction end of the suction pump 8 is connected to the upper part of the partition 7 through a pipeline passing through the partition 7, and a connecting pipe 9 is fixedly installed at the output end of the suction pump 8, and a ring pipe 10 is fixedly installed on the inner wall of the rim 6, and the connecting pipe 9 passes through The partition 7 and the edge 6 are connected to the annular tube 10, and a nozzle 11 is fixedly provided on the surface of the annular tube 10, and the nozzle 11 passes through the edge 6. Guide columns 12 are fixedly installed at the four corners above the outer surface of the base 1, and an upper mold die-casting block 13 is slidably penetrated on the surface of the guide column 12. A fixed plate 14 is fixedly installed on the top of the guide column 12, and a hydraulic cylinder 15 is fixedly provided in the middle above the surface of the fixed plate 14, and the movable end of the hydraulic cylinder 15 passes through the fixed plate 14 and is connected to the upper mold die-casting block 13.

[0028] Furthermore, the partition 7 is located in the middle and lower part of the inner surface of the base 1, so that the interior of the base 1 is divided into two layers, the bottom end of the lower mold base 2 is located in the upper space, and cold water is injected into the upper space, thereby being able to cool the bottom of the lower mold base 2.

[0029] Furthermore, the input end of the suction pump 8 is connected to the upper space by a pipeline, and can absorb water, transport it to the ring tube 10 through the connecting pipe 9, and spray it out through the nozzle 11 to cool the edges around the lower mold base 2, which can further quickly and effectively cool and dissipate heat on all surfaces of the lower mold base 2.

[0030] Working principle: When using the zinc-aluminum alloy die-casting mold, first, put the zinc-aluminum alloy part into the groove body of the lower mold base 2, and then use the hydraulic cylinder 15 to push the upper mold die-casting block 13 down along the guide column 12 to die-cast the zinc-aluminum alloy part. After die-casting, the suction pump 8 can suck the upper layer of water, transport it to the ring pipe 10 through the connecting pipe 9, and spray it out through the nozzle 11 to cool down the edges around the lower mold base 2, which can further quickly and effectively cool and dissipate heat on all surfaces of the lower mold base 2. , so that the internal die-casting is cooled. After cooling, the fan 3 is started again to inhale air, input it into the delivery pipe 4, and then blow it to the inside of the groove 501 through the air hole 506. The continuously input wind pressure will push the top plate 505 upward, and then push the die-casting upward through the top plate 505 to complete the automatic demoulding. There is no need to manually trigger the demoulding, which improves the demoulding efficiency. After the top plate 505 moves up, the gap between the flow of the top plate 505 and the groove 501 will allow the wind to flow out, and the die-casting can also be cooled. This is the working principle of the zinc-aluminum alloy die-casting mold.

Claims

1. A zinc-aluminum alloy die-casting mold, comprising a base (1), characterized in that: A lower mold base (2) is arranged inside the base (1), a fan (3) is fixedly installed on the front side of the outer surface of the base (1), the upper end of the fan (3) is connected to two conveying pipes (4) via a three-way pipe, and a demoulding mechanism (5) is arranged below the inner surface of the lower mold base (2).

2. A zinc-aluminum alloy die-casting mold according to claim 1, characterized in that: The demoulding mechanism (5) comprises grooves (501) provided on both sides of the lower inner surface of the lower mold base (2); limit plates (502) are fixedly installed on both sides of the inner surface of the groove (501); recessed grooves (503) are provided on both sides of the groove (501) and located on the surface of the lower mold base (2); limit rods (504) are slidably provided inside the recessed grooves (503); a top plate (505) is fixedly installed on the upper end of the limit rod (504); the top plate (505) is located inside the groove (501); the conveying pipe (4) passes through the base (1) and the lower mold base (2) and is located inside the groove (501); and an air hole (506) is provided on a section of the surface of the conveying pipe (4) located inside the groove (501).

3. The zinc-aluminum alloy die-casting mold according to claim 1, characterized in that: The inner surface of the base (1) is provided with edges (6) protruding around the periphery, and the lower mold base (2) is fixedly installed above the surface of the edge (6) by bolts, and a partition (7) is fixedly installed below the inner surface of the base (1).

4. The zinc-aluminum alloy die-casting mold according to claim 1, characterized in that: A suction pump (8) is fixedly installed on the bottom of the inner surface of the base (1) below the partition (7), and the suction end of the suction pump (8) is connected to the top of the partition (7) through a pipeline penetrating the partition (7), and a connecting pipe (9) is fixedly provided on the output end of the suction pump (8).

5. The zinc-aluminum alloy die-casting mold according to claim 3, characterized in that: An annular tube (10) is fixedly mounted on the inner wall of the edge (6), and the connecting tube (9) passes through the partition (7) and the edge (6) to communicate with the annular tube (10), and a nozzle (11) is fixedly arranged on the surface of the annular tube (10), and the nozzle (11) passes through the edge (6).

6. The zinc-aluminum alloy die-casting mold according to claim 1, characterized in that: Guide columns (12) are fixedly installed at the four corners above the outer surface of the base (1), and an upper mold die-casting block (13) is slidably penetrated through the surface of the guide column (12).

7. A zinc-aluminum alloy die-casting mold according to claim 6, characterized in that: A fixing plate (14) is fixedly mounted on the top of the guide column (12), and a hydraulic cylinder (15) is fixedly arranged in the middle above the surface of the fixing plate (14), and the movable end of the hydraulic cylinder (15) penetrates the fixing plate (14) and is connected to the upper die casting block (13).