Corrosion-resistant sulfur dioxide flue gas conveying pipeline joint

By introducing an anti-corrosion mechanism into the joints of the sulfur dioxide flue gas transportation pipes and using materials such as activated carbon plates and acid-resistant layers for preliminary desulfurization treatment, the problem of poor corrosion resistance of the pipe joints is solved, the service life is extended and the desulfurization effect is maintained.

CN221880577UActive Publication Date: 2024-10-22HEBEI HUAYE HESHUN ENG TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323466735.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-19
Publication Date
2024-10-22
Estimated Expiration
2033-12-19

AI Technical Summary

Technical Problem

The existing sulfur dioxide flue gas transportation pipeline joints have poor corrosion resistance during use and are easily corroded by sulfur dioxide flue gas, shortening their service life.

Method used

A corrosion-resistant sulfur dioxide flue gas delivery pipe joint is designed. It adopts an anti-corrosion mechanism, including a neutralization component and a connecting component. The neutralization component uses activated carbon plates, acid-resistant layers and corrosion-resistant layers to guide the flue gas through the air guide plate to make it Contact with the activated carbon plate for preliminary desulfurization treatment, and improve the corrosion resistance of the pipe joints through the acid-resistant layer and corrosion-resistant layer, while providing a structure that facilitates the replacement of the activated carbon plate.

Benefits of technology

It effectively weakens the corrosiveness of flue gas, extends the service life of pipe joints, maintains the desulfurization effect, and ensures the corrosion resistance and desulfurization effect of pipe joints.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221880577U_ABST
    Figure CN221880577U_ABST
Patent Text Reader

Abstract

The utility model relates to a corrosion-resistant sulfur dioxide flue gas conveying pipeline joint which comprises two bodies, each body is provided with a corrosion-resistant mechanism, each corrosion-resistant mechanism comprises a neutralizing assembly and a connecting assembly, each neutralizing assembly comprises a connecting column arranged in the two bodies, an air guide plate is fixed on the outer side of each connecting column, and each air guide plate is fixed on the outer side of the corresponding connecting column. The air guide plate abuts against the interior of the body, and an activated carbon plate is fixed to the front face of the air guide plate. According to the corrosion-resistant sulfur dioxide flue gas conveying pipeline joint, the corrosion-resistant mechanism is arranged, and through mutual cooperation of all structures of the corrosion-resistant mechanism, flue gas can be subjected to preliminary desulfurization treatment after entering the pipeline joint, so that the corrosion of the flue gas is weakened, and the situation that the service life of the pipeline joint is shortened under the long-time action of the flue gas is avoided; under the cooperation of the lug plate, the bolt and the nut, the activated carbon plate losing the neutralizing effect can be conveniently replaced, so that the desulfurization effect of the pipeline joint can be kept, and the use effect is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of pipeline joints, in particular to a corrosion-resistant sulfur dioxide fume conveying pipeline joint. Background Art

[0002] Sulfur dioxide is a common pollutant that has serious impacts on the environment and human health. In industry, sulfur dioxide flue gas is usually emitted in industrial production, the power industry, and coal-fired power plants, and the flue gas is transported to the desulfurization equipment through pipelines.

[0003] For example, Chinese utility model patent publication number CN 219062710 U: discloses a connection assembly for a pipe joint, including a threaded pipe, threaded sleeves are threadedly connected at both ends of the threaded pipe, grooves are arranged inside the threaded sleeves near the outside, the inner wall of the first sealing pad is fixedly connected with a rubber pad, the end of the rubber pad away from each other is provided with an outer bevel, the threaded sleeve is provided with a tight bevel near the outside, the end of the rubber pad close to each other is provided with an inner bevel, the threaded pipe is provided with an extrusion bevel near the left and right sides, and a sealing ring is arranged in the middle position of the threaded pipe. The utility model can make the rubber pad squeeze the outer wall of the copper pipe and fix it by turning the knob threaded pipe and the threaded sleeve, and at the same time, due to the sealing effect of the self-adjusting bevel, the adjusting ring further improves the sealing effect between the structures in the process of being driven and squeezed into the annular groove, and the sealing effect is better than that of the traditional connector.

[0004] The connecting assembly of the above-mentioned pipe joint can improve the fixing effect when in use, but it still has some shortcomings when in use. For example, the corrosion resistance of the pipe joint is poor. When the pipe joint is used in the transportation of sulfur dioxide flue gas, the sulfur dioxide flue gas is corrosive, which will cause corrosion to the pipe joint, thereby shortening the service life of the pipe joint. Utility Model Content

[0005] In view of the deficiencies in the prior art, the utility model provides a corrosion-resistant sulfur dioxide flue gas conveying pipeline joint, which has the advantages of corrosion resistance and the like, and solves the problem of flue gas corroding the pipeline joint.

[0006] To achieve the above object, the utility model provides the following technical solutions: a corrosion-resistant sulfur dioxide flue gas conveying pipeline joint, comprising two bodies, the bodies are provided with an anti-corrosion mechanism, the anti-corrosion mechanism comprises a neutralization component and a connection component;

[0007] The neutralization component includes a connecting column arranged inside the two main bodies, an air guide plate is fixed to the outside of the connecting column, the air guide plate abuts against the inside of the main body, an activated carbon plate is fixed on the front of the air guide plate, and no less than two air holes are opened inside the activated carbon plate.

[0008] Furthermore, the neutralization component also includes an acid-resistant layer fixed on the inner side of the body, a second corrosion-resistant layer is fixed on the inner side of the acid-resistant layer, and a first corrosion-resistant layer is fixed on the inner side of the second corrosion-resistant layer.

[0009] Furthermore, the connecting assembly includes a positioning block fixed to the outer side of the connecting column, a positioning groove is opened inside the main body, the side of the positioning block away from the connecting block penetrates and extends to the inside of the positioning groove, the positioning block is slidably connected to the inside of the positioning groove, an ear plate is fixed to the outer side of the main body, the two ear plates abut each other, the right side of the right ear plate abuts with a bolt, the left end of the bolt penetrates and extends to the left side of the left ear plate, the outer side of the bolt is threadedly connected with a nut, and the nut abuts against the left side of the left ear plate.

[0010] Furthermore, the air guide plate is in a spiral shape, and the length of the connecting column is equal to the length of the body.

[0011] Furthermore, the acid-resistant layer is KPI acid-resistant putty, the second corrosion-resistant layer is an epoxy resin paint layer, and the first corrosion-resistant layer is a polyethylene coating.

[0012] Furthermore, the positioning block is loosely matched with the positioning groove, and a through hole for the bolt to penetrate is provided inside the ear plate.

[0013] Compared with the prior art, the technical solution of this application has the following beneficial effects:

[0014] 1. The corrosion-resistant sulfur dioxide flue gas conveying pipeline joint is provided with an anti-corrosion mechanism. Through the cooperation between the various structures of the anti-corrosion mechanism, the flue gas can be preliminarily desulfurized after entering the pipeline joint to reduce the corrosiveness of the flue gas and avoid the pipeline joint from being shortened in service life due to the long-term action of the flue gas.

[0015] 2. The corrosion-resistant sulfur dioxide flue gas conveying pipeline joint, with the cooperation of ear plates, bolts and nuts, can facilitate the replacement of activated carbon plates that have lost their neutralization effect, so that the pipeline joint can maintain the desulfurization effect to improve the use effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic diagram of the structure of the utility model;

[0017] Figure 2 This is a schematic diagram of the internal structure of the utility model body;

[0018] Figure 3 This is a schematic diagram of the connection structure of the connection column and the air guide plate of the utility model;

[0019] Figure 4 This is a schematic diagram of the connection structure of the positioning block and the positioning groove of the utility model;

[0020] Figure 5 This is a schematic diagram of the connection structure between the acid-resistant layer and the second corrosion-resistant layer of the utility model.

[0021] In the figure: 1, main body; 2, anti-corrosion mechanism; 201, connecting column; 202, activated carbon plate; 203, air hole; 204, air guide plate; 205, acid-resistant layer; 206, second corrosion-resistant layer; 207, first corrosion-resistant layer; 208, positioning groove; 209, bolt; 210, ear plate; 211, nut; 212, positioning block. DETAILED DESCRIPTION

[0022] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0023] See also Figure 1-2 A corrosion-resistant sulfur dioxide flue gas conveying pipeline joint in this embodiment includes two main bodies 1, and an anti-corrosion mechanism 2 is provided on the main body 1. The anti-corrosion mechanism 2 includes a neutralization component and a connection component.

[0024] See also Figure 3-5 The neutralization component in this embodiment includes a connecting column 201 arranged inside the two main bodies 1, and a wind guide plate 204 is fixed on the outer side of the connecting column 201. The wind guide plate 204 can guide the flue gas and make the flue gas stay in the pipe joint for a long time, so that the flue gas can fully react with the activated carbon plate 202. The wind guide plate 204 is in contact with the inside of the main body 1, and an activated carbon plate 202 is fixed on the front of the wind guide plate 204. The activated carbon can effectively adsorb and remove sulfur dioxide in the flue gas. The activated carbon has a highly porous structure and a huge specific surface area, and can adsorb a large number of harmful gas molecules, including sulfur dioxide. By contacting sulfur dioxide with activated carbon, sulfur dioxide will be adsorbed on the surface of the activated carbon to form sulfate, thereby achieving a desulfurization effect. There are no less than two pores 203 inside the activated carbon plate 202, and the pores 203 can increase the contact area between the flue gas and the activated carbon plate 202 to improve the reaction effect.

[0025] The neutralization component also includes an acid-resistant layer 205 fixed on the inner side of the main body 1. The acid-resistant layer 205 has excellent corrosion resistance, especially acid resistance. A second corrosion-resistant layer 206 is fixed on the inner side of the acid-resistant layer 205. The second corrosion-resistant layer 206 has excellent chemical resistance, especially alkali resistance. A first corrosion-resistant layer 207 is fixed on the inner side of the second corrosion-resistant layer 206. The first corrosion-resistant layer 207 can improve the corrosion resistance of the pipe joint. Polyethylene has good chemical stability and can withstand most acid and alkali erosion. With the cooperation of the second corrosion-resistant layer 206 and the acid-resistant layer 205, the corrosion resistance of the pipe joint can be further improved.

[0026] The connecting assembly includes a positioning block 212 fixed to the outside of the connecting column 201, and a positioning groove 208 is provided inside the main body 1. With the cooperation of the positioning block 212 and the positioning groove 208, the activated carbon plate 202 can be easily reinstalled. The side of the positioning block 212 away from the connecting block penetrates and extends to the inside of the positioning groove 208, and the positioning block 212 is slidably connected to the inside of the positioning groove 208. An ear plate 210 is fixed to the outside of the main body 1, and the two ear plates 210 are abutted against each other. The right side of the right ear plate 210 is abutted with a bolt 209, and the left end of the bolt 209 penetrates and extends to the left side of the left ear plate 210. The outer side of the bolt 209 is threadedly connected with a nut 211. The nut 211 is rotated to separate the nut 211 from the bolt 209 to release the locking of the two main bodies 1. The nut 211 abuts against the left side of the left ear plate 210. After the pipeline joint is disassembled, the activated carbon plate 202 can be easily replaced to ensure the desulfurization effect of the pipeline joint.

[0027] The air guide plate 204 is spiral in shape, the length of the connecting column 201 is equal to the length of the main body 1, the acid-resistant layer 205 is KPI acid-resistant putty, the second corrosion-resistant layer 206 is an epoxy resin paint layer, the first corrosion-resistant layer 207 is a polyethylene coating, the positioning block 212 is clearance-matched with the positioning groove 208, and a through hole is opened inside the ear plate 210 for the bolt 209 to pass through.

[0028] The flue gas can be desulfurized by the activated carbon plate 202 and the air guide plate 204 , and the corrosion resistance of the pipe joint can be improved with the cooperation of the acid-resistant layer 205 , the second corrosion-resistant layer 206 and the first corrosion-resistant layer 207 .

[0029] The above-mentioned anti-corrosion mechanism 2 can perform preliminary desulfurization treatment on the flue gas after the flue gas enters the pipe joint to reduce the corrosiveness of the flue gas, avoid shortening the service life of the pipe joint under the long-term action of the flue gas, and facilitate the replacement of the activated carbon plate 202 that has lost its neutralization effect.

[0030] The working principle of the above embodiment is:

[0031] (1) When the pipe joint is in use, corrosive flue gas enters from the left end of the pipe joint. After the flue gas enters the pipe joint, it will be guided by the air guide plate 204. After the flue gas enters the pipe joint, it will come into contact with the activated carbon plate 202, and the acid in the flue gas will be neutralized by the activated carbon plate 202. Under the action of the spiral air guide plate 204, the flue gas can stay in the pipe joint for a long time to improve the effect of the flue gas and the activated carbon plate 202. At the same time, under the action of the first corrosion-resistant layer 207 composed of polyethylene, the corrosion resistance of the pipe joint can be improved. Polyethylene has good chemical stability and can withstand the erosion of most acids and alkalis. The second corrosion-resistant layer 206 composed of epoxy resin paint has excellent chemical resistance, especially alkali resistance. The acid-resistant layer 205 composed of KPI acid-resistant glue has excellent corrosion resistance, especially acid resistance. With the cooperation of the second corrosion-resistant layer 206 and the acid-resistant layer 205, the corrosion resistance of the pipe joint can be further improved.

[0032] (2) After the activated carbon plate 202 has been used for a long time, the neutralization effect of the activated carbon plate 202 will be reduced, thereby affecting the desulfurization effect on the flue gas. At this time, the nut 211 can be rotated to separate the nut 211 from the bolt 209 to release the lock of the two main bodies 1, so as to facilitate the separation of the two main bodies 1. After the pipe joint is disassembled, the activated carbon plate 202 can be easily replaced to ensure the desulfurization effect of the pipe joint. When the activated carbon plate 202 is reinstalled, it can also be easily installed with the cooperation of the positioning block 212 and the positioning groove 208.

[0033] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A corrosion-resistant sulfur dioxide flue gas conveying pipeline joint, comprising two bodies (1), Features: The main body (1) is provided with an anti-corrosion mechanism (2), and the anti-corrosion mechanism (2) comprises a neutralization component and a connection component; The neutralization component comprises a connecting column (201) disposed inside two main bodies (1), an air guide plate (204) is fixed to the outside of the connecting column (201), the air guide plate (204) abuts against the inside of the main body (1), an activated carbon plate (202) is fixed to the front of the air guide plate (204), and at least two air holes (203) are provided inside the activated carbon plate (202).

2. A corrosion-resistant sulfur dioxide flue gas conveying pipeline joint according to claim 1, Features: The neutralization component further comprises an acid-resistant layer (205) fixed on the inner side of the body (1), a second corrosion-resistant layer (206) is fixed on the inner side of the acid-resistant layer (205), and a first corrosion-resistant layer (207) is fixed on the inner side of the second corrosion-resistant layer (206).

3. A corrosion-resistant sulfur dioxide flue gas conveying pipeline joint according to claim 1, Features: The connection assembly comprises a positioning block (212) fixed to the outside of the connection column (201); a positioning groove (208) is provided inside the body (1); the positioning block (212) penetrates through and extends to the inside of the positioning groove (208) on a side away from the connection block; the positioning block (212) is slidably connected to the inside of the positioning groove (208); an ear plate (210) is fixed to the outside of the body (1); the two ear plates (210) are abutted against each other; a bolt (209) is abutted on the right side of the right ear plate (210); the left end of the bolt (209) penetrates through and extends to the left side of the left ear plate (210); a nut (211) is threadedly connected to the outside of the bolt (209); the nut (211) abuts against the left side of the left ear plate (210).

4. A corrosion-resistant sulfur dioxide flue gas conveying pipeline joint according to claim 1, Features: The wind guide plate (204) is in a spiral shape, and the length of the connecting column (201) is equal to the length of the main body (1).

5. A corrosion-resistant sulfur dioxide flue gas conveying pipeline joint according to claim 2, Features: The acid-resistant layer (205) is a KPI acid-resistant mastic coating, the second corrosion-resistant layer (206) is an epoxy resin paint layer, and the first corrosion-resistant layer (207) is a polyethylene coating.

6. A corrosion-resistant sulfur dioxide flue gas conveying pipeline joint according to claim 3, Features: The positioning block (212) is loosely matched with the positioning groove (208), and a through hole for the bolt (209) to pass through is provided inside the ear plate (210).