Low-copper-ratio copper-niobium single-core rod of high-current-carrying-density Ni3Sn wire

By combining ion beam evaporation and copper electroplating on the surface of the niobium rod, and performing hexagonal mold drawing processing, the problem of insufficient current carrying capacity of the niobium three-tin superconducting wire was solved, and high load carrying capacity of the copper-niobium single core rod with a low copper ratio was achieved. Flow density and optimized extensibility reduce production costs and processing difficulty.

CN221884731UActive Publication Date: 2024-10-22HEFEI QUAF SUPERCONDUCTING TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420115754.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-17
Publication Date
2024-10-22
Estimated Expiration
2034-01-17

AI Technical Summary

Technical Problem

It is difficult to effectively improve the current carrying capacity of niobium three-tin superconducting wires with the existing technology, especially due to the problem that the extensibility and copper ratio of the copper-niobium single core rod cannot reach the ideal level at the same time.

Method used

A niobium rod with uniform hexagonal grains is used, and its surface is plated with copper through a combination of ion beam evaporation and electroplating, and a hexagonal mold drawing process is performed to ensure uniform coverage of the copper layer, reduce the proportion of copper volume, and at the same time increase the ratio of copper to niobium. the binding force.

Benefits of technology

A low-copper ratio copper-niobium single-core rod with high current-carrying density niobium three-tin wire is realized, ensuring the elongation of the copper-niobium composite rod and optimizing the copper ratio, and reducing production costs and processing difficulty.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221884731U_ABST
    Figure CN221884731U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of superconducting material processing, and particularly relates to a low-copper-ratio copper-niobium single-core rod of a high-current-carrying-density Ni3Sn wire rod, which is manufactured in a mode of combining ion beam evaporation and electroplating. On one hand, good extensibility of the copper-niobium single-core rod is ensured by using the small-size niobium rod with uniform grain size, and on the other hand, the binding force between copper and niobium is ensured by combining ion beam evaporation and electroplating, and the cost and the efficiency are balanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of superconducting materials, and in particular relates to a low-copper-ratio copper-niobium single core rod of a high-current-carrying-density niobium-tin wire, which is used for manufacturing the high-current-carrying-density niobium-tin wire. Background Art

[0002] NbSn low-temperature superconductors are currently the most important materials for high-field superconducting magnets above 10T, and have been widely used in many fields such as high-energy particle accelerators, nuclear magnetic resonance spectrometers (NMR), and magnetic confinement nuclear fusion (ITER). The main factors affecting the critical current density of NbSn superconducting wires are their superconducting phase content and the density of grain boundary pinning centers. In order to improve the current carrying capacity of NbSn superconducting wires, it is necessary to significantly increase the Nb and Sn content in the wires to obtain a high volume fraction of the NbSn superconducting phase.

[0003] In the prior art, there are two methods for preparing the copper-niobium single core rod required for high current density niobium-tin.

[0004] Method 1: After assembling niobium ingots and copper tubes, they are hot extruded, and after a large amount of cold deformation, they are processed into copper-niobium hexagonal composite rods, and then the composite rods are subjected to high-temperature annealing. The main purpose is to achieve recrystallization of niobium and improve the ductility of copper-niobium composite rods. The disadvantages of this method are as follows: First, there is a genetic effect in the grain size of niobium. From niobium ingots to single core rods, the grain size deforms in proportion. Therefore, to obtain copper-niobium single core rods with good ductility (3-5 mm), it is necessary to make niobium ingots with extremely uniform grain size (grain range of 0.5-1 level). Due to the smelting restrictions of large-sized (500-600 mm) niobium ingots, it is extremely difficult to obtain niobium ingots with a grain size difference of less than 1 level (200-300 mm) through billet forging with a small deformation amount. Therefore, it is very difficult to obtain copper-niobium single core rods with very good ductility (>50%) through existing methods.

[0005] Method 2: Small-sized niobium rods are loaded into thin-walled copper tubes, and then produced by cold processing methods such as tube drawing. When the copper-niobium composite rod is produced, it is difficult to obtain a copper-niobium single-core rod with a chemical metallurgical bond because copper and niobium are cold-bonded and have poor bonding strength. In addition, the copper tube size needs to maintain a certain thickness to ensure that it will not break during the subsequent cold drawing process. Therefore, the copper ratio of the single-core rod cannot be reduced to an ideal level. Utility Model Content

[0006] The utility model aims to overcome the defects of the prior art and provide a low copper ratio copper-niobium single core rod of a high current density niobium-tin wire.

[0007] The utility model discloses a low copper ratio copper-niobium single core rod of a niobium-tin wire with high current density. The copper-niobium single core rod is hexagonal, and comprises a hexagonal niobium rod with uniform grains, an ion beam evaporated copper layer, and an electroplated copper layer from the inside to the outside. The opposite side distance of the hexagonal niobium rod is 3-12 mm, and the thickness of the ion beam evaporated copper layer is 1-2 microns. After the copper-niobium single core rod is drawn by a hexagonal die, the copper layer evenly covers the surface of the niobium rod.

[0008] Furthermore, the copper volume proportion of the copper-niobium single core rod is 5-20%.

[0009] Furthermore, the grain size difference of the hexagonal niobium rod is within 1 level.

[0010] Furthermore, a high current density niobium-tin wire is prepared using the aforementioned low copper ratio copper-niobium single core rod.

[0011] Compared with the prior art, a 1-2 micron thick copper layer is plated on the surface of a cleaned niobium rod with uniform grains (grain size difference less than 1 level) by ion beam evaporation, and then copper is electroplated on the surface of the copper-niobium composite rod by conventional electroplating, thereby obtaining a copper-niobium composite rod with uniform thickness and low copper ratio. On the one hand, in the process of forging, rolling and other processes from niobium ingots with a diameter of 200-300 mm to niobium rods with a width across margins of 3-12 mm, the niobium ingots can be repeatedly forged and annealed because the processing deformation is large enough. Therefore, it is very easy to obtain small-sized niobium rods with very uniform grain sizes, thereby obtaining small-sized niobium rods with very good elongation (>50%). On the other hand, if copper is directly electroplated on the surface of the niobium rod, the copper electroplating layer and the surface affinity of the niobium rod are poor, and the bonding strength between the two is not good. The present invention uses ion beam evaporation to ensure good bonding between copper and niobium, but the evaporation speed is slow and the cost is high. Combining ion beam evaporation with electroplating can ensure the bonding strength between copper and niobium and balance the cost and efficiency.

[0012] The electroplated copper-niobium composite rod is then processed through a hexagonal die to ensure that the copper layer is evenly covered on the surface of the niobium rod. The die processing rate is 5-12%. The use of a die with a small processing rate ensures that deformation is basically only carried out on the outer copper layer of the composite rod, so that the internal niobium core rod is as little deformed as possible to avoid affecting its elongation. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 This is a schematic diagram of the low copper ratio copper-niobium single core rod structure of the high current density niobium-tin wire of the utility model. DETAILED DESCRIPTION

[0014] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. Example 1

[0015] A low copper ratio copper-niobium single core rod for a high current density niobium-tin wire, the copper-niobium single core rod is hexagonal, and comprises, from inside to outside, a hexagonal niobium rod 1 with uniform grains, an ion beam evaporated copper layer 2, and an electroplated copper layer 3, the grain size difference of the hexagonal niobium rod 1 is within 1 level, the opposite side distance of the hexagonal niobium rod 1 is 3 mm, the thickness of the ion beam evaporated copper layer 2 is 2 microns, and after the copper-niobium single core rod is drawn by a hexagonal die, the copper layer uniformly covers the surface of the niobium rod 1, the processing rate of the hexagonal die is 8%, and the copper volume proportion of the copper-niobium single core rod is 10%. Example 2

[0016] A low copper ratio copper-niobium single core rod for a high current density niobium-tin wire, the copper-niobium single core rod is hexagonal, and comprises, from inside to outside, a hexagonal niobium rod 1 with uniform grains, an ion beam evaporated copper layer 2, and an electroplated copper layer 3, the grain size difference of the hexagonal niobium rod 1 is within 1 level, the opposite side distance of the hexagonal niobium rod 1 is 6 mm, the thickness of the ion beam evaporated copper layer 2 is 1 micron, and after the copper-niobium single core rod is drawn by a hexagonal die, the copper layer is uniformly covered on the surface of the niobium rod 1, the processing rate of the hexagonal die is 12%, and the copper volume proportion of the copper-niobium single core rod is 20%. Example 3

[0017] A low copper ratio copper-niobium single core rod for a high current density niobium-tin wire, the copper-niobium single core rod is hexagonal, and comprises, from inside to outside, a hexagonal niobium rod 1 with uniform grains, an ion beam evaporated copper layer 2, and an electroplated copper layer 3, the grain size difference of the hexagonal niobium rod 1 is within 1 level, the opposite side distance of the hexagonal niobium rod 1 is 12 mm, the thickness of the ion beam evaporated copper layer 2 is 1.5 microns, and after the copper-niobium single core rod is drawn by a hexagonal die, the copper layer is uniformly covered on the surface of the niobium rod 1, the processing rate of the hexagonal die is 5%, and the copper volume proportion of the copper-niobium single core rod is 5%.

Claims

1. A low copper ratio copper-niobium single core rod of a high current density niobium-tin wire, characterized in that: The copper-niobium single core rod is hexagonal, and from the inside to the outside, it is a hexagonal niobium rod with uniform grains, an ion beam evaporated copper layer, and an electroplated copper layer. The opposite side distance of the hexagonal niobium rod is 3-12 mm, and the thickness of the ion beam evaporated copper layer is 1-2 microns. After the copper-niobium single core rod is drawn by a hexagonal die, the copper layer evenly covers the surface of the niobium rod.

2. The low copper ratio copper-niobium single core rod of the high current density niobium-tin wire according to claim 1, characterized in that: The copper volume proportion of the copper-niobium single core rod is 5-20%.

3. The low copper ratio copper-niobium single core rod of the high current density niobium-tin wire according to claim 1, characterized in that: The grain size difference of the hexagonal niobium rod is within 1 level.