Wiring terminal

By using copper material, solder blocks and flux paste in the terminal blocks, combined with the design of anti-oxidation conductive layer and soldering iron bath, the problem of oxidation of traditional terminal blocks in high temperature environment is solved, achieving stable conductive performance and convenient maintenance. operate.

CN221885424UActive Publication Date: 2024-10-22ZHEJIANG BORDA ELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420512064.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-15
Publication Date
2024-10-22
Estimated Expiration
2034-03-15

AI Technical Summary

Technical Problem

Traditional terminal blocks are easily oxidized in high-temperature environments, affecting their conductive properties, and are difficult to meet the usage standards of new wires during maintenance and disassembly.

Method used

A terminal block including a terminal barrel and a terminal board is designed. It is made of red copper and has a built-in solder block and flux paste. The solder block can melt the welding conductor, and the anti-oxidation conductive layer prevents oxidation. The soldering iron slot and grooves improve thermal conductivity and Cleanability.

Benefits of technology

It maintains good electrical conductivity in high temperature environments, facilitates maintenance, disassembly and reconnection, prevents oxidation, and improves the reliability and convenience of maintenance of the terminal block.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221885424U_ABST
    Figure CN221885424U_ABST
Patent Text Reader

Abstract

The wiring terminal comprises a wiring cylinder and a terminal plate which is arranged at one end of the wiring cylinder and is integrally connected with the wiring cylinder, one end, facing the terminal plate, of the wiring cylinder is sealed, a soldering tin block is arranged at the bottom of an inner cavity of the wiring cylinder, and the inner cavity of the wiring cylinder is further provided with flux paste which seals the soldering tin block in the wiring cylinder to isolate air; the surface of the terminal board is provided with an anti-oxidation conductive layer. The utility model has the advantages of stable connection, suitability for long-term high-temperature occasions, and convenience in maintenance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of electronic accessories, in particular to a wiring terminal. Background Art

[0002] Terminal blocks are used for connecting cables, and the temperature of their operating environment is generally room temperature. Therefore, traditional terminal blocks are often directly connected to cables by pressing them together, and then fixed to the terminal posts. However, in some electric heating equipment fields, long-term high temperatures can easily cause oxidation of the terminal blocks and cables, thereby affecting their reliability. Utility Model Content

[0003] In view of the above problems, the present invention aims to provide a terminal block which has stable connection, is suitable for long-term use in high-temperature environments, and is easy to maintain.

[0004] In response to the above problems, the following technical solutions are provided: a terminal block comprising a terminal barrel and a terminal plate integrally connected to the terminal barrel at one end of the terminal barrel, the terminal barrel being sealed at one end facing the terminal plate, a solder block being provided at the bottom of the inner cavity of the terminal barrel, and a flux paste being provided in the inner cavity of the terminal barrel to seal the solder block in the terminal barrel and isolate it from air; an anti-oxidation conductive layer being provided on the surface of the terminal plate.

[0005] In the above structure, for example, for some food machinery using cast aluminum heating plates, the heating tubes of the cast aluminum heating plates need to be connected to the high-temperature wires through terminal blocks. If the traditional riveting process is used, it is easy to cause oxidation after long-term use and affect the conductive performance. Although the terminal blocks can be replaced during later maintenance and disassembly, the conductors of the high-temperature wires will oxidize due to the high temperature (even if the exposed conductors are cut off and the internal conductors are exposed by re-stripping, for soft wires, the internal conductors will also slowly oxidize due to long-term high temperatures), and thus it is difficult to meet the use standards of new wires during the second riveting. This terminal block is suitable for both normal and high temperature environments. The terminal barrel and the terminal board are made of copper, which can ensure good conductive performance. When the conductor is inserted during wiring, the conductor will adhere to the flux paste, and then the solder block will be melted by heating the terminal barrel, causing the solder to soak The inner surface of the terminal barrel and the surface of the conductor are lubricated and the two are welded together. After welding, the contact part between the conductor of the wire and the inner cavity of the terminal barrel will not be oxidized even when used in high temperature environments (not higher than the melting temperature of the solder). When maintenance and disassembly are required, the two can be separated by reheating to melt the solder. After separation, the two can be reconnected again by welding. In addition to direct welding, the terminal barrel can also be flattened by crimping pliers before the solder solidifies to achieve a non-detachable connection by riveting, and the gap between the inner cavity of the terminal barrel and the conductor of the wire is filled with solder, thereby preventing high-temperature oxidation; the anti-oxidation conductive layer can reduce or avoid oxidation of the terminal board to ensure it has a good conductive effect; the flux paste not only improves the wettability of welding, but also plays a sealing role to prevent moisture in the air from entering the inner cavity of the terminal barrel to oxidize the inner wall of the terminal barrel and the solder block.

[0006] The present invention is further configured such that the outer wall of the wiring barrel is provided with a soldering iron groove which is concave by stamping, and the inner cavity of the wiring barrel is convex corresponding to the position of the soldering iron groove to prevent the solder block from falling out.

[0007] In the above structure, the soldering iron groove is used to adapt to the soldering iron tip of the electric soldering iron, thereby increasing the contact area between the terminal barrel and the soldering iron tip, so that the heat of the soldering iron tip can be quickly transferred to the terminal barrel; the soldering iron groove can also be filled with solder by tinning in the position of the soldering iron groove, so that the gap between the soldering iron groove and the soldering iron tip can be filled with solder, thereby further improving the heat conduction effect and quickly melting the solder block in the terminal barrel; at the same time, the concave part of the soldering iron groove forms a bulge on the inner wall of the terminal barrel, which can also be used to fix the solder block to prevent it from falling out.

[0008] The present invention is further configured such that the axis of the soldering iron slot projected onto a virtual plane coplanar with the terminal board surface is perpendicular to the axis of the wiring barrel.

[0009] In the above structure, it is convenient for the user to adjust the direction of the soldering iron tip, making it easier to hold the soldering iron during soldering.

[0010] The present invention is further configured such that there are two soldering iron slots, which are arranged at intervals of 180 degrees along the circumferential direction of the terminal barrel.

[0011] In the above structure, it is ensured that the soldering iron slot can be exposed when the terminal board is located at the front and back sides.

[0012] The present invention is further configured such that a wiring hole arranged in a through manner is provided at the center of the terminal board, and a plurality of grooves uniformly distributed along the circumferential direction of the terminal board are provided on the front and back sides of the terminal board.

[0013] In the above structure, the wiring hole is used to adapt to the screw of the terminal; the groove is used to hold chips, and when the screw is tightened, dirt, oxide scale, etc. on the screw gasket can be collected in the groove to ensure the cleanliness of the contact surface of the terminal board.

[0014] The present invention is further configured such that one end of the groove faces the wiring hole and the other end faces the outer edge of the terminal board, and the end of the groove facing the outer edge of the terminal board is inclined in a clockwise direction.

[0015] In the above structure, when the screw is tightened, its rotation direction is clockwise, so the end of the groove facing the outer edge of the terminal board is inclined in the clockwise direction, which is conducive to discharging dirt and oxide scale.

[0016] The present invention is further configured such that an inner chamfer is provided at one end of the wiring barrel facing away from the terminal board.

[0017] In the above structure, the conductor of the high-temperature flexible wire is woven from a number of fine wires and is easy to spread out. Therefore, providing an inner chamfer helps to guide the conductor into the terminal barrel.

[0018] The utility model is further configured such that an anti-oxidation conductive layer is provided on the surface of the soldering iron tank.

[0019] In the above structure, the anti-oxidation conductive layer on the surface of the soldering iron tank is convenient for tinning.

[0020] The utility model is further configured such that the anti-oxidation conductive layer is a gold-plated layer, a silver-plated layer, a nickel-plated layer, a tin-plated layer, or a zinc-plated layer.

[0021] In the above structure, the anti-oxidation conductive layer is preferably a silver-plated layer.

[0022] The beneficial effects of the utility model are as follows: the terminal block is suitable for both normal temperature and high temperature occasions. The terminal barrel and the terminal plate are made of copper, which can ensure good electrical conductivity. When the conductor is inserted during wiring, the conductor will adhere to the solder paste, and then the solder block is melted by heating the terminal barrel, so that the solder soaks the inner surface of the terminal barrel and the conductor surface, and the two are welded together. After the welding is completed, even if it is used in a high temperature occasion (not higher than the melting temperature of the solder), the contact part between the conductor of the wire and the inner cavity of the terminal barrel will not be oxidized. When maintenance and disassembly are required, only secondary heating is required to melt the solder. The two can be separated, and after the separation is completed, the two can be reconnected again by welding. In addition to direct welding, the terminal barrel can also be flattened by wire crimping pliers before the solder solidifies to achieve a non-detachable connection by riveting, and the gap between the inner cavity of the terminal barrel and the conductor of the wire is filled with solder, thereby preventing high-temperature oxidation; the anti-oxidation conductive layer can reduce or avoid oxidation of the terminal board, ensuring it has a good conductive effect; the flux paste not only improves the wettability of welding, but also plays a sealing role to prevent moisture in the air from entering the inner cavity of the terminal barrel to oxidize the inner wall of the terminal barrel and the solder block. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a schematic diagram of the three-dimensional structure of the utility model from the first perspective.

[0024] Figure 2 This is a schematic diagram of the three-dimensional structure of the utility model from a second viewing angle.

[0025] Figure 3 It is a schematic diagram of the full-section three-dimensional structure of the utility model.

[0026] Figure 4 This is a schematic diagram of the fully exploded three-dimensional structure of the utility model.

[0027] The meaning of the numbers in the figure are: 10-wire barrel; 11-terminal board; 111-wire hole; 112-groove; 12-soldering iron slot; 13-bump; 14-inner chamfer; 20-solder block; 21-flux paste. DETAILED DESCRIPTION

[0028] The following embodiments are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0029] refer to Figures 1 to 4 ,like Figures 1 to 4The terminal shown includes a terminal barrel 10 and a terminal plate 11 integrally connected to the terminal barrel 10 at one end of the terminal barrel 10. The terminal barrel 10 is sealed at one end facing the terminal plate 11. A solder block 20 is provided at the bottom of the inner cavity of the terminal barrel 10. The inner cavity of the terminal barrel 10 is also provided with flux paste 21 for sealing the solder block 20 in the terminal barrel 10 and isolating it from air; the surface of the terminal plate 11 is provided with an anti-oxidation conductive layer (not shown in the figure).

[0030] In the above structure, for example, for some food machinery using cast aluminum heating plates, the heating tubes of the cast aluminum heating plates need to be connected to the high-temperature wires through terminal blocks. If the traditional riveting process is used, it is easy to cause oxidation after long-term use and affect the conductive performance. Although the terminal blocks can be replaced during later maintenance and disassembly, the conductors of the high-temperature wires will oxidize due to the high temperature (even if the exposed conductors are cut off and the internal conductors are exposed by re-stripping, for soft wires, the internal conductors will also slowly oxidize due to long-term high temperatures), and thus it is difficult to meet the use standards of new wires during the second riveting. This terminal block is suitable for both normal and high temperature environments. The terminal barrel 10 and the terminal board 11 are made of copper, which can ensure good conductive performance. When the conductor is inserted during wiring, the conductor will adhere to the flux paste 21, and then the solder block 20 is melted by heating the terminal barrel 10, so that the solder penetrates the inner cavity of the terminal barrel 10. The surface and the conductor surface are welded together. After welding, even if used in high-temperature environments (not higher than the melting temperature of solder), the contact part between the conductor of the wire and the inner cavity of the terminal barrel 10 will not be oxidized. When maintenance and disassembly are required, the two can be separated by heating them again to melt the solder. After separation, the two can be reconnected again by welding. In addition to direct welding, the terminal barrel 10 can also be flattened by crimping pliers before the solder solidifies to achieve a non-detachable connection by riveting, and the gap between the inner cavity of the terminal barrel 10 and the conductor of the wire is filled with solder, thereby preventing high-temperature oxidation; the anti-oxidation conductive layer (not shown in the figure) can reduce or avoid oxidation of the terminal plate 11, ensuring that it has a good conductive effect; the flux paste 21 not only improves the welding wettability, but also plays a sealing role to prevent moisture in the air from entering the inner cavity of the terminal barrel 10 to oxidize the inner wall of the terminal barrel 10 and the solder block 20.

[0031] In this embodiment, the outer wall of the wire barrel 10 is provided with a soldering iron groove 12 which is concave by stamping, and the inner cavity of the wire barrel 10 is raised at a position corresponding to the soldering iron groove 12 to prevent the solder block 20 from falling out.

[0032] In the above structure, the soldering iron groove 12 is used to adapt to the soldering iron tip of the electric soldering iron, thereby increasing the contact area between the terminal barrel 10 and the soldering iron tip, so that the heat of the soldering iron tip can be quickly transferred to the terminal barrel 10; solder can also be filled in the position of the soldering iron groove 12 by tinning, so that the gap between the soldering iron groove 12 and the soldering iron tip can be filled with solder, thereby further improving the thermal conductivity and quickly melting the solder block 20 in the terminal barrel 10; at the same time, the concave part of the soldering iron groove 12 forms a protrusion 13 on the inner wall of the terminal barrel 10, which can also be used to fix the solder block 20 to prevent the solder block 20 from falling out.

[0033] In this embodiment, the axis of the soldering iron slot 12 projected onto a virtual plane coplanar with the surface of the terminal board 11 is perpendicular to the axis of the wire barrel 10 .

[0034] In the above structure, it is convenient for the user to adjust the direction of the soldering iron tip, making it easier to hold the soldering iron during soldering.

[0035] In this embodiment, there are two soldering iron slots 12 , which are arranged 180 degrees apart in the circumferential direction of the wire barrel 10 .

[0036] In the above structure, it is ensured that the soldering iron slot 12 is exposed when the terminal board 11 is located at the front and back sides.

[0037] In this embodiment, a wiring hole 111 is provided in the center of the terminal board 11 , and a plurality of grooves 112 are provided on the front and back sides of the terminal board 11 and are evenly distributed along the circumferential direction of the terminal board 11 .

[0038] In the above structure, the wiring hole 111 is used to adapt to the screw of the terminal; the groove 112 is used to accommodate chips. When the screw is tightened, the dirt, oxide scale, etc. on the screw gasket can be collected in the groove 112 to ensure the cleanliness of the contact surface of the terminal board 11.

[0039] In this embodiment, one end of the groove 112 faces the wiring hole 111 , and the other end faces the outer edge of the terminal board 11 . The end of the groove 112 facing the outer edge of the terminal board 11 is inclined in a clockwise direction.

[0040] In the above structure, when the screw is tightened, the screw is rotated clockwise, so the end of the groove 112 facing the outer edge of the terminal board 11 is inclined clockwise, which is conducive to discharging dirt and oxide scale.

[0041] In this embodiment, an inner chamfer 14 is provided at one end of the wire barrel 10 facing away from the terminal board 11 .

[0042] In the above structure, the conductor of the high-temperature flexible wire is woven from a number of fine wires and is easily spread out. Therefore, the inner chamfer 14 is provided to help guide the conductor to be inserted into the terminal barrel 10.

[0043] In this embodiment, an anti-oxidation conductive layer is provided on the surface of the soldering iron tank 12 .

[0044] In the above structure, the anti-oxidation conductive layer on the surface of the soldering iron tank 12 facilitates tinning.

[0045] In this embodiment, the anti-oxidation conductive layer (not shown in the figure) is a gold-plated layer, a silver-plated layer, a nickel-plated layer, a tin-plated layer, or a zinc-plated layer.

[0046] In the above structure, the anti-oxidation conductive layer (not shown in the figure) is preferably a silver-plated layer.

[0047] The beneficial effects of the present invention are as follows: the terminal block is suitable for both normal and high temperature applications; the terminal barrel 10 and the terminal plate 11 are made of copper, which ensures good electrical conductivity; when the conductor is inserted during wiring, the conductor will adhere to the solder paste 21, and then the solder block 20 is melted by heating the terminal barrel 10, so that the solder soaks the inner surface of the terminal barrel 10 and the conductor surface, and the two are welded together; after welding, even when used in high temperature applications (not higher than the melting temperature of the solder), the contact portion between the conductor of the wire and the inner cavity of the terminal barrel 10 will not be oxidized; when maintenance and disassembly are required, only secondary heating is required to melt the solder to weld the two together. After the separation is completed, the two can be reconnected by welding. In addition to direct welding, the terminal barrel 10 can also be flattened by crimping pliers before the solder solidifies to achieve a non-detachable connection by riveting, and the gap between the inner cavity of the terminal barrel 10 and the conductor of the wire is filled with solder, thereby preventing high-temperature oxidation; the anti-oxidation conductive layer (not shown in the figure) can reduce or avoid oxidation of the terminal plate 11, ensuring its good conductive effect; the flux paste 21 not only improves the welding wettability, but also plays a sealing role to prevent moisture in the air from entering the inner cavity of the terminal barrel 10 to oxidize the inner wall of the terminal barrel 10 and the solder block 20.

[0048] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications based on the above assumptions should also be regarded as within the scope of protection of the present invention.

Claims

1. A terminal block, comprising a terminal barrel and a terminal plate integrally connected to the terminal barrel at one end of the terminal barrel, characterized in that: The end of the wiring barrel facing the terminal board is sealed, a solder block is provided at the bottom of the inner cavity of the wiring barrel, and the inner cavity of the wiring barrel is also provided with flux paste to seal the solder block in the wiring barrel and isolate it from air; an anti-oxidation conductive layer is provided on the surface of the terminal board.

2. A terminal block according to claim 1, characterized in that: The outer wall of the wiring barrel is provided with a soldering iron groove which is concave by stamping, and the inner cavity of the wiring barrel has a protrusion corresponding to the position of the soldering iron groove to prevent the solder block from falling out.

3. A terminal block according to claim 2, characterized in that: The axis of the soldering iron groove projected onto a virtual plane coplanar with the surface of the terminal board is perpendicular to the axis of the wiring barrel.

4. A terminal block according to claim 2 or 3, characterized in that: There are two soldering iron slots, which are arranged 180 degrees apart in the circumferential direction of the wire barrel.

5. A terminal block according to claim 1, characterized in that: The center of the terminal board is provided with a wiring hole arranged in a through manner, and the front and back sides of the terminal board are provided with a plurality of grooves evenly distributed along the circumferential direction of the terminal board.

6. A terminal block according to claim 5, characterized in that: One end of the groove faces the wiring hole, and the other end faces the outer edge of the terminal board. The end of the groove facing the outer edge of the terminal board is inclined in a clockwise direction.

7. A terminal block according to claim 1, characterized in that: An end of the wiring barrel facing away from the terminal board is provided with an inner chamfer.

8. A terminal block according to claim 2, characterized in that: An anti-oxidation conductive layer is provided on the surface of the soldering iron tank.

9. A terminal block according to claim 1 or 8, characterized in that: The anti-oxidation conductive layer is a gold-plated layer, a silver-plated layer, a nickel-plated layer, a tin-plated layer, or a zinc-plated layer.