Composite forming die for thin-wall stainless steel pipe fitting
By designing the step-by-step processing process of the composite forming mold, the problems of pipe breakage and high mold cost during the molding process of stainless steel pipe fittings are solved, efficient and low-cost pipe molding is achieved, and production quality and efficiency are improved.
Patent Information
- Application Number
- CN202323090013.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-15
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2033-11-15
AI Technical Summary
In the existing stainless steel pipe fittings forming process, mechanical extrusion molding can easily lead to punch wear and pipe fitting strain. Although the water swelling molding process reduces punch wear, it is difficult to avoid pipe rupture when processing pipe fittings with complex structures, and the mold cost is high, which increases production costs.
Design a composite molding mold for thin-walled stainless steel pipe fittings. The step-by-step processing of rough pipes is completed through the first cavity and the second cavity in a single mold. The buckling structure of the upper mold and the lower mold and the injection mechanism are used to avoid Pipe rupture, improve production efficiency and reduce costs.
Through the step-by-step water swelling forming process, the problem of pipe rupture is avoided, production quality and efficiency are improved, marginal costs are saved, and the service life of the mold is extended.
Smart Images

Figure CN221892448U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of pipe moulds, and more specifically to a composite forming mould for thin-wall stainless steel pipe fittings. Background Art
[0002] Stainless steel water supply pipes are widely used in many fields such as automobiles and ships, building water supply and drainage, floor heating projects, urban gas, solar heating, fine mist fire fighting, etc. Among them, the common production processes of three-way / four-way stainless steel socket pipe fittings are mechanical extrusion forming and water expansion forming. Among these two methods, mechanical extrusion forming is a process in which a punch is pushed by a hydraulic cylinder to forcibly squeeze the pipe fittings to deform them. This method has a simple structure, but because the interference between the two is very large when the punch is forced to squeeze, it is easy to cause marks of strain inside the pipe fittings after the punch is worn, and the versatility is general. The water expansion forming process is currently the more mainstream manufacturing process. This process uses a high-pressure device to drive a liquid (emulsion) as a medium into the inner cavity of the pipe fitting, and under the action of the high-pressure liquid, it forces the pipe wall to deform to match the mold. This molding process is simple and can produce products with complex shapes. Moreover, this water expansion process has less wear on the punch and a longer service life. In the water expansion forming process, for pipes with more complex structures, a step-by-step processing method is usually adopted to avoid problems such as pipe rupture.
[0003] Prior art CN209849640U discloses a water swelling forming mold, which relates to the technical field of pipe processing and forming, and solves the problem that the common pipe manufacturing method is to directly use the mold for production and forming, and different non-standard pipes need to correspond to different molds, but the high mold cost will increase the production cost of the enterprise. The key points of its technical solution are that it includes an upper mold and a lower mold that can be interlocked, and an injection device that matches the upper mold and the lower mold. An expansion forming upper cavity is provided in the upper mold, and an expansion forming lower cavity matching the expansion forming upper cavity is provided in the lower mold. The injection device extends into the expansion forming lower cavity and the expansion forming upper cavity. The expansion forming upper cavity and the expansion forming lower cavity are provided with the following structures: a first through groove, a first oblique groove, a second through groove, a second oblique groove and a third through groove that are connected in sequence along the axial direction; the first through groove, the second through groove and the third through groove are straight grooves, so as to facilitate the processing of pipes whose intermediate contours need to be expanded, and to facilitate the purpose of reducing the processing cost of pipes. The mold of the prior art forms the pipe in one step, which is prone to problems such as pipe rupture. Utility Model Content
[0004] In order to solve the above problems, the utility model proposes a composite forming mold for thin-walled stainless steel pipe fittings. The mold can complete the two-step processing of the rough pipe through a first cavity and a second cavity with different structures in a single mold, solving the problem of easy rupture of the pipe mouth, improving production efficiency and saving marginal costs.
[0005] To achieve the above-mentioned purpose, the utility model provides a composite forming mold for thin-walled stainless steel pipe fittings, comprising an interlocking upper mold and a lower mold, a punch mechanism and an injection mechanism, a first cavity and a second cavity for forming a first pipe and a second pipe are formed between the upper mold and the lower mold, the first cavity and the second cavity are separated, the punch mechanism is arranged at one end of the first cavity and the second cavity, and the injection mechanism is arranged at the other end of the first cavity and the second cavity.
[0006] In the utility model, the first pipe is a straight pipe with at least one port on the side wall. The second pipe is based on the structure of the first pipe, with the pipe sections at both ends of the straight pipe expanded and annular bulge structures added to the side walls at both ends.
[0007] The technical solution is achieved by buckling the upper and lower dies, and then using a punch mechanism and an injection mechanism to interference fit at both ends to form a sealed first cavity and a second cavity. The injection mechanism injects liquid into the rough tube and the inner wall of the first tube in the first cavity and the second cavity, wherein the first cavity completes the first step of the rough tube to form the first tube, and then the first tube is placed in the second cavity for the second step to form the second tube. The two-step processing can prevent the tube from breaking.
[0008] As a preferred embodiment, at least one parallel first upper cavity and second upper cavity are provided in the upper mold, and at least one parallel first lower cavity and second lower cavity are provided in the lower mold. The first cavity is formed between the first lower cavity and the first upper cavity, and the second cavity is formed between the second lower cavity and the second upper cavity. The first upper cavity and the second upper cavity of the upper mold respectively form the upper half of the first cavity and the second cavity, and the first lower cavity and the second lower cavity of the lower mold respectively form the lower half of the first cavity and the second cavity.
[0009] As a preferred solution, in order to form the structure of the first tube, the structures of the first upper cavity and the first lower cavity are the same and both include a first semicircular through groove arranged along the axial direction, and at least one vertically connected first circular groove is provided on the first semicircular through groove of the first upper cavity.
[0010] As a preferred solution, in order to form the structure of the second tube, the structures of the second upper cavity and the second lower cavity are the same and both include two second semicircular through grooves and one third semicircular through groove arranged along the axial direction. The two second semicircular through grooves are respectively connected to the two ends of the third semicircular through groove, and at least one vertically connected second circular groove is provided on the third semicircular through groove of the second upper cavity.
[0011] As a preferred solution, in order to avoid the formation of a step at the connection between the second semicircular through groove and the third semicircular through groove, the connection between the second semicircular through groove and the third semicircular through groove is recessed inward to form an inclined surface, so that the connection between the pipe sections after the second pipe is formed forms a chamfer.
[0012] As a preferred solution, in order to form an annular bulge structure of the second tube, the second semicircular through grooves of the second upper cavity and the second lower cavity are respectively recessed inward to form corresponding semicircular grooves.
[0013] As a preferred embodiment, the punch mechanism includes two punch parts and two first telescopic structures, one end of each of the punch parts is respectively fixed to the telescopic ends of the two first telescopic structures, and the other end of one of the punch parts penetrates into the first cavity, and the other end of the other punch part penetrates into the second cavity, and the first telescopic structure drives the punch part to extend and cooperate with the upper mold and the lower mold to close the mold; after processing is completed, the first telescopic structure drives the punch part to retract for mold opening.
[0014] As a preferred embodiment, the injection mechanism includes two injection parts and two second telescopic structures, one end of each injection part is respectively fixed to the telescopic ends of the two second telescopic structures, and the other end of one of the injection parts extends into the first cavity, and the other end of the other injection part extends into the second cavity, and the second telescopic structure drives the injection part to extend so that the injection part cooperates with the other end of the upper mold and the lower mold to close the mold, and the injection part injects liquid into the first cavity and the second cavity at the same time; after processing is completed, the second telescopic structure drives the injection part to retract for mold opening.
[0015] As a preferred solution, one end of the two injection parts is respectively provided with an injection port, one injection part is connected with the first cavity through its injection port, and the other injection part is connected with the second cavity through its injection port, and the injection parts inject liquid into the first cavity or the second cavity through the injection port.
[0016] As a preferred solution, in order to make the upper mold and the lower mold fit accurately, guide holes are respectively provided at the four corners of the upper mold and the lower mold, and guide pillars are slidably connected in the guide holes.
[0017] Compared with the prior art, the beneficial effects of the utility model are:
[0018] 1. The utility model completes the step-by-step water swelling forming of the rough tube through the first cavity and the second cavity, thereby avoiding the problem of tube rupture during the tube forming process and improving the production quality of the tube.
[0019] 2. The utility model forms the first cavity and the second cavity for step-by-step molding of the rough tube through a single mold, which simplifies the production process, improves production efficiency and saves marginal costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is an exploded schematic diagram of a composite forming die using a novel thin-walled stainless steel pipe fitting;
[0021] Figure 2 yes Figure 1 A partial enlarged view of part A;
[0022] Figure 3 It is a structural diagram of the upper die;
[0023] Figure 4 It is a structural diagram of the lower die;
[0024] Figure 5 is a schematic diagram of the structure of the first pipe;
[0025] Figure 6 Schematic diagram of the structure of the second pipe.
[0026] In the figure: upper die 1; lower die 2; punch member 3; first telescopic structure 4; injection member 5; injection port 501; second telescopic structure 6; guide column 7; guide hole 8; first semicircular through groove 9; first circular groove 10; second circular groove 11; second semicircular through groove 12; third semicircular through groove 13; semicircular ring groove 14; inclined surface 15; first pipe 16; second pipe 17. DETAILED DESCRIPTION
[0027] The drawings are only for illustrative purposes and cannot be construed as limiting the present invention. To better illustrate the present embodiment, some parts of the drawings may be omitted, enlarged, or reduced, and do not represent the size of the actual product. For those skilled in the art, it is understandable that some well-known structures and their descriptions may be omitted in the drawings. The positional relationships described in the drawings are only for illustrative purposes and cannot be construed as limiting the present invention.
[0028] The same or similar numbers in the drawings of the embodiments of the present invention correspond to the same or similar parts; in the description of the present invention, it should be understood that if the terms "upper", "lower", "left", "right", "long", "short" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the drawings, they are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, the terms describing the positional relationship in the drawings are only used for illustrative purposes and cannot be understood as limitations on this patent. For ordinary technicians in this field, the specific meanings of the above terms can be understood according to specific circumstances.
[0029] The technical solution of the present invention is further described in detail below through specific embodiments and in conjunction with the accompanying drawings:
[0030] Embodiment 1:
[0031] like Figures 1 to 4 As shown, a composite forming mold for thin-walled stainless steel pipe fittings is provided, including an upper mold 1 and a lower mold 2 that are interlocked, a punch mechanism and an injection mechanism, a first cavity and a second cavity for molding a first pipe 16 and a second pipe 17 are formed between the upper mold 1 and the lower mold 2, the first cavity and the second cavity are separated, the punch mechanism is arranged at one end of the first cavity and the second cavity, and the injection mechanism is arranged at the other end of the first cavity and the second cavity.
[0032] In this embodiment, the upper mold 1 and the lower mold 2 are made of Cr12MoV material, and the upper mold 1 and the lower mold 2 are buckled up and down to form the first cavity and the second cavity inside, and then the punch mechanism and the injection mechanism are respectively interference fit with the two ends of the first cavity and the second cavity to complete the mold closing. The rough tube is a straight-through tube adapted to the first cavity and is made of stainless steel. During the processing, the robot first puts the rough tube into the first cavity, and the injection mechanism passes 150MPa of liquid into the inner wall of the rough tube and maintains the pressure for 5 seconds. The rough tube is then swelled and formed into the first tube 16. Then the mold is opened, and the robot puts the first tube 16 into the second cavity, and puts the next rough tube to be processed into the first cavity, realizing the synchronous processing of the rough tube to the first tube 16 and the first tube 16 to the second tube 17.
[0033] Specifically, at least one parallel first upper cavity and second upper cavity are provided in the upper mold 1, and at least one parallel first lower cavity and second lower cavity are provided in the lower mold 2. The first cavity is formed between the first lower cavity and the first upper cavity, and the second cavity is formed between the second lower cavity and the second upper cavity.
[0034] In this embodiment, the first cavity is formed by the first upper cavity of the upper mold 1 and the first lower cavity of the lower mold 2, and the second cavity is formed by the second upper cavity of the upper mold 1 and the second lower cavity of the lower mold 2, so as to perform two steps of simultaneous processing on the rough tube.
[0035] Specifically, the first upper cavity and the first lower cavity have the same structure and both include a first semicircular through groove 9 arranged along the axial direction. At least one vertically connected first circular groove 10 is provided on the first semicircular through groove 9 of the first upper cavity.
[0036] In this embodiment, the blank tube expands under the pressure of the liquid until it fits with the inner wall of the first cavity to form a Figure 5 The first pipe 16.
[0037] Specifically, the second upper cavity and the second lower cavity have the same structure and both include two second semicircular through grooves 12 and one third semicircular through groove 13 arranged along the axial direction. The two second semicircular through grooves 12 are respectively connected to the two ends of the third semicircular through groove 13, and at least one vertically connected second circular groove 11 is provided on the third semicircular through groove 13 of the second upper cavity.
[0038] In this embodiment, the first tube 16 expands under the pressure of the liquid until it fits with the inner wall of the second cavity to form a Figure 6 The second pipe 17 of the three-way structure is shown.
[0039] Specifically, the connecting portion between the second semicircular through groove 12 and the third semicircular through groove 13 is recessed inward to form an inclined surface 15 . In this embodiment, the inclined surface 15 is used to form a chamfered structure of the second pipe 17 .
[0040] Specifically, the second semicircular through grooves 12 of the second upper cavity and the second lower cavity are respectively recessed inward to form corresponding semicircular ring grooves 14 . In this embodiment, the semicircular ring grooves 14 are used to form annular bulge structures at both ends of the second pipe 17 .
[0041] Specifically, the punch mechanism includes two punch parts 3 and two first telescopic structures 4, one end of each punch part 3 is respectively fixed to the telescopic ends of the two first telescopic structures 4, and the other end of one of the punch parts 3 penetrates into the first mold cavity, and the other end of the other punch part 3 penetrates into the second mold cavity.
[0042] In this embodiment, the punch member 3 is fixed to the first telescopic structure 4 by bolts, and the first telescopic structure 4 is a hydraulic cylinder.
[0043] Specifically, the injection mechanism includes two injection parts 5 and two second telescopic structures 6, one end of each injection part 5 is respectively fixed to the telescopic ends of the two second telescopic structures 6, and the other end of one of the injection parts 5 extends into the first cavity, and the other end of the other injection part 5 extends into the second cavity.
[0044] In this embodiment, the injection component 5 is fixed to the second telescopic structure 6 by bolts, and the second telescopic structure 6 is a hydraulic cylinder.
[0045] Specifically, one end of the two injection parts 5 is respectively provided with an injection port 501, one injection part 5 is connected to the first cavity through its injection port 501, and the other injection part 5 is connected to the second cavity through its injection port 501. In this embodiment, the injection parts 5 inject emulsion through their two injection ports 501.
[0046] Specifically, the four corners of the upper mold 1 and the lower mold 2 are respectively provided with guide holes 8, and the guide holes 8 are slidably connected with guide pillars 7. In this embodiment, the upper mold 1 and the lower mold 2 are slidably connected to the guide pillars 7 through their guide holes 8, and the upper mold 1 realizes mold closing and mold opening by sliding up and down.
[0047] Embodiment 2:
[0048] This embodiment is similar to Embodiment 1, except that, in this embodiment, a plurality of first cavities and second cavities are formed between the upper die 1 and the lower die 2, and the number of the punch mechanisms and the injection mechanisms is increased accordingly.
[0049] In this embodiment, a plurality of blank tubes and the first tube 16 can be processed at one time through a plurality of first cavities and a second cavities, thereby improving production efficiency.
[0050] Embodiment 3:
[0051] This embodiment is similar to Embodiment 1, except that, in this embodiment, the structure of the first upper cavity includes a first semicircular through groove 9 arranged along the axial direction and two first circular grooves 10 vertically connected to the first semicircular through groove 9 respectively.
[0052] Specifically, the structure of the second upper cavity includes two second semicircular through grooves 12, a third semicircular through groove 13 and two second circular grooves 11 arranged along the axial direction, the two second semicircular through grooves 12 are respectively connected to the two ends of the third semicircular through groove 13, and the two second circular grooves 11 are respectively vertically connected to the third semicircular through groove 13.
[0053] In this embodiment, the forming of the four-way structure pipe can be completed accordingly by changing the number of the first circular grooves 10 and the second circular grooves 11.
[0054] Although the embodiments of the present invention have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations of the present invention. Ordinary technicians in the field can change, modify, replace and modify the above embodiments within the scope of the present invention.
[0055] Obviously, the above embodiments of the utility model are only examples for clearly explaining the utility model, and are not intended to limit the implementation methods of the utility model. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made on the basis of the above description. It is not necessary and impossible to list all the implementation methods here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the utility model should be included in the protection scope of the claims of the utility model.
Claims
1. A composite forming die for thin-walled stainless steel pipe fittings, characterized in that: The invention comprises an upper die (1) and a lower die (2) which are interlocked with each other, a punch mechanism and an injection mechanism, wherein at least one first cavity and a second cavity for molding a first tube (16) and a second tube (17) are formed between the upper die (1) and the lower die (2), the first cavity and the second cavity are separated from each other, the punch mechanism is arranged at one end of the first cavity and the second cavity, the injection mechanism is arranged at the other end of the first cavity and the second cavity, the upper die (1) is provided with at least one first upper cavity and a second upper cavity which are parallel to each other, the lower die (2) is provided with at least one first lower cavity and a second lower cavity which are parallel to each other, the first lower cavity and the first upper cavity are formed between the first lower cavity and the first upper cavity A mold cavity, wherein the second mold cavity is formed between the second lower cavity and the second upper cavity, the first upper cavity and the first lower cavity have the same structure and both include a first semicircular through groove (9) arranged along the axial direction, the first semicircular through groove (9) of the first upper cavity is provided with at least one vertically connected first circular groove (10), the second upper cavity and the second lower cavity have the same structure and both include two second semicircular through grooves (12) and one third semicircular through groove (13) arranged along the axial direction, the two second semicircular through grooves (12) are respectively connected to the two ends of the third semicircular through groove (13), and the third semicircular through groove (13) of the second upper cavity is provided with at least one vertically connected second circular groove (11).
2. A composite forming die for a thin-walled stainless steel pipe according to claim 1, characterized in that: The connecting point between the second semicircular through groove (12) and the third semicircular through groove (13) is recessed inwards to form an inclined surface (15).
3. The composite forming die for a thin-walled stainless steel pipe according to claim 1, characterized in that: The second semicircular through grooves (12) of the second upper cavity and the second lower cavity are respectively recessed inwards to form corresponding semicircular ring grooves (14).
4. The composite forming die for a thin-walled stainless steel pipe according to claim 1, characterized in that: The punch mechanism comprises two punch parts (3) and two first telescopic structures (4), one end of each of the punch parts (3) is respectively fixed to the telescopic ends of the two first telescopic structures (4), and the other end of one of the punch parts (3) penetrates into the first cavity, while the other end of the other punch part (3) penetrates into the second cavity.
5. The composite forming die for a thin-walled stainless steel pipe according to claim 1, characterized in that: The injection mechanism comprises two injection pieces (5) and two second telescopic structures (6), one end of each of the injection pieces (5) being respectively fixed to the telescopic ends of the two second telescopic structures (6), and the other end of one of the injection pieces (5) extending into the first cavity, and the other end of the other injection piece (5) extending into the second cavity.
6. A composite forming die for thin-walled stainless steel pipe fittings according to claim 5, characterized in that: An injection port (501) is respectively provided at one end of the two injection pieces (5); one of the injection pieces (5) is connected to the first cavity through its injection port (501), and the other of the injection pieces (5) is connected to the second cavity through its injection port (501).
7. The composite forming die for a thin-walled stainless steel pipe according to claim 1, characterized in that: The four corners of the upper die (1) and the lower die (2) are respectively provided with guide holes (8), and guide pillars (7) are slidably connected in the guide holes (8).