Sliding chip, sliding chip assembly and mold for manufacturing sliding chip assembly

By designing molds and components for the SlipChip, combined with the injection and curing of PDMS materials, the bubble-mediated acoustic mixing function in the SlipChip is achieved, solving the problem of low mixing efficiency in the SlipChip and significantly shortening the mixing time.

CN221913066UActive Publication Date: 2024-10-29SHANGHAI CARBOXY BIOPHARMACEUTICAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420577063.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-22
Publication Date
2024-10-29
Estimated Expiration
2034-03-22

AI Technical Summary

Technical Problem

The lack of bubble-mediated sonic mixing in the SlipChip results in low mixing efficiency and long mixing times.

Method used

Design a mold, including a first template and a second template. A molding cavity is formed through the combination of the molds. PDMS material is injected and solidified to form a sliding chip component. The component includes a bubble generating part and a piezoelectric mounting part to realize bubble-mediated Sonic mix.

Benefits of technology

The bubble-mediated acoustic mixing function in the sliding chip is realized, which significantly improves the mixing efficiency and shortens the mixing time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221913066U_ABST
    Figure CN221913066U_ABST
Patent Text Reader

Abstract

The utility model discloses a sliding chip, an assembly thereof and a mould used for manufacturing the sliding chip assembly, the mould comprises a first template and a second template, the first template is provided with an injection groove, a recessed groove and a projection, the second template is provided with a hollow area and a structural member, and a molding cavity is formed between the first template and the second template after the first template and the second template are combined. A manufacturing material such as PDMS is injected into a forming cavity and then cured, a sliding chip assembly is manufactured, and the sliding chip assembly is bonded to a glass-based chip to form a first micro-fluidic chip, so that the sliding chip kit provided with the first micro-fluidic chip and a second micro-fluidic chip which slide relatively has a bubble-mediated sound wave mixing function.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of biotechnology, in particular to a sliding chip and a component thereof and a mold for manufacturing the sliding chip component. Background Art

[0002] Microfluidics Chip, also known as Lab-on-a Chip (LOC), is a chip that can precisely manipulate microfluids in micron-scale microtubes to perform various functions of conventional physical, chemical or biological experiments on micron-scale chips. Microfluidics chips are characterized by miniaturization, automation, integration, portability, high throughput and low sample requirements. They provide a promising analytical platform for in vitro diagnosis, integrating sample pretreatment, sample addition, reagent mixing, reaction and detection analysis, achieving "sample in, result out".

[0003] Take the Slip Chip as an example. The Slip Chip is composed of two hydrophobic chips with precision microstructures and microchannels. When the two chips are in close contact, a complete fluid channel can be formed, and the sample can be loaded into the internal chamber of the chip. By simply sliding the two chips relative to each other, the original connected fluid path can be cut off, thereby generating an independent chamber space to complete various reactions. At the same time, through the ingenious chip design, the chip can change its different connection states by sliding position control, thereby realizing a multi-step sample addition reaction process. The Slip Chip can quickly control the fluid in the chamber without the need for traditional pumps, valves and other complex mechanical equipment. It is a simple, low-cost microfluidic device.

[0004] Mixing is generally considered to be a necessary process for reactants to contact before the reaction. It is crucial to form a fast, efficient, easy-to-control and easy-to-integrate micromixer in a microfluidic chip. The micromixers in a microfluidic chip are mainly divided into passive micromixers and active micromixers. Passive micromixers rely on the geometric shape or fluid properties in the microfluidic chip to produce a mixing effect. In addition to the force that drives the fluid flow, the mixing generally does not rely on other external forces, and the internal structure design of the chip is usually more complex. Active micromixers rely on external forces such as electric fields, magnetic fields, acoustic fields, and thermal effects to help the mixing of microfluids. They have high mixing efficiency and can flexibly control the time and location of microfluid mixing.

[0005] The bubble induced acoustic mixing (BIAM) method is a method that uses an acoustic field to achieve active mixing. A series of bubbles that meet the size requirements are introduced into the solution to be mixed, and ultrasonic waves are excited through lead zirconate titanate (PZT) ceramics with a high electromechanical coupling coefficient. The stable circulating flow induced by the acoustic field causes the bubbles remaining on the solid surface to vibrate, thereby forming spherical convection and accelerating the mixing process. Using this method, the time to completely mix, for example, 22 μL of solution can be reduced from several hours (mixing based entirely on diffusion) to tens of seconds. However, the general BIAM function is applied in an integrated microfluidic chip, and there is currently no use of the BIAM function in a sliding chip to mix solutions. Utility Model Content

[0006] In view of the above-mentioned defects or shortcomings of the prior art, the present invention discloses a slip chip and its components and a mold for making the slip chip components, so as to fill the problem that the existing slip chip lacks the bubble-mediated acoustic wave mixing function.

[0007] To achieve the above-mentioned purpose, the utility model discloses a mold for making a sliding chip assembly, the mold comprising: a first template, comprising a first template body, an injection groove is provided on the first template body, a recessed groove is provided in a first configuration area of ​​the injection groove, and a protrusion for forming a bubble generating portion is provided on the recessed groove; a second template, comprising a second template body, the second template body is provided with a hollow area, and a structure for forming a piezoelectric mounting portion is provided in a second configuration area of ​​the second template body; wherein a molding cavity is formed between the second template and the first template after the second template is combined, and the second configuration area of ​​the second template corresponds to the first configuration area of ​​the first template.

[0008] In a preferred embodiment of the present invention, a placement groove for placing the second template is provided on the first template body, the size of the placement groove is adapted to the second template body of the second template, the bottom of the placement groove is higher than the bottom of the injection groove, and after the second template is placed in the placement groove of the first template, a gap is left between the two.

[0009] In a preferred embodiment of the present invention, the recessed groove comprises a circular recessed groove, a triangular recessed groove, a rectangular recessed groove, or a hexagonal recessed groove.

[0010] In a preferred embodiment of the present invention, a plurality of protrusions are evenly distributed in the recessed groove, the protrusions protrude from the recessed groove and the tops of the protrusions are higher than the bottom of the injection groove.

[0011] In a preferred embodiment of the present invention, the protrusion is a cylinder, a truncated cone that is wider at the bottom and narrower at the top, a regular polygonal prism with a regular polygonal cross section, or a regular polygonal cone with a regular polygonal cross section.

[0012] In a preferred embodiment of the present invention, an injection mark for marking the injection amount of PDMS material is provided on the second template body.

[0013] In a preferred embodiment of the present invention, the injection mark is a concave notch on the second template body, and the bottom surface of the concave notch is higher than the bottom surface of the structural member but lower than the top surface of the structural member.

[0014] In a preferred embodiment of the present invention, the structural member is connected to the second template body via a connecting member.

[0015] In a preferred embodiment of the present invention, the structural member is a circular panel or a polygonal panel.

[0016] The utility model also discloses a sliding chip assembly, which includes a chip substrate, a bubble generating portion provided on a first surface of the chip substrate, and a piezoelectric mounting portion provided on a second surface of the chip substrate. Alternatively, the sliding chip assembly is defined by the molding cavity of the mold as described above.

[0017] The utility model further discloses a sliding chip, which includes a glass-based chip and the aforementioned sliding chip assembly, wherein a side of the sliding chip assembly provided with a bubble generating portion is bonded to the glass-based chip, and a piezoelectric device is provided in a piezoelectric mounting portion of the sliding chip assembly.

[0018] The utility model further discloses a slip chip kit, comprising a first microfluidic chip and a second microfluidic chip that are used in conjunction with each other and can slide relatively, wherein the first microfluidic chip is the slip chip as described above.

[0019] The utility model discloses a slip chip and its components and a mold for making the slip chip components. The mold comprises a first template and a second template. The first template is provided with an injection groove, a concave groove and a protrusion. The second template is provided with a hollow area and a structure. The first template and the second template are combined to form a molding cavity between the two. A manufacturing material, such as PDMS, is injected into the molding cavity and then solidified to make a slip chip component. The slip chip component is bonded to a glass-based chip to form a first microfluidic chip, so that the slip chip kit configured with the first microfluidic chip and the second microfluidic chip that slide relatively has a bubble-mediated acoustic wave mixing function.

[0020] The concept, specific structure and technical effects of the present invention will be further described below in conjunction with the accompanying drawings to fully understand the purpose, characteristics and effects of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 Shown is an exploded schematic diagram of one embodiment of a mold used to make a SlipChip assembly.

[0022] Figure 2 Shown is an overall schematic diagram of a mold used to make a SlipChip assembly in one embodiment.

[0023] Figure 3 It is a schematic structural diagram of the first surface of the slip chip assembly of the present invention.

[0024] Figure 4 It is a schematic diagram showing the structure of the second surface of the slip chip assembly of the present invention.

[0025] Figure 5 Shown is a schematic structural diagram of a glass-based chip in one embodiment.

[0026] Figure 6 Shown is a schematic cross-sectional view of an embodiment of the SlipChip kit of the present invention. DETAILED DESCRIPTION

[0027] The following is an explanation of the embodiments of the present disclosure by specific examples, and those skilled in the art can easily understand other advantages and effects of the present disclosure from the information disclosed by the present disclosure. The present disclosure can also be implemented or applied through other different specific embodiments, and the details in the present disclosure can also be modified or changed in various ways according to different viewpoints and application modules without departing from the spirit of the present disclosure. It should be noted that the embodiments in the present disclosure and the features in the embodiments can be combined with each other without conflict.

[0028] The following is a detailed description of the embodiments of the present disclosure with reference to the accompanying drawings so that those skilled in the art can easily implement the present disclosure. The present disclosure can be embodied in many different forms and is not limited to the embodiments described herein.

[0029] In the representation of the present disclosure, the terms "first", "second" are only used for representation purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. Although the terms first, second, etc. are used to represent various elements in this article in some examples, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. For example, the first interface and the second interface, etc. are represented. Moreover, as used in this article, the singular forms "one", "one" and "the" are intended to also include plural forms, unless there is an opposite indication in the context. It should be further understood that the terms "comprising", "including" indicate that there are described features, steps, operations, elements, modules, projects, kinds, and / or groups, but do not exclude the existence, occurrence or addition of one or a group of other features, steps, operations, elements, modules, projects, kinds, and / or groups. The terms "or" and "and / or" used herein are interpreted as inclusive, or mean any one or any combination. Thus, “A, B, or C” or “A, B and / or C” means “any of the following: A; B; C; A and B; A and C; B and C; A, B, and C.” An exception to this definition will occur only when a combination of elements, functions, steps, or operations are inherently mutually exclusive in some manner.

[0030] In the prior art, for a sliding chip, the microstructures on the two chips can be connected and disconnected by sliding the first chip relative to the second chip for alignment operation, thereby completing the mixing of reagents and the corresponding reaction. However, the mixing of reagents in the sliding chip is mostly done without the help of external force, and the internal structure design of the first chip and the second chip in the sliding chip is relatively complex. Therefore, the mixing takes a long time, is inefficient, and the mixing effect is also poor. The industry has also proposed active micro-mixing technology, which uses external forces such as electric fields, magnetic fields, acoustic fields, and thermal effects to help the mixing of microfluids. The mixing efficiency is high and the time and location of microfluid mixing can be flexibly controlled. Among them, bubble-mediated acoustic mixing BIAM is a commonly used method. However, this type of technology has not been applied to sliding chips.

[0031] In view of this, the present invention discloses a slip chip and its components and a mold for making the slip chip components, which are used to solve various deficiencies in the existing related technologies.

[0032] See also Figure 1 and Figure 2 ,in, Figure 1 Shown is an exploded schematic diagram of a mold used to make a SlipChip assembly in one embodiment, Figure 2 Shown is an overall schematic diagram of a mold used to make a SlipChip assembly in one embodiment.

[0033] like Figure 1 and Figure 2As shown, the mold for making the SlipChip assembly includes a first template 11 and a second template 13.

[0034] The first template 11 includes a first template body 111, which is substantially in the shape of a rectangular panel. The first template body 111 is provided with an injection groove 113, which is substantially in the shape of a rectangle. The transverse dimension of the injection groove 113 (the area formed by the length and width of the injection groove 113) determines the dimension of the chip substrate in the SlipChip assembly to be manufactured (the area formed by the length and width of the chip substrate), and the groove depth of the injection groove 113 is related to the thickness of the chip substrate in the SlipChip assembly to be manufactured.

[0035] A recessed groove 114 is provided in the first configuration area of ​​the injection groove 113. The first configuration area is located in the middle area of ​​the injection groove 113, and the recessed groove 114 is formed by being recessed on the basis of the injection groove 113. The injection groove 113 may be provided with one or more first configuration areas, and one or more recessed grooves 114 may be provided at each first configuration area. The shape of the recessed groove 114 may vary according to the production process and the application of the sliding chip kit, and the recessed groove 114 may be a circular recessed groove, a triangular recessed groove, a rectangular recessed groove, a hexagonal recessed groove, or a recessed groove of other shapes. Figure 1 In the illustrated embodiment, a first configuration area may be provided on each side of the central region of the injection groove 113 , and two parallel recessed grooves 114 may be provided at each first configuration area. The recessed grooves 114 are hexagonal recessed grooves.

[0036] The depression 114 is provided with a protrusion 115 for forming a bubble generating portion, and the protrusion 115 is provided at the bottom of the depression 114 and protrudes from the depression 114. The protrusion can be a cylinder, a truncated cone with a wide bottom and a narrow top, a regular polygonal prism with a regular polygonal cross section, a regular polygonal cone with a regular polygonal cross section, or a column structure of other shapes. Figure 1 In the illustrated embodiment, a plurality of protrusions 115 are evenly arranged in the recessed groove 114, and the protrusions 115 are cylindrical structures. In some embodiments, the diameter of the protrusions 115 is approximately 0.60 mm to 1.00 mm, for example, 0.60 mm, 0.65 mm, 0.70 mm, 0.75 mm, 0.80 mm, 0.85 mm, 0.90 mm, 0.95 mm, 1.00 mm, or other diameter sizes. In addition, the protrusions 115 protrude from the recessed groove 114 and the top of the protrusions 115 is higher than the bottom of the injection groove 113 (i.e., the top of the recessed groove 114), that is, the height of the protrusions 115 is greater than the groove depth of the recessed groove 114.

[0037] The second template 13 includes a second template body 131, which is roughly a rectangular panel-shaped structure. The second template body 131 is provided with a hollow area, and a structural member 132 for forming a piezoelectric mounting portion is provided in the second configuration area of ​​the second template body 131. The second configuration area is located in the middle area of ​​the hollow area, and the hollow area may be provided with one or more second configuration areas, and one or more structural members 132 may be provided at each second configuration area. The shape of the structural member 132 may vary depending on the production process and the shape of the piezoelectric generating part. The structural member 132 may be a circular panel, a polygonal panel (such as a regular hexagon, a regular octagon, a regular dodecagon, etc.), or a panel of other shapes. In the case of Figure 1 In the illustrated embodiment, a second configuration area may be provided on each side of the central region of the hollow area, and a structural member 132 may be provided at each second configuration area. The structural member 132 is connected to the second template body 131 via a connecting member 133, and the structural member 132 may be a circular panel.

[0038] The thickness of the structural member 132 may be consistent with the thickness of the second template body 131, but it is not limited thereto. The thickness of the structural member 132 may also be inconsistent with the thickness of the second template body 131. For example, in some embodiments, the thickness of the structural member 132 may be less than the thickness of the second template body. In some embodiments, the thickness of the structural member 132 may be greater than the thickness of the second template body. In addition, the connecting member 133 is mainly used to connect the structural member 132 with the second template body 131, so the shape and thickness of the connecting member 133 are not limited here.

[0039] As mentioned above, the second template body 131 is roughly in the shape of a rectangular panel. In order to combine the second template 13 with the first template 11, the first template body 111 is provided with a placement groove 112 for placing the second template 13. The size of the placement groove 112 is adapted to the second template body 131 of the second template 13. In this way, the second template 13 can be fitted and placed in the placement groove 112, ensuring that the first template 11 will not shift and can be stably combined with the first template 11. Figure 1 In the illustrated embodiment, the seating groove 112 is roughly rectangular, with a size larger than that of the injection groove. The seating groove 112 has four side walls, which are recessed downward from the first template body 111 and form a step portion relative to the injection groove 113, that is, the bottom of the seating groove 112 is higher than the bottom of the injection groove 113.

[0040] Regarding the groove depth of the placement groove 112, in some embodiments, the groove depth of the placement groove 112 is less than the thickness of the second template body 131, so that when the second template 13 is placed in the placement groove 112 of the first template 11, the second template body 131 in the second template 13 is protruding from the first template body 111 in the first template 11. In some embodiments, the groove depth of the placement groove 112 is equal to the thickness of the second template body 131, so that when the second template 13 is placed in the placement groove 112 of the first template 11, the second template body 131 in the second template 13 is flush with the first template body 111 in the first template 11. In some embodiments, the groove depth of the placement groove 112 is greater than the thickness of the second template body 131, so that when the second template 13 is placed in the placement groove 112 of the first template 11, the second template body 131 in the second template 13 is recessed in the first template body 111 in the first template 11. When the groove depth of the placement groove 112 is greater than or equal to the thickness of the second template body 131, in some embodiments, at least one corner of the placement groove is provided with a prying groove for facilitating the grabbing of the second template. For example, a prying groove is provided at each of the four corners of the placement groove, the prying groove is connected to the placement groove, the prying groove is a semicircular structure or a petal-shaped structure as a whole, and the depth of the prying groove may be less than or equal to the depth of the placement groove. In actual applications, the experimenter manually contacts the second template in the placement groove through the prying groove and takes it out of the placement groove.

[0041] In certain embodiments, such as Figure 1 As shown, taking the top surface of the first template body 111 as a reference, the bottom of the injection groove 113 is lower than the top surface of the first template body 111 by H (i.e., the groove depth of the injection groove 113 is H), the bottom of the recessed groove 114 is lower than the bottom of the injection groove 113 by h (i.e., the groove depth of the recessed groove 114 is h), the height of the protrusion 115 is t, and the height t of the protrusion is greater than the groove depth h of the recessed groove 114, the bottom of the seating groove 112 is lower than the top surface of the first template body 111 by s (i.e., the groove depth of the seating groove 112 is s), and the groove depth s of the seating groove 112 is less than the groove depth H of the injection groove 113.

[0042] In practical applications, after the second template 13 is placed in the seating groove 112 of the first template 11, a gap is left between the two, which is the distance between the bottom of the second template 13 (i.e., the bottom of the seating groove 112) and the bottom of the injection groove 113 in the first template 11. Therefore, if the height difference between the bottom of the seating groove and the bottom of the injection groove 113 determines the size of the injection gap, that is, the greater the height difference, the greater the injection gap, and the greater the thickness of the formed SlipChip assembly, the smaller the height difference, the smaller the injection gap, and the smaller the thickness of the formed SlipChip assembly.

[0043] Correspondingly, the second template body 131 may also be provided with an injection mark for displaying the injection amount of the injection material.

[0044] For bubble-mediated acoustic wave mixing technology, when sound waves enter another different medium from one phase, most of the sound waves will be reflected at the interface due to the mismatch of acoustic impedance. Different chip materials have different acoustic impedances and different degrees of reflection of sound waves. If the acoustic impedance is more mismatched, the efficiency of sound wave transmission will be greatly reduced, thereby affecting the efficiency of bubble vibration and further affecting the efficiency of liquid mixing. Therefore, choosing the right chip material is crucial to the final mixing effect. Among the commonly used materials for chips, the acoustic impedance of polydimethylsiloxane (PDMS) material is 1.048*10 6 kg / m 2 s -1 Acoustic impedance with aqueous solution 1.5*10 6 kg / m 2 s -1 The appearance of the PDMS material varies from a colorless and transparent volatile liquid to a very high viscosity liquid or silica gel, and the PDMS material has good chemical stability. Therefore, in this embodiment, the PDMS material is used as the manufacturing material and injected into the mold to form the SlipChip assembly. Of course, in other embodiments, other suitable polymers can also be selected according to actual applications.

[0045] Thus, the injection mark on the second template body 131 can identify the injection amount of the PDMS material. Thus, according to the injection mark, the injection amount of the PDMS can be known and the thickness of the SlipChip assembly to be manufactured can be controlled. Specifically, the injection mark is used to identify the injection amount of the PDMS material in the hollow area, and the injection mark can be used to know the injection amount of the PDMS in the hollow area and control the thickness of the hollow area in the SlipChip assembly to be manufactured.

[0046] After the placement is completed, there is a gap between the bottom of the second template 13 and the bottom of the injection groove 113 in the first template 11. The injected PDMS material will fill the gap between the bottom of the second template 13 and the bottom of the injection groove 113 in the first template 11. After continued injection, the injection liquid level gradually rises and begins to submerge the structure 132 until it covers and submerges the structure 132. Therefore, the injection mark can be used to know the injection amount of PDMS in the hollow area and control the thickness of the hollow area in the SlipChip assembly to be manufactured. Figure 1 In the embodiment shown, injection marks 134 for marking the injection amount of PDMS material are provided on the four sides of the second template body 131. The injection marks 134 are provided on the recess 134 on the second template body 131. The bottom surface of the recess 134 is higher than the bottom surface of the structural member 132 but lower than the top surface of the structural member 132. In this way, the injection amount of PDMS in the hollow area is known by using the recess 134 as the injection mark, and the thickness of the hollow area in the SlipChip assembly to be manufactured is controlled. For example, when the injection amount of PDMS in the hollow area reaches the bottom of the recess 134 and until the recess is partially covered, the injection of PDMS is stopped. In this way, the second surface of the chip substrate in the manufactured SlipChip assembly can be formed with a piezoelectric mounting portion corresponding to the structural member 132. As mentioned above, in some embodiments, the structural member 132 is a circular panel, and the piezoelectric mounting portion formed corresponding to the structural member 132 is a circular mounting groove.

[0047] When the application Figure 1 and Figure 2 When a mold for making a SlipChip assembly is shown, the operation process may generally include:

[0048] First, preparation work is performed, providing a mold and configuring a PDMS prepolymer. The provision of the mold includes providing the first template 11 and the second template 13 as described above. The configuration of the PDMS prepolymer includes: weighing the PDMS monomer and the curing agent according to a certain ratio (for example, the mass ratio of the PDMS monomer to the curing agent is 10:1); fully stirring the PDMS monomer and the curing agent; after mixing evenly, placing the mixed PDMS prepolymer in a vacuum drying oven, turning on the vacuum pump, and completely expelling the bubbles in the PDMS prepolymer.

[0049] Next, the second template 13 is placed in the recess of the first template 11 . At this time, a molding cavity is formed between the second template 13 and the first template 11 .

[0050] The prepared PDMS prepolymer is injected into the molding cavity, for example, the PDMS prepolymer is injected into the molding cavity through the hollow area of ​​the second template 13. After the injected PDMS prepolymer fills the molding cavity and reaches the injection mark position of the second template 13, the injection of the PDMS prepolymer is stopped.

[0051] The mold injected with the PDMS prepolymer is placed in an oven for curing. In some embodiments, the mold injected with the PDMS prepolymer can be placed in an oven and cured for a certain time (the curing time can be, for example, 2 hours to 4 hours) at 60° C. to 80° C. (for example, 60° C., 65° C., 70° C., 75° C., 80° C., or other temperatures).

[0052] The mold after curing is taken out and demolded to obtain a molded SlipChip assembly.

[0053] See also Figure 3 and Figure 4 ,in, Figure 3 It is a schematic diagram showing the structure of the first surface of the slip chip assembly of the utility model, Figure 4 The schematic diagram of the structure of the second surface of the slip chip assembly of the utility model is shown. The slip chip assembly disclosed in the utility model is obtained by Figure 1 and Figure 2 The mold shown is made.

[0054] Combination Figure 3 and Figure 4 As shown, the slide chip assembly 2 includes a chip substrate 21 , a bubble generating portion 23 disposed on a first surface of the chip substrate 21 , and a piezoelectric mounting portion 24 disposed on a second surface of the chip substrate 21 .

[0055] The chip substrate 21 is formed by injecting PDMS material (eg, PDMS prepolymer) into a molding cavity formed by combining the second template 13 and the first template 11 .

[0056] A bubble generating portion 23 is formed on the first surface of the chip substrate 21 for generating stable bubbles. In some embodiments, the bubble generating portion 23 is a concave hole grown on the boss 22. The boss 22 corresponds to the concave groove 114 of the first template 11. For example, the concave groove 114 is a hexagonal concave groove, and the formed boss 22 is a hexagonal boss. The concave hole 23 corresponds to the protrusion 115 in the first template 11. For example, the protrusion 115 is a cylinder, and the concave hole 23 is a circular concave hole. In some embodiments, considering the size of the microfluidic chamber in the microfluidic chip in the sliding chip kit, the larger the size of the bubble generated, the lower the required frequency, and the optimal acoustic wave frequency of the PZT ceramic is 4kHz to 5kHz, so the maximum diameter of the circular concave hole can be set to 1.0 mm. The diameter of the circular recessed hole 23 is approximately 0.60 mm to 1.00 mm, for example, 0.60 mm, 0.65 mm, 0.70 mm, 0.75 mm, 0.80 mm, 0.85 mm, 0.90 mm, 0.95 mm, 1.00 mm, or other diameter sizes.

[0057] A piezoelectric mounting portion 24 is formed on the second surface of the chip substrate 21. The piezoelectric mounting portion 24 is used to mount a piezoelectric device (the piezoelectric device can be a piezoelectric ceramic, such as a PZT ceramic). In some embodiments, the piezoelectric mounting portion 24 is a circular mounting groove. The piezoelectric mounting portion 24 corresponds to the structure 132 of the second template 13.

[0058] The present embodiment further provides a sliding chip, which includes a glass substrate chip and the sliding chip assembly 2, wherein a side of the sliding chip assembly 2 provided with a bubble generating portion 23 is bonded to the glass substrate chip, and a piezoelectric device, such as PZT ceramic, is provided in the piezoelectric mounting portion 24 of the sliding chip assembly 2.

[0059] See also Figure 5 , which is a schematic diagram of the structure of the glass-based chip in one embodiment. Figure 5 As shown, the glass substrate chip 3 includes a glass substrate chip body 31, on which a cavity sleeve 32, a flow channel 33, and a through hole 34 are provided. The cavity sleeve 32 penetrates the glass substrate chip body 31, the flow channel 33 is communicated with the cavity sleeve 32, and the through hole 34 penetrates the glass substrate chip body 31 and is communicated with the flow channel 33. The shape of the cavity sleeve 32 is consistent with the shape of the boss 22 in the sliding chip assembly 2. For example, if the boss of the sliding chip assembly 2 is a hexagonal boss, the cavity sleeve 32 is a hexagonal cavity sleeve.

[0060] When the aforementioned Figure 3 and Figure 4When the Slipchip assembly 2 in the embodiment is bonded to the glass substrate chip 3, the Slipchip assembly 2 is buckled with its first surface corresponding to the first surface of the glass substrate chip 3, wherein the bosses 22 on the first surface of the Slipchip assembly 2 correspond to the cavity sleeve 32 of the glass substrate chip 3, and the Slipchip assembly 2 is bonded to the glass substrate chip 3, and each of the recessed holes 23 on the bosses 22 in the Slipchip assembly 2 can be seen from the second surface of the glass substrate chip 3.

[0061] In the present invention, the PDMS material is relatively soft and cannot be used alone to achieve sliding operation. Therefore, the sliding chip assembly is combined with a glass-based chip suitable for sliding operation to obtain a luminescent oxygen channeling immunoassay (LOCI) sliding chip that can integrate BIAM function and has good sliding function, referred to as LOCI sliding chip.

[0062] See also Figure 6 , which is a schematic cross-sectional view of a slip chip kit of the present invention in one embodiment. Figure 6 As shown, the slip chip kit includes a first microfluidic chip and a second microfluidic chip 4 that are used in conjunction with each other and can slide relatively, wherein the first microfluidic chip is a slip chip that bonds the glass-based chip 3 and the slip chip assembly 2, and a PZT ceramic 5 is disposed in the piezoelectric mounting portion 24 of the slip chip assembly 2, and the PZT ceramic sheet 5 is bonded in the piezoelectric mounting portion 24 (for example, a circular piezoelectric mounting groove) on the second surface of the slip chip assembly 2.

[0063] When in actual application, the first microfluidic chip and the second microfluidic chip 4 are in close contact up and down and can form a corresponding fluid channel by sliding relative to the corresponding position, at which time the sample can be loaded into the internal chamber of the chip. Afterwards, the first microfluidic chip and the second microfluidic chip 4 are relatively slid, so that the original connecting fluid passage can be cut off, thereby generating an independent chamber space to complete various reactions. During the reaction, when the liquid sample is added to the chamber, bubbles will form in the concave hole 23. At the same time, an alternating voltage is applied to the PZT ceramic 5, and the PZT ceramic 5 will produce piezoelectric effect to produce electrostrictive vibration, which can generate sound waves. The acoustic signal of the PZT ceramic sheet is excited by the square signal, so that the bubbles in the concave hole 23 vibrate and make sounds, thereby forming a spherical convection to achieve the mixing of the LOCI immune reaction solution.

[0064] The preferred specific embodiments of the utility model are described in detail above. It should be understood that ordinary technicians in this field can make many modifications and changes based on the concept of the utility model without creative work. Therefore, all technical solutions that can be obtained by technicians in this technical field based on the concept of the utility model through logical analysis, reasoning or limited experiments on the basis of the existing technology should be within the scope of protection determined by the claims.

Claims

1. A mold for making a SlipChip assembly, characterized in that: The mold comprises: The first template comprises a first template body, wherein the first template body is provided with an injection groove, a concave groove is provided in a first configuration area of ​​the injection groove, and a protrusion for forming a bubble generating portion is provided on the concave groove; and The second template includes a second template body, wherein the second template body is provided with a hollow area, and a structural member for forming a piezoelectric mounting portion is provided in a second configuration area of ​​the second template body; Wherein, after the second template is combined with the first template, a molding cavity is formed between the two, and the second configuration area of ​​the second template corresponds to the first configuration area of ​​the first template.

2. The mold for making a SlipChip assembly according to claim 1, wherein The first template body is provided with a placement groove for accommodating the second template. The size of the placement groove is adapted to the second template body of the second template. The bottom of the placement groove is higher than the bottom of the injection groove. After the second template is placed in the placement groove of the first template, a gap is left between the two.

3. The mold for making a SlipChip assembly according to claim 1, wherein The concave groove includes a circular concave groove, a triangular concave groove, a rectangular concave groove, or a hexagonal concave groove.

4. The mold for making a SlipChip assembly according to claim 1 or 3, characterized in that: A plurality of protrusions are evenly arranged in the concave groove, the protrusions protrude from the concave groove and the tops of the protrusions are higher than the bottom of the injection groove.

5. The mold for making a SlipChip assembly according to claim 1, wherein The second template body is provided with an injection mark for marking the injection amount of the manufacturing material.

6. The mold for making a SlipChip assembly according to claim 5, wherein: The injection mark is a concave notch on the second template body, and a bottom surface of the concave notch is higher than a bottom surface of the structural member but lower than a top surface of the structural member.

7. The mold for making a SlipChip assembly according to claim 1 or 6, characterized in that: The structural member is connected to the second template body via a connecting member.

8. A SlipChip assembly, characterized in that The SlipChip assembly includes a chip substrate, a bubble generating portion provided on a first surface of the chip substrate, and a piezoelectric mounting portion provided on a second surface of the chip substrate, or the SlipChip assembly is defined by a molding cavity of a mold according to any one of claims 1 to 7.

9. A SlipChip, characterized in that The invention comprises a glass substrate chip and the SlipChip assembly according to claim 8, wherein a side of the SlipChip assembly provided with a bubble generating portion is bonded to the glass substrate chip, and a piezoelectric device is provided in a piezoelectric mounting portion of the SlipChip assembly.

10. A SlipChip kit, characterized in that The invention comprises a first microfluidic chip and a second microfluidic chip which are used in cooperation and can slide relatively, wherein the first microfluidic chip is the sliding chip as claimed in claim 9.