Test piece mold for testing tensile breaking strength of emulsified asphalt evaporation residues
By designing a cast emulsified asphalt evaporation residue tensile fracture strength test mold with adjustable mold cavity depth, the crack problems caused by cutting and volume shrinkage problems caused by evaporation are solved, and high-precision test results and simple demolding process are achieved. .
Patent Information
- Application Number
- CN202323656870.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-31
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-12-31
AI Technical Summary
The existing tensile fracture strength test specimen molds are prone to cause cracks in the edge or internal part of the specimen during the cutting process, which affects the accuracy of the test results. The evaporation of water-based epoxy emulsified asphalt causes volume shrinkage, making it difficult to ensure the specimen. The thickness meets the standards, resulting in a breaking strength test error.
A casting mold is designed with adjustable cavity depth, adopting a base inner core and drive shaft that can move up and down, and adjusting the depth of the base inner core through the knob and control rod to ensure that the evaporated residue reaches the standard thickness and pass The extraction channel is easy to release and avoid stress damage.
It improves the accuracy of the test results and the integrity of the test piece, reduces the error in the fracture strength test, ensures the surface finish and inner wall cleanliness of the test piece, and enhances the reliability of the test.
Smart Images

Figure CN221945681U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of asphalt testing molds, in particular to a tensile fracture strength testing specimen mold for emulsified asphalt evaporation residues. Background Art
[0002] As an important material in highway maintenance, emulsified asphalt is favored for its many advantages such as easy construction, energy saving and consumption reduction, and low cost. However, simply using emulsified asphalt as a binder can no longer meet the stringent requirements of large traffic volume and heavy traffic. Water-based epoxy resin is a type of "green" engineering material with strong adhesion, high curing strength, and excellent high-temperature stability. Water-based epoxy emulsified asphalt prepared with it as a modifier is used in cold mixes, micro-surfacing, fog seal cold recycled mixtures, etc. It has a series of potential advantages such as high strength, durability, anti-skid, and ultra-thinness.
[0003] The evaporation residue performance of emulsified asphalt materials is a key indicator to characterize their road performance. Since water-based epoxy modified emulsified asphalt demulsifies and solidifies into epoxy asphalt, the evaporation residue property test of modified emulsified asphalt in the industry standard JTGF40-2019 no longer meets the requirements of water-based epoxy modified emulsified asphalt. In view of this, GB∕T 38990-2020 refers to the technical requirements of JT / T1131 for epoxy asphalt, and proposes to use the tensile fracture strength and elongation at break of the evaporation residue of water-based epoxy emulsified asphalt to evaluate its performance. The preparation method of the test specimen is as follows: the water-based epoxy emulsified asphalt is mixed with the curing agent in proportion and then evenly poured into the template, cured at room temperature for 24 hours, and then placed in a 60℃ oven for further curing for 16 hours, and then taken out and cut out a "dumbbell"-shaped specimen with a cutter for tensile testing. Considering that the residue has a certain thermosetting property, it is very easy to cause cracks (stress damage) on the edge or inside of the specimen during the cutting process, which seriously affects the accuracy of the test results; the casting type sample preparation can better ensure the integrity of the specimen. Since the specimen size must meet (reference) the requirements of the Type I "dumbbell" specimen for the tensile stress-strain performance test specimen of vulcanized rubber or thermoplastic rubber in GBT / 528, that is, "the total length of the specimen is ≥115mm, the length of the narrow part is 33.0mm±2.0mm, the width of the narrow part is 6.0mm (upper tolerance 0.4mm), the standard thickness of the narrow part is 2.0mm±0.2mm (non-standard specimens such as specimens taken from finished products have a maximum thickness of 3mm), and the test length is 25.0mm±0.5mm". Considering the volatilization of water in the process of demulsification and curing of water-based epoxy emulsified asphalt, the evaporation residue will inevitably shrink in volume, and the different contents of the water-based epoxy system will cause differences in the volume shrinkage rate of the residue. Due to the "bite" effect of the ends of the mold cavity (the wide parts at both ends), the transverse volume shrinkage of the sample during the evaporation of water is not obvious, but the longitudinal volume shrinkage is more significant, which is intuitively manifested as a reduction in the thickness of the sample. If the thickness is less than the standard thickness, the "size effect" will cause test errors in the fracture strength.
[0004] Therefore, it is an urgent problem to develop a casting type (non-cutting type) mold that can adjust the mold cavity depth according to the shrinkage rate of the solidified material after demulsification of water-based epoxy emulsified asphalt to ensure that the evaporation residue reaches the standard thickness, and can prepare high-quality tensile fracture strength test specimens of the evaporation residue of water-based epoxy resin modified emulsified asphalt. Summary of the invention
[0005] In view of this, the utility model provides a casting type emulsified asphalt evaporation residue tensile fracture strength test specimen mold with adjustable mold cavity depth and simple structure.
[0006] The emulsified asphalt evaporation residue tensile fracture strength test specimen mold comprises a mold body 1, wherein the mold body 1 has a groove 2 formed along the width direction and three parallel cavities 3. A base core 4 which can move up and down in the vertical direction is inserted into the cavity 3.
[0007] The groove 2 and the main part of the cavity 3 of the mold body 1 are in a "dumbbell" shape, and are laterally provided with an indicating ruler 5 with a scale and a track 6 for the base core 4 to move the control rod up and down. The bottom of the track 6 is provided with a withdrawal channel 7 that can withdraw the base core 4 from the mold body 1.
[0008] The base inner core 4 is composed of a main body 8, a control rod 9 and a limiting module 10. The control rod 9 is provided with a knob 11 at one end, a pointer 12 and a handle module 13 that can assist the up and down movement of the control rod 9 at the other end. The control rod 9 and the limiting module 10 are directly connected with a transmission shaft 14.
[0009] The total length of the groove 2 and the main part of the cavity 3 is 120-125 mm, the width of the end is 12-13 mm, the length of the middle part is 33-35 mm, the width of the middle part is 6.0-6.4 mm, and the transition part is arc-shaped. The depth of the groove 2 is 10-11 mm, the depth of the main part of the cavity 3 is 18-20 mm; the width of the track 6 is 2-3 mm; the width of the extraction channel 7 is 14-15 mm, and the height is 10-12 mm.
[0010] The main body 8 of the base inner core 4 is in a "dumbbell" shape, with a total length of 119-124mm, a thickness of 2-3mm, an end width of 11-12mm, a middle length of 33-35mm, a middle width of 5.8-6.2mm, and an arc-shaped transition portion. The control rod 9, the limiting module 10, and the transmission shaft 14 are all arranged at the bottom of the main body 8. There are twelve limiting modules 10, which are distributed on each side of the main body 8 (including the arc-shaped transition portion). The limiting modules are 1-2mm wide and 2-3mm thick.
[0011] The mold body 1 and the main body of the base inner core 4 are both made of polytetrafluoroethylene.
[0012] The groove 2 is used to examine the shrinkage of the sample evaporation residue before the formal test (the difference in sample thickness before and after evaporation); the cavity 3 cooperates with the base core 4 to cast the test piece for the formal test.
[0013] The base inner core 4 can move up and down to achieve any depth within the range of 2-15mm; the limiting module 10 is connected to the control rod 9 and the knob 11 through the transmission shaft 14. When the depth value is determined, the knob 11 is rotated clockwise to push the limiting module outward through the transmission shaft 14 to fix the base inner core 4 at this height; in addition, the limiting module also plays a role in sealing the gap, so that the cast sample is prevented from flowing down along the gap between the cavity 3 and the main part 8. The base inner core 4 can be pulled out as a whole after the withdrawal channel 7.
[0014] Compared with the prior art, the emulsified asphalt evaporation residue tensile fracture strength test specimen mold described in the utility model has the following characteristics:
[0015] 1). The test specimen mold base can be adjusted to any depth (2-15mm). Considering that the water-based epoxy emulsified asphalt sample will shrink in volume during the process of obtaining the residue through evaporation, it is mainly manifested as longitudinal shrinkage (thickness reduction); and different water-based epoxy system contents will cause differences in the volume shrinkage rate of the residue. Before the formal test, the evaporation residue can be prefabricated in the groove 2, and the thickness difference before and after evaporation can be measured and calculated to convert the shrinkage rate; then the depth (thickness) of the base core 4 can be set so that the thickness of the final evaporation residue reaches the standard thickness, thereby improving the accuracy of the test results;
[0016] 2) After the evaporation residue is prepared, the base inner core 4 can be lowered to the extraction channel 7 and then extracted together with the sample. The demoulding is simple and quick. Compared with the conventional "cutting type", the sample surface is smoother and has no stress damage cracks, making the test results more accurate. The extraction of the inner core 4 also makes it easier to clean the inner wall of the cavity 3. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a top view of the internal structure of the mold for the tensile fracture strength test piece of emulsified asphalt evaporation residue provided by the utility model;
[0018] Figure 2 This is a front view of a test piece mold for the tensile fracture strength test of emulsified asphalt evaporation residue provided by the utility model;
[0019] Figure 3 It is a top view of the inner core structure of the mold base of the emulsified asphalt evaporation residue tensile fracture strength test specimen provided by the utility model.
[0020] The symbols in the accompanying drawings represent:
[0021] 1-mold body; 2-groove; 3-cavity; 4-base core; 5-indicator scale; 6-track; 7-extraction channel; 8-base core main body; 9-control lever; 10-limiting module; 11-knob; 12-pointer; 13-handle module; 14-transmission shaft. DETAILED DESCRIPTION
[0022] The following is a further description of the tensile fracture strength test specimen mold for emulsified asphalt evaporation residue described in the utility model in conjunction with specific embodiments. Example
[0023] The tensile fracture strength test specimen mold of emulsified asphalt evaporation residue includes a mold body 1, and the mold body 1 is provided with a groove 2 along the width direction, and three cavities 3 are provided in parallel. A base core 4 that can move up and down in the vertical direction is inserted into the cavity 3. The groove 2 and the main part of the cavity 3 of the mold body 1 are in the shape of a "dumbbell", and a scale indicator 5 with scales and a track 6 for the base core 4 control rod to move up and down are provided on the side. The bottom of the track 6 has a withdrawal channel 7 that can pull the base core 4 out of the mold body 1. The base core 4 is composed of a main part 8, a control rod 9 and a limiting module 10. The control rod 9 is provided with a knob 11 at one end, and a pointer 12 and a handle module 13 that can assist it to move up and down with external force at the other end. The control rod 9 and the limiting module 10 are directly connected to a transmission shaft 14.
[0024] The total length of the groove 2 and the main part of the cavity 3 is 120 mm, the width of the end is 12 mm, the length of the middle part is 35 mm, the width of the middle part is 6.0 mm, and the transition part is arc-shaped. The depth of the groove 2 is 10 mm, the depth of the main part of the cavity 3 is 20 mm; the width of the track 6 is 3 mm; the width of the extraction channel 7 is 15 mm and the height is 12 mm.
[0025] The main body 8 of the base inner core 4 is in a "dumbbell" shape, with a total length of 120mm, a thickness of 3mm, an end width of 12mm, a middle length of 35mm, a middle width of 6.0mm, and an arc-shaped transition portion. The control rod 9, the limiting module 10, and the transmission shaft 14 are all arranged at the bottom of the main body 8. There are twelve limiting modules 10, which are distributed on each side of the main body 8 (including the arc-shaped transition portion). The limiting module is 2mm wide and 2mm thick.
[0026] The mold body 1 and the main body of the base inner core 4 are both made of polytetrafluoroethylene.
[0027] The groove 2 is used to examine the shrinkage of the sample evaporation residue before the formal test (the difference in sample thickness before and after evaporation); the cavity 3 cooperates with the base core 4 to cast the test piece for the formal test.
[0028] The base inner core 4 can move up and down to achieve any depth within the range of 2-15mm; the limiting module 10 is connected to the control rod 9 and the knob 11 through the transmission shaft 14. When the depth value is determined, the knob 11 is rotated clockwise to push the limiting module outward through the transmission shaft 14 to fix the base inner core 4 at this height; in addition, the limiting module also plays a role in sealing the gap, so that the cast sample is prevented from flowing down along the gap between the cavity 3 and the main part 8. The base inner core 4 can be pulled out as a whole after the withdrawal channel 7.
[0029] The tensile strength test specimen of the evaporation residue of water-based epoxy emulsified asphalt with a water-based epoxy resin system dosage of 10% was prepared. About 50g of water-based epoxy emulsified asphalt sample was prepared in advance and poured into groove 2 with a depth of 10mm, that is, the thickness D1 before evaporation was 10mm. After the mold was placed in a 25℃ environmental box for 24h, it was placed in a 60℃ oven for curing for 16h. After cooling to room temperature, the depth D2 from the surface of the residue to the surface of the mold was measured with a ruler and was 5mm. The actual thickness of the residue was (the difference between D1-D2) 5mm. Considering that there was basically no lateral shrinkage, it was preliminarily determined that the thickness shrinkage rate of the sample was 50%. Then set the depth of the inner core of the base to 4mm, tighten the knob clockwise to make the limiting module "bite" the inner wall of the cavity, and then cast the formal test specimen. The curing process is the same as above. After the residue preparation is completed, the knob is rotated in the opposite direction, the limiting module is withdrawn, the inner core of the base is lowered to the withdrawal channel and then pulled out of the cavity, the evaporation residue specimen is removed, and the thickness is measured with a vernier caliper. The thickness is 1.94mm, which meets the standard thickness range of 2.0mm±0.2mm, and then the tensile fracture strength test can be carried out.
[0030] Compared with the prior art, the utility model has the following characteristics: the depth of the base core can be adjusted according to the shrinkage of different water-based epoxy emulsified asphalt evaporation residues to ensure that the thickness of the sample after evaporation is within the standard thickness range, thereby increasing the test accuracy; the prepared sample can be removed from the mold body together with the base core, the sample has a high surface finish, is free of stress-damaged cracks, and is easy and quick to demold.
Claims
1. A tensile strength test specimen mold for emulsified asphalt evaporation residue, characterized in that: The mold comprises a mold body (1), a groove (2) provided along the width direction, and three cavities (3) provided in parallel, wherein a base inner core (4) which can move up and down in the vertical direction is inserted into the cavity (3); The groove (2) and the main part of the cavity (3) are in the shape of a "dumbbell". The mold body (1) is laterally provided with an indicating scale (5) with a scale and a track (6) for the base inner core control rod (9) to move up and down. The bottom is provided with a withdrawal channel (7) for withdrawing the base inner core from the mold body.
2. The tensile strength test specimen mold for emulsified asphalt evaporation residue according to claim 1, characterized in that: The base inner core (4) is composed of a base inner core main body (8), a control rod (9) and a limiting module (10); a knob (11) is provided at one end of the control rod, and a pointer (12) and a handle module (13) for assisting the upward and downward movement of the control rod by external force are provided at the other end; the control rod and the limiting module are directly connected to a transmission shaft (14).
3. The tensile strength test specimen mold for emulsified asphalt evaporation residue according to claim 1, characterized in that: The total length of the groove (2) and the main part of the cavity (3) is 120-125 mm, the width of the end is 12-13 mm, the length of the middle part is 33-35 mm, the width of the middle part is 6.0-6.4 mm, and the transition part is arc-shaped; the depth of the groove (2) is 10-11 mm, and the depth of the main part of the cavity (3) is 18-20 mm; the width of the track (6) is 2-3 mm; the width of the extraction channel (7) is 14-15 mm, and the height is 10-12 mm.
4. The tensile strength test specimen mold for emulsified asphalt evaporation residue according to claim 2, characterized in that: The base inner core main body (8) is in the shape of a "dumbbell", with a total length of 119-124 mm, a thickness of 2-3 mm, an end width of 11-12 mm, a middle length of 33-35 mm, a middle width of 5.8-6.2 mm, and an arc-shaped transition portion.
5. The tensile strength test specimen mold for emulsified asphalt evaporation residue according to claim 2, characterized in that: The control rod (9), the limiting module (10), and the transmission shaft (14) are all arranged at the bottom of the base inner core main body part (8); there are twelve limiting modules (10) in total, which are distributed on each side of the base inner core main body part (8); the limiting modules are 1-2 mm wide and 2-3 mm thick.