Bending-resistant FPC (Flexible Printed Circuit) multilayer board

By designing a layered structure and hollow area on the FPC multi-layer board, the flexibility of the bending area is increased, and the problem that existing FPC multi-layer boards are prone to break after bending is solved, and the bending resistance and service life are improved.

CN221948426UActive Publication Date: 2024-11-01ZHU HAI HE YI CHUANG CHENG DIAN ZI KE JI YOU XIAN GONG SI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420460010.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-11
Publication Date
2024-11-01
Estimated Expiration
2034-03-11

AI Technical Summary

Technical Problem

Existing FPC multi-layer boards are prone to deformation and fracture after bending or stretching, resulting in reduced durability and service life.

Method used

A multi-layered plate with bending resistance is designed, adopting a layered structure, including a main body area and a bending area, and a hollow area is provided between the first bending substrate layer and the second bending substrate layer of the bending area. , and are equipped with grid-like filling areas to reduce the hardness of the flexible area and increase flexibility.

Benefits of technology

Through layered design and hollowed-out area settings, bending stress is reduced, bending resistance is enhanced and service life is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221948426U_ABST
    Figure CN221948426U_ABST
Patent Text Reader

Abstract

The utility model discloses a bending-resistant FPC (Flexible Printed Circuit) multilayer board, which comprises a first main body area, a second main body area and a bending area, the first main body area comprises a first base material layer, a second base material layer and a first adhesive layer arranged between the first base material layer and the second base material layer; the second main body area comprises a third base material layer, a fourth base material layer and a second adhesive layer arranged between the third base material layer and the fourth base material layer; the bending area comprises a first bending base material layer and a second bending base material layer, a hollow area is arranged between the first bending base material layer and the second bending base material layer, and the first bending base material layer and the second bending base material layer are each provided with a latticed filling area. According to the bending-resistant FPC multilayer board, the hollowed-out areas and the latticed filling areas are arranged, and the bending areas are designed in a layered manner, so that the hardness of the flexible areas is reduced, and the flexibility of the flexible areas is improved; and during bending, the bending stress is released, the bending resistance is enhanced, and the service life is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of flexible circuit boards, in particular to a bending-resistant FPC multilayer board. Background Art

[0002] With the development of thin and lightweight electronic products, FPC (Flexible Printed Circuit) has the characteristics of light weight and dense wiring, and is widely used in mobile phones, computers, new energy batteries and other products. The use of FPC has increased significantly, the installation space is getting smaller and smaller, and the circuits often need to be folded for installation; after the FPC is bent or stretched by external force, the bending area of ​​the FPC board will be deformed and broken. The existing FPC multilayer board has the disadvantage of poor bending performance, and after multiple bending, the service life of the product will be reduced. Utility Model Content

[0003] The utility model aims to solve at least one of the technical problems existing in the prior art. To this end, the utility model proposes a bending-resistant FPC multilayer board, which can enhance the bending-resistant performance and increase the service life.

[0004] An embodiment of the utility model provides a bending-resistant FPC multilayer board, comprising a first main body area, a second main body area and a bending area; the first main body area comprises a first substrate layer, a second substrate layer and a first adhesive layer arranged between the first substrate layer and the second substrate layer; the second main body area comprises a third substrate layer, a fourth substrate layer and a second adhesive layer arranged between the third substrate layer and the fourth substrate layer; the bending area comprises a first bending substrate layer and a second bending substrate layer, a hollow area is arranged between the first bending substrate layer and the second bending substrate layer, the first bending substrate layer and the second bending substrate layer are both provided with a grid-shaped filling area, the first end of the first bending substrate layer is connected to the first substrate layer, the second end of the first bending substrate layer is connected to the third substrate layer, the first end of the second bending substrate layer is connected to the second substrate layer, and the second end of the second bending substrate layer is connected to the fourth substrate layer.

[0005] According to some embodiments of the present invention, the first substrate layer, the second substrate layer, the third substrate layer and the fourth substrate layer all include a main copper layer and a main PI film, and the main copper layer is arranged on or below the main PI film.

[0006] According to some embodiments of the present invention, the first bent substrate layer and the second bent substrate layer both include a bent copper layer and a bent PI film, and the bent copper layer is disposed on or below the bent PI film.

[0007] According to some embodiments of the present invention, the bent copper layer is arranged in a grid shape to form the grid-shaped filling area.

[0008] According to some embodiments of the present invention, the grid line width of the bent ground copper layer is 0.2±0.01 mm, and the grid spacing of the bent ground copper layer is 0.6±0.01 mm.

[0009] According to some embodiments of the present invention, the main copper layer is connected to the bent copper layer, and the main PI film is connected to the bent PI film.

[0010] According to some embodiments of the present invention, a first via hole is provided between the bending area and the first main area, a second via hole is provided between the bending area and the second main area, and both the first via hole and the second via hole are copper-plated.

[0011] According to some embodiments of the present invention, the grid-shaped filling area is a rectangular structure.

[0012] According to some embodiments of the present invention, both the first adhesive layer and the second adhesive layer are thermosetting adhesive layers.

[0013] According to some embodiments of the present invention, both the main PI film and the bent PI film are made of polyimide film.

[0014] The embodiments of the present invention have at least the following beneficial effects:

[0015] The above-mentioned bending-resistant FPC multilayer board includes a first main body area, a second main body area and a bending area. No thermosetting adhesive is filled between the first bending substrate layer and the second bending substrate layer in the bending area, thereby forming a hollow area. The first bending substrate layer and the second bending substrate layer are both provided with a grid-shaped filling area; the bending area adopts a layered design to reduce the hardness of the flexible area, thereby increasing its flexibility; when the FPC multilayer board is bent, the bending stress is released, the bending stress is reduced, the bending resistance is enhanced and the service life is improved.

[0016] Additional aspects and advantages of the present invention will be given in part in the following description, and in part will become apparent from the following description, or will be learned through the practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:

[0018] Figure 1 This is a schematic structural diagram of a bending-resistant FPC multilayer board according to an embodiment of the utility model;

[0019] Figure 2 for Figure 1 The longitudinal cross-sectional structure schematic diagram of the bending-resistant FPC multilayer board is shown;

[0020] Figure 3 for Figure 1 A schematic diagram of the longitudinal cross-sectional structure of the first main body area and the bending area of ​​the bending-resistant FPC multilayer board is shown;

[0021] Figure 4 This is a schematic diagram of the top surface structure of the bending-resistant FPC double-sided board according to an embodiment of the utility model;

[0022] Figure 5 It is a schematic diagram of the back structure of the bending-resistant FPC double-sided board according to an embodiment of the utility model.

[0023] Reference numerals:

[0024] The first main body region 100, the first substrate layer 110, the main copper layer 111, the main PI film 112, the second substrate layer 120, and the first adhesive layer 130;

[0025] The second main body region 200, the third substrate layer 210, the fourth substrate layer 220, and the second adhesive layer 230;

[0026] The bending area 300 , the first bending substrate layer 310 , the bending copper layer 311 , the bending PI film 312 , the second bending substrate layer 320 , the hollow area 330 , the grid-shaped filling area 340 , the first via hole 351 , and the second via hole 352 . DETAILED DESCRIPTION

[0027] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0028] In the description of the present invention, it should be understood that descriptions involving orientation, such as up, down, front, back, left, right, etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0029] In the description of the present utility model, "several" means one or more, "multiple" means more than two, greater than, less than, and exceeding are understood as not including the number itself, and "above", "below", and "within" are understood as including the number itself. If there is a description of "first", "second", etc., it is only used for the purpose of distinguishing technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.

[0030] In the description of the present utility model, unless otherwise clearly defined, words such as “set,” “install,” “connect,” and “connected” should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above words in the present utility model based on the specific content of the technical solution.

[0031] Please refer to Figure 1 and Figure 2 The present embodiment discloses a bending-resistant FPC multilayer board, which includes a first main body area 100, a second main body area 200 and a bending area 300; the first main body area 100 includes a first substrate layer 110, a second substrate layer 120 and a first adhesive layer 130 disposed between the first substrate layer 110 and the second substrate layer 120; the second main body area 200 includes a third substrate layer 210, a fourth substrate layer 220 and a second adhesive layer 230 disposed between the third substrate layer 210 and the fourth substrate layer 220; the bending area 300 includes a first bending substrate layer 110, a second substrate layer 120 and a first adhesive layer 130 disposed between the first substrate layer 110 and the second substrate layer 120; The first bent substrate layer 310 and the second bent substrate layer 320, a hollow area 330 is provided between the first bent substrate layer 310 and the second bent substrate layer 320, the first bent substrate layer 310 and the second bent substrate layer 320 are both provided with a grid-shaped filling area 340, the first end of the first bent substrate layer 310 is connected to the first substrate layer 110, the second end of the first bent substrate layer 310 is connected to the third substrate layer 210, the first end of the second bent substrate layer 320 is connected to the second substrate layer 120, and the second end of the second bent substrate layer 320 is connected to the fourth substrate layer 220. There is no thermosetting adhesive filled between the first bending substrate layer 310 and the second bending substrate layer 320, forming a hollow area 330, and the first bending substrate layer 310 and the second bending substrate layer 320 are both provided with a grid-shaped filling area 340; the bending area 300 uses a layered design to reduce the hardness of the flexible area, thereby increasing its flexibility; when the FPC multilayer board is bent, the bending stress is released, the bending stress is reduced, the bending resistance is enhanced, and the service life is increased.

[0032] Please refer to Figure 2 The first substrate layer 110 , the second substrate layer 120 , the third substrate layer 210 and the fourth substrate layer 220 all include a main copper layer 111 and a main PI film 112 , and the main copper layer 111 is disposed on or below the main PI film 112 .

[0033] Please refer to Figure 3 In some embodiments, the first bending substrate layer 310 and the second bending substrate layer 320 both include a bending ground copper layer 311 and a bending PI film 312, and the bending ground copper layer 311 is arranged on or below the bending PI film 312; the bending ground copper layer 311 is arranged in a grid shape to form a grid-shaped filling area 340; the grid-shaped filling area 340 is a rectangular structure. Exemplarily, the grid line width of the bending ground copper layer 311 is 0.2±0.01mm, and the grid spacing of the bending ground copper layer 311 is 0.6±0.01mm; the main copper layer 111 is connected to the bending ground copper layer 311, and the main PI film 112 is connected to the bending PI film 312. The circuit in the bending area 300 is not plated with copper, which reduces the overall thickness, and the bending ground copper layer 311 is in a grid shape, which enhances the bending resistance and improves the service life.

[0034] Please refer to Figure 3 In some embodiments, a first via 351 is provided between the bending area 300 and the first main area 100, and a second via 352 is provided between the bending area 300 and the second main area 200. The first via 351 and the second via 352 are both copper plated to connect the copper foil layers that need to be connected in the middle layers.

[0035] Please refer to Figure 2 In some embodiments, the first adhesive layer 130 and the second adhesive layer 230 are both thermosetting adhesive layers. The first substrate layer 110 and the second substrate layer 120, and the third substrate layer 210 and the fourth substrate layer 220 are bonded together by thermosetting adhesive. The first bending substrate layer 310 and the second bending substrate layer 320 are not filled with thermosetting adhesive, forming a hollow area 330, which enhances the bending resistance and improves the service life.

[0036] Please refer to Figure 3 In some embodiments, both the main PI film 112 and the bent PI film 312 are made of polyimide film. Polyimide film has excellent high and low temperature resistance, electrical insulation, and adhesion.

[0037] Please refer to Figure 4 and Figure 5 In some embodiments, the FPC multilayer board adopts a double-sided wiring structure, that is, a double-sided substrate is used, and both copper layers on both sides have wiring. There is no thermosetting glue filled between the first bending substrate layer 310 and the second bending substrate layer 320 of the bending area 300, forming a hollow area 330; the first bending substrate layer 310 and the second bending substrate layer 320 are both provided with a grid-shaped filling area 340, and the bending area 300 uses a layered design to reduce the hardness of the flexible area, thereby increasing its flexibility; when the FPC multilayer board is bent, the bending stress is released, the bending stress is reduced, the bending resistance is enhanced, and the service life is improved.

[0038] The embodiments of the present invention are described in detail above in conjunction with the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in the relevant technical field without departing from the purpose of the present invention.

Claims

1. A bending-resistant FPC multilayer board, characterized in that: include: A first main body region (100), the first main body region (100) comprising a first substrate layer (110), a second substrate layer (120), and a first adhesive layer (130) disposed between the first substrate layer (110) and the second substrate layer (120); A second main body region (200), the second main body region (200) comprising a third substrate layer (210), a fourth substrate layer (220), and a second adhesive layer (230) disposed between the third substrate layer (210) and the fourth substrate layer (220); A bending zone (300), the bending zone (300) comprising a first bending substrate layer (310) and a second bending substrate layer (320), a hollow area (330) being provided between the first bending substrate layer (310) and the second bending substrate layer (320), the first bending substrate layer (310) and the second bending substrate layer (320) both being provided with a grid-shaped filling area (340), the first end of the first bending substrate layer (310) being connected to the first substrate layer (110), the second end of the first bending substrate layer (310) being connected to the third substrate layer (210), the first end of the second bending substrate layer (320) being connected to the second substrate layer (120), and the second end of the second bending substrate layer (320) being connected to the fourth substrate layer (220).

2. The bending-resistant FPC multilayer board according to claim 1, characterized in that: The first substrate layer (110), the second substrate layer (120), the third substrate layer (210) and the fourth substrate layer (220) all comprise a main copper layer (111) and a main PI film (112), wherein the main copper layer (111) is arranged on or below the main PI film (112).

3. The bending-resistant FPC multilayer board according to claim 2, characterized in that: The first bent substrate layer (310) and the second bent substrate layer (320) both comprise a bent ground copper layer (311) and a bent PI film (312), wherein the bent ground copper layer (311) is arranged on or below the bent PI film (312).

4. The bending-resistant FPC multilayer board according to claim 3, characterized in that: The bent copper layer (311) is arranged in a grid shape to form the grid-shaped filling area (340).

5. The bending-resistant FPC multilayer board according to claim 4, characterized in that: The grid line width of the bent ground copper layer (311) is 0.2±0.01 mm, and the grid spacing of the bent ground copper layer (311) is 0.6±0.01 mm.

6. The bending-resistant FPC multilayer board according to claim 4, characterized in that: The main copper layer (111) is connected to the bent copper layer (311), and the main PI film (112) is connected to the bent PI film (312).

7. The bending-resistant FPC multilayer board according to claim 1, characterized in that: A first via hole (351) is provided between the bending area (300) and the first main area (100), and a second via hole (352) is provided between the bending area (300) and the second main area (200), and both the first via hole (351) and the second via hole (352) are copper plated.

8. The bending-resistant FPC multilayer board according to claim 1, characterized in that: The grid-shaped filling area (340) is a rectangular structure.

9. The bending-resistant FPC multilayer board according to claim 1, characterized in that: The first adhesive layer (130) and the second adhesive layer (230) are both thermosetting adhesive layers.

10. The bending-resistant FPC multilayer board according to claim 4, characterized in that: The main PI film (112) and the bent PI film (312) are both made of polyimide film.