Tin blocking strip for tin passing of circuit board

By setting a horizontal tube and indicator liquid on the solder resist strip, the problem of non-parallelism during soldering of the circuit board is solved, and the uniformity and effect of soldering of the circuit board are improved.

CN221948482UActive Publication Date: 2024-11-01XIAMEN YUSHENGXIN PRECISION MASCH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420455913.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-11
Publication Date
2024-11-01
Estimated Expiration
2034-03-11

AI Technical Summary

Technical Problem

Existing solder resist strips make it difficult to ensure that the circuit board is parallel to the solder surface during the soldering process, resulting in uneven soldering.

Method used

A solder resist strip for circuit board soldering was designed, comprising a centrally symmetrical positioning groove and a horizontal tube. The horizontal tube contains a horizontal indicator liquid. The horizontal state of the circuit board is determined by judging the alignment of the indicator liquid with the identification line, and the circuit board is positioned in conjunction with a fixture.

Benefits of technology

It improves the uniformity and effectiveness of tinning on circuit boards, avoiding unevenness caused by manual operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221948482U_ABST
    Figure CN221948482U_ABST
Patent Text Reader

Abstract

The utility model discloses a tin blocking bar for tin passing of a circuit board, which belongs to the technical field of tin blocking bars and comprises a tin blocking bar body, two sides of the tin blocking bar body are respectively provided with a first positioning groove and a second positioning groove, the first positioning groove and the second positioning groove are in central symmetry, two sides of the tin blocking bar body are respectively provided with a horizontal pipe, and the horizontal pipes are connected with the first positioning groove and the second positioning groove. A horizontal identification line is arranged on the outer wall of the horizontal pipe, horizontal indicating liquid is arranged in the horizontal pipe, and the liquid level of the horizontal indicating liquid does not exceed the horizontal identification line in a horizontal state. Therefore, the circuit board can be timely adjusted when the circuit board is out of level, and the tinning effect of the circuit board is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of tin-blocking bars, in particular to a tin-blocking bar used for tinning a circuit board. Background Art

[0002] The tin stop bar is an auxiliary fixture used to clamp the PCB when the PCB is tinned to prevent the tin inside the tin furnace from flowing onto the PCB and increase the tinning effect of the PCB.

[0003] The existing tin-blocking bar is provided with two positioning grooves, one for clamping the circuit board and the other for connecting the clamping tool, so as to realize tinning the place where the circuit board needs to be soldered.

[0004] The above technical conditions still have defects: some circuit boards are tinned with manual handheld clamps, and then the circuit boards are placed on the top of the tin furnace for tinning. Since manual operation cannot completely ensure that the circuit board and the tin surface are parallel, it is easy to cause uneven tinning and reduce the effect of tinning.

[0005] Based on this, the utility model designs a tin blocking bar for tinning a circuit board to solve the above problem. Utility Model Content

[0006] The utility model aims to provide a tin-blocking bar for tinning a circuit board to solve the above technical problems.

[0007] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a tin-blocking bar for tinning a circuit board, comprising a tin-blocking bar body, a first positioning groove and a second positioning groove are respectively arranged on both sides of the tin-blocking bar body, the first positioning groove and the second positioning groove are centrally symmetrical, horizontal tubes are arranged on both sides of the tin-blocking bar body, a horizontal identification line is arranged on the outer wall of the horizontal tube, a level indicator liquid is arranged inside the horizontal tube, and the liquid level of the level indicator liquid does not exceed the horizontal identification line in a horizontal state.

[0008] By adopting the above technical solution, it is possible to judge whether the circuit board is level during tinning by whether the liquid surface of the level indicating liquid is flush with the horizontal identification line.

[0009] Preferably, the horizontal tube is made of high temperature resistant transparent glass.

[0010] By adopting the above technical solution, the use effect can be increased and the heat-induced cracking during tinning can be avoided.

[0011] Preferably, the level indicating fluid is a colored liquid epoxy resin.

[0012] By adopting the above technical solution, the observation effect can be increased.

[0013] Preferably, the top and the bottom of the tin-blocking bar body are extended outward to form a supporting portion, and the thickness of the supporting portion is not greater than 1 mm.

[0014] By adopting the above technical solution, the tinning effect of the circuit board is improved.

[0015] Preferably, the thickness of the No. 1 positioning groove and the No. 2 positioning groove is 1.7 mm.

[0016] By adopting the above technical solution, the circuit board can be well positioned.

[0017] In summary, the present application has the following beneficial technical effects: by setting up a level tube and a level indicator liquid, it is possible to determine whether the circuit board is in a horizontal state during tinning, thereby facilitating timely adjustment when it is not level, thereby increasing the tinning effect of the circuit board. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for describing the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0019] Figure 1 Schematic diagram of the overall structure of this embodiment;

[0020] Figure 2 is a schematic diagram of the side structure of this embodiment;

[0021] Figure 3 Schematic diagram of the internal structure of the horizontal tube in this embodiment.

[0022] In the accompanying drawings, the components represented by the reference numerals are listed as follows:

[0023] 1. Tin retaining bar body; 2. Positioning groove No. 1; 3. Positioning groove No. 2; 4. Horizontal tube; 5. Horizontal identification line. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0025] The following is combined with Figure 1-3 This application is described in further detail.

[0026] Reference Figure 1 and Figure 2 A tin-blocking bar for tinning a circuit board comprises a tin-blocking bar body 1, the tin-blocking bar body 1 is made of synthetic stone, a first positioning groove 2 and a second positioning groove 3 are respectively arranged on both sides of the tin-blocking bar body 1, the first positioning groove 2 and the second positioning groove 3 are centrally symmetrical, and horizontal tubes 4 are arranged on both sides of the tin-blocking bar body 1, semicircular grooves are opened on both sides of the tin-blocking bar body 1, and the horizontal tubes 4 are welded to the grooves on the tin-blocking bar body 1, so that half of the horizontal tubes 4 are located on the outside, the horizontal tubes 4 are in the same direction as the tin-blocking bar body 1, a horizontal identification line 5 is arranged on the outer wall of the horizontal tube 4, a horizontal indicator liquid is arranged inside the horizontal tube 4, and the liquid level of the horizontal indicator liquid does not exceed the horizontal identification line 5 in a horizontal state.

[0027] Reference Figure 3 The material of the horizontal tube 4 is high temperature resistant transparent glass, which can increase its high temperature resistance and avoid heat damage during tinning. The level indicator liquid is a colored liquid epoxy resin, which can increase the effect of liquid level observation.

[0028] Reference Figure 2 The top and bottom of the tin-blocking bar body 1 are extended outward to form a supporting portion. The thickness of the supporting portion is no more than 1 mm. The supporting portion is used to support the circuit board and will not affect the tinning of the circuit board. The thickness of the No. 1 positioning groove 2 and the No. 2 positioning groove 3 is 1.7 mm, which can increase the positioning effect of the circuit board.

[0029] The implementation principle of this embodiment is: when in use, the two sides of the circuit board are clamped into the inside of the No. 2 positioning groove 3 on the two sets of tin-blocking bar bodies 1, and then the circuit board is clamped and positioned through the clamping tool and the No. 1 positioning groove 2. Then, when tinning, the circuit board is first moved to the top of the tin furnace. At this time, first determine whether the level indicator liquid inside the horizontal tube 4 is in a horizontal state. After confirming that the circuit board is in a horizontal state, slowly move the circuit board downward. If it is found that it is not level during the movement, it should be adjusted in time, which can effectively increase the uniformity of tinning of the circuit board.

[0030] In the description of the present invention, it should be understood that the terms "coaxial", "bottom", "one end", "top", "middle", "the other end", "upper", "one side", "top", "inside", "front", "center", "both ends" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0031] In the present utility model, unless otherwise clearly stipulated and limited, the terms such as "installation", "setting", "connection", "fixation" and "screw-on" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integrated connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. Unless otherwise clearly defined, ordinary technicians in this field can understand the specific meanings of the above terms in the utility model according to the specific circumstances.

[0032] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A tin-blocking bar for tinning a circuit board, comprising a tin-blocking bar body (1), characterized in that: A first positioning groove (2) and a second positioning groove (3) are respectively arranged on both sides of the tin retaining bar body (1), and the first positioning groove (2) and the second positioning groove (3) are centrally symmetrical. A horizontal tube (4) is arranged on both sides of the tin retaining bar body (1), and a horizontal identification line (5) is arranged on the outer wall of the horizontal tube (4). A level indicator liquid is arranged inside the horizontal tube (4), and the liquid level of the level indicator liquid does not exceed the horizontal identification line (5) in a horizontal state.

2. The tin-blocking strip for tinning a circuit board according to claim 1, characterized in that: The material of the horizontal tube (4) is high temperature resistant transparent glass.

3. The tin-blocking strip for tinning a circuit board according to claim 1, characterized in that: The level indicator fluid is a colored liquid epoxy resin.

4. The tin-blocking strip for tinning a circuit board according to claim 1, characterized in that: The top and bottom of the tin-blocking bar body (1) are both extended outwards to form a support portion, and the thickness of the support portion is no more than 1 mm.

5. The tin-blocking strip for tinning a circuit board according to claim 1, characterized in that: The thickness of the No. 1 positioning groove (2) and the No. 2 positioning groove (3) is 1.7 mm.