Preparation system of polyester film for compounding aluminum foil film
By combining 5-15μm metal aluminum foil with polyester film and reducing the thickness by using rolling and stretching technology, the problem of difficult reduction of metal foil thickness in the prior art is solved, and the thickness uniformity and conductivity of the composite aluminum foil film are achieved. , reducing process complexity and cost.
Patent Information
- Application Number
- CN202323499765.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-20
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2033-12-20
AI Technical Summary
In the existing preparation process of composite aluminum foil film, the thickness of the metal foil is difficult to reduce, resulting in insufficient conductivity and strength, and the process is complex and costly, making it prone to damage and stress curling problems.
5-15μm metal aluminum foil is used to combine with polyester film, and the thickness is reduced to 3-8μm by rolling and stretching technology. In the process, nylon protective film and lubricating oil are used to avoid rupture, combined with high-speed mixing and longitudinal stretching By lateral stretching and other processes, a polyester film with uniform thickness is prepared as the base material layer.
The preparation of thinner metal aluminum foil films is achieved, maintaining conductivity and strength while avoiding damage and stress curling, reducing process complexity and cost.
Smart Images

Figure CN221985890U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a preparation system of a polyester film for composite aluminum foil film. Background Art
[0002] In lithium-ion batteries, aluminum foil is commonly used as the positive electrode current collector, and copper foil is commonly used as the negative electrode current collector. In order to increase the energy density of the battery, composite current collectors composed of plastic film and metal layer have appeared, such as composite aluminum current collectors used as positive electrodes and composite copper current collectors used as negative electrodes. The metal layer in the composite current collector is either bonded to the plastic film using metal foil or formed on the plastic film using evaporation or sputtering processes. Metal foil has excellent conductivity, but is relatively thick; the metal layer formed by sputtering and evaporation is relatively thin and has poor conductivity, requiring repeated coating, with high process requirements, and repeated coating of the plastic film is prone to wrinkles, with a low yield and high cost.
[0003] For example, CN 114695900 B discloses a composite current collector, comprising a first aluminum foil layer, a PET layer, and a second aluminum foil layer stacked in sequence, the first aluminum foil layer and the second aluminum foil layer are both fixedly connected to the PET layer, the upper end surface of the first aluminum foil layer is provided with a plurality of first grooves, and the lower end surface of the second aluminum foil layer is provided with a plurality of second grooves. In order to obtain the grooves, the prior art adopts a thicker aluminum foil structure.
[0004] Then, the aluminum foil and copper foil used as current collectors are mainly used for conductivity and do not participate in active reactions. Therefore, one of the means to increase the energy density of batteries at this stage is to reduce the mass proportion of current collectors: on the one hand, use a composite metal foil film with a lower density, and on the other hand, reduce the thickness of the metal layer. Therefore, using thicker aluminum foil is not advisable at this stage. Summary of the invention
[0005] The technical problem to be solved by the present application is to provide a system for preparing a polyester film for a composite aluminum foil film, so as to reduce or avoid the above-mentioned problems.
[0006] In order to solve the above technical problems, the present application proposes a preparation system of polyester film for composite aluminum foil film, which at least includes a modification treatment equipment for nano-montmorillonite; the outlet of the modification treatment equipment is connected to the inlet of a high-speed mixer for high-speed mixing of polyisobutylene succinimide, tetrabutyl titanate, 1,4-dimethoxybenzene, cyanoacrylate, nano-modified montmorillonite particles and PET slices; the outlet of the high-speed mixer is connected to the inlet of a venting twin-screw extruder; the outlet of the venting twin-screw extruder is connected to the inlet of a thick sheet longitudinal stretching equipment; the outlet of the thick sheet longitudinal stretching equipment is connected to the inlet of a stretching sheet transverse stretching mechanism; the outlet of the stretching sheet transverse stretching mechanism is connected to the inlet of a cooling and shaping equipment; the outlet of the cooling and shaping equipment is connected to a slitting and winding mechanism.
[0007] Preferably, the modification treatment equipment includes: a dispersion tank for dispersing nano-montmorillonite into a polyvinyl alcohol aqueous solution, the outlet of the dispersion tank is connected to the first inlet of a freeze-drying spray device, the freeze-drying spray device is connected to the inlet of a cleaning tank through a pipeline, the outlet of the cleaning tank is connected to the second inlet of the freeze-drying spray device through a pipeline, and the freeze-drying spray device is connected to the high-speed mixer through a modified outlet pipeline.
[0008] The polyester film prepared by the preparation system of the present application can maintain a uniform thickness after various treatments for preparing the composite aluminum foil film, and will not suffer from problems such as breakage and stress curling due to the preparation treatment of the composite aluminum foil film. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] The following drawings are only intended to illustrate and explain the present application, and do not limit the scope of the present application.
[0010] Figure 1 Shown is a cross-sectional view of a composite aluminum foil film according to a specific embodiment of the present application.
[0011] Figure 2 Shown is a schematic structural diagram of a system for preparing a polyester film for a composite aluminum foil film according to a specific embodiment of the present application. DETAILED DESCRIPTION
[0012] In order to have a clearer understanding of the technical features, purposes and effects of the present application, the specific implementation of the present application is now described with reference to the accompanying drawings, wherein the same components are numbered the same.
[0013] Existing lithium batteries generally use aluminum foil obtained by rolling aluminum as the positive electrode current collector. Due to the strength limitation of the material itself, it is difficult to reduce the thickness of the aluminum foil, otherwise it is easy to tear during operation. Even if the aluminum foil is composited with a plastic film, it is impossible to use a too thin aluminum foil for composite operation.
[0014] In view of this, the present application proposes a composite aluminum foil film, such as Figure 1 As shown, the composite aluminum foil film is composed of a substrate layer 1 and a metal aluminum foil 2 adhered to both sides of the substrate layer 1. The substrate layer 1 can be made of a plastic film of a material such as polyolefin or polyester. In a preferred embodiment, the substrate layer 1 is preferably made of a polyester film. The metal aluminum foil 2 can be bonded to both sides of the substrate layer 1 by an adhesive.
[0015] Furthermore, the metal aluminum foil 2 in the composite aluminum foil film of the present application can be composed of a metal aluminum foil of a first thickness of 5-15 μm, which is rolled and stretched on both sides of the substrate layer 1 to a metal aluminum foil of a second thickness of 3-8 μm. That is, the metal aluminum foil 2 of the present application initially has a first thickness, and becomes the final second thickness after being attached to both sides of the substrate layer 1 and rolled and stretched. Since the material strength of metal aluminum is not very good, it is expensive and difficult to perform bonding and other composite operations directly using a metal aluminum foil of a second thickness of 3-8 μm. Therefore, the present application uses a metal aluminum foil of a first thickness of 5-15 μm as the initial raw material, and after bonding and compounding it with the substrate layer 1, it is rolled and stretched to become the second thickness, and then no further composite operation is required, so that a thinner metal aluminum foil can be obtained while ensuring conductivity and strength.
[0016] For example, the metal aluminum foil 2 used is formed by rolling metal aluminum with an aluminum content exceeding 98%, and an existing metal aluminum foil finished product with a thickness of 5-15 μm sold on the market can be selected as the initial raw material of the first thickness.
[0017] Furthermore, as shown in the figure, a layer of rolling protection film 3 is attached to the outer side of the metal aluminum foil 2 to protect the surface of the metal aluminum foil 2 from scratches and tearing during the rolling and stretching process. The rolling protection film 3 can also be made of plastic films made of polyolefin, polyester, nylon and other materials. In a preferred embodiment, the rolling protection film 3 is preferably made of a nylon film with excellent strength and self-lubricating properties, preferably a nylon film with a thickness of 8-10 μm.
[0018] When preparing the composite aluminum foil film of the present application, adhesive can be first applied to both sides of the substrate layer 1 with an initial thickness of 10-20 μm, and then the metal aluminum foil 2 of the first thickness can be bonded to the surface of the substrate layer 1. After that, a lubricant such as machine oil or silicone grease can be applied to the outside of the metal aluminum foil 2, and then a rolling protective film 3 made of nylon with a thickness of 8-10 μm can be attached to the surface of the oiled metal aluminum foil 2. By applying the machine lubricant, the adhesion of the rolling protective film 3 to the metal aluminum foil 2 can be increased, and the friction can be reduced in the subsequent rolling and stretching process to avoid the rupture of the film layer.
[0019] Then, the film layer with the rolling protective film 3 attached is placed between at least one pair of rolling rollers, and the metal aluminum foil 2 is rolled from the first thickness to the second thickness of 3-8 μm by the pressure of the rolling rollers. It is easy to destroy the film structure by thinning the film layer by pure hard extrusion. Therefore, the rolling protective film 3 in contact with the rolling roller is made of nylon to improve the sliding property and avoid extrusion. At the same time, the friction between the film layer and the rolling roller during rolling can be further reduced by auxiliary coating of lubricating oil. After rolling and stretching, the thickness of the substrate layer 1 changes from 10-20 μm to about 6-12 μm.
[0020] In addition, the film layer can be heated before being rolled by the rolling roller to increase the ductility of the plastic film and improve the efficiency of rolling thinning. At the same time, the rebound amount of the heated plastic film will be reduced, which is conducive to maintaining the thickness of the film layer after stretching. In a preferred embodiment, the film layer can be heated by infrared heating, and the heating temperature of the film layer is preferably 150-170°C.
[0021] In addition, the two sides of the film layer can be stretched outward while the film layer is being rolled by the rolling roller. That is, the film layer is longitudinally stretched by the rolling roller, and at the same time, the two sides are clamped by the clamping device in the width direction for transverse stretching to speed up the thinning speed of the material. Because the stretching of the metal aluminum foil is involved, the entire film layer needs to be clamped during clamping and stretching, and the speed of transverse stretching needs to be controlled to avoid the problem of inconsistent stretching ratios between the film layers.
[0022] In addition, after the film layer is rolled and stretched, in order to avoid the film layer rebounding due to stress, the film layer can be further heated and annealed to eliminate the stress in the film layer. The preferred annealing temperature is 130-150° C. and the annealing time is 5-15 minutes.
[0023] Finally, the rolling protective film 3 of the film layer after annealing is removed, and the lubricating oil on the outer surface of the metal aluminum foil 2 is removed with a cleaning agent, and then rinsed with clean water, dried, trimmed, and rolled up to obtain the composite aluminum foil film of the present application.
[0024] Through the description of the structure and preparation process of the composite aluminum foil film of the present application, the present application further proposes a polyester film suitable for the composite aluminum foil film of the present application, and the polyester film is used as the substrate layer 1 of the composite aluminum foil film. In addition to having excellent mechanical properties, the substrate layer 1 prepared by the polyester film of the present application can also withstand the heating, rolling, stretching and annealing treatment of the composite aluminum foil film of the present application, and maintain a uniform thickness after the treatment, and will not be damaged or stress curled due to the preparation treatment of the composite aluminum foil film.
[0025] Specifically, the present application proposes a polyester film for composite aluminum foil film, which is used as the substrate layer 1 of the composite aluminum foil film, and the two sides of the substrate layer of the composite aluminum foil film are bonded with metal aluminum foil 2, and the metal aluminum foil 2 can be composed of a metal aluminum foil of a first thickness of 5-15 μm rolled and stretched on both sides of the substrate layer to a metal aluminum foil of a second thickness of 3-8 μm. Wherein, the polyester film is prepared from the following components in parts by weight: 10-20 parts by weight of polyisobutylene succinimide, 1-3 parts by weight of tetrabutyl titanate, 3-5 parts by weight of 1,4-dimethoxybenzene, 5-10 parts by weight of cyanoacrylate, 2-4 parts by weight of nano-modified montmorillonite particles, and 1000-2000 parts by weight of PET chips. In a specific embodiment of the present application, 10-20 parts by weight of polyisobutylene succinimide, 1-3 parts by weight of tetrabutyl titanate, 3-5 parts by weight of 1,4-dimethoxybenzene, 5-10 parts by weight of cyanoacrylate, 2-4 parts by weight of nano-modified montmorillonite particles and 1000-2000 parts by weight of PET slices can be added to a high-speed mixer for pre-dispersion mixing at room temperature, with a rotation speed of 1500-2000 rpm and mixed for 30-60 minutes to form a mixture. The mixture then enters a venting twin-screw extruder, and the temperature of the twin-screw extruder is adjusted to 270°C-280°C. After the material is melted in the extruder, it is filtered and extruded into a thick sheet. The thickness and profile of the thick sheet can be adjusted by the extruder extrusion amount, the casting roller speed, and the die opening. The thick sheet is preheated at a temperature of 50°C to 90°C, placed in an infrared heating zone of 300°C to 500°C, and longitudinally stretched at a line speed of 40 to 150 m / min, with a longitudinal stretching ratio of 4.0 to obtain a stretched sheet. The stretched sheet is preheated at a temperature of 90°C to 120°C, and transversely stretched at a temperature of 100°C to 160°C, with a transverse stretching ratio of 3.8. After that, it is shaped at a temperature of 160°C to 240°C, and then cooled at a temperature of 100°C to 50°C to obtain the polyester film of the present application. The obtained polyester film can be slit and rolled for use. Among them, in order to facilitate the uniform dispersion of nano-montmorillonite in the organic components of the polyester film, the nano-montmorillonite needs to be surface modified. The specific steps are: adding 10-20 parts by weight of nano-montmorillonite to 100-200 parts by weight of polyvinyl alcohol aqueous solution, stirring continuously for 60-120 minutes to fully disperse; then freeze-drying and spraying the dispersed mixture to obtain a surface-modified solid particle mixture; adding the obtained solid particle mixture to clean water for multiple washing and filtration to obtain a dispersion liquid with a solid content of 20-40wt% without soluble matter, freeze-drying and spraying the dispersion liquid again, and screening to obtain particles with a particle size of 10-20nm, which are the nano-modified montmorillonite particles. Wherein, the content of polyvinyl alcohol in the polyvinyl alcohol aqueous solution is 10wt%-15wt%.
[0026] Correspondingly, the present application also proposes a system for preparing a polyester film for composite aluminum foil film, such as Figure 2 As shown. Figure 2 In the specific embodiment shown, the preparation system of the present application at least includes a modification treatment device 300 for nano-montmorillonite. The outlet of the modification treatment device 300 is connected to the inlet of a high-speed mixer 101 for high-speed mixing of polyisobutylene succinimide, tetrabutyl titanate, 1,4-dimethoxybenzene, cyanoacrylate, nano-modified montmorillonite particles and PET chips.
[0027] The outlet of the high-speed mixer 101 is connected to the inlet of the venting twin-screw extruder 102; the outlet of the venting twin-screw extruder 102 is connected to the inlet of the thick film longitudinal stretching equipment 103; the outlet of the thick film longitudinal stretching equipment 103 is connected to the inlet of the stretching film transverse stretching mechanism 104; the outlet of the stretching film transverse stretching mechanism 104 is connected to the inlet of the cooling and shaping equipment 105; the outlet of the cooling and shaping equipment 105 is connected to the slitting and winding mechanism 106.
[0028] In another specific embodiment of the present application, Figure 2 As shown, the modification treatment equipment 300 includes: a dispersion tank 301 for dispersing nano-montmorillonite into a polyvinyl alcohol aqueous solution, the outlet of the dispersion tank 301 is connected to the first inlet 3021 of the freeze-drying spray equipment 302, the freeze-drying spray equipment 302 is connected to the inlet of the cleaning tank 303 through a pipeline, the outlet of the cleaning tank 303 is connected to the second inlet 3022 of the freeze-drying spray equipment 302 through a pipeline, and the freeze-drying spray equipment 302 is connected to the high-speed mixer 101 through the modification outlet pipeline 304.
[0029] Examples 1-5
[0030] According to the weight proportions of the raw materials in the following table, polyester films for the substrate layer of the composite aluminum foil film were prepared respectively.
[0031] Example 1 Example 2 Example 3 Example 4 Example 5 Polyisobutylene succinimide 10 12 15 18 20 Tetrabutyl titanate 1.0 1.5 2.0 2.5 3.0 1,4-Dimethoxybenzene 3.0 3.5 4.0 4.5 5.0 Cyanoacrylate 5.0 6.0 7.5 9.0 10.0 Nano-modified montmorillonite particles 2.0 2.5 3.0 3.5 4.0 PET 1000 1200 1500 1800 2000 Polyester film thickness μm 10 12 15 18 20
[0032] Comparative Examples 6-10
[0033] In the same manner as in the above example, a polyester film for comparison was prepared according to the weight proportions of the raw materials shown in the following table.
[0034] Comparative Example 6 Comparative Example 7 Comparative Example 8 Comparative Example 9 Comparative Example 10 Polyisobutylene succinimide 0 12 15 20 22 Tetrabutyl titanate 3.0 0 3.5 4.5 4.0 1,4-Dimethoxybenzene 5.0 4.0 0 6.5 6.0 Cyanoacrylate 10.0 6.0 9.0 0 10.0 Nano-modified montmorillonite particles 4.0 3.5 5.0 4.5 0 PET 1000 1200 1500 1800 2000 Polyester film thickness μm 10 12 15 18 20
[0035] The performance parameters of each polyester film were tested and prepared respectively, and a 15μm thick film prepared from pure PET without adding any ingredients was compared. Examples 1-5, comparative examples 6-10, and the pure PET film for comparison were used as the substrate layer of the present application, and were subjected to treatments such as bonding metal aluminum foil, rolling and stretching, and the performance of the composite aluminum foil film finally obtained was checked. The test shows that the polyester film of Examples 1-5 can maintain a uniform thickness after various treatments for preparing the composite aluminum foil film, and no defects such as breakage and stress curling due to the preparation treatment of the composite aluminum foil film were found. However, comparative examples 6-10 and the pure PET film failed to withstand the preparation treatment process, and different degrees of breakage and curling were found. In summary, the polyester film prepared by the preparation system of the present application can still maintain a uniform thickness after various treatments for preparing the composite aluminum foil film, and will not suffer from problems such as breakage and stress curling due to the preparation treatment of the composite aluminum foil film.
[0036] Those skilled in the art should understand that although the present application is described in the form of multiple embodiments, not every embodiment contains only one independent technical solution. Such description in the specification is only for the sake of clarity, and those skilled in the art should understand the specification as a whole and regard the technical solutions involved in each embodiment as being able to be combined into different embodiments to understand the scope of protection of the present application.
[0037] The above description is only an illustrative embodiment of the present application and is not intended to limit the scope of the present application. Any equivalent changes, modifications and combinations made by any technician in the field without departing from the concept and principle of the present application shall fall within the scope of protection of the present application.
Claims
1. A system for preparing a polyester film for composite aluminum foil film, characterized in that: The preparation system at least comprises a modification treatment device (300) for nano-montmorillonite; the outlet of the modification treatment device (300) is connected to the inlet of a high-speed mixer (101) for high-speed mixing of polyisobutylene succinimide, tetrabutyl titanate, 1,4-dimethoxybenzene, cyanoacrylate, nano-modified montmorillonite particles and PET slices; the outlet of the high-speed mixer (101) is connected to the inlet of a venting twin-screw extruder (102); the outlet of the venting twin-screw extruder (102) is connected to the inlet of a thick sheet longitudinal stretching device (103); the outlet of the thick sheet longitudinal stretching device (103) is connected to the inlet of a stretching sheet transverse stretching mechanism (104); the outlet of the stretching sheet transverse stretching mechanism (104) is connected to the inlet of a cooling and shaping device (105); the outlet of the cooling and shaping device (105) is connected to a slitting and winding mechanism (106).
2. The preparation system according to claim 1, characterized in that: The modification treatment equipment (300) comprises: a dispersion tank (301) for dispersing nano-montmorillonite into a polyvinyl alcohol aqueous solution, the outlet of the dispersion tank (301) is connected to a first inlet (3021) of a freeze-drying spray device (302), the freeze-drying spray device (302) is connected to an inlet of a cleaning tank (303) via a pipeline, the outlet of the cleaning tank (303) is connected to a second inlet (3022) of the freeze-drying spray device (302) via a pipeline, and the freeze-drying spray device (302) is connected to the high-speed mixer (101) via a modification outlet pipeline (304).