Bearing structure
By depositing specific layers on the semiconductor substrate and separating the release layer with infrared light, the complexity of wafer bonding process and high-density wiring problems in three-dimensional integration of semiconductor devices are solved, and the removal and reuse of semiconductor substrates are realized, simplifying the process flow and reducing the The cost.
Patent Information
- Application Number
- CN202420239351.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Priority Date
- 2023-02-22
- Filing Date
- 2024-01-31
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2034-01-31
AI Technical Summary
In the three-dimensional integration process of semiconductor devices, the wafer bonding process is complex and needs improvement, especially the problem of high-density wiring is difficult to effectively solve.
A method of forming a load-bearing structure includes depositing a dielectric layer, a release layer (formed by physical vapor deposition of TiN material), a reflective layer and a bonding layer on a semiconductor substrate, and separating the release layer from the dielectric layer by infrared light exposure. This enables the removal and reuse of semiconductor substrates.
This method simplifies the backside process, improves the efficiency of high-density signal wiring, avoids semiconductor substrate damage, reduces costs, and enables easier etching processes to expose the interconnect structure.
Smart Images

Figure CN222015403U_ABST
Abstract
Description
Technical Field
[0001] An embodiment of the utility model relates to a bearing structure, and in particular to a bearing structure of a semiconductor device. Background Art
[0002] The semiconductor industry continues to improve the processing power and power consumption of integrated circuits (ICs) by reducing the minimum feature size. However, in recent years, process limitations have made it difficult to continue to reduce the minimum feature size. Stacking two-dimensional (2D) integrated circuits into three-dimensional (3D) integrated circuits has become a potential way to continue to improve the processing power and power consumption of integrated circuits. For example, in wafer-to-wafer multilayer stacking applications, the wafers bonding process and the backside process can improve high-density wiring problems. This bonding process uses complex technology and needs to be improved. Utility Model Content
[0003] The purpose of the present disclosure is to provide a bearing structure to solve at least one of the above problems.
[0004] In order to solve the aforementioned problems, an embodiment of the present disclosure provides a method for forming a supporting structure, comprising: forming one or more devices on a substrate; forming a first interconnect structure on the one or more devices; bonding the first interconnect structure to a supporting structure, the supporting structure comprising a semiconductor substrate, a release layer and a first dielectric layer, and the release layer comprising a metal nitride; flipping one or more devices so that the supporting structure is located at a bottom; performing multiple back-side processes; flipping one or more devices so that the supporting structure is located at a top; and exposing the supporting structure to infrared light, so that part of the release layer is separated from the first dielectric layer.
[0005] The disclosed embodiment also provides a method for forming a carrier structure, comprising: forming a carrier structure, comprising: depositing a first dielectric layer on a semiconductor substrate; depositing a release layer on the first dielectric layer by a physical vapor deposition process, the release layer comprising TiN; depositing a second dielectric layer on the release layer; depositing a reflective layer on the second dielectric layer; and depositing a bonding layer on the reflective layer; bonding the carrier structure to a semiconductor device structure; flipping the semiconductor device structure; performing one or more processes on the semiconductor device structure; and removing the carrier structure.
[0006] The present disclosure also provides a supporting structure, including a semiconductor substrate, a first dielectric layer, a release layer, a second dielectric layer, a reflective layer and a bonding layer. The first dielectric layer is disposed on the semiconductor substrate. The release layer is disposed on the first dielectric layer. The release layer is carbon-free and includes a metal nitride. The second dielectric layer is disposed on the release layer. The reflective layer is disposed on the second dielectric layer. The bonding layer is disposed on the reflective layer.
[0007] According to one embodiment of the present disclosure, the release layer is a TiN layer.
[0008] According to one embodiment of the present disclosure, the TiN layer is formed by physical vapor deposition.
[0009] According to one embodiment of the present disclosure, the TiN layer includes a columnar structure.
[0010] According to one embodiment of the present disclosure, a top surface of the release layer is rough.
[0011] According to one embodiment of the present disclosure, the top surface of the release layer has a surface roughness ranging from 0.2 nanometers to 5 nanometers.
[0012] According to one embodiment of the present disclosure, the release layer expands by absorbing heat from infrared light.
[0013] According to one embodiment of the present disclosure, the infrared light is generated by an infrared laser.
[0014] According to one embodiment of the present disclosure, the infrared light is a picosecond infrared laser.
[0015] According to one embodiment of the present disclosure, a pulse duration of the infrared light is in a range of 10 picoseconds to 100 picoseconds. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Aspects of the present disclosure can be best understood from the following detailed description when read in conjunction with the accompanying drawings. It is noteworthy that, in accordance with standard practice in the industry, the various features are not drawn to scale. In fact, the sizes of various features may be arbitrarily increased or decreased for clarity of discussion.
[0017] Figure 1A is a perspective view of one of the various stages in fabricating a semiconductor device structure according to some embodiments.
[0018] Figure 1B According to some embodiments, Figure 1A A cross-sectional side view of a semiconductor device structure at a manufacturing stage taken along line AA.
[0019] Figure 2is a cross-sectional side view of a stage in the fabrication of a semiconductor device structure according to some embodiments.
[0020] 3A to Fig. 3I are cross-sectional side views of various stages in the fabrication of a semiconductor device structure in accordance with some embodiments.
[0021] Figure 4 is a cross-sectional side view of a load-bearing structure according to some embodiments.
[0022] FIG. 5A to FIG. 5C is a cross-sectional side view of a load-bearing structure being heated by a laser, according to some embodiments.
[0023] The reference numerals are as follows:
[0024] 100:Semiconductor device structure
[0025] 102:Substrate
[0026] 108: Channel area
[0027] 114: Quarantine
[0028] 122: Gate spacer
[0029] 123: Fin-type sidewall spacer
[0030] 124: Source / drain region
[0031] 126: Contact Etch Stop Layer
[0032] 128: Interlayer dielectric layer
[0033] 136: Gate dielectric layer
[0034] 138: Gate electrode layer
[0035] 140: Gate stack
[0036] 200: Installation
[0037] 300: Interconnection structure
[0038] 302: Intermetallic dielectric layer
[0039] 304: Conductive characteristics
[0040] 306: Conductive characteristics
[0041] 310: Dielectric layer
[0042] 312: Bearing structure
[0043] 314:Semiconductor substrate
[0044] 316: Release layer
[0045] 318: Bonding layer
[0046] 320: Bearing structure
[0047] 322: Dielectric layer
[0048] 324: Conductive pad
[0049] 326: Etching stop layer
[0050] 328: Conductive bump
[0051] 400: Backside interconnection structure
[0052] 402: Dielectric layer
[0053] 404: Dielectric layer
[0054] 406: Reflection layer
[0055] 410: Top surface
[0056] 502: Light
[0057] 504: Light
[0058] 506: Light DETAILED DESCRIPTION
[0059] The following disclosure provides many different embodiments or examples for realizing different features of the provided subject matter. Specific examples of components and arrangements are described below to simplify the present disclosure. Of course, these are merely examples and are not restrictive. For example, forming a first feature on or on a second feature in the following description may include an embodiment in which the first feature and the second feature are formed to be in direct contact, and may also include an embodiment in which additional features may be formed between the first feature and the second feature, so that the first feature and the second feature may not be in direct contact. In addition, the present disclosure may repeat reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself dictate the relationship between the various embodiments and / or configurations discussed.
[0060] Additionally, spatially relative terms, such as "below," "lower," "above," "over," "up," "top," "upper," and the like, may be used herein to facilitate understanding of describing the relationship of one element or feature to another element or feature as illustrated in the figures. Spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein interpreted accordingly.
[0061] Figure 1A and Figure 1B1 shows the stages of manufacturing a semiconductor device structure 100. Figure 1A and Figure 1B As shown, the semiconductor device structure 100 includes a substrate 102 and one or more devices 200 formed on the substrate 102. The substrate 102 may be a semiconductor substrate. In some embodiments, the substrate 102 includes a single crystalline semiconductor layer at least on a surface of the substrate 102. The substrate 102 may include a crystalline semiconductor material, such as, but not limited to, silicon (Si), germanium (Ge), silicon germanium (SiGe), gallium arsenide (GaAs), indium antimonide (InSb), gallium phosphide (GaP), gallium antimonide (GaSb), indium aluminum arsenide (InAlAs), indium gallium arsenide (InGaAs), gallium antimony phosphide (GaSbP), gallium arsenic antimonide (GaAsSb), and indium phosphide (InP). For example, the substrate 102 is made of silicon. In some embodiments, the substrate 102 is a silicon-on-insulator (SOI) substrate, which includes an insulating layer (not shown) disposed between two silicon layers. In one aspect, the insulating layer is an oxygen-containing material, such as an oxide.
[0062] The substrate 102 may include one or more buffer layers (not shown) on the surface of the substrate 102. The buffer layer may be used to gradually change the lattice constant from that of the substrate to that of the source / drain. The buffer layer may be formed of an epitaxially grown crystalline semiconductor material, such as, but not limited to, Si, Ge, germanium tin (GeSn), SiGe, GaAs, InSb, GaP, GaSb, InAlAs, InGaAs, GaSbP, GaAsSb, gallium nitride (GaN), and zinc phosphide.
[0063] The substrate 102 may include various regions that have been appropriately doped with impurities (eg, p-type or n-type impurities), such as phosphorus for n-type fin field effect transistors (FinFETs) and boron for p-type FinFETs.
[0064] As described above, device 200 can be any suitable device, such as a transistor, a diode, an image sensor, a resistor, a capacitor, an inductor, a storage unit, or a combination thereof. In some embodiments, device 200 is a transistor, such as a planar field effect transistor (FET), a fin field effect transistor, a nanostructure transistor, or other suitable transistor. Nanostructure transistors may include nanosheet transistors, nanowire transistors, gate-all-around (GAA) transistors, multi-bridge channel (MBC) transistors, or any transistor having a gate electrode surrounding a channel. An example of device 200 formed on substrate 102 is a fin field effect transistor, which is Figure 1A and Figure 1B The device 200 includes a source / drain (S / D) region 124 and a gate stack 140 ( Figure 1A Each gate stack 140 may be disposed between a source / drain region 124 used as a source region and a source / drain region 124 used as a drain. For example, each gate stack 140 may extend along the Y axis between one or more source / drain regions 124 used as a source region and one or more source / drain regions 124 used as a drain. Figure 1B As shown, two gate stacks 140 are formed on the substrate 102. In some embodiments, more than two gate stacks 140 are formed on the substrate 102. The channel region 108 is formed between the source / drain region 124 serving as a source region and the source / drain region 124 serving as a drain region.
[0065] The source / drain region 124 may include a semiconductor material such as Si or Ge, a III-V compound semiconductor, a II-VI compound semiconductor, or other suitable semiconductor material. Exemplary source / drain regions 124 may include, but are not limited to, Ge, SiGe, GaAs, AlGaAs, GaAsP, SiP, InAs, AlAs, InP, GaN, InGaAs, InAlAs, GaSb, AlP, GaP, etc. The source / drain region 124 may include a p-type dopant, such as boron; an n-type dopant, such as phosphorus or arsenic; and / or other suitable dopants including combinations thereof. The source / drain region 124 may be formed by an epitaxial growth method using chemical vapor deposition (CVD), atomic layer deposition (ALD), or molecular beam epitaxy (MBE). In the present disclosure, source and drain are used interchangeably, and their structures are substantially the same. In addition, depending on the context, the source / drain region may refer to the source or drain individually or collectively.
[0066] The channel region 108 may include one or more semiconductor materials, such as Si, Ge, GeSn, SiGe, GaAs, InSb, GaP, GaSb, InAlAs, InGaAs, GaSbP, GaAsSb, GaN, or InP. In some embodiments, the channel region 108 includes the same semiconductor material as the substrate 102. In some embodiments, the device 200 is a fin field effect transistor, and the channel region 108 is a plurality of fins disposed below the gate stack 140. In some embodiments, the device 200 is a nanostructure transistor, and the channel region 108 is surrounded by the gate stack 140.
[0067] like Figure 1A and Figure 1B As shown, each gate stack 140 includes a gate electrode layer 138 disposed above the channel region 108 (or around the channel region 108 of the nanostructure transistor). The gate electrode layer 138 can be a metal-containing material, such as tungsten, cobalt, aluminum, ruthenium, copper, multiple layers thereof, etc., and can be deposited by atomic layer deposition, plasma enhanced chemical vapor deposition (PECVD), molecular beam deposition (MBD), physical vapor deposition (PVD), or any suitable deposition technology. Each gate stack 140 can also include a gate dielectric layer 136 disposed above the channel region 108. The gate electrode layer 138 can be disposed on the gate dielectric layer 136. In some embodiments, an interfacial layer (not shown) can be disposed between the channel region 108 and the gate dielectric layer 136, and one or more work function layers (not shown) can be formed between the gate dielectric layer 136 and the gate electrode layer 138. The interfacial dielectric layer may include a dielectric material, such as an oxygen-containing material or a nitrogen-containing material, or a multilayer thereof, and may be formed by any suitable deposition method, such as chemical vapor deposition, plasma enhanced chemical vapor deposition, or atomic layer deposition. The gate dielectric layer 136 may include a dielectric material such as an oxygen-containing material or a nitrogen-containing material, a high-k dielectric material having a dielectric value greater than that of silicon dioxide, or a multilayer thereof. The gate dielectric layer 136 may be formed by any suitable method, such as chemical vapor deposition, plasma enhanced chemical vapor deposition, or atomic layer deposition. In some embodiments, the gate dielectric layer 136 may be a conformal layer. The term "conformal" may be used herein to facilitate description of a layer having substantially the same thickness in various regions. One or more work function layers may include aluminum titanium carbide, aluminum titanium oxide, aluminum titanium nitride, and the like.
[0068] The sidewalls of the gate stack 140 (e.g., the sidewalls of the gate dielectric layer 136) form the gate spacers 122. The gate spacers 122 may include silicon oxycarbide, silicon nitride, silicon oxynitride, silicon carbonitride, etc., multiple layers thereof, or combinations thereof, and may be deposited by chemical vapor deposition, atomic layer deposition, or other suitable deposition techniques.
[0069] like Figure 1A As shown, the fin sidewall spacer 123 can be disposed on opposite sides of each source / drain region 124, and the fin sidewall spacer 123 can include the same material as the gate spacer 122. Portions of the gate stack 140, the gate spacer 122, and the fin sidewall spacer 123 can be disposed on the isolation region 114. The isolation region 114 is disposed on the substrate 102. The isolation region 114 may include an insulating material such as an oxygen-containing material, a nitrogen-containing material, or a combination thereof. In some embodiments, the isolation region 114 is a shallow trench isolation (STI). The insulating material can be formed by high-density plasma chemical vapor deposition (HDP-CVD), flowable chemical vapor deposition (FCVD), or other suitable deposition processes. On the one hand, the isolation region 114 includes silicon oxide formed by a flowable chemical vapor deposition process.
[0070] like Figure 1A and Figure 1BAs shown, a contact etch stop layer (CESL) 126 is formed on the source / drain regions 124 and the isolation regions 114, and an interlayer dielectric (ILD) layer 128 is formed on the contact etch stop layer 126. The contact etch stop layer 126 can provide a mechanism to stop the etching process when an opening is formed in the interlayer dielectric layer 128. The contact etch stop layer 126 can be conformally deposited on the surfaces of the source / drain regions 124 and the isolation regions 114. The contact etch stop layer 126 can include an oxygen-containing material or a nitrogen-containing material, such as silicon nitride, silicon carbonitride, silicon oxynitride, carbon nitride, silicon oxide, silicon oxycarbide, etc., or a combination thereof, and can be deposited by chemical vapor deposition, plasma enhanced chemical vapor deposition, atomic layer deposition, or any suitable deposition technique. The interlayer dielectric layer 128 may include an oxide formed of tetraethylorthosilicate (TEOS), undoped silicate glass, or doped silicon oxide, such as borophosphosilicate glass (BPSG), fused silica glass (FSG), phosphosilicate glass (PSG), boron doped silicon glass (BSG), organosilicate glass (OSG), SiOC and / or any suitable low-k dielectric material (e.g., a material having a lower dielectric constant than silicon dioxide), and may be deposited by spin coating, chemical vapor deposition, flowable chemical vapor deposition, plasma enhanced chemical vapor deposition, physical vapor deposition, or any suitable deposition technique.
[0071] Conductive contacts (not shown) may be disposed in the interlayer dielectric layer 128 and on the source / drain regions 124. The conductive contacts may be conductive and include a material having one or more of Ru, Mo, Co, Ni. W, Ti, Ta, Cu, Al, TiN or TaN, and the conductive contacts may be formed by any suitable method, such as electrochemical plating (ECP) or physical vapor deposition. A silicide layer (not shown) may be disposed between the conductive contacts and the source / drain regions 124.
[0072] like Figure 2As shown, the semiconductor device structure 100 may also include an interconnect structure 300 disposed above the device 200 and the substrate 102. The interconnect structure 300 includes various conductive features, such as a plurality of first conductive features 304 and a plurality of second conductive features 306, and an intermetal dielectric (IMD) layer 302 to separate and isolate the various conductive features 304, 306. In some embodiments, the plurality of first conductive features 304 are wires and the plurality of second conductive features 306 are conductive vias. The interconnect structure 300 includes multiple layers of conductive features 304, and the conductive features 304 are arranged in each layer to provide electrical paths to various devices 200 disposed below. The conductive features 306 provide vertical electrical routing from the device 200 to the conductive features 304 and between the conductive features 304. For example, the bottommost conductive feature 306 of the interconnect structure 300 may be electrically connected to a source / drain region 124 ( Figure 1B ) and the gate electrode layer 138 ( Figure 1B ). Conductive features 304 and conductive features 306 may be made of one or more conductive materials, such as metals, metal alloys, metal nitrides, or silicides. For example, conductive features 304 and conductive features 306 are made of copper, aluminum, aluminum-copper alloys, titanium, titanium nitride, tantalum, tantalum nitride, titanium silicon nitride, zirconium, gold, silver, cobalt, nickel, tungsten, tungsten nitride, tungsten silicon nitride, platinum, chromium, molybdenum, hafnium, other suitable conductive materials, or combinations thereof.
[0073] The intermetallic dielectric layer 302 includes one or more dielectric materials to provide isolation functions for the various conductive features 304, 306. The intermetallic dielectric layer 302 may include multiple dielectric layers that embed the multiple conductive features 304, 306. The intermetallic dielectric layer 302 is made of a dielectric material, such as SiO x 、SiO x C y H z or SiO x C y , where x, y, and z are integers or non-integers. In some embodiments, intermetal dielectric layer 302 includes a dielectric material having a dielectric value ranging from about 1 to about 5.
[0074] FIG. 3A to FIG. 3I 1 is a cross-sectional side view of various stages of manufacturing a semiconductor device structure 100 according to some embodiments. Figure 3A As shown, the semiconductor device structure 100 includes a substrate 102, a device 200, an interconnect structure 300, and a dielectric layer 310 formed on the interconnect structure 300. The dielectric layer 310 may be used to support a structure 312 ( Figure 3B) bonding layer. In some embodiments, dielectric layer 310 includes an oxide, such as silicon oxide. Dielectric layer 310 may have a thickness ranging from about 5 nanometers to about 1 micron. In some embodiments, dielectric layer 310 has a surface roughness of less than about 10 angstroms.
[0075] like Figure 3B As shown, the carrier structure 312 is bonded to the semiconductor device structure 100. The carrier structure 312 includes at least a semiconductor substrate 314, a release layer 316, and a bonding layer 318. The bonding layer 318 may include the same material as the dielectric layer 310 and may be bonded to the dielectric layer 310. The bonding layer 318 and the dielectric layer 310 may be bonded by any suitable method. In some embodiments, the carrier structure 312 includes additional layers. The carrier structure 312 may be bonded to the semiconductor device structure 100. Figure 4 Described in detail in.
[0076] like Figure 3C As shown, the semiconductor device structure 100 together with the supporting structure 312 is flipped over and subjected to backside processing. Figure 3D As shown, the substrate 102 is removed. In some embodiments, as Figure 3E As shown, a backside interconnect structure 400 is formed on the device 200 after removing the substrate 102. The backside interconnect structure 400 may include the same material as the interconnect structure 300. For example, one or more layers of conductive features (not shown) (e.g., conductive features 304, 306) may be embedded in an intermetallic dielectric layer (e.g., intermetallic dielectric layer 302). The conductive features located in the backside interconnect structure 400 may be electrically connected to the source / drain regions 124 and / or the gate electrode layer 138. By forming conductive features on the backside of the semiconductor device structure 100, high-density signal routing may be achieved.
[0077] like Figure 3F As shown, another carrier structure 320 is formed on the backside interconnect structure 400, and the semiconductor device structure 100 is flipped again so that the carrier structure 320 is located below the semiconductor device structure 100. In some embodiments, the carrier structure 320 includes the same layer as the carrier structure 312 and can be bonded to the backside interconnect structure 400 by the same process as bonding the carrier structure 312 to the dielectric layer 310.
[0078] like Figure 3F As shown, the semiconductor substrate 314 is released from the semiconductor device structure 100. The release of the semiconductor substrate 314 is achieved without damaging the semiconductor substrate 314. Therefore, the semiconductor substrate 314 can be reused in the supporting structure. FIG. 5A to FIG. 5CDetailed description of the release of the semiconductor substrate 314 is given in FIG. In some embodiments, the release of the semiconductor substrate 314 occurs at the release layer 316, and the bonding layer 318 remains on the semiconductor device structure 100, such as Figure 3F as shown in .
[0079] like Figure 3G As shown, the bonding layer 318 is removed from the semiconductor device structure 100. The bonding layer 318 may be removed by any suitable method. In some embodiments, the dielectric layer 310 is also removed. Figure 3H As shown, dielectric layer 322 is formed on dielectric layer 310 (or interconnect structure 300 if dielectric layer 310 is removed), and conductive pad 324 is formed in dielectric layer 322. Dielectric layer 322 may include the same material as intermetallic dielectric layer 302, and conductive pad 324 may include a conductive material, such as a metal (e.g., Al). In some embodiments, etch stop layer 326 is formed between dielectric layer 322 and dielectric layer 310. Fig. 3I As shown, the conductive bump 328 is formed on the corresponding conductive pad 324. Subsequent processes may be performed to form the stacked semiconductor device structure 100. For example, before forming the dielectric layer 310, the dielectric layer 322, the conductive pad 324, and the conductive bump 328, another carrier structure such as the carrier structure 320 may be bonded to the interconnect structure 300. Next, the semiconductor device structure 100 together with the carrier structure 320 and the carrier structure bonded to the interconnect structure 300 may be turned over, the carrier structure 320 may be removed, and another semiconductor device structure 100 may be bonded to the interconnect structure 400. Figure 3F As described in , after a predetermined number of semiconductor device structures 100 are stacked on the interconnect structure 400, the structure can be flipped, and the carrier structure formed on the interconnect structure 300 can be removed by any suitable process, such as releasing the semiconductor substrate 314. Figure 3F As described in , in some embodiments, the removal of the carrier structure 320 is performed by the same process as the release of the semiconductor substrate 314 .
[0080] A cross-sectional side view of a carrier structure 312 according to some embodiments. In some embodiments, the carrier structure 312 includes a semiconductor substrate 314, a dielectric layer 402 disposed on the semiconductor substrate 314, a release layer 316 disposed on the dielectric layer 402, a dielectric layer 404 disposed on the release layer 316, a reflective layer 406 disposed on the dielectric layer 404, and a bonding layer 318 disposed on the reflective layer 406. The carrier structure 312 can be formed by depositing the above layers in sequence. In some embodiments, the semiconductor substrate 314 is a silicon substrate, such as a silicon wafer, such as a 200 mm silicon wafer, a 300 mm silicon wafer, or a 450 mm silicon wafer. In some embodiments, the semiconductor substrate 314 has a thickness uniformity greater than about 99% and a surface roughness less than about 10 angstroms. Return to reference Figure 3B In some embodiments, the substrate 102 and the semiconductor substrate 314 are both silicon wafers. Therefore, there is no mismatch in coefficients of thermal expansion (CTE) between the substrate 102 and the semiconductor substrate 314 .
[0081] The dielectric layer 402 may be a dielectric layer with low thermal conductivity. In some embodiments, the dielectric layer 402 is an oxide, such as silicon oxide. The dielectric layer 402 may be formed by oxidizing a portion of the semiconductor substrate 314 or by depositing an oxide layer on the semiconductor substrate 314. The dielectric layer 402 has a thickness ranging from about 50 nanometers to about 400 nanometers. The dielectric layer 402 serves as a thermal insulator between the release layer 316 and the semiconductor substrate 314. Therefore, if the thickness of the dielectric layer 402 is less than about 50 nanometers, the heat absorbed by the release layer 316 will heat the semiconductor substrate 314. On the other hand, if the thickness of the dielectric layer 402 is greater than about 400 nanometers, the manufacturing cost increases without significant advantages.
[0082] The release layer 316 may include a metal or a metal nitride. In some embodiments, the release layer 316 includes a refractory metal or a refractory metal nitride. For example, the release layer 316 is a TiN layer. In some embodiments, the TiN layer is formed by physical vapor deposition. The physical vapor deposition TiN layer includes a columnar structure, each of which includes small crystals. The small crystals may have different lattice planes, and each may have a bare crystal size greater than about 4 nanometers, for example, about 5 nanometers to about 13 nanometers. The columnar structure of the physical vapor deposition TiN causes the top surface 410 of the release layer 316 to be rough, for example, having a surface roughness ranging from about 0.2 nanometers to about 5 nanometers. Therefore, when irradiated by an infrared (IR) laser, the release layer 316 absorbs heat from the infrared laser and expands, and a portion of the release layer 316 is separated from the dielectric layer 404. Therefore, the fracture energy at the interface between the release layer 316 and the dielectric layer 404 is low, for example, less than about 10 joules per square meter (J / m 2 ). In addition, separation occurs at the interface between the release layer 316 and the dielectric layer 404. For example, the bonding layer 318, the reflective layer 406, and the dielectric layer 404 remain on the semiconductor device structure 100, while the semiconductor substrate 314, the dielectric layer 402, and the release layer 316 are separated from the semiconductor device structure 100. In some embodiments, the dielectric layer 404, the reflective layer 406, and the bonding layer 318 are removed to expose the interconnect structure 300 disposed thereunder, and the conductive pad 324 is formed on the interconnect structure 300 ( Figure 3H ). By separating the semiconductor substrate 314, the dielectric layer 402, and the release layer 316 at the interface between the release layer 316 and the dielectric layer 404, it becomes easier to remove the dielectric layer 404, the reflective layer 406, and the bonding layer 318. In some embodiments, the release layer 316 is carbon-free because carbon may contaminate the processing environment.
[0083] In some embodiments, the release layer 316 includes TiN formed by chemical vapor deposition, metal nitrides other than TiN, or metals such as Ti or Au. The TiN layer formed by chemical vapor deposition, metal nitrides other than TiN, or metals forming the smooth top surface 410 are different from the rough top surface 410 formed by physical vapor deposition TiN. When the infrared laser is irradiated to the support structure 312, the release layer 316 absorbs the heat from the infrared laser and expands, and cracks may be formed in the release layer 316. Therefore, the release layer 316 may be split in the process of releasing the semiconductor substrate 314, and a higher fracture energy may be applied to release the semiconductor substrate 314. In addition, an additional etching process may be performed to remove the portion of the release layer 316 remaining on the semiconductor device structure 100.
[0084] In some embodiments, release layer 316 is a TiN layer formed by physical vapor deposition and ranges from about 10 nanometers to about 100 nanometers. If the thickness of release layer 316 is less than about 10 nanometers, no columnar structure is formed in release layer 316, and top surface 410 of release layer 316 is smooth. On the other hand, if the thickness of release layer 316 is greater than about 100 nanometers, more energy from the infrared laser is required to separate portions of release layer 316 from dielectric layer 404 without significant advantage.
[0085] The dielectric layer 404 may be a dielectric layer with low thermal conductivity. In some embodiments, the dielectric layer 404 is an oxide, such as silicon oxide. The dielectric layer 402 may be formed by depositing an oxide layer using a tetraethyl orthosilicate precursor on the semiconductor substrate 314. The dielectric layer 404 has a thickness ranging from about 300 nanometers to about 600 nanometers. The dielectric layer 404 serves as a thermal insulator between the release layer 316 and the reflective layer 406. Therefore, if the thickness of the dielectric layer 404 is less than about 300 nanometers, the heat absorbed by the reflective layer 406 may cause the reflective layer 406 to expand and separate from the dielectric layer 404 or the bonding layer 318. On the other hand, if the thickness of the dielectric layer 404 is greater than about 600 nanometers, the manufacturing cost increases without significant advantages. In some embodiments, the reflective layer 406 includes a material that expands at a lower temperature than the material of the release layer 316, and the thickness of the dielectric layer 404 is significantly greater than the thickness of the dielectric layer 402.
[0086] Reflective layer 406 includes a material that can absorb or reflect infrared light. Because semiconductor substrate 314 and dielectric layers 402, 404 are transparent to infrared light, reflective layer 406 absorbs or reflects any infrared light that is not absorbed by release layer 316. Reflective layer 406 protects conductive features 304, 306 located in interconnect structure 300 because conductive features 304, 306 are opaque to infrared light. If reflective layer 406 is formed of a material that is transparent to infrared light, infrared light can pass through reflective layer 406 and heat conductive features 304, 306, which may cause local heating of interconnect structure 300. In some embodiments, reflective layer 406 includes a metal, such as Cu, Ru or other suitable metals, or a metal nitride, such as TiN, TaN, or other suitable metal nitrides. In some embodiments, reflective layer 406 includes the same material as release layer 316. In some embodiments, reflective layer 406 and release layer 316 include different materials. Reflective layer 406 has a thickness ranging from about 10 nanometers to about 50 nanometers. If the thickness of the reflective layer 406 is less than about 10 nanometers, the risk of infrared light reaching the conductive features 304, 306 increases. On the other hand, if the thickness of the reflective layer 406 is greater than about 50 nanometers, the manufacturing cost increases without significant advantages. In some embodiments, the surface roughness of the reflective layer 406 is less than about 10 angstroms.
[0087] The bonding layer 318 may include a dielectric material, such as silicon oxide. The bonding layer 318 may have a thickness ranging from about 10 nanometers to about 2 micrometers. The bonding layer 318 may have a surface roughness of less than about 10 angstroms.
[0088] A cross-sectional side view of a carrier structure 312 heated by a laser according to some embodiments. The carrier structure 312 is disposed above the semiconductor device structure 100 and is FIG. 5A to FIG. 5C For the sake of clarity, the reflective layer 406 and the semiconductor device structure 100 are omitted. Figure 5A As shown, light 502 (e.g., infrared light) from a laser (e.g., an infrared laser) passes through the semiconductor substrate 314 and the dielectric layer 402 and is absorbed by the release layer 316. The laser can be a femtosecond (fs) infrared laser, and the light 502 can have a pulse duration of about 100 femtoseconds. The photons in the light 502 cause the electrons in the release layer 316 to collide and heat. However, the light 502 does not cause a portion of the release layer 316 to separate from the dielectric layer 404.
[0089] like Figure 5BAs shown, light 504 (e.g., infrared light) from a laser (e.g., an infrared laser) passes through semiconductor substrate 314 and dielectric layer 402 and is absorbed by release layer 316. The laser can be a picosecond (ps) infrared laser, and light 504 can have a pulse duration ranging from about 10 picoseconds to about 100 picoseconds. Light 504 causes lattice heating in release layer 316, and spallation may occur. Laser-induced spallation causes stress in release layer 316 due to thermal expansion of release layer 316. As described above, in some embodiments, release layer 316 is a TiN layer formed by physical vapor deposition and includes a rough top surface 410 (now the bottom surface after support structure 312 is bonded to semiconductor device structure 100). As a result of the laser-induced spallation, portions of rough top surface 410 are separated from dielectric layer 404. As shown in FIG. Figure 5B As shown, in some embodiments, cracks may be formed in the release layer 316. After the release layer 316 is exposed to light 504 multiple times at different locations, a majority of the top surface 410 of the release layer 316 is separated from the dielectric layer 404. The remaining portion of the release layer 316 that is still attached to the dielectric layer 404 may be separated from the dielectric layer 404 by a subsequent stripping process. The de-bonding force applied in the stripping process to separate the entire release layer 316 and the dielectric layer 404 after exposure to light 504 is relatively small, for example, less than about 13 joules per square meter. In some embodiments, the stripping process includes inserting a wedge between the release layer 316 and the dielectric layer 404. In some embodiments, the stripping process includes applying suction to the semiconductor substrate 314 and the substrate 102 and then pulling them away from each other.
[0090] like Figure 5C As shown, light 506 (e.g., infrared light) from a laser (e.g., an infrared laser) passes through the semiconductor substrate 314 and the dielectric layer 402 and is absorbed by the release layer 316. The laser may be a nanosecond (ns) infrared laser, and the light 506 may have a pulse duration in the nanosecond range. The light 506 causes decomposition and evaporation of the release layer 316, and a phase explosion and plasma formation may occur. As a result, in addition to the separation of a portion of the release layer 316 from the dielectric layer 404, a portion of the release layer 316 may also separate from the dielectric layer 402, and cracks may also be generated in the dielectric layers 402 and 404. During the subsequent debonding process, the separation of the support structure 312 from the semiconductor device structure 100 is not clean and may occur at multiple layers.
[0091] Both the nanosecond infrared laser and the picosecond infrared laser can separate portions of the release layer 316 from the dielectric layer 404. However, the picosecond infrared laser can cause a clean separation of the release layer 316 from the dielectric layer 404, while the nanosecond infrared laser can separate the carrier structure 312 from the semiconductor device structure 100 across multiple layers, such as the dielectric layer 402, the release layer 316, and the dielectric layer 404, which results in a more complex removal process to expose the interconnect structure 300.
[0092] In some embodiments, the infrared laser can have a depth of focus ranging from about 10 microns to about 100 microns, a laser energy ranging from about 2 microjoules (μJ) to about 8 microjoules, and a power density ranging from about 10E14 microjoules per square meter to about 10E16 microjoules per square meter. In some embodiments, the infrared laser imprint diameter is in the range of about 10 microns to about 100 microns, and the infrared laser line spacing is in the range of about 10 microns to about 100 microns.
[0093] The carrier structure 312 and the method of removing the carrier structure 312 from the structure can be used for any suitable application. For example, the carrier structure 312 can be used for integrated fan-out (InFO) packaging technology. In some embodiments, the bare die can be placed on the carrier structure 312 instead of on the carrier structure including a glass substrate. In some embodiments, because the bare die includes a silicon substrate, there is a lower risk of a mismatch in the coefficient of thermal expansion (CTE) between the silicon substrate of the bare die and the semiconductor substrate 314 of the carrier structure 312 compared to a glass substrate of a different carrier structure.
[0094] The present disclosure provides a support structure and a method for forming the same in various embodiments. In some embodiments, the support structure includes a semiconductor substrate 314, a first dielectric layer 402 disposed on the semiconductor substrate 314, a release layer 316 disposed on the first dielectric layer 402, a second dielectric layer 404 disposed on the release layer 316, a reflective layer 406 disposed on the second dielectric layer 404, and a bonding layer 318 disposed on the reflective layer 406. The release layer 316 is a carbon-free metal nitride layer. Some embodiments can achieve advantages. For example, the semiconductor substrate 314 and the substrate 102 include the same material and there is no mismatch in thermal expansion coefficients. In addition, the carbon-free metal nitride layer can result in a clean separation at the interface of the release layer 316 and the dielectric layer 404, resulting in an easier etching process to expose the interconnect structure 300. In addition, the semiconductor substrate 314 will not be damaged during the separation process and can be reused to save costs.
[0095] The embodiment of the present disclosure provides a method for forming a supporting structure, comprising: forming one or more devices on a substrate; forming a first interconnect structure on the one or more devices; bonding the first interconnect structure to a supporting structure, wherein the supporting structure comprises a semiconductor substrate, a release layer and a first dielectric layer, and the release layer comprises a metal nitride; flipping the one or more devices so that the supporting structure is located at a bottom; performing multiple back-side processes; flipping the one or more devices so that the supporting structure is located at a top; and exposing the supporting structure to infrared light so that part of the release layer is separated from the first dielectric layer.
[0096] In one embodiment, the one or more devices include transistors, diodes, image sensors, resistors, capacitors, inductors, memory cells, or combinations thereof. In one embodiment, the backside process includes removing the substrate and forming a second interconnect structure on the one or more devices. In one embodiment, the infrared light is from a picosecond infrared laser. In one embodiment, a pulse duration of the infrared light is in the range of 10 picoseconds to 100 picoseconds. In one embodiment, the release layer includes TiN. In one embodiment, the release layer is deposited by physical vapor deposition. In one embodiment, during exposure of the support structure to the infrared light, the infrared light is absorbed by the release layer. In one embodiment, the infrared light causes lattice heating of the release layer, and a portion of the release layer is separated from the first dielectric layer by spallation.
[0097] The disclosed embodiment also provides a method for forming a carrier structure, comprising: forming a carrier structure, comprising: depositing a first dielectric layer on a semiconductor substrate; depositing a release layer on the first dielectric layer by a physical vapor deposition process, the release layer comprising TiN; depositing a second dielectric layer on the release layer; depositing a reflective layer on the second dielectric layer; and depositing a bonding layer on the reflective layer; bonding the carrier structure to a semiconductor device structure; flipping the semiconductor device structure; performing one or more processes on the semiconductor device structure; and removing the carrier structure.
[0098] In one embodiment, the semiconductor device structure includes one or more devices and an interconnect structure disposed on the one or more devices. In one embodiment, removing the support structure includes exposing the support structure to a plurality of infrared lights. In one embodiment, each of the infrared lights has a pulse duration ranging from 10 picoseconds to 100 picoseconds. In one embodiment, the infrared light is generated by an infrared laser. In one embodiment, the infrared laser is a picosecond infrared laser. In one embodiment, removing the support structure also includes applying a peeling force. In one embodiment, the peeling force is less than 13 joules per square meter.
[0099] The present disclosure also provides a supporting structure, including a semiconductor substrate, a first dielectric layer, a release layer, a second dielectric layer, a reflective layer and a bonding layer. The first dielectric layer is disposed on the semiconductor substrate. The release layer is disposed on the first dielectric layer. The release layer is carbon-free and includes a metal nitride. The second dielectric layer is disposed on the release layer. The reflective layer is disposed on the second dielectric layer. The bonding layer is disposed on the reflective layer.
[0100] In one embodiment, the release layer is a TiN layer. In one embodiment, the TiN layer is formed by physical vapor deposition.
[0101] The features of several embodiments are summarized above so that those skilled in the art can better understand aspects of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to achieve the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art should also recognize that such equivalent structures do not depart from the spirit and scope of the present disclosure, and they can make various changes, substitutions and modifications thereto without departing from the spirit and scope of the present disclosure.
Claims
1. A load-bearing structure, It is characterized in that include: a semiconductor substrate; a first dielectric layer disposed on the semiconductor substrate; a release layer disposed on the first dielectric layer, wherein the release layer is carbon-free and comprises a metal nitride; a second dielectric layer disposed on the release layer; a reflective layer disposed on the second dielectric layer; and A bonding layer is disposed on the reflective layer.
2. The bearing structure according to claim 1, It is characterized in that The release layer is a TiN layer.
3. The bearing structure according to claim 2, It is characterized in that The TiN layer is formed by physical vapor deposition.
4. The bearing structure according to claim 3, It is characterized in that The TiN layer includes a columnar structure.
5. The bearing structure according to claim 4, It is characterized in that A top surface of the release layer is rough.
6. The bearing structure according to claim 5, It is characterized in that The top surface of the release layer has a surface roughness ranging from 0.2 nanometers to 5 nanometers.
7. The bearing structure according to claim 1, It is characterized in that The release layer absorbs heat from an infrared light and expands.
8. The bearing structure according to claim 7, It is characterized in that The infrared light is generated by an infrared laser.
9. The load-bearing structure according to claim 8, It is characterized in that The infrared light is a picosecond infrared laser.
10. The load-bearing structure according to claim 7, It is characterized in that The duration of a pulse of the infrared light is in the range of 10 picoseconds to 100 picoseconds.