Photovoltaic texturing device based on two-step method

By introducing protective components and agitator blades into the photovoltaic texturing device, the problem of solvent splashing was solved, thereby improving safety and efficiency.

CN222029098UActive Publication Date: 2024-11-19JIANGSU JINGKAISHENG NEW ENERGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420530430.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-19
Publication Date
2024-11-19
Estimated Expiration
2034-03-19

AI Technical Summary

Technical Problem

Existing photovoltaic texturing equipment lacks protection around the texturing tank, which could cause solvent splashes that could injure workers.

Method used

A photovoltaic texturing device based on a two-step method was designed. The device employs protective components including a protective baffle, a limiting frame, and a sliding sleeve. The protective baffle is adjustable and shields the solvent by means of screws and nuts to prevent solvent splashing. The device also uses a drive motor to drive stirring blades to improve solvent flow and accelerate texturing efficiency.

Benefits of technology

It effectively prevents solvent splashes from injuring workers, improves the safety of the texturing process, and increases texturing efficiency by agitating the solvent.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222029098U_ABST
    Figure CN222029098U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of photovoltaic texturing, in particular to a photovoltaic texturing device based on a two-step method, which comprises a working table, mounting grooves are symmetrically formed in the top of the working table, supporting guide rods are mounted on the inner bottom walls of the mounting grooves, and protection assemblies are arranged on the outer sides of the supporting guide rods. The protection assembly is used for avoiding the situation that a solvent is sputtered in the texturing process to hurt workers. According to the utility model, before texturing treatment is carried out on the silicon wafer, a worker can rotate the nut to enable the nut to exit from the screw, rotate the screw to exit from the slot and enable the sliding sleeve to slide into the mounting groove, at the moment, the sliding sleeve does not support the limiting frame, and the worker can pull the limiting frame downwards to enable the limiting frame to drive the protective baffle to descend; and the protective baffle shields the periphery of the texturing treatment groove until the bottom of the limiting frame is in contact with the top of the workbench, so that the solvent is prevented from splashing to damage nearby workers, and the safety protection performance in the texturing treatment process is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of photovoltaic texturing, in particular to a photovoltaic texturing device based on a two-step method. Background Art

[0002] Texturing, a term in the photovoltaic industry, is a process for processing solar-grade silicon wafers and a process in the production of silicon solar cells. Two-step texturing refers to the etching of acid and alkali in sequence. During the processing, the surface of the silicon wafer needs to be etched into a uniform velvet surface to increase the absorption of sunlight, reduce reflection, increase the PN junction area, and thus improve the photoelectric conversion efficiency of the battery.

[0003] When the existing photovoltaic texturing device is in use, in order to facilitate the taking of silicon wafers, there is no shielding around the texturing tank, and there is no protective baffle around the texturing tank. During the texturing process, the solvent may splash nearby and injure the staff. Utility Model Content

[0004] One purpose of the present application is to provide a photovoltaic texturing device based on a two-step method to solve the problem in the prior art that there is no protective baffle around the texturing tank, and the solvent during the texturing process may splash nearby and injure workers.

[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a photovoltaic texturing device based on a two-step method, comprising a workbench, wherein the top of the workbench is symmetrically provided with mounting grooves, the inner bottom wall of the mounting grooves is provided with supporting guide rods, and the outer side of the supporting guide rods is provided with a protective component, and the protective component is used to prevent injuries to workers caused by splashing of solvents during the texturing process.

[0006] Preferably, the protective assembly includes a protective baffle, a limit frame and a sliding sleeve. The protective baffle is slidably installed on the outside of four groups of supporting guide rods. The limit frame is installed on the bottom of the protective baffle, and the limit frame is slidably connected to the supporting guide rod. A slot is opened through one side of the supporting guide rod, and a sliding sleeve is movably installed on the outside of the supporting guide rod. A screw is installed through one side of the sliding sleeve, and the middle section of the screw is located inside the slot, and a nut is installed on the outside of one end of the screw through a thread.

[0007] Preferably, the top of the supporting guide rod is connected to a top plate, the bottom of the top plate is symmetrically mounted with an electric telescopic push rod, and the telescopic end of the electric telescopic push rod is connected to a placement rack.

[0008] Preferably, a texturing groove is provided at the top center of the workbench, and a heating partition net is installed on the inner side wall of the texturing groove.

[0009] Preferably, a driving motor is embedded and installed inside the workbench, and the output end of the driving motor passes through the inner bottom wall of the texturing tank.

[0010] Preferably, the output end of the driving motor is connected to a rotating shaft, and stirring blades are symmetrically installed on the outer side of the rotating shaft, and the stirring blades are located below the heating partition net.

[0011] Preferably, an overflow groove is provided on the inner side wall of the texturing tank, and the overflow groove is close to the top opening of the texturing tank, a guide pipe is installed through one side of the workbench, and one end of the guide pipe is connected to the overflow groove, and a valve is installed on the outside of the guide pipe.

[0012] Compared with the prior art, the beneficial effects of the utility model are:

[0013] The nut is rotated and set on the outside of the screw so that the sliding sleeve is fixed on the supporting guide rod. At this time, the four sets of sliding sleeves provide supporting force for the limiting frame, and the restriction of the limiting frame by the sliding sleeve makes the protective baffle plate be located at the upper end of the supporting guide rod, without blocking the staff from taking out the silicon wafer after the texturing is completed.

[0014] 2. In the utility model, after the silicon wafer on the placement rack is completely under the liquid level of the solvent in the texturing tank, the drive motor is started to drive the rotating shaft to rotate, and the rotating shaft drives the stirring blades to rotate together, so that the solvent in the texturing tank is stirred, which can improve the fluidity of the solvent and accelerate the texturing efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a three-dimensional diagram of the utility model;

[0016] Figure 2 It is a front cross-sectional view of the utility model;

[0017] Figure 3 For the utility model Figure 2 A magnified schematic diagram of point A;

[0018] Figure 4 For the utility model Figure 2 An enlarged schematic diagram of point B.

[0019] In the figure: 1. workbench; 2. mounting groove; 3. support guide rod; 4. top plate; 5. protective baffle; 6. limit frame; 7. slot; 8. sleeve; 9. screw; 10. nut; 11. electric telescopic push rod; 12. placement rack; 13. velvet making groove; 14. heating separation net; 15. driving motor; 16. rotating shaft; 17. stirring blade; 18. overflow groove; 19. guide pipe; 20. valve. DETAILED DESCRIPTION

[0020] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0021] In the description of the present invention, it should be noted that the terms "upper", "lower", "inner", "outer", "front end", "rear end", "two ends", "one end", "the other end" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.

[0022] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0023] The following is combined with Figure 1-4 , the technical solution of the utility model is further explained:

[0024] Embodiment 1: Figure 1-Figure 3As shown, a photovoltaic texturing device based on a two-step method includes a workbench 1, a mounting groove 2 is symmetrically opened on the top of the workbench 1, a support guide rod 3 is installed on the inner bottom wall of the mounting groove 2, and a protective component is arranged on the outer side of the support guide rod 3, and the protective component is used to prevent the solvent from splashing during the texturing process and causing harm to the staff. The protective component includes a protective baffle 5, a limit frame 6 and a sliding sleeve 8, the protective baffle 5 is slidably installed on the outer side of the four groups of support guide rods 3, the bottom of the protective baffle 5 is installed with a limit frame 6, and the limit frame 6 is slidably connected with the support guide rod 3, a slot 7 is opened through one side of the support guide rod 3, a sliding sleeve 8 is movably installed on the outer side of the support guide rod 3, a screw 9 is installed through one side of the sliding sleeve 8, and the middle section of the screw 9 is located inside the slot 7, and a nut 10 is installed on the outer side of one end of the screw 9 through a thread. The workbench 1 provides a location for the mounting groove 2. The mounting groove 2 provides a mounting location for the support guide rod 3. The support guide rod 3 provides a mounting location for the protective component. The support guide rod 3 provides a slidable installation position for the protective baffle 5, and at the same time, the support guide rod 3 provides a guide function for the sliding of the protective baffle 5. The protective baffle 5 provides an installation position for the limit frame 6. The support guide rod 3 provides an opening position for the slot 7. The slot 7 provides an insertion position for the screw 9. The support guide rod 3 provides an installation position for the sliding sleeve 8. The sliding sleeve 8 provides an installation position for the screw 9. The screw 9 provides an installation position for the nut 10. The nut 10 and the screw 9 cooperate with each other to fix the sliding sleeve 8 on the outside of the support guide rod 3. Before the silicon wafer is subjected to the texturing treatment, the staff can rotate the nut 10 to make the nut 10 withdraw from the screw 9, rotate the screw 9 to withdraw from the slot 7, and make the sliding sleeve 8 slide into the installation slot 2. At this time, the sliding sleeve 8 has no supporting effect on the limit frame 6. The staff can pull the limit frame 6 downward to make the limit frame 6 drive the protective baffle 5 to descend until the bottom of the limit frame 6 contacts the top of the workbench 1. At this time, the protective baffle 5 shields the surrounding areas of the texturing treatment slot to prevent the solvent from splashing and injuring nearby staff, thereby improving the safety and protection of the texturing treatment process. ; When the texturing is completed, the staff can push the protective baffle 5 upwards and slide the sleeve 8 upwards until the screw 9 on the sleeve 8 corresponds to the slot 7, rotate the screw 9 to make the screw 9 pass through the slot 7 until the other end of the screw 9 is exposed from the sleeve 8, and rotate the nut 10 to be set on the outside of the screw 9 so that the sleeve 8 is fixed on the supporting guide rod 3. At this time, the four groups of sleeves 8 provide supporting force for the limit frame 6. The restriction of the sleeve 8 on the limit frame 6 makes the protective baffle 5 located at the upper end of the supporting guide rod 3, and does not block the staff from taking out the silicon wafer after the texturing is completed.

[0025] Embodiment 2: Figure 1-Figure 4As shown, the top of the support guide rod 3 is connected to the top plate 4, and the bottom of the top plate 4 is symmetrically installed with an electric telescopic push rod 11, and the telescopic end of the electric telescopic push rod 11 is connected to the placement rack 12. A texturing groove 13 is opened at the top center of the workbench 1, and a heating partition net 14 is installed on the inner side wall of the texturing groove 13. A driving motor 15 is embedded and installed inside the workbench 1, and the output end of the driving motor 15 passes through the inner bottom wall of the texturing groove 13. The output end of the driving motor 15 is connected to a rotating shaft 16, and a stirring blade 17 is symmetrically installed on the outer side of the rotating shaft 16, and the stirring blade 17 is located below the heating partition net 14. The support guide rod 3 provides an installation connection position for the top plate 4 and provides support force for the top plate 4. The top plate 4 provides an installation position for the electric telescopic push rod 11. The electric telescopic push rod 11 provides an installation position for the placement rack 12, and also provides a driving force for the placement rack 12. The workbench 1 provides an installation position for the texturing groove 13. The texturing groove 13 provides space for the texturing process. The texturing tank 13 provides an installation position for the heating partition net 14. The heating partition net 14 heats the solvent during the texturing process and separates the stirring blade 17 from the placement rack 12. The workbench 1 provides an installation position for the drive motor 15. The drive motor 15 provides an installation connection position and driving force for the rotating shaft 16. The rotating shaft 16 provides an installation position for the stirring blade 17. The stirring blade 17 can rotate with the rotating shaft 16 to stir the solvent in the texturing tank 13. When texturing is required, the electric telescopic push rod 11 pushes the placement rack 12 into the interior of the texturing tank 13, and the heating partition net 14 heats the solvent. After the silicon wafer on the placement rack 12 completely enters the liquid level of the solvent in the texturing tank 13, the drive motor 15 is started to drive the rotating shaft 16 to rotate, and the rotating shaft 16 drives the stirring blade 17 to rotate together, so that the solvent in the texturing tank 13 is stirred, which can improve the fluidity of the solvent and speed up the texturing efficiency.

[0026] Embodiment 3: An overflow groove 18 is provided on the inner side wall of the texturing tank 13, and the overflow groove 18 is close to the top opening of the texturing tank 13. A guide tube 19 is installed through one side of the workbench 1, and one end of the guide tube 19 is connected to the overflow groove 18, and a valve 20 is installed on the outside of the guide tube 19. The overflow groove 18 provides an installation position. The workbench 1 provides an installation position for the guide tube 19. The guide tube 19 provides a channel for the overflowed solvent to flow out, and also provides an installation position for the valve 20. The valve 20 can control the on and off of the guide tube 19, so that the overflowed solvent can flow out of the guide tube 19. When the placement rack 12 carries the silicon wafer into the texturing tank 13, the solvent liquid level in the texturing tank 13 rises. When the solvent liquid level is higher than the overflow groove 18, the excess solvent will flow into the overflow groove 18, and finally flow out along the guide tube 19.

[0027] Working principle: Before using the photovoltaic texturing device based on the two-step method, you should first check whether there are any problems that affect the use of the photovoltaic texturing device based on the two-step method. First, place the photovoltaic texturing device based on the two-step method at the location where it needs to be used. Before texturing the silicon wafer, the staff can rotate the nut 10 to make the nut 10 withdraw from the screw 9, rotate the screw 9 to withdraw from the slot 7, and make the sliding sleeve 8 slide into the installation slot 2. At this time, the sliding sleeve 8 has no supporting effect on the limit frame 6. The staff can pull the limit frame 6 downward, so that the limit frame 6 drives the protective baffle 5 to descend until the bottom of the limit frame 6 contacts the top of the workbench 1. At this time, the protective baffle 5 will be texturized. The groove is shielded on all sides to prevent the splashing of solvent from injuring nearby workers, thereby improving the safety and protection of the texturing process; when the texturing is completed, the worker can push the protective baffle 5 upwards, slide the sleeve 8 upwards until the screw 9 on the sleeve 8 corresponds to the slot 7, rotate the screw 9, and pass the screw 9 through the slot 7 until the other end of the screw 9 exposes the sleeve 8, and rotate the nut 10 to the outside of the screw 9 so that the sleeve 8 is fixed on the support guide rod 3. At this time, the four groups of sleeves 8 provide support for the limit frame 6, and the limit of the limit frame 6 by the sleeve 8 makes the protective baffle 5 located at the upper end of the support guide rod 3, so as not to block the worker from taking out the silicon wafer after the texturing is completed. When texturing is required, the electric telescopic push rod 11 pushes the placement rack 12 into the interior of the texturing groove 13, and the heating partition net 14 heats the solvent. After the silicon wafer on the placement rack 12 is completely below the liquid level of the solvent in the texturing tank 13, the drive motor 15 is started to drive the rotating shaft 16 to rotate, and the rotating shaft 16 drives the stirring blade 17 to rotate together, so that the solvent in the texturing tank 13 is stirred, which can improve the fluidity of the solvent and speed up the texturing efficiency.

[0028] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims are included in the present invention, and any figure mark in the claims should not be regarded as limiting the claims involved.

Claims

1. A photovoltaic texturing device based on a two-step method, comprising a workbench (1), Features: The top of the workbench (1) is symmetrically provided with an installation groove (2), the inner bottom wall of the installation groove (2) is installed with a support guide rod (3), and the outer side of the support guide rod (3) is provided with a protective component, which is used to prevent the splashing of solvent during the texturing process from causing harm to the workers.

2. A photovoltaic texturing device based on a two-step method according to claim 1, Features: The protection component comprises a protection baffle (5), a limit frame (6) and a sliding sleeve (8); the protection baffle (5) is slidably mounted on the outer sides of the four groups of support guide rods (3); a limit frame (6) is mounted on the bottom of the protection baffle (5), and the limit frame (6) is slidably connected to the support guide rod (3); a slot (7) is provided through one side of the support guide rod (3); a sliding sleeve (8) is movably mounted on the outer side of the support guide rod (3); a screw (9) is installed through one side of the sliding sleeve (8), and the middle section of the screw (9) is located inside the slot (7); a nut (10) is threadedly mounted on the outer side of one end of the screw (9).

3. A photovoltaic texturing device based on a two-step method according to claim 1, Features: The top of the supporting guide rod (3) is connected to a top plate (4), the bottom of the top plate (4) is symmetrically mounted with an electric telescopic push rod (11), and the telescopic end of the electric telescopic push rod (11) is connected to a placement frame (12).

4. A photovoltaic texturing device based on a two-step method according to claim 1, Features: A texturing groove (13) is provided at the top center of the workbench (1), and a heating partition net (14) is installed on the inner side wall of the texturing groove (13).

5. A photovoltaic texturing device based on a two-step method according to claim 1, Features: A driving motor (15) is embedded and installed inside the workbench (1), and the output end of the driving motor (15) passes through the inner bottom wall of the texturing tank (13).

6. A photovoltaic texturing device based on a two-step method according to claim 5, Features: The output end of the driving motor (15) is connected to a rotating shaft (16), and stirring blades (17) are symmetrically mounted on the outer side of the rotating shaft (16), and the stirring blades (17) are located below the heating partition net (14).

7. A photovoltaic texturing device based on a two-step method according to claim 4, Features: An overflow groove (18) is provided on the inner side wall of the texturing groove (13), and the overflow groove (18) is close to the top opening of the texturing groove (13). A guide pipe (19) is installed through one side of the workbench (1), and one end of the guide pipe (19) is connected to the overflow groove (18), and a valve (20) is installed on the outside of the guide pipe (19).