Glass touch screen capable of preventing short circuit and open circuit
By adopting wear-resistant components and transparent insulating layer design in glass touch screens, the short circuit and circuit breaking problems caused by foreign objects, water vapor, etc. are solved, which improves yield and production efficiency and reduces costs.
Patent Information
- Application Number
- CN202420778629.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-16
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-04-16
AI Technical Summary
During the production process, conventional glass touch screens are prone to short-circuit or breakage due to foreign objects, water vapor, dust, scratches, and crushing, resulting in high production costs and low efficiency, which cannot meet the needs of batch processing.
A glass touch screen that is anti-short and broken is designed, using a trace composed of wear-resistant components to increase the wiring distance between traces, use a transparent insulation layer to improve moisture resistance, and enhance the trace through a combination of silver paste and carbon paste. Scratch and pressure resistance of the wire.
有效减少了短路和断路现象,提高了玻璃触摸屏的良品率,降低了生产成本,提升了加工效率,使电测良率达到95%以上。
Smart Images

Figure CN222071206U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a glass touch screen, in particular to a glass touch screen which is short-circuit and open-circuit proof. Background Art
[0002] During the production process, conventional glass touch screens often suffer from short circuits or disconnections due to foreign matter, water vapor, dust, scratches, pressure, etc. For example, when the size of solid particles such as foreign matter or dust is larger than the distance between the traces, the solid particles are more likely to overlap between the two traces, causing the channel to short-circuit; when in an environment with high humidity, external moisture will enter the surface of the conductive layer of the glass sensor, making the electrical capacitance value too large, causing a short circuit; when the glass sensor is scratched or pressed, the edge traces do not have good scratch resistance and are prone to breakage or tearing, causing a disconnection.
[0003] Due to the above reasons, during the production process of conventional glass touch screens, the electrical test yield of the glass touch screen generally fluctuates between 80% and 85%. The increase in short circuits and open circuits of the touch screen will greatly reduce the production yield and increase production costs. Therefore, the existing touch screen design cannot meet the mass processing needs of enterprises. Utility Model Content
[0004] The utility model aims to overcome the deficiencies of the prior art and provide a glass touch screen which is resistant to short circuit and disconnection, has high yield, low production cost and high processing efficiency.
[0005] To achieve the above object, the technical solution adopted by the utility model is: a glass touch screen that prevents short circuit and disconnection, including a cover plate, an adhesive, a sensor, an adhesive and a liquid crystal display module that are sequentially connected from top to bottom;
[0006] The upper surface and the lower surface of the sensor are respectively provided with a first edge routing and a second edge routing, which are used to overlap with the conductive layer in the sensor to form a loop; the first edge routing and the second edge routing are respectively composed of a plurality of first routings and second routings overlapped and connected with the conductive layer, and the line spacing between two adjacent first routings is greater than the line width of each first routing, and the line spacing between two adjacent second routings is greater than the line width of each second routing; the materials of the first routing and the second routing are both made of wear-resistant components;
[0007] The upper surface of the first edge wiring and the conductive layer on the upper surface of the sensor are respectively provided with a first transparent insulating layer and a second transparent insulating layer;
[0008] The lower surface of the second edge wiring and the conductive layer on the lower surface of the sensor are respectively provided with a third transparent insulating layer and a fourth transparent insulating layer.
[0009] Furthermore, the wear-resistant component includes silver paste; and carbon paste is provided on the upper surface of the silver paste.
[0010] Furthermore, the overall thickness of the silver paste and the carbon paste is 10 to 20 um.
[0011] Furthermore, the line width of the first edge routing and the second edge routing is 15um-20um, and the line spacing is 40um-45um.
[0012] Furthermore, the first transparent insulating layer, the second transparent insulating layer, the third transparent insulating layer and the fourth transparent insulating layer are made of insulating ink.
[0013] Furthermore, the light transmittance of the first transparent insulating layer, the second transparent insulating layer, the third transparent insulating layer and the fourth transparent insulating layer is 99.9%.
[0014] Furthermore, the adhesive is solid optically transparent glue, liquid silicone water glue or acrylic water glue.
[0015] Furthermore, the sensor is a touch sensor.
[0016] Due to the application of the above technical solution, the utility model has the following advantages compared with the prior art:
[0017] 1. The utility model is a glass touch screen that prevents short circuit and open circuit, optimizes the wiring design, reduces the line width of the first wiring and the second wiring, and increases the line distance between the adjacent first wiring and the second wiring respectively, so that the wiring distance is larger than the particle size of solid particles. Even if solid particles adhere between the wirings, the two wirings will not overlap with each other, thereby not causing a short circuit.
[0018] 2. The wear-resistant component is composed of silver paste and carbon paste. The first edge routing and the second edge routing composed of the wear-resistant component can improve the scratch resistance and pressure resistance of the silver paste due to the excellent wear resistance of the carbon paste, thereby preventing the touch screen from breaking.
[0019] 3. Ultra-thin transparent insulation is printed on the first edge routing, the second edge routing and the conductive layer of the sensor. This insulation will not affect the optical performance of the touch screen, but can improve the moisture resistance of the sensor surface and prevent the conductive layer on the sensor surface from absorbing moisture and causing a short circuit. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The technical solution of the utility model is further described below in conjunction with the accompanying drawings:
[0021] Figure 1 This is a schematic diagram of the structure of an embodiment of the utility model;
[0022] Figure 2 A top view of a sensor connected to a first edge wiring in an embodiment of the utility model;
[0023] Figure 3 for Figure 2 A schematic diagram of a structure having a first transparent insulating layer, a second transparent insulating layer, a third transparent insulating layer and a fourth transparent insulating layer printed thereon;
[0024] Figure 4 A side view of a sensor connected to a first edge wiring in an embodiment of the utility model;
[0025] Figure 5 It is a partial schematic diagram of the first edge routing in one embodiment of the utility model;
[0026] Wherein: cover plate 1, adhesive 2, sensor 3, liquid crystal display module 4, first edge wiring 5, second edge wiring 6, first transparent insulating layer 7, second transparent insulating layer 8, third transparent insulating layer 9, fourth transparent insulating layer 10, conductive layer 30, first wiring 50, silver paste 80, carbon paste 81. DETAILED DESCRIPTION
[0027] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present application.
[0028] The utility model provides a glass touch screen that prevents short circuit and disconnection, so as to solve the problem in the prior art that the glass touch screen is often short-circuited or disconnected due to foreign matter, water vapor, dust, scratches, pressure damage, etc. during the production process, resulting in high production cost and low production efficiency.
[0029] For ease of understanding, the specific process in the embodiments of the present application is described below. Figures 1 to 3A glass touch screen for preventing short circuit and open circuit in an embodiment of the present application comprises a cover plate 1, an adhesive 2, a sensor 3, an adhesive 2 and a liquid crystal display module 4 which are sequentially connected from top to bottom; a first edge wiring 5 and a second edge wiring 6 are respectively arranged around the upper surface and the lower surface of the sensor 3, which are respectively overlapped with the conductive layer 30 in the sensor 3 to form a loop; the first edge wiring 5 and the second edge wiring 6 are respectively composed of a plurality of first wirings 50 and a second wiring which are overlapped and connected with the conductive layer 30.
[0030] The line spacing between two adjacent first routing lines 50 is greater than the line width of each first routing line 50, and the line spacing between two adjacent second routing lines is greater than the line width of each second routing line; the materials of the first routing line 50 and the second routing line 5 are both composed of wear-resistant components; the upper surface of the first edge routing line 5 and the conductive layer on the upper surface of the sensor 3 are respectively provided with a first transparent insulating layer 7 and a second transparent insulating layer 8; the lower surface of the second edge routing line 6 and the conductive layer on the lower surface of the sensor 3 are respectively provided with a third transparent insulating layer 9 and a fourth transparent insulating layer 10.
[0031] In the glass touch screen that prevents short circuit and open circuit of the utility model, the materials of the first wiring 50 and the second wiring are both made of wear-resistant components, which improves the wear resistance and avoids open circuit; secondly, the line distance between two adjacent first wirings and two adjacent second wirings is respectively greater than the line width of the first wiring and the second wiring, thereby preventing solid particles from adhering to the two wirings and causing short circuit; in addition, insulating layers are provided on the first edge wiring, the second edge wiring and the front and back sides of the sensor, which improves the moisture-proof performance and avoids short circuit, thereby making the glass touch screen have a high yield rate, improving production efficiency and reducing production costs.
[0032] based on Figure 4 In this embodiment, the wear-resistant component includes a silver paste 80, and a carbon paste 81 is provided on the upper surface of the silver paste 80. The first edge routing 5 is specifically described below, that is, the silver paste corresponding to the plurality of first routings 50 is printed, cured, and lasered to form a silver paste circuit with a certain short line width and long line spacing, and then a layer of carbon paste is printed on the surface of the silver paste routing. After carbon paste printing, curing, and lasering, a carbon paste circuit with a certain short line width and long line spacing is formed. The carbon paste circuit is arranged on the upper surface of sensor 3, and the line width and line spacing of the carbon paste are consistent with the line width and line spacing of the silver paste, with a thickness of 5 to 10 um. At this time, the overall thickness of the silver paste thickness and the carbon paste thickness is 10 to 20 um, and the first routing 50 is composed of silver paste and carbon paste.
[0033] In addition, the wear-resistant component can be prepared by mixing carbon paste, silver paste, organic solvent, and organic resin in a certain ratio to prepare a silver paste mixture containing carbon paste, and then printing the silver paste mixture containing carbon paste on sensor 3. After curing and laser, a first edge wiring layer of carbon paste and silver paste mixture with a thickness of 5 to 10 um is obtained. This first edge wiring is also located on the upper surface of sensor 3.
[0034] Since carbon paste has excellent wear resistance, the above two methods can prevent the silver paste from being crushed, scratched, and scratched during the sensor manufacturing process, thereby protecting the silver paste and preventing the silver paste from breaking, thereby protecting the first edge wiring 5 and the second edge wiring.
[0035] based on Figure 5 In this embodiment, the line width and line spacing of two adjacent first routing lines 50 and two adjacent second routing lines are adjusted. Two adjacent first routing lines 50 are listed below for illustration. Specifically, by reducing the line width b of the two adjacent first routing lines 5 and increasing the line spacing a between the two adjacent first routing lines, when foreign matter, dust, debris and other solid particles in the environment adhere to the first routing line of sensor 3, the line spacing between the two adjacent first routing lines is larger, and the possibility of solid particles overlapping between the two routing lines is smaller, so that the risk of short circuit in the channel is smaller, thereby reducing the possibility of short circuit.
[0036] Specifically, in this embodiment, the line width of the first wiring 50 and the second wiring is 15um, and the line distance is 40um, which can prevent solid particles from overlapping between two first wirings or two second wirings, thereby reducing the probability of short circuit on the glass touch screen.
[0037] based on Figures 1 to 3 In this embodiment, the first transparent insulating layer 7, the second transparent insulating layer 8, the third transparent insulating layer 9, and the fourth transparent insulating layer 10 are all highly transparent insulating inks, mainly composed of polyol resin, acrylic resin, ethylene glycol butyl ether acetate, diethylene glycol monoethyl ether and other components. The first transparent insulating layer 7 and the third transparent insulating layer 9 are printed on the upper surface of the first edge wiring 5 and the lower surface of the second edge wiring, with a thickness of 5 to 10 um. The second transparent insulating layer 8 and the fourth transparent insulating layer 10 are printed on the upper surface and the lower surface of the sensor 3.
[0038] Specifically, the second transparent insulating layer 8 and the fourth transparent insulating layer 10 are printed on the conductive layer 30 of sensor 3 and are in direct contact with the conductive layer 30, and the other part is printed on the surface of the first edge wiring and the second edge wiring, which can effectively prevent the conductive layer 30 in sensor 3 and the first edge wiring and the second edge wiring from contacting external moisture and causing a short circuit, and prevent the conductive layer 30 from being oxidized due to excessive moisture.
[0039] The above-mentioned insulating layer is a highly transparent insulating ink with a transmittance of up to 99.9%. It will not affect the transmittance of the product or the user's visual experience.
[0040] Furthermore, the cover plate 1 can be made of glass, PC, PMMA, PET, TAC or the like, and can be a flat 2D cover plate, or a 2.5D or 3D cover plate.
[0041] Furthermore, the adhesive 2 can be a solid optically transparent adhesive, or a liquid silicone water-based adhesive or acrylic water-based adhesive, which has a high transmittance and a high viscosity, and the thickness is generally 150um, 175um, 200um, 250um, etc.
[0042] Furthermore, the substrate of sensor 3 is glass, and ITO or Cu or Ag is used as a transparent conductive material, and a touch sensor capable of receiving and transmitting signals is prepared through processes such as yellow light.
[0043] Furthermore, the liquid crystal display module 4 may be a TFT liquid crystal display module, an IPS liquid crystal display module, or a flexible OLED display.
[0044] In actual use, the utility model makes the above-mentioned corresponding changes to the glass touch screen, which can greatly reduce the risk of short circuit and open circuit of the glass touch screen, increase the electrical test yield of the glass touch screen to more than 95%, and reduce the production cost.
[0045] As described above, the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, a person of ordinary skill in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features thereof may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the application.
Claims
1. A glass touch screen that prevents short circuits and disconnections. It is characterized in that It includes a cover plate, an adhesive, a sensor, an adhesive and a liquid crystal display module which are sequentially connected from top to bottom; The upper surface and the lower surface of the sensor are respectively provided with a first edge routing and a second edge routing, which are used to overlap with the conductive layer in the sensor to form a loop; the first edge routing and the second edge routing are respectively composed of a plurality of first routings and second routings overlapped and connected with the conductive layer, and the line spacing between two adjacent first routings is greater than the line width of each first routing, and the line spacing between two adjacent second routings is greater than the line width of each second routing; the materials of the first routing and the second routing are both made of wear-resistant components; The upper surface of the first edge wiring and the conductive layer on the upper surface of the sensor are respectively provided with a first transparent insulating layer and a second transparent insulating layer; The lower surface of the second edge wiring and the conductive layer on the lower surface of the sensor are respectively provided with a third transparent insulating layer and a fourth transparent insulating layer.
2. The glass touch screen that prevents short circuit and disconnection as claimed in claim 1, Features: The wear-resistant component comprises silver paste; and carbon paste is arranged on the upper surface of the silver paste.
3. The glass touch screen that prevents short circuit and disconnection as claimed in claim 2, Features: The overall thickness of the silver paste and the carbon paste is 10-20 um.
4. The glass touch screen that prevents short circuit and disconnection as claimed in claim 1, Features: The line width of the first edge routing and the second edge routing is 15um-20um, and the line spacing is 40um-45um.
5. The glass touch screen that prevents short circuit and disconnection as claimed in claim 1, Features: The first transparent insulating layer, the second transparent insulating layer, the third transparent insulating layer and the fourth transparent insulating layer are made of insulating ink.
6. The glass touch screen that prevents short circuit and disconnection as claimed in claim 1, Features: The light transmittance of the first transparent insulating layer, the second transparent insulating layer, the third transparent insulating layer and the fourth transparent insulating layer is 99.9%.
7. The glass touch screen that prevents short circuit and disconnection as claimed in claim 1, Features: The adhesive is solid optical transparent glue, liquid silicone water glue or acrylic water glue.
8. The glass touch screen that prevents short circuit and disconnection as claimed in claim 1, Features: The sensor is a touch sensor.