Steel mesh, printed circuit board and display panel
By using multiple steel mesh groups in the LED display screen to adjust the solder paste distribution, the Yin and Yang surface problems are solved, the symmetrical effect of the light-emitting element is achieved, and the display quality of the display panel is improved.
Patent Information
- Application Number
- CN202420684798.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-01
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-04-01
AI Technical Summary
There are problems with the yin and yang surface in the LED display screen, resulting in uneven display effect and affecting the display quality.
Design a steel mesh, including an open array arranged in multiple arrays, each of which contains four steel mesh groups, and by adjusting the position and offset of the steel mesh openings, ensure uniform distribution of solder paste on the printed circuit board. , reduce the inclination of the light emitting element and form a symmetrical light emitting effect.
By centrally distributing 50% of solder paste, 25% tilting in one direction and 25% tilting in the other direction, the light-emitting elements are consistently emitted from left and right, reducing the problem of yin and yang surfaces and improving the display quality of the display panel.
Smart Images

Figure CN222073529U_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of display technology, and specifically relates to a steel mesh, a printed circuit board and a display panel. Background Art
[0002] With the development of science and technology and the advancement of manufacturing technology, LED displays are also constantly improving and perfecting. We have entered a higher-end field and have higher and higher requirements for display effects.
[0003] The production process of LED display panels uses surface mount technology (SMT) to solder various components to the printed circuit board (PCB). The commonly used surface mount process is to first print solder paste on one side of the printed circuit board, and then mount the components to be soldered to the corresponding positions of the printed circuit board. After the components are mounted, reflow soldering (Dry and Ref low) is performed. In this way, the installation of components on one side of the printed circuit board is completed. After passing the inspection, the lamp bead surface can be installed in the same way.
[0004] However, there is a problem of yin and yang sides in the LED display industry that needs to be solved urgently. Utility Model Content
[0005] The purpose of the present application is to provide a steel mesh, a printed circuit board and a display panel, which can reduce the problem of positive and negative sides of the display panel.
[0006] In a first aspect, the present application provides a steel mesh, which is used to align with a printed circuit board and print solder paste onto the printed circuit board; the steel mesh comprises a steel mesh sheet, the steel mesh sheet comprises a plurality of array-arranged opening arrays, each of the opening arrays comprises a first steel mesh group, a second steel mesh group, a third steel mesh group and a fourth steel mesh group, the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group are all provided with steel mesh openings, the first steel mesh group and the second steel mesh group are arranged in sequence in a row direction, the first steel mesh group and the third steel mesh group are arranged in sequence in a column direction, the fourth steel mesh group and the second steel mesh group are arranged in sequence in the column direction, and the fourth steel mesh group and the third steel mesh group are arranged in sequence in the row direction;
[0007] Among them, the steel mesh openings of the second steel mesh group and the steel mesh openings of the third steel mesh group are aligned with the center of the pad of the printed circuit board, the center of the steel mesh openings of the first steel mesh group and the center of the steel mesh openings of the fourth steel mesh group are offset from the center of the pad of the printed circuit board in the horizontal direction, and the offset direction of the steel mesh openings of the first steel mesh group is opposite to the offset direction of the steel mesh openings of the fourth steel mesh group.
[0008] In an exemplary embodiment of the present application, the steel mesh opening areas of the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group are smaller than the pad area of the printed circuit board.
[0009] In an exemplary embodiment of the present application, the ratio of the steel mesh opening area to the pad area of the printed circuit board ranges from 80% to 95%.
[0010] In an exemplary embodiment of the present application, the steel mesh openings of the first steel mesh group are offset to the right in the horizontal direction, and the steel mesh openings of the fourth steel mesh group are offset to the left in the horizontal direction.
[0011] In an exemplary embodiment of the present application, the spacing between adjacent steel mesh openings in the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group is the same.
[0012] In an exemplary embodiment of the present application, the steel mesh opening areas of the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group are the same.
[0013] In an exemplary embodiment of the present application, the steel mesh further includes a steel mesh frame, and the steel mesh frame is arranged around the steel mesh sheet.
[0014] A second aspect of the present application provides a printed circuit board, comprising a light-emitting element and a pad group with solder paste printed using any one of the steel meshes described above, wherein the light-emitting element is soldered to the pad group with solder paste.
[0015] In another exemplary embodiment of the present application, the pads in the pad group have the same area.
[0016] A third aspect of the present application provides a display panel, comprising a backplane and a printed circuit board as described in any one of the above items, wherein the printed circuit board is arranged in the backplane.
[0017] The steel mesh, printed circuit board and display panel of the present application have at least the following beneficial effects:
[0018] The steel sheet includes a plurality of array-arranged opening arrays, each of which includes four steel mesh groups, namely the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group. The first steel mesh group is arranged in the same line with the second steel mesh group, the first steel mesh group is arranged in the same column with the third steel mesh group, the fourth steel mesh group is arranged in the same column with the second steel mesh group, and the fourth steel mesh group is arranged in the same line with the third steel mesh group; that is, the first steel mesh group and the fourth steel mesh group are arranged diagonally, and the second steel mesh group and the third steel mesh group are arranged diagonally. Among them, the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group are all provided with steel mesh openings, the steel mesh openings on the second steel mesh group and the third steel mesh group are aligned with the center of the pad on the printed circuit board, the center of the steel mesh openings on the first steel mesh group and the fourth steel mesh group are offset from the center of the pad on the printed circuit board in the horizontal direction, and the offset direction of the steel mesh openings of the first steel mesh group is opposite to the offset direction of the steel mesh openings of the fourth steel mesh group. By setting the above four steel mesh groups, when the steel mesh is used to form solder paste on the printed circuit board, 50% of the solder paste is normally centered, 25% of the solder paste is tilted in one direction, and the other 25% of the solder paste is tilted in another direction. When the light-emitting components are soldered on the printed circuit board, 50% of the light-emitting components will not tilt, 25% of the light-emitting components will tilt in one direction, and the other 25% of the light-emitting components will tilt in another direction. When the display panel is viewed from the entire surface, the light-emitting components of the display panel emit light uniformly from left to right, so as to reduce the yin and yang sides of the display panel product and improve the display quality of the display panel.
[0019] Other features and advantages of the present application will become apparent from the following detailed description, or may be learned in part by the practice of the present application.
[0020] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] The drawings herein are incorporated into the specification and constitute a part of the specification, illustrate embodiments consistent with the present application, and together with the specification are used to explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0022] Figure 1 A schematic diagram of the structure of the steel mesh provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application is shown;
[0023] Figure 2 A schematic diagram of the structure in which four steel mesh groups are arranged in the opening array provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application is shown;
[0024] Figure 3A schematic structural diagram showing a printed circuit board provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application having four pad groups;
[0025] Figure 4 A schematic diagram showing the structure of aligning a steel mesh with a printed circuit board provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application is shown;
[0026] Figure 5 A schematic diagram of the structure of printing solder paste into the opening of the steel mesh provided in the first embodiment, the second embodiment or the third embodiment of the present application is shown;
[0027] Figure 6 A schematic diagram of the structure of the light-emitting element provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application is shown;
[0028] Figure 7 A schematic diagram showing a structure in which the light emitting element provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application is shifted to the left;
[0029] Figure 8 It shows a schematic diagram of a structure in which the light-emitting element provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application is shifted to the right;
[0030] Fig. 9 A schematic diagram of the structure of the unaverted light emitting element provided in Embodiment 1, Embodiment 2 or Embodiment 3 of the present application is shown.
[0031] Description of reference numerals:
[0032] 100, steel mesh; 110, steel mesh sheet; 120, steel mesh frame; 130, opening array; 131, first steel mesh group; 132, second steel mesh group; 133, third steel mesh group; 134, fourth steel mesh group; 140, steel mesh opening;
[0033] 200, printed circuit board; 210, first pad group; 220, second pad group; 230, third pad group; 240, fourth pad group; 250, pad;
[0034] 300, solder paste; 400, light-emitting component. DETAILED DESCRIPTION
[0035] Example embodiments will now be described more fully with reference to the accompanying drawings. However, example embodiments can be implemented in a variety of forms and should not be construed as limited to the examples set forth herein; rather, these embodiments are provided so that this application will be more comprehensive and complete and fully convey the concept of the example embodiments to those skilled in the art.
[0036] In this application, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0037] In this application, unless otherwise clearly specified and limited, the terms "assembly", "connection" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0038] In addition, described feature, structure or characteristic can be combined in one or more embodiments in any suitable manner. In the following description, many specific details are provided to provide a full understanding of the embodiments of the present application. However, those skilled in the art will appreciate that the technical scheme of the present application can be put into practice without one or more of the specific details, or other methods, components, devices, steps, etc. can be adopted. In other cases, known methods, devices, realizations or operations are not shown or described in detail to avoid blurring the various aspects of the application.
[0039] Embodiment 1
[0040] Embodiment 1 of the present application provides a steel mesh 100, which is used to deposit semi-solid welding material, such as solder paste 300, onto a printed circuit board 200 to form a welding piece on the printed circuit board 200, and the welding piece is used to weld the pins of the light-emitting element 400 to the pads 250 of the printed circuit board 200 to form an LED backlight module and an LED display panel. The LED backlight module and the LED display panel are electrically connected to a power source to form a display device.
[0041] When the steel mesh 100 is used to deposit soldering material onto the printed circuit board 200, the solder paste 300 on the pad 250 is easily offset to the left or right, causing the light-emitting surface of the light-emitting element 400 to tilt to the left or right during subsequent soldering of the light-emitting element 400, thereby causing the display panel to form a positive and negative side problem.
[0042] To improve the yin-yang problem, see Figure 1 As shown, Figure 1A structural schematic diagram of a steel mesh 100 provided in an embodiment of the present application is shown. The embodiment of the present application proposes a steel mesh 100, which includes a steel mesh sheet 110 and a steel mesh frame 120. The steel mesh frame 120 is arranged around the steel mesh sheet 110, which can ensure the stability of the steel mesh sheet 110, avoid damage to the steel mesh sheet 110, and facilitate taking.
[0043] Among them, see Figure 2 As shown, Figure 2 The schematic diagram of the structure of the opening array 130 provided in the embodiment of the present application is shown; the steel mesh sheet 110 includes a plurality of array-arranged opening arrays 130, and each opening array 130 includes four steel mesh groups, namely, the first steel mesh group 131, the second steel mesh group 132, the third steel mesh group 133, and the fourth steel mesh group 134. The first steel mesh group 131, the second steel mesh group 132, the third steel mesh group 133, and the fourth steel mesh group 134 are all provided with steel mesh openings 140, and the steel mesh openings 140 can be cut by laser equipment according to the opening size of the pad 250 group on the printed circuit board 200 and the position of the pad 250 group.
[0044] In the examples of this application, see Figure 2 As shown, the first steel mesh group 131 and the second steel mesh group 132 are sequentially arranged in the row direction, the first steel mesh group 131 and the third steel mesh group 133 are sequentially arranged in the column direction, the fourth steel mesh group 134 and the second steel mesh group 132 are sequentially arranged in the column direction, and the fourth steel mesh group 134 and the third steel mesh group 133 are sequentially arranged in the row direction; that is, the first steel mesh group 131 and the fourth steel mesh group 134 are diagonally arranged, and the second steel mesh group 132 and the third steel mesh group 133 are diagonally arranged, as shown in FIG. Figure 2 shown.
[0045] Please note that, see Figures 2 to 4 As shown, the center of the steel mesh opening 140 of the first steel mesh group 131 is offset in the horizontal direction from the center of the pad 250 of the first pad group 210 of the printed circuit board 200; that is, when printing solder paste 300 into the pad 250 of the first pad group 210, the solder paste 300 is unevenly distributed in the pad 250, and the solder paste 300 on one side will be more than the solder paste 300 on the other side.
[0046] See also Figures 2 to 4As shown, the steel mesh openings 140 of the second steel mesh group 132 and the steel mesh openings 140 of the third steel mesh group 133 are aligned with the centers of the second pad group 220 and the pads 250 of the third pad group 230 of the printed circuit board 200; that is, the centers of the steel mesh openings 140 of the second steel mesh group 132 and the steel mesh openings 140 of the third steel mesh group 133 and the centers of the pads 250 of the second pad group 220 and the third pad group 230 of the printed circuit board 200 are located on the same vertical line, that is, when the solder paste 300 is printed in the second pad group 220 and the third pad group 230, the solder paste 300 is evenly distributed in the pads 250 and is not easily offset.
[0047] See also Figures 2 to 4 As shown, the center of the steel mesh opening 140 of the fourth steel mesh group 134 is offset in the horizontal direction from the center of the pad 250 of the fourth pad group 240 of the printed circuit board 200; that is, when printing solder paste 300 into the pad 250 of the fourth pad group 240, the solder paste 300 is unevenly distributed in the pad 250, and the solder paste 300 on one side will be more than the solder paste 300 on the other side.
[0048] Moreover, the offset direction of the steel mesh opening 140 of the first steel mesh group 131 is opposite to the offset direction of the steel mesh opening 140 of the fourth steel mesh group 134; that is, the offset direction of the solder paste 300 of the pad 250 in the first pad group 210 is opposite to the offset direction of the solder paste 300 of the pad 250 in the fourth pad group 240, thereby making the light-emitting surface of the light-emitting element 400 have a different offset direction when the light-emitting element 400 is subsequently welded.
[0049] For an example, see Figure 4 As shown, the steel mesh openings 140 of the first steel mesh group 131 are horizontally offset to the right, and the steel mesh openings 140 of the fourth steel mesh group 134 are horizontally offset to the left, and the horizontal rightward offset amount of the steel mesh openings 140 of the first steel mesh group 131 is the same as the horizontal leftward offset amount of the steel mesh openings 140 of the fourth steel mesh group 134, so as to ensure that the offset angles of the subsequently formed light-emitting elements 400 are the same, so that the light emission on the left and right sides is consistent, thereby improving the problem of the positive and negative sides of the display panel and improving the display quality of the display panel.
[0050] By forming two steel mesh groups with opposite offsets and two steel mesh groups with normal settings in one opening array 130, 50% of the normal designs, 25% of the designs offset to the right, and 25% of the designs offset to the left exist on the entire steel mesh 100. Figure 5As shown, the above steel mesh 100 is used to print the welding material, and 50% of the normally set solder paste 300, 25% of the solder paste 300 offset to the right, and 25% of the solder paste 300 offset to the left are formed on the printed circuit board 200. After the solder paste 300 is printed, the light-emitting element 400 is mounted and reflow soldered to obtain an LED backlight module. In the LED backlight module formed by soldering using the above solder paste 300, 50% of the light-emitting elements 400 have a light-emitting surface that is left, right, or not tilted, 25% of the light-emitting elements 400 have a light-emitting surface that is offset to the left, and 25% of the light-emitting elements 400 have a light-emitting surface that is offset to the right. When the display panel is lit, because the human eye has a strong sense of the entire surface (100%) of the light-emitting element 400 emitting to the left or right, and the light-emitting sense of the light-emitting element 400 (25% and 75%) is opposite, the user's eye light sense is weak after superposition, thereby reducing the yin and yang sides of the display panel and improving the display quality.
[0051] In the embodiment of the present application, the area of the steel mesh openings 140 of the first steel mesh group 131, the second steel mesh group 132, the third steel mesh group 133 and the fourth steel mesh group 134 is smaller than the area of the pads 250 of the printed circuit board 200. This ensures that the welding material can be completely injected into the pads 250 to avoid the waste of welding material, and also prevents the solder paste 300 between adjacent pads 250 from adhering to each other and forming a short circuit problem.
[0052] In the embodiments of the present application, Figure 4 As shown, the ratio of the area of the opening 140 of the steel mesh to the area of the pad 250 of the printed circuit board 200 ranges from 80% to 95%, for example, 80%, 85%, 90%, 95%. When the steel mesh 100 is used to print the solder paste 300, the solder paste 300 will be in the pad 250 of the printed circuit board 200. When the light-emitting element 400 is soldered, the solder paste 300 in the printed circuit board 200 will be in a molten state. The surface tension of the solder paste 300 in the molten state is small, which reduces the pulling force on the light-emitting element 400 and reduces the angle of the light-emitting element 400 offset, thereby further reducing the yin and yang colors of the display panel.
[0053] In the embodiment of the present application, the spacing between adjacent steel mesh openings 140 in the first steel mesh group 131, the second steel mesh group 132, the third steel mesh group 133 and the fourth steel mesh group 134 is the same, so as to ensure that the spacing between the solder paste 300 formed in the pad 250 group is the same, and when the light emitting elements 400 are subsequently formed, the spacing between adjacent light emitting elements 400 is the same, so as to ensure display uniformity.
[0054] In the embodiment of the present application, the stencil openings 140 of the first stencil group 131, the second stencil group 132, the third stencil group 133 and the fourth stencil group 134 are of the same size, and when the stencil openings 140 are formed, they can be formed together by a laser device, thereby reducing the manufacturing cost. In addition, since the stencil openings 140 of the four stencil groups are of the same size, the amount of solder paste printed in the four stencil groups is ensured to be the same, thereby avoiding waste of solder paste.
[0055] In addition, the orthographic projections of the steel mesh openings 140 of the first steel mesh group 131 and the fourth steel mesh group 134 on the printed circuit board 200 are located inside the pads 250 of the pad 250 group, so as to avoid the solder paste 300 being printed outside the pads 250 when printing the solder paste 300, and to avoid the problem of adjacent solder pastes 300 being connected and causing a short circuit between subsequent adjacent light-emitting elements 400, thereby ensuring the display effect. The orthographic projections of the steel mesh openings 140 of the second steel mesh group 132 and the third steel mesh group 133 on the printed circuit board 200 overlap with the pads 250 of the pad 250 group or are located inside the pads 250, so as to avoid the problem of adjacent solder pastes 300 being adhered and causing a short circuit between subsequent adjacent light-emitting elements 400.
[0056] Embodiment 2
[0057] Embodiment 2 of the present application provides a printed circuit board 200, such as Figures 6 to 9 As shown, the printed circuit board 200 includes a light-emitting element 400 and a group of pads 250 printed with welding material using the steel mesh 100 described in any one of the first embodiments. When the solder paste 300 is printed on the group of pads 250 using the steel mesh 100, the solder paste 300 is offset to the left and right directions at the same proportion, thereby causing the light-emitting element 400 to be offset to the left and right directions at the same proportion during welding, so that the LED display panel emits light uniformly on the left and right sides, which can reduce the positive and negative sides of the display panel and improve the quality of the display panel.
[0058] For example, Figures 7 to 9As shown, when the steel mesh opening 140 on the steel mesh 100 corresponds to the pad 250 group, solder paste 300 is added to the pad 250 group. The solder paste 300 on the first pad group 210 corresponding to the first steel mesh group 131 is fixedly offset to the right, the solder paste 300 on the second pad group 220 and the third pad group 230 corresponding to the second steel mesh group 132 and the third steel mesh group 133 is fixedly offset to the left, and the solder paste 300 printing is offset to the right by 25%, the solder paste 300 printing is centered by 50%, and the solder paste 300 printing is offset to the left by 25%. After the light-emitting element 400 is mounted, it is reflow soldered with the solder paste 300 on the pad 250 group to obtain a backlight module. Among them, the light-emitting surface of the first light-emitting element 400 corresponding to the first pad group 210 will tilt to the left, the light-emitting surfaces of the second light-emitting element 400 and the third light-emitting element 400 corresponding to the second pad group 220 and the third pad group 230 will tilt to the left / right or not tilt, and the light-emitting surface of the fourth light-emitting element 400 corresponding to the fourth pad group 240 will tilt to the right. When the entire backlight module is lit, the user's eyes will have a strong sense of the light source's entire surface (100%) of the light-emitting elements 400 emitting light to the left or right, and a weak sense of the light-emitting elements 400 (25% and 75%). After superposition, the user's eyes will have a weak sense of light, which can reduce the yin and yang sides of the display panel and improve the display quality.
[0059] It is worth mentioning that the pads 250 in each pad 250 group in the printed circuit board 200 have the same area, so that each pad 250 receives the same amount of solder paste 300.
[0060] Embodiment 3
[0061] Embodiment 3 of the present application provides a display panel, which includes a backplane and a printed circuit board 200 described in embodiment 2, wherein the printed circuit board 200 is disposed in the backplane.
[0062] According to the embodiments of the present application, the specific type of the display panel is not particularly limited, and any display panel type commonly used in the art can be used, such as liquid crystal display screens, mobile phones, laptop computers and other mobile devices, wearable devices such as watches, VR devices, etc. Those skilled in the art can make corresponding choices based on the specific purpose of the display device, which will not be repeated here.
[0063] In the description of this specification, the description with reference to the terms "some embodiments", "exemplarily", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0064] Although the embodiments of the present application have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations on the present application. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present application. Therefore, any changes or modifications made in accordance with the claims and description of the present application should fall within the scope of the patent of this application.
Claims
1. A steel mesh, the steel mesh is used to align with a printed circuit board and print solder paste onto the printed circuit board; characterized in that: The steel mesh comprises a steel mesh sheet, the steel mesh sheet comprises a plurality of array-arranged opening arrays, each of the opening arrays comprises a first steel mesh group, a second steel mesh group, a third steel mesh group and a fourth steel mesh group, the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group are all provided with steel mesh openings, the first steel mesh group and the second steel mesh group are sequentially arranged in a row direction, the first steel mesh group and the third steel mesh group are sequentially arranged in a column direction, the fourth steel mesh group and the second steel mesh group are sequentially arranged in the column direction, and the fourth steel mesh group and the third steel mesh group are sequentially arranged in the row direction; Among them, the steel mesh openings of the second steel mesh group and the steel mesh openings of the third steel mesh group are aligned with the center of the pad of the printed circuit board, the center of the steel mesh openings of the first steel mesh group and the center of the steel mesh openings of the fourth steel mesh group are offset from the center of the pad of the printed circuit board in the horizontal direction, and the offset direction of the steel mesh openings of the first steel mesh group is opposite to the offset direction of the steel mesh openings of the fourth steel mesh group.
2. The steel mesh according to claim 1, characterized in that: The steel mesh opening areas of the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group are smaller than the pad area of the printed circuit board.
3. The steel mesh according to claim 2, characterized in that: The ratio of the steel mesh opening area to the pad area of the printed circuit board is in a range of 80% to 95%.
4. The steel mesh according to claim 2 or 3, characterized in that: The steel mesh openings of the first steel mesh group are offset to the right in the horizontal direction, and the steel mesh openings of the fourth steel mesh group are offset to the left in the horizontal direction.
5. The steel mesh according to claim 1, characterized in that: The spacing between adjacent steel mesh openings in the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group is the same.
6. The steel mesh according to claim 2, characterized in that: The steel mesh opening areas of the first steel mesh group, the second steel mesh group, the third steel mesh group and the fourth steel mesh group are the same.
7. The steel mesh according to claim 1, characterized in that: The steel mesh also includes a steel mesh frame, and the steel mesh frame is arranged around the steel mesh sheet.
8. A printed circuit board, characterized in that: The printed circuit board comprises a light-emitting element and a pad group printed with solder paste using the steel screen according to any one of claims 1 to 7, and the light-emitting element is soldered on the pad group with solder paste.
9. The printed circuit board according to claim 8, characterized in that: The pads in the pad group have the same area.
10. A display panel, characterized in that: The display panel comprises a backplane and a printed circuit board according to any one of claims 8 to 9, wherein the printed circuit board is arranged in the backplane.