Reaction sintering silicon carbide ceramic impeller

By setting a second cavity in the blade and reinforcing with adhesive, and setting a front liner on the impeller profile, the problem of large-scale and insufficient reliability of the reactive sintered silicon carbide ceramic impeller is solved, and the impact resistance of the impeller is improved Performance and mechanical strength.

CN222084779UActive Publication Date: 2024-11-29湖南省拓道新材料科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420823733.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-19
Publication Date
2024-11-29
Estimated Expiration
2034-04-19

AI Technical Summary

Technical Problem

The prior art cannot effectively scale up and improve the reliability and impact resistance of the reactive sintered silicon carbide ceramic impeller, resulting in low yield and insufficient mechanical strength, especially in large impeller manufacturing.

Method used

A second cavity is provided in the blade to uniformize the thickness and density, a adhesive is used to fill the cavity to reinforce, and a front liner is provided on the impeller profile to enhance impact resistance, forming a high-strength frame structure and reducing residuals Stress and hidden cracks.

Benefits of technology

The actual mechanical strength and impact resistance of the reactive sintered silicon carbide ceramic impeller are significantly improved, the probability and cost of fracture are reduced, and the high reliability and wear resistance of large impellers are achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222084779U_ABST
    Figure CN222084779U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of functional ceramic materials, and particularly discloses a reaction sintering silicon carbide ceramic impeller which comprises a hub and a plurality of ceramic impeller bodies arranged on the hub, and the ceramic impeller bodies are arranged in a circumferential mode. Each ceramic impeller body comprises a front plate, a rear plate and a blade which are sintered into a whole, and a second cavity extending to the outlet direction of the impeller along the working surface of the blade is formed in the blade; and a second framework is arranged in the second cavity. Through the arrangement, the reaction sintering silicon carbide ceramic impeller disclosed by the utility model can realize large scale, and is better in structural performance and higher in reliability at the same time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of functional ceramic materials, and more specifically relates to a reaction-sintered silicon carbide ceramic impeller. Background Art

[0002] The impeller of a slurry pump is the most severely worn component of a slurry pump, and is generally made of wear-resistant alloy or wear-resistant rubber. However, in some working conditions with severe wear, wear-resistant alloy impellers and wear-resistant rubber impellers often cannot meet the use requirements. In order to increase the life of the impeller, silicon carbide ceramic materials with good wear resistance are currently being tried to be used to make the impeller. Depending on the process and raw materials, common silicon carbide ceramics mainly include pressureless sintered silicon carbide, hot-pressed sintered silicon carbide, reaction-sintered silicon carbide, silicon nitride combined with silicon carbide, and oxide combined with silicon carbide. Among them, pressureless sintered silicon carbide and hot-pressed sintered silicon carbide can only manufacture some simple-shaped workpieces due to the complex molding and sintering processes, and cannot manufacture complex large parts such as slurry pump impellers; the latter three can be formed by casting or grouting processes, so they can manufacture workpieces with complex shapes. At present, almost all silicon carbide ceramic impellers are made of the latter three materials.

[0003] Silicon nitride bonded with silicon carbide and oxide bonded with silicon carbide can be cast, which is easy to manufacture workpieces with complex shapes such as impellers. The basic production process of silicon nitride bonded with silicon carbide and oxide bonded with silicon carbide is: mix α-SiC particles with metal silicon powder, binder, water, etc. evenly, inject into the mold for molding, demold and dry; heat the blank to 1420℃ under high-purity nitrogen, then the metal silicon powder and nitrogen in the blank react to form silicon nitride, and finally obtain silicon nitride bonded with silicon carbide; place the blank in oxygen or air and heat to 1420℃, then the metal silicon powder and oxygen in the blank react to form silicon oxide, and finally obtain oxide bonded with silicon carbide. The porosity of silicon nitride bonded with silicon carbide is generally 8%-15%, and the α-Si C content is generally 65%-80%. The flexural strength is generally 30-60Mpa. The porosity of oxide bonded with silicon carbide is generally 15%-20%, and the α-Si C content is generally 75%-85%. The flexural strength is generally 20-30Mpa.

[0004] Reaction-bonded silicon carbide ceramics generally refer to reaction-bonded silicon carbide. There is also reaction-formed silicon carbide, sometimes also called reaction-bonded silicon carbide, that is, the material is all β-SiC generated by carburization reaction, but this material has poor processability and high cost, and there is no report of its commercial application in manufacturing impellers. When manufacturing workpieces with complex shapes such as impellers, they are all reactively bonded silicon carbide, and grouting molding is generally used. The manufacturing process is: raw materials containing α-SiC micropowder and carbon black micropowder are added with water, a binder, a dispersant, etc., and mixed evenly to form a slurry, which is then injected into the cavity of a gypsum mold (or other water-absorbing mold). The gypsum mold absorbs the water in the slurry. After the slurry loses some of its water, the binder gives the blank a certain strength. The gypsum mold is removed to obtain the blank. After the ceramic blank is dried, the blank and excess metallic silicon particles are stacked in a reactive sintering furnace, and the temperature is raised to about 800°C in a vacuum or inert gas. The binder and the dispersant are completely carbonized. The temperature is further raised to 1500-1700°C, and the metallic silicon is liquefied or vaporized. Under the action of capillaries, it penetrates into the blank and reacts with the carbon in the blank to form β-SiC, and the α-SiC in the blank is formed. C powder is combined together, and the excess metallic silicon fills the pores in the blank at the same time. After cooling, a ceramic material with very low porosity (generally less than 0.1%) is obtained, and the main components are silicon carbide (generally α-SiC+β-SiC content is 85-93%) and free silicon (also called residual silicon, generally 7-15%). Reaction-sintered silicon carbide not only has much higher wear resistance than silicon nitride combined with silicon carbide and oxide combined with silicon carbide, but also has much higher mechanical strength than the latter two. Generally, the bending strength can reach 250-500Mpa. Therefore, the impeller made of reaction-sintered silicon carbide should be significantly better than that of silicon nitride combined with silicon carbide and oxide combined with silicon carbide in terms of wear resistance and strength. However, the actual situation is not the case. The impeller using the latter two materials can currently achieve a diameter of about 1700mm, and its reliability can meet the use requirements. The reaction-sintered silicon carbide impeller manufactured by conventional technology can only achieve a diameter of about 500mm; for example, China's authorized utility model patent (authorization announcement number is CN209687784U) discloses "an integral ceramic impeller". At present, some models of silicon carbide ceramic impellers manufactured according to this technical solution have been put into commercial use. However, the current successful market use is limited to some small models and their diameters generally do not exceed 500mm. When manufacturing reaction-sintered silicon carbide impellers with larger diameters, it is found that the yield rate is very low, which leads to a sharp increase in costs, and the manufactured impellers have poor impact resistance. Not only are they prone to rupture when used under strong impact conditions, but the probability of rupture is also high under slight impact conditions.

[0005] In order to solve the problem that the impeller is difficult to enlarge, the Chinese authorized utility model patent (authorization announcement number is CN209687784U) also discloses another ceramic impeller. The invention concept of this ceramic impeller is to split the large ceramic impeller into several easy-to-manufacture parts for separate manufacturing, and then splice these parts into one. In practice, it is found that when this technical solution is used to manufacture large impellers, if the ceramic material is silicon nitride combined with silicon carbide or oxide combined with silicon carbide, under the current process technology conditions, larger impellers can indeed be manufactured; the maximum impeller diameter can currently be about 1700mm; but if the ceramic material is reaction-sintered silicon carbide, when the impeller is enlarged, especially when the impeller diameter exceeds 700mm, there are still problems that the impeller is easy to break and the yield is low, and the mechanical strength and reliability of the impeller are much lower than those of silicon nitride combined with silicon carbide impellers or oxide combined with silicon carbide impellers.

[0006] In view of the above problems, technicians naturally thought of increasing the thickness of impeller-related parts to improve the strength of the impeller. For example, the

[0063] paragraph in the Chinese authorized utility model patent (authorization announcement number CN209687784U) points out that increasing the thickness of the blades can improve the strength of the impeller. This is consistent with the experience of ordinary technicians. Therefore, in the design, the front cover plate, Rear cover Or the thickness of the blades, which is often designed to reach 70-120mm. Our further research found that this experience should be correct for other ceramics, such as silicon nitride bonded to silicon carbide, oxide bonded to silicon carbide, alumina ceramics, etc., and the expected effect can be achieved after thickening; but for reaction-sintered silicon carbide, this is not always the case. In many cases, the reliability of the impeller after thickening has not been improved, and there have even been many contrary cases. Through further calculations, it can be found that the theoretical strength of these reaction-sintered silicon carbide impellers that have been broken during use is not only much greater than that of silicon nitride bonded to silicon carbide or oxide bonded to silicon carbide, but the strength safety factor is also much greater than the actual requirements of the impeller.

[0007] Through in-depth research on this phenomenon, it was found that for silicon nitride-bonded silicon carbide ceramics and oxide-bonded silicon carbide ceramics, due to their high porosity, these tiny pores can greatly reduce the internal stress generated during the ceramic sintering process and absorb the stress caused by external impact. Therefore, the residual stress of the workpiece is small, and the front cover plate, Rear cover After the blades are thickened, the mechanical strength of the impeller can be improved accordingly.

[0008] Through research, it is also found that: since reaction sintered silicon carbide is currently formed by grouting with a plaster mold or other water-absorbing mold, the surface of the workpiece is in contact with the mold during grouting, and the water in the slurry is quickly absorbed. However, the water content of the part far from the mold inside the workpiece is significantly higher than that of the workpiece surface at the end of molding due to the relatively weak capillary action of the mold, which makes the density of the surface of the blank after drying significantly higher than that of the inside of the blank. After the carbonization reaction is completed during sintering, the excess metal silicon liquid will fill the gaps between the silicon carbides, so that the free silicon content of the part with higher density of the blank after sintering will be lower than that of the part with lower density of the blank, that is, the free silicon content of the workpiece surface will be lower than that of the inside of the workpiece. According to the normal process of the prior art, the free silicon content of the surface can be controlled at 8-12%, and the further away from the surface, the higher the free silicon content, and the free silicon content of the core can reach 15-18%. Free silicon not only reduces wear resistance and bending strength, but more importantly, it increases the brittleness of the ceramic and reduces impact resistance. Therefore, in production, efforts are generally made to increase the density of the blank to reduce the free silicon content of the product. However, in production practice, improving the density of the blank is restricted by various factors, and the existing gypsum mold grouting molding technology is difficult to significantly improve the density and consistency of the blank. Therefore, for impellers with smaller diameters, such as impellers with a diameter of 500mm, the thickness of the blades and cover plates generally does not exceed 50mm. At this time, appropriately increasing the thickness of the blades or cover plates has a relatively small effect on the density of the impeller blank, which is an important reason for the relatively high reliability of small reaction-sintered silicon carbide impellers. However, for large impellers, for strength and wear resistance considerations, the thickness of the blades and cover plates is often designed to be 80-120mm. At this time, the density of the cast impeller blank is quite different, which will lead to large differences in the microstructure of the ceramic organization after sintering. In some cases, the so-called silicon core even appears, and the free silicon content in the center is close to 100%, which will cause the workpiece to produce large residual stress when cooling after sintering; the greater the thickness of the workpiece and the larger the outer dimensions, the greater the residual stress. Unlike silicon nitride bonded silicon carbide or oxide bonded silicon carbide ceramics which have a large number of pores, the porosity of reaction-sintered silicon carbide ceramics is close to zero, so the stress generated by sintering cannot be eliminated through the pores. Therefore, for thicker workpieces, under the same external dimensions, the residual stress of reaction-sintered silicon carbide workpieces is much greater than that of silicon nitride bonded silicon carbide and oxide bonded silicon carbide. On the one hand, the larger residual stress causes the workpiece to break or produce hidden cracks during the sintering process, which reduces the yield of the product. On the other hand, it causes the workpiece to have a larger residual stress, which is easy to break from the part with greater stress when subjected to external force or impact. Therefore, for reaction-sintered silicon carbide impellers, increasing the thickness of the blades or cover plates does not necessarily increase the strength and impact resistance of the impeller, and sometimes it may even be counterproductive.

[0009] Therefore, through the above research, it is found that the main or important reason why the existing technology cannot achieve large-scale and high reliability of reaction-sintered silicon carbide ceramic impellers is precisely the key to solving the problem. Utility Model Content

[0010] In order to solve the deficiencies and shortcomings of the prior art, the purpose of the utility model is to provide a reaction-sintered silicon carbide ceramic impeller.

[0011] The technical solution of the utility model for solving the problems of the prior art is:

[0012] A reaction-sintered silicon carbide ceramic impeller comprises a hub and a plurality of ceramic impeller bodies arranged on the hub, wherein the plurality of ceramic impeller bodies are arranged in a circumference; each ceramic impeller body comprises a front plate sintered into one body, Back panel and a blade, wherein a second cavity extending along the working surface of the blade toward the impeller outlet is arranged in the blade; and a second skeleton is arranged in the second cavity.

[0013] Among them, a second cavity is provided in the blade and extends along the working surface of the blade toward the impeller outlet. The plaster mold corresponding to the second cavity can prevent the distance between the core of the blade and the surface of the plaster mold from being too large during molding, so that the thickness of each part of the blade is relatively uniform, thereby reducing the density difference of the blank, making the residual silicon content in the ceramic impeller body after sintering relatively uniform, and the residual internal stress is small, thereby reducing the probability of the ceramic impeller body breaking. Since the reaction-sintered silicon carbide ceramic has a very high bending strength, after the second cavity is set, although the theoretical mechanical strength calculated by the ceramic impeller body will decrease, the theoretical mechanical strength calculation cannot take into account the influence of residual stress, and the filling adhesive reinforces the second cavity. Therefore, the mechanical strength of the ceramic impeller body of the utility model is actually significantly improved compared with the scheme without the second cavity, and its impact resistance is also significantly improved.

[0014] Preferably, the Back panel A first cavity is provided on the upper surface, in which a first skeleton is installed; the first skeleton is connected to a second skeleton in the second cavity; the torque of the main shaft is transmitted to the ceramic impeller body through the first skeleton, and after the second skeleton is combined with the adhesive, the second skeleton can be prevented from escaping from the second cavity.

[0015] Preferably, the first skeleton is far away from the Back panel A rear lining plate is arranged on one side; a groove is arranged on the front plate of the ceramic impeller body. After the ceramic impeller body is assembled, the grooves are assembled to form a third cavity, and a front lining plate made of ceramic material is arranged in the third cavity.

[0016] Preferably, the first cavity, the second cavity and the third cavity penetrate each other.

[0017] The purpose is that after the mutually interpenetrating first cavity, second cavity and third cavity are filled with adhesive, the hardened adhesive can form a high-strength frame that penetrates most of the impeller and completely fits the impeller body and has a certain toughness, thereby enhancing the overall strength of the ceramic impeller.

[0018] Preferably, the first cavity, the second cavity and the third cavity are filled with an adhesive to bind the first frame, the second frame, the front plate, Back panel , the blade, the front lining plate, and the rear lining plate are bonded into a whole;

[0019] The purpose is to solve the problem that for a larger reaction-sintered silicon carbide ceramic impeller body, there may be defects such as hidden cracks and local stress concentration. When the first skeleton, the second skeleton and the ceramic impeller body are bonded together with an adhesive, the hidden cracks will be reinforced, thereby reducing the probability of the ceramic impeller body breaking from the stress concentration point. The probability of hidden cracks in the front liner of ceramic material is much smaller than that of the ceramic impeller body due to its small size. When the front liner is bonded together with the ceramic impeller body in the third cavity, the probability of hidden cracks in the same direction in the same place of the ceramic impeller body and the front liner on the front cover will be greatly reduced. Therefore, the above structure will greatly improve the reliability of the reaction-sintered silicon carbide impeller.

[0020] Preferably, the depth of the third cavity is 25%-75% of the thickness of the front cover plate, and the front cover plate includes a front plate and a front lining plate.

[0021] When the third cavity is too deep, the strength or wear resistance of the ceramic impeller body at the front cover plate will be insufficient. Conversely, if the thickness of the ceramic impeller body at the front cover plate is too thick, a large area of ​​thicker area will be formed at the front cover plate, causing the workpiece to have a reduced impact resistance due to greater residual stress. When the depth of the third cavity is 25%-75% of the thickness of the front cover plate, the above contradiction can be better balanced.

[0022] Since the front cover of large impellers is thicker, often reaching 60mm-100mm, for large impellers with thicker front cover, if the third cavity is not provided, the thickness of the front cover will be significantly higher than the blade or Rear cover, which makes the density of the blank after grouting very different, and will produce large residual stress after sintering, increasing the probability of hidden cracks or ruptures in the ceramic impeller body and reducing the impact resistance of the impeller. After setting the third cavity, the thickness of the ceramic impeller body at the front cover plate can be reduced, thereby reducing the residual stress of the ceramic impeller body. Since the bending strength of the reaction-sintered silicon carbide ceramic material is very high, the theoretical strength of the large impeller designed according to the existing technology is much higher than the actual need, but in actual use, the main reason for the low reliability of large ceramic impellers is that it is difficult to consider the influence of residual stress in theoretical calculations, and this factor has a great impact on the results. When the front liner and the ceramic impeller body are bonded, on the one hand, the residual stress at the front cover plate is significantly reduced due to the reduction in thickness, and on the other hand, the probability of the hidden cracks at the front cover plate of the ceramic impeller body and the hidden cracks and stress concentration parts on the front liner overlap is very low, thereby blocking the transmission of residual stress, and the influence of residual stress on the impeller strength is much smaller. Therefore, after the front lining plate and the third cavity are provided, although the theoretical strength of the front cover plate portion is not improved, and may even be reduced, its actual strength and impact resistance are significantly improved.

[0023] In addition, since the weight and size of the front liner are much smaller than the ceramic impeller body and the shape is simple, the front liner can be made of ceramic materials with better impact resistance and wear resistance, such as pressureless sintered silicon carbide, hot-pressed silicon nitride ceramics, etc., at an appropriate cost increase, which can further improve the reliability and life of the impeller. At the same time, the front liner can protect the joint line between the ceramic impeller body it covers from erosion and reduce the rapid wear of the adhesive between the joint lines, thereby further improving the life and reliability of the impeller.

[0024] Preferably, the length of the second cavity extending along the working surface of the blade toward the impeller outlet is 30%-80% of the length of the blade. When the length of the second cavity is too long, the head and tail of the blade will be too thin, resulting in insufficient wear resistance of the blade. Otherwise, the blade will have more areas with larger thickness, resulting in a large density difference of the blank after grouting, a large overall stress after sintering, and poor impact resistance of the impeller. According to the size of the impeller and the shape of the blade, when the extension length of the second cavity along the working surface of the blade toward the impeller outlet is set to 30%-80% of the length of the blade, the above contradiction can be better balanced.

[0025] Preferably, the width of the second cavity is 20%-50% of the average thickness of the blade.

[0026] Through the above arrangement, when the average width of the second cavity is too small, the mold corresponding to the second cavity is also thinner, resulting in insufficient water absorption capacity or insufficient strength of the mold, which in turn will cause large density differences in the blade portion of the blank, resulting in greater residual stress in the impeller after sintering; conversely, the flow surface of the blade portion will be too thin and its wear resistance will be significantly reduced. When the average width of the second cavity is 20%-50% of the average width of the blade, the above contradiction can be better balanced.

[0027] Preferably, a surface of the second cavity is partially configured as an equidistant surface of a blade working surface or a blade back surface, and an area of ​​the equidistant surface is greater than or equal to 40% of an area of ​​the second cavity.

[0028] Since the organizational structure between the equidistant surfaces is the most uniform, when the second cavity is provided with equidistant surfaces on the working surface or / and the back of the blade, the residual internal stress after sintering will be smaller, which is beneficial to improve the impact strength of the impeller. However, since the surface of the blade is a complex curved surface, it is not only difficult to achieve the surface of the second cavity strictly as an equidistant surface in its geometric sense in terms of technology, but also unnecessary in practice. Experiments show that when the difference between the distance from a certain surface of the second cavity to the working surface or back of the blade and the distance from another surface to the working surface or back of the blade is less than 20%, the residual stress caused by uneven thickness after sintering is not much different from the complete equidistant, so it can be recognized in technology that the two are equidistant surfaces. When the area of ​​the equidistant surface in the second cavity is greater than or equal to 40% of its total area, the effect of reducing residual stress and improving impact resistance can be achieved.

[0029] Preferably, a third skeleton is provided in the third cavity; its purpose is that, since a metal material with almost no residual stress can be used, hidden cracks in the front lining plate and the ceramic impeller body at the front cover plate position can be strengthened, thereby improving the reliability and life of the impeller.

[0030] Preferably, a sealing cone surface is provided on the impeller suction port side of the ceramic impeller body, and the distance from the inner edge of the third cavity to the sealing cone surface is 5mm-50mm;

[0031] The front cover plate suction port is severely worn due to the scouring of the slurry leaking from the high-pressure area to the inlet. Therefore, a sealing cone with a concave angle of 15°-30° is often designed at the suction port to improve the cavitation performance. The sealing cone at the suction port is the part of the front cover plate that is most severely scoured by the leaking slurry. The third cavity designed on the side of the front cover plate can avoid the formation of sharp-angled joint lines on or near the sealing cone surface, thereby improving the wear resistance and impact resistance of the joint part of the sealing cone surface. When the inner edge of the third cavity is too small from the inner edge of the suction port, the strength and life of the suction port are easily affected. When the distance is too large, it is easy to form a too thick area at this part, resulting in a large difference in the density of the cast impeller blank and a large residual stress in the impeller body after sintering. When the distance is 30-80mm, the above contradictions can be better balanced.

[0032] Compared with the prior art, the utility model has the following beneficial effects:

[0033] 1. The reaction-sintered silicon carbide ceramic impeller of the utility model is provided with a second cavity extending along the working surface of the blade toward the impeller outlet. The plaster mold corresponding to the second cavity can prevent the distance between the core of the blade and the surface of the plaster mold from being too large during molding, so that the thickness of each part of the blade is relatively uniform, thereby reducing the density difference of the blank, making the residual silicon content in the ceramic impeller body after sintering relatively uniform, and the residual internal stress is small, thereby reducing the probability of the ceramic impeller body breaking. Since the reaction-sintered silicon carbide ceramic has a very high bending strength, after the second cavity is set, although the theoretical mechanical strength of the ceramic impeller body will decrease, the theoretical mechanical strength calculation cannot consider the influence of residual stress, and the filling adhesive reinforces the second cavity. Therefore, the actual reliability of the ceramic impeller body of the utility model will be significantly improved compared with the scheme without the second cavity, and its impact resistance is also significantly improved.

[0034] 2. The reaction-sintered silicon carbide ceramic impeller of the utility model can be large-scaled, and has better structural performance and higher reliability.

[0035] 3. The reaction-sintered silicon carbide ceramic impeller of the present invention is composed of multiple ceramic impeller bodies. In this way, the outer dimensions of the ceramic impeller body can be significantly smaller than the dimensions of the reaction-sintered silicon carbide ceramic impeller of the present invention, thereby greatly reducing the difficulty of manufacturing the reaction-sintered silicon carbide ceramic impeller of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 This is a cross-sectional view of the reaction-sintered silicon carbide ceramic impeller of the utility model in Example 1.

[0037] Figure 2 for Figure 1Section view at AA.

[0038] Figure 3 This is a three-dimensional diagram of the ceramic impeller body after assembly in Example 1.

[0039] Figure 4 This is a cross-sectional view of the ceramic impeller body after assembly in Example 1.

[0040] Figure 5 for Figure 4 A cross-sectional view of the BB.

[0041] Figure 6 This is a stereoscopic view of the ceramic impeller body of Example 1.

[0042] Figure 7 This is a cross-sectional view of the ceramic impeller body in Example 1 at the center plane of the flow channel.

[0043] Figure 8 This is a cross-sectional view of the rear lining plate in Example 1.

[0044] Fig. 9 This is a cross-sectional view of the reaction-sintered silicon carbide ceramic impeller of the utility model in Example 2.

[0045] Fig.10 This is a cross-sectional view of the ceramic impeller body after assembly in Example 2.

[0046] Fig.11 It is a cross-sectional view of the ceramic impeller body in Example 2 at the center plane of the flow channel.

[0047] In the figure: 1-ceramic impeller body, 2-first frame, 3-hub, 4-front liner, 5-second frame, 6-joining line, 7-third cavity, 8-rear liner, 9-first cavity, 10-third frame, 11-blade, 12- Back panel , 13-front plate, 14-second cavity, 15-sealing cone surface. DETAILED DESCRIPTION

[0048] The present invention is further described in detail below in conjunction with embodiments and drawings, but the implementation manner of the present invention is not limited thereto.

[0049] Example 1

[0050] like Figure 1-8 As shown, the impeller diameter of the reaction-sintered silicon carbide ceramic impeller of the utility model is 1430 mm. The reaction-sintered silicon carbide ceramic impeller comprises a hub 3 and a plurality of ceramic impeller bodies 1 arranged on the hub 3, wherein the plurality of ceramic impeller bodies 1 are arranged in a circumference; each ceramic impeller body 1 comprises a front plate 13 sintered into one body, Back panel12 and a blade 11, wherein the blade 11 is provided with a second cavity 14 extending along the working surface of the blade 11 toward the impeller outlet; the second cavity 14 is provided with a second skeleton 5; Back panel 12 is provided with a first cavity 9, in which a first frame 2 is installed; the first frame 2 is connected to a second frame 5 in the second cavity 14; the first frame 2 is far away from the second frame 5 in the first cavity 14. Back panel A rear liner 8 is provided on one side of the ceramic impeller body 12; a groove is provided on the front plate 13 of the ceramic impeller body 1. After two adjacent ceramic impeller bodies 1 are spliced ​​together, the two grooves are spliced ​​together to form a third cavity 14, and a front liner 4 made of ceramic material is provided in the third cavity 14; the first cavity 9, the second cavity 14 and the third cavity 7 penetrate each other; the first cavity 9, the second cavity 14 and the third cavity 7 are filled with an adhesive to bind the first frame 2, the second frame 5, the front plate 13, Back panel 12. The blade 11, the front lining plate 4 and the rear lining plate 8 are bonded into a network structure.

[0051] In this embodiment, there are five ceramic impeller bodies 1, and correspondingly, there are also five blades.

[0052] The “front cover plate” described in this embodiment is a general term for the front side plate of the silicon carbide ceramic impeller of the present invention, including the front plate 13 and the front lining plate 4; correspondingly, the “rear cover plate” described in this embodiment is a general term for the rear side plate of the silicon carbide ceramic impeller of the present invention, including the rear plate 12 and the rear lining plate 8.

[0053] Figure 7 It is a cross-sectional view of the ceramic impeller body 1 at its outlet center plane (i.e., the plane where the distances from the impeller outlet to the front cover plate and the rear cover plate are equal). In this plane, the extension length L1 of the second cavity 14 is 538 mm, and the length L2 of the blade is 739 mm, i.e., the length of the second cavity 14 is 72.8% of the length of the blade 11.

[0054] Figure 7 The area of ​​blade 11 in this plane is 87941 mm 2 (including the area of ​​the second cavity 14), and dividing this area by the longest dimension L2 of the blade 11, the average thickness of the blade 11 is 119 mm, and the area of ​​the second cavity 14 is 22165 mm 2 , divided by the longest length L1 of the second cavity 14 , the average width of the second cavity 14 is obtained to be 41.2 mm, that is, the width of the second cavity 14 is 34.6% of the average thickness of the blade 11 .

[0055] like Figure 5 , Figure 7As shown, part of the surface of the second cavity 14 close to the working surface of the blade 11 is set as the equidistant surface of the working surface of the blade 11, and the distance T1 is 38 mm. The surface of the second cavity 14 from the working surface of the blade 11 within the range of T1±20% is defined as the equidistant surface of the working surface of the blade 11; the surface of the second cavity 14 close to the back side of the blade 11 is set as the equidistant surface of the back side of the blade 11, and the distance T2 is 42 mm. The surface of the second cavity 14 from the back side of the blade 11 within the range of T2±20% is defined as the equidistant surface of the back side of the blade 11. The sum of the two is measured and divided by the surface area of ​​the second cavity 14, and it is concluded that 92% of the surface of the second cavity 14 is the working surface of the blade 11 or the equidistant surface of the back side of the blade 11.

[0056] like Figure 1 , Figure 4 As shown, the front liner 4 is made of pressureless sintered silicon carbide and is composed of 8 to 12 pieces assembled into a ring.

[0057] like Figure 1 , 3 As shown in FIG. 4 , the first cavity 9, the second cavity 14 and the third cavity 7 penetrate each other, are filled with adhesive, and are interconnected to form a network structure. In this embodiment, the adhesive is epoxy resin 6101. In order to improve the wear resistance, 50%-80% of silicon carbide powder is added to the adhesive.

[0058] In order to improve the anti-cavitation performance of the impeller pump, a sealing cone 15 is provided at the suction port, and the distance B between the inner edge of the third cavity 7 and the outer edge of the sealing cone 15 is 5 mm.

[0059] like Figure 4 As shown, the depth h of the third cavity 7 is 15 mm, and the thickness H of the front cover plate is 60 mm, that is, the former is 25% of the latter.

[0060] like Figure 8 As shown, the rear liner 8 is made of reaction-sintered silicon carbide and is assembled from 8 to 12 pieces. After assembly, a first cavity 9 for accommodating the first skeleton 2 is provided therein.

[0061] Example 2

[0062] This embodiment is substantially the same as Embodiment 1, and the main differences are as follows:

[0063] like Fig. 9 , 10 As shown in FIG. 11 , after the five ceramic impeller bodies 1 are assembled, they are assembled into a third cavity 7 for accommodating the front liner 4 at the front cover plate portion, and a third frame 10 made of carbon steel is also provided between the front liner 4 and the ceramic impeller body 1 .

[0064] In order to improve the anti-cavitation performance of the impeller pump, a sealing cone 15 is provided at the suction port, and the distance B between the inner edge of the third cavity 7 and the outer edge of the sealing cone 15 is 30 mm.

[0065] like Fig.10 As shown, the depth h of the third cavity 7 is 75% of the thickness H of the front cover plate.

[0066] The length of the second cavity 14 is 52.4% of the length of the blade 11 .

[0067] The width of the second cavity 14 is 27.7% of the average thickness of the blade 11 .

[0068] The adhesive is vinyl resin.

[0069] Example 3

[0070] This embodiment is substantially the same as Embodiment 1, and the main differences are as follows:

[0071] The distance B between the inner edge of the third cavity 7 and the outer edge of the sealing cone surface 15 is 50 mm.

[0072] The depth of the third cavity 7 is 50% of the thickness of the front cover plate.

[0073] The length of the second cavity 14 is 30% of the length of the blade 11 .

[0074] The width of the second cavity 14 is 20% of the average thickness of the blade 11 .

[0075] Example 4

[0076] This embodiment is substantially the same as Embodiment 1, and the main differences are as follows:

[0077] The length of the second cavity 14 is 80% of the length of the blade 11 .

[0078] Example 5

[0079] This embodiment is substantially the same as Embodiment 1, and the main differences are as follows:

[0080] The width of the second cavity 14 is 50% of the average thickness of the blade 11 .

[0081] The above is a preferred implementation mode of the present invention, but the implementation mode of the present invention is not limited by the above content. Any other changes, modifications, substitutions, combinations, and simplifications that do not deviate from the spirit and principle of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.

Claims

1. A reaction-sintered silicon carbide ceramic impeller, characterized in that: It includes a hub and a plurality of ceramic impeller bodies arranged on the hub, wherein the plurality of ceramic impeller bodies are arranged in a circle; each ceramic impeller body includes a front plate, a rear plate and a blade sintered into one body, wherein a second cavity extending along the working surface of the blade toward the impeller outlet is arranged in the blade; and a second skeleton is arranged in the second cavity.

2. The reaction-sintered silicon carbide ceramic impeller according to claim 1, characterized in that: A groove is arranged on the front plate of the ceramic impeller body. After the ceramic impeller body is assembled, the groove is assembled to form a third cavity. A front lining plate made of ceramic material is arranged in the third cavity.

3. The reaction-sintered silicon carbide ceramic impeller according to claim 2, characterized in that: The rear plate is provided with a first cavity, in which a first frame is installed; the first frame is connected to a second frame in the second cavity, and a rear lining plate is provided on a side of the first frame away from the rear plate.

4. The reaction-sintered silicon carbide ceramic impeller according to claim 3, characterized in that: The first cavity, the second cavity and the third cavity penetrate each other; the first cavity, the second cavity and the third cavity are filled with adhesive to bond the first frame, the second frame, the front plate, the rear plate, the blades, the front lining plate and the rear lining plate into a network structure.

5. The reaction-sintered silicon carbide ceramic impeller according to claim 2, characterized in that: The depth of the third cavity is 25%-75% of the thickness of the front cover plate, and the front cover plate includes a front plate and a front lining plate.

6. The reaction-sintered silicon carbide ceramic impeller according to any one of claims 1 to 5, characterized in that: The length of the second cavity extending along the working surface of the blade toward the impeller outlet is 30%-80% of the length of the blade.

7. The reaction-sintered silicon carbide ceramic impeller according to any one of claims 1 to 5, characterized in that: The width of the second cavity is 20%-50% of the average thickness of the blade.

8. The reaction-sintered silicon carbide ceramic impeller according to any one of claims 1 to 5, characterized in that: The surface of the second cavity is partially configured as an equidistant surface of a blade working surface or a blade back surface, and the area of ​​the equidistant surface is greater than or equal to 40% of the area of ​​the second cavity.

9. The reaction-sintered silicon carbide ceramic impeller according to claim 2, characterized in that: A third frame is arranged in the third cavity.

10. The reaction-sintered silicon carbide ceramic impeller according to claim 2, characterized in that: A sealing cone surface is provided on the impeller suction port side of the ceramic impeller body, and the distance from the inner edge of the third cavity to the sealing cone surface is 5mm-50mm.