Thin film fixed attenuator
The thin film fixed attenuator addresses impedance and frequency issues by optimizing electrode arrangements and incorporating a C-shaped groove, enhancing performance and stability in communication systems.
Patent Information
- Application Number
- CN202420875298.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-25
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-04-25
AI Technical Summary
Existing fixed attenuators suffer from poor impedance matching, signal reflections, narrow frequency band range, and low attenuation accuracy, which affect system performance and cannot meet the needs of advanced communication systems.
A thin film fixed attenuator design featuring a ceramic substrate with specific electrode arrangements, resistance film layers, and a C-shaped clearance groove in the middle electrode, along with a π-shaped encapsulation protection layer, optimized for better impedance matching and temperature stability.
The design achieves improved impedance matching, reduced return loss, enhanced power handling capacity, and frequency response, ensuring stable attenuation across varying temperatures and limited spaces.
Smart Images

Figure CN222106989U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of electronic component preparation, and in particular relates to a thin film fixed attenuator. Background Art
[0002] A fixed attenuator is an electronic component with a predetermined and unchangeable attenuation. When the fixed attenuator is set to a specific attenuation, it will provide the set value of attenuation at a specific frequency. Fixed attenuators are very important in radio frequency (RF) and microwave applications. For example, in communication systems, test equipment, and measurement equipment, they are used to control the strength of the signal to prevent overload or damage to sensitive electronic equipment. Fixed attenuators are divided into a variety of structures, including but not limited to π-type, T-type or bridge structure or more complex matching attenuator design. Fixed attenuators of different structures have specific application scenarios. For example, π-type fixed attenuators usually have a wider frequency range, and bridge-type fixed attenuators have better impedance matching. At present, attenuators generally have poor impedance matching, causing unnecessary signal reflections and losses, thereby affecting the performance of the system; in addition, attenuators currently have problems such as narrow frequency band range and low attenuation accuracy, which cannot meet the needs of some communication systems and need further improvement. Utility Model Content
[0003] The utility model aims to overcome the shortcomings of the prior art and provide a thin film fixed attenuator.
[0004] The utility model adopts the following technical solutions:
[0005] A thin film fixed attenuator comprises a ceramic substrate, a first electrode arranged on one side of the ceramic substrate, two second electrodes arranged at intervals on the other side of the ceramic substrate opposite to the first electrode, an intermediate electrode connected to the first electrode and extending in a direction close to the two second electrodes, two resistance film layers respectively connected between the intermediate electrode and the opposite second electrodes, and an encapsulation protection layer arranged on the ceramic substrate and covering the two resistance film layers. The intermediate electrode is located between the two second electrodes and comprises two main body sections arranged at intervals on the ceramic substrate opposite to each other, a connecting section arranged between the two main body sections, and a giving way groove extending inward from the outer surface of the main body section; one end of the resistance film layer is connected to the main body section and the other end is connected to the opposite second electrode.
[0006] Furthermore, the clearance groove is arranged in a C shape.
[0007] Furthermore, the recess is located above the resistance film layer.
[0008] Furthermore, the first electrode includes a first surface electrode disposed on the surface of the ceramic substrate, a first side electrode connected to the first surface electrode and extending downward along the side of the ceramic substrate, and a first back electrode disposed on the back of the ceramic substrate and connected to the first side electrode.
[0009] Furthermore, the first surface electrode and the first back electrode are consistent in shape and size.
[0010] Furthermore, it also includes a first electroplating layer arranged on the surface of the first electrode and two second electroplating layers respectively arranged on the surfaces of the two second electrodes.
[0011] Furthermore, the first electroplating layer is a tin plating layer or a tin-lead plating layer, and the second electroplating layer is a tin plating layer or a tin-lead plating layer.
[0012] Furthermore, the encapsulation protection layer is arranged in a π shape on the ceramic substrate to cover the middle electrode and the two resistance film layers.
[0013] Furthermore, the thickness of the encapsulation protection layer is not less than 30 um.
[0014] Furthermore, the resistor film layer is formed by coating resistor slurry on the surface of the ceramic substrate through a screen printing process and then sintering and curing.
[0015] From the above description of the utility model, it can be seen that compared with the prior art, the beneficial effects of the utility model are as follows: the utility model optimizes the structural design of the attenuator, limits the arrangement of the first electrode, the two second electrodes, the middle and the resistance film layer, thereby achieving better impedance matching, reducing return loss, improving power handling capacity and frequency response characteristics, and has a small size, and can realize complex circuit designs in applications with limited space; wherein, the middle electrode is provided with a yield groove to ensure that the attenuation of the fixed attenuator can remain stable under different temperature conditions, thereby ensuring the performance stability of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a structural schematic diagram of a thin film fixed attenuator;
[0017] Figure 2 It is the exploded schematic diagram of the thin film fixed attenuator;
[0018] In the figure, 1-ceramic substrate, 2-first electrode, 3-second electrode, 4-middle electrode, 5-resistance film layer, 6-encapsulation protection layer, 7-first electroplating layer, 8-second electroplating layer, 21-first surface electrode, 22-first side electrode, 23-first back electrode 31-second surface electrode, 32-second side electrode, 33-second back electrode, 41-main section, 42-connecting section, 43-allowance groove. DETAILED DESCRIPTION
[0019] The present invention is further described below through specific implementation methods.
[0020] Reference Figure 1 to Figure 2As shown, a thin film fixed attenuator comprises a ceramic substrate 1, a first electrode 2 arranged on one side of the ceramic substrate 1, two second electrodes 3 arranged at intervals on the other side of the ceramic substrate 1 and opposite to the first electrode 2, an intermediate electrode 4 connected to the first electrode 2 and extending in a direction close to the second electrode 3, two resistance film layers 5 respectively connected between the intermediate electrode 4 and the opposite second electrode 3, an encapsulation protection layer 6 arranged on the ceramic substrate 1 and covering the two resistance film layers 5 and the intermediate electrode 4, a first electroplating layer 7 arranged on the surface of the first electrode 2, and two second electrodes 3 respectively arranged on the surface of the second electrode 3. The two second electroplating layers 8 on the surface; specifically, the present application defines a thin film fixed attenuator, whose overall length should be 1.60mm±0.10mm, width should be 0.80mm±0.10mm, and thickness should be 0.50mm±0.05mm; the nominal attenuation accuracy is 1~10dB; the attenuation accuracy is ±0.3dB for 1~4dB, ±0.5dB for 5~7dB, and ±0.7dB for 8~10dB; under the conditions of ambient temperature of 25℃ and frequency of 1GHz, the standing wave ratio is ≤1.30; the rated power is 0.1W.
[0021] The first electrode 2 includes a first surface electrode 21 arranged on the surface of the ceramic substrate 1, a first side electrode 22 connected to the first surface electrode 21 and extending downward along the side of the ceramic substrate 1, and a first back electrode 23 arranged on the back of the ceramic substrate 1 and connected to the first side electrode 22. Specifically, the first surface electrode 21 and the first back electrode 23 are consistent in shape and size.
[0022] The second electrode 3 includes a second surface electrode 31 arranged on the surface of the ceramic substrate 1, a second side electrode 32 connected to the second surface electrode 31 and extending downward along the side of the ceramic substrate 1, and a second back electrode 33 arranged on the back side of the ceramic substrate 1 and connected to the first side electrode 32. Specifically, the second surface electrode 31 and the second back electrode 33 are consistent in shape and size.
[0023] The middle electrode 4 is located between the two second electrodes 3, and includes two main sections 41 spaced apart on the ceramic substrate 1, a connecting section 42 arranged between the two main sections 41, and a clearance groove 43 extending inward from the outer surface of the main section 41. Specifically, the clearance groove 43 is located above the resistor film layer 5 and is arranged in a C shape, which can ensure that the attenuation of the fixed attenuator can remain stable under different temperature conditions, thereby ensuring the performance stability of the product.
[0024] The resistor film layer 5 has one end connected to the main body section 41 and the other end connected to the opposite second surface electrode 21. Specifically, the resistor film layer 5 is screen-printed on the surface of the ceramic substrate 1 using NTC series resistor paste and solidified using a high-temperature sintering process at 850°C. Two layers of resistor paste with the same designed resistance are simultaneously applied by screen printing to accurately control the thickness of the resistor film layer, thereby ensuring the consistency of the resistance values of the two resistor film layers 5 and effectively improving the reliability of the finished resistor network.
[0025] The encapsulation protection layer 6 is arranged in a π-shape on the ceramic substrate 1 to cover the middle electrode 4 and the two resistance film layers 5, and has a thickness of not less than 30um. Specifically, the encapsulation protection layer 6 is made of ink slurry ZSR-150 (BK3) by printing and covering the two resistance film layers 5 and the middle electrode 4, and is sintered at a high temperature of 200°C; further, the encapsulation protection layer 6 adopts a monomer graphic design to avoid friction and breakage caused by the cracking process, thereby improving the reliability of the product.
[0026] The first electroplating layer 7 is a tin plating layer or a tin-lead plating layer, covering the first electrode 2, and the thickness is controlled between 8-4 um.
[0027] The second electroplating layer 8 is a tin plating layer or a tin-lead plating layer, covering the exposed second electrode 3, and the thickness is controlled between 8-4 um.
[0028] The utility model optimizes the structural design of the attenuator and limits the arrangement of the first electrode 2, the two second electrodes 3, the middle electrode 4 and the resistance film layer 5, so as to achieve better impedance matching, reduce return loss, improve power handling capacity and frequency response characteristics, and have a small size, so that complex circuit design can be implemented in applications with limited space; wherein, the middle electrode 4 is provided with a yield groove 43 to ensure that the attenuation of the fixed attenuator can remain stable under different temperature conditions, thereby ensuring the performance stability of the product.
[0029] The above description is only a preferred embodiment of the present invention, and therefore cannot be used to limit the scope of implementation of the present invention. That is, equivalent changes and modifications made according to the scope of application of the present invention and the contents of the specification should still fall within the scope covered by the present invention.
Claims
1. A thin film fixed attenuator, Features: It includes a ceramic substrate, a first electrode arranged on one side of the ceramic substrate, two second electrodes arranged at intervals on the other side of the ceramic substrate opposite to the first electrode, an intermediate electrode connected to the first electrode and extending in a direction close to the two second electrodes, two resistance film layers respectively connected between the intermediate electrode and the opposite second electrodes, and an encapsulation protection layer arranged on the ceramic substrate to cover the two resistance film layers. The intermediate electrode is located between the two second electrodes and includes two main body sections arranged at intervals on the ceramic substrate opposite to each other, a connecting section arranged between the two main body sections, and a make-way groove extending inward from the outer surface of the main body section; one end of the resistance film layer is connected to the main body section and the other end is connected to the opposite second electrode.
2. A thin film fixed attenuator according to claim 1, Features: The giving way groove is arranged in a C shape.
3. A thin film fixed attenuator according to claim 1, Features: The recess is located above the resistance film layer.
4. The thin film fixed attenuator according to claim 1, Features: The first electrode includes a first surface electrode disposed on the surface of the ceramic substrate, a first side electrode connected to the first surface electrode and extending downward along the side of the ceramic substrate, and a first back electrode disposed on the back of the ceramic substrate and connected to the first side electrode.
5. A thin film fixed attenuator according to claim 4, Features: The first surface electrode and the first back electrode have the same shape and size.
6. The thin film fixed attenuator according to claim 1, Features: It also includes a first electroplating layer arranged on the surface of the first electrode and two second electroplating layers respectively arranged on the surfaces of the two second electrodes.
7. A thin film fixed attenuator according to claim 6, Features: The first electroplating layer is a tin plating layer or a tin-lead plating layer, and the second electroplating layer is a tin plating layer or a tin-lead plating layer.
8. The thin film fixed attenuator according to claim 1, Features: The encapsulation protection layer is arranged in a π shape on the ceramic substrate to cover the middle electrode and the two resistance film layers.
9. The thin film fixed attenuator according to claim 1, Features: The thickness of the encapsulation protection layer is not less than 30um.
10. The thin film fixed attenuator according to claim 1, Features: The resistor film layer is formed by coating resistor slurry on the surface of a ceramic substrate through a screen printing process and then sintering and curing.