By using a combined design of polyester film, linear low-density polyethylene tensile-resistant layer and fiberglass-fiber film in the protective film, combined with the auxiliary tearing structure, the damage and tensile properties of the existing protective film when tearing is solved. The poor problem achieves higher tear and scratch resistance.
Patent Information
- Application Number
- CN202323652265.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-30
- Publication Date
- 2025-01-14
- Estimated Expiration
- 2033-12-30
AI Technical Summary
The existing protective film is prone to damage when tearing, and the lack of tensile properties leads to tearing, making it inconvenient to use.
A tear-proof protective film was designed, using a polyester film protective layer, a linear low-density polyethylene tensile-resistant layer, a reinforced fiberglass toughened film layer and an outer polyester film protective layer, and the structure was assisted to tear, including the end The clamping method of the partial tearing film and the upper protective tearing film avoids corner tearing, and uses a linear low-density polyethylene tensile resistance layer to improve tensile resistance.
It effectively avoids tearing of the protective film when tearing it, improves the convenience and practicality of use, and enhances scratch and tear resistance.
Smart Images

Figure CN222348925U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to a protective film, in particular to a tear-resistant protective film. Background Art
[0002] Protective films can be divided into digital product protective films, car protective films, household protective films, food preservation protective films, etc. according to their uses. With the popularity of digital products such as mobile phones in China, protective films have gradually become a general term for screen protective films. The self-adhesive layer of self-adhesive protective films is generally EVA, ultra-low density polyethylene or polyolefin plastic resin.
[0003] When the protective film is pasted on the screen, the side film on the protective film is torn off first, and then the protective film is aligned and pasted on the screen. When tearing off the protective film, it is easy to damage the protective film by only lifting one corner and then tearing it off. In addition, since the traditional protective film does not have tensile properties, it is easy to crack when torn off, resulting in damage to the protective film. Therefore, an anti-tear protective film is proposed to address the above problems. Summary of the invention
[0004] In this embodiment, a tear-resistant protective film is provided to solve the problem of tearing of the protective film in the prior art due to the inconvenience of tearing and poor tensile properties during use.
[0005] According to one aspect of the present application, a tear-proof protective film is provided, comprising a protective film main body; a self-adhesive layer is provided on the bottom surface of the protective film main body, and a dust-proof side protective film is pasted on the bottom surface of the self-adhesive layer, an end tear film is inserted inside one end of the dust-proof side protective film, and the top surface of the end tear film is pasted on the bottom surface of the protective film main body, an upper protective tear film is fixed on the top surface of the end tear film on the side of the protective film main body, and a connecting pad is fixed on the top surface of the upper protective tear film, and the bottom surface of the connecting pad on the side of the upper protective tear film is attached to the top of the protective film main body.
[0006] Furthermore, the protective film body includes an inner polyester film protective layer, a linear low-density polyethylene anti-stretch layer, a reinforced glass tempered film layer, a special treatment layer and an outer polyester film protective layer, the bottom surface of the inner polyester film protective layer is provided with a linear low-density polyethylene anti-stretch layer, and the bottom surface of the linear low-density polyethylene anti-stretch layer is provided with a reinforced glass tempered film layer, the bottom surface of the reinforced glass tempered film layer is provided with a special treatment layer, and the bottom surface of the special treatment layer is provided with an outer polyester film protective layer.
[0007] Furthermore, the length of the dustproof side protective film is equal to the length of the protective film body, and one end of the dustproof side protective film close to the end tear film is attached to the bottom surface of the end tear film.
[0008] Furthermore, the thickness of the connecting spacer is equal to the thickness of the protective film body, and the length of the end tear film is equal to the length of the upper protective tear film.
[0009] Furthermore, the thickness of the linear low-density polyethylene anti-stretching layer is less than the thickness of the polyester film protective layer, and the thickness of the reinforced glass tempered film layer is equal to the thickness of the polyester film protective layer.
[0010] Furthermore, the thickness of the special treatment layer is equal to the thickness of the reinforced glass tempered film layer, and the thickness of the outer polyester film protective layer is equal to the thickness of the linear low-density polyethylene tensile resistance layer.
[0011] Through the above-mentioned embodiments of the present application, an auxiliary tearing structure is adopted. When tearing off the protective film, one end of the protective film body can be completely separated from the dustproof side protective film by clamping the end tearing film and the upper protective tearing film, thereby avoiding the tearing caused by tearing through the corner of the protective film body. The tensile strength of the linear low-density polyethylene tensile strength layer is used to reduce the tearing caused by the protective film being torn, thereby solving the problem of tearing caused by the inconvenience of tearing and poor tensile strength of the existing protective film during use, and greatly improving the practicality of the protective film. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0013] Figure 1 This is a schematic structural diagram of an embodiment of the present application;
[0014] Figure 2 A protection schematic diagram of an embodiment of the present application;
[0015] Figure 3 It is a schematic side cross-sectional view of a local structure of an embodiment of the present application.
[0016] In the figure: 1. Protective film body; 111. Inner polyester film protective layer; 112. Linear low-density polyethylene tensile strength layer; 113. Reinforced glass tempered film layer; 114. Special treatment layer; 115. Outer polyester film protective layer; 2. Self-adhesive layer; 3. Dust-proof side protective film; 4. End tear film; 5. Upper protective tear film; 6. Connecting spacer. DETAILED DESCRIPTION
[0017] In order to enable those skilled in the art to better understand the present application, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of this application.
[0018] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0019] In the present application, the terms "upper", "lower", "left", "right", "front", "back", "top", "bottom", "inner", "outer", "middle", "vertical", "horizontal", "lateral", "longitudinal" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings. These terms are mainly used to better describe the present application and its embodiments, and are not used to limit the indicated devices, elements or components to have a specific orientation, or to be constructed and operated in a specific orientation.
[0020] In addition, some of the above terms may be used to express other meanings in addition to indicating orientation or positional relationship. For example, the term "on" may also be used to express a certain dependency or connection relationship in some cases. For those of ordinary skill in the art, the specific meanings of these terms in this application can be understood according to specific circumstances.
[0021] In addition, the terms "installed", "set", "provided with", "connected", "connected", and "socketed" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0022] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0023] See also Figure 1-3 As shown, an anti-tear protective film comprises a protective film body 1; a self-adhesive layer 2 is arranged on the bottom surface of the protective film body 1, and a dustproof side protective film 3 is pasted on the bottom surface of the self-adhesive layer 2, an end tear film 4 is inserted inside one end of the dustproof side protective film 3, and the top surface of the end tear film 4 is pasted on the bottom surface of the protective film body 1, an upper protective tear film 5 is fixed on the top surface of the end tear film 4 on the side of the protective film body 1, and a connecting spacer 6 is fixed on the top surface of the upper protective tear film 5, and the bottom surface of the connecting spacer 6 on the side of the upper protective tear film 5 is pasted on the top of the protective film body 1, and through the auxiliary tearing structure, when tearing the protective film, the protective film body 1 can be torn in a manner of clamping the end tear film 4 and the upper protective tear film 5, so as to prevent the protective film body 1 from being torn;
[0024] The protective film body 1 comprises an inner polyester film protective layer 111, a linear low-density polyethylene anti-stretching layer 112, a reinforced glass tempered film layer 113, a special treatment layer 114 and an outer polyester film protective layer 115. The inner polyester film protective layer 111 is provided with a linear low-density polyethylene anti-stretching layer 112 on its bottom surface, and a reinforced glass tempered film layer 113 is provided on its bottom surface. The reinforced glass tempered film layer 113 is provided with a special treatment layer 114 on its bottom surface, and an outer polyester film protective layer 115 is provided on its bottom surface. The combination design of the inner polyester film protective layer 111 and the outer polyester film protective layer 115 greatly improves the anti-scratch performance of the protective film, and the anti-tear performance of the protective film can be improved by combining the tensile performance of the linear low-density polyethylene anti-stretching layer 112.
[0025] The length of the dustproof side protective film 3 is equal to the length of the protective film body 1, and one end of the dustproof side protective film 3 close to the end tear film 4 is attached to the bottom surface of the end tear film 4; the thickness of the connecting gasket 6 is equal to the thickness of the protective film body 11, and the length of the end tear film 4 is equal to the length of the upper protective tear film 5; the thickness of the linear low-density polyethylene tensile layer 112 is less than the thickness of the inner polyester film protective layer 111, and the thickness of the reinforced glass tempered film layer 113 is equal to the thickness of the inner polyester film protective layer 111; the thickness of the special treatment layer 114 is equal to the thickness of the reinforced glass tempered film layer 113, and the special treatment layer 114 has been subjected to anti-glare treatment, and the thickness of the outer polyester film protective layer 115 is equal to the thickness of the linear low-density polyethylene tensile layer 112.
[0026] When the present application is in use, when the protective film main body 1 needs to be opened for use, first slightly bend the protective film main body 1, and pull the dustproof side protective film 3 on the bottom of the end tear film 4 to separate the dustproof side protective film 3 from the self-adhesive layer 2, and then pull the upper protective tear film 5 so that the upper protective tear film 5 drives the end tear film 4 to separate from the protective film main body 1 through the connecting spacer 6, so that one side of the protective film main body 1 can be completely separated from the end tear film 4 and the upper protective tear film 5, and then the protective film main body 1 can be pasted on the screen.
[0027] The circuits, electronic components and modules involved are all prior art and can be fully implemented by those skilled in the art. Needless to say, the content protected by this application does not involve improvements to software and methods.
[0028] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.
Claims
1. A tear-resistant protective film, comprising a protective film body (1); characterized in that: The bottom surface of the protective film body (1) is provided with a self-adhesive layer (2), and a dustproof side protective film (3) is adhered to the bottom surface of the self-adhesive layer (2); an end tear film (4) is inserted into one end of the dustproof side protective film (3), and the top surface of the end tear film (4) is adhered to the bottom surface of the protective film body (1); an upper protective tear film (5) is fixed to the top surface of the end tear film (4) on the side of the protective film body (1), and a connecting spacer (6) is fixed to the top surface of the upper protective tear film (5); the bottom surface of the connecting spacer (6) on the side of the upper protective tear film (5) is adhered to the top of the protective film body (1).
2. The tear-resistant protective film according to claim 1, characterized in that: The protective film body (1) comprises an inner polyester film protective layer (111), a linear low-density polyethylene anti-stretching layer (112), a reinforced glass tempered film layer (113), a special treatment layer (114) and an outer polyester film protective layer (115); the bottom surface of the inner polyester film protective layer (111) is provided with a linear low-density polyethylene anti-stretching layer (112); the bottom surface of the linear low-density polyethylene anti-stretching layer (112) is provided with a reinforced glass tempered film layer (113); the bottom surface of the reinforced glass tempered film layer (113) is provided with a special treatment layer (114); and the bottom surface of the special treatment layer (114) is provided with an outer polyester film protective layer (115).
3. The tear-resistant protective film according to claim 1, characterized in that: The length of the dustproof side protective film (3) is equal to the length of the protective film body (1), and one end of the dustproof side protective film (3) close to the end tear film (4) is attached to the bottom surface of the end tear film (4).
4. The tear-resistant protective film according to claim 1, characterized in that: The thickness of the connecting spacer (6) is equal to the thickness of the protective film body (1) 1, and the length of the end tear film (4) is equal to the length of the upper protective tear film (5).
5. The tear-resistant protective film according to claim 2, characterized in that: The thickness of the linear low-density polyethylene anti-stretching layer (112) is less than the thickness of the polyester film protective layer (111), and the thickness of the reinforced glass tempered film layer (113) is equal to the thickness of the polyester film protective layer (111).
6. The tear-resistant protective film according to claim 2, characterized in that: The thickness of the special treatment layer (114) is equal to the thickness of the reinforced glass tempered film layer (113), and the thickness of the outer polyester film protective layer (115) is equal to the thickness of the linear low-density polyethylene tensile resistance layer (112).