Green table tennis bat free of glue adhesion

By using an adhesive plate and groove structure in the table tennis racket, combined with the molecular force of the silicone coating and film layer, the rubber adheres to the adhesive plate, solving the problem of using glue in the existing table tennis racket, realizing green environmental protection and convenience of rubber replacement.

CN222955884UActive Publication Date: 2025-06-10YANCHENG AST SPORTING GOODS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202421022674.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-05-13
Publication Date
2025-06-10
Estimated Expiration
2034-05-13

AI Technical Summary

Technical Problem

The existing table tennis rackets use glue to adhere to rubber, which has problems such as health hazards, high viscosity and long drying time, and the rubber replacement time is long and it is troublesome to clean it.

Method used

A green glue-free ping-pong racket is designed, using an adhesive plate and a groove structure. The lower part of the rubber is coated on the adhesive plate and fixed. The molecular force of the silicone coating and film layer is used to make the rubber adhere to the adhesive plate to avoid the use of glue.

Benefits of technology

The rubber is tightly attached, avoids the use of glue, and has the advantages of green and environmental protection. The rubber replacement is similar to mobile phone film, which is convenient and fast.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222955884U_ABST
    Figure CN222955884U_ABST
Patent Text Reader

Abstract

The utility model provides a green glue-adhesion-free table tennis bat which comprises a bottom plate, adhesion plates are fixedly connected to the two sides of the bottom plate, grooves are formed in the middles of the adhesion plates in a sinking mode, rubber sheets are arranged in the grooves in a matched mode, the side walls of the grooves of the adhesion plates are obliquely arranged, and the side edges of the rubber sheets are obliquely arranged. The rubber sheet comprises a bottommost silica gel coating, the bottom wall of the groove of the adhesion plate is smooth, and the silica gel coating is matched with the bottom wall of the groove. According to the invention, the traditional mode of gluing glue skin is abandoned, the use of glue is avoided, and the negative influence caused by the glue is eliminated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of table tennis racket technology, and particularly to a green glue-free table tennis racket. Background Art

[0002] A table tennis racket consists of three parts: a bottom plate, a rubber sheet, and a sponge. The reasonable combination of the three determines the quality of a racket. The rubber sheet is usually adhered and fixed to the bottom plate with glue. Glue can be divided into organic glue and inorganic glue. Organic glue contains substances harmful to human health, such as formaldehyde. Inorganic glue has a higher viscosity and a slower drying time compared to organic glue. Therefore, the replacement time of the rubber sheet is longer, and it is troublesome to clean inorganic glue, so it needs to be handled with extra care when using. Summary of the Invention

[0003] To solve the above problems, the present invention discloses a green glue-free table tennis racket, which includes a bottom plate. Both sides of the bottom plate are fixedly connected with adhesion plates. A groove is sunken in the middle of the adhesion plate, and a rubber sheet is cooperatively arranged in the groove. That is, the lower part of the rubber sheet is covered and fixed on the adhesion plate, and the use of glue can be avoided.

[0004] The side wall of the groove of the adhesion plate is inclined, and the side of the rubber sheet is inclined, and they are cooperatively arranged in the groove with an anti-detachment inclination angle. That is, the convex edge at the edge of the adhesion plate has a larger upper size and a smaller lower size, and the outer side wall of the convex plate is vertical. Through this structure, the adhesion effect of the rubber sheet is further improved.

[0005] Preferably, the rubber sheet includes a silica gel coating on the lowermost layer. The bottom wall of the groove of the adhesion plate is smooth, and the silica gel coating is cooperatively arranged on the bottom wall of the groove. The purpose of setting the silica gel coating is to make the rubber sheet adhere to the adhesion plate by using the intermolecular force, so that the adhesion effect of the rubber sheet can be achieved without using glue.

[0006] Preferably, the rubber sheet includes a rubber layer. A sponge layer is arranged below the rubber layer, and a film layer is arranged below the sponge layer. The silica gel coating is applied on the film layer. The film layer is used for sealing to prevent the gas in the sponge layer from entering the space where the silica gel coating is located and reducing the effect of intermolecular force.

[0007] Preferably, a plurality of through holes are arranged on the edge of the racket, and a fixing buckle structure is arranged in the through holes. The fixing buckle structure includes a plug and a buckle ring. The plug and the buckle ring are in interference fit to clamp the rubber sheets on both sides. The rubber sheets are further fixed, and at the same time, the fixing buckle structure is placed on the edge of the racket to reduce the influence on hitting the ball.

[0008] Preferably, gaskets are arranged at one ends of the plug and the buckle ring respectively. This makes the rubber sheet flat and improves the aesthetics of the racket.

[0009] Preferably, a handle is arranged on the bottom plate.

[0010] The beneficial effects of the present invention are as follows:

[0011] 1. An adhesion plate is added, and the structure of the rubber sheet is optimized, that is, a thin film layer and a silica gel coating are added. Combined with the inclined setting of the edge of the film, the rubber sheet can be tightly attached to the adhesion plate without using glue, which has the advantage of being green and environmentally friendly.

[0012] 2. With this structure, the replacement of the rubber sheet is similar to applying a mobile phone film, which has the advantages of convenience and speed. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 is a three-dimensional schematic diagram of the present invention;

[0014] Figure 2 is an exploded schematic diagram of the present invention;

[0015] Figure 3 is a schematic diagram of the fixing buckle structure of the present invention;

[0016] Figure 4 is a schematic diagram of the edge structure of the rubber sheet of the present invention;

[0017] Figure 5 is a schematic diagram of the edge of the adhesion plate of the present invention.

[0018] LIST OF REFERENCE NUMERALS:

[0019] 1. Handle; 2. Bottom plate; 3. Rubber sheet; 4. Adhesion plate; 5. Gasket; 6. Plug; 7. Buckle ring;

[0020] 31. Silica gel coating; 32. Thin film layer; 33. Sponge layer; 34. Rubber layer. DETAILED DESCRIPTION OF THE INVENTION

[0021] The present invention will be further clarified below in conjunction with the drawings and specific embodiments. It should be understood that the following specific embodiments are only used to illustrate the present invention and not to limit the scope of the present invention. It should be noted that the terms "front", "rear", "left", "right", "upper" and "lower" used in the following description refer to the directions in the drawings, and the terms "inner" and "outer" respectively refer to the directions towards or away from the geometric center of a specific component.

[0022] Combined with Figure 1 and Figure 2As shown, a green glue-free table tennis racket includes a bottom plate 2, which is a solid wood board instead of an artificial board to achieve the purpose of green environmental protection. Adhesion plates 4 are fixedly connected to both sides of the bottom plate 2. The adhesion plates 4 are a plastic plate and can be fixedly connected to the bottom plate 2 by thermoplastic one-piece molding. The bottom plates are placed together in a mold for injection molding. A groove is set in the middle of the adhesion plate 4, and a rubber 3 is matched in the groove, that is, the lower part of the rubber 3 is accommodated in the groove.

[0023] Combination Figure 4 and Figure 5 As shown, the side wall of the groove of the adhesive plate 4 is inclined, the side edge of the rubber 3 is inclined, and is fitted in the groove at an anti-slip angle, that is, the lower end size of the rubber 3 is larger than the upper end size, and the inclination angle of the side wall of the groove and the inclination angle of the side edge of the rubber 3 are both α, and α is an acute angle, preferably 45°.

[0024] The rubber 3 includes a bottom layer of silicone coating 31, the bottom wall of the groove of the adhesive plate 4 is smoothly arranged, and the silicone coating 31 is matched on the bottom wall of the groove, that is, the rubber 3 is adhered to the adhesive plate 4 by molecular force.

[0025] Furthermore, when replacing and installing the rubber 3, it is necessary to wipe the bottom wall of the groove of the adhesive plate 4 clean, and then attach the rubber 3 to the groove, and the lower part of the rubber 3 is received in the groove, and then use a rolling type tool to roll one side of the rubber 3 to completely expel the air between the two. The process is similar to that of applying a film to a mobile phone.

[0026] like Figure 4 As shown, the rubber 3 includes a rubber layer 34, a sponge layer 33 is arranged below the rubber layer 34, and both the rubber layer 34 and the sponge layer 33 are of conventional structure. A film layer 32 is arranged below the sponge layer 33, and a silicone coating 31 is coated on the film layer 32. The film layer 32 is used for sealing to prevent the air in the sponge layer 33 from entering the silicone coating 31, thereby reducing the molecular force.

[0027] like Figure 3 As shown, the edge of the racket is provided with a plurality of through holes to reduce the impact on the hitting, and a fixing buckle structure is provided in the through hole, and the fixing buckle structure includes a latch 6 and a buckle ring 7, and the latch 6 and the buckle ring 7 are interference fit to clamp the rubber 3 on both sides. When replacing the rubber 3, a thin rod is used to support one end of the latch 6 in advance and press it out. After the rubber 3 is finished, the latch 6 and the buckle ring 7 are replaced and installed. The use of the latch 6 and the buckle ring 7 further improves the effect of the attachment and fixing of the rubber 3.

[0028] One end of the latch pin 6 and the buckle ring 7 is provided with a sealing pad 5. It is used to improve the aesthetics of the racket and reduce the impact on the ball.

[0029] A handle 1 is provided on the bottom plate 2 .

[0030] The technical means disclosed in the solution of the present invention are not limited to those disclosed in the above embodiments, but also include technical solutions formed by any combination of the above technical features.

Claims

1. A green glue-free table tennis racket, characterized in that: It comprises a bottom plate (2), both sides of the bottom plate (2) are fixedly connected to adhesive plates (4), a groove is sunken in the middle of the adhesive plate (4), and a rubber sheet (3) is matched and arranged in the groove; The side wall of the groove of the adhesive plate (4) is arranged at an angle, and the side edge of the rubber (3) is arranged at an angle and fits in the groove at an anti-slip angle; The rubber (3) comprises a lowermost layer of a silicone coating (31); the bottom wall of the groove of the adhesive plate (4) is smoothly arranged, and the silicone coating (31) is fitted on the bottom wall of the groove.

2. A green glue-free table tennis racket according to claim 1, characterized in that: The rubber (3) comprises a rubber layer (34), a sponge layer (33) is arranged below the rubber layer (34), a film layer (32) is arranged below the sponge layer (33), and the silicone coating (31) is coated on the film layer (32).

3. A green glue-free table tennis racket according to claim 1, characterized in that: The racket edge is provided with a plurality of through holes, and a fixing buckle structure is provided in the through holes. The fixing buckle structure comprises a latch (6) and a buckle ring (7). The latch (6) and the buckle ring (7) are interference-fitted to clamp the rubber (3) on both sides.

4. A green glue-free table tennis racket according to claim 3, characterized in that: A sealing gasket (5) is provided at one end of each of the latch pin (6) and the buckle ring (7).

5. A green glue-free table tennis racket according to claim 1, characterized in that: A handle (1) is provided on the bottom plate (2).