A type of atomizing coil, atomizer

By employing a porous metal layer and an electrode layer in the atomizing core, the problems of poor wetting, unstable bonding, low vapor consumption ratio, and poor reliability in existing technologies have been solved, achieving efficient atomization and excellent aroma delivery.

CN224948427UActive Publication Date: 2026-11-10SHENZHEN SMOORE TECH LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202521938833.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-09-08
Publication Date
2026-11-10
Estimated Expiration
2035-09-08

AI Technical Summary

Technical Problem

Existing atomizing cores have problems in the manufacturing process, such as the liquid medium not being able to completely wet the heating layer during atomization, the metal wires or mesh being easily deformed and not being able to bond stably with the ceramic substrate, low atomization consumption ratio, insufficient aroma, poor taste consistency, poor reliability, and high production costs.

Method used

A porous metal layer is used as the heating layer, with a pore size of 10–100 μm, an open porosity of 25%–80%, and a heating area of ​​0.8–10 mm². Combined with an electrode layer and a cover layer, the porosity of the heating substrate is 50%–80%, with a pore size of 20–75 μm. Stainless steel or iron-chromium-aluminum metal materials are used, and the metal mesh is prepared by laser etching or weaving to ensure a tight connection between the heating layer and the substrate.

Benefits of technology

It achieves full wetting of the heating layer by liquid medium, reduces obvious splattering noise, improves the mist consumption ratio to over 1.3, has a full aroma, excellent consistent taste, excellent reliability, no failure after 1500 puffs, and good combination effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224948427U_ABST
    Figure CN224948427U_ABST
Patent Text Reader

Abstract

This utility model relates to the field of electronic atomization technology, specifically to an atomizing core and an atomizer. The atomizing core includes a heating substrate, a connecting layer located on one side of the heating substrate, and a heating layer located on the side of the connecting layer away from the heating substrate. The heating layer includes a heating area and an electrode area, with the electrode area in contact with the heating area and located at both ends of the heating area. The heating layer includes a porous metal layer; the pore size of the porous metal layer is 10–100 μm, and the porosity is 25%–80%. The area of ​​the heating area is 0.8–10 mm². 2 It also includes an electrode layer that covers at least a portion of the surface of the electrode area. During use, the liquid medium can fully wet the heating layer, preventing noticeable splattering sounds, and the heating layer is not easily loosened, resulting in excellent reliability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of electronic atomization technology, specifically to an atomizing core and an atomizer. Background Technology

[0002] In existing technologies, the heating layer of ceramic atomizing cores typically falls into three categories. The first is a thick-film metal heating film, usually 10–100 μm thick, prepared by printing a thick-film slurry onto a porous ceramic substrate and then sintering it. The second is a metal wire or mesh, placed inside or on the surface of the porous ceramic substrate through embedding or bonding processes. The third is a thin-film metal heating film, usually less than 10 μm thick, prepared primarily through sputtering. Of these three methods, the first and second suffer from the problem of the liquid medium not completely wetting the heating layer during atomization, affecting the atomizing core's performance, such as low mist consumption ratio, insufficient aroma, and sometimes even a burnt smell. The second method also suffers from the problem of easily deformable metal wires or meshes that are unstable in their adhesion to the porous ceramic substrate. While the third method offers relatively good performance, it suffers from poor reliability and is unsuitable for industrial production due to the high equipment cost of metal sputtering processes.

[0003] Existing technologies have proposed a method for preparing a porous heating layer ceramic atomizing core by attaching it to the surface pore structure of a ceramic substrate. While this method can reduce mist consumption and improve aroma quality while controlling costs, it suffers from inconsistent taste due to varying pore sizes and uneven distribution, and issues such as noticeable popping sounds exceeding 50 dB during use. Existing technologies also propose methods for fixing metal wires or meshes to a porous ceramic substrate using clamping blocks; however, during operation, the atomizing core is prone to loosening due to repeated thermal expansion and contraction, leading to failure. Summary of the Invention

[0004] The purpose of this invention is to overcome the limitations of existing technologies, which fail to maintain a low manufacturing cost for the atomizing core while achieving excellent performance; and to address issues such as the tendency for metal mesh to deform as a heating layer and unstable bonding with the ceramic substrate during use. Therefore, this invention provides an atomizing core and an atomizer.

[0005] To achieve the above objectives, the present invention adopts the following technical solution:

[0006] This invention provides an atomizing core, comprising a heating substrate, a connecting layer located on one side of the heating substrate, and a heating layer located on the side of the connecting layer away from the heating substrate; the heating layer includes a heating area and an electrode area, the electrode area being in contact with the heating area and located at both ends of the heating area; the heating layer includes a porous metal layer; the pore size of the porous metal layer is 10–100 μm, and the porosity is 25%–80%; the area of ​​the heating area is 0.8–10 mm². 2 It also includes an electrode layer that covers at least a portion of the surface of the electrode region.

[0007] In the atomizing core provided by this utility model, the shape of the heating zone circuit is not limited, such as it can be a double parallel line, an S-line, a wavy line, a sine line, a W-shaped line, etc., as long as it meets the area requirement. The heating substrate can use commonly used heating substrates in the art. Typically, without limitation, the porosity of the heating substrate is 50% to 80%, and the pore size is 20 to 75 μm.

[0008] Optionally, a cover layer is also included, located on the side of the heating layer away from the connecting layer; the coverage area of ​​the cover layer is the heating zone. By ensuring the cover layer avoids the electrode area and exists only in the heating zone, it is possible to prevent the cover layer material from reacting with the electrodes, thereby affecting the use of the atomizing core.

[0009] Optionally, the pore size of the connecting layer is 10–60 μm, the porosity is 30%–70%, and the thickness is 30–200 μm.

[0010] The pore size characterization method of the connecting layer in the atomizing core provided by this utility model is as follows: the size of 10 pores is measured under SEM, and the average value is taken as the pore size data. Porosity is characterized by observing the number of pores per square millimeter under an SEM electron microscope, and combined with the pore size, calculated using the following method: (π×(pore size / 2)²×number of pores)÷(1000×1000)×100%. The pore size of the heating substrate is tested by the bubble point method, and the porosity is tested by the water displacement method.

[0011] Optionally, the thickness of the porous metal layer is 20–200 μm.

[0012] Optionally, the thickness of the capping layer is 30–150 μm, the porosity is 35%–75%, and the pore size is 5–50 μm.

[0013] Optionally, the perforated metal layer may include a metal mesh.

[0014] Optionally, the metal material used for the porous metal layer includes stainless steel, and at least one of iron-chromium-aluminum. Commonly available stainless steel grades can be used; typically, but not limited to, stainless steel includes at least one of 201 stainless steel, 316 stainless steel, 316L stainless steel, 304 stainless steel, 304L stainless steel, 430 stainless steel, 302 stainless steel, 310 stainless steel, 310S stainless steel, and duplex stainless steel.

[0015] Optionally, the thickness of the porous metal layer is 20–120 μm.

[0016] Optionally, the metal mesh includes at least one of woven metal mesh, stamped metal mesh, laser-etched metal mesh, and chemically etched metal mesh.

[0017] Optionally, the thickness of the porous metal layer is 30–80 μm.

[0018] Optionally, the woven metal mesh includes a rolled woven metal mesh. Rolling can make the metal layer flatter, helping to improve the adhesion between the heating layer and the connecting layer and the heating substrate.

[0019] Optionally, the diameter of the metal wire used in the woven metal mesh is 10 to 100 μm, and the mesh count of the woven metal mesh is 100 to 1000 mesh.

[0020] Optionally, the thickness of the rolled woven metal mesh is 40% to 90% of the thickness of the woven metal mesh.

[0021] Optionally, the wire diameter used in the woven metal mesh is 15–60 μm, and the mesh size of the woven metal mesh is 250–700 mesh. Wires with too small a diameter are difficult to manufacture and have weak strength, while wires with too large a diameter will affect the wetting effect of the liquid medium during subsequent use of the atomizing core; a reasonable range needs to be selected to achieve better performance.

[0022] The weaving method of the metal mesh is not particularly limited; plain weave, twill weave, and mat weave can all be used. Plain weave refers to a weaving method where each warp wire crosses over and under each weft wire, with the warp and weft wires being the same thickness and forming a 90-degree angle. Twill weave refers to a weaving method where the warp and weft wires are of the same thickness, with each warp wire crossing over and under every two weft wires, and each weft wire crossing over and under every two warp wires. Mat weave refers to a weaving method where the warp and weft wires have different diameters, usually with the warp wire diameter being larger than the weft wire diameter; there are two types: plain weave mat weave and twill weave mat weave. The method of cutting perforated metal materials is also not particularly limited; common methods such as chemical etching and laser engraving are acceptable.

[0023] This utility model also provides an atomizer, including the above-mentioned atomizing core.

[0024] The beneficial effects of this utility model are:

[0025] The atomizing core provided by this utility model includes a heating substrate, a connecting layer located on one side of the heating substrate, and a heating layer located on the side of the connecting layer away from the heating substrate; the heating layer includes a heating area and an electrode area, the electrode area being in contact with the heating area and located at both ends of the heating area; the heating layer includes a porous metal layer; the pore size of the porous metal layer is 10-100 μm, and the porosity is 25%-80%; the area of ​​the heating area is 0.8-10 mm². 2 It also includes an electrode layer that covers at least a portion of the surface of the electrode area. The atomizing core provided by this invention allows the liquid medium to fully wet the heating layer during use, preventing noticeable splattering sounds and exhibiting excellent reliability. The heating zone includes a porous metal layer with numerous uniformly sized pores. These pores facilitate rapid transfer of the liquid medium, ensuring the heating layer is fully and completely wetted. This results in an atomizing core with a vapor consumption ratio greater than 1.3, a full aroma, excellent flavor consistency, and operating noise below 40dB. Furthermore, the high strength of the metal mesh itself contributes to the excellent reliability of the atomizing core, achieving 1500 puffs without failure. The connecting layer tightly connects the heating layer to the heating substrate, preventing internal loosening of the atomizing core.

[0026] The area of ​​the heating zone is 0.8–10 mm. 2 It can maintain the surface power density within a reasonable range, providing a high mist consumption ratio and a better taste; combined with a certain heating zone shape design, it can provide better performance.

[0027] The atomizing core provided by this utility model further includes a covering layer, which is located on the side of the heating layer away from the connecting layer; the coverage area of ​​the covering layer is the heating zone. The covering layer can further improve the mist consumption ratio of the atomizing core and make the bonding between the heating layer and the substrate more precise. Attached Figure Description

[0028] To more clearly illustrate the specific embodiments of this utility model or the technical solutions in the prior art, the drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this utility model. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.

[0029] Figure 1 A top view schematic diagram of the atomizing core provided in Embodiment 1 of this utility model;

[0030] Figure 2 This is a schematic front view of the atomizing core provided in Embodiment 1 of this utility model;

[0031] Figure 3 A top view schematic diagram of the individual heating layer portion in the atomizing core provided in Embodiment 1 of this utility model;

[0032] Figure 4 The SEM image of the atomizing core provided in Embodiment 2 of this utility model without a covering layer is shown.

[0033] Figure 5 SEM image of the atomizing core provided in Embodiment 2 of this utility model;

[0034] Figure 6 This is a top view schematic diagram of the atomizing core provided in Comparative Example 2 of this utility model;

[0035] Figure 7 This is a SEM image of the atomizing core provided in Comparative Example 2 of this utility model.

[0036] Explanation of reference numerals in the attached figures:

[0037] 1-Heating substrate; 2-Connecting layer; 3-Heating layer; 301-Heating area; 302-Electrode area; 4-Electrode layer; 5-Covering layer. Detailed Implementation

[0038] The following embodiments are provided to better understand the present invention and are not limited to the preferred embodiments described herein. They do not constitute a limitation on the content and scope of protection of the present invention. Any product that is the same as or similar to the present invention, derived by any person under the guidance of the present invention or by combining the features of the present invention with other prior art, falls within the protection scope of the present invention.

[0039] In the description of this utility model, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the accompanying drawings and are only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this utility model. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0040] In the description of this utility model, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "joining" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model based on the specific circumstances.

[0041] Furthermore, the technical features involved in the different embodiments of this utility model described below can be combined with each other as long as they do not conflict with each other.

[0042] For experiments not specifically described in the examples, the procedures or conditions should be followed according to the conventional experimental procedures described in the literature in this field. Reagents or instruments whose manufacturers are not specified are all commercially available conventional reagent products.

[0043] Example 1

[0044] This embodiment provides an atomizing core, as described below. Figures 1-3 The atomizing core provided in this embodiment is described.

[0045] The atomizing core provided in this embodiment includes a heating substrate 1, a connecting layer 2 located on one side of the heating substrate 1, and a heating layer 3 located on the side of the connecting layer 2 away from the heating substrate 1;

[0046] The heating layer 3 includes a heating area 301 and an electrode area 302. The electrode area 302 is in contact with the heating area 301 and is located at both ends of the heating area 301.

[0047] The heating layer 3 includes a metal layer with holes;

[0048] The pore size of the porous metal layer is 10-100 μm, and the porosity is 25%-80%.

[0049] The area of ​​the heating zone 301 is 0.8–10 mm². 2 ;

[0050] It also includes an electrode layer 4, which covers at least a portion of the surface of the electrode region 302.

[0051] In some optional embodiments, a cover layer 5 is included, which is located on the side of the heating layer 3 away from the connecting layer 2; the coverage area of ​​the cover layer 5 is the heating area 301.

[0052] In some optional embodiments, the pore size of the connecting layer 2 is 10-60 μm, the porosity is 30%-70%, and the thickness is 30-200 μm.

[0053] In some optional embodiments, the thickness of the perforated metal layer is 20–200 μm; in some further optional embodiments, the thickness of the perforated metal layer is 20–120 μm; and in some even further optional embodiments, the thickness of the perforated metal layer is 30–80 μm.

[0054] In some optional embodiments, the porosity of the heating substrate 1 is 50% to 80%, and the pore size is 20 to 75 μm.

[0055] In some optional embodiments, the thickness of the capping layer 5 is 30–150 μm, the porosity is 35%–75%, and the pore size is 5–50 μm.

[0056] In some optional embodiments, the perforated metal layer comprises a metal mesh; in some further optional embodiments, the metal mesh comprises at least one of a woven metal mesh, a stamped metal mesh, a laser-etched metal mesh, and a chemically etched metal mesh.

[0057] In some optional embodiments, the metal material used for the porous metal layer includes at least one of stainless steel, iron-chromium-aluminum.

[0058] In some optional embodiments, the woven metal mesh comprises a rolled woven metal mesh; in some further optional embodiments, the thickness of the rolled woven metal mesh is 40% to 90% of the thickness of the woven metal mesh.

[0059] In some optional embodiments, the wire diameter of the woven metal mesh is 10-100 μm, and the mesh count of the woven metal mesh is 100-1000 mesh; in some further optional embodiments, the wire diameter of the woven metal mesh is 15-60 μm, and the mesh count of the woven metal mesh is 250-700 mesh.

[0060] Example 2

[0061] This embodiment provides an atomizing core and its preparation method. A top view of the atomizing core is shown below. Figure 1 As shown in the diagram, the main view is as follows: Figure 2 As shown, the top view of the three heating layers is as follows: Figure 3As shown. The atomizing core provided in this embodiment includes a heating substrate 1, a connecting layer 2 located on one side of the heating substrate 1, and a heating layer 3 located on the side of the connecting layer 2 away from the heating substrate 1; the heating layer 3 includes a heating area 301 and an electrode area 302, the electrode area 302 being in contact with the heating area 301 and located at both ends of the heating area 301; the heating layer 3 includes a perforated metal layer; the perforated metal layer uses a plain-weave metal mesh (total thickness approximately twice the wire diameter) made of 316L steel with a wire diameter of 38μm, 300 mesh, and 38μm; the heating area 301 consists of two metal meshes, each 3.6mm long and 0.34mm wide (the area of ​​the heating area 301 is 2.04mm²). 2 The heating layer 3 comprises two parallel metal meshes placed parallel to each other, with their ends aligned and a 0.6 mm gap in the middle. It also includes an electrode layer 4 covering at least a portion of the surface of the electrode region 302, and a cover layer 5 located on the side of the heating layer 3 away from the connecting layer 2, covering the heating region 301. The connecting layer 2 has a pore size of 42 μm, a porosity of 53%, and a thickness of 102 μm. The heating substrate 1 has a porosity of 68% and a pore size of 44 μm. The cover layer 5 has a thickness of 71 μm, a porosity of 66%, and a pore size of 15 μm.

[0062] The preparation method includes the following steps:

[0063] (1) Take a plain-weave metal wire mesh (total thickness approximately twice the wire diameter) of 316L steel with a wire diameter of 38μm, 300 mesh, and make it according to... Figure 3 The heating layer 3 pattern shown is cut into metal mesh of a certain size using laser engraving. Specifically, it includes: two metal meshes 3.6 mm long and 0.34 mm wide, used to form the heating area 301; and two metal meshes 2.5 mm long and 2.0 mm wide, used to form the electrode area 302.

[0064] (2) Preparation of bonding layer slurry: The composition is 29wt% borosilicate calcium glass powder, 30wt% alumina powder, 20wt% polystyrene spheres, and 21wt% organic carrier (the composition of the organic carrier is 12wt% ethyl cellulose, 44wt% terpineol, and 44wt% diethylene glycol butyl ether acetate, unless otherwise specified, the same applies below);

[0065] Preparation of the coating slurry: The composition is 16wt% alumina powder, 15wt% borosilicate calcium glass powder, 21wt% polystyrene spheres, and 48wt% organic carrier;

[0066] Preparation of electrode metal paste: The composition is 74 wt% silver powder, 9 wt% borosilicate zinc glass powder, and 17 wt% organic carrier (with an additional 1 wt% dispersant added by weight of the total electrode metal paste).

[0067] (3) A porous ceramic system with a porosity of 68% and a pore size of 44 μm is used as the heating substrate 1. A bonding layer slurry is coated on the heating substrate 1. The metal mesh cut in step (1) is attached to the bonding layer slurry. Two metal meshes with a length of 3.6 mm and a width of 0.34 mm are parallel to the long side of the heating substrate 1. The two metal meshes are placed parallel to each other, with the ends aligned and the middle gap 0.6 mm, forming the heating zone 301. Two metal meshes with a length of 2.5 mm and a width of 2.0 mm are placed close to the left and right ends of the two metal meshes respectively, forming the electrode zone 302. The heating zone 301 and the electrode zone 302 form the heating layer 3, which is located at the center of the heating substrate 1. A cover layer slurry is coated on the heating zone 301 and dried at 120°C for 30 min. Electrode metal slurry is coated on parts of the two electrode zones 302 and sintered at 800°C for 30 min to obtain the atomizing core.

[0068] Before applying the coating slurry, observe the SEM image of the atomizing core, see... Figure 4 After coating the slurry and sintering, SEM images of the atomizing core were observed, see [link to image]. Figure 5 It can be seen that the covering layer 5 completely covers the heating area 301.

[0069] Examples 3-7

[0070] Examples 3-7 provide an atomizing core and its preparation method. Compared with Example 2, the only difference is the metal wire mesh used, as detailed in Table 1.

[0071] Examples 8 and 9

[0072] Examples 8 and 9 provide an atomizing core and its preparation method. Compared with Example 2, the difference is that the metal mesh used is different, as detailed in Table 1; step (2) does not include the step of preparing the covering layer slurry, and step (3) does not include the step of coating the heating zone 301 with the covering layer slurry and drying it at 120°C for 30 minutes.

[0073] Example 10

[0074] Example 10 provides an atomizing core and its preparation method. Compared with Example 2, the difference is that the metal mesh used is different, as detailed in Table 1. In step (1), the metal mesh used to form the heating zone 301 is two metal meshes with a length of 3.6 mm and a width of 0.42 mm. In step (2), there is no step of preparing the covering layer slurry. In step (3), there is no step of coating the heating zone 301 with the covering layer slurry and drying it at 120°C for 30 min.

[0075] Example 11

[0076] Example 11 provides an atomizing core and its preparation method. Compared with Example 2, the difference is that the metal mesh used is different, as detailed in Table 1. In step (1), the metal mesh used to form the heating zone 301 is two metal meshes with a length of 3.6 mm and a width of 0.30 mm. In step (2), there is no step of preparing the covering layer slurry. In step (3), there is no step of coating the heating zone 301 with the covering layer slurry and drying it at 120°C for 30 min.

[0077] Example 12

[0078] Example 12 provides an atomizing core and its preparation method. Compared with Example 2, the difference is that the metal mesh used is different, as detailed in Table 1. In step (1), the metal mesh used to form the heating zone 301 is two metal meshes with a length of 3.6 mm and a width of 0.23 mm. In step (2), there is no step of preparing the covering layer slurry. In step (3), there is no step of coating the heating zone 301 with the covering layer slurry and drying it at 120°C for 30 min.

[0079] Example 13

[0080] Example 13 provides an atomizing core and its preparation method, which differs from Example 2 in that:

[0081] The connecting layer 2 has a pore size of 10 μm, a porosity of 30%, and a thickness of 30 μm. The heating substrate 1 has a porosity of 68% and a pore size of 44 μm, and is a porous ceramic based on diatomaceous earth. The capping layer 5 has a thickness of 71 μm, a porosity of 66%, and a pore size of 15 μm.

[0082] In step (1) of the preparation method, a plain weave metal wire mesh with a wire diameter of 100μm, 100 mesh, and 316L steel is used. The two metal wire meshes used to form the heating zone 301 have a length of 3.6mm and a width of 0.12mm.

[0083] In step (2) of the preparation method, the bonding layer slurry is prepared with the following components: 30wt% borosilicate calcium glass powder, 30wt% alumina powder, 12wt% polystyrene spheres, and 28wt% organic carrier.

[0084] In step (3) of the preparation method, after coating the heating zone 301 with a covering slurry, it is dried at 100°C for 60 min; after coating the two electrode zones 302 with electrode metal slurry, it is sintered at 500°C for 60 min.

[0085] Example 14

[0086] Example 14 provides an atomizing core and its preparation method, which differs from Example 2 in that:

[0087] The connecting layer 2 has a pore size of 60 μm, a porosity of 70%, and a thickness of 200 μm. The heating substrate 1 has a porosity of 68% and a pore size of 44 μm, and is a porous ceramic based on diatomaceous earth. The capping layer 5 has a thickness of 71 μm, a porosity of 66%, and a pore size of 15 μm.

[0088] In step (1) of the preparation method, a plain weave metal wire mesh with a wire diameter of 10μm, 1000 mesh, and 316L steel is used. The two metal wire meshes used to form the heating zone 301 have a length of 3.6mm and a width of 1.38mm.

[0089] In step (2) of the preparation method, the bonding layer slurry is prepared with the following components: 20wt% borosilicate calcium glass powder, 20wt% alumina powder, 29wt% polystyrene spheres, and 31wt% organic carrier.

[0090] In step (3) of the preparation method, after coating the heating zone 301 with a covering slurry, it is dried at 150°C for 20 min; after coating the two electrode zones 302 with electrode metal slurry, it is sintered at 1000°C for 20 min.

[0091] Example 15

[0092] Example 15 provides an atomizing core and its preparation method, which differs from Example 2 in that:

[0093] The connecting layer 2 has a pore size of 42 μm, a porosity of 53%, and a thickness of 102 μm. The heating substrate 1 has a porosity of 68% and a pore size of 44 μm, and is a porous ceramic based on diatomaceous earth. The capping layer 5 has a thickness of 30 μm, a porosity of 35%, and a pore size of 5 μm.

[0094] In step (1) of the preparation method, a plain weave metal wire mesh with a wire diameter of 100μm, 100 mesh, and 316L steel is used. The two metal wire meshes used to form the heating zone 301 have a length of 3.6mm and a width of 0.12mm.

[0095] In step (2) of the preparation method, the coating slurry is prepared with the following components: 19wt% alumina powder, 18wt% borosilicate calcium glass powder, 15wt% polystyrene spheres, and 48wt% organic carrier.

[0096] Example 16

[0097] Example 16 provides an atomizing core and its preparation method, which differs from Example 2 in that:

[0098] The connecting layer 2 has a pore size of 42 μm, a porosity of 53%, and a thickness of 102 μm. The heating substrate 1 has a porosity of 68% and a pore size of 44 μm, and is a porous ceramic based on diatomaceous earth. The capping layer 5 has a thickness of 150 μm, a porosity of 75%, and a pore size of 50 μm.

[0099] In step (1) of the preparation method, a plain weave metal wire mesh with a wire diameter of 100μm, 100 mesh, and 316L steel is used. The two metal wire meshes used to form the heating zone 301 have a length of 3.6mm and a width of 0.12mm.

[0100] In step (2) of the preparation method, the coating slurry is prepared with the following components: 11wt% alumina powder, 10wt% borosilicate calcium glass powder, 31wt% polystyrene spheres, and 48wt% organic carrier.

[0101] Comparative Example 1

[0102] This comparative example provides an atomizing core and its preparation method. Compared with Example 2, the only difference is the metal wire mesh used, as detailed in Table 1.

[0103] Comparative Example 2

[0104] This comparative example provides an atomizing core and its preparation method, as shown in the schematic diagram of its top view. Figure 6 As shown, it includes the following steps:

[0105] A porous ceramic based on diatomaceous earth with a porosity of 68% and a pore size of 44 μm was used as the heating substrate 1.

[0106] A silver-palladium alloy slurry was prepared, consisting of 78 wt% silver-palladium powder, 2.5 wt% ethyl cellulose, 17.5 wt% terpineol, and 2 wt% organic additives.

[0107] Preparation of silver paste electrode paste: The composition is 75wt% silver powder, 5wt% glass powder, 2.5wt% ethyl cellulose, 16.5wt% terpineol, and 1wt% organic additives.

[0108] The prepared silver-palladium alloy paste is screen-printed onto the surface of the heating substrate 1 in an "S" shape. After settling and drying at 120°C for 30 minutes, some of the silver-palladium alloy paste is allowed to penetrate into the porous ceramic substrate. The substrate is then sintered at 880°C for 40 minutes. The thickness of the sintered silver-palladium alloy heating layer 3 penetrating into the heating substrate 1 is 50–120 μm, and its thickness above the surface of the heating substrate 1 is 7–12 μm. Silver paste is printed at both ends of the "S"-shaped heating layer 3, and the substrate is sintered at 800°C for 40 minutes to form the electrode layer 4, thus obtaining the atomizing core. The two electrodes in the electrode layer 4 are 2.5 mm wide in the width direction and 2 mm long in the length direction of the heating substrate 1.

[0109] SEM images of the atomizer core prepared in Comparative Example 2 are shown below. Figure 7 It can be seen that the sintered silver-palladium alloy heating layer 3 exhibits a porous structure.

[0110] Comparative Example 3

[0111] Comparative Example 3 provides an atomizing core and its preparation method. Compared with Example 2, the difference is that the metal mesh used is different, as detailed in Table 1. In step (2), there is no step of preparing the covering layer slurry, and in step (3), there is no step of coating the heating zone 301 with the covering layer slurry and drying it at 120°C for 30 minutes. In step (1), the metal mesh used to form the heating zone 301 is cut into two metal meshes with a length of 3.6 mm and a width of 1.53 mm.

[0112] Comparative Example 4

[0113] Comparative Example 4 provides an atomizing core and its preparation method. Compared with Example 2, the difference is that the metal mesh used is different and the step of preparing the covering layer 5 is not performed. See Table 1 for details. In step (1), the metal mesh used to form the heating zone 301 is cut into a whole piece of metal mesh with a length × width of 6.2 mm × 3.2 mm.

[0114] Table 1

[0115]

[0116] Test Example 1

[0117] The atomizing cores prepared in Examples 2 to 16 and the comparative examples were assembled into complete electronic atomizers. The working power of the atomizing cores prepared in the examples and the comparative examples was 7.5W. They were filled with watermelon ice e-liquid (produced by Shenzhen Zhenwei Biotechnology Co., Ltd.) and their vapor consumption ratio, vaping noise, 1500 puff lifespan and vaping taste were tested.

[0118] The mist consumption ratio is the ratio of aerosol volume to the working power of the atomizing coil. The higher the ratio, the higher the atomization efficiency. The mist consumption ratio test method is as follows: Use an automatic suction machine to test the total aerosol volume for 500 puffs, then calculate the aerosol volume per puff (mg / puff), and finally divide by the working power of 7.5W to obtain the mist consumption ratio (mg / W).

[0119] Suction noise: The noise during the suction of the atomizing core is tested using a sound pressure meter.

[0120] 1500 puff lifespan: This test measures the number of 50 atomizer cores that fail after 1500 puffs.

[0121] Taste evaluation: The taste is scored by professional tasters, with a maximum score of 100.

[0122] The test results are shown in Table 2.

[0123] Table 2

[0124] sample Fog consumption ratio Suction lifespan Suction noise (dB) Taste rating Example 2 1.41 0 36.1 95 Example 3 1.41 0 36.2 95 Example 4 1.42 0 36.1 95 Example 5 1.41 0 37.3 95 Example 6 1.42 0 37.1 95 Example 7 1.43 0 37.4 95 Example 8 1.36 0 37.3 90 Example 9 1.34 0 36.3 90 Example 10 1.36 0 36.5 90 Example 11 1.35 0 36.1 90 Example 12 1.37 0 36.2 90 Example 13 1.33 0 38.2 90 Example 14 1.34 0 38.5 90 Example 15 1.35 0 38.3 90 Example 16 1.36 0 38.6 90 Comparative Example 1 1.2 0 50.5 70 Comparative Example 2 1.1 5 51.2 70 Comparative Example 3 0.9 0 36.5 70 Comparative Example 4 0.7 0 36.6 60

[0125] As shown in Table 2, the atomizing cores of Examples 2-16 all exhibit excellent performance. Examples 2, 4, 6, and 8 use metal mesh with the same wire diameter and mesh count, as do Examples 3, 5, 7, 9, 10, 11, and 12. Examples 2-7 are schemes with a covering layer 5, and their mist consumption ratio is slightly higher than that of Examples 8-12 without a covering layer 5. Examples 13-16 are affected by the selected metal mesh wire diameter and mesh count; although a covering layer 5 is present, their mist consumption ratio is relatively low. Comparative Example 1 uses a 66-micron diameter, 150-mesh wire mesh, meaning its pore size is >100μm. Its mist consumption ratio is significantly lower, and its suction noise is significantly higher, indicating that when the pore size is too large, it affects the transmission of the liquid medium, thereby reducing the amount of atomized mist, the mist consumption ratio, and significantly increasing the suction noise. The applicant speculates that the reason for the loud suction noise is that when the orifice is too large, a thick liquid film will be generated. The liquid film obstructs the transmission of flue gas, thereby producing a loud splattering sound, which makes the suction noise too loud.

[0126] Comparative Example 2 has a poor suction life. In addition, due to the uneven size and distribution of pores on the heating layer 3, it causes a loud splattering sound, resulting in excessive suction noise. Furthermore, its taste score is not as good as that of the Example.

[0127] Example 10 uses a twill woven rolled wire mesh with a wire diameter of 25μm, 500 mesh, and 316L material, without the cover layer (scheme 5), and has an area power density of 2.5W / mm². 2 Example 11 uses a twill woven rolled wire mesh with a wire diameter of 20μm, 500 mesh, and 316L material, without a cover layer (scheme 5), and has an area power density of 3.5W / mm². 2 Example 12 uses a twill woven rolled wire mesh with a wire diameter of 25μm, 500 mesh, and 316L material, without a cover layer (scheme 5), and has an area power density of 4.5W / mm². 2 As shown in Table 2, the atomizing cores of Examples 10-16 all exhibit excellent performance. Comparative Example 3 has a larger heating zone 301 area and lower surface power density, resulting in a significantly lower vapor consumption ratio and a noticeably inferior taste compared to the Examples. Comparative Example 4 uses a heating layer 3 covering the entire atomizing surface; due to its even lower surface power density, its vapor consumption ratio and taste are even worse than Comparative Example 3.

[0128] Test Example 2

[0129] The adhesion of the heating layer 3 was tested using atomizing cores prepared in Examples 2-16 and the comparative examples. The testing method included: fixing the atomizing core to a specialized fixture, applying 3M tape to ensure tight contact with the core, then peeling off the tape at a 60-90 degree angle, and observing whether the heating layer 3 detached. Ten atomizing cores were tested, and no detachment of the heating layer 3 was allowed after a single test. Multiple tests were performed on the same samples, and the adhesion was quantified based on the number of tests that resulted in detachment. Detailed test data are shown in Table 3.

[0130] Table 3

[0131]

[0132]

[0133] In Examples 6-9, the heating layer 3 uses rolled metal mesh, and the limit number of adhesion tests is 3; in other examples, unrolled metal mesh is used, and the limit number of adhesion tests is 2, indicating that rolled wire mesh has a better bonding effect.

[0134] Obviously, the above embodiments are merely illustrative examples for clear explanation and are not intended to limit the implementation. Those skilled in the art will recognize that other variations or modifications can be made based on the above description. It is neither necessary nor possible to exhaustively list all possible implementations here. However, obvious variations or modifications derived therefrom are still within the scope of protection of this invention.

Claims

1. An atomizing core, characterized in that, It includes a heating substrate, a connecting layer located on one side of the heating substrate, and a heating layer located on the side of the connecting layer away from the heating substrate; The heating layer includes a heating area and an electrode area, wherein the electrode area is in contact with the heating area and is located at both ends of the heating area; The heating layer includes a porous metal layer; The pore size of the porous metal layer is 10-100 μm, and the porosity is 25%-80%. The area of ​​the heating zone is 0.8–10 mm. 2 ; It also includes an electrode layer that covers at least a portion of the surface of the electrode region.

2. The atomizing core according to claim 1, characterized in that, It also includes a cover layer, which is located on the side of the heating layer away from the connecting layer; The coverage area of ​​the covering layer is the heating zone.

3. The atomizing core according to claim 1, characterized in that, The pore size of the connecting layer is 10–60 μm, the porosity is 30%–70%, and the thickness is 30–200 μm.

4. The atomizing core according to claim 1, characterized in that, The thickness of the porous metal layer is 20–200 μm; And / or, the thickness of the capping layer is 30–150 μm, the porosity is 35%–75%, and the pore size is 5–50 μm; And / or, the porous metal layer comprises a metal mesh; And / or, the metal material used in the porous metal layer includes at least one of stainless steel, iron-chromium-aluminum.

5. The atomizing core according to claim 4, characterized in that, The thickness of the porous metal layer is 20–120 μm; And / or, the metal mesh includes at least one of woven metal mesh, stamped metal mesh, laser-etched metal mesh, and chemically etched metal mesh.

6. The atomizing core according to claim 5, characterized in that, The thickness of the porous metal layer is 30–80 μm.

7. The atomizing core according to claim 5, characterized in that, The woven metal mesh includes rolled woven metal mesh; And / or, the wire diameter used in the woven metal mesh is 10 to 100 μm, and the mesh count of the woven metal mesh is 100 to 1000 mesh.

8. The atomizing core according to claim 7, characterized in that, The thickness of the rolled woven metal mesh is 40% to 90% of that of the woven metal mesh.

9. The atomizing core according to claim 7, characterized in that, The diameter of the metal wire used in the woven metal mesh is 15-60 μm, and the mesh count of the woven metal mesh is 250-700 mesh.

10. An atomizer, characterized in that, Includes the atomizing core as described in any one of claims 1 to 9.