A wear-resistant repair tool for a cyclone inlet section

By installing wear-resistant repair fixtures with cast stone plates and metal mesh structures in the hydrocyclone feed section, the problems of short service life and high maintenance costs of the hydrocyclone feed body are solved, achieving long service life and low-cost operation of the equipment.

CN224951346UActive Publication Date: 2026-11-10YANKUANG ENERGY GRP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522596838.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-08
Publication Date
2026-11-10
Estimated Expiration
2035-12-08

AI Technical Summary

Technical Problem

The second-stage feed body of the hydrocyclone has a short service life, high maintenance costs, and frequent shutdowns affect production continuity. Existing modification solutions are either costly or ineffective.

Method used

Wear-resistant repair fixtures are installed in the wear area of ​​the hydrocyclone feed section. The fixtures consist of cast stone plates and metal mesh structures, which are fixed by spot welding and wear-resistant adhesive to form a tightly fitting support layer.

Benefits of technology

It extends the service life of the feed body, reduces the wear rate and maintenance frequency, and reduces equipment downtime and maintenance costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224951346U_ABST
    Figure CN224951346U_ABST
Patent Text Reader

Abstract

The utility model provides a kind of wear-resistant repair tool for cyclone inlet section, more particularly to equipment maintenance technical field.The tool is installed on the outer side wall of the wear area of cyclone inlet section, including two side fixed plates, several horizontal rib plates and several longitudinal rib plates;Several horizontal rib plates are equidistantly arranged between the two side fixed plates;Several cast stone plates are tightly laid between the two adjacent horizontal rib plates;Several longitudinal rib plates are equidistantly arranged on the side of several horizontal rib plates away from the outer side wall of the inlet section, and several horizontal rib plates and several longitudinal rib plates form a grid structure.The utility model effectively solves the problem of frequent replacement of the inlet body affecting production efficiency and high cost by laying cast stone plates on the surface of the wear area of the inlet section combined with metal grid structure, greatly reduces the number of equipment downtime, and ensures the continuity of production process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of equipment maintenance technology, specifically to a wear-resistant repair tool for the feed section of a hydrocyclone. Background Technology

[0002] Hydrocyclones are core equipment in coal preparation processes, with their secondary feed section playing a crucial role in material conveying and diversion. In actual operation, the secondary feed section is subjected to the scouring of high-concentration, high-velocity materials (such as coal slurry and gangue particles) for extended periods, resulting in extremely rapid wear on its easily worn parts (such as the inner wall of the feed inlet and the diversion chamber).

[0003] The existing two-stage feed body has the following problems: 1. Short service life: Traditional feed bodies use ordinary steel or simple wear-resistant coatings, with an average service life of only 2 months, requiring frequent replacement; 2. High maintenance costs: The cost of spare parts for a single set of feed bodies (including the body and seals) is 800 yuan, and the annual spare parts cost for one set of equipment reaches 4,800 yuan. At the same time, replacement requires 2 maintenance workers and takes 1 day, with a labor cost of 600 yuan per replacement; 3. Frequent production interruptions: Each replacement causes the equipment to be shut down for more than 8 hours, affecting the continuity of the coal preparation process, with an annual cumulative downtime of more than 72 hours.

[0004] Existing renovation solutions use high-chromium alloy feedstocks (renovation cost of 3,000 yuan per set, which is too expensive) or a single ceramic coating (poor adhesion, which peels off within 3 months), which cannot simultaneously achieve "low cost" and "long lifespan".

[0005] Therefore, there is an urgent need for a wear-resistant repair solution that is low-cost, easy to operate, and can effectively extend the service life of the feed body in the second stage of the hydrocyclone to solve the above-mentioned technical problems. Utility Model Content

[0006] To overcome the shortcomings of the prior art, this utility model provides a wear-resistant repair tooling for the feed section of a hydrocyclone, the specific technical solution of which is as follows: A wear-resistant repair tooling for the feed section of a hydrocyclone is used to install on the outer wall of the wear area of ​​the feed section of the hydrocyclone. It includes two side fixing plates, several transverse stiffeners and several longitudinal stiffeners. The transverse stiffeners are evenly spaced between the two side fixing plates. Several cast stone plates are tightly laid between adjacent transverse stiffeners. The longitudinal stiffeners are evenly spaced on the side of the transverse stiffeners away from the outer wall of the feed section. The transverse stiffeners and the longitudinal stiffeners form a grid structure.

[0007] Preferably, the two side fixing plates and several transverse stiffeners are tightly fitted to the outer wall of the feed section and fixed by spot welding; the longitudinal stiffeners and the transverse stiffeners are fixed by spot welding.

[0008] Preferably, several of the cast stone plates are bonded and fixed to the transverse stiffeners and the outer wall of the feed section with wear-resistant adhesive, and the gaps are further filled with wear-resistant adhesive.

[0009] Preferably, the thickness of the cast stone slab is 20±1mm.

[0010] Preferably, the thickness of the wear-resistant adhesive is 2 mm.

[0011] More preferably, both the transverse stiffeners and the longitudinal stiffeners are made of Q355 steel.

[0012] More preferably, several of the cast stone plates are pre-processed according to the three-dimensional dimensions of the wear area of ​​the feed section to ensure the fit between each cast stone plate and the outer wall of the feed section.

[0013] The beneficial effects of this utility model are: This invention involves densely laying several cast stone slabs in conjunction with a metal mesh structure in the wear area of ​​the feed section. This improves the adhesion of the cast stone slabs and forms a support and repair layer that fits tightly against the outer wall of the feed section in the wear area. If the feed section is damaged, there is no need to replace the entire section to solve the problems of material leakage and unstable flow rate. The high-alumina cast stone slabs, with their high hardness and strong wear resistance, can withstand the impact of materials through their own strength, thus solving the problems of high cost and limited service life caused by the need for complete replacement of the traditional feed section once it is damaged. Attached Figure Description

[0014] The accompanying drawings constituting this utility model are provided to further understand this application and do not constitute an undue limitation on this application.

[0015] Figure 1 This is a schematic diagram of the overall structure of this utility model; In the diagram, 1-side fixing plate; 2-transverse stiffener; 3-longitudinal stiffener; 4-cast stone plate. Detailed Implementation

[0016] The following description, in conjunction with the accompanying drawings and embodiments, further illustrates the specific implementation of a wear-resistant repair tool for the feed section of a hydrocyclone provided by this utility model.

[0017] like Figure 1 As shown, a wear-resistant repair tooling for the feed section of a hydrocyclone is used for installation on the outer wall of the wear area of ​​the feed section. Specifically, it includes two side fixing plates 1, several transverse stiffeners 2, and several longitudinal stiffeners 3; the transverse stiffeners 2 are evenly spaced between the two side fixing plates 1. Several cast stone plates 4 are tightly laid between adjacent transverse stiffeners 2; the longitudinal stiffeners 3 are evenly spaced on the side of the transverse stiffeners 2 away from the outer wall of the feed section, and the transverse stiffeners 2 and longitudinal stiffeners 3 form a grid structure, further improving the adhesion and stability of the cast stone plates 4.

[0018] It is worth noting that the two side fixing plates 1 and the several transverse stiffeners 2 are all tightly fitted to the outer wall of the feed section and fixed by spot welding; the longitudinal stiffeners 3 are fixed to the transverse stiffeners 2 by spot welding. Several cast stone plates 4 are pre-processed according to the three-dimensional dimensions of the wear area of ​​the feed section to ensure the fit between each cast stone plate 4 and the outer wall of the feed section. Preferably, the spacing between the weld points is 50mm.

[0019] Preferably, several cast stone slabs 4 are bonded and fixed to the transverse stiffeners 2 on both sides and the outer wall of the feed section using a special wear-resistant adhesive. Simultaneously, the gaps around the perimeter are further filled with wear-resistant adhesive to ensure a tight bond. The thickness of the cast stone slab is 20±1mm. The thickness of the wear-resistant adhesive is 2mm.

[0020] More preferably, both the transverse stiffener 2 and the longitudinal stiffener 3 are made of Q355 steel.

[0021] During installation, first use a 0.8MPa high-pressure water gun to clean the coal sludge and rust on the outer wall of the wear area of ​​the feed body, then sand it with sandpaper and wipe it clean with a cloth. Check that the surface flatness error is ≤0.5mm. Next, the side fixing plate is welded and fixed to the outer wall of the feeding section, and several transverse stiffeners are fixed between the two side fixing plates by spot welding, with the weld spacing less than or equal to 50mm. Next, several pre-cut cast stone slabs, based on the three-dimensional dimensions of the side wall of the feeding section, are tightly laid between each pair of adjacent transverse stiffeners using a special wear-resistant adhesive. It is worth noting that the special wear-resistant adhesive is applied evenly with a thickness of 2mm, and the cast stone slabs are placed one by one and pressed for more than 30 seconds to ensure a tight fit with the outer wall of the feeding section. To further improve adhesion, the gaps around each cast stone slab are filled with wear-resistant adhesive.

[0022] Finally, several longitudinal stiffeners are spot-welded at equal intervals to the side of several transverse stiffeners away from the outer wall of the feed section.

[0023] After installation, this utility model can also be further improved by using several fastening bolts to pass through the longitudinal stiffening plate, the cast stone plate, the transverse stiffening plate and the side wall of the feeding section in sequence, and then fastening it to the side wall of the feeding section with nuts, so as to further improve the fastness of the cast stone plate 4 on the outer wall of the feeding section.

[0024] After installation, check each cast stone slab for cracks or warping and clean up any excess wear-resistant adhesive. Run the hydrocyclone under no-load for 2 hours. Adjust the vibration value to 0.08 mm / s. If there is no abnormal noise, the installation is considered qualified.

[0025] The beneficial effects of this utility model are further explained below based on actual operational results: Feed body wear: Before the modification, the monthly wear was 1.2mm; after the modification, the monthly wear was 0.3mm, and the wear rate was reduced by 75%. Maintenance cycle: extended from 2 months to 8.5 months, far exceeding the design target; Equipment downtime frequency: Before the upgrade, the equipment stopped once a month; after the upgrade, it stopped once every 8 months, reducing the downtime frequency by 87.5%.

[0026] In this utility model, terms such as "upper," "lower," "bottom," and "top" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. These terms are merely used to facilitate the description of the structural relationships of the various components or elements of this utility model and do not specifically refer to any part or element of this utility model; they should not be construed as limiting this utility model. Terms such as "connected" and "linked" should be interpreted broadly, indicating a fixed connection, an integral connection, or a detachable connection; a direct connection or an indirect connection through an intermediate medium. For those skilled in the art, the specific meaning of the above terms in this utility model can be determined according to the specific circumstances, and they should not be construed as limiting this utility model.

[0027] Of course, the above description is not intended to limit the present utility model, and the present utility model is not limited to the examples given above. Any changes, modifications, additions or substitutions made by those skilled in the art within the scope of the present utility model should also fall within the protection scope of the present utility model.

Claims

1. A wear-resistant repair tooling for the feed section of a hydrocyclone, used for installation on the outer wall of the wear area of ​​the feed section of the hydrocyclone, characterized in that, It includes two side fixing plates, several transverse stiffeners, and several longitudinal stiffeners; Several transverse stiffeners are evenly spaced between two side fixing plates; several cast stone slabs are tightly laid between adjacent transverse stiffeners; Several longitudinal stiffeners are evenly spaced on the side of several transverse stiffeners away from the outer wall of the feed section, and the several transverse stiffeners and several longitudinal stiffeners form a grid structure.

2. The wear-resistant repair tooling for the feed section of a hydrocyclone according to claim 1, characterized in that, The two side fixing plates and several transverse stiffeners are tightly fitted to the outer wall of the feed section and fixed by spot welding; The longitudinal stiffeners and the transverse stiffeners are fixed together by spot welding.

3. The wear-resistant repair tooling for the feed section of a hydrocyclone according to claim 1, characterized in that, Several of the cast stone slabs are bonded and fixed to the transverse stiffeners and the outer wall of the feed section with wear-resistant adhesive, and the gaps are further filled with wear-resistant adhesive.

4. The wear-resistant repair tooling for the feed section of a hydrocyclone according to claim 3, characterized in that, The thickness of the cast stone slab is 20±1mm.

5. The wear-resistant repair tooling for the feed section of a hydrocyclone according to claim 4, characterized in that, The thickness of the wear-resistant adhesive is 2 mm.

6. The wear-resistant repair tooling for the feed section of a hydrocyclone according to claim 1, characterized in that, Both the transverse stiffeners and the longitudinal stiffeners are made of Q355 steel.

7. The wear-resistant repair tooling for the feed section of a hydrocyclone according to claim 5, characterized in that, Several of the cast stone plates are pre-processed according to the three-dimensional dimensions of the wear area of ​​the feed section to ensure the fit between each cast stone plate and the outer wall of the feed section.