A battery cell and battery pack

By setting multiple recessed structures and extended holes on the surface of a single electrode, the problem of decreased cycle performance caused by electrode wrinkles in the battery cell is solved, the insulation and conductivity of the battery cell are improved, and the service life of the battery cell is extended.

CN224958681UActive Publication Date: 2026-11-10SUNWODA MOBILITY ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522437313.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-17
Publication Date
2026-11-10
Estimated Expiration
2035-11-17

AI Technical Summary

Technical Problem

As the number of battery cell cycles increases, the wrinkles on the electrode plates become more pronounced, affecting the cell's cycle performance.

Method used

Multiple recessed structures are set on the surface of a single electrode, extending inward to form multiple interconnected extended hole segments. The cross-sectional area of ​​the hole segment near the bottom of the groove is smaller than that of the hole segment far from the bottom of the groove, so as to reserve expansion space and disperse expansion stress.

Benefits of technology

It alleviates the problems of electrode deformation and wrinkling, improves the insulation performance of the cell, shortens the liquid injection time, enhances the conductivity and cycle capacity retention of the cell, and extends the service life of the cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224958681U_ABST
    Figure CN224958681U_ABST
Patent Text Reader

Abstract

This application provides a battery cell and a battery pack, relating to the field of battery technology. The battery cell includes an electrode assembly; the electrode assembly includes multiple single electrode sheets wound or stacked, with the thickness direction of each single electrode sheet being a first direction; at least one surface of each single electrode sheet has multiple spaced-apart recessed structures, the recessed structures extending from the surface of the single electrode sheet into the interior of the single electrode sheet to form a groove bottom; the recessed structure includes interconnected first and second hole segments, the second hole segment being located on the side of the first hole segment facing the groove bottom; the cross-sectional area of ​​the second hole segment perpendicular to the first direction is smaller than the cross-sectional area of ​​the first hole segment perpendicular to the first direction. In the single-cell battery of this application, by making the cross-sectional area of ​​the extended hole segment near the groove bottom perpendicular to the first direction smaller than the cross-sectional area of ​​the extended hole segment away from the groove bottom perpendicular to the first direction, the ability of the recessed structure to disperse the expansion stress of the electrode sheet is improved, alleviating the wrinkling phenomenon of the electrode sheet.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application belongs to the field of battery technology, specifically relating to a battery cell and a battery pack. Background Technology

[0002] As a core energy storage device with cyclic charging and discharging capabilities, the battery cell can efficiently store and release electrical energy. The charging and discharging function of the battery cell relies on the chemical reaction between its internal electrodes and electrolyte, thereby achieving the bidirectional conversion of electrical energy and chemical energy.

[0003] During battery cell charging, the electrode plates expand, leading to electrode wrinkling. As the number of battery cell cycles increases, the wrinkling of the electrode plates becomes more pronounced, adversely affecting the cycle performance of the battery cell. Utility Model Content

[0004] This application aims to provide a battery cell and battery pack that at least solves the problem that as the number of battery cell cycles increases, the wrinkling of the electrode sheets becomes more and more significant, affecting the cycle performance of the battery cell.

[0005] To solve the above-mentioned technical problems, this application is implemented as follows: In a first aspect, embodiments of this application provide a battery cell including an electrode assembly; The electrode assembly includes an electrode sheet, which is wound or stacked. The electrode sheet includes multiple single electrode sheets, and the thickness direction of the single electrode sheet is a first direction. At least one side surface of the single electrode sheet is provided with a plurality of spaced recessed structures, the recessed structures extending from the surface of the single electrode sheet into the interior of the single electrode sheet to form a groove bottom; The recessed structure includes a first hole segment and a second hole segment connected to each other, the second hole segment being located on the side of the first hole segment facing the bottom of the groove; the cross-sectional area of ​​the second hole segment in the direction perpendicular to the first direction is smaller than the cross-sectional area of ​​the first hole segment in the direction perpendicular to the first direction.

[0006] Optionally, a stepped surface is formed at the junction of the second hole segment and the first hole segment, and the stepped surface is arranged circumferentially around the second hole segment.

[0007] Optionally, the monolithic electrode includes a current collector and an active material layer; the active material layer is disposed on at least one side of the current collector, and the recessed structure is disposed in the active material layer.

[0008] Optionally, the current collector has a groove portion located on the side of the current collector facing the active material layer; the active material layer is at least partially embedded in the groove portion.

[0009] Optionally, along the first direction, the orthogonal projection of the recessed structure onto the current collector covers the groove portion.

[0010] Optionally, the current collector has a protrusion that protrudes from the side of the current collector away from the recessed structure; along the first direction, the orthographic projection of the protrusion on the current collector at least partially overlaps with the orthographic projection of the recess on the current collector.

[0011] Optionally, the single electrode has a first side and a second side disposed opposite to each other, and both the first side and the second side are provided with the recessed structure; Along the first direction, the orthographic projection of the recessed structure on the second side onto the monolithic electrode is spaced apart from the orthographic projection of the recessed structure on the first side onto the monolithic electrode.

[0012] Optionally, multiple single electrode sheets are wound to form the electrode assembly, each single electrode sheet having a bending region, and the recessed structure is provided at least in the bending region.

[0013] Optionally, along the first direction, the depth of the recessed structure is less than or equal to 22 μm.

[0014] Secondly, embodiments of this application propose a battery pack comprising: a battery cell as described in any of the first aspects.

[0015] In the embodiments of this application, by providing multiple spaced recessed structures on at least one side surface of the monolithic electrode, and extending these recessed structures from the surface of the monolithic electrode towards its interior, expansion space is reserved for the monolithic electrode to absorb its expansion, thereby alleviating the wrinkling problem caused by deformation of the monolithic electrode. Simultaneously, by including multiple interconnected extended hole segments in the recessed structure, and by ensuring that the cross-sectional area of ​​the extended hole segment near the bottom of the groove in the direction perpendicular to the first direction is smaller than that of the extended hole segment away from the bottom of the groove in the same direction, the complexity of the sidewalls extending from the surface of the monolithic electrode towards its interior in the recessed structure is increased. This enhances the ability of the recessed structure to disperse the expansion stress of the monolithic electrode, reduces the amount of expansion generated by the monolithic electrode, and further alleviates the wrinkling phenomenon of the monolithic electrode.

[0016] Additional aspects and advantages of this invention will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the accompanying drawings used in the description of the embodiments will be briefly introduced below, wherein: Figure 1 This is a schematic diagram of the battery cell structure provided in an embodiment of this application; Figure 2 Schematic diagram of the electrode assembly provided in the embodiments of this application Figure 1 ; Figure 3 Schematic diagram of the electrode assembly provided in the embodiments of this application Figure 2 ; Figure 4 for Figure 3 Sectional view of part A shown Figure 1 ; Figure 5 Schematic diagram of the electrode structure provided in the embodiments of this application Figure 1 ; Figure 6 Schematic diagram of the electrode structure provided in the embodiments of this application Figure 2 ; Figure 7 This is a schematic diagram of the structure of the embossing roller provided in the embodiments of this application; Figure 8 for Figure 3 Sectional view of part A shown Figure 2 ; Figure 9 for Figure 3 Sectional view of part A shown Figure 3 ; Figure 10 Schematic diagram of the electrode assembly provided in the embodiments of this application Figure 3 ; Figure 11 Schematic diagram of the electrode assembly provided in the embodiments of this application Figure 4 .

[0018] Figure label: 100: Electrode assembly; 101: Positive electrode; 102: Separator; 103: Negative electrode; 110: Electrode; 110a: Groove bottom; 110b: Opening; 110c: First side; 110d: Second side; 110e: Bending area; 111: Single electrode; 1111: Current collector; 111a: Groove portion; 111b: Protrusion portion; 1112: Active material layer; 120: Recessed structure; 121: Extended hole section; 121a: First hole section; 121b: Second hole section; 121c: Stepped surface; 121d: Third hole section; 121e: Fourth hole section; 121f: Fifth hole section; 200: Housing; 300: Top cover; 400: Embossing roller; 410: Roller body; 420: Embossing section; 421: Boss structure; h1: First depth; h2: Second depth; h3: Third depth; H: Total depth; M: First direction. Detailed Implementation

[0019] The embodiments of this utility model will now be described in detail. Examples of these embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain this utility model, and should not be construed as limiting this utility model. All other embodiments obtained by those skilled in the art based on the embodiments in this application without inventive effort are within the scope of protection of this application.

[0020] The terms "first" and "second" in the specification and claims of this application may explicitly or implicitly include one or more of the features. In the description of this utility model, unless otherwise stated, "a plurality of" means two or more. Furthermore, in the specification and claims, "and / or" indicates at least one of the connected objects, and the character " / " generally indicates that the preceding and following objects are in an "or" relationship.

[0021] In the description of this utility model, it should be understood that the terms "center", "longitudinal", "transverse", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc., indicating the orientation or positional relationship are based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this utility model and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this utility model.

[0022] In the description of this utility model, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "joining" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model based on the specific circumstances.

[0023] The single battery and battery pack provided in this application will be described in detail below with reference to the accompanying drawings, through specific embodiments and application scenarios.

[0024] like Figures 1-5As shown, a battery cell provided according to some embodiments of this application includes an electrode assembly 100; the electrode assembly 100 includes electrode sheets 110, which are wound or stacked, and the electrode sheets 110 include multiple single electrode sheets 111, the thickness direction of the single electrode sheet 111 being a first direction M; at least one side surface of the single electrode sheet 111 is provided with a plurality of spaced recessed structures 120, the recessed structures 120 extending from the surface of the single electrode sheet 111 toward the interior of the single electrode sheet 111 to form a groove bottom 110a; the recessed structure 120 includes a first hole segment 121a and a second hole segment 121b connected to each other, the second hole segment 121b being disposed on the side of the first hole segment 121a facing the groove bottom 110a; the cross-sectional area of ​​the second hole segment 121b in the direction perpendicular to the first direction M is smaller than the cross-sectional area of ​​the first hole segment 121a in the direction perpendicular to the first direction M.

[0025] In one embodiment, the battery cell includes a housing 200, and an electrode assembly 100 is disposed within the housing 200.

[0026] In the embodiments of this application, by providing a plurality of spaced recessed structures 120 on at least one side surface of the single electrode 111, and extending the recessed structures 120 from the surface of the single electrode 111 to the interior of the single electrode 111, expansion space is reserved for the single electrode 111 to absorb the expansion of the single electrode 111, thereby alleviating the wrinkling problem caused by deformation of the single electrode 111. Meanwhile, by making the recessed structure 120 include a first hole segment 121a and a second hole segment 121b that are interconnected, and by making the cross-sectional area of ​​the second hole segment 121b near the bottom of the groove 110a in the direction perpendicular to the first direction M smaller than the cross-sectional area of ​​the first hole segment 121a away from the bottom of the groove 110a in the direction perpendicular to the first direction M, the complexity of the sidewalls extending from the surface of the single electrode 111 to the interior of the single electrode 111 in the recessed structure 120 is increased, thereby improving the ability of the recessed structure 120 to disperse the expansion stress of the single electrode 111, reducing the amount of expansion generated by the single electrode 111, and further alleviating the wrinkling phenomenon of the single electrode 111.

[0027] Specifically, the electrode 110 includes multiple single electrode sheets 111. In the structure of the electrode assembly 100 formed by stacking the electrode sheets 110, the multiple single electrode sheets 111 specifically include multiple positive electrode sheets 101 and multiple negative electrode sheets 103. The multiple positive electrode sheets 101 and multiple negative electrode sheets 103 are stacked alternately, and adjacent positive electrode sheets 101 and negative electrode sheets 103 are separated by a separator 102.

[0028] In the structure of the electrode assembly 100 formed by winding the electrode sheets 110, the multiple single electrode sheets 111 specifically include a positive electrode sheet 101 and a negative electrode sheet 103. The positive electrode sheet 101, the separator 102, and the negative electrode sheet 103 are stacked and then wound to form the electrode assembly 100. In the unfolded state, the single electrode sheet 111 has a sheet-like structure, and the first direction M refers to the thickness direction of the sheet-like single electrode sheet 111.

[0029] The battery cell includes a housing 200, with the electrode assembly 100 located within the internal space of the housing 200. There is no direct fixed connection between the two, or the housing 200 encapsulates and fixes the electrode assembly 100. The housing 200 serves to isolate, protect, and fix the electrode assembly 100. The shape of the housing 200 is adapted to the shape of the electrode assembly 100 to enclose it. For example, if the electrode assembly 100 is formed by winding a single electrode sheet 111 into a cylindrical or flat cylindrical shape, the housing 200 will also be cylindrical or flat cylindrical accordingly; if the electrode assembly 100 is formed by stacking single electrode sheets 111 into a layered block shape, the housing 200 will be strip-shaped or rectangular. Furthermore, the battery cell also includes a top cover 300, which is connected to one side of the housing 200.

[0030] In one embodiment, the monolithic electrode 111 has a recessed structure 120 as a functional structure. The recessed structure 120 is formed on one or both surfaces of the monolithic electrode 111 and does not penetrate the other surface of the monolithic electrode 111. The recessed structure 120 can be provided on one side of the surface of the monolithic electrode 111, that is, the recessed structure 120 is only provided on one side surface of the monolithic electrode 111; the recessed structure 120 can also be provided on both sides opposite to each other, that is, the recessed structure 120 is provided at corresponding positions on both sides of the monolithic electrode 111; the recessed structure 120 can also be provided on both sides spaced apart, that is, the recessed structure 120 is provided at corresponding positions on both sides of the monolithic electrode 111, but the center positions of the recessed structures 120 on both sides are staggered to avoid insufficient local strength of the monolithic electrode 111.

[0031] Furthermore, the recessed structure 120 is integrally formed with the single electrode 111, meaning it is formed by recessing the material of the single electrode 111 itself, without any additional splicing parts. The processing method of the recessed structure 120 can be stamping, laser engraving, or etching. The recessed structure 120 is a hole-like structure recessed into the single electrode 111. Multiple recessed structures 120 are spaced apart along the surface of the single electrode 111, and the spacing can be arrayed, staggered, or random. Meanwhile, as... Figure 8 As shown, multiple recessed structures 120 can be provided on a portion of the monolithic electrode 111; or, as... Figure 9 As shown, multiple recessed structures 120 can also be provided in all areas of a single electrode 111.

[0032] In one embodiment, the recessed structure 120 has a groove bottom 110a extending along the first direction M into the interior of the single electrode 111. The groove bottom 110a is the end region of the recessed structure 120, corresponding to the extreme position of the extension of the recessed structure 120. The groove bottom 110a can be a plane, an arc surface, or a stepped surface. The orthographic projection shape of the groove bottom 110a perpendicular to the first direction M onto the single electrode 111 can be circular, square, elliptical, or polygonal, etc. Simultaneously, the recessed structure 120 extends from the surface of the single electrode 111 into its interior, forming an opening 110b on the surface of the single electrode 111. The orthographic projection shape of the opening 110b along the first direction M onto the single electrode 111 can be the same as or different from the groove bottom 110a.

[0033] The recessed structure 120 includes a plurality of interconnected extended hole segments 121, which are coaxially connected sequentially along a first direction M to form a complete recessed structure 120. The number of extended hole segments 121 can be as follows: Figure 2 The two shown can also be as follows: Figure 3 The three shown can also be four or more. The first hole segment 121a is one of a plurality of extended hole segments 121, and the second hole segment 121b is an extended hole segment 121 located on the side of the first hole segment 121a facing the bottom of the groove 110a.

[0034] The shape of the extended hole segment 121 can be cylindrical, square prism, or conical truncated hole segment, etc., and the shapes of different extended hole segments 121 can be the same or different. The change in cross-sectional area between adjacent extended hole segments 121 can be a step-like abrupt change or a gradual transition. Furthermore, annular protrusions, annular grooves, or anti-slip textures can be added between adjacent extended hole segments 121 to improve the stress dispersion ability and structural stability of the recessed structure 120.

[0035] In one embodiment, such as Figure 5 As shown, a stepped surface 121c is formed at the junction of the second hole segment 121b and the first hole segment 121a, and the stepped surface 121c is arranged around the circumference of the second hole segment 121b.

[0036] In the embodiments of this application, by forming a stepped surface 121c at the junction of two adjacent extended hole segments 121 and circumferentially surrounding the second hole segment 121b, the expansion and compression borne by the sidewall of the first hole segment 121a is uniformly transmitted to the entire stepped surface 121c, thereby improving the ability of the recessed structure 120 to disperse the expansion stress of the single electrode 111.

[0037] In one embodiment, such as Figure 5As shown, the single electrode 111 includes a current collector 1111 and an active material layer 1112; the active material layer 1112 is disposed on at least one side of the current collector 1111, and the recessed structure 120 is disposed in the active material layer 1112.

[0038] In the embodiments of this application, by placing the recessed structure 120 in the active material layer 1112, it is possible to reduce the damage to the function of the current collector 1111 in carrying the active material and conducting current, and the expansion space reserved by the recessed structure 120 can directly buffer the expansion of the active material layer 1112, thereby improving the directness and efficiency of expansion buffering.

[0039] In one embodiment, such as Figure 5 As shown, the current collector 1111 has a groove 111a, which is located on the side of the current collector 1111 facing the active material layer 1112; the active material layer 1112 is at least partially embedded in the groove 111a.

[0040] In the embodiments of this application, by embedding the active material layer 1112 at least partially into the groove portion 111a, the contact area and bonding strength between the current collector 1111 and the active material layer 1112 are increased, so as to compensate for the local structural weakness of the active material layer 1112 caused by the recessed structure 120 provided in the active material layer 1112, thereby improving the structural stability of the recessed structure 120.

[0041] In one embodiment, such as Figure 5 As shown, along the first direction M, the orthogonal projection of the recessed structure 120 onto the current collector 1111 covers the groove portion 111a.

[0042] In the embodiments of this application, by making the orthogonal projection of the recessed structure 120 along the first direction M onto the current collector 1111 cover the groove portion 111a, the groove portion 111a supports the recessed structure 120, thereby further improving the structural stability of the recessed structure 120.

[0043] In one embodiment, such as Figure 5 As shown, the current collector 1111 has a protrusion 111b, which protrudes from the side of the current collector 1111 away from the recessed structure 120; along the first direction M, the orthographic projection of the protrusion 111b on the current collector 1111 at least partially overlaps with the orthographic projection of the groove 111a on the current collector 1111.

[0044] In the embodiments of this application, by having a protrusion 111b on the side of the current collector 1111 away from the recessed structure 120, and by making the orthographic projection of the protrusion 111b on the current collector 1111 at least partially overlap with the orthographic projection of the groove 111a on the current collector 1111 along the first direction M, the local thinning of the current collector 1111 caused by the groove 111a is compensated, thereby improving the structural stability of the current collector 1111 and the reliability of the current collector 1111 in supporting the active material layer 1112.

[0045] For example, along the first direction M, the protrusion distance of the protrusion 111b is less than or equal to 10 μm, and the compaction increase of the active material layer 1112 is less than or equal to 0.5. If, along the first direction M, the protrusion distance of the protrusion 111b is greater than 10 μm, and / or the compaction increase of the active material layer 1112 is greater than 0.5 μm. This is detrimental to the function of current collector 1111 in carrying active materials and conducting current.

[0046] In one embodiment, such as Figure 5 As shown, the single electrode 111 has a first side 110c and a second side 110d arranged opposite to each other, and both the first side 110c and the second side 110d are provided with recessed structures 120; along the first direction M, the orthographic projection of the recessed structure 120 on the single electrode 111 on the second side 110d is spaced apart from the orthographic projection of the recessed structure 120 on the first side 110c on the single electrode 111.

[0047] In the embodiments of this application, by providing recessed structures 120 on both the first side 110c and the second side 110d, the expansion space reserved in the recessed structures 120 is increased, thereby increasing the amount of expansion of the single electrode 111 that can be buffered by the recessed structures 120. Simultaneously, along the first direction M, the orthographic projection of the recessed structure 120 on the single electrode 111 on the second side 110d is spaced apart from the orthographic projection of the recessed structure 120 on the first side 110c, thereby reducing the local strength deficiency of the single electrode 111 caused by the overlapping projections of the recessed structures 120 on the first side 110c and the second side 110d, and thus improving the structural stability of the single electrode 111.

[0048] For example, along the first direction M, the orthographic projection of the recessed structure 120 on the second side 110d onto the monolithic electrode 111 is spaced apart from the orthographic projection of the recessed structure 120 on the first side 110c onto the monolithic electrode 111, with a minimum distance between them being less than or equal to 10 mm. Here, the minimum distance between the two orthographic projections refers to the minimum straight-line distance between any point on one orthographic projection and any point on the other. If the minimum distance between the orthographic projections of the recessed structure 120 on the second side 110d onto the monolithic electrode 111 and the first side 110c onto the monolithic electrode 111 along the first direction M is greater than 10 mm, it is detrimental to the stress dispersion and expansion buffering effect of the recessed structure 120.

[0049] In one embodiment, such as Figure 8 As shown, multiple single-piece electrode sheets 111 are wound to form an electrode assembly 100. Each single-piece electrode sheet 111 has a bending region 110e, and a recessed structure 120 is provided at least in the bending region 110e.

[0050] In the embodiments of this application, multiple single electrode sheets 111 are wound together to form an electrode assembly 100. Since the bending region 110e of the electrode assembly 100 is the core area of ​​the single electrode sheet 111 that bears bending stress, and the bending region 110e is also superimposed with the expansion stress of the single electrode sheet 111, the bending region 110e is more prone to wrinkling of the single electrode sheet 111 than the non-bending region 110e. Based on this, a recessed structure 120 is provided at least in the bending region 110e. The recessed structure 120 buffers the expansion generated in the bending region 110e and disperses the expansion stress and bending stress in the bending region 110e, thereby alleviating the deformation of the cell and the wrinkling of the single electrode sheet 111 at the bending region 110e.

[0051] Specifically, the bending region 110e is an inherent region formed after the single electrode 111 is wound. The bending region 110e is in the shape of a continuous arc or ellipse and extends along the winding direction of the single electrode 111. In addition, the single electrode 111 also has a straight region, and bending regions 110e are provided on both sides of the straight region, with the straight region connecting the two bending regions 110e.

[0052] In some embodiments of this application, such as Figure 9 As shown, the recessed structure 120 is at least partially located in the flat area to buffer the expansion generated in the flat area and disperse the expansion stress in the flat area, thereby alleviating the deformation of the cell in the flat area and the wrinkling phenomenon of the single electrode 111.

[0053] In one embodiment, the depth of the recessed structure 120 along the first direction M is less than or equal to 22 μm.

[0054] In the embodiments of this application, when the depth of the recessed structure 120 is greater than 22 μm, it will affect the structural integrity of the single electrode 111, which will lead to the shedding of the active material of the single electrode 111, damage to the current collector and obstruction of electrolyte wetting, thereby causing a decrease in the cycle capacity of the battery cell.

[0055] In some embodiments of this application, multiple single electrode sheets 111 are selected and assembled into battery cells for performance testing. The multiple single electrode sheets 111 are identical in structure except for the recessed structure 120, and the assembly process from the single electrode sheets 111 is also the same. In the comparative examples, the single electrode sheet 111 may or may not have a recessed structure 120, but the recessed structure 120 only includes one extension hole segment 121. In the embodiments, the electrode sheet has a recessed structure 120, which includes multiple interconnected extension hole segments 121 extending from the surface of the single electrode sheet 111 into its interior. From the surface of the single electrode sheet 111 into its interior, the extension hole segments 121 are respectively designated as the third hole segment 121d, the fourth hole segment 121e, and the fifth hole segment 121f. The data for the recessed structure 120 of the multiple single electrode sheets 111 are shown in Table 1 below. Table 1

[0056] The total depth H is equal to the sum of the depths of the third hole segment h1, the fourth hole segment h2, and the fifth hole segment h3.

[0057] The performance parameters of different battery cells were tested and recorded, including Hi-Pot resistance, electrolyte filling time, and DCR resistance. The specific experimental results are shown in Table 2 below. Table 2

[0058] The Hi-Pot resistance value refers to the high potential resistance value, which is used to measure the insulation performance of the electrode assembly 100. The higher the Hi-Pot resistance value, the better the insulation performance of the electrode assembly 100, that is, the insulation layer inside and on the surface of the electrode assembly 100 is undamaged and free of impurities, and the current leakage is small. This means that the probability of internal short circuits, leakage and other safety risks in the battery cell under subsequent charging and discharging, high temperature and other operating conditions is lower.

[0059] The electrolyte injection time is the total time consumed throughout the entire electrolyte injection process of the battery cell. It is used to ensure the consistency of the electrolyte injection process and the wetting effect of the electrolyte. The electrolyte injection time includes the time consumed for the first electrolyte injection (i.e., the first injection time) and the time consumed for the supplementary electrolyte injection (i.e., the second injection time). The shorter the electrolyte injection time, the smoother the electrolyte injection process and the more uniform the filling and wetting of the electrode assembly 100 by the electrolyte. This means that the battery cell has better efficiency and stability under subsequent charging and discharging, high temperature and other operating conditions.

[0060] DCR (Direct Current Resistance) refers to the internal resistance of a battery cell when a direct current flows through it. It is used to measure the conductivity of the electrode assembly 100, electrolyte, and various connection parts. A higher DCR indicates better cell consistency and a smoother internal conductive path, which means that the cell's stability and lifespan are better guaranteed under subsequent charging and discharging, high-temperature, and other operating conditions.

[0061] Furthermore, the battery cells of Examples 1, 3, Comparative Example 1, and Comparative Example 3 were subjected to cyclic charge-discharge at 25°C, and the cycle capacity retention rate was detected and recorded for each preset number of cycles. The specific experimental data are shown in Table 3 below: Table 3

[0062] The battery cells of Example 1, Example 3, Comparative Example 1, and Comparative Example 3 were subjected to cyclic charge-discharge at 45°C. The cycle capacity retention rate was detected and recorded for each preset number of cycles. The specific experimental data are shown in Table 4 below. Table 4

[0063] The capacity retention rate after the Nth cycle can be calculated using the following formula: Capacity retention rate after the Nth cycle (%) = (Discharge capacity after the Nth cycle / Initial discharge capacity) × 100%. The initial discharge capacity refers to the discharge capacity measured when the cell is first charged and discharged according to the standard charging and discharging regime. The discharge capacity after the Nth cycle refers to the discharge capacity measured according to the same standard after the cell has undergone N complete charge and discharge cycles. By comparing the change in capacity retention rate before and after the cycles, the degree of cell capacity decay can be quantified. A higher cycle capacity retention rate indicates better cell lifespan performance.

[0064] As can be seen from the test data in Tables 1 to 4 above, by comparing Examples 1 to 3, compared with Comparative Example 3, the injection time of Examples 1 to 3 is reduced, the DCR resistance is decreased, and the cycle capacity retention rate at 25℃ and 45℃ is increased, indicating that the performance of the cell with the recessed structure 120 is improved compared with the cell without the recessed structure.

[0065] By comparing Example 3 with Comparative Example 1, the Hi-Pot resistance of Example 3 increased, the injection time decreased, the DCR resistance decreased, and the cycle capacity retention rate increased at 25°C and 45°C. This indicates that the performance of the cell with two extended hole segments 121 is improved compared to the cell with only one extended hole segment 121.

[0066] By comparing Examples 1 and 2, compared to Comparative Example 1, Examples 1 and 2 show increased Hi-Pot resistance, decreased injection time, decreased DCR resistance, and increased cycle capacity retention at 25°C and 45°C. This indicates that the battery cell with three extended aperture segments 121 has improved performance compared to the battery cell with only one extended aperture segment 121. Furthermore, compared to Comparative Example 3, Examples 1 and 2 show increased Hi-Pot resistance, indicating that the battery cell with three extended aperture segments 121 can compensate for the impact of the recessed structure 120 on the battery cell's insulation performance.

[0067] When H is less than 22 μm, by comparing Examples 1 and 2, the Hi-Pot resistance of Examples 1 and 2 increases compared to Example 4. Meanwhile, the Hi-Pot resistance of Example 4 is less than that of Comparative Examples 1 and 3, and the recessed structure 120 of Example 4 is detrimental to the safe use of the battery cell.

[0068] As can be seen from the above structural design, cells with two or three extended aperture segments 121 can increase the Hi-Pot resistance, thereby improving the cell's insulation performance; they can also shorten the electrolyte injection time, thereby improving the electrolyte wetting efficiency; they can also reduce the DCR resistance, thereby improving the cell's conductivity; and they can also increase the cycle capacity retention rate, thereby increasing the cell's service life. Compared to cells with only one extended aperture segment 121, cells with three extended aperture segments 121 show a 3.2% increase in cycle capacity retention rate after 1800 cycles at 25°C; and a 5.01% increase in cycle capacity retention rate after 1500 cycles at 45°C.

[0069] In one embodiment, the depth of the recessed structure (120) along the first direction (M) is greater than or equal to 5 μm.

[0070] In the embodiments of this application, if the depth of the recessed structure 120 is reduced, the depth of the extended hole segment 121 will also be reduced accordingly, which will increase the difficulty of forming the recessed structure 120 and make the integrity of the recessed structure 120 easily damaged, thus weakening the stress dispersion and expansion buffering effect of the recessed structure 120.

[0071] According to process experience data, in the rolling process of the recessed structure 120, in order to ensure the stress dispersion and expansion buffering effect of the recessed structure 120, the depth of the recessed structure 120 along the first direction M should not be less than 5μm.

[0072] In some embodiments of this application, the proportion of the area of ​​the hole segment to the area of ​​the electrode sheet in the cell corresponding to each depth combination is also recorded. Specifically, the proportion of the cross-sectional area of ​​the third hole segment 121d in the direction perpendicular to the first direction M to the area of ​​the electrode sheet is set as S1, the proportion of the cross-sectional area of ​​the fourth hole segment 121e in the direction perpendicular to the first direction M to the area of ​​the electrode sheet is S2, and the proportion of the cross-sectional area of ​​the fifth hole segment 121f in the direction perpendicular to the first direction M to the area of ​​the electrode sheet is S3. In embodiments 1, 2, and 4, S1 is 58%, S2 is 35%, and S3 is 21%; in embodiment 3, S1 is 62% and S2 is 37%.

[0073] In some embodiments of this application, the preparation of the electrode 110 and the assembly of the battery cell are required in order to record the performance parameters and test the cycle capacity retention rate of the battery cell corresponding to each depth combination. The preparation steps of the electrode 110 and the battery cell include the following: The preparation steps of electrode 110 include: First, positive electrode material is coated onto the current collector in a certain proportion, and then processed through baking, rolling, and other processes to obtain positive electrode sheet 101; simultaneously, negative electrode material is coated onto the current collector in a certain proportion, and then processed through baking, rolling, and other processes to obtain negative electrode sheet 103. Secondly, using... Figure 7 The embossing roller 400 shown rolls out recessed structures 120 on both sides of the positive electrode sheet 101, resulting in the three-layer embossed electrode sheet in Examples 1, 2, and 4, the double-layer embossed electrode sheet in Example 3, and the single-layer embossed electrode sheet in Comparative Examples 1 and 2. The embossing roller 400 includes a roller body 410 and an embossing portion 420 disposed on the roller body 410. The embossing portion 420 has multiple boss structures 421, the number of which can be [missing information]. Figure 7 The three shown can also be two. Finally, the positive electrode 101, the separator 102 and the negative electrode 103 are wound using a die-cutting and winding machine to obtain the electrode assembly 100.

[0074] II. The battery cell assembly process includes: First, the electrode assembly 100 is hot-pressed according to preset parameters. During this process, the Hi-Pot resistance of the cell is recorded. Second, the insulating spacer assembly is wrapped around the hot-pressed electrode assembly 100, wound up, and then installed into the housing 200 for assembly, resulting in the cell to be injected with electrolyte. Third, the cell is injected with electrolyte using the same injection equipment and with the same injection volume, ensuring no overflow from the injection port; the time from the start to the completion of injection is recorded. Finally, the cell formation and capacity testing processes are completed using the same formation and capacity testing equipment with identical specifications; the DCR resistance of the cell is recorded during this process.

[0075] After the battery cells are assembled, the cycle capacity retention rate of the battery cells is tested under environmental conditions of 25℃ and 45℃ respectively.

[0076] Optionally, embodiments of this application also provide a battery pack, including the battery cells described in the above embodiments.

[0077] In embodiments of this application, the battery pack includes battery cells, such as... Figures 1-4 As shown, in the battery cell, by providing a plurality of spaced recessed structures 120 on at least one side surface of the single electrode 111, and extending the recessed structures 120 from the surface of the single electrode 111 to the interior of the single electrode 111, expansion space is reserved for the single electrode 111 to absorb the expansion of the single electrode 111, thereby alleviating the wrinkling problem caused by the deformation of the single electrode 111. Meanwhile, by making the recessed structure 120 include a plurality of interconnected extended hole segments 121, and in the two extended hole segments 121, making the cross-sectional area of ​​the extended hole segment 121 near the bottom of the groove 110a in the direction perpendicular to the first direction M smaller than the cross-sectional area of ​​the extended hole segment 121 away from the bottom of the groove 110a in the direction perpendicular to the first direction M, the complexity of the sidewalls extending from the surface of the single electrode 111 to the interior of the single electrode 111 in the recessed structure 120 is increased, thereby improving the ability of the recessed structure 120 to disperse the expansion stress of the single electrode 111, reducing the amount of expansion generated by the single electrode 111, and further alleviating the wrinkling phenomenon of the single electrode 111.

[0078] In the description of this specification, the references to terms such as "one embodiment," "some embodiments," "illustrative embodiment," "example," "specific example," or "some examples," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the present invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.

[0079] Although embodiments of the present invention have been shown and described, those skilled in the art will understand that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the present invention, the scope of which is defined by the claims and their equivalents.

Claims

1. A battery cell, characterized in that, Includes electrode assembly (100); The electrode assembly (100) includes an electrode sheet (110), which is wound or stacked. The electrode sheet (110) includes multiple single electrode sheets (111), and the thickness direction of the single electrode sheet (111) is a first direction (M). The single electrode (111) has at least one side surface provided with a plurality of spaced recessed structures (120), the recessed structures (120) extending from the surface of the single electrode (111) toward the interior of the single electrode (111) to form a groove bottom (110a). The recessed structure (120) includes a first hole segment (121a) and a second hole segment (121b) connected to each other. The second hole segment (121b) is located on the side of the first hole segment (121a) facing the bottom of the groove (110a). The cross-sectional area of ​​the second hole segment (121b) in the direction perpendicular to the first direction (M) is smaller than the cross-sectional area of ​​the first hole segment (121a) in the direction perpendicular to the first direction (M).

2. The battery cell according to claim 1, characterized in that, A stepped surface (121c) is formed at the junction of the second hole segment (121b) and the first hole segment (121a), and the stepped surface (121c) is arranged circumferentially around the second hole segment (121b).

3. The battery cell according to claim 1, characterized in that, The single electrode (111) includes a current collector (1111) and an active material layer (1112); the active material layer (1112) is disposed on at least one side of the current collector (1111), and the recessed structure (120) is disposed in the active material layer (1112).

4. The battery cell according to claim 3, characterized in that, The current collector (1111) has a groove (111a) on the side of the current collector (1111) facing the active material layer (1112); the active material layer (1112) is at least partially embedded in the groove (111a).

5. The battery cell according to claim 4, characterized in that, Along the first direction (M), the orthogonal projection of the recessed structure (120) onto the current collector (1111) covers the groove portion (111a).

6. The battery cell according to claim 5, characterized in that, The current collector (1111) has a protrusion (111b) that protrudes from the current collector (1111) on the side opposite to the recessed structure (120); along the first direction (M), the orthographic projection of the protrusion (111b) on the current collector (1111) at least partially overlaps with the orthographic projection of the groove (111a) on the current collector (1111).

7. The battery cell according to any one of claims 1-6, characterized in that, The single electrode (111) has a first side (110c) and a second side (110d) arranged opposite to each other, and both the first side (110c) and the second side (110d) are provided with the recessed structure (120). Along the first direction (M), the orthographic projection of the recessed structure (120) on the second side (110d) onto the monolithic electrode (111) is spaced apart from the orthographic projection of the recessed structure (120) on the first side (110c) onto the monolithic electrode (111).

8. The battery cell according to any one of claims 1-6, characterized in that, Multiple single electrode sheets (111) are wound to form the electrode assembly (100), each single electrode sheet (111) having a bending region (110e), and the recessed structure (120) is provided at least in the bending region (110e).

9. The battery cell according to any one of claims 1-6, characterized in that, Along the first direction (M), the depth of the recessed structure (120) is less than or equal to 22 μm.

10. A battery pack, characterized in that, include: The battery cell as described in any one of claims 1 to 9.