Horizontal casting mold

By employing a multi-sprue and riser structure in the horizontal casting mold, uniform dispersion and sequential solidification of molten metal are achieved, solving the problem of untimely feeding during casting and improving the qualification rate and performance of castings.

CN224977442UActive Publication Date: 2026-11-17CHIFENG JIANZHI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522643068.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-12
Publication Date
2026-11-17
Estimated Expiration
2035-12-12

AI Technical Summary

Technical Problem

Existing horizontal casting molds, due to their single gating system and fixed riser positions, result in untimely feeding of castings during the casting process, which easily leads to internal defects such as shrinkage cavities and porosity, affecting the casting's pass rate and performance.

Method used

A horizontal casting mold was designed, which adopts a structure with multiple runners and risers, including a first runner, a second runner, a third runner and multiple risers. The multi-runner system allows the molten metal to be evenly dispersed and quickly fill the casting cavity. Riser is set at the intersection to collect oxides and inclusions, realizes sequential solidification and feeding, and prevents shrinkage cavities and porosity.

Benefits of technology

It improves the qualification rate and performance of castings. Through uniform pouring and feeding measures, it reduces defects such as incomplete pouring and cold shut, ensuring the high quality and stability of castings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224977442U_ABST
    Figure CN224977442U_ABST
Patent Text Reader

Abstract

This application provides a horizontal casting mold, comprising: an upper mold plate with a plurality of downward-facing convex cavities evenly distributed on the upper mold plate, and a vertical pouring channel vertically disposed in the middle of the upper mold plate, wherein a first gating channel is connected to opposite sides of the pouring channel and extends along the length direction of the upper mold plate; a lower mold plate with a plurality of upward-facing concave cavities evenly distributed on the lower mold plate, wherein the plurality of concave cavities correspond one-to-one with the plurality of convex cavities; wherein, when the upper mold plate and the lower mold plate are sealed together, each convex cavity and its corresponding concave cavity form a casting cavity; a plurality of second gating channels are vertically connected to the first gating channel, and a third gating channel is vertically connected to each second gating channel for pouring material into the casting cavities located on both sides of its own length direction; a first riser is disposed at the intersection of the first gating channel and the third gating channel with the second gating channel. This application can prevent the generation of shrinkage cavities and porosity, thereby improving the yield of castings and ensuring the subsequent performance of castings.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of casting technology, and in particular to a horizontal line casting mold. Background Technology

[0002] Horizontal casting molds specifically refer to molds used on automated molding production lines where the parting surface is horizontal. It is a subclass of casting molds, and its design and structure must be adapted to the automated workflow of the horizontal molding line (such as automatic mold closing, pouring, and conveying).

[0003] Existing horizontal casting molds typically include an upper mold, lower mold, cavity, sprue, and riser. The sprue is simply a vertical main channel through which molten metal is poured from the pouring cup into the mold. The riser is located on the side or top of the cavity. Due to the diverse shapes of castings and the uneven thickness of different parts of each type of casting, the thin-walled parts of the casting cool and shrink faster than the thick-walled parts. This uneven shrinkage causes tensile stress in the thick-walled areas of the casting, which are still at high temperatures, leading to cracks in the thick-walled areas. To avoid this, timely feeding is necessary. However, the single sprue and fixed riser position of existing horizontal casting molds result in untimely feeding during the casting process, leading to internal defects such as shrinkage cavities and porosity. Consequently, the finished castings have a low yield rate and poor performance. Utility Model Content

[0004] This application provides a horizontal casting mold to solve the technical problems described in the background art above.

[0005] To solve the above-mentioned technical problems, this application adopts the following technical solution: This application provides a horizontal line casting mold, comprising: The upper template has multiple downward-facing convex cavities evenly distributed on its upper surface, and a pouring channel is vertically arranged in the middle of the middle. The two opposite sides of the pouring channel are connected to a first gating channel extending along the length of the upper template. The lower template has a plurality of upward-facing concave cavities evenly distributed on it, and the plurality of concave cavities correspond one-to-one with the plurality of upward-facing convex cavities; When the upper template and the lower template are sealed together, each of the upper convex cavities and its corresponding lower concave cavity forms a casting cavity; The first gating system has a plurality of second gating systems vertically connected to it. Each second gating system has a third gating system vertically connected to it for injecting material into the casting cavity located on both sides of its own length direction. The first gating system and the third gating system are respectively provided with a first riser at the intersection with the first gating system.

[0006] Optionally, the plurality of convex cavities and the concave cavities corresponding one-to-one with the plurality of convex cavities are arranged in a matrix.

[0007] Optionally, the number of casting cavities is at least four and is an even number.

[0008] Optionally, the pouring channel is connected to a fourth gating channel extending along the width direction of the upper template on the other two opposite sides. The fourth gating channel is vertically connected to a fifth gating channel for pouring material into the casting cavity located on both sides of its own length direction. A second riser is provided at the intersection of the fifth gating channel and the fourth gating channel.

[0009] Optionally, both the first riser and the second riser are made of heat-insulating and heat-generating materials.

[0010] Optionally, the upper template is provided with positioning holes, and the lower template is provided with positioning pins; or, The upper template is provided with a positioning pin, and the lower template is provided with a positioning hole; The positioning hole is adapted to the positioning pin.

[0011] Optionally, the upper template is provided with an exhaust pipe that communicates with the casting cavity; The diameter of the exhaust pipe is 1.5mm to 3mm.

[0012] The horizontal casting mold provided in this application connects a first gating channel to the pouring channel, and vertically connects multiple second gating channels to the first gating channel, as well as a third gating channel vertically connected to each second gating channel for pouring molten metal into the casting cavity located on both sides of the length direction of the third gating channel. The arrangement of the first gating channel, multiple second gating channels, and multiple third gating channels can make the molten metal evenly dispersed and quickly fill the casting cavity. This stable pouring method can minimize the occurrence of defects such as incomplete pouring and cold shut in the casting, thereby improving the casting qualification rate. In addition, first risers are set at the intersections of the first and third runners with the second runner. The setting of multiple first risers facilitates the collection of oxides and inclusions at the intersections of the first and second runners, as well as the intersections of the third and second runners, which helps to improve the quality of the casting. Furthermore, the placement of the first risers facilitates the sequential solidification of the casting, ensuring that the molten metal at the first riser is the last to solidify. Moreover, multiple first risers can effectively compensate for the shrinkage of the casting, preventing the formation of shrinkage cavities and porosity, thereby improving the casting's pass rate and ensuring its subsequent performance. Attached Figure Description

[0013] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0014] Figure 1 A schematic diagram of the upper and lower templates of a horizontal casting mold provided in an embodiment of this application, showing the structure of the mold together. Figure 2 This is a structural schematic diagram of a horizontal casting mold in the separated state of the upper and lower templates, as provided in another embodiment of this application. Figure 3 This is a schematic diagram of the structure of the upper template provided in one embodiment of this application; Figure 4 This is a schematic diagram of the structure of the lower template provided in one embodiment of this application; Figure 5 A cross-sectional view of a horizontal casting mold provided in an embodiment of this application.

[0015] In the diagram: 100, upper mold plate; 101, upper convex cavity; 102, pouring channel; 103, vent pipe; 200, first runner; 201, second runner; 2011, third runner; 300, lower mold plate; 301, lower concave cavity; 400, casting cavity; 500, first riser; 600, fourth runner; 601, fifth runner; 700, second riser; 800, positioning hole; 900, positioning pin. Detailed Implementation

[0016] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions in the embodiments of this application are described clearly and completely below. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without creative effort are also within the scope of protection of this application.

[0017] refer to Figures 1 to 5 This application provides a horizontal line casting mold, comprising: The upper template 100 has multiple downward-facing convex cavities 101 evenly distributed on its upper surface, and a pouring channel 102 is vertically arranged in its middle. The two opposite sides of the pouring channel 102 are connected to a first gating channel 200 extending along the length of the upper template 100. The number of convex cavities 101 is generally even, such as four, six, or eight convex cavities 101 on the upper template 100. The figure shows that the upper template 100 has eight convex cavities 101.

[0018] The lower template 300 has multiple upward-facing concave cavities 301 evenly distributed on it, with each concave cavity 301 corresponding to a multiple convex cavity 101. The shapes of the concave cavities 301 and the convex cavities 101 are adapted to the shape of the casting to be formed.

[0019] When the upper template 100 and the lower template 300 are sealed together, each upper convex cavity 101 and its corresponding lower concave cavity 301 form a casting cavity 400; wherein the casting cavity 400 is adapted to the shape of the casting to be cast.

[0020] Multiple second runners 201 are vertically connected to the first runner 200. Each second runner 201 is vertically connected to a third runner 2011 for injecting molten metal into the casting cavities 400 located on both sides of its length. First risers 500 are provided at the intersections of the first runner 200 and the third runner 2011 with the second runners 201. A riser is an additional portion added to the top or side of the casting to prevent defects. The first riser 500 is cylindrical in shape. Multiple first risers 500 can provide the required amount of molten metal to compensate for during the casting process, minimizing shrinkage cavities and porosity.

[0021] The horizontal casting mold provided in this application connects a first gating 200 to the pouring channel 102, and vertically connects multiple second gatings 201 to the first gating 200, as well as a third gating 2011 vertically connected to each second gating 201 for injecting molten metal into the casting cavity 400 located on both sides of the length direction of the third gating 2011. The arrangement of the first gating 200, multiple second gatings 201, and multiple third gatings 2011 allows the molten metal to be evenly dispersed and quickly fill the casting cavity 400. This stable pouring method can minimize defects such as incomplete pouring and cold shuts in the casting, thereby improving the casting yield. In addition, first risers 500 are provided at the intersections of the first gating 200 and the third gating 2011 with the second gating 201, respectively. The provision of multiple first risers 500 facilitates the collection of oxides and inclusions at the intersections of the first gating 200 and the second gating 201, as well as the intersections of the third gating 2011 and the second gating 201, which helps to improve the quality of the casting. Furthermore, the placement of the first risers 500 facilitates the sequential solidification of the casting, ensuring that the molten metal at the first riser 500 is the last to solidify. Moreover, the multiple first risers 500 can effectively compensate for the shrinkage of the casting, preventing the formation of shrinkage cavities and porosity, thereby improving the casting's pass rate and ensuring its subsequent performance.

[0022] During the casting process, after the molten metal is added through the pouring channel 102, it flows through the first gating channel 200 and enters the casting cavity 400 connected to each of the multiple second gating channels 201 and the two third gating channels 2011 connected to each second gating channel 201 in sequence. After each casting cavity 400 is filled with molten metal, it gradually flows to and fills each first riser 500. During the cooling and solidification process of the molten metal in the casting cavity 400, the molten metal in the first riser 500 can enter the casting cavity 400 in time to compensate for the shrinkage of the casting, thereby preventing shrinkage cavities and porosity during the casting process, thus improving the casting qualification rate and ensuring the subsequent performance of the casting.

[0023] In some embodiments, reference Figure 1 and Figure 2 In this application, the multiple convex cavities 101 and the concave cavities 301 corresponding to the multiple convex cavities 101 are arranged in a matrix. This can ensure the uniformity of the molten metal flow process during the casting process, making the cast parts more uniform and improving the casting qualification rate.

[0024] In some embodiments, the number of casting cavities 400 in this application is at least four and is an even number.

[0025] In the above embodiments, the casting cavity 400 has at least four, enabling mass production of castings and allowing multiple castings to be formed at once, thereby improving the casting efficiency. Furthermore, the number of casting cavities 400 is even, ensuring uniform stress distribution of the molten metal during filling. This ensures uniform thermal balance and mechanical stress distribution during the pouring process of the horizontal casting mold, minimizing deformation or cracking caused by uneven stress, and thus extending the service life of the horizontal casting mold.

[0026] In some embodiments, reference Figure 1 and Figure 2 In this application, the pouring channel 102 is connected to the other two opposite sides by a fourth gating channel 600 extending along the width direction of the upper template 100. The fourth gating channel 600 is vertically connected to a fifth gating channel 601 for pouring material into the casting cavity 400 located on both sides of its own length direction. A second riser 700 is provided at the intersection of the fifth gating channel 601 and the fourth gating channel 600.

[0027] In the above embodiments, the fourth gating system 600 and the fifth gating system 601 are configured such that, during the casting process, after the molten metal is added from the casting channel 102, the molten metal flows through the first gating system 200 and sequentially enters the casting cavity 400 connected to each of the multiple second gating systems 201 connected to the first gating system 200. Simultaneously, the molten metal entering the casting channel 102 flows through the fourth gating system 600 and sequentially enters the casting cavity 400 connected to each of the multiple fifth gating systems 601 connected to the fourth gating system 600. This accelerates the filling rate of the molten metal in the casting cavity 400 and improves the casting efficiency. Furthermore, the second riser 700 and the first riser 500 can store a sufficient amount of molten metal to achieve the required feeding amount during the casting cooling and forming process.

[0028] It should be noted that the paired casting cavities 400 are typically arranged along the length of the mold. In this case, there are two first runners 200, multiple second runners 201, and each second runner 201 corresponds to two third runners 2011. There are also multiple first risers 500. There are two fourth runners 600 perpendicular to the first runners 200, and each fourth runner 600 corresponds to two fifth runners 601. There are also two second risers 700. See details below. Figure 1 and Figure 2 As shown.

[0029] In some embodiments, both the first riser 500 and the second riser 700 in this application are made of thermal insulation and heat-generating materials. The thermal insulation and heat-generating materials are a mixture of thermal insulation materials and heat-generating reactive materials (for example, the mixing ratio of thermal insulation materials and heat-generating reactive materials is 2:1). The thermal insulation materials are a mixture of materials such as rock wool, asbestos, refractory fiber, glass fiber, expanded perlite, carbonized rice husk, and cenospheres, with the aim of forming a porous structure to reduce heat loss and maintain a high-temperature environment. The heat-generating reactive materials are a mixture of aluminum powder, silicon powder, iron oxide powder, and carbon powder, with the aim of undergoing a violent exothermic reaction (e.g., aluminothermic reaction) upon contact with high-temperature molten metal, instantly releasing a large amount of heat energy, reducing the solidification rate of the molten metal in the first riser 500 and the second riser 700, so that the molten metal in the first riser 500 and the second riser 700 solidifies last compared to the molten metal in the casting cavity 400, and timely compensating for shrinkage and porosity during the cooling and solidification process of the casting cavity 400. The heat-insulating and heating materials are purchased, and their preparation, composition, and proportions are not innovative aspects of this application. Therefore, this application will not elaborate on them here.

[0030] In some embodiments, reference Figure 1 In this application, the upper template 100 is provided with a positioning hole 800 and the lower template 300 is provided with a positioning pin 900; or, the upper template 100 is provided with a positioning pin 900 and the lower template 300 is provided with a positioning hole 800; wherein, the positioning hole 800 and the positioning pin 900 are adapted to each other.

[0031] In the above embodiment, the lower template 300 is inserted into the positioning hole 800 on the upper template 100 via a positioning pin 900, thereby connecting the upper template 100 and the lower template 300, and forming a sealed casting cavity 400 between the connected upper template 100 and the lower template 300. Similarly, the upper template 100 is also connected to the lower template 300 via a positioning pin 900 inserted into the positioning hole 800 on the lower template 300, again forming a sealed casting cavity 400 between the connected upper template 100 and the lower template 300. This connection method facilitates the installation and disassembly of the upper template 100 and the lower template 300, and the positioning pin 900 improves the accuracy of the installation of the upper template 100 and the lower template 300.

[0032] In some embodiments, reference Figure 1 and Figure 2In this application, the upper template 100 is provided with an exhaust pipe 103 communicating with the casting cavity 400. The exhaust pipe 103 allows for the timely discharge of air and gases generated by the heating of the molding sand within the casting cavity 400, preventing air blockage and preventing the molten metal from filling the cavity and becoming trapped inside the casting, thus creating porosity. This results in a higher yield of cast parts. In addition, the diameter of the exhaust pipe 103 is 1.5mm to 3mm. A smaller diameter makes the exhaust pipe 103 susceptible to blockage by paint or sand particles, affecting exhaust performance. Conversely, a larger diameter may result in poor airflow stability. Therefore, the diameter of the exhaust pipe 103 needs to be within a suitable range. An exhaust pipe 103 with a diameter between 1.5mm and 3mm not only ensures more stable gas flow and reduces the likelihood of vortices being drawn into the molten metal, but also avoids excessive exhaust resistance.

[0033] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.

Claims

1. A horizontal line casting mold characterized by, include: The upper template (100) has a plurality of downward-facing convex cavities (101) evenly provided on the upper template (100), and a pouring channel (102) is vertically provided in the middle of the middle. The pouring channel (102) has a first sprue (200) extending along the length direction of the upper template (100) on its opposite sides. The lower template (300) has a plurality of upward-facing concave cavities (301) evenly provided on it, and the plurality of concave cavities (301) correspond one-to-one with the plurality of upward-facing convex cavities (101); When the upper template (100) and the lower template (300) are sealed together, each of the upper convex cavities (101) and its corresponding lower concave cavity (301) forms a casting cavity (400). The first gating (200) is vertically connected to a plurality of second gatings (201), and each second gating (201) is vertically connected to a third gating (2011) for injecting material into the casting cavity (400) located on both sides of its own length direction. The first gating (200) and the third gating (2011) are respectively provided with a first riser (500) at the intersection with the second gating (201).

2. The horizontal line casting mold of claim 1, wherein, The plurality of the convex cavities (101) and the concave cavities (301) corresponding one-to-one with the plurality of the convex cavities (101) are arranged in a matrix.

3. The horizontal line casting mold according to claim 2, characterized in that, The number of the casting cavities (400) is at least four and is an even number.

4. The horizontal line casting mold according to claim 1, characterized in that, The pouring channel (102) is connected to the other two opposite sides by a fourth gating channel (600) extending along the width direction of the upper template (100). The fourth gating channel (600) is vertically connected to a fifth gating channel (601) for pouring material into the casting cavity (400) located on both sides of its own length direction. A second riser (700) is provided at the intersection of the fifth gating channel (601) and the fourth gating channel (600).

5. The horizontal line casting mold according to claim 4, characterized in that, Both the first riser (500) and the second riser (700) are made of heat-insulating and heat-generating materials.

6. The horizontal line casting mold according to claim 1, characterized in that, The upper template (100) is provided with positioning holes (800), and the lower template (300) is provided with positioning pins (900); or, The upper template (100) is provided with a positioning pin (900), and the lower template (300) is provided with a positioning hole (800). The positioning hole (800) is adapted to the positioning pin (900).

7. The horizontal line casting mold according to any one of claims 1 to 6, characterized in that, The upper template (100) is provided with an exhaust pipe (103) that communicates with the casting cavity (400). The diameter of the exhaust pipe (103) is 1.5mm to 3mm.