A composite manufacturing apparatus based on interlayer alternating additive polishing
By using a composite manufacturing device based on interlayer alternating additive polishing, polishing and three-axis platform movement are performed using a co-source laser, interlayer defects in additive manufacturing are repaired in real time. This solves the problem of defects being amplified layer by layer in traditional additive manufacturing, and improves the surface quality of parts and manufacturing efficiency.
Patent Information
- Application Number
- CN202522281295.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Priority Date
- 2025-08-14
- Filing Date
- 2025-10-28
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-10-28
AI Technical Summary
In traditional additive manufacturing, defects such as surface roughness or microcracks are magnified layer by layer, affecting the overall precision and strength of the parts, and there is a lack of effective real-time repair methods.
A composite manufacturing device based on interlayer alternating additive polishing is adopted. Polishing is performed using a homogeneous laser, and a three-axis platform is used to move the laser in three directions to repair interlayer defects in real time. Additive manufacturing and polishing are performed by time-division multiplexing of the laser, and the residual heat of polishing is used to preheat the next additive layer to control the thermal cycle efficiency.
It significantly improves surface quality, reduces thermal stress accumulation and warping deformation, increases the yield of finished products, reduces manufacturing costs and energy consumption from repeated heating, and reduces surface roughness by more than 80%.
Smart Images

Figure CN224977508U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of additive manufacturing and surface finishing composite technology, specifically relating to a composite manufacturing device based on interlayer alternating additive polishing. Background Technology
[0002] With the increasing demands for performance in complex metal components from aerospace, high-end mold making, and biomedical fields, Laser Additive Manufacturing (LAM) technology has emerged as a revolutionary "moldless" manufacturing solution. It eliminates the reliance on complex molds, using a high-energy laser beam to precisely melt metal powder or filament, achieving layer-by-layer melting, solidification, and deposition of materials to directly form three-dimensional solid parts. This process not only significantly improves the utilization rate of metal materials but also enables the rapid and direct transformation of highly complex structures, internal cavities, or functionally graded materials into reality. A typical process flow usually includes substrate preparation, metal powder (or filament) placement / transfer, selective melting / cladding with a high-power laser beam, rapid solidification of the molten pool, and layer-by-layer movement of the stage / laser head, repeating this cycle until the part is complete.
[0003] However, in traditional additive manufacturing, if the surface of a layer is rough or contains microcracks, these defects will be inherited and amplified layer by layer, ultimately affecting the overall precision and strength of the part. Common defects include molten pool ripples, spatter adhesion, and uneven cooling shrinkage. Summary of the Invention
[0004] To address the problems existing in the prior art, this utility model provides a composite manufacturing device based on interlayer alternating additive polishing, which uses a laser of the same origin as the additive process for polishing, thereby reducing the drawback of defects being magnified layer by layer in additive manufacturing.
[0005] To achieve the above objectives, the present invention adopts the following technical solution: A composite manufacturing apparatus based on interlayer alternating additive polishing includes a base and an additive powder feeding system. A sealed chamber and a column are installed on the base. A three-axis platform, a laser generator and a temperature sensor are installed inside the sealed chamber. A clamping component is installed on the side of the column facing the laser generator, and the clamping component is used to fix the substrate or the formed body; The three-axis platform is used to drive the laser generator to move in three mutually perpendicular directions.
[0006] Furthermore, the three-axis platform includes an x-axis motion module, a y-axis motion module, and a z-axis motion module, wherein the y-axis motion module is slidably mounted on the x-axis motion module, and the z-axis motion module is slidably mounted on the y-axis motion module; The x-axis motion module includes an x-axis track support, a dual lead screw structure, and two synchronously operating x-axis track motors; The dual lead screw structure includes a first x-axis track lead screw and a second x-axis track lead screw, which are synchronously driven by two x-axis track motors respectively. The first x-axis track lead screw and the second x-axis track lead screw are mounted side by side on the x-axis track bracket. Each of the first x-axis track lead screw and the second x-axis track lead screw is equipped with an x-axis nut, and the x-axis nut is fixedly connected to the y-axis motion module.
[0007] Furthermore, the y-axis motion module includes a y-axis track bracket and a y-axis track screw mounted on the y-axis track bracket, and a y-axis nut is mounted on the y-axis track screw; The z-axis motion module includes a z-axis track bracket fixed to a y-axis nut and a z-axis track screw mounted on the z-axis track bracket. A z-axis nut is mounted on the z-axis track screw, and a laser mounting bracket is fixed on the z-axis nut. The laser generator is mounted on the laser mounting bracket.
[0008] Furthermore, the laser generator is mounted on a three-axis platform via a laser mounting bracket. The lower end of the laser mounting bracket is equipped with a servo motor-driven rotating device, which drives the laser generator to adjust its angle.
[0009] Furthermore, reinforcing ribs are provided between the side wall of the column and the clamping parts.
[0010] Furthermore, the temperature sensor is equipped with dual probes, which monitor the ambient temperature of the sealed chamber and the temperature of the substrate on the clamped parts in real time.
[0011] Furthermore, in additive powder feeding systems: The output end of the powder feeder is connected to the feed inlet of the powder distributor; The powder separator's outlet extends through a powder pipe directly above the clamping part.
[0012] Furthermore, the laser generator has an additive mode and a polishing mode, with the linear energy density in the polishing mode being 25%-35% of the linear energy density in the additive mode.
[0013] Furthermore, the detection sensing system also includes an ambient oxygen sensor for measuring the oxygen concentration inside the sealed chamber, a molten pool sensor for real-time monitoring of the molten pool penetration depth and linear energy density, and a spectral sensor for measuring the spectral wavelength characteristics of the polished area.
[0014] Furthermore, the molten pool sensor and the spectral sensor are mounted on the top of the column, with their signal receiving ends facing the working area above the clamped part.
[0015] Compared with the prior art, the present invention has at least the following beneficial technical effects: This utility model provides a composite manufacturing device based on interlayer alternating additive polishing. The three-axis platform enables the laser to move in three directions. The laser is used for additive manufacturing and polishing, realizing timely repair of interlayer defects during the additive manufacturing process. This solves the problem of interlayer defect accumulation and can eliminate surface defects in a timely manner during the layer-by-layer forming process. It also eliminates the drawback of defect amplification layer by layer in additive manufacturing and improves surface quality.
[0016] Furthermore, this invention significantly improves the efficiency of additive-polishing composite manufacturing by time-division multiplexing of the same source laser, while saving manufacturing costs. It can also use the residual heat from polishing to directly preheat the next additive layer, reducing the energy consumption of repeated heating and improving thermal cycling efficiency. Interlayer temperature gradient control reduces thermal stress accumulation by 60%, significantly suppressing warping deformation.
[0017] Furthermore, by using a molten pool sensor to monitor the molten pool penetration depth and linear energy density in real time, the roughness Ra value can be calculated from the molten pool penetration depth and linear energy density. The polishing parameters can be dynamically corrected based on the roughness Ra value, avoiding process instability caused by material fluctuations and greatly improving the finished product qualification rate. Attached Figure Description
[0018] Figure 1 A schematic diagram of the additive polishing composite manufacturing device provided by this utility model; Figure 2 Schematic diagram of the additive polishing composite manufacturing apparatus provided by this utility model; Figure 3 A flowchart of an additive polishing composite manufacturing method; Figure 4 This is a schematic diagram of the surface roughness feedback mechanism.
[0019] In the attached diagram: 1-Computer; 2-Laser generator; 3-Powder feeder; 4-Powder distributor; 5-Powder pipe; 6-Column; 7-Base; 8-Temperature sensor; 9-Ambient oxygen sensor; 10-Molten pool sensor; 11-Spectrometer sensor; 12-Clamping part; 13-Sealed chamber; 14-X-axis track motor; 15-X-axis track support; 16-First X-axis track lead screw; 17-Second X-axis track lead screw; 18-Y-axis track motor; 19-Y-axis track support; 20-Y-axis track lead screw; 21-Z-axis track motor; 22-Z-axis track support; 23-Z-axis track lead screw. Detailed Implementation
[0020] The present invention will now be described in detail with reference to the accompanying drawings and specific embodiments.
[0021] To enable those skilled in the art to better understand the technical solutions of this utility model, the technical solutions of the embodiments of this utility model will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this utility model, and not all embodiments. Based on the embodiments of this utility model, all other embodiments obtained by those skilled in the art without creative effort should fall within the protection scope of this utility model.
[0022] It should be noted that when an element is referred to as being "set on" another element, it can be directly on the other element or may be interposed with another element. When an element is considered to be "connected" to another element, it can be directly connected to the other element or may be interposed with another element. The terms "upper," "lower," "front," "rear," "left," "right," "top," "bottom," "inner," and "outer," etc., used herein to indicate orientation or positional relationships are based on the orientation or positional relationships shown in the accompanying drawings and are only for the convenience of describing the present invention and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the present invention.
[0023] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.
[0024] Reference Figure 1 and Figure 2 A composite manufacturing apparatus based on interlayer alternating additive polishing includes a base 7, a sealed chamber 13 mounted on the base 7, a multi-axis guide rail laser system disposed in the sealed chamber 13, as well as a detection sensing system and an additive powder feeding system.
[0025] The base 7 is a rigid platform supporting the main structure of the device, which can be made of cast iron or welded steel, providing stable support for each functional module. The sealed chamber 13 is a closed processing cavity, which can be made of a stainless steel shell with an observation window to isolate it from external environmental interference. The multi-axis guide rail laser system is a three-dimensional motion mechanism, which can be implemented using a combination of ball screws and linear guide rails to ensure precise laser focus positioning. The clamping part 10 is a workpiece fixing device, which can be implemented using hydraulic clamps or electromagnetic chucks to keep the workpiece position constant during processing.
[0026] The multi-axis guide rail laser system includes a three-axis platform mounted on a base 7 and a laser generator 2 mounted on the three-axis platform. The three-axis platform includes an x-axis motion module, a y-axis motion module, and a z-axis motion module. The y-axis motion module is slidably mounted on the x-axis motion module, and the z-axis motion module is slidably mounted on the y-axis motion module. The x-axis motion module includes an x-axis track bracket 15, an x-axis track motor 14, and an x-axis rolling screw. The y-axis motion module includes a y-axis track bracket 19, a y-axis track motor 18, and a y-axis rolling screw. The z-axis motion module includes a z-axis track bracket 22, a z-axis track motor 21, and a z-axis rolling screw.
[0027] The x-axis track bracket 15 is equipped with an x-axis track motor 14 and an x-axis rolling screw. The x-axis rolling screw includes a first x-axis track screw 16, a second x-axis track screw 17, and an x-axis nut on the screw. The first x-axis track screw 16 and the second x-axis track screw 17 are mounted on the x-axis track bracket 15 at both ends. One end of the first x-axis track screw 16 and the second x-axis track screw 17 passes through a screw bearing support seat and is connected to the output shafts of the two x-axis track motors through a coupling. The two x-axis track motors work synchronously. Through the symmetrical drive layout of the dual screws, the driving force is evenly distributed on both sides of the motion module, which effectively controls the linearity of the movement of the y-axis motion module in the x-axis direction, reduces the vibration amplitude of the motion mechanism during high-speed movement, and provides a stable motion reference for the alternating execution of laser additive manufacturing and polishing processes, thereby ensuring the consistency of the processing position between layers.
[0028] The x-axis track bracket 15 is equipped with a y-axis track bracket 19 that can move and slide along the first x-axis track screw 16 and the second x-axis track screw 17. Specifically, the y-axis track bracket 19 is fixed on the x-nut. The y-axis track bracket 19 is equipped with a y-axis track motor 18 and a y-axis rolling screw. The y-axis rolling screw includes a y-axis track screw 20 and a y-axis nut. Both ends of the y-axis track screw 20 are installed on the y-axis track bracket 19. One end of the y-axis track screw 20 passes through the screw bearing support seat and is connected to the output shaft of the y-axis track motor 18 through a coupling. A z-axis track bracket 22, movable along the z-axis track screw 20, is mounted on the z-axis track bracket 19. The z-axis track bracket 22 is fixed to the z-nut. A z-axis track motor 21 and a z-axis rolling screw are mounted on the z-axis track bracket 22. The z-axis rolling screw includes a z-axis track screw 23 and a z-axis nut. Both ends of the z-axis track screw 23 are mounted on the z-axis track bracket 22. One end of the z-axis track screw 23 passes through a screw bearing support and is connected to the output shaft of the z-axis track motor 21 via a coupling. A laser mounting bracket, movable along the z-axis track screw 23, is mounted on the z-axis track bracket 22. Specifically, the laser mounting bracket is fixedly connected to the z-axis nut. A servo motor-driven rotating device is mounted on the lower end face of the laser mounting bracket. This rotating device drives the laser generator 2 to rotate. The x-track bracket 15 is fixedly connected to the column 6 by bolts. The column 6 and the side wall opposite to the z-axis track bracket 22 are fixedly connected to the clamping part 12. The clamping part 12 is also fixedly connected to the column 6 by reinforcing ribs. The clamping part 12 is used to clamp the substrate or the formed body. The multi-axis guide rail laser system realizes the precision manufacturing and polishing of the device, and at the same time realizes the precision manufacturing and polishing of complex areas (such as the curved surface and groove of the original part).
[0029] The detection sensing system includes a temperature sensor 8, an ambient oxygen sensor 9, a molten pool sensor 10, and a spectral sensor 11 mounted on the column 6. The temperature sensor 8 and the ambient oxygen sensor 9 are mounted on the side wall of the column 6, while one end of the molten pool sensor 10 and the spectral sensor 11 is mounted on the top of the column 6, with the signal receiving end located above the clamping part 12. An additive powder feeding system is located on the left side of the sealed chamber 13. The additive powder feeding system includes a powder feeder 3, a powder distributor 4, and a powder pipe 5. The additive powder material is transferred through the powder distributor 4 and the powder pipe 5. The output port of the powder feeder 4 is connected to the inlet of the powder distributor 5, and the outlet of the powder distributor 5 is connected to the powder pipe 5. The end of the powder pipe 5 is located above the clamping part 12.
[0030] Temperature sensor 8 is equipped with dual probes for measuring the ambient temperature of the sealed chamber and the substrate temperature. A dual-probe temperature sensor refers to a sensor device containing two independent temperature detection units, specifically implemented using a combination of thermocouples and an infrared temperature measurement module. The first probe collects the air temperature inside the sealed chamber, while the second probe acquires the substrate surface temperature through contact or non-contact measurement. Specifically, the first probe is positioned in the central area of the top of the chamber to monitor the ambient temperature; the second probe is fixed to the side of the clamped part by a flexible bracket, with its detection end pointing towards a preset temperature measurement point on the substrate surface. Ambient oxygen sensor 9 measures the oxygen concentration inside the sealed chamber 13, molten pool sensor 10 measures the molten pool depth and linear energy density, and spectral sensor 11 measures the spectral wavelength characteristics of the polished area.
[0031] The above technical solution enables the alternating execution of additive manufacturing and polishing processes, effectively blocking the accumulation path of interlayer defects. By real-time monitoring of the molten pool state, the ambient temperature of the sealing chamber, and the substrate temperature, processing parameters can be adjusted, significantly improving the surface quality of the formed parts and reducing the burden on subsequent finishing processes.
[0032] In one possible embodiment, the servo motor-driven rotation device refers to a mechanical transmission mechanism that provides rotational power through a servo motor and has angle feedback. Specifically, it can be implemented by combining a worm gear reducer with a rotary encoder to precisely control the incident direction of the laser beam.
[0033] In one possible embodiment, a computer 1 is also included. The powder feeder 3 is connected to the computer 1 via wires and can receive computer commands. The computer 1 is connected to the laser generator 2 via wires and adjusts the parameters of the laser generator 2 to switch between additive manufacturing and polishing modes. The parameters of the laser generator 2 can be adjusted manually or through the built-in software of the laser generator within the computer 1. The computer 1 is connected to the x-track motor 14, y-track motor 18, and z-track motor 21 via wires to drive the supports in each direction to move in the target direction. After a single layer of material deposition is completed, the laser power is switched to polishing mode, and the three-axis platform drives the laser head along a predetermined path to remelt and trim the surface of the current layer. The detection data is transmitted to the control system in real time, and the laser power and scanning speed are dynamically adjusted to achieve closed-loop control of interlayer quality.
[0034] Temperature sensor 8, ambient oxygen sensor 9, molten pool sensor 10, and spectral sensor 11 are all connected to computer 1 via wires for real-time feedback of monitoring data. (Refer to...) Figure 3 The composite manufacturing method using the above-mentioned composite manufacturing apparatus based on interlayer alternating additive polishing includes the following periodic timing control steps: Step 1: Fix the substrate or pre-formed body with clamping part 12. Adjust the laser generator 2 to the target position through x-track bracket 15, y-track bracket 19 and z-track bracket 22. Start the argon gas filling system to replace the air in the sealed chamber and monitor the data of the ambient oxygen sensor 9 in real time. When the concentration is ≥100ppm, continue argon filling. When the concentration is <100ppm, close the inlet and outlet ports. The computer 1 controls the powder feeder 3 to deposit the kth additive layer powder on the substrate or pre-formed body through the powder distributor 4 and powder pipe 5. Then, the laser generator 2 melts the additive layer powder at a preset power and scanning speed. The specific additive process parameters are: the laser power for powder bed melting is 50-500W, the laser scanning speed is 0.5-3.0m / s, the powder feeding rate for directional energy deposition is 10-50g / min, the melt pool sensor 10 monitors the melt pool penetration depth and linear energy density in real time. If the melt pool penetration depth and linear energy density exceed the threshold, the laser generator 2 is paused. The temperature sensor 8 measures the substrate temperature in real time. Step 2: After the additive manufacturing of the kth additive layer is completed and the ambient temperature of the sealed chamber drops to the preset temperature (40-45℃), deposit the (k+1)th additive layer on the kth additive layer. Furthermore, in the additive manufacturing processes of steps one and two, the powder layer thickness and powder spreading speed are controlled to ensure the smooth progress of the additive manufacturing stage. The single-layer powder thickness H and the powder particle size satisfy the following:
[0035] In the formula: The particle size corresponding to 10% and 90% cumulative powder distribution. The compaction compensation during the additive manufacturing process is typically 2-5 mm; while the powder spreading speed is important to meet the rheological properties of the powder material. Satisfy the following formula:
[0036] In the formula: This represents the particle size corresponding to 50% of the cumulative powder distribution. It is the acceleration due to gravity. This refers to the angle of repose of the powder material; specific values can be found online. The coefficient of friction between the powder and the substrate.
[0037] Furthermore, the laser melting performed after the powder material is laid in step one follows the powder melting kinetics model, and the theoretical molten pool penetration depth can be calculated. The molten pool sensor 10 monitors the actual molten pool penetration depth h and the actual linear energy density in real time, as well as the theoretical molten pool penetration depth. and actual molten pool penetration depth The relation is:
[0038] In the formula: For laser power, Thermal conductivity, The initial temperature of the substrate. For real-time substrate temperature, The thermal diffusivity of additive powder materials, For laser dwell time, The radius of the light spot is... It continued to melt at that time, when Immediately turn off the laser to stop melting.
[0039] Actual linear energy density The stability criterion is ,in, The material density of the additive powder; The formula for calculating the actual linear energy density of additive powder is:
[0040] in, For laser scanning speed, until linear energy density The process proceeds to the next step only after the stability threshold is met. During this determination process, data is monitored in real-time by temperature sensor 8 and molten pool sensor 10 to calculate... The value is determined, and stability is judged according to the stability criterion. If it exceeds the specified range, melting is stopped, and the laser is restarted to continue melting when the substrate temperature returns to a suitable value (120-150℃).
[0041] Step 3: After completing the deposition of the (k+1)th layer, the exposed surface of the (k+1)th additive layer is polished in situ using a laser with time-division output from the same source laser as the additive layer; the polishing depth h1 is calculated using formula (5), and the laser power, scanning speed, and scanning time are adjusted according to the polishing depth h1. The polishing process in this step is energy-assisted laser polishing; the relationship between the polishing depth h1 and the thickness H of the additive single layer is as follows:
[0042] In the formula: This is the depth adjustment factor, 0.1≤ ≤0.8, When the value is less than 0.1, the polishing energy is insufficient, and traces of molten pool fluctuation remain. When the value is greater than 0.8, excessive melting leads to a decrease in interlayer bonding strength and material bonding strength. With depth adjustment coefficient They are negatively correlated, specifically:
[0043] In the formula: The material attenuation coefficient is determined by the material's inherent properties. It is the theoretical maximum bonding strength of the material.
[0044] Furthermore, for this step, a laser polishing process using a laser from the same source as the additive manufacturing laser with time-division output is adopted, and the energy density of the laser polishing is set to... The calculation formula is:
[0045] In the formula: The linear energy density during laser polishing. For linear energy density during additive manufacturing, The energy conversion coefficient is preferably 0.25-0.35.
[0046] Furthermore, to ensure the elimination of directional lines in additive scanning, the angle between the polishing scanning path and the additive scanning path is adjusted to satisfy the following relationship:
[0047] In the formula: To reduce the angle between the laser polishing path and the additive manufacturing scanning path, To avoid the angle being too small, which would prevent the texture from being effectively covered, This refers to the scanning path direction vector during additive manufacturing. This is the scanning path direction vector during laser polishing, designed to control the included angle. To eliminate directional lines generated during additive manufacturing, computer 1 determines the polishing path at an optimal angle. The optimal solution for this angle is:
[0048] in, The optimal polishing path angle is used to maximize the effect of texture elimination.
[0049] In this process, a multi-axis guide rail laser system is used for angle adjustment, and the optimal solution is calculated according to equation (9). Then, it drives the x-track motor 14, y-track motor 18, and z-track motor 21, causing the laser generator 2 to rotate. After angling, scanning is performed to eliminate textures and create polished curved surfaces.
[0050] Reference Figure 4 Furthermore, throughout the polishing process, surface data is monitored in real time, and the surface roughness of the (k+1)th layer is obtained through the spectral sensor 11. value:
[0051] In the formula: The first data collected by the spectral sensor Height data of each point (unit: ), The average height of all measurement points. This represents the number of sampling points in a single scan by the sensor.
[0052] when > Threshold At that time, the polishing energy density is adaptively increased as follows:
[0053] In the formula: This is the adaptive adjustment coefficient, typically 0.2 ≤ γ ≤ 0.5; Let be the minimum achievable roughness of the material, and be an inherent property of the material itself. The maximum roughness is set; For the new polishing energy density after adaptation, The original polishing density before adaptation, and .
[0054] Step 4: Let k = k + 2, and repeat steps 1 to 3 until the workpiece is completed, where k is an integer ≥ 1. After step 3 of each cycle is completed, residual heat remains in the sealed chamber; this residual heat is used to preheat the next additive layer. After the final additive layer is completed, two consecutive polishing processes are performed, with the first polishing depth being 0.5H and the second polishing depth being 0.2H.
[0055] During the cycle, the interval time and the temperature of preheating using residual heat need to be monitored simultaneously. When polishing ends, timing starts and a command is sent to temperature sensor 8 to record the surface temperature at the end of polishing. Calculate the time interval After an interval Then, a new round of additive polishing begins from step one, with the time interval between the end of polishing in step three and the beginning of step one in the next cycle. satisfy:
[0056] In the formula: The melting point of the additive powder material. The workpiece surface temperature at the end of polishing. The material cooling rate coefficient of additive powder.
[0057] Furthermore, after each cycle, during the preheating of the starting additive layer for the new cycle using residual heat from the in-situ polishing step, the initial deposition temperature of the additive layer and the final polishing temperature satisfy the following:
[0058] In the formula: The initial deposition temperature of a new additive manufacturing cycle (i.e., the surface temperature at which the (k+2)th layer begins deposition), and the terminal-initial temperature coefficient. This is an inherent property of the material itself, specifically the optimal initial-final temperature coefficient of the material is determined experimentally and calculated. The interlayer temperature gradient... satisfy:
[0059] In the formula: Temperature field distribution function , representing any point in the additive-polishing composite structure The temperature is z, and z is the thickness of the additive polishing layer in the vertical direction.
[0060] Furthermore, the method for adjusting specific layers during the cycle is as follows: when k=1, polishing is skipped and the second layer is deposited directly; and if the kth or k+1th layer is a support structure, polishing is skipped. Furthermore, after every three cycles, an additional cross-layer fine polishing is added. Specifically, this means polishing the second layer after the first and second additive manufacturing layers; polishing the fourth layer after the third and fourth additive manufacturing layers; and fine polishing the sixth layer after the fifth and sixth additive manufacturing layers, and so on, to begin a new three-cycle process. The depth of cross-layer fine polishing in this step... Relationship with single-layer thickness and material removal volume for:
[0061]
[0062] Where: interlayer thickness parameter In polishing, the specific number of layers is 2 or 3, and the layer relationship is determined experimentally; The polishing energy threshold, This represents the polishing energy density.
[0063] This method breaks through the limitations of traditional additive manufacturing and post-processing, enabling real-time repair of interlayer defects and control of residual stress. It can significantly improve the surface quality and density of components, reduce surface roughness, and decrease the cumulative effect of surface roughness by more than 80%. It improves manufacturing efficiency and is suitable for manufacturing precision parts from metals, ceramics, and polymers.
[0064] The term "constituting of" in describing a combination should include the identified elements, components, parts, or steps, as well as other elements, components, parts, or steps that do not substantially affect the essential novel features of the combination. The use of the terms "comprising" or "including" to describe combinations of elements, components, parts, or steps herein also contemplates embodiments that are essentially composed of such elements, components, parts, or steps. The use of the term "may" herein is intended to indicate that any described attribute included by "may" is optional.
[0065] Multiple elements, components, parts, or steps can be provided by a single integrated element, component, part, or step. Alternatively, a single integrated element, component, part, or step can be divided into multiple separate elements, components, parts, or steps. The use of the word "a" or "an" to describe an element, component, part, or step does not imply the exclusion of other elements, components, parts, or steps.
[0066] It should be understood that the above description is for illustrative purposes and not for limitation. Many embodiments and applications beyond the provided examples will be apparent to those skilled in the art upon reading the above description. Therefore, the scope of this teaching should not be determined by reference to the above description, but rather by reference to the foregoing claims and the full scope of their equivalents. For purposes of completeness, all articles and references, including patent applications and publications, are incorporated herein by reference. The omission of any aspect of the subject matter disclosed herein in the foregoing claims is not intended as a waiver of that subject matter, nor should it be construed as an indication that the applicant has not considered that subject matter as part of the disclosed inventive subject matter.
Claims
1. A hybrid manufacturing apparatus based on interlaminar alternating additive polishing, characterized by, It includes a base (7) and an additive powder feeding system. A sealed chamber (13) and a column (6) are installed on the base (7). A three-axis platform, a laser generator (2) and a temperature sensor (8) are provided inside the sealed chamber (13). A clamping part (12) is installed on the side of the column (6) facing the laser generator (2), and the clamping part (12) is used to fix the substrate or the formed body. The three-axis platform is used to drive the laser generator (2) to move in three mutually perpendicular directions.
2. A hybrid manufacturing apparatus based on interlaminar alternating additive polishing according to claim 1, characterized in that, The three-axis platform includes an x-axis motion module, a y-axis motion module, and a z-axis motion module. The y-axis motion module is slidably mounted on the x-axis motion module, and the z-axis motion module is slidably mounted on the y-axis motion module. The x-axis motion module includes an x-axis track support (15), a double lead screw structure, and two synchronously operating x-axis track motors (14). The dual lead screw structure includes a first x-axis track lead screw (16) and a second x-axis track lead screw (17) driven synchronously by two x-axis track motors (14). The first x-axis track lead screw (16) and the second x-axis track lead screw (17) are mounted side by side on the x-axis track bracket (15). An x-axis nut is installed on both the first x-axis track lead screw (16) and the second x-axis track lead screw (17). The x-axis nut is fixedly connected to the y-axis motion module.
3. A hybrid manufacturing apparatus based on interlaminar alternating additive polishing according to claim 2, characterized in that, The y-axis motion module includes a y-axis track bracket (19) and a y-axis track screw (20) mounted on the y-axis track bracket (19), and a y-axis nut is mounted on the y-axis track screw (20). The z-axis motion module includes a z-axis track bracket (22) fixed to the y-axis nut and a z-axis track screw (23) installed on the z-axis track bracket (22). A z-axis nut is installed on the z-axis track screw (23), and a laser mounting bracket is fixed on the z-axis nut. The laser generator (2) is installed on the laser mounting bracket.
4. The hybrid manufacturing apparatus based on interlaminar alternating additive polishing according to claim 1, characterized in that, The laser generator (2) is mounted on a three-axis platform via a laser mounting bracket. The lower end of the laser mounting bracket is equipped with a servo motor-driven rotating device, which drives the laser generator (2) to adjust its angle.
5. The hybrid manufacturing apparatus based on interlaminar alternating additive polishing according to claim 1, characterized in that, The column (6) has reinforcing ribs between its side wall and the clamping part (12).
6. The hybrid manufacturing device based on interlaminar alternating additive polishing according to claim 1, characterized in that, The temperature sensor (8) is equipped with dual probes, which monitor the ambient temperature of the sealed chamber (13) and the substrate temperature on the clamping part (12) in real time.
7. A composite manufacturing apparatus based on interlayer alternating additive polishing according to claim 1, characterized in that, In the additive powder feeding system: The output end of the powder feeder (3) is connected to the feed inlet of the powder distributor (4); The discharge port of the powder separator (4) extends through the powder pipe (5) directly above the clamping part (12).
8. The hybrid manufacturing device based on interlaminar alternating additive polishing according to claim 1, characterized in that, The laser generator (2) has an additive mode and a polishing mode, and the linear energy density in the polishing mode is 25%-35% of the linear energy density in the additive mode.
9. The hybrid manufacturing device based on interlaminar alternating additive polishing according to claim 1, characterized in that, It also includes an ambient oxygen sensor (9) for measuring the oxygen concentration inside the sealed chamber (13), a molten pool sensor (10) for real-time monitoring of the molten pool penetration depth and linear energy density, and a spectral sensor (11) for measuring the spectral wavelength characteristics of the polished area.
10. A hybrid manufacturing apparatus based on interlaminar alternating additive polishing according to claim 9, characterized in that, The molten pool sensor (10) and the spectral sensor (11) are mounted on the top of the column (6), with their signal receiving ends facing the working area above the clamping part (12).