A semiconductor testing structure and wafer bonding structure

By designing a semiconductor test structure and utilizing metal connecting pillars to connect the key pads, and employing different voltage tests, the accuracy problem of key pad reliability testing in hybrid bonding processes was solved, and reliability assessment was achieved under alignment deviation conditions.

CN224988008UActive Publication Date: 2026-11-17NEXCHIP SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522481134.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-21
Publication Date
2026-11-17
Estimated Expiration
2035-11-21

AI Technical Summary

Technical Problem

In the prior art, the dielectric breakdown method and the ramp voltage breakdown method cannot accurately test the reliability of the bond pads in the wafer bonding structure in the hybrid bonding process.

Method used

A semiconductor test structure is designed, including a first metal layer, a first test layer, a second metal layer, and a second test layer, which are connected by metal connecting pillars to form aligned or offset bonding pads. Different voltage tests are used to evaluate the reliability of the bonding pads.

Benefits of technology

In hybrid bonding where keypad alignment deviations exist, this method enables more accurate testing of keypad reliability, thus improving test accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224988008U_ABST
    Figure CN224988008U_ABST
Patent Text Reader

Abstract

This invention proposes a semiconductor testing structure and a wafer bonding structure. The semiconductor testing structure includes a first metal layer formed on the surface of a first wafer, comprising multiple spaced-apart first metal segments; a first test layer connected to a portion of the first metal segments; a second metal layer formed on the surface of a second wafer, comprising multiple spaced-apart second metal segments; bonding pads formed on the first and second metal segments, with corresponding connections between the bonding pads of the first and second metal segments; and a second test layer connected to a portion of the second metal segments. The first and second test layers form two metal bonding pads, one of which is coupled to a high-level voltage, and the other to a low-level voltage or ground. This invention enables more accurate testing of bonding pad reliability even in hybrid bonding systems where alignment deviations exist.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of semiconductor technology, and in particular to a semiconductor testing structure and wafer bonding structure. Background Technology

[0002] Three-dimensional integration is achieved by using a hybrid bonding process involving metal interconnects between two wafers. For reliability studies of the hybrid bonding pad structure, existing technologies employ dielectric breakdown and ramp voltage breakdown methods. However, these methods utilize comb and chain structures, respectively, which cannot accurately test the reliability of the bonding pads within the hybrid bonding process. Therefore, improvements are needed. Utility Model Content

[0003] In view of the shortcomings of the prior art described above, the purpose of this utility model is to provide a semiconductor testing structure and a wafer bonding structure to improve the electrical testing problem of pad alignment deviation in the wafer bonding structure.

[0004] To achieve the above and other related objectives, this utility model provides a semiconductor testing structure, comprising:

[0005] A first metal layer is formed on the surface of a first wafer, and the first metal layer includes a plurality of spaced-apart first metal segments;

[0006] The first test layer is connected to a portion of the first metal segment;

[0007] A second metal layer is formed on the surface of a second wafer, and the second metal layer includes a plurality of spaced-apart second metal segments;

[0008] Key pads are formed on the first metal segment and the second metal segment, and the key pads of the first metal segment and the key pads of the second metal segment are correspondingly connected;

[0009] The second test layer is connected to a portion of the second metal segment;

[0010] The first test layer and the second test layer form two metal pads, one of which is coupled to a high-level voltage and the other is coupled to a low-level voltage or ground.

[0011] In one embodiment of this utility model, a through hole is formed between the first test layer and the first metal layer, and a metal connecting post is disposed in the through hole;

[0012] The first test layer is connected to the plurality of first metal segments by the plurality of metal connecting posts.

[0013] In one embodiment of the present invention, the side edge of the key pad on the first metal segment does not exceed the boundary of the first metal segment, nor does it exceed the boundary of the second metal segment corresponding to the first metal segment;

[0014] The side edge of the key pad on the second metal segment does not extend beyond the boundary of the first metal segment, nor does it extend beyond the boundary of the second metal segment.

[0015] In one embodiment of this utility model, the key pads on the first metal segment are completely aligned with the key pads on the second metal segment;

[0016] Alternatively, the key pads on the first metal segment and the key pads on the second metal segment are offset from each other.

[0017] In one embodiment of this utility model, the cross-section of the key pad is rectangular in the horizontal direction;

[0018] The key pads on the first metal segment are offset along one corner of the key pads on the second metal segment, and the ratio of the offset distance of the key pads on the first metal segment to the side length of the key pads is 5% to 20%.

[0019] In one embodiment of this utility model, the cross-section of the key pad is rectangular in the horizontal direction;

[0020] The key pads on the first metal segment are offset along one side of the key pads on the second metal segment, and the ratio of the offset distance of the key pads on the first metal segment to the side length of the key pads is 5% to 20%.

[0021] In one embodiment of the present invention, a plurality of key pads are arranged in an array between the first metal layer and the second metal layer.

[0022] In one embodiment of this utility model, the key pads that are fully aligned are referred to as the first key pads, and the key pads that are offset from each other are referred to as the second key pads.

[0023] In the row and column directions of the matrix, the first and second bond pads are distributed alternately.

[0024] In one embodiment of this invention, second key pads of different offset types are periodically distributed in the row and column directions of the matrix.

[0025] This utility model also proposes a wafer bonding structure, including:

[0026] A first wafer has a first metal layer and a first test layer formed on its surface; the first metal layer includes a plurality of spaced-apart first metal segments; the first test layer is connected to a portion of the first metal segments.

[0027] A second wafer has a second metal layer and a second test layer formed on its surface; the second metal layer includes a plurality of spaced-apart second metal segments; the second test layer is connected to a portion of the second metal segments.

[0028] Key pads are formed on the first metal segment and the second metal segment, and the key pads of the first metal segment and the key pads of the second metal segment are correspondingly connected;

[0029] The first test layer and the second test layer form two metal pads, one of which is coupled to a high-level voltage and the other is coupled to a low-level voltage or ground.

[0030] As described above, the semiconductor testing structure and wafer bonding structure of this utility model have an unexpected technical effect: in the case of alignment deviations in the bonding pads during hybrid bonding, the reliability of the bonding pads can be tested more accurately. Attached Figure Description

[0031] Figure 1 This is a top view of a semiconductor test structure provided in an embodiment of the present invention.

[0032] Figure 2 Provided for an embodiment of this utility model Figure 1 Schematic diagram of the cross section along the AA direction.

[0033] Figure 3 Provided for an embodiment of this utility model Figure 1 Top view of the first metal layer.

[0034] Figure 4 Provided for an embodiment of this utility model Figure 1 Top view of the keypads in the first metal layer and the keypads in the second metal layer.

[0035] Reference numerals: 10, first metal layer; 100, first metal segment; 20, first test layer; 30, second metal layer; 300, second metal segment; 40, second test layer; 50, key pad; 60, metal connecting post. Detailed Implementation

[0036] The following specific examples illustrate the implementation of this utility model. Those skilled in the art can easily understand other advantages and effects of this utility model from the content disclosed in this specification. This utility model can also be implemented or applied through other different specific embodiments, and various details in this specification can also be modified or changed based on different viewpoints and applications without departing from the spirit of this utility model. It should be noted that, unless otherwise specified, the following embodiments and features described therein can be combined with each other.

[0037] It should be noted that the illustrations provided in the following embodiments are only schematic representations of the basic concept of the present invention. Therefore, the drawings only show the components related to the present invention and are not drawn according to the number, shape and size of the components in actual implementation. In actual implementation, the form, quantity and proportion of each component can be arbitrarily changed, and the layout of the components may also be more complex.

[0038] In the following description, numerous details are explored to provide a more thorough explanation of embodiments of the present invention. However, it will be apparent to those skilled in the art that embodiments of the present invention may be practiced without these specific details. In other embodiments, well-known structures and devices are shown in block diagram form rather than in detail to avoid obscuring embodiments of the present invention.

[0039] Please see Figures 1 to 4 This invention proposes a semiconductor testing structure and a wafer bonding structure that can be applied to hybrid bonding processes for wafer metal interconnects. In the case of pad alignment deviations in the hybrid bonding process, it can accurately assess the reliability of the pads.

[0040] Please see Figure 1 , Figure 2 and Figure 3 In one embodiment of the present invention, the semiconductor test structure may include a first metal layer 10, a first test layer 20, a second metal layer 30, a second test layer 40, and a bonding pad 50.

[0041] Specifically, the first metal layer 10 and the first test layer 20 are formed on the surface of the first wafer. Both the first metal layer 10 and the first test layer 20 are metal layers; the first metal layer 10 is the top metal layer (TM), and the first test layer is the lower metal layer. The top metal layer is the highest metal layer in the metal interconnect stack structure and is typically thicker (by several micrometers) than the lower metal layers (M1, M2…) to reduce resistance and improve current carrying capacity.

[0042] like Figure 1 , Figure 2 and Figure 3 As shown, the first metal layer 10 includes a plurality of spaced-apart first metal segments 100, which are separated from each other. The first test layer 20 is connected to the plurality of first metal segments 100. It should be understood that, as Figure 2 As shown, the first test layer 20 is connected to a portion of the first metal segment 100, not to all of the first metal segment 100.

[0043] Specifically, the second metal layer 30 and the second test layer 40 are formed on the surface of the second wafer. Both the second metal layer 30 and the second test layer 40 are metal layers, with the second metal layer 30 being the top metal layer (TM) and the second test layer being the bottom metal layer.

[0044] like Figure 1 , Figure 2 and Figure 3 As shown, the second metal layer 30 includes a plurality of spaced-apart second metal segments 300, which are separated from each other. The second test layer 40 is connected to the plurality of second metal segments 300. It should be understood that, as Figure 2 As shown, the second test layer 40 is connected to a portion of the second metal segment 300, not to all of the second metal segment 300.

[0045] Please see Figure 1 , Figure 2 and Figure 3 The first wafer and the second wafer are bonded together, and bonding pads 50 are formed on the first metal segment 100 and the second metal segment 300. The bonding pads 50 of the first metal segment 100 and the bonding pads 50 of the second metal segment 300 are correspondingly connected. That is, bonding pads 50 are formed on the first metal segment 100 and the second metal segment 300, and the bonding pads 50 on the first metal segment 100 and the bonding pads 50 on the second metal segment 300 are correspondingly connected.

[0046] Specifically, such as Figure 2 As shown, the first test layer 20 and the second test layer 40 form two metal pads, one of which is coupled to a high-level voltage, and the other is coupled to a low-level voltage or ground. The first test layer 20 and the second test layer 40 are not connected and are connected to external circuitry for testing. For example, the first test layer 20 and the second test layer 40 can form two test ports, with different voltages applied to create a voltage difference. Reliability testing can then be performed to measure the breakdown voltage between the key pads 50, and time-related dielectric breakdown testing can be performed to evaluate the breakdown life of the key pads 50 under long-term use.

[0047] Please see Figure 1 and Figure 2 In one embodiment of this utility model, a through hole is formed between the first test layer 20 and the first metal layer 10, and a metal connecting post 60 is disposed in the through hole. The first test layer 20 is connected to a plurality of first metal segments 100 through a plurality of metal connecting posts 60.

[0048] Similarly, a through-hole is formed between the second test layer 40 and the second metal layer 30, and a metal connecting post 60 is disposed within the through-hole. The second test layer 40 is connected to the plurality of second metal segments 300 through the plurality of metal connecting posts 60.

[0049] Specifically, a via is a vertical through-hole that connects different metal layers to achieve electrical connection. Through the design of vias, the breakdown characteristics of the dielectric layer between key pads can be tested to evaluate the reliability of the dielectric layer.

[0050] Please see Figure 1 , Figure 2 and Figure 3 In one embodiment of this utility model, the side edge of the key pad 50 on the first metal segment 100 does not exceed the boundary of the first metal segment 100, nor does it exceed the boundary of the corresponding second metal segment 300. Furthermore, the side edge of the key pad 50 on the second metal segment 300 does not exceed the boundary of either the first metal segment 100 or the second metal segment 300.

[0051] like Figure 2 As shown, the key pad 50 between the first metal segment 100 and the second metal segment 300 is confined between the boundary of the first metal segment 100 and the boundary of the second metal segment 300, ensuring that the key pad 50 can be effectively evaluated during the test.

[0052] Please see Figure 2 and Figure 4 In one embodiment of the present invention, the key pads 50 on the first metal segment 100 are completely aligned with the key pads on the second metal segment 300, or the key pads 50 on the first metal segment 100 and the key pads on the second metal segment 300 are offset from each other.

[0053] Specifically, the keypad 50 on the first metal segment 100 is completely aligned with the keypad on the second metal segment 300, such as... Figure 2 As shown in the keypads 50 on both sides, the keypads 50 on the first metal segment 100 correspond exactly to the keypads 50 on the second metal segment 300.

[0054] It should be understood that, between the key pads 50 on the first metal segment 100 and the key pads 50 on the second metal segment 300, when the ratio of the offset distance of the key pads 50 on the first metal segment 100 to the side length of the key pads 50 is less than 5% (or 3%), the key pads 50 on the first metal segment 100 and the key pads 50 on the second metal segment 300 can be considered to correspond completely.

[0055] Specifically, the keypads 50 on the first metal segment 100 and the keypads on the second metal segment 300 are offset from each other, such as... Figure 2The keypad 50 in the middle can be offset from one corner of the keypad 50 on the first metal segment 100 along the second metal segment 300, and the ratio of the offset distance of the keypad on the first metal segment to the side length of the keypad is 5% to 20%. Alternatively, the keypad 50 on the first metal segment 100 can be offset from one side of the keypad 50 on the second metal segment 300 (not shown in the figure), and the ratio of the offset distance of the keypad on the first metal segment to the side length of the keypad is 5% to 20%.

[0056] In this embodiment, the semiconductor test structure takes into account the common alignment deviation of the bond pads 50 in the hybrid bonding process, and designs different shift situations to more realistically simulate the bonding situation in actual production.

[0057] Please see Figure 2 and Figure 4 In one embodiment of this invention, the key pads 50 are arranged in a matrix between the first metal layer 10 and the second metal layer 30. Fully aligned key pads 50 are designated as first key pads, and mutually offset key pads 50 are designated as second key pads. The first and second key pads are alternately distributed along the row and column directions of the matrix.

[0058] Specifically, such as Figure 2 and Figure 4 As shown, the first and second bond pads are alternately distributed along each row of the matrix. Furthermore, the first and second bond pads are alternately distributed along each column of the matrix.

[0059] By alternating the first and second key pads in a regular pattern, the mutual offset between the key pads 50 can be analyzed to determine its impact on the reliability of the dielectric layer in hybrid bonding.

[0060] Please see Figure 2 and Figure 4 In one embodiment of this utility model, the second key pads of different offset types are periodically distributed in the row and column directions of the matrix.

[0061] Specifically, in each row of the matrix, the second key pads with different offset types are periodically distributed. Furthermore, in each column of the matrix, the second key pads with different offset types are periodically distributed. Offset type refers to the offset direction of the first key pad relative to the second key pad.

[0062] For example, in Figure 4In the first row and second column, the key pad 50 of the first metal segment 100 is located at the lower right corner of the key pad 50 of the first metal segment 100. In the first row and fourth column, the key pad 50 of the first metal segment 100 is located at the upper left corner of the key pad 50 of the first metal segment 100. In the sixth column of the first row and the other columns after the first row, the key pads 50 are periodically distributed according to the offset type of the key pads 50 in the first row and second column and the first row and fourth column as described above.

[0063] For example, in Figure 4 In the first column, second row, the keypad 50 of the first metal segment 100 is located at the lower left corner of the keypad 50 of the first metal segment 100. In the first column, fourth row, the keypad 50 of the first metal segment 100 is located at the upper right corner of the keypad 50 of the first metal segment 100. In the first column, sixth row and other rows after the first column, the keypad 50 offset types of the first column, second row and first column, fourth row are periodically distributed.

[0064] Of course, in other embodiments, the key pads 50 may also be periodically distributed according to other offset types in the row direction and column direction of the matrix, which will not be listed here.

[0065] Please see Figure 1 , Figure 2 In one embodiment of this utility model, a wafer bonding structure may also be proposed, which may include a first wafer and a second wafer.

[0066] A first metal layer 10 and a first test layer 20 are formed on the surface of a first wafer. The first metal layer 10 includes a plurality of spaced-apart first metal segments 100. The first test layer 20 is connected to the plurality of first metal segments 100.

[0067] A second metal layer 30 and a second test layer 40 are formed on the surface of a second wafer. The second metal layer 30 includes a plurality of spaced-apart second metal segments 300. The second test layer 40 is connected to the plurality of second metal segments 300.

[0068] Key pads 50 are formed on the first metal segment 100 and the second metal segment 300, and the key pads 50 of the first metal segment 100 and the key pads 50 of the second metal segment 300 are connected accordingly.

[0069] The first test layer 20 and the second test layer 40 form two metal pads, one of which is coupled to a high-level voltage and the other is coupled to a low-level voltage or ground.

[0070] In summary, the semiconductor testing structure and wafer bonding structure disclosed in this utility model have an unexpected technical advantage: they enable more accurate testing of bond pad reliability even when alignment deviations exist in hybrid bonding. Therefore, this utility model effectively overcomes the various shortcomings of the prior art and has high industrial applicability.

[0071] The above embodiments are merely illustrative of the principles and effects of this utility model and are not intended to limit the scope of this utility model. Any person skilled in the art can modify or alter the above embodiments without departing from the spirit and scope of this utility model. Therefore, all equivalent modifications or alterations made by those skilled in the art without departing from the spirit and technical concept disclosed in this utility model should still be covered by the claims of this utility model.

Claims

1. A semiconductor testing structure, characterized in that, include: A first metal layer is formed on the surface of a first wafer, and the first metal layer includes a plurality of spaced-apart first metal segments; The first test layer is connected to a portion of the first metal segment; A second metal layer is formed on the surface of a second wafer, and the second metal layer includes a plurality of spaced-apart second metal segments; Key pads are formed on the first metal segment and the second metal segment, and the key pads of the first metal segment and the key pads of the second metal segment are correspondingly connected; The second test layer is connected to a portion of the second metal segment; The first test layer and the second test layer form two metal pads, one of which is coupled to a high-level voltage and the other is coupled to a low-level voltage or ground.

2. The semiconductor test structure according to claim 1, characterized in that, A through-hole is formed between the first test layer and the first metal layer, and a metal connecting post is disposed in the through-hole; The first test layer is connected to the plurality of first metal segments by the plurality of metal connecting posts.

3. The semiconductor test structure according to claim 1, characterized in that, The side edge of the key pad on the first metal segment does not extend beyond the boundary of the first metal segment, nor does it extend beyond the boundary of the corresponding second metal segment; The side edge of the key pad on the second metal segment does not extend beyond the boundary of the first metal segment, nor does it extend beyond the boundary of the second metal segment.

4. The semiconductor test structure according to claim 1, characterized in that, The key pads on the first metal segment are perfectly aligned with the key pads on the second metal segment; Alternatively, the key pads on the first metal segment and the key pads on the second metal segment are offset from each other.

5. The semiconductor test structure according to claim 4, characterized in that, In the horizontal direction, the cross-section of the key pad is rectangular; The key pads on the first metal segment are offset along one corner of the key pads on the second metal segment, and the ratio of the offset distance of the key pads on the first metal segment to the side length of the key pads is 5% to 20%.

6. The semiconductor test structure according to claim 4, characterized in that, In the horizontal direction, the cross-section of the key pad is rectangular; The key pads on the first metal segment are offset along one side of the key pads on the second metal segment, and the ratio of the offset distance of the key pads on the first metal segment to the side length of the key pads is 5% to 20%.

7. The semiconductor test structure according to claim 5 or 6, characterized in that, The plurality of key pads are arranged in an array between the first metal layer and the second metal layer.

8. The semiconductor test structure according to claim 7, characterized in that, The keypads that are perfectly aligned are designated as the first keypads, and the keypads that are offset from each other are designated as the second keypads. In the row and column directions of the matrix, the first and second bond pads are distributed alternately.

9. The semiconductor test structure according to claim 8, characterized in that, In the row and column directions of the matrix, the second bond pads of different offset types are periodically distributed.

10. A wafer bonding structure, characterized in that, include: A first wafer has a first metal layer and a first test layer formed on its surface; the first metal layer includes a plurality of spaced-apart first metal segments; the first test layer is connected to a portion of the first metal segments. A second wafer has a second metal layer and a second test layer formed on its surface; the second metal layer includes a plurality of spaced-apart second metal segments; the second test layer is connected to a portion of the second metal segments. Key pads are formed on the first metal segment and the second metal segment, and the key pads of the first metal segment and the key pads of the second metal segment are correspondingly connected; The first test layer and the second test layer form two metal pads, one of which is coupled to a high-level voltage and the other is coupled to a low-level voltage or ground.