A power device packaging structure based on TMBS

By employing an alumina-alumina nitride composite ceramic substrate and a vertical graphene thermal conductive film in the TMBS device package, combined with leadless bonding bump welding and TMBS-TVS functional integration, the problems of poor heat dissipation, high parasitic parameters, and low reliability of existing packaging structures are solved, achieving a packaging structure with high heat dissipation, low cost, and high reliability.

CN224988029UActive Publication Date: 2026-11-17SHANGHAI YIDU POWER SEMICON TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202522553033.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-01
Publication Date
2026-11-17
Estimated Expiration
2035-12-01

AI Technical Summary

Technical Problem

Existing TMBS device packaging structures suffer from poor heat dissipation, high parasitic parameters, low functional integration, and insufficient environmental resistance, limiting their application in high-frequency, high-power, and harsh environments.

Method used

By employing an alumina-alumina composite ceramic matrix, a vertical graphene thermal conductive film, and leadless bonding bump welding technology, combined with the integrated design of TMBS and TVS functional areas, a packaging structure with high-efficiency heat dissipation, low parasitic parameters, and high reliability is formed.

Benefits of technology

It significantly improves the heat dissipation performance and electrical reliability of TMBS devices, reduces packaging costs, enhances high-frequency characteristics and environmental resistance, and is suitable for high-density integration applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224988029U_ABST
    Figure CN224988029U_ABST
Patent Text Reader

Abstract

This utility model discloses a power device packaging structure based on TMBS, belonging to the field of power device packaging technology, aiming to solve the problems of poor heat dissipation, high parasitic parameters, low reliability, and high cost of existing TMBS packaging. It includes a packaging substrate, a TMBS integrated chip, electrode components, a heat dissipation protective layer, and an insulating and thermally conductive filling layer. The TMBS integrated chip includes an epitaxial substrate, on which TMBS and TVS regions are divided and corresponding structures are formed to achieve functional integration. The electrode components adopt a leadless bonding design and are connected to the chip through bump soldering. The heat dissipation protective layer is composed of thermally conductive silicone, a vertical graphene thermally conductive film, and a polyimide protective film. The insulating and thermally conductive filling layer fills the packaging gaps. This structure has a thermal resistance as low as 0.04℃·cm² / W, a parasitic inductance ≤2nH, and stable performance after 1000h dual 85 aging test. It is suitable for high-frequency, high-power scenarios such as photovoltaics and new energy, and can reduce packaging costs by more than 30%.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of power semiconductor device packaging technology, and in particular to a power device packaging structure based on TMBS, specifically a power device packaging structure based on trench-merged PIN Schottky (TMBS) diodes. This structure is particularly suitable for high-frequency, high-power applications such as photovoltaic new energy, electric vehicle charging piles, and industrial frequency converters. It can significantly improve the heat dissipation performance and electrical reliability of TMBS devices while reducing packaging costs, representing a key technological improvement in the field of power electronic packaging. Background Technology

[0002] TMBS diodes, as power devices combining the advantages of PIN diodes and Schottky barrier diodes, feature short reverse recovery time, low forward voltage drop, and strong surge resistance, making them a core freewheeling and protection device in modern power electronic systems. Especially in photovoltaic solar cell bypass protection systems, TMBS devices effectively prevent hot spot effects caused by localized shading, ensuring the long-term stable operation of photovoltaic modules. However, with the rapid development of industries such as photovoltaics and new energy vehicles, increasingly higher demands are being placed on the power density, reliability, and cost control of TMBS devices, and existing packaging technologies are gradually revealing many shortcomings that urgently need to be addressed.

[0003] First, the insufficient heat dissipation performance of existing TMBS devices has become a major bottleneck limiting their power output. Traditional TMBS packaging often uses epoxy resin as the encapsulation substrate, combined with ordinary silicone grease as the thermal interface material. This approach has extremely low thermal conductivity. The thermal conductivity of epoxy resin is only 0.2-0.5 W / (m·K), while the thermal resistance of ordinary silicone grease is typically between 0.15-0.3℃·cm² / W, resulting in the inability to quickly dissipate the heat generated by the TMBS chip during operation. Taking a commonly used 1200V / 50A TMBS device in photovoltaic systems as an example, its power consumption under rated conditions is approximately 15W. When using traditional packaging, the chip junction temperature can reach over 140℃, far exceeding the device's rated junction temperature (125℃), directly leading to a sharp increase in reverse leakage current and a reduction in lifespan of more than 30%. Meanwhile, as chip size increases (such as large-size TMBS chips of 800mm² and above), the warping problem caused by the mismatch of coefficient of thermal expansion (CTE) between the substrate, chip and heat sink becomes more prominent. Conventional thermal interface materials cannot adapt to this dynamic deformation and are prone to "pumping out effect", which leads to the generation of interface voids and further deteriorates heat dissipation performance.

[0004] Secondly, the high parasitic parameters of existing packaging structures affect the high-frequency characteristics of TMBS devices. Traditional packaging uses wire bonding to achieve electrical connection between the chip and electrodes. The connection resistance between the gold wire and the chip pad is typically between 50-100mΩ, and the parasitic inductance can reach 5-10nH. Under high-frequency conditions (such as switching power supply systems above 100kHz), these parasitic parameters can increase the switching losses of the device by 20%-40%, while also causing severe voltage overshoot and oscillation phenomena. This not only reduces system efficiency but may also cause electromagnetic interference to surrounding circuits. In addition, problems such as gold wire creep and bond point detachment in the wire bonding process also significantly reduce the mechanical reliability of the device. In vibration environments (such as electric vehicle charging piles), the failure probability of wire bonding is as high as 15% / 10000h.

[0005] Third, existing packaging solutions suffer from low functional integration, leading to high system costs and poor reliability. In photovoltaic and other applications, TMBS devices typically need to be used in conjunction with transient voltage suppressor diodes (TVS) to achieve overvoltage protection. Currently, TMBS and TVS are packaged separately and externally connected to form a protection system. This approach has several drawbacks: firstly, separate packaging increases the amount of substrate material, package housing, and wiring, increasing system costs by more than 40%; secondly, external connections introduce additional parasitic resistance and inductance, while also increasing the risk of failures such as wiring errors and poor contact. According to industry statistics, failures in photovoltaic systems caused by TMBS and TVS connection problems account for as much as 25%.

[0006] Fourth, the environmental resistance of existing encapsulations is insufficient and cannot meet the requirements of harsh operating conditions. Traditional epoxy resin encapsulations have poor resistance to high and low temperature shocks and damp heat. In high and low temperature shock cycling tests of -40℃ to 85℃, the encapsulation is prone to cracking after 500 cycles. After aging for 1000 hours in a dual 85 environment (85℃, 85% relative humidity), the insulation performance of the encapsulation will decrease by more than 50%, leading to excessive leakage current in the device. This greatly limits the application of TMBS devices in harsh environments such as high altitudes and coastal areas.

[0007] To address the aforementioned issues, the industry has made some attempts at improvement. For example, Chinese patent application CN118969733A proposes a "Diode Integrated Manufacturing Method and Integrated Diode," which achieves monolithic integration of two devices by dividing functional regions on the same epitaxial substrate and fabricating TMBS diode structures and TVS transient suppression structures separately, effectively reducing the system's integration cost and size. However, this solution only focuses on the integration design in the chip manufacturing stage and does not involve the optimization and upgrading of the packaging structure. Therefore, the core problems of poor heat dissipation performance and high parasitic parameters remain unresolved. Shenzhen Hongfucheng New Materials Co., Ltd. has developed a vertical graphene thermal pad with advantages such as low thermal resistance (≤0.04℃·cm² / W), good elasticity, and aging resistance, which can effectively solve the heat dissipation problem of large-size chips. However, the specific application structure design of this material in TMBS packaging has not been publicly reported. How to combine it with the structural characteristics of TMBS devices to achieve a synergistic improvement in heat dissipation and electrical performance is a technical problem that urgently needs to be solved.

[0008] In summary, existing TMBS-based power device packaging structures suffer from drawbacks such as poor heat dissipation, high parasitic parameters, low functional integration, and insufficient environmental resistance, severely limiting the widespread adoption of TMBS devices in high-power, high-frequency, and harsh environment applications. Therefore, developing a TMBS power device packaging structure with efficient heat dissipation, low parasitic parameters, high integration, and high reliability has significant engineering value and market potential. Utility Model Content

[0009] In view of the shortcomings of the existing technology, the purpose of this utility model is to provide a power device packaging structure based on TMBS, which solves the problems of poor heat dissipation, high parasitic parameters, low reliability and high cost of existing TMBS packaging.

[0010] The above-mentioned utility model objective is achieved through the following technical solution: This invention provides a power device packaging structure based on TMBS, including a packaging substrate, a TMBS integrated chip embedded in the packaging substrate, an electrode assembly electrically connected to the TMBS integrated chip, a heat dissipation and protection layer covering the outside of the packaging substrate, and an insulating and thermally conductive filling layer filling the gap between the packaging substrate and the TMBS integrated chip; the TMBS integrated chip includes an epitaxial substrate, on which TMBS functional regions and TVS functional regions are divided; the TMBS functional regions form TMBS trench gates and Schottky contact structures, and the TVS functional regions form PN junctions and TVS trench gates; a back metal layer is disposed on the back side of the epitaxial substrate; the electrode assembly includes a source lead, a drain lead, and a gate lead, each lead being electrically connected to the metal layer on the front side of the TMBS integrated chip through a bump soldering structure.

[0011] According to one embodiment of the present invention, the encapsulation substrate is an alumina-alumina nitride composite ceramic structure, consisting of a base layer and a surface coating; the base layer is an alumina ceramic substrate with a thickness of 1.8-2.2 mm, the surface coating is an aluminum nitride sputtered layer with a thickness of 450-550 nm, and a titanium transition layer with a thickness of 50-80 nm is provided between the base layer and the surface coating.

[0012] According to one embodiment of the present invention, the trench depth of the TMBS trench gate is 1.5-2.0 μm, the trench width is 0.8-1.2 μm, and the center-to-center distance between adjacent trenches is 3.0-3.5 μm; the trench depth of the TVS trench gate is 2.0-2.5 μm, and the trench width and adjacent spacing are consistent with those of the TMBS trench gate; the junction depth of the PN junction is 0.8-1.0 μm, and the distance between the PN junction and the TMBS trench gate is 1.5-2.0 μm.

[0013] According to one embodiment of the present invention, the bump soldering structure includes pads disposed on the metal layer of the TMBS integrated chip, bumps formed on the surface of the pads, and a soldering layer connecting the bumps and the electrode leads; the bumps are made of gold-tin alloy with a gold-tin mass ratio of 88:12, the bump diameter is 80-100μm, the height is 50-70μm, and the spacing between adjacent bumps is 200-250μm; the soldering layer is lead-free solder with a melting point of 217-225℃.

[0014] According to one embodiment of this utility model, the heat dissipation protective layer is a three-layer composite structure, consisting of a thermally conductive silicone layer, a longitudinal graphene thermally conductive film, and a polyimide protective film from the inside out; the thermally conductive silicone layer has a thickness of 0.1-0.3 mm and a thermal conductivity of 3.0-5.0 W / ; the longitudinal graphene thermally conductive film has a thickness of 0.05-0.1 mm, a thermal conductivity of 500-800 W / , and a thermal resistance ≤0.04℃·cm² / W; the polyimide protective film has a thickness of 0.03-0.05 mm and a temperature resistance range of -60℃ to 200℃.

[0015] According to one embodiment of this utility model, the insulating and thermally conductive filling layer is made by mixing boron nitride powder, alumina powder, and organosilicon resin in a mass ratio of 4:3:3; the boron nitride powder has a particle size of 5-10 μm, the alumina powder has a particle size of 1-3 μm, the filling layer has a thermal conductivity of 4.5-6.0 W / m², and a volume resistivity ≥1×10¹⁰. 6 Ω·cm, breakdown field strength ≥20kV / mm.

[0016] According to one embodiment of the present invention, the lead-out terminals of the electrode assembly are made of copper-tungsten alloy with a copper-tungsten mass ratio of 7:3. A nickel plating layer and a gold plating layer are sequentially disposed on the surface of the lead-out terminals. The thickness of the nickel plating layer is 3-5 μm, and the thickness of the gold plating layer is 0.5-1.0 μm. The cross-sections of the source lead-out terminals and the drain lead-out terminals are trapezoidal, with an upper base width of 1.5-2.0 mm and a lower base width of 2.0-2.5 mm. The cross-section of the gate lead-out terminal is rectangular, with a width of 0.8-1.0 mm.

[0017] According to one embodiment of the present invention, the TMBS integrated chip has an interlayer dielectric layer and a passivation layer on its front side. The interlayer dielectric layer is silicon dioxide with a thickness of 200-300nm; the passivation layer is silicon nitride with a thickness of 150-200nm. A contact window is provided on the passivation layer corresponding to the pad position, and the window size is 10-20μm larger than the pad.

[0018] According to one embodiment of the present invention, the four corners of the encapsulation substrate are provided with arc transition structures with an arc radius of 0.5-1.0 mm; the upper surface of the encapsulation substrate is provided with positioning grooves with a depth of 0.2-0.3 mm and a diameter of 2.0-2.5 mm for encapsulation positioning.

[0019] According to one embodiment of the present invention, the back metal layer is a titanium-nickel-silver composite layer, consisting of a titanium adhesion layer, a nickel barrier layer, and a silver conductive layer from the inside out. The titanium layer has a thickness of 50-80 nm, the nickel layer has a thickness of 100-150 nm, the silver layer has a thickness of 300-500 nm, and the sheet resistance of the back metal layer is ≤5 mΩ / sq.

[0020] In summary, compared with the prior art, the present invention has at least one of the following beneficial technical effects: 1. A qualitative leap in heat dissipation performance: The synergistic design of a vertical graphene thermally conductive film and a composite insulating filler layer reduces the overall thermal resistance of the packaging structure to below 0.04℃·cm² / W, improving heat dissipation efficiency by 60%-80% compared to traditional packaging solutions. Under rated conditions of 1200V / 50A, the chip junction temperature can be controlled below 85℃, far below the rated junction temperature, reducing reverse leakage current by more than 50% and extending lifespan by more than 2 times. Simultaneously, the porous structure of the graphene film effectively absorbs interface warpage displacement of 0.1-0.3mm, completely solving the "pumping effect" problem of large-size chips. After 1000h high-temperature aging test, the thermal resistance change rate is <5%, demonstrating stable and reliable heat dissipation performance.

[0021] 2. Significantly Reduced Parasitic Parameters: The use of a leadless bump soldering structure replaces traditional gold wire bonding, reducing package parasitic inductance from 5-10nH to below 2nH and parasitic resistance from 50-100mΩ to below 20mΩ. At 100kHz high frequencies, device switching losses are reduced by 50%-60%, and voltage overshoot is reduced by over 40%, effectively improving the system's high-frequency characteristics and efficiency. Simultaneously, the shear strength of the bump soldering is ≥20MPa, resulting in more than three times the mechanical reliability compared to gold wire bonding, and reducing the failure probability in vibration environments to below 1% / 10000h.

[0022] 3. High functional integration and significantly reduced cost: By integrating the TMBS and TVS functional areas on the same epitaxial substrate, the two devices are integrated into a single package, eliminating the need for separate packaging shells, wiring, and connection costs, thus reducing the total system cost by more than 30%. Simultaneously, it eliminates the failure risk associated with external connections, reducing the proportion of related failures in photovoltaic systems from 25% to below 5%. The integrated chip design also reduces the package size, shrinking it by 40%-50% compared to traditional discrete packaging solutions, facilitating high-density integration applications.

[0023] 4. Excellent environmental resistance: The composite ceramic structure of the encapsulation substrate and the three-layer composite heat dissipation and protection layer form a comprehensive protection system, giving the encapsulation excellent resistance to high and low temperatures, damp heat, and chemical corrosion. After high and low temperature shock cycle testing (1000 cycles) from -60℃ to 200℃, the encapsulation showed no cracking; after aging for 1000 hours in a dual 85 environment (85℃, 85% relative humidity), the insulation performance degradation rate was <5%, and the leakage current change rate was <10%, which can meet the application requirements of harsh environments such as high altitudes and coastal areas.

[0024] 5. Excellent process compatibility and easy mass production: The bump welding, vacuum potting, and sputtering coating processes used in this structure are all mature semiconductor packaging processes that can achieve automated mass production. The graphene thermal pad can be mounted using an automated chip mounter, eliminating the complex processes of gold plating and vacuum reflow soldering compared to indium wafer packaging. This reduces packaging time by more than 60% and equipment investment costs by 50%, making it suitable for large-scale industrial production. Attached Figure Description

[0025] Figure 1 This is a schematic diagram of the overall structure of this utility model.

[0026] Figure 2 This is a cross-sectional view of the heat dissipation protective layer of this utility model.

[0027] Reference numerals: 1. Encapsulation substrate; 2. TMBS integrated chip; 3. Electrode assembly; 31. Source lead; 32. Drain lead; 33. Gate lead; 4. Heat dissipation and protection layer; 41. Thermally conductive silicone layer; 42. Vertical graphene thermally conductive film; 43. Polyimide protective film; 5. Insulating and thermally conductive filling layer; 6. Positioning groove. Detailed Implementation

[0028] The technical solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.

[0029] In the description of this application, it should be noted that the terms "upper," "lower," "inner," "outer," "top / bottom," etc., indicating the orientation or positional relationship are based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0030] In the description of this application, it should be noted that, unless otherwise expressly specified and limited, the terms "installed," "equipped with," "sleeved / connected," "connected," etc., should be interpreted broadly. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium; it can be a connection within two components. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.

[0031] The core objective of this invention is to overcome the aforementioned defects in existing TMBS power device packaging structures and provide a TMBS-based power device packaging structure, specifically achieving the following objectives: significantly improving the heat dissipation performance of TMBS devices, controlling the chip junction temperature below 85℃ (under rated operating conditions), and reducing the thermal resistance to below 0.04℃·cm² / W; reducing the parasitic inductance of the packaging structure to below 2nH and the parasitic resistance to below 20mΩ, optimizing the high-frequency characteristics of the device; achieving integrated packaging of TMBS and TVS functions, reducing system costs by more than 30% and reducing the risk of connection failures; improving the environmental resistance of the package, meeting the requirements of 1000h high temperature, high and low temperature shock, and dual 85 aging tests, with a performance change rate ≤5%; simplifying the packaging process, achieving automated mass production, improving production efficiency, and reducing manufacturing costs.

[0032] To achieve the above objectives, the present invention adopts the following technical solution, with reference to... Figure 1 and Figure 2 A power device packaging structure based on TMBS is disclosed. Its core structure includes a packaging substrate 1, a TMBS integrated chip 2, an electrode assembly 3, a heat dissipation and protection layer 4, and an insulating and thermally conductive filling layer 5. The specific design of each part is as follows: Package Substrate 1 Design: Package substrate 1 adopts an alumina-alumina nitride composite ceramic structure, which combines the low cost of alumina with the high thermal conductivity of aluminum nitride. The substrate consists of a base layer and a surface coating. The base layer is an alumina ceramic substrate with a thickness controlled at 1.8-2.2 mm, a bulk density ≥3.6 g / cm³, and a bending strength ≥300 MPa, providing stable mechanical support for the chip. The surface coating is an aluminum nitride sputtered layer with a thickness of 450-550 nm. The thermal conductivity of aluminum nitride can reach 180-200 W / (m·K), which is much higher than that of pure alumina substrates, significantly improving the thermal conductivity of the substrate. To improve the adhesion between the base layer and the coating, a titanium transition layer with a thickness of 50-80 nm is set between them. The transition layer is prepared by sputtering, which can achieve a peel strength of ≥15 MPa for the coating. The four corners of the packaging substrate 1 are provided with rounded transition structures with a radius of 0.5-1.0mm to reduce stress concentration; the upper surface is provided with positioning grooves 6 with a depth of 0.2-0.3mm and a diameter of 2.0-2.5mm for precise positioning during the packaging process and to improve the packaging yield.

[0033] TMBS Integrated Chip 2 Design: TMBS integrated chip 2 is the core functional component of this structure, integrating the functions of TMBS and TVS using an epitaxial substrate. The epitaxial substrate is an N-type heavily doped silicon substrate (resistivity ≤0.005Ω·cm), on which a lightly doped N-type epitaxial layer (resistivity 5-8Ω·cm, thickness 10-12μm) is grown. The TMBS and TVS functional regions are divided on the epitaxial substrate using photolithography. The area ratio of the two functional regions is set according to application requirements, with a typical value of 7:3 (suitable for photovoltaic bypass protection scenarios).

[0034] In the TMBS functional region, trenches with a depth of 1.5-2.0 μm and a width of 0.8-1.2 μm are formed by dry etching, with a center-to-center spacing of 3.0-3.5 μm between adjacent trenches, forming the TMBS trench gate. A 50-80 nm thick silicon dioxide insulating layer is grown on the inner wall of the trench using a thermal oxidation process, achieving a breakdown field strength ≥10 MV / cm. Schottky contact structures are formed on the bottom and sides of the trenches, with the contact metal being a platinum-titanium alloy with a thickness of 100-150 nm. The Schottky barrier height is controlled at 0.6-0.7 eV to reduce the forward conduction voltage drop.

[0035] In the TVS functional region, a PN junction is first formed through an ion implantation process, with boron ions implanted as the impurity at a dose of 1×10¹. 5 -5×10¹ 5 The injection energy is 80-100 keV, and after annealing, a P-type region with a junction depth of 0.8-1.0 μm is formed. The spacing between the PN junction and the TMBS trench gate is controlled at 1.5-2.0 μm to avoid mutual interference. Subsequently, a trench gate with the same structure as the TMBS functional region is formed in the TVS functional region, with a trench depth of 2.0-2.5 μm to ensure that the TVS device has sufficient surge absorption capability.

[0036] The front side of the chip features an interlayer dielectric layer and a passivation layer. The interlayer dielectric layer, made of silicon dioxide with a thickness of 200-300 nm, is fabricated using PECVD and serves to insulate the metal layers. The passivation layer, made of silicon nitride with a thickness of 150-200 nm, exhibits excellent resistance to damp heat and chemical corrosion. Contact windows, 10-20 μm larger than the pads, are provided on the passivation layer to facilitate soldering. The back side of the chip features a fully covered back metal layer, a titanium-nickel-silver composite layer. From the inside out, it consists of a titanium adhesion layer (50-80 nm), a nickel barrier layer (100-150 nm), and a silver conductive layer (300-500 nm). The sheet resistance of the back metal layer is ≤5 mΩ / sq, ensuring good current conduction capability.

[0037] Electrode assembly 3 design: Electrode assembly 3 includes a source lead 31, a drain lead 32, and a gate lead 33, employing a leadless bump soldering design to reduce parasitic parameters. Each lead is made of copper-tungsten alloy with a copper-tungsten mass ratio of 7:3. This material combines the high conductivity of copper with the low coefficient of thermal expansion of tungsten (CTE≈7.5ppm / ℃), which matches well with the CTE (≈7-8ppm / ℃) of the ceramic packaging substrate 1, reducing soldering failures caused by thermal stress.

[0038] The lead-out surfaces are protected by a double-layer plating, consisting of a nickel plating layer and a gold plating layer. The nickel plating layer is 3-5 μm thick to prevent oxidation of the copper-tungsten alloy; the gold plating layer is 0.5-1.0 μm thick to reduce contact resistance. The source lead-out 31 and drain lead-out 32 have trapezoidal cross-sections, with an upper base width of 1.5-2.0 mm and a lower base width of 2.0-2.5 mm. This structure enhances the bonding force between the lead-out terminals and the package substrate 1. The gate lead-out 33 has a rectangular cross-section with a width of 0.8-1.0 mm to meet the requirements of low gate current transmission.

[0039] The bump soldering structure includes pads, bumps, and a solder layer. The pads are located on the metal layer on the front side of the TMBS integrated chip 2, made of aluminum-copper alloy, with a thickness of 200-300 nm and an area of ​​100 × 100 μm². The bumps are formed on the surface of the pads, made of gold-tin alloy (gold-tin mass ratio 88:12), prepared using an electroplating process. The bump diameter is 80-100 μm, the height is 50-70 μm, and the spacing between adjacent bumps is 200-250 μm. This spacing design avoids the risk of bridging between bumps. The solder layer uses lead-free solder (Sn-Ag-Cu alloy, Ag content 3.0%, Cu content 0.5%), with a melting point of 217-225℃. The connection between the bumps and the electrode leads is achieved through a reflow soldering process. The shear strength of the solder layer is ≥20 MPa, ensuring reliable connection.

[0040] The heat dissipation protection layer 4 is a three-layer composite structure covering the outside of the encapsulation substrate 1. From the inside to the outside, it consists of a thermally conductive silicone layer 41, a longitudinal graphene thermally conductive film 42, and a polyimide protective film 43, achieving the dual functions of efficient heat dissipation and environmental protection.

[0041] The inner thermally conductive silicone layer 41 has a thickness of 0.1-0.3 mm, is made of addition-type silicone, and is filled with alumina micropowder (particle size 1-3 μm). It has a thermal conductivity of 3.0-5.0 W / (m·K) and a Shore hardness of 20-30 A, exhibiting good elasticity and interfacial adhesion. It can fill microscopic depressions on the surface of the encapsulation substrate 1, reducing contact thermal resistance. The middle layer, a longitudinally continuous graphene thermally conductive film 42, is the core component for heat dissipation. It has a thickness of 0.05-0.1 mm and is composed of longitudinally continuous high thermal conductivity graphene. Through an alignment process, the graphene sheets are arranged perpendicular to the film surface. After applying an encapsulation pressure of 50-100 N, the thermal resistance can be as low as 0.04 °C·cm² / W, far superior to traditional thermal interface materials. The porous internal structure of this graphene film can quickly adapt to localized interface deformation, absorbing warpage displacement of the substrate and chip (maximum warpage of 0.3 mm), effectively preventing the "pumping effect." The outer polyimide protective film 43 has a thickness of 0.03-0.05mm and has excellent resistance to high and low temperatures, chemical corrosion and insulation properties. The temperature range is -60℃ to 200℃ and the dielectric strength is ≥15kV / mm. It can protect the internal structure from the corrosion of moisture, dust and chemical media.

[0042] Insulating and thermally conductive filling layer 5 design: The insulating and thermally conductive filling layer 5 fills the gap between the package substrate 1 and the TMBS integrated chip 2 (typical gap width is 0.2-0.5mm) to achieve thermal conduction and electrical insulation between the chip and the substrate. This filling layer is made of boron nitride powder, alumina powder and silicone resin in a mass ratio of 4:3:3. The boron nitride powder is hexagonal with a particle size of 5-10μm and has excellent thermal conductivity and insulation properties; the alumina powder is α phase with a particle size of 1-3μm, which can fill the gaps between the boron nitride powder and improve the filling density; the silicone resin is the matrix material and has good aging resistance and high and low temperature resistance.

[0043] The filler layer is prepared using a vacuum infusion process to ensure no air bubbles remain. Its thermal conductivity can reach 4.5-6.0 W / (m·K), and its volume resistivity is ≥1×10¹. 6 The dielectric strength is Ω·cm, and the breakdown field strength is ≥20kV / mm, meeting the insulation requirements of TMBS devices. Simultaneously, this filler layer exhibits good flexibility, with a linear expansion coefficient of 15-20ppm / ℃, which can alleviate thermal stress between the chip and the packaging substrate 1, preventing chip cracking.

[0044] Example 1: TMBS encapsulation structure suitable for photovoltaic bypass protection This embodiment provides a TMBS-based power device packaging structure suitable for photovoltaic bypass protection systems. Its specific parameters and fabrication process are as follows: 1. Preparation of Encapsulation Substrate 1: Alumina ceramic powder with a purity of 99.5% was mixed with 10% polyvinyl alcohol binder by mass and pressed into a substrate with a thickness of 2.0 mm under a pressure of 20 MPa. The substrate was then sintered at 1600℃ for 2 hours to obtain an alumina base layer with a bulk density of 3.7 g / cm³ and a flexural strength of 320 MPa. A titanium transition layer was deposited on the surface of the base layer using magnetron sputtering at a sputtering power of 300 W, an argon flow rate of 20 sccm, and a deposition time of 10 min, resulting in a titanium layer with a thickness of 60 nm. Subsequently, an aluminum nitride coating was sputtered onto the titanium transition layer at a sputtering power of 500 W, a nitrogen flow rate of 15 sccm, an argon flow rate of 25 sccm, and a deposition time of 30 min, resulting in an aluminum nitride coating with a thickness of 500 nm. The ceramic substrate was cut to a size of 10×12mm using a diamond tool, and the four corners were sanded to a radius of 0.8mm. Finally, a positioning groove 6 with a depth of 0.25mm and a diameter of 2.2mm was formed on the upper surface by laser etching.

[0045] 2. Fabrication of TMBS Integrated Chip 2: A 4-inch diameter, 500μm thick N-type heavily doped silicon substrate (resistivity 0.003Ω·cm) was selected. An 11μm thick N-type lightly doped epitaxial layer (resistivity 6.5Ω·cm) was grown on its surface using vapor phase epitaxy. TMBS functional regions (7mm × 10mm) and TVS functional regions (3mm × 10mm) were then defined on the substrate using photolithography to form a photoresist mask.

[0046] In the TMBS functional region, dry etching was performed using an SF6 / O2 mixed gas (volume ratio 4:1) to an etching depth of 1.8 μm, a width of 1.0 μm, and a center-to-center spacing of 3.2 μm between adjacent trenches, forming the TMBS trench gate. Subsequently, thermal oxidation was performed at 1050 °C to grow a 65 nm thick silicon dioxide insulating layer. A platinum-titanium alloy (mass ratio 9:1) with a thickness of 120 nm was deposited using electron beam evaporation to form a Schottky contact structure. After annealing (450 °C, 30 min), the Schottky barrier height was 0.65 eV.

[0047] In the TVS functional area, boron ion implantation (dose 3×10¹) was used. 5 (cm⁻², energy 90keV), and then annealed at 1100℃ for 30 min to form a P-type region with a junction depth of 0.9μm. The spacing between the P-type region and the TMBS trench gate is 1.8μm. Subsequently, a TVS trench gate with a depth of 2.2μm is formed using the same etching process as the TMBS functional region.

[0048] A 250 nm thick silicon dioxide interlayer dielectric layer was deposited on the front side of the chip using PECVD, followed by a 180 nm thick silicon nitride passivation layer. Contact windows (110 × 110 μm²) were then formed on the passivation layer using photolithography and etching. On the back side of the chip, a titanium layer (60 nm), a nickel layer (120 nm), and a silver layer (400 nm) were sequentially deposited using electron beam evaporation to form the back metal layer, which has a sheet resistance of 3.5 mΩ / sq.

[0049] 3. Electrode assembly 3 fabrication and connection: Electrode leads were fabricated using a copper-tungsten alloy (Cu70W30). The source and drain leads 32 have trapezoidal cross-sections (top base 1.8mm, bottom base 2.2mm, length 10mm), while the gate lead 33 has a rectangular cross-section (width 0.9mm, length 10mm). A nickel layer (4μm) and a gold layer (0.8μm) were sequentially deposited on the lead surfaces using an electroplating process.

[0050] Gold-tin alloy bumps (Au88Sn12) were prepared on the chip pads using an electroplating process. The bumps had a diameter of 90 μm, a height of 60 μm, and a spacing of 220 μm between adjacent bumps. After aligning the electrode leads with the bumps, reflow soldering was performed using lead-free solder (Sn3.0Ag0.5Cu) at a temperature of 230℃ for 10 seconds to form a solder layer with a shear strength of 22 MPa.

[0051] 4. Insulating and thermally conductive filling layer 5 infusion: Boron nitride powder (particle size 5-10μm), alumina powder (particle size 1-3μm), and silicone resin are mixed in a mass ratio of 4:3:3. After stirring evenly, vacuum degassing is performed (vacuum degree -0.095MPa, time 30min) to obtain the filling slurry. The TMBS integrated chip 2 is fixed in the positioning groove 6 of the packaging substrate 1. The filling slurry is injected into the gap between the chip and the substrate using a vacuum infusion process at an infusion pressure of 0.1MPa. Then, it is cured at 120℃ for 2 hours to form the insulating and thermally conductive filling layer 5, which has a thermal conductivity of 5.2W / (m·K) and a volume resistivity of 5×10¹. 6 Ω·cm.

[0052] 5. Heat dissipation and protective layer 4 coating: A 0.2 mm thick thermally conductive silicone layer 41 (thermal conductivity 4.0 W / (m·K)) is uniformly coated on the outside of the encapsulation substrate 1. Then, a 0.08 mm thick longitudinal graphene thermally conductive film 42 is bonded to the surface of the silicone layer using an automated pick-and-place machine, applying a pressure of 80 N to ensure tight adhesion. The thermal resistance of the graphene film is 0.04 °C·cm² / W. Finally, a 0.04 mm thick polyimide protective film 43 is coated on the outside of the graphene film and fixed using a hot-pressing process (temperature 150 °C, pressure 0.5 MPa).

[0053] 6. Performance Test Results: The performance of the TMBS power device package structure prepared in this embodiment was tested, and the results are as follows: Heat dissipation performance: Under 1200V / 50A conditions, the chip junction temperature is 82℃ and the thermal resistance is 0.038℃·cm² / W; after 1000h of high temperature (125℃) aging, the thermal resistance change rate is 3.2%.

[0054] Electrical performance: parasitic inductance is 1.8nH, parasitic resistance is 18mΩ; forward voltage drop is 0.45V (25℃, 50A), and reverse leakage current is 0.5μA (1200V, 25℃).

[0055] Reliability: After 1000 high and low temperature shocks (-60℃-200℃), the package showed no cracking and the electrical performance change rate was <5%; after 1000 hours of dual 85 aging, the leakage current was 0.55μA and the change rate was <10%.

[0056] Cost: Compared to traditional TMBS+TVS discrete packaging, the cost per device is reduced by 35%, and the package size is reduced by 45%.

[0057] Example 2: TMBS Packaging Structure for Electric Vehicle Charging Stations This embodiment provides a high-power TMBS packaging structure suitable for electric vehicle charging piles. Its main differences from Embodiment 1 are a larger chip size and a strengthened heat dissipation structure. Specific parameters are as follows: The packaging substrate 1 has a size of 15×18mm, an aluminum oxide base layer thickness of 2.2mm, and an aluminum nitride coating thickness of 550nm; the TMBS integrated chip 2 has a size of 12×15mm, an epitaxial layer thickness of 12μm, a TMBS trench gate depth of 2.0μm, and a TVS trench gate depth of 2.5μm; the bump diameter is 100μm, the height is 70μm, and the adjacent spacing is 250μm; the heat dissipation protection layer 4 has a graphene thermally conductive film thickness of 0.1mm and a thermally conductive silicone layer 41 thickness of 0.3mm; the proportion of boron nitride powder in the insulating and thermally conductive filling layer 5 is increased to 50%, and the thermal conductivity can reach 6.0W / (m·K).

[0058] Performance test results: Under 1200V / 100A conditions, the chip junction temperature is 88℃, the thermal resistance is 0.04℃·cm² / W; the parasitic inductance is 2.0nH, and the parasitic resistance is 20mΩ; after 1000 high and low temperature shocks, the electrical performance change rate is <8%; after 1000 hours of dual 85 aging, the leakage current change rate is <12%, meeting the high power and high reliability requirements of electric vehicle charging piles.

[0059] Example 3: Comparative Experiment To verify the superiority of this invention, a comparison group (traditional TMBS packaging structure) was set up to compare its performance with that of Embodiment 1 of this invention. The comparison results are shown in the table below:

[0060] As shown in the table above, the packaging structure of this utility model is significantly superior to the traditional packaging structure in terms of thermal resistance, parasitic parameters, service life, cost and reliability, and has obvious technical advantages.

[0061] The implementation principle of this utility model is as follows: This utility model discloses a power device packaging structure based on TMBS, belonging to the field of power device packaging technology, aiming to solve the problems of poor heat dissipation, high parasitic parameters, low reliability, and high cost of existing TMBS packaging. It includes a packaging substrate 1, a TMBS integrated chip 2, an electrode assembly 3, a heat dissipation protective layer 4, and an insulating and thermally conductive filling layer 5. The TMBS integrated chip 2 includes an epitaxial substrate, on which TMBS and TVS regions are divided and corresponding structures are formed to achieve functional integration. The electrode assembly 3 adopts a leadless bonding design and is connected to the chip through bump welding. The heat dissipation protective layer 4 is composed of thermally conductive silicone, a longitudinal graphene thermally conductive film 42, and a polyimide protective film 43. The insulating and thermally conductive filling layer 5 fills the packaging gap. This structure has a thermal resistance as low as 0.04℃·cm² / W, a parasitic inductance ≤2nH, and stable performance after 1000h of double 85 aging test. It is suitable for high-frequency, high-power scenarios such as photovoltaics and new energy, and can reduce packaging costs by more than 30%.

[0062] The embodiments described herein are preferred embodiments of this utility model and are not intended to limit the scope of protection of this utility model. Therefore, all equivalent changes made to the structure, shape, and principle of this utility model should be included within the scope of protection of this utility model.

Claims

1. A power device packaging structure based on TMBS, characterized in that, The package includes a packaging substrate (1), a TMBS integrated chip (2) embedded inside the packaging substrate (1), an electrode assembly (3) electrically connected to the TMBS integrated chip (2), a heat dissipation protective layer (4) covering the outside of the packaging substrate (1), and an insulating and thermally conductive filling layer (5) filling the gap between the packaging substrate (1) and the TMBS integrated chip (2); the TMBS integrated chip (2) includes an epitaxial substrate, on which TMBS functional regions and TVS functional regions are divided, the TMBS functional regions are formed with TMBS trench gates and Schottky contact structures, the TVS functional regions are formed with PN junctions and TVS trench gates, and a back metal layer is provided on the back side of the epitaxial substrate; the electrode assembly (3) includes a source lead-out terminal (31), a drain lead-out terminal (32) and a gate lead-out terminal (33), and each lead-out terminal is electrically connected to the metal layer on the front side of the TMBS integrated chip (2) through a bump soldering structure.

2. The power device packaging structure based on TMBS according to claim 1, characterized in that, The encapsulation substrate (1) is an alumina-alumina nitride composite ceramic structure, consisting of a base layer and a surface coating; the base layer is an alumina ceramic substrate, the surface coating is an aluminum nitride sputtered layer, and a titanium transition layer is provided between the base layer and the surface coating.

3. The power device packaging structure based on TMBS according to claim 1, characterized in that, The TMBS trench gate has a trench depth of 1.5-2.0 μm, a trench width of 0.8-1.2 μm, and a center-to-center distance between adjacent trenches of 3.0-3.5 μm; the TVS trench gate has a trench depth of 2.0-2.5 μm, and its trench width and adjacent spacing are the same as those of the TMBS trench gate; the PN junction has a junction depth of 0.8-1.0 μm and a distance of 1.5-2.0 μm from the TMBS trench gate.

4. The power device packaging structure based on TMBS according to claim 1, characterized in that, The heat dissipation protective layer (4) is a three-layer composite structure, consisting of a thermally conductive silicone layer (41), a longitudinal graphene thermally conductive film (42), and a polyimide protective film (43) from the inside out.

5. The power device packaging structure based on TMBS according to claim 1, characterized in that, The TMBS integrated chip (2) has an interlayer dielectric layer and a passivation layer on its front side. The interlayer dielectric layer is silicon dioxide, and the passivation layer is silicon nitride. A contact window is provided on the passivation layer corresponding to the pad position.

6. The power device packaging structure based on TMBS according to claim 1, characterized in that, The four corners of the encapsulation substrate (1) are provided with arc transition structures; the upper surface of the encapsulation substrate (1) is provided with positioning grooves (6) for encapsulation positioning.

7. The power device packaging structure based on TMBS according to claim 1, characterized in that, The back metal layer is a titanium-nickel-silver composite layer, consisting of a titanium adhesion layer, a nickel barrier layer, and a silver conductive layer from the inside out.

Citation Information

Patent Citations

  • Diode integrated manufacturing method and integrated diode

    CN118969733A