Vertical tunnel field-effect transistor cell and its fabrication
The vertical TFET design with optimized contact formation and high-K/metal gate stacks addresses scaling challenges in TFETs, reducing contact resistance and energy consumption for improved performance.
Patent Information
- Application Number
- DE102013105449
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2013-01-24
- Filing Date
- 2013-05-28
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2033-05-28
AI Technical Summary
Existing tunnel field effect transistors (TFETs) face challenges in further scaling due to increased leakage currents and energy consumption, despite their potential for reducing power supply voltage.
A vertical tunnel field effect transistor (TFET) design with a frustoconical protrusion structure, a gate stack wrapped around the protrusion, and optimized contact formation to reduce contact resistance and device area, utilizing materials like high-K/metal gate stacks and selective etching processes.
The design achieves reduced contact resistance and device area, enhancing the scalability and energy efficiency of TFETs while maintaining low off-state leakage currents.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
background
[0001] The semiconductor integrated circuit industry has experienced rapid growth in recent decades. Technological advances in semiconductor materials and design have led to increasingly smaller and more complex circuits. These material and design advances have been made possible by advances in processing and manufacturing technologies. As semiconductors have evolved, the number of interconnected components per unit area has increased as the size of the smallest component that can be reliably manufactured has decreased.
[0002] However, with the shrinking size of the smallest components, numerous challenges have arisen. As structures are placed closer together, leakage current becomes more noticeable, signals can overlap more easily, and power consumption has become a significant concern. The semiconductor integrated circuit industry has produced numerous developments to continue the scaling process. One of these developments is the potential replacement or supplementation of the conventional MOS field-effect transistor with the tunneling field-effect transistor (TFET).
[0003] TFETs are promising devices that enable further scaling of power supply voltage without significantly increasing off-state leakage currents, which is due to their oscillation below a 60 mV / dec subthreshold. However, existing TFETs are not satisfactory in all respects.
[0004] US 2011 / 0253981A1 describes a vertical tunneling field effect transistor cell comprising: a substrate; a frustoconical protrusion structure having a first width disposed above the substrate and protruding from the plane of the substrate; a drain region having a second width disposed above the substrate adjacent the protrusion structure and extending to a lower portion of the protrusion structure as a raised drain region; a gate stack having a third width disposed over the substrate, the gate stack having a planar portion parallel to the surface of the substrate and a gating surface wrapped around a central portion of the protrusion structure; a source region at an upper portion of the protrusion structure, the source region overlapping an upper portion of the gating surface of the gate stack; a dielectric insulation layer disposed over the source region, the gate stack, and between the planar portion of the gate stack and the drain region; and a gate contact formed on the planar portion of the gate stack and extending to a portion of the dielectric insulation layer.
[0005] Similar TFETs are also known from US 2007 / 0228491 A1 and US 2010 / 0163845 A1. Short description of the drawings Fig. 1 shows a flowchart of an exemplary method for manufacturing a semiconductor device constructed in accordance with various aspects of the present disclosure. Fig. 2 to 11 show cross-sectional views of an exemplary semiconductor device in stages of manufacture, which according to the method of Fig. 1 were constructed. Detailed description
[0006] It should be understood that the following disclosure provides many different embodiments or examples for implementing different structures of the disclosure. Specific examples of components and arrangements are described below to simplify the present disclosure. Moreover, in the following description, the performance of a first process before a second process may include embodiments in which the second process is performed immediately after the first process, and may also include embodiments in which additional processes are performed between the first and second processes. Numerous structures may be arbitrarily drawn at different scales for simplicity and clarity.Furthermore, in the following description, forming a first structure over or on a second structure may include embodiments in which the first and second structures are formed in direct contact with each other, and may also include embodiments in which additional structures may be formed between the first and second structures such that the first and second structures need not be in direct contact with each other.
[0007] Fig. 1 shows a flowchart of one embodiment of a method 100 for fabricating one or more TFET devices according to aspects of the present disclosure. The method 100 is discussed in detail below with reference to a TFET device 200 shown in Fig. 2 to 11 is shown as an example.
[0008] With reference to Fig. 1 and Fig. 2, the method 100 begins at step 102 by providing a substrate 210. The substrate 210 includes silicon. In alternative embodiments, the substrate 210 may include germanium, silicon germanium, gallium arsenide, silicon carbide, indium arsenide, indium phosphide, gallium arsenophosphide, gallium indium, or other suitable semiconductor materials. Alternatively, and in some embodiments, the substrate 210 may include an epitaxial layer. For example, the substrate 210 may include an epitaxial layer overlying a bulk semiconductor. Further, the substrate 210 may be strained to enhance performance.For example, the epitaxial layer may include a semiconductor material different from that of the bulk semiconductor, such as a layer of silicon germanium overlying bulk silicon or a layer of silicon overlying bulk silicon germanium formed by a process including selective epitaxial growth (SEG). Furthermore, the substrate 210 may include a semiconductor-on-insulator (SOI) structure, such as a buried dielectric layer. Alternatively, the substrate 210 may include a buried dielectric layer, such as a buried oxide (BOX) layer, such as that formed by a process known as separation by implantation of oxygen (SIMOX) technology, wafer bonding, SEG, or other suitable processes.Indeed, numerous embodiments may include any of a variety of substrate structures and materials. Substrate 210 may also include various p-type doped regions and / or n-type doped regions implemented by a process such as ion implantation and / or diffusion. These doped regions include n-well and p-well.
[0009] The method 100 continues at step 104 by etching the substrate 210 to form a frustoconical protrusion structure 220 having a first height h1 protruding from the plane of the substrate 210. The frustoconical structure 220 is referred to as a core structure 220. The core structure 220 may be formed by lithography and etching processes. In one embodiment, a hard mask layer 215 is first deposited on the substrate 210. The hard mask 215 includes silicon oxide, silicon nitride, silicon oxynitride, or any other suitable dielectric material. The hard mask 215 may be patterned by lithography and etching processes to define the core structure 220 having a first width w1. The substrate 210 is etched using the patterned hard mask 215 as an etch mask to form the core structure 220. The etching process may include wet etching, dry etching, or a combination thereof.The core structure 220 may be formed with sidewalls having an angle α with the planar surface of the substrate 210 ranging from approximately 45 degrees to about 90 degrees.
[0010] In one embodiment, the core structure 220 is formed as a cylindrical shape. Alternatively, the core structure 220 is formed as a square column, an oval cylinder, a rectangular column, a hexagonal column, or another polygonal column shape.
[0011] With reference to Fig. 1 and Fig. 3, the method 100 continues at step 106 by forming isolation structures 230 on the substrate 210, including between each core structure 220. The isolation structures 230 may comprise similar or different structures formed using different processing technologies. In one embodiment, the isolation structures 230 are shallow trench isolation (STI) structures. Forming an STI may include etching a trench in the substrate 210 and filling the trench with insulator materials, such as silicon oxide, silicon nitride, or silicon oxynitride. The filled trench may comprise a multi-layer structure, such as a liner layer of thermal oxide, with silicon nitride filling the trench.
[0012] With reference to Fig. 1 and Fig. 4, the method 100 continues at step 108 by forming a drain region 310 having a second width w2 on the substrate 210. The second width w2 is substantially greater than the first width w1. In one embodiment, the drain region 310 is concentric with the core structure 220 and isolated from it by the isolation structure 230. The drain region 310 is doped by doping a predetermined upper portion of the substrate 210 by a suitable technique, such as implantation with a patterned photoresist as an implantation mask. In the present embodiment, the drain region 310 is located adjacent to the core structure 220 and between the isolation structures 230. For a p-type TFET, the drain region 310 may be doped with p-type dopants, such as boron or BF2.For an n-type TFET, the drain region may be doped with n-type dopants, such as phosphorus, arsenic, or combinations thereof. After implantation, one or more annealing processes may be performed for dopant activation. The annealing processes may include rapid thermal annealing (RTA), laser annealing, or another suitable annealing process. As an example, high-temperature annealing includes a "spike" annealing process that has a very short duration. During formation, the dopant is diffused down to a lower portion of the core structure 220 having a second height h2, referred to as the raised drain region 310.
[0013] With reference to Fig. 1 and Fig. 5, the method 100 continues at step 110 by forming a first dielectric insulation layer 410 over the drain region 310 through deposition and recession processes. The first dielectric insulation layer 410 includes silicon oxide, silicon nitride, silicon carbide, oxynitride, or other suitable materials. The first dielectric insulation layer 410 may include a single layer or multiple layers. The first dielectric insulation layer 410 is deposited by a suitable technique, such as chemical vapor deposition (CVD), atomic layer deposition (ALD), physical vapor deposition (PVD), thermal oxidation, or combinations thereof. In the present embodiment, the dielectric insulation layer 410 is etched back to a third height h3 that is substantially smaller than the second height h2 of the raised drain region 310.The first dielectric insulation layer 410 may be recessed or recessed by a selective dry etch, a selective wet etch, or a combination thereof.
[0014] With reference to Fig. 1 and Fig. 6, the method 100 continues at step 112 by forming a gate stack 510. The gate stack 510 includes a planar portion 512 parallel to the surface of the substrate 210 and over the first dielectric insulation layer 410, and a gating surface wrapped around a central portion of the core structure 220. The planar portion may be asymmetric with respect to the core structure 220. An overall width of the gate stack 510, a third width w3, is substantially greater than the first width w1 of the core structure 220 and less than the second width w2 of the drain region 310. In one embodiment, the out-of-plane gating surface of the gate stack 510 overlaps a portion of the raised drain region 310.
[0015] The gate stack 510 is formed by any suitable process or processes. For example, the gate stack 510 is formed by a method including deposition, photolithography patterning, and etching processes. The deposition processes include CVD, PVD, ALD, metal-organic CVD (MOCVD), other suitable processes, and / or combinations thereof. The photolithography patterning processes include photoresist coating (e.g., spin-on coating), soft baking, mask alignment, exposure, post-exposure baking, photoresist development, washout, drying (e.g., hard baking), other suitable processes, and / or combinations thereof. The etching process includes a dry etch, a wet etch, or a combination of dry etching and wet etching.The dry etching process may implement fluorine-containing gas (e.g., CF4, SF6, CH2F2, CHF3, and / or C2F6), chlorine-containing gas (e.g., Cl2, CHCl3, CCl4, and / or BCl3), bromine-containing gas (e.g., HBr and / or CHBR3), iodine-containing gas, or other suitable gases and / or plasmas and / or combinations thereof. The etching process may include multi-step etching to achieve etch selectivity, flexibility, and the desired etch profile.
[0016] In one embodiment, the gate stack 510 is a high-k (HK) / metal gate (MG). The HK / MG includes a gate dielectric layer 520 and an MG 530. The gate dielectric layer 520 may include an interfacial layer (IL) and a high-k dielectric layer (HK). The IL includes oxide, HfSiO, and oxynitride. The HK dielectric layer may include LaO, AlO, ZrO, TiO, Ta2O5, Y2O3, SrTiO3 (STO), BaTiO3 (BTO), BaZrO, HfZrO, HfLaO, HfSiO, LaSiO, AlSiO, HfTaO, HfTiO, (Ba,Sr)TiO3 (BST), Al2O3, Si3N4, oxynitride (SiON), or other suitable materials. The MG 530 can contain a single layer or multiple layers, such as a metal layer, a liner layer, a wetting layer, and an adhesion layer. The MG 530 can contain Ti, Ag, Al, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, TaN, Ru, Mo, Al, WN, Cu, W, or any suitable materials.
[0017] In another embodiment, gate stack 510 is a polysilicon gate stack. The polysilicon gate stack may include a gate dielectric layer and a polysilicon layer deposited over the gate dielectric layer. The gate dielectric layer may include silicon oxide, silicon nitride, or any other suitable materials.
[0018] With reference to Fig. 1 and Fig. 7, the method 100 continues at step 114 by forming a second dielectric insulation layer 610 over the first dielectric insulation layer 410, including over the planar portion of the gate stack. The second dielectric insulation layer 610 is similar in many respects to the second dielectric insulation layer 610 described above in connection with the first dielectric insulation layer 410 in Fig. 5. The second dielectric insulation layer 610 is etched back to expose a predetermined height of a top portion of the gating surface of the gate stack 510. In one embodiment, the predetermined height is substantially greater than a thickness of the hard mask layer 215.
[0019] With reference to Fig. 1 and Fig. 8, the method 100 continues at step 116 by removing an upper portion of the gating surface of the gate stack 510 to expose an upper portion of the core structure 220 having a fourth height h4. The upper portion of the gating surface of the gate stack 510 may be removed by a selective dry etch, a selective wet etch, a combination thereof, or other suitable processes. The hard mask layer 215 is also removed in the same etch process or in a separate etch process. In one embodiment, the gating surface of the gate stack 510 above the second dielectric isolation layer 610 is removed.
[0020] With reference to Fig. 1 and Fig. 9, the method 100 continues at step 118 by forming a source region 710 in the upper portion of the core structure 220. In one embodiment, the source region 710 is formed by photolithography patterning and implantation, which is similar in many respects to the steps described above in connection with the drain region 310 in Fig. 4. The source region 710 has a different doping type than the drain region 310. In another embodiment, the core structure 220 is first recessed, and then the source region 710 is formed as the upper portion of the recessed core structure 220 by photolithography patterning and implantation. In yet another embodiment, a semiconductor material is epitaxially grown on the recessed core structure 220. The semiconductor material layer includes elemental semiconductor material, such as germanium (Ge) or silicon (Si); or compound semiconductor materials, such as gallium arsenide (GaAs), aluminum gallium arsenide (AlGaAs); or semiconductor alloy, such as silicon germanium (SiGe), gallium arsenide phosphide (GaAsP).These epitaxial processes include CVD deposition techniques (e.g., vapor-phase epitaxy (VPE) and / or ultra-high vacuum CVD (UHV-CVD), molecular beam epitaxy, and / or other suitable processes. The S / D structures may be formed by one or more epitaxial or epitaxial (epi) processes. The source region 710 may be doped in-situ during the epitaxial process. In one embodiment, the source region 710 is not doped in-situ; an implantation process (i.e., a junction implantation process) is performed to dope the source region 710.
[0021] With reference to Fig. 1 and Fig. 10, the method 100 continues at step 120 by depositing a third dielectric insulation layer 810 over the second dielectric insulation layer 610, including over the source region 710. The third dielectric insulation layer 810 is similar in many respects to the steps described above in connection with the first dielectric insulation layer 410 in Fig. 3. In addition, a CMP process is performed to planarize the top surface of the third dielectric insulation layer 810.
[0022] With reference to Fig. 1 and Fig.11, the method 100 continues at step 122 by forming a source contact 910, a gate contact 920, and a drain contact 930. The contacts 910, 920, and 930 may be formed by lithography patterning processes and etching processes. The photolithography patterning processes include photoresist coating (e.g., spin-on coating), soft baking, mask alignment, exposure, post-exposure baking, photoresist development, washout, drying (e.g., hard baking), other suitable processes, and / or combinations thereof. The etching process includes a dry etch, a wet etch, or a combination of dry etching and wet etching.The dry etching process may implement fluorine-containing gas (e.g., CF4, SF6, CH2F2, CHF3, and / or C2F6), chlorine-containing gas (e.g., Cl2, CHCl3, CCl4, and / or BCl3), bromine-containing gas (e.g., HBr and / or CHBR3), iodine-containing gas, other suitable gases and / or plasmas, and / or combinations thereof. The etching process may include multi-step etching to achieve etch selectivity, flexibility, and the desired etch profile.
[0023] In the present embodiment, the contact etch is configured to have appropriate selectivity with respect to the source region 710, the gate stack 510, and the drain region 310. In one embodiment, the gate contact 920 is formed on the planar portion of the gate stack 510. Alternatively, the gate contact 920 is formed on the planar portion of the gate stack 510 and overlies at least a portion (925) of the second dielectric insulation layer 610 or a portion of both the first and second dielectric insulation layers 610 and 410. The drain contact 930 is formed on the drain region 310 and overlies at least a portion (935) of the isolation structure 230 by removing the portion 935 of the isolation structure 230 in the contact etch.In the drain contact 930, a portion of the drain region 310 is exposed within the isolation structure 230, which increases the drain contact interface and may lead to a reduction in contact resistance. By jointly forming the gate contact 920 in the planar region of the gate stack 510 and the portion 925 of the dielectric isolation layer, and the drain contact 930 in the drain region 310 and the portion 935 of the isolation structure 230, a required active area of the device 200 may be reduced and a limitation of the contact lithography process may be relaxed.
[0024] The TFET device 200 may undergo further processing using CMOS or MOS technology to form various structures and regions known in the art. For example, subsequent processing may form numerous vias / lines and multilayer interconnect structures (e.g., metal layers and interlayer dielectrics) on the substrate 210 configured to interconnect the various features or structures of the TFET device 200. For example, a multilayer interconnect includes vertical interconnects, as is conventional, and horizontal interconnects, such as metal lines. The numerous interconnect structures may implement numerous conductive materials, including copper, tungsten, and / or silicon.
[0025] Additional steps may be provided before, during, and after the method 100, and some of the described steps may be substituted, omitted, or shifted for further embodiments of the method 100.
[0026] Based on the above, the present disclosure provides a TFET device employing a gate contact layer on the dielectric insulation layer and a drain contact layer on the insulation structure, as well as a manufacturing method. By overlaying the insulation structure, the drain contact resistance is reduced by increasing the contact interface, the required area of a device is reduced by saving gate and drain contact area, and contact lithography process constraints are relaxed. The method is feasible with existing TFET manufacturing.
[0027] The invention is defined by the main claim and the subordinate claim. Further embodiments of the invention are recited in the dependent claims.
Claims
[1] Vertical tunneling field effect transistor cell (200), comprising: a substrate (210); a protrusion structure (220) having a first width (w1) disposed above the substrate (210) and protruding from the plane of the substrate (210); a drain region (310) having a second width (w2) disposed above the substrate (210) adjacent to the protrusion structure (220) and extending to a lower portion of the protrusion structure (220) as a raised drain region; a gate stack (510) having a third width (w3) disposed over the substrate (210), the gate stack (510) having a planar portion (512) parallel to the surface of the substrate (210) and a gating surface wrapped around a central portion of the protrusion structure; a source region (710) at an upper portion of the protrusion structure (220), the source region (710) overlapping an upper portion of the gating surface of the gate stack (510); a dielectric insulation layer (810) disposed over the source region (710), the gate stack (510), and between the planar portion (512) of the gate stack (510) and the drain region (310); and a gate contact (920) formed on the planar portion (512) of the gate stack (510) and extending to a portion of the dielectric insulation layer (810); wherein the vertical tunnel field-effect transistor cell further comprises an insulation structure (230) between the drain region (310) and another drain region and a drain contact (930), wherein the drain contact (930) is formed on the drain region (310) through the dielectric insulation layer (810) and extends to a portion of the insulation structure (230), wherein a portion of the drain region (310) in the insulation structure (230) is exposed in the drain contact (930), and the drain contact (930) lies at least over the portion (935) of the insulation structure (230), wherein the gating surface of the gate stack (510) overlaps with the raised drain region (310). [2] Vertical tunnel field effect transistor cell (200) according to claim 1, characterized by that the drain region (310) has a different doping type than the source region (710). [3] Vertical tunnel field effect transistor cell (200) according to one of the preceding claims, characterized by that the side wall of the projection structure (220) forms an angle with the planar surface of the substrate (210) ranging from about 45 degrees to about 90 degrees. [4] Vertical tunnel field effect transistor cell (200) according to one of the preceding claims, characterized by that the second width (w2) is substantially larger than the third width (w3), which is substantially larger than the first width (w1). [5] Vertical tunnel field effect transistor cell (200) according to one of the preceding claims, characterized by that the central portion of the projection structure (220) is made of the same material as the substrate (210). [6] Vertical tunnel field effect transistor cell (200) according to one of the preceding claims, characterized bythat the projection structure has a cylinder structure, a square column structure, an oval cylinder column structure or hexagonal column structure. [7] Vertical tunnel field effect transistor cell (200) according to one of the preceding claims, characterized by that the gate stack (510) has a high-K / metal gate or a polysilicon gate. [8] Vertical tunnel field effect transistor cell (200) according to one of the preceding claims, characterized by that the source region (710) has a different polygon shape than the central portion of the projection structure (220). [9] Vertical tunnel field effect transistor cell (200) according to one of the preceding claims, further comprising: a source contact (910) arranged on the source region (710). [10] A method of manufacturing a vertical tunneling field effect transistor cell, the method comprising: Providing a substrate (210); Etching the substrate (210) to form a protrusion on a surface of the substrate (210); Forming insulation structures on the substrate; Doping a portion of the substrate (210) adjacent the protrusion to form a drain region (310) between the isolation structures (230), including extending to a lower portion of the protrusion to form a raised drain region (310); Forming a first dielectric insulation layer (410) over the drain region (310); Forming a gate stack (510) having a planar portion (512) above the drain region (310) that is parallel to the surface of the substrate (210) and a gating surface wrapped around a central portion of the protrusion, including overlapping with the raised drain region; Forming a second dielectric insulation layer (610) over the planar portion (512) of the gate stack (510) and the drain region (310); recessing a portion of the gating surface of the gate stack (510) to expose an upper portion of the protrusion; Forming a source region (710) on the upper portion of the protrusion with a different doping type than that of the drain region (310), including overlapping with the gating surface of the gate stack (510); Forming a third dielectric insulation layer (810) over the source region (710), the gate stack (510) and the second dielectric insulation layer (610); jointly forming a drain contact (930) on the drain region (310) and a portion of the insulation structure (230), and removing the portion (935) of the insulation structure (230) to expose a portion of the drain region (310) in the drain contact (930); and simultaneously with the formation of the drain contact (930), forming a gate contact (920) on the planar portion of the gate stack (510) and extending to a portion of the dielectric insulation layer (410,610, 810), and a source contact (910) on the source region (710).
Citation Information
Patent Citations
Tunneling transistor with sublithographic channel
US20070228491A1
Tunnel field effect transistor and method of manufacturing same
US20100163845A1
Method of manufacturing a vertical tfet
US20110253981A1