Grain boundary diffusion process for rare earth magnets
Patent Information
- Application Number
- DE102014219893
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2013-10-09
- Filing Date
- 2014-10-01
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2034-10-01
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
One or more embodiments relate to a method of forming a reduced heavy rare earth element magnet and a magnet manufactured according to this method.Permanent magnet motors may have high efficiency, potentially being suitable for use in traction motors for hybrid and electric vehicles. In this type of motor, the design and selection of the permanent magnet is important. Rare earth permanent magnets such as neodymium magnets (Nd) are often used in traction motors in electric vehicles due to their high flux density and high anti-demagnetization capability compared to traditional non-rare earth magnets such as alnico (iron alloys containing aluminum, nickel, and cobalt) and ferrite. However, rare earth permanent magnets may contain a large amount of rare earth elements (e.g., at least 30 wt %) in some commercial magnets, making the magnets expensive. In addition, in order to ensure the high-temperature operation of the permanent magnet in the transmission environment of vehicles, about 10 wt % of heavy rare earth elements (HRE) such as dysprosium (Dy) and terbium (Tb) may need to be added to the neodymium magnetic alloys. This makes the magnets even more expensive because the price of Dy and Tb may be about ten times higher than that of neodymium.JP 2001-68 317 A discloses a sintered magnet comprising Nd-Fe-B and a method for producing the same.US 2011 / 0012460 A2 discloses a permanent magnet for a motor and a method for producing such a magnet.US 2013 / 0049909 A1 discloses a magnet with a high resistance and a method for producing such a magnet.DE 11 2011 100 574 T5 discloses a composite magnet comprising rare earth metals with increased electrical resistance.DE 11 2008 000 992 T5 discloses a sintered magnet with light and heavy rare earth metals.In at least one embodiment, a method of forming a magnet is provided, comprising the steps of:alternate lamination in a magnetic powder mold or tool with a rare earth element and heavy rare earth-containing material to form a laminated structure of a plurality of magnetic powder layers and a plurality of heavy rare earth layers;pressing the layered assembly into a green compact;Subsequent sintering to form the solid unitary magnet; wherein the heavy rare earth layers intersect.In at least one embodiment, a magnet made by the method is provided, comprising: a single sintered magnet having a heavy rare earth element (HRE) concentration profile within a continuously sintered rare earth magnet (RE) volume. The concentration profile may include at least one local maximum of HRE element concentration that is between local minima of the HRE element concentration within the volume, such that a corresponding coercivity profile of the magnet includes at least one local maximum that is between local minima within the volume.In another embodiment, the concentration profile of HRE elements contains multiple local maxima with HRE element concentrations within the volume. The concentration profile of the HRE elements may be periodic with alternating relative maxima and minima, or the concentration profile of the HRE elements may be of substantially sinusoidal shape. In another embodiment, the single sintered magnet has a thickness of over 6 mm. The RE magnet volume may include at least one of a RE-Fe-B or Sm-Co alloy. The magnet may further include electrically resistive material within the volume, which may be formed as at least one layer within the volume. In an embodiment, there may be a concentration profile of electrically resistive material within the volume that is periodic with alternating relative maxima and minima. The electrically resistive material may include a magnetic material.In one embodiment, at least three layers of material comprising an HRE element or an HRE alloy are placed in the mold. The layers of material comprising an HRE element or an HRE alloy may have a thickness of 25 to 250 μm. The layers of material comprising an HRE element or an HRE alloy may each have the same thickness. In one embodiment, the material comprising a HRE element or alloy is a powder. The powder may be selected from any one of DyF 3, TbF 3, Dy 2 O 3, Tb 2 O 3 and DyFe. In another embodiment, the material comprising an HRE element or an HRE alloy is a liquid. The material with an HRE element or an HRE alloy can be mixed with an electrically resistive material before being placed in the mold. In an embodiment, the electrically resistive material includes a magnetic material.In at least one embodiment, a rare earth magnet is provided. The magnet may include a green compact having a compacted layer of magnetic powder including a rare earth element or a rare earth alloy and at least two layers of a material including a heavy rare earth element (HRE element) or a heavy rare earth alloy. FIG. 1A is a schematic diagram of a layered magnet assembly having alternating layers of heavy rare-earth (HRE)-containing material and a magnetic powder; FIG. 1B is a schematic diagram of the layered arrangement of FIG. 1A pressed into a green compact; FIG. 1C is a schematic diagram of the green compact of FIG. 1B sintered into a magnet with HRE-containing material present in the volume of the magnet; FIG. 2 is a schematic coercive force profile showing the coercive force of a laminated magnet as compared with the coercive force profile of a conventional grain boundary diffusion process magnet; FIG. 3A is a schematic diagram of a layered magnet assembly having alternating layers of a mixture of HRE-containing material and electrically insulating material and a magnetic powder; FIG. 3B is a schematic diagram of the layered arrangement of FIG. 3A pressed into a green compact; FIG. 3C is a schematic diagram of the green compact of FIG. 3B sintered into a magnet with HRE-containing material present in the volume of the magnet and spaced electrically insulating material layers; FIG. 4A is a schematic diagram of a layered magnet assembly having alternating layers of electrically insulating material and a magnetic powder with a magnetic field oriented in a vertical direction; FIG. 4B is a schematic diagram of a sintered magnet having electrically insulating layers parallel to the c-axis of a magnetic hard phase; FIG. 4C is a schematic diagram of a sintered magnet having electrically insulating layers oblique to the c-axis of a magnetic hard phase; and FIG. 4D is a schematic diagram of a sintered magnet having electrically insulating layers in a cross-linked configuration relative to the c-axis of a magnetically hard phase.As required, detailed embodiments of the present invention are disclosed herein; however, it is to be understood that the disclosed embodiments are merely exemplary of the invention that may be embodied in various and alternative embodiments. The figures are not necessarily to scale; some features may be exaggerated or minimized to show details of particular components. Therefore, specific structural and functional details disclosed herein are not to be interpreted as limiting, but merely as a representative basis for teaching one skilled in the art to variously employ the present invention.Because of the relatively high cost of heavy rare earth (HRE) rare earth (HRE) magnets, it would be advantageous to reduce the amount of HRE elements employed and further maintain the improved properties provided by the HRE elements. One method of reducing the amount of HRE elements used in permanent magnets is to apply a layer or coating of HRE media to the surface of sintered magnets, followed by a heat treatment to improve diffusion. The sintered magnets may be any suitable rare earth magnets, for example, a neodymium-iron-boron magnet in which the sintered magnet has grains of Nd 2 Fe 14 B and grain boundaries with an Nd-rich phase.The method may be a grain boundary diffusion process (hereinafter referred to as GBDP) including coating a surface of the sintered magnets with a layer of HRE elements by, for example, wet coating or metal vapor deposition. The magnets may then be heated to a temperature at which the Nd-rich grain boundaries melt, thereby significantly increasing the diffusion of the HRE elements into the grain boundaries. During this process, some of the HRE elements diffuse further into the outer shell of the grains, for example, Nd 2 Fe 14 B grains. The HRE elements in the outer shell provide an enhanced anisotropy field and enhanced anti-demagnetization properties of the magnets, resulting in an increased coercive force in the magnets.Although the grain boundary diffusion process discussed above may increase the coercivity and reduce the amount of HRE elements required as compared to mixing HRE elements into the original magnetic alloy, further reduction in the HRE elements would be advantageous for reducing cost. In addition, the above-described GBDP has a maximum diffusion depth of about 3 mm. That is, if two opposing surfaces of the magnet are coated with a layer of HRE elements, the maximum thickness of the magnet is about 6 mm. In some applications it may be advantageous or necessary to have magnets thicker than 6 mm. Although it may be possible to stack a plurality of magnets treated using the above-described GBDP together to form a magnet having a thickness of over 6 mm, such a stacked magnet has poor mechanical properties. For example, magnets thinner than 6 mm may be bonded to each other to form a magnet thicker than 6 mm, but the adhesive has poor mechanical strength as compared with the unitary magnet. Also, mechanical bundling of thin magnets is possible to form a magnet that is thicker than 6 mm, but this is associated with additional costs and may be impractical in some applications.Referring to FIGS. 1A to 1C, a process for forming a magnet 10 having a flexible thickness range and more homogeneous characteristics than in the above-described GBDP is shown. The magnetic powder 12 forming the volume of the magnet may be any suitable magnetic material. In one embodiment, magnetic powder 12 is a rare earth magnetic powder. Examples of suitable rare earth magnetic compositions include, but are not limited to, RE-Fe-B and Sm-Co, where RE is a rare earth element such as Nd, Pr, Sm, Gd, or others. The magnetic powders 12 may be prepared by alloying and pulverizing, but other suitable methods may be used.As shown in FIG. 1A, the magnetic powder 12 may be coated with a material 14 containing an HRE element in a mold or a tool (not shown). The HRE-containing material 14 may be a powder such as DyF 3-, TbF 3-, Dy 2 O 3-, Tb 2 O 3-, DyFe alloys, or others. The HRE-containing material 14 may also be a liquid solution / suspension containing one or more HRE elements, such as Tb, Dy, Ho, Er, Tm, Yb, Lu, or Y. The magnetic powder 12 and the HRE-containing material 14 may be alternately layered to form magnetic powder layers 16 and HRE layers 18. The HRE layers 18 may have a uniform thickness throughout, or they may have a varying thickness. In addition, the HRE layers 18 may be parallel or non-parallel to each other, and in some embodiments, may intersect. In at least one embodiment, HRE layers 18 form a continuous layer over an entire dimension (e.g., width) of magnet. However, in some embodiments, the HRE layers 18 may not form a continuous layer (e.g., the magnetic powder layers may contact each other).In one embodiment, the first and last layers of the magnet 10 are the HRE-containing material 14. After the magnetic powder 12 and the HRE-containing material 14 are placed in the mold or die, the layered assembly can be pressed into a green compact 20. In one embodiment, the pressure used to form green compact 20 may be between 100 and 1000 MPa. In another embodiment, the pressure used to form green compact 20 may be between 250 and 750 MPa. In at least one embodiment, green compact 20 may be pressed to a density of 40 to 80% (e.g., percent of theoretical density). In another embodiment, green compact 20 may be pressed to a density of 50 to 70%. During the pressing step, a magnetic field 22 may be applied to the layered assembly to provide the resulting magnet 10 with the desired magnetic orientation and characteristics. The magnetic field direction may be designed according to an application. For example, in some embodiments, the magnetic field direction could be parallel or perpendicular to the layer direction. In other embodiments, the field direction may not be parallel or perpendicular to the slice direction (e.g., oblique). A radiation field may also be applied, the radiation field configured to cause the final magnet to have radiative easy axes (e.g., the easy axes extend generally outward from the center in a radial direction). In some embodiments, the external field applied may be between 0.2 T and 2.5 T to aid in the alignment of the magnetic powder 12 during pressing. However, any suitable external field acting may be used.After the laminated assembly is pressed, it is sintered to form a solid unitary magnet 10. The solid unitary magnet 10 may be described as "continuously sintered" in that each layer is sintered adjacent to the adjacent layer rather than being bonded after sintering (e.g., using an adhesive, mechanical fasteners, or other known methods). As shown in FIG. 1B, during the intermediate stage of the sintering process, the HRE-containing material 14 (shown as a powder in FIGS. 1A-1C) initially forms layers 18 between the pressed magnetic powder 12. In addition to the grain boundaries, the HRE elements diffuse into the outer shell of the grains, which increases the anisotropy field and the anti-demagnetization capability of the magnet 10. The process can therefore combine sintering and diffusing into a single step, rather than separate sintering and diffusing steps. Combining sintering and diffusing into a single step may allow better control of HRE diffusion and provide reduced overall processing time, energy, cost, and materials.Referring to FIG. 1C, the magnet 10 may have a concentration profile or gradient 24 of the HRE-containing material 14 after sintering. The profile 24 may vary depending on the number, thickness, concentration of HRE content of the HRE layers 18 and spacing of the HRE layers 18 and / or the time and temperature of the sintering process, as well as other processing parameters. In at least one embodiment, concentration profile 24 of HRE material 14 has at least one local maximum 26 of HRE concentration within the volume of magnet 10 (e.g., not at opposing surfaces of magnet). The local maximum 26 may be located between local minima 28 of the HRE concentration in the concentration profile. In another embodiment, there are multiple local maxima 26 of HRE concentration within the volume of the magnet 10. At local maximum 26, the HRE concentration is higher than on either side of local maximum 26. a given local maximum 26 may also be the global or total maximum (e.g., the highest HRE concentration may occur within the volume). A sintered magnet having an HRE concentration profile 24 with a local maximum 26 within the volume is another distinguishing feature from a GBDP magnet in which diffusion causes the gradient to gradually decrease toward a center of the magnet having a local minimum.In another embodiment, the magnet may have a concentration profile 24 of HRE elements that is periodic and has alternating relative maxima 30 and minima 32. As used herein, "periodic" may include, but does not require, identical or regular intervals. Referring to FIG. 3C, in areas where the HRE layers 18 were originally prior to sintering, there are relative maxima 30, and in areas where magnetic powder 12 was originally present, there are relative minima 32. In one embodiment, the concentration profile 24 of the HRE elements is of substantially sinusoidal shape. This may occur when the layers 18 are substantially equally spaced and have similar or the same thicknesses.In at least one embodiment, the sintering temperature may be in the range of 800 to 1150° C. The sintering time may depend on the sintering temperature, but may vary between 1 and 24 hours, for example. Generally, higher sintering temperatures will require a shorter sintering time, while lower temperatures will require longer sintering times. However, the sintering temperature and time may be adjusted as required to obtain a fully sintered magnet 10. After the sintering is completed, a permanent magnet 10 is formed with HRE elements substantially diffused through the thickness of the magnet 10. As a result, the coercive force of the magnet after the diffusion process can be significantly increased. Compared to a conventional GBDP process, the described embodiment requires only a single-stage heat treatment.Because of the multiple layers 18 of HRE-containing material 14 within the layered arrangement, the diffusion distance between layers 18 of HRE material 14 is significantly reduced compared to the GBDP described above, in which the HRE material 14 is deposited on two surfaces of already sintered magnets. As a result, the coercive force of the magnet is more constant by the thickness of the magnet 10 as compared with the GBDP. The difference in coercive force for a magnet of the same thickness formed using the laminated structure as compared with the GBDP is schematically shown in Fig. 2. While the coercivity profile 34 of the layered array magnet 10 continues to have peaks 36 at depths corresponding to the local maxima 26 of the HRE material layers 18, the valleys 38 (corresponding to the local maxima 28) are much shallower than in the GBDP magnet due to the reduced diffusion distance of the HRE material 14 and because the HRE material 14 was present during sintering rather than being deposited as a layer on an already sintered magnet.The coercivity profile 34 may be controlled by the thickness or HRE concentration of the HRE layers 18. In one embodiment, the one or more outer HRE layers 18 may be thicker or have a higher HRE content than the inner HRE layers. Thereby, a final sintered magnet having a larger coercive force / anti-demagnetization capability in outer / corner regions can be produced, which can be useful for permanent magnet motors that require a higher coercive force in the surface / corner of the magnet.Magnets 10 having a layered arrangement of magnetic powder 12 and HRE-containing material 14 may have any substantially adequate thickness. In contrast to the GBDP which has an effective maximum thickness of 6 mm due to the limits of diffusion from the surfaces, the layered-arrangement magnet can have a thickness of over 6 mm while still consistently having a high coercive force. In one embodiment, the layered array magnet has a thickness of at least 10 mm. In another embodiment, the layered array magnet has a thickness of at least 15 mm. In another embodiment, the layered array magnet has a thickness of at least 20 mm. In another embodiment, the layered array magnet has a thickness of at least 25 mm. Accordingly, magnets constituting a layered arrangement may be large enough to replace multiple magnet arrangements or for applications where GBDP magnets are inadequate.In addition to the advantages of making thicker magnets and achieving a more uniform coercivity distribution, the disclosed method has the additional advantage of allowing tuned magnetic profiles (e.g., coercivity) for various applications. For example, the coercivity (H c-) profile 34 shown in FIG. 2 can be tuned by the number of HRE-containing layers 18 and the thickness of each magnetic sublayer 16, 18. The period modulation of the H c- profile 34 can be tuned by the number of HRE-containing layers 18, while the thickness of each magnet 10 can determine the value of the smallest coercivity.The number of layers 18 of HRE-containing material 14 in magnet 10 and their thickness may vary depending on the total thickness of magnet 10 and the desired level of coercivity, as well as other factors. In at least one embodiment, the layered assembly prior to sintering has at least three layers 18 of HRE-containing material 14. For example, prior to sintering, the magnet 10 may include at least 4, 5, 6, 10, or more layers 18 of HRE-containing material 14. In one embodiment, the outer layers of the layered assembly are each comprised of HRE-containing material 14. however, all of the HRE-containing layers 18 may be within the volume of the layered assembly. The number of layers 18 of HRE-containing material 14 may be defined as a ratio of the layers to mm thickness. For example, if a magnet had a thickness of 6 mm and three layers of HRE containing material, the ratio would be 3:6 or 1:2. In at least one embodiment, the ratio of HRE-containing layers to mm thickness is at least 1:3. in another embodiment, the ratio of HRE-containing layers to mm thickness is at least 1:2. in another embodiment, the ratio of HRE-containing layers to mm thickness is at least 1:1. in another embodiment, the ratio of HRE-containing layers to mm thickness is at least 3:2. in another embodiment, the ratio of HRE-containing layers to mm thickness is at least 2:1.The thickness of the HRE-containing material layers 18 may vary depending on the number of layers and the total thickness of the magnet. The HRE-containing layers 18 may be thick enough to contain sufficient HRE material 14 to diffuse at least to the center to the adjacent HRE-containing layer 18. In at least one embodiment, HRE-containing material layers 18 each have a thickness of 25 to 250 μm prior to sintering. In a further embodiment, the HRE-containing material layers 18 each have a thickness of 50 to 150 μm before sintering. In a further embodiment, the HRE-containing material layers 18 each have a thickness of 50 to 100 μm before sintering. The sintered magnet 10 may have any suitable HRE content depending on the desired magnetic properties. In at least one embodiment, sintered magnet 10 has between 1 and 8 wt % HRE. In another embodiment, the sintered magnet 10 has between 1.5 and 5 wt% HRE. In another embodiment, the sintered magnet 10 has between 1.5 and 4 wt% HRE.The disclosed method is not only suitable for magnets which are pressed almost in the form, but can also be applicable to large or large block magnets. If large ingot magnets are produced during manufacture, the disclosed method may provide further advantages in terms of time and / or cost savings. For the conventional GBDP using a large block magnet, the block must be cut into a shape close to the end application, and then the GBDP process must be applied to each magnet. In the disclosed method, the diffusion process can take place in the large block magnet. First, the HRE layers 18 may be prepared during the pressing process. The number of layers and the thickness of the layers may depend on the application requirement. Second, sintering / diffusion may be performed. Third, the large ingot can be cut / ground into multiple smaller magnets for one or more applications without further heat treatment. Therefore, the time-consuming individual HRE coating process of the GBDP for each smaller magnet can be avoided.In at least one embodiment, in addition to increasing magnet thickness, coercive force, and homogeneity, layered assembly manufacturing process may be used to increase electrical resistance within magnet. The increased electrical resistance may reduce eddy current losses that may occur within the magnet. The layered assembly manufacturing process may be substantially similar to that described above, but with the addition of electrically insulating material 40 to the HRE-containing material 14 prior to the layered process. For example, an electrically insulating material 40 may be mixed with a HRE-containing material 14 and the mixture 42 may be alternately layered with magnetic powder 12 to form a layered assembly. Instead of mixing the insulating material 40 and the HRE-containing material 14, the HRE-containing layers 18 and the insulating layers 44 may be separately laminated in the magnet 10. For example, the layered structure may be HRE-insulating-magnetically-insulating-HRE-insulating-magnetically-insulating-HRE or HRE-magnetically-insulating-magnetic-HRE, or any other combination. The laminated assembly may then be pressed under an external magnetic field 22 and thereafter sintered to form a permanent magnet 10 according to the process described above. The electrically insulating material 40 may be any suitable sinterable material, for example a ceramic powder. In one embodiment, the insulating material 40 is a fluoride or oxide of Ca, Mg, Li, Sr, Na, Ba, Sr, or Fe, or others such as SiO 2 etc.Referring to Figs. 3A-3C, the layered assembly fabrication process including electrically insulating material 40 is shown. The electrically insulating material 40 may be mixed with the HRE-containing material 14 in each layer 18 of HRE-containing material, in some layers and not others, or it may be present as a separate, distinct layer 44. As shown in FIG. 3A, the electrically insulating material 40 is blended with the HRE-containing material 14 in all internal layers but not in the surface layers of the HRE-containing material 14. FIG. 3B shows the layered arrangement after pressing under an external magnetic field 22, wherein the electrically insulating material 40 and the HRE-containing material 14 are arranged in layers between the magnetic powder. By controlling the sintering time and temperature and the selection of the insulating material, a permanent magnet 10 can be formed having HRE material 14 that is still diffused into the grain boundaries and outer grain shells and the insulating material 40 substantially in its original position between magnetic powder layers 16, as shown in FIG. 3C. The insulating material 40 may remain at its original position due, at least in part, to the inblendability with the other materials present. The electrically insulating material thereby forms electrical insulating layers 44 separating high coercivity magnetic layers 16 within the magnet. In another embodiment, rather than remaining at its original position, the electrically insulating material 40 may diffuse within the magnetic powder along with the HRE-containing material 14, but not necessarily to the same depth. In this embodiment, the eddy current loss can be further reduced by increasing the resistance by diffusing the insulating material 40 to the grain boundaries. The processing conditions used to form magnets with HRE and insulating layers may be similar or the same as for magnets with only HRE layers described above.In addition to the electrically insulating materials described above, such as fluorides or oxides, the electrically insulating material 40 may include a magnetic material 46. Using electrically insulating materials, which are also magnetic materials, can result in a magnet with excellent magnetic properties compared to a magnet using non-magnetic insulating material because there is no "wasted" volume inside the magnet that does not contribute to the magnetic strength. The magnetic insulating material 46 may be any suitable material that is both magnetic and electrically insulating. In at least one embodiment, magnetic insulating material 46 has "hard magnetic" properties. A non-depletion list of possible materials may include iron oxide, barium ferrite powder, strontium ferrite powder, or others. The magnetic insulating material 46 may also include magnetic materials coated with an electrically insulating material, for example iron powder with an insulating coating.In at least one embodiment, magnetic insulating material 46 may be mixed with HRE-containing material 14, as described above for electrically insulating material 40. However, in other embodiments not according to the invention, the magnetic insulating material 46 may replace the HRE-containing material in the layered arrangement such that the arrangement includes alternating layers of magnetic powder 12 and magnetic insulating material 46. This layered assembly can be manufactured, compacted and sintered using substantially the same methods as described above. The resulting magnet may be less expensive to manufacture than those with HRE layers 18, but may also provide substantially reduced eddy current losses compared to standard magnets. As shown in FIGS. 4A-4D, the layers 48 of magnetic insulating material 46 may be oriented to be perpendicular, parallel, or at an oblique angle to the c-axis of the magnetic hard phase by aligning the layers under the magnetic field 22 during the pressing process. The magnetic insulating material 46 may also be formed into a cross-linked pattern with intersecting layers 48 of the material to further increase the electrical resistance within the magnet 10.Although the above-described embodiments include a layered structure having multiple layers of magnetic material 12 and layers of HRE material 14, the described process may also be used to form a magnetic structure similar to those formed using the conventional GBDP. An HRE-containing layer 18 may be deposited on the top and bottom with a layer of magnetic material 12 interposed therebetween. This method can therefore produce a GBDP-type magnetic structure in a single-step heat treatment, instead of the conventional method requiring two steps: first sintering and then diffusion heat treatment. This method can then save time and cost for the same magnetic structure and magnetic properties.While exemplary embodiments are described above, the features of various implementing embodiments may be combined to form further embodiments of the invention.
Claims
A method of forming a magnet (10), characterized bythe steps of: - alternately laminating in a magnetic powder mold or tool (12) a rare earth element and heavy rare earth-containing material (14) to form a laminated structure of a plurality of magnetic powder layers (16) and a plurality of heavy rare earth layers (18); - pressing the laminated assembly into a green compact (20); - then sintering to form the solid unitary magnet (10); wherein the heavy rare earth layers (18) intersect.A magnet made according to a method of claim 1, having a heavy rare earth element concentration profile with a continuously sintered rare earth magnet volume, the concentration profile including at least one local maximum of heavy rare earth element concentration located between local minima of the heavy rare earth element concentration within the volume, such that a corresponding coercivity profile of the magnet includes at least one local maximum located between local minima within the volume.The magnet of claim 2, wherein the heavy rare earth element concentration profile contains multiple local maxima of the heavy rare earth element concentration within the volume.The magnet of claim 2, wherein the concentration profile of the heavy rare earth elements is periodic with alternating relative maxima and minima.The magnet of claim 4, wherein the concentration profile of the heavy rare earth elements is of substantially sinusoidal shape.The magnet of claim 2, wherein the single sintered magnet (10) has a thickness of over 6 mm.The magnet of claim 2, wherein the rare earth magnet volume contains at least one of a RE-Fe-B or Sm-Co alloy.The magnet of claim 2, further comprising an electrically resistive material within the volume.The magnet of claim 8, wherein the electrically resistive material is formed as at least one layer within the volume.The magnet according to claim 8, wherein within the volume there is a concentration profile of the electrically resistive material that is periodic with alternating relative maxima and minima.The magnet of claim 8, wherein the electrically resistive material includes a magnetic material.
Citation Information
Patent Citations
Method for producing an R-T-B sintered magnet
DE112008000992T5
Laminated composite magnets containing rare earth metals with increased electrical resistance
DE112011100574T5
Nd-Fe-B SINTERED MAGNET AND ITS MANUFACTURING METHOD
JP2001068317A
Permanent magnet for motor, and method for manufacturing the permanent magnet for motor
US20110012460A1
High resistivity magnetic materials
US20130049909A1