Platelet-shaped, randomly shaped, sintered abrasive particles and a method for their production

DE102015108812B4Active Publication Date: 2024-10-17IMERTECH SAS
View PDF 19 Cites 0 Cited by

Patent Information

Application Number
DE102015108812
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2015-06-03
Publication Date
2024-10-17
Estimated Expiration
2035-06-03

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Platelet-shaped, randomly shaped, sintered abrasive particles based on alpha-aluminum oxide, which have a body with a first surface and a second surface arranged opposite the first surface, wherein both surfaces are separated by a randomly shaped sidewall with a thickness (T) between 20 µm and 500 µm, wherein the abrasive particles have a length to thickness ratio between 2 and 10 and have a crystal structure with an average crystal size between 100 nm and 300 nm, wherein the chemical composition of the abrasive particles comprises between 1 wt.% and 20 wt.% zirconium oxide and between 0.5 wt.% and 5 wt.% magnesium oxide, wherein at least 50 wt.% of the zirconium oxide is in the tetragonal modification, wherein the crystal structure comprises a dominant continuous phase of α-aluminium oxide crystals and a secondary phase with intragranular zirconium oxide crystals, wherein the crystal size of the zirconium oxide crystals is below 100 nm.
Need to check novelty before this filing date? Find Prior Art

Description

The present invention relates to platelet-shaped, randomly shaped, sintered abrasive particles, a process for their preparation and their use.About 30 years ago, a new, substantially improved type of alpha alumina abrasive grain, commonly referred to as sol-gel abrasive grain, was developed and marketed. The abrasive performance of this new type of abrasive grain versus metal, as measured, for example, as material removal or G-factor (quotient of material removal and abrasive wear), was dramatically higher than that achieved with conventional fused alumina abrasive grains.Originally, the sol-gel abrasive grains were developed as an alternative to the fused microcrystalline zirconia corundum abrasive grains. Accordingly, EP 0 024 099 B1, which originates from 1979, claims a granular abrasive mineral based on α-aluminum oxide, which contains at least 10% zirconium oxide, hafnium oxide or combinations of zirconium oxide and hafnium oxide as modifying component. In the following years, numerous sol-gel abrasive grains have been published in patents and patent applications, whereby the original idea of an aluminum oxide-zirconium oxide composite has been abandoned, because it has obviously been generally found that pure aluminum oxide-based products or sol-gel abrasive grains containing small amounts of other modifying additives different from zirconium oxide have been more efficient than sol-gel-based zirconium corundum abrasive grains.Sol-gel abrasive grains are usually prepared by dispersing alumina monohydrate in acidic water, gelling the dispersion, drying the resulting gel, crushing the dried gel into gel particles, calcining the dried particles to remove the water and other volatiles, and sintering the particles at a temperature far below the melting point of alumina. Often, one or more modifiers, nucleating agents, grain growth inhibitors, or other additives are additionally used to further improve the properties and abrasive performance of the alumina abrasive grains.The production of dense alumina-based sol-gel abrasive grains is described, for example, in U.S. Pat. Nos. 4,314,827; 4,881,951 and 5,227,104.In the last 15 years, moreover, numerous patents and patent applications have been published which describe sol-gel abrasive particles based on alpha-aluminum oxide which have a precisely predetermined shape.U.S. Patent No. 5,201,916 describes abrasive grain particles having shapes that can be characterized as thin particles having triangular, rectangular, or other geometric shapes. Such abrasive grain particles are made by providing a dispersion comprising particles that can be converted to alpha alumina and placing this dispersion in a forming cavity having a predetermined shape. After gelling and drying, abrasive grain particle precursors having a predetermined shape are obtained. These particles are removed from the forming cavity and subsequently calcined and sintered.Similarly shaped products and methods, as well as individual properties and aspects of such products and methods, are described, for example, in U.S. Pat. Nos. 7,384,437; 8,123,828; 8,764,865; 8,142,531; 8,142,891 and 8,142,532 as well as in the publications U.S. Pat. No. 5,551,963 A; U.S. Pat. No. 4,744,802 A; U.S. Pat. No. 4,623,364 A; U.S. Pat. No. 4,964,883 A and U.S. Pat. No. 2013 / 0 074 418 A1 which go beyond the state of the art already cited in the description in the testing method.The methods and products described in the above-mentioned documents have the disadvantage that, in order to obtain a predetermined shape, shapes having a specific size and shape are used, which correspond to the size and shape of the desired abrasive grain. However, the average particle size of the desired abrasive grains is in the range of 1 mm or less, so that the above-mentioned shaping technique is complicated and, above all, less productive in most cases.EP 0 318 168 B1 describes abrasive grains in the form of platelets. The platelets are produced by the sol-gel process, in which case, for example, the gel is formed by extrusion into a layer having a certain thickness, then dried and then comminuted to particles. The crushed particles are calcined and sintered. As for the obtained plate-shaped abrasive grains, neither a particular crystal structure nor a particular chemical composition is described. Such abrasive grains have not been appeared on the market, although the patent already goes back to 1987.U.S. Patent Application 2010 / 0319269 A1 describes triangular shaped abrasive particles with a low circularity factor. It is stated that higher grinding powers are achieved by particularly exact shaping of the shaped grinding particles.Although many abrasive grains of different shapes have been described in the last 15 years, only one abrasive grain of a triangular shape has been successfully marketed as a product under the trade name of "Cubitron II". However, at the same time, those skilled in the art will apply a high performance potential to shaped abrasive grains, so there is a great demand for alternative shaped abrasive grains having high abrasive performance.It is therefore an object of the present invention to provide shaped abrasive particles which are inexpensive to produce and have a high performance. It is a further object of the present application to provide a method for making such shaped abrasive particles based on α-alumina.Surprisingly, it has been found in the context of the present invention that platelet-shaped, randomly shaped, sintered abrasive particles based on α-aluminum oxide also have superior properties for certain grinding operations, provided that these abrasive particles have a very fine crystal structure with an average crystal size between 100 nm and 300 nm and a high hardness H V of more than 20 GPa.According to the invention, the platelet-shaped, randomly shaped, sintered abrasive particles according to the invention have a chemical composition comprising between 1% by weight and 20% by weight zirconium oxide. In this case, the crystal structure comprises a dominant continuous phase of α-alumina crystals and a secondary phase with substantially intragranular zirconia crystals, wherein the mean crystal size of the alumina and zirconia crystals is between 100 nm and 300 nm and the crystal size of the zirconia crystals is below 100 nm.The platelet-shaped, randomly shaped, sintered abrasive particles generally have a shaped body having a first surface and a second surface disposed opposite the first surface, both surfaces being separated from each other by a randomly shaped sidewall having a thickness (T) between 20 μm and 500 μm.The plate-like, randomly shaped sintered abrasive particles can be effectively characterized by various grain shape factors based on image analyses.The equivalent circle diameter (X) is defined as the diameter of the circle having the same area as that of the particle to be determined. The equivalent circle diameter (X) can be calculated based on the measured area (A) of the particle according to the equation (1):Circularity (C) is defined as the degree of similarity of the particle with a circle. The farther the particle is from a perfect circle, the lower the value for circularity. Circularity can be calculated based on the measured area (A) and the circumferential length (P). ISO 9276-6 (2006) defines circularity according to equation (2):As in most prior literature, the aspect ratio (AR = aspect ratio) in the present case is calculated as the length divided by width. The length is the maximum distance between two points on the circumference of the particle parallel to the main axis. The width is the maximum distance between two points on the circumference parallel to the minor axis. The major axis passes through the center of mass of the particle corresponding to the shape with the minimum rotational energy. The minor axis passes through the center of mass of the particle and is always perpendicular to the major axis.The inequality factor (UE) takes into account different geometries (i.e., a circle, a rectangle, a square, and an equilateral triangle) in the calculation based on the measured area (A) and the circumferential length (P) according to equation (3)):Some example UE values for different geometries sinare summarized in Table 1 below:Table 1 Table 12 π ~ 9.874π ~ 12.573√3π ~ 16.32~ 13.09~ 14.13~ 16.76A further possibility for characterizing the platelet-shaped, randomly shaped, sintered abrasive particles results from the use of a circumferential random factor (PRF= perimeter randomity factor), which is determined by the tangents of an equilateral triangle, a rectangle or a circle along the side wall of the circumference of the platelet-shaped, randomly shaped abrasive particles. The PRF (%) is calculated by dividing the area (M) missing to complete the regular geometric body by the actual area (A) of the platelet shaped, randomly shaped abrasive particle and multiplying by 100. The measurement is performed using image analysis software or similar suitable measurement technique. The measurement is repeated until the peripheries of at least 50 individual platelet-shaped, randomly shaped abrasive particles have been measured, the average peripheral random factor (APRF) being obtained from the average value of the at least 50 results. An average circumferential random factor of 100% would mean that the missing surface area is exactly as large as the actual surface area of the measured abrasive grains.It has been found that particularly good grinding results can be achieved with platelet-shaped abrasive grains if the mean peripheral random factor is more than 15%, preferably more than 20% and particularly preferably between 30% and 100%. One possible explanation for this is that the irregularly arranged corners, edges of a multiplicity of platelets in the abrasive mean a relatively uniform abrasive surface provided with a particularly large number of cutting edges and in this way generate a high amount of material removal. This explanation is based primarily on optical investigations of the abrasives.Another way to describe the "random nature" of platelets can be determined by examining the scattering of the surface areas or aspect ratios of the individual platelet shaped particles as compared to a selected shaped particle, such as an equilateral triangle such as Cubitron II. The scattering of the surface areas from particle to particle is presented along with some important grain shape factors for some selected abrasive particles in the following Table 2. To describe the scattering of the surface areas, the Excel software program ANOVA was used. Table 2 Table 2C. C0.630.610.680.6150.730.58AR1.741.941.581.691.541.08UE15.9416.5514.7516.70413.7017.02X (μm)853801696790746655APRF (%)34.844.532.428.926.33.3Scattering of the Surface AreasSum of the deviations (μm 2)6925171062519501266118015663869197022Mean value of the deviations between the individual particles (μm 2)796087813298131136141741Scattering (μm 2) 21924244785507675502680269917958317262346291212040501Standard deviation (μm 2)1387223468517742377153181428%971164336229671072100The selected abrasive grains listed in Table 2 are platelet-shaped, randomly shaped abrasive particles according to the invention in the grain P36 with in each case 2.5% by weight (ZTA 2.5), 5% by weight (ZTA 5) or 10% by weight (ZTA 10) proportions of zirconium oxide which were obtained according to Examples 7, 8 and 9. As a comparison, a commercially available non-shaped abrasive grain (Cub. 321) and an abrasive grain (cube) formed in the shape of equilateral triangles. II). The chemical composition of the latter two abrasive grains corresponds to Comparative Example 1.It has been found that particularly good results are obtained with the platelet-shaped, randomly shaped abrasive particles if they have a certain degree of circularity and small differences in length and width. Advantageously, the typical ratio of length to width is between 1.20 and 1.90, preferably between 1.40 and 1.70, particularly preferably below 1.60. An example of the latter type of platelet shaped abrasive particles is ZTA 5cc which was prepared according to Example 8 but additionally comminuted and classified after sintering. One possible explanation for this is that particularly uniform abrasive surfaces can be formed in this case if the platelet-shaped abrasive particles are perpendicular to the abrasive backing with their side wall after the electrostatic scattering.Thus, good grinding results are obtained particularly when circularity (C) is in the range of 0.6 to 0.7. It has also been found that it is advantageous if the inequality factor (UE) of the platelet-shaped, randomly shaped abrasive particles is between 10 and 17.Another suitable characteristic for characterizing the platelet shaped, randomly shaped, sintered abrasive particles is the ratio of length to thickness, which is typically in the range of 2 to 10, preferably in the range of 4 to 8. Here again, it has been found that the platelet-shaped, randomly shaped abrasive particles must have a certain compactness with a corresponding ratio of length to thickness in order to be able to be used successfully in abrasives.In a preferred embodiment of the present invention, the randomly shaped sidewall has a thickness (T) between 150 μm and 450 μm. The mean crystal size of the aluminum oxide and zirconium oxide crystals is advantageously below 250 nm.If the corresponding grain shape factors do not already result from the thickness of the predetermined gel layer and the subsequent comminution, the ratios can be adjusted by additional classification measures, such as sieving or grain shape sorting, for example via a vibration table.Particle sizes and shapes were measured using a STEMI SV6 optical microscope (Carl Zeiss GmbH). Particle size and particle shape were analyzed using ImageJ software, which, when imaging, calculates the corresponding surface areas and circumferential length of each individual matched and separated particle. The method is reliable and provides reproducible values.Because a magnesium nitrate solution is used as a crystal growth inhibitor and a peptizer in the sol-gel process, the chemical composition of the platelet-shaped, randomly shaped sol-gel abrasive particles preferably comprises between 0.5% and 5% MgO by weight.Moreover, it has been found that even a proportion of between 1% by weight and 10% by weight zirconium oxide is sufficient to obtain powerful abrasive particles for certain grinding operations. Thus, in an advantageous embodiment of the present invention, the platelet-shaped, randomly shaped abrasive particles contain between 1% by weight and 10% by weight zirconium oxide.At least 50 wt.%, preferably 75 wt.%, of the zirconia is present in the tetragonal modification.In a further preferred embodiment of the present invention, at least one surface is uniformly structured and has structural elements such as knobs, depressions, shafts, teeth, saw teeth, pyramids, cones and / or other depressions or protrusions. In this way, the incorporation of the platelet-shaped abrasive particles into abrasives, such as grinding wheels, grinding belts and fiber discs, is improved and their wear can be additionally reduced. It goes without saying that a further improvement results if both surfaces are uniformly structured and have the above-mentioned structural elements. The structural elements can be imparted to the surface of the platelet shaped randomly shaped abrasive particle by applying the gel to a backing having a mirror image structure prior to drying. The second uniformly structured surface can be obtained by treating the surface of the applied gel layer with a texture roll which also has a mirror image structure. In this case, it is of course a prerequisite that the consistency of the gel is strong enough to maintain the applied structure during the drying process.The method for producing the platelet shaped random shaped abrasive particles comprises the following steps:preparing a dispersion of α-aluminum monohydrate in acidified water containing α-alumina seeds having a particle size of less than 300 nm;gelling the dispersion by adding an aqueous solution of a zirconium and magnesium compound in the form of a salt solution;forming the gel into a layer of uniform thickness by any suitable method, such as extrusion, filling into a mold, pressing, spreading, or coating;drying the molded gel to obtain platelet shaped abrasive grain precursor material;crushing and sieving the platelet shaped abrasive grain precursor material to obtain platelet shaped randomly shaped abrasive particle precursors;optionally calcining the abrasive grain precursor particles;sintering the abrasive grain precursor particles at temperatures below 1450° C. to obtain platelet shaped, randomly shaped abrasive particles; andredissizing and classifying optionally; andoptionally, additionally crushing, screening and classifying the sintered platelet shaped random shaped abrasive particles to obtain platelet shaped random shaped abrasive particles having an aspect ratio (AR) of less than 1.70, preferably less than 1.60.The preparation of the α-alumina cores is a particularly important process step which is carried out, for example, by wet grinding a fine-grained α-alumina powder having a particle size of less than 3 μm in a ball mill and then centrifuging the ground dispersion to obtain α-alumina cores having a particle size of less than 100 nm. The amount of seeds used for the production of platelet-shaped, randomly shaped abrasive particles is typically in the range of from 1% to 5% by weight, advantageously about 2% by weight, based on the weight of the abrasive particle product. The centrifuged seed dispersion is added to a 20% by weight-30% by weight aqueous solution of α-aluminium oxide monohydrate to produce the germinated dispersion of α-aluminium hydrate in acidic aqueous solution, the pH of the solution being adjusted to about 2.5 by addition of sufficient nitric acid. The resulting solution is homogenized using a high shear mixer and then gelled at room temperature by adding a salt solution containing sufficient zirconium acetate and magnesium nitrate to obtain abrasive particles having a chemical composition comprising 1 wt% - 20 wt% zirconium oxide and 1 wt% - 5 wt% magnesium oxide. The gel is shaped, for example, by extrusion over a die with a corresponding slot die to form a flat layer with a layer thickness of approximately 800 μm-1600 μm. The flat layer is dried at temperatures around 100° C., whereby the thickness of the layer shrinks very much and cracks are formed. The dried material is crushed and sieved to obtain platelet shaped random abrasive particle precursors. These precursor particles are optionally calcined at a temperature between 600 and 700° C. and then sintered at about 1380° C. in a rotary kiln for 20 minutes. After sintering, the sintered abrasive particles are preferably comminuted once again, sieved and / or classified, for example with the aid of a vibration table, in order to obtain platelet-shaped abrasive particles having an aspect ratio of less than 1.70, preferably less than 1.60.Besides extrusion, any other suitable method such as pressing, filling into a mold, spreading, spraying and coating may also be used to form the gel.Generally, the platelet shaped random abrasive particles have a hardness H V of more than 20 GPa, preferably more than 22 GPa, and a density of more than 97% of the theoretical density.The essence of the present invention will be explained in addition with the aid of figures which are attached to the description as FIGS. 1 to 4. FIG. 1 shows a scanning electron micrograph of an etched grind of a platelet-shaped, randomly shaped abrasive particle. FIG. 2A shows the surface areas of a platelet-shaped, randomly shaped abrasive particle measured with the aid of a uniform triangle FIG. 2B shows the surface areas of a platelet-shaped, randomly shaped abrasive particle measured with the aid of a rectangle. FIG. 2C shows the surface areas of a platelet-shaped, randomly shaped abrasive particle measured with the aid of a circle. FIG. 3A is a plan view of the platelet shaped randomly shaped abrasive particle of FIGS. 2A-2C. FIG. 3B shows a perspective view of the platelet shaped randomly shaped abrasive particle of FIGS. 2A-2C. FIG. 4 is a comparative graph showing the grinding performance of the plate-shaped random abrasive particles and abrasive particles of the prior artFigure 1 shows the microcrystalline structure of the platelet shaped randomly shaped abrasive particles comprising a predominant continuous phase of α-alumina crystals and a secondary phase of substantially intergranular oriented zirconia crystals 1. The chemical composition of the analyzed example comprises 2.5 wt % zirconium oxide and 1 wt % magnesium oxide. The pattern was prepared using 2% by weight α-alumina seeds having a particle size below 100 nm. The above-described platelet-shaped abrasive particle has a hardness H V of 23.6 GPa and a density of 98.6% of the theoretical density. The mean crystal size is between 100 and 300 nm and the crystal size of the zirconium oxide crystals 1 is below 100 nm.FIGS. 2A to 2C illustrate the measurement method for determining the mean circumferential random factor (APRF). The circumferential random factor (PRF) is determined by the tangents of a regular triangle (see FIG. 2A ), a rectangle (see FIG. 2B ), or a circle (see FIG. 2C ) drawn along the side wall of the circumference of the platelet-shaped, randomly shaped abrasive particle. The PRF (%) is calculated by dividing the area (M) missing to complete the regular geometric body by the actual area (A) of the platelet shaped, randomly shaped abrasive particle and then multiplying by 100. The measurement is repeated until the peripheries of at least 50 individual platelet-shaped, randomly shaped abrasive particles have been measured, the average peripheral random factor (APRF) being obtained from the average of the at least 50 results. The closest uniform geometry should be used for the calculation. Thus, for a plate-shaped, random shaped abrasive particle having a circumference as shown in Figs. 2A to 2C, a circle or a rectangle should be employed.FIG. 3A is a plan view of the platelet shaped random shaped abrasive particle of FIGS. 2A to 2C. The length (L) is the maximum distance between two points on the circumference of the particle parallel to the major axis. The width (W) is the maximum distance between two points on the circumference parallel to the minor axis. The major axis passes through the center of mass of the particle corresponding to the shape with the minimum rotational energy. The minor axis passes through the center of mass of the particle and is always perpendicular to the major axis.FIG. 3B is a perspective view of the platelet shaped random abrasive particle of FIGS. 2A to 2C. The platelet shaped random abrasive particle has a body with a first surface 2 and a second surface opposite the first surface, both surfaces being defined by a random shaped (extending) sidewall 3 having a thickness (T) between 20 μm and 500 μm.FIG. 4 is a graphical representation of some selected grinding tests of flake shaped, randomly shaped abrasive particles as compared to non-shaped sintered abrasive grains. FIG. 4 is discussed in more detail in the context of the following description of the grinding tests.The present invention is additionally explained in more detail with reference to the following examples, wherein the particular materials and amounts mentioned in the examples and the other conditions and details should not be interpreted as an undesired limitation of the invention.Example 1 (Comparative Example)Comparative Example 1 was prepared by the impregnation method using about 2% by weight of La 2 O 3, 1 % by weight of Y 2 O 3 and 1% by weight of MgO as modifiers, according to the teaching of U.S. Patent 4,881,951. The abrasive grain thus obtained corresponds to the sol-gel abrasive grain commercially available under the trade name "Cubitron 321".Example 2 (Comparative Example)A dispersion of about 30 wt.% solids content was obtained by mixing alpha alumina monohydrate together with 2 wt.% seeds based on the total weight of the desired product in a solution containing water and 70% concentrated nitric acid, adjusting the pH to about 2.5. The sol obtained was added with 1% by weight of oxide equivalent of magnesium nitrate and 2.5% by weight of oxide equivalent of zirconium acetate as modifying components, based in each case on the weight of the desired product. After the addition of the zirconium acetate and magnesium nitrate, gelation was carried out at room temperature. The gel was dried at about 100°C to obtain abrasive particle precursor material which was comminuted to reduce the particle size to a size slightly above that of the desired product and subsequently sieved. The screened abrasive particle precursors were sintered for 20 minutes at 1380° C. in a rotary kiln to obtain abrasive particles. After sintering, the abrasive particles were finally sieved to obtain a grain P36 according to FEPA.Examples 3-6 (Comparative Examples)Examples 3-6 were produced analogously to Comparative Example 2, with the exception that 5% by weight (Example 3), 10% by weight (Example 4), 15% by weight (Example 5) or 20% by weight (Example 6) of oxide equivalent zirconium acetate was used as modifying component.Example 7A dispersion of about 30 wt.% solids content was obtained by mixing alpha alumina monohydrate together with 2 wt.% seeds based on the total weight of the desired product in a solution containing water and 70% concentrated nitric acid, adjusting the pH to about 2.5. The sol obtained was added with 1% by weight of oxide equivalent of magnesium nitrate and 2.5% by weight of oxide equivalent of zirconium acetate as modifying components, based in each case on the weight of the desired product. After the addition of the zirconium acetate and magnesium nitrate, gelation was carried out at room temperature. The gel was extruded onto a support plate by means of a die having a rectangular die of 1.5 mm in thickness and 3 cm in length to obtain a sheet. The shaped gel was dried at about 100°C to obtain abrasive particle precursor material which was comminuted to reduce the particle size to a size slightly above that of the desired product and subsequently sieved. The screened abrasive particle precursors were sintered for 20 minutes at 1380° C. in a rotary kiln to obtain abrasive particles. After sintering, the abrasive particles were finally sieved to obtain a grain P36 according to FEPA.The sintered plate-shaped random abrasive particles have a Vickers hardness H V of 23.6 GPa, a density of 98.6% of the theoretical density, and a crystal structure having an average crystal size of 170 nm. The particles have an average length of about 1080 μm, an average width of about 620 μm and an average thickness of about 180 μm.Examples 8 and 9Examples 8 and 9 were produced analogously to Example 7, with the difference that 5% by weight (Example 8) and 10% by weight (Example 9) of oxide equivalent zirconium acetate were used as modifying component.Example 11 (Grinding test / 250 mm fiber discs)The fiber discs were prepared by electrostatically scattering about 40 grams of abrasive particles by an electrostatic abrasive grit scattering system (Peter Schwabe GmbH) onto vulcanized fiber paper coated with about 5 grams of resin base binder using an electrostatic field of 22-35 kV for 6-10 seconds. The coated fiber grinding wheels were cured for 6 hours below 100° C. and subsequently coated with about 35 g of size coat binder and then cured for 12 hours at temperatures below 140° C.The tests were performed on a P36 grain with the following sieve analysis. Table 3 Table 3118100001 +225710<11 up to 33060010-181 up to 43550052 - 701 up to 540425>92pass through 540425<8The workpiece, a Cr-Ni stainless steel 1.457 rod with a diameter of 20 mm, was pressed with a force of 40 N and 60 N, respectively, against the fiber disk rotating at 2000 revolutions per minute. In the test, the material removal on the workpiece was measured in each case after a 2 minute cycle. Each test run comprised a total of 8 grinding cycles, each interrupted by a 2 minute cooling period. After the test run, the wear of the fiber disk was additionally determined. Table 4 Table 41 (Comparison)25020.2137.6100230.71002 (Comparison)17021.9145.9104227.21063 (Comparison)17522.4126.292220.11034 (Comparison)17523.8131.498212.61025 (Comparison)14024.4128.592209.3986 (Comparison)20020.9124.487198.4897 (Invention)17023.6151.6117252.61258 (Invention)19023.2148.0118283.31429 (Invention)14522.2135.5102252.1121A graph of the grinding tests of some selected examples (1, 2, 7 and 8) is shown in Fig. 4. Comparative example 1 is designated here as Cubitron 321. Comparative example 2 is a sol-gel corundum doped with 2.5% by weight zirconium oxide and designated ZTA-SG2.5. Example 7, a platelet shaped random abrasive particle having the same composition as Example 2, is designated ZTA-SG2.5 (Plates). Example 8, an abrasive particle according to the invention doped with 5% by weight zirconium oxide, has the designation ZTA-SG5 (Plates).The G factor is calculated from equation (4) making a direct reference to comparative example 1:It can clearly be seen from the graph that the two platelet-shaped sample examples 7 and 8 exhibit significantly higher removal performance than the non-shaped abrasive grains, in particular in the first cycle, wherein the example 8 doped with 5% by weight zirconium oxide remains at a high level over the entire test. A further advantage is that the wear of the abrasive is lower in all examples doped with zirconium oxide than in comparative example 1, which is noticeable in particular in the test with higher pressures, so that an increase in performance of 42% is to be seen for example 8 at high pressure with a G factor of 142%.

Claims

Platelet-shaped, randomly shaped, sintered abrasive particles based on alpha-aluminium oxide, which have a body with a first surface and a second surface arranged opposite the first surface, wherein both surfaces are separated by a randomly shaped side wall with a thickness (T) between 20 μm and 500 μm, wherein the abrasive particles have a ratio of length to thickness between 2 and 10 and have a crystal structure with an average crystal size between 100 nm and 300 nm, wherein the chemical composition of the abrasive particles comprises between 1 wt.% and 20 wt.% zirconium oxide and between 0.5 wt.% and 5 wt.% magnesium oxide, wherein at least 50 wt.% of the zirconium oxide is present in the tetragonal modification, wherein the crystal structure comprises a dominant continuous phase of α-alumina crystals and a secondary phase with intragranular zirconia crystals, wherein the crystal size of the zirconia crystals is below 100 nm.Abrasive particles according to claim 1, characterized in that the chemical composition of the abrasive particles comprises between 1 wt.% and 10 wt.% zirconia.Abrasive particles according to either of Claims 1 and 2, characterized in that at least 75% by weight of the zirconium oxide is present in the tetragonal phase.Abrasive particles according to any one of claims 1 to 3, characterized in that the mean crystal size of the aluminium oxide and zirconium oxide crystals is less than 250 nm.Abrasive particles according to any one of claims 1 to 4, characterized in that the abrasive particles have a circularity (C) greater than 0.60.Abrasive particles according to one of Claims 1 to 5, characterized in that the abrasive particles have one of the inequality factors (UE) between 10 and 17.Abrasive particles according to one of Claims 1 to 6, characterized in that the abrasive particles have an average peripheral random factor (ARPF) of greater than 15%.Abrasive particles according to any one of claims 1 to 7, characterized in that the randomly shaped side wall has a thickness (T) comprised between 100 μm and 450 μm.Abrasive particles according to one of Claims 1 to 8, characterized in that the abrasive particles have an aspect ratio (AR) of between 1.20 and 1.90.Abrasive particles according to one of Claims 1 to 9, characterized in that the abrasive particles have an aspect ratio (AR) of between 1.40 and 1.70.Abrasive particles according to one of Claims 1 to 10, characterized in that at least one surface is uniformly structured with structural elements such as knobs, depressions, shafts, teeth, saw teeth, pyramids, cones and / or other depressions or protrusions.A method for the production of abrasive particles according to any of the preceding claims, the method comprising the steps of: - preparing a dispersion of α-alumina monohydrate in acidified water containing α-alumina seeds having a particle size of less than 300 nm, the α-alumina seeds being obtained by wet milling a fine-grained α-alumina powder having a particle size of less than 3 μm in a ball mill and subsequently centrifuging the milled dispersion; - gelling the dispersion by adding an aqueous solution of a zirconium and magnesium compound in the form of a salt solution; - forming the gel into a flat layer having a uniform layer thickness of 800 μm - 1600 μm by any suitable method, such as extrusion, filling into a mold, pressing, spreading or coating; drying the shaped gel to obtain platelet shaped abrasive grain precursor material having a length to thickness ratio in the range between 2 and 10; crushing and sieving the platelet shaped abrasive grain precursor material to obtain platelet shaped randomly shaped abrasive particle precursors having a length to thickness ratio in the range between 2 and 10; optionally calcining the abrasive grain precursor particles; and sintering the abrasive grain precursor particles at temperatures below 1450° C. to obtain platelet shaped randomly shaped abrasive particles having a length to thickness ratio in the range between 2 and 10.The method according to claim 12, wherein the method comprises an additional step of crushing, screening and / or classifying the sintered platelet shaped randomly shaped abrasive particles to obtain abrasive particles having an average aspect ratio (AR) of less than 1.70, preferably less than 1.60.

Citation Information

Patent Citations

  • Non-fused aluminium oxide-based abrasive mineral, a process for its production and abrasive products comprising the said abrasive mineral

    EP0024099B1

  • Abrasive grains in the shape of platelets

    EP0318168B1

  • Shaped abrasive particles with low roundness factor

    US20100319269A1

  • Non-fused aluminum oxide-based abrasive mineral

    US4314827A

  • Abrasive grits formed of ceramic containing oxides of aluminum and rare earth metal, method of making and products made therewith

    US4881951A