Light-emitting diode chip and method for manufacturing a light-emitting diode chip

By applying a magnesium nitride and oxide passivation layer on the side surfaces of InGaAlP-based LED chips, the non-radiative recombinations caused by oxygen bonds are mitigated, enhancing the efficiency of the chips, especially in those with a small lateral extent.

DE102017112875B4Active Publication Date: 2024-10-10AMS OSRAM INT GMBH
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
DE102017112875
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2017-06-12
Publication Date
2024-10-10
Estimated Expiration
2037-06-12

AI Technical Summary

Technical Problem

Light-emitting diode chips based on InGaAlP suffer from non-radiative recombination of charge carriers on etched side surfaces due to oxygen-induced intermediate states in the band gap, leading to reduced efficiency, especially in chips with a small lateral extent.

Method used

Applying a passivation layer comprising magnesium nitride and magnesium oxide on the side surfaces of the epitaxial semiconductor layer sequence to replace oxygen bonds with nitrogen bonds, thereby reducing intermediate states and enhancing radiative recombination of charge carriers.

Benefits of technology

The passivation layer significantly increases the efficiency of the light-emitting diode chip by minimizing non-radiative recombinations, particularly in chips with a high ratio of side surface to light exit surface.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Light-emitting diode chip comprising: - an epitaxial semiconductor layer sequence (1) with an active zone (2) which generates electromagnetic radiation (S) during operation, and - a passivation layer (3) comprising magnesium oxide and magnesium nitride, wherein the passivation layer (3) is applied to a side surface (1c) of the semiconductor layer sequence (1) and the passivation layer (3) covers at least the active zone (2), wherein the passivation layer (3) comprising magnesium oxide and magnesium nitride has a common interface with the epitaxial semiconductor layer sequence (1), wherein - the epitaxial semiconductor layer sequence (1) is based on a III / V semiconductor composite material and the III / V semiconductor composite material is a phosphide semiconductor composite material.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] A light-emitting diode chip and a method for producing a light-emitting diode chip are specified.

[0002] Light-emitting diode chips, especially those based on InGaAlP, often have non-radiative Recombinations of charge carriers in the active radiation-generating zone on etched side surfaces have a low efficiency.

[0003] The document US 2010 / 0 270 570 A1 describes a light-emitting element.

[0004] The document US 2002 / 0 173 165 A1 describes the production of semiconductor materials and components with controlled electrical conductivity.

[0005] The document US 2012 / 0 202 304 A1 describes a III-nitride semiconductor device and a method for Fabrication of a III-nitride semiconductor device.

[0006] An object of the present application is to provide a light-emitting diode chip which, in comparison to the The present application also aims to provide a method for Manufacture of such a light-emitting diode chip.

[0007] These objects are achieved by a light-emitting diode chip having the features of patent claim 1 and by a Method solved with the steps of patent claim 8.

[0008] Advantageous embodiments and further developments of the light-emitting diode chip and the method are the subject the respective dependent claims.

[0009] A light-emitting diode chip is specified. The light-emitting diode chip comprises an epitaxial semiconductor layer sequence with an active zone that generates electromagnetic radiation when the LED chip is in operation.

[0010] According to at least one embodiment, the light-emitting diode chip comprises a passivation layer comprising or consisting of magnesium oxide and magnesium nitride. The passivation layer is applied to one side surface of the Semiconductor layer sequence is applied and covers at least the active zone of the epitaxial semiconductor layer sequence laterally.

[0011] According to at least one embodiment, the passivation layer comprises or consists of MgO and Mg N . 3 2

[0012] Furthermore, it is also possible for the passivation layer to extend over the entire side surface of the epitaxial Alternatively or additionally, the passivation layer can also be at least partially a first main surface, in particular a light exit surface of the epitaxial semiconductor layer sequence or the LED chips, can be arranged.

[0013] According to at least one embodiment, the passivation layer is in direct contact with a Semiconductor composite material of the epitaxial semiconductor layer sequence. In other words, the Passivation layer has a common interface with the epitaxial semiconductor layer sequence.

[0014] According to at least one embodiment, the side surface of the epitaxial semiconductor layer sequence is etched generated.

[0015] The inventors have found that on the side surfaces or side edges, in particular on etched Side surfaces of the active zone of the epitaxial semiconductor layer sequence increase non-radiative recombinations of Charge carriers, i.e. electrons and holes, take place. Especially on the side surfaces of the epitaxial Semiconductor layer sequence, non-saturated states are created by disruption of the crystal structure and thus free valences or bonding sites are saturated by the binding of oxygen. In other words, the semiconductor composite material is oxidized in the area of ​​the side surface of the semiconductor layer sequence. This creates intermediate states in the band gap, i.e. between the valence and conduction bands, which lead to non-radiative recombinations of charge carriers. As a result, these charge carriers are no longer available to generate electromagnetic radiation, which Reduction of radiation and thus the efficiency of the LED chip. The idea of ​​the present The aim of the application is to reduce the oxygen bonds of the semiconductor composite material on the side surfaces of the epitaxial semiconductor layer sequence, especially in the active zone, with other bonds in order to To avoid intermediate states in the band gap resulting from oxygen bonding or to For this purpose, a layer comprising or consisting of magnesium nitride is applied to the side surface of the Semiconductor layer sequence is applied and this covers at least the active zone of the epitaxial Semiconductor layer sequence laterally and completely. Since magnesium has a higher affinity for oxygen than that in a The elements contained in the semiconductor composite material are exchanged between oxygen and nitrogen and form at the interface to the epitaxial semiconductor layer sequence instead of the bin bonds to nitrogen. At the same time, a layer of comprising the magnesium nitride magnesium oxide and resulting in a passivation layer comprising or consisting of Magnesium nitride and magnesium oxide. In other words, at the interface of the epitaxial Semiconductor layer sequence and the layer comprising or consisting of magnesium nitride, a nitriding of the semiconductor composite material of the epitaxial semiconductor layer sequence. This allows the intermediate states in the band gap at the side surfaces of the semiconductor layer sequence in the area of ​​the active zone is avoided or significantly reduced, thereby increasing the radiative recombination of charge carriers in the active zone and thus the The efficiency of the LED chip is increased. In particular, a significant increase in efficiency can be observed when the LED chip has a small lateral dimension. Preferably, the LED chip has an edge length which does not exceed 500 µm, particularly preferably 100 µm.

[0016] According to at least one embodiment, on the side surface of the semiconductor layer sequence on which the passivation layer is arranged, and thus at the interface of the epitaxial semiconductor layer sequence and the Passivation layer nitrides of the semiconductor composite material. In other words, bonds of the semiconductor composite material to nitrogen.

[0017] According to one embodiment, the epitaxial semiconductor layer sequence is based on a III / V Semiconductor composite material.

[0018] The III / V semiconductor composite material is a phosphide semiconductor composite material. A phosphide Semiconductor composite material is a semiconductor composite material that contains phosphorus.

[0019] In a preferred embodiment, the III / V semiconductor composite material is a phosphide semiconductor composite material from the system In Al Ga P with 0 ≤ x ≤ 1, 0 ≤ y ≤ 1 and x+y ≤ 1. In particular, the epitaxially xy 1-xy The semiconductor layer sequence grown on the substrate comprises or consists of one of these materials. Magnesium with a standard electrode potential of E° = -2.7 V has a higher affinity to oxygen than Aluminum, gallium, phosphorus, and indium. For example, aluminum has a standard electrode potential of E° = -1.66 V. After applying the layer comprising or consisting of magnesium nitride on the side surface of the Semiconductor layer sequence involves nitriding of In Al Ga P with formation of indium nitrogen, aluminum xy 1-xy Nitrogen, gallium-nitrogen and / or phosphorus-nitrogen bonds on the side surface of the epitaxial At the same time, magnesium nitride forms in the layer, magnesium oxide and This results in a passivation layer comprising or consisting of magnesium nitride and magnesium oxide. Intermediate states in the band gap, which are formed by the oxygen bond to gallium, indium, phosphorus and / or aluminum, in particular through the bonding of oxygen to aluminium, can be avoided or reduced. This advantageously means that the LED chip has a very high efficiency.

[0020] According to at least one embodiment, the epitaxial semiconductor layer sequence at the interface to the Passivation layer indium-nitrogen, aluminum-nitrogen, phosphorus-nitrogen and / or gallium-nitrogen bonds on.

[0021] The passivation layer preferably has a layer thickness of between 1 nm and 1000 nm. nm, preferably between 5 nm and 100 nm inclusive.

[0022] The increase in efficiency is particularly effective in a light-emitting diode chip that has a comparatively high ratio The ratio of side surface to light exit surface of the LED chips is preferably at least 0.01.

[0023] According to at least one embodiment, a protective layer is provided over the passivation layer or consisting of silicon nitride, in particular comprising or consisting of Si N . This makes the 3 4 LED chip protected from oxygen and / or moisture.

[0024] According to at least one embodiment, the protective layer has a layer thickness of 1 nm to including 1000 nm, preferably from 5 nm up to and including 100 nm.

[0025] A method for producing a light-emitting diode chip is provided. All features of the light-emitting diode chip also apply to the process for manufacturing a light-emitting diode chip and vice versa.

[0026] The method for producing a light-emitting diode chip comprises the following steps, preferably in the specified order: A) Providing an epitaxially grown semiconductor layer sequence with an active zone suitable is to generate electromagnetic radiation, B) Applying a layer comprising or consisting of magnesium nitride to a side surface of the epitaxial semiconductor layer sequence. In particular, the layer is applied in such a way that it at least the active zone of the epitaxial semiconductor layer sequence is covered laterally. D) Annealing the composite produced in step B) comprising a semiconductor layer sequence and a layer comprising Magnesium nitride to form a passivation layer comprising magnesium oxide and magnesium nitride. Tempering temperature is preferably between 100 and 800 °C.

[0027] During the annealing in step D), nitriding of the semiconductor composite material of the epitaxial semiconductor layer sequence, over which the layer comprising or consisting of magnesium nitride was applied. Magnesium has a higher affinity for oxygen than the elements contained in a semiconductor composite material, In particular, an exchange of oxygen and nitrogen takes place and at the interface to the epitaxial semiconductor layer sequence instead of the bonds of the semiconductor composite material to the oxygen bonds to nitrogen. At the same time, magnesium nitride magnesium oxide forms in the layer and results a passivation layer comprising or consisting of magnesium nitride and magnesium oxide. The exchange of Oxygen and nitrogen are also removed due to the higher stability of magnesium oxide compared to magnesium nitride promoted.

[0028] According to at least one embodiment of the method, at least parts of the side surface of the Semiconductor layer sequences are created by etching, particularly by dry etching. This is also known as mesa etching. The side surface of the semiconductor layer sequence can initially be partially produced by etching, while a further Part of the side surface by another separation process, such as breaking, sawing or laser cutting, can be produced. Particularly preferably, the active zone of the semiconductor layer sequence is separated by etching.

[0029] According to at least one embodiment, the epitaxial semiconductor layer sequence is based on a phosphide Semiconductor composite material and in step D) at the interface between the semiconductor layer sequence and the Passivation layer indium-nitrogen, phosphorus-nitrogen, aluminum-nitrogen and / or gallium-nitrogen bonds In particular, after step D), no or hardly any indium-oxygen, phosphorus-oxygen, aluminum-oxygen and / or gallium-oxygen bonds at the interface between the semiconductor layer sequence and the passivation layer available.

[0030] According to at least one embodiment, the magnesium nitride is applied in step B) by sputtering.

[0031] According to at least one embodiment, the magnesium nitride in step B) is applied in direct contact to the side surface of the epitaxial semiconductor layer sequence.

[0032] According to at least one embodiment, a step C) takes place between step B) and step D): C) Applying a protective layer to the layer comprising or consisting of silicon nitride, preferably Si N . 3 4 If process step C) takes place, a composite produced in step C) is tempered in step D).

[0033] Further advantageous embodiments and developments of the invention will become apparent from the following in The embodiments described in connection with the figures.

[0034] In the embodiments and figures, identical, similar or equally effective components are each The elements shown and their relative sizes are not Rather, individual elements, especially layer thicknesses, can be adjusted for better Understanding may be exaggerated. Fig. 1A and Fig. 1B show LED chips without a passivation layer. Figures 2A to 2F schematically show a process for manufacturing a light-emitting diode chip. Fig. 3 shows a schematic side view of a light-emitting diode chip.

[0035] The light-emitting diode chip according to Fig. 1a has an epitaxially grown semiconductor layer sequence 1. The epitaxial semiconductor layer sequence 1 comprises an active zone 2 which is designed to be LED chips to generate electromagnetic radiation S. The epitaxial semiconductor layer sequence 1 is based preferably on a phosphide semiconductor composite material of the formula In Al Ga P with 0 ≤ x ≤ 1, 0 ≤ y ≤ 1 and xy 1-xy x+y ≤ 1. The side surface of the semiconductor layer sequence 1c was created by dry etching. The side surface 1c is characterized in this case by the fact that they are formed obliquely to a central axis of the LED chip. epitaxial semiconductor layer sequence 1 is arranged on a substrate 6, for example made of GaAs. In particular, the epitaxial semiconductor layer sequence 1 is arranged on a first main surface of the substrate 6a, while on a second main surface of the substrate 6b a second electrical contact 5 is arranged. Over a first main surface of the semiconductor layer sequence 1a, the in particular also represents the light exit surface, a first electrical contact 4 is arranged. For example, the first electrical contact 4 is a p-contact and the second electrical contact 5 is an n- Contact.

[0036] Fig. 1b shows the LED chip shown in Fig. 1a in operation. In particular, by etching the Side surfaces 1c, the crystal system or the crystal structure of the semiconductor material compound is disturbed and Free valences or bonding sites are created, which are saturated particularly by oxygen. In particular, aluminium-oxygen bonds are formed, since aluminium has a particularly high affinity to oxygen In the active zone 2 of the LED chip, negative charge carriers, i.e. electrons, and positive Charge carriers, i.e. holes, emitting electromagnetic radiation S. At the side surfaces of the active zone Non-radiative recombinations nS of the charge carriers occur more frequently. This is due to the formation of intermediate states within the band gap, which are formed by the oxygen-saturated free Bonding sites of the semiconductor composite material are formed. This leads to efficiency losses of the LED chip. This loss is particularly large when the LED chip has a small lateral dimension.

[0037] In the process shown in Figs. 2a to 2f, an epitaxially grown Semiconductor layer sequence 1 with an active zone 2 is provided. The active zone 2 is suitable for operation of the LED chip to generate electromagnetic radiation. The semiconductor layer sequence 1 is based on a Phosphide semiconductor composite material of the formula In Al Ga P with 0 ≤ x ≤ 1, 0 ≤ y ≤ 1 and x+y ≤ 1. The active xy 1-xy Zone 2 is preferably based on In Al Ga P with 0 < x < 1, 0 < y < 1 and x+y < 1, the n-conducting zone 7 on In Al P with 0 < xy 1-xy xy x < 1, 0 < y < 1 and x+y = 1 and the p-conducting zone 8 on In Al P with 0 < x < 1, 0 < y < 1 and x+y = 1. The side surface xy The semiconductor layer sequence 1c is produced by dry etching. The side surface 1c is inclined to a central axis of the LED chips. In particular, the etching of the side surface 1c creates the crystal system of the semiconductor material compound is interrupted or disturbed and free binding sites are created, which are Oxygen is saturated. In particular, indium-oxygen, aluminum-oxygen, gallium-oxygen and / or phosphorus-oxygen bonds. This leads to undesirable non-radiative recombinations of charge carriers through the formation of intermediate states within the band gap. This is illustrated in the energy diagram of Fig. 2b. There, the energy E of the valence band E and the V conduction band E of the semiconductor composite material of the active zone 2 and the gallium-oxygen bonds and C Intermediate states arising from aluminum-oxygen bonds within the band gap between valence and The loss of efficiency due to non-radiative recombinations of charge carriers is particularly during wet and dry etching of the side surfaces of the semiconductor layer sequence.

[0038] In the step of the method shown in Fig. 2c, a layer comprising or consisting of Magnesium nitride 10, preferably Mg N , over the entire surface 1c of the epitaxial semiconductor layer sequence 1 and 3 2 first main surface of the semiconductor layer sequence 1a, in particular the light exit surface, by sputtering. In particular, layer 10 laterally covers the active zone 2. In a next step, as shown in Fig. 2d, Optionally, a protective layer 9 is applied over the layer 10. The protective layer 9 is applied over the entire side surface the epitaxial semiconductor layer sequence 1c and first main surface 1a and comprises or consists of Silicon nitride.

[0039] In a next step of the process, the composite of epitaxial semiconductor layer sequence 1, layer 10 and protective layer 9 at a temperature of 100 to 800 °C, for example 300 °C. Magnesium has a higher affinity to oxygen than the elements aluminum, indium, contained in the semiconductor composite material. Gallium and phosphorus. During annealing, nitriding of the semiconductor compound material of the epitaxial Semiconductor layer sequence 1, over which the layer 10 is arranged, forming indium-nitrogen, aluminum- Nitrogen, gallium-nitrogen and / or phosphorus-nitrogen bonds. At the same time, magnesium oxide forms in the layer 10 and a passivation layer 3 comprising or consisting of of magnesium oxide and magnesium nitride, preferably MgO and MgN (Fig. 2e). This can advantageously produce the structures shown in Fig. 2b 3 2 shown intermediate states in the band gap at the side surface of the active zone 2a are avoided or significantly reduced, thereby increasing the radiative recombination of charge carriers in the active zone 2 and thus the Efficiency of the LED chip increases.

[0040] In a further step, the passivation layer 3 and the protective layer 9 can be at least partially removed from the first main surface 1a are removed, for example by etching, and a first electrical contact 4 on the first Main area 1a and applied in direct mechanical and electrical contact with it, as shown in Fig. 2f.

[0041] Fig. 3 shows an embodiment of a light-emitting diode chip. The light-emitting diode chip has an epitaxial grown semiconductor layer sequence 1. The epitaxial semiconductor layer sequence 1 comprises an active zone 2, which is arranged to generate electromagnetic radiation S during operation of the light-emitting diode chip, in particular with a wavelength of approximately 620 nanometers. The epitaxial semiconductor layer sequence 1 is preferably based on a phosphide Semiconductor compound material of the formula In Al Ga P with 0 ≤ x ≤ 1, 0 ≤ y ≤ 1 and x+y ≤ 1. The active zone 2 xy 1x-y is preferably based on In Al Ga P with In Al Ga P with 0 < x < 1, 0 < y < 1 and x+y < 1, the n-conducting zone 7 on In Al xy 1-x- yxy 1-xy x P with 0 < x < 1, 0 < y < 1 and x+y = 1 and the p-conducting zone 8 on In Al P with 0 < x < 1, 0 < y < 1 and x+y = 1. The yxy The side surface of the semiconductor layer sequence 1c is produced by dry etching. The side surface 1c is characterized in this case characterized by the fact that it is formed obliquely to a central axis of the LED chip. The epitaxial Semiconductor layer sequence 1 is arranged on a substrate 6, for example made of GaAs. In particular, the epitaxial Semiconductor layer sequence 1 is arranged on a first main surface of the substrate 6a, while on a second A second electrical contact 5 is arranged on the main surface of the substrate 6b. Above a first main surface of the Semiconductor layer sequence 1a, which in particular also represents the light exit surface, is a first electrical contact 4 The first electrical contact 4 is a p-contact and the second electrical contact 5 is an n-contact. On the Side surface of the epitaxial semiconductor layer sequence 1c and on parts of the first main surface of the Semiconductor layer sequence 1a is a passivation layer 3 comprising or consisting of magnesium oxide and Magnesium nitride is arranged. In particular, the passivation layer 3 extends over the side surface of the active zone 2a. The passivation layer 3 has, for example, a layer thickness of 50 nm. At the interface of the Semiconductor layer sequence 1 and the passivation layer 3 are indium-nitrogen, aluminum-nitrogen, gallium-nitrogen and / or phosphorus-nitrogen bonds are present. List of reference symbols 1 epitaxial semiconductor layer sequence or epitaxially grown semiconductor layer sequence 1a first main surface of the semiconductor layer sequence or light exit surface 1b second main surface of the semiconductor layer sequence 1c Side surface of the semiconductor layer sequence 2 active zones 2a Side surface of the active zone 3 Passivation layer 4 first electrical contact 5 second electrical contact 6 Substrat 6a first main surface of the substrate 6b second main surface of the substrate 7 n-conducting zone 8 p-conducting zone 9 Protective layer 10 layer comprising magnesium nitride S electromagnetic radiation E Energy Ec Energy Valence Band Ec energy conduction band nS non-radiative recombination

Claims

1. LED chip with: - an epitaxial semiconductor layer sequence (1) with an active zone (2) which, during operation, emits electromagnetic radiation (S) is generated, and - a passivation layer (3) comprising magnesium oxide and magnesium nitride, wherein the passivation layer (3) is a side surface (1c) of the semiconductor layer sequence (1) and the passivation layer (3) has at least the active zone (2), wherein the one passivation layer (3) comprising magnesium oxide and magnesium nitride is covered with the epitaxial semiconductor layer sequence (1) has a common interface, wherein - the epitaxial semiconductor layer sequence (1) is based on a III / V semiconductor composite material and the III / V Semiconductor composite material is a phosphide semiconductor composite material.

2. Light-emitting diode chip according to the preceding claim, wherein at an interface of the epitaxial semiconductor layer sequence (1) and the passivation layer (3) nitrides of the semiconductor composite material are present.

3. Light-emitting diode chip according to one of the preceding claims, wherein the phosphide semiconductor composite material is In Al Ga P xy 1-x-y with 0 ≤ x ≤ 1, 0 ≤ y ≤ 1 1 and x+y ≤ 1.

4. Light-emitting diode chip according to the preceding claim, wherein the semiconductor layer sequence (1) is the interface to the passivation layer (3) indium-nitrogen, aluminum-nitrogen, phosphorus-nitrogen and / or gallium nitrogen bonds.

5. Light-emitting diode chip according to one of the preceding claims, wherein the passivation layer (3) has a layer thickness of including 1 nm up to and including 1000 nm, preferably from and including 5 nm up to and including 100 nm.

6. Light-emitting diode chip according to one of the preceding claims, whose edge length is 500 µm, preferably 100 µm, not exceeds.

7. Light-emitting diode chip according to one of the preceding claims, wherein a protective layer (9) is provided over the passivation layer (3). comprising or consisting of silicon nitride.

8. A method for manufacturing a light-emitting diode chip comprising the following steps: A) Providing an epitaxial semiconductor layer sequence (1) with an active zone (2) which is suitable for to generate electromagnetic radiation (S), wherein the epitaxial semiconductor layer sequence (1) is based on a III / V semiconductor composite material and the III / V semiconductor composite material is a phosphide semiconductor composite material, B) applying a layer comprising magnesium nitride (10) to a side surface of the semiconductor layer sequence (1c), wherein the magnesium nitride is applied in direct contact to the side surface of the semiconductor layer sequence (1c), D) annealing the composite produced in step B) comprising semiconductor layer sequence (1) and layer comprising Magnesium nitride (10) for forming a passivation layer (3) comprising magnesium oxide and magnesium nitride.

9. Method according to the preceding claim, wherein the phosphide semiconductor composite material is In Al Ga P with 0 ≤ x ≤ xy 1-xy 1, 0 ≤ y ≤ 1 and x+y ≤ 1 and in step D) at the interface between the semiconductor layer sequence (1) and the passivation layer (3) indium-nitrogen, phosphorus-nitrogen, aluminum-nitrogen and / or gallium Form nitrogen bonds.

10. Method according to one of claims 8 or 9, wherein the side surface (1c) of the semiconductor layer sequence (1) is etching is produced.

11. A method according to any one of claims 8 to 10, wherein the magnesium nitride in step B) is applied by sputtering becomes.

12. The method according to any one of claims 8 to 11, wherein between step B) and step D) a step C) takes place: C) Applying a protective layer (9) to the layer comprising magnesium nitride (10).

Citation Information

Patent Citations

  • Fabrication of semiconductor materials and devices with controlled electrical conductivity

    US20020173165A1

  • Light emitting element

    US20100270570A1

  • Iii-nitride semiconductor laser device, and method of fabricating the iii- nitride semiconductor laser device

    US20120202304A1