Vacuum chamber, device and method

The vacuum chamber design with sealed welds and ambient-pressure cavities effectively prevents leaks and corrosion, maintaining high-vacuum integrity for lithography mask analysis and processing.

DE102023114526B3Active Publication Date: 2024-11-28CARL ZEISS SMS GMBH +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
DE102023114526
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-06-02
Publication Date
2024-11-28
Estimated Expiration
2043-06-02

AI Technical Summary

Technical Problem

Existing vacuum chambers for lithography masks suffer from virtual leaks and corrosion due to inadequate sealing at weld joints, leading to compromised vacuum integrity and potential contamination from ambient air.

Method used

A vacuum chamber design featuring first and second weld seams that seal the joint from the interior and environment, respectively, with a cavity or channel connected to the joint to maintain ambient pressure, allowing for easy detection and prevention of leaks through inert gas flow.

Benefits of technology

Ensures reliable vacuum maintenance and prevents corrosion by immediately detecting and addressing leaks, ensuring consistent high-vacuum conditions and reducing contamination risks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

vacuum chamber (110) for receiving a sample (1), in particular a lithography mask, especially for analyzing and / or processing the sample (10) or the lithography mask, comprising: a first and a second joining partner (200, 202), each made of a soft magnetic material and forming a butt joint (206) with each other; a first weld (212) that seals the joint (206) against an interior (214) of the vacuum chamber (110); a second weld (216) that seals the joint (206) against an environment (218) of the vacuum chamber (110); and at least a cavity (220) which is formed in the first and / or second joining partner (200, 202) is fluidly connected to the joint (206) and in which ambient pressure prevails.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a vacuum chamber for accommodating a sample, for example a lithography mask, in particular for analyzing and / or processing the sample or lithography mask. Furthermore, the present invention relates to a device for analyzing and / or processing a sample, in particular a lithography mask. The present invention further relates to a method for producing and / or operating a vacuum chamber for accommodating a sample, in particular a lithography mask.

[0002] Microlithography is used to manufacture microstructured components, such as integrated circuits. The microlithography process is carried out using a lithography system equipped with an illumination system and a projection system. The image of a mask (also called a reticle or lithography mask) illuminated by the illumination system is projected by the projection system onto a substrate, such as a silicon wafer, coated with a light-sensitive layer (photoresist) and arranged in the image plane of the projection system. This transfers the mask structure to the light-sensitive coating of the substrate.

[0003] The mask is used for a wide variety of exposures. Its defect-free state is therefore of utmost importance. Accordingly, considerable effort is put into inspecting the mask for defects and repairing any detected defects. Defects in such masks can be on the order of a few nanometers. Repairing such defects requires devices that offer very high spatial resolution for the repair processes.

[0004] Devices that activate local etching or deposition processes based on particle beam-induced processes are suitable for this purpose. For example, EP 1 587 128 B1 discloses such a device. According to this document, an electron beam from an electron microscope is used to trigger the chemical processes.

[0005] Devices such as those described in EP 1 587 128 B1 always have a vacuum chamber. A sample, such as a lithography mask, is placed in this chamber and exposed to the particle beam, for example, to trigger the etching or deposition processes described above or simply to capture an image of the sample.

[0006] To ensure that such particle beam-induced processes, for example based on electron beams or ion beams, can proceed unhindered, it is known to manufacture such vacuum chambers from soft magnetic steel. Soft magnetic steel, for example, is prone to corrosion compared to known stainless steel alloys. To prevent this, the vacuum chamber, which usually consists of several welded steel plates, is surface-coated. For example, it is known to create a nickel-phosphorus coating on the surfaces of the vacuum chamber by electrical, galvanic, or chemical nickel plating (the latter, for example, according to ISO 4527). However, such a coating does not penetrate, or only insufficiently penetrates, the joints of the vacuum chamber. Joints at butt joints, where, for example, two steel plates of the vacuum chamber are welded together, are particularly problematic.

[0007] A first state of the art is shown Fig. 5 illustrates the two soft magnetic steel plates 500, 502. These form a corner joint 504 with each other. The actual joint is designated 506 and is referred to below as the "joint". The two steel plates 500, 502 are welded together by means of a fillet weld 508. The fillet weld 508 is arranged in the corner area between the steel plates 500, 502, which corresponds to an interior space 510 of the vacuum chamber (in Fig. 5 not shown as a whole). The weld seam 508 seals the interior 510 against the environment 512 of the vacuum chamber by the joint 506 in Fig. 5 is closed on the left side by the weld seam 508. Opposite, the joint 506 is open. The corresponding point is marked with the reference numeral 514 in Fig. 5 marked.

[0008] During nickel plating, the galvanic liquid can only penetrate insufficiently through point 514 into the joint 506. Due to unevenness of the steel plates 500, 502 in the area of ​​the joint 506, as well as due to thermal distortion or other loads, a microscopic volume is always present in the area of ​​the joint 506. The galvanic liquid penetrates this volume only insufficiently, so that there is insufficient protection against corrosion. This can further lead to damage to the weld seam 508 and thus to leaks in the vacuum chamber. In particular, ambient air then flows through point 514, through the joint 506 and through the leak or a crack in the weld seam 508 into the vacuum chamber 510. The required vacuum of, for example, 10 -7 or 10 -8 mbar can then no longer be achieved. Furthermore, corrosion generates particles, meaning that cleanroom requirements in the interior of the 510-meter range can no longer be met.

[0009] Another approach known from the state of the art for producing a vacuum chamber is described in Fig. 6. An outer fillet weld 600 is welded opposite the inner fillet weld 508. This seals the joint 506 and the microscopic volume formed by it on both sides, i.e., toward the interior 510 and the surrounding area 512.

[0010] It becomes problematic if the inner weld seam 508, for example due to thermal stresses, has one or more cracks that make its cross-section permeable to gas. This creates a so-called virtual leak. This means that the enclosed microscopic volume in the joint 506 must also be pumped out if the desired vacuum is to be created in the interior 510. Likewise, the vacuum must be released again to remove the sample, so that the microscopic volume must be refilled through the weld seam 508 or the fluid path formed therein. To make matters worse, such a crack is almost impossible to detect using conventional testing methods. If, for example, helium is applied to the inside of the weld seam 508, it cannot be detected in the surrounding area 512 because the weld seam 600 ensures a corresponding seal.

[0011] Fig. 7 shows the Fig. 6, but with the difference that the outer weld seam 600 also has one or more cracks, i.e., its cross-section is gas-permeable. If helium is now supplied to the outside of the weld seam 600 via a nozzle 700, it can in principle be detected by the detector 702 on the inside of the weld seam 508. However, the amount of helium that diffuses through both cracks (i.e., in the outer and inner weld seams 600 and 508, respectively) is very small, and this also requires a long time. Therefore, cracks in the weld seams 508, 600 can hardly be practically detected.

[0012] KR 20140047893 A discloses a method for producing a vacuum chamber. Fig. In the process shown in Figure 3b, fillet welds 115, 125 are formed at a corner joint 110. An area 121 forms a collecting reservoir for galvanic liquid during electroplating of the vacuum chamber.

[0013] JP H09-297 738 A discloses a nuclear fuel rod in which end plugs are welded to both ends of a cladding tube. The cladding tube is filled with nuclear fuel. The end plug has a narrow end with a diameter smaller than the inner diameter of the cladding tube. The narrow end of the end plug is placed in one end of the cladding tube. A groove runs along the outer circumference of the narrow end of the end plug. When the end plug is welded on, the groove creates a round notch between the narrow end of the end plug and the end of the cladding tube to which it is connected.

[0014] Furthermore, US 5 269 894 A discloses a method for joining an arrangement intended for a vacuum process. The arrangement consists of a cooling plate having at least one recess and at least one bayonet connection point. A thermally conductive membrane is placed over each recess of the cooling plate. A closure plate, which also has at least one bayonet connection point, is connected to the cooling plate via the bayonet connection points of the two plates. The connection of the two plates via the bayonet connection point is created by a slight axial and rotational movement between the two plates. The closure plate is arranged over the recesses of the cooling plate. A coolant under increased pressure is supplied into the at least one recess of the cooling plate.

[0015] Furthermore, KR 10 2009 0 131 435 A is known from the prior art. This document discloses a welded construction constituting a vacuum chamber, wherein a horizontal section and a vertical section have an L-shaped step. The two L-shaped steps of the horizontal and vertical sections are joined together. The external joint of the two sections is joined by welding.

[0016] Against this background, it is an object of the present invention to provide an approach that is improved over the prior art.

[0017] Accordingly, a vacuum chamber is provided for accommodating a sample. The sample is, for example, a lithography mask. The vacuum chamber is particularly configured for analyzing and / or processing the sample or the lithography mask. The vacuum chamber comprises: a first and a second joining partner, each made of a soft magnetic material and forming a joint with each other; a first weld sealing the joint against an interior of the vacuum chamber; a second weld seam sealing the joint from the environment of the vacuum chamber; and at least one cavity which is formed in the first or in the second joining partner, is fluidly connected to the joint and in which ambient pressure prevails.

[0018] Advantageously, this solution eliminates any virtual leaks. As soon as the first weld develops a leak, gas (especially air or inert gas) flows through the corresponding crack in the first weld into the interior. This gas is at ambient pressure, so that no vacuum can be created in the interior of the vacuum chamber. In particular, a vacuum leak results in a pressure below atmospheric pressure.

[0019] The aforementioned analysis and / or processing of the sample can be carried out, for example, using an electron beam and / or ion beam. The particle source can be an electron or ion source. In particular, the analysis of the sample can include a meteorological measurement of a sample, in particular of imaging structures in the case of a lithography mask. The processing of the sample can, in particular, include the removal of one or more particles (such as contaminants) attached to the sample, for example, with a diameter of < 100, preferably < 10 µm.

[0020] The joining partners can each be manufactured as a single plate. Such a plate has, for example, a thickness of > 0.5, 1, or 2 cm. A soft magnetic material is understood, for example, to be a steel with a low carbon content and / or with added silicon. Soft magnetic steel is, in particular, E355, 1.0580 (standard EN 10305-4). The following alloys can be added: C up to a maximum of 0.22%, Si up to a maximum of 0.55%, Mn up to a maximum of 1.6%, P and S each up to a maximum of 0.025%.

[0021] Alternatively or additionally, a soft magnetic metal such as iron, cobalt and nickel (and alloys thereof) can be used instead of the soft magnetic steel.

[0022] In the "joint," the two joining partners are at least partially in contact with each other. In particular, a microscopic volume is formed between the first and second joining partners. This may arise, for example, from unevenness in the surface of the respective joining partners adjacent to the joint.

[0023] Preferably, the first and second weld seams are each continuous. This means that they extend in one piece over the entire length of the joint. A "one-piece" weld seam is understood here to mean a weld seam that is produced from one and the same material in a single (uninterrupted) welding process or an overlapping welding process (in which at least two adjacent weld seams overlap). This ensures the desired sealing of the joint. In particular, it can be provided that the first and / or second weld seam are each designed in the form of a closed ring that surrounds the vacuum chamber or its interior. The ring can have any shape, for example with straight and curved sections. The only decisive factor is that it is closed in order to ensure complete sealing.

[0024] The cavity can, for example, be more than ten, one hundred, one thousand, ten thousand, one hundred thousand, or a million times the microscopic volume of the joint (without the cavity). The cavity can be directly adjacent to the joint, so that the microscopic volume merges directly into the cavity, at least for a portion of the joint. In other variants, the cavity can be fluidically connected to the joint via a channel. "Fluidically connected" in this context refers to a gas- or liquid-conducting connection.

[0025] The ambient pressure, for example, is 1 bar. Depending on the altitude and temperature, the air pressure in the vicinity of the vacuum chamber and / or in the cavity may deviate from the aforementioned value.

[0026] According to one embodiment, the cavity is sealed from the environment.

[0027] This advantageously prevents moisture or other corrosion-promoting substances from the environment from penetrating the joint. This provides better protection for the first and second welds.

[0028] According to a further embodiment, the at least one cavity is designed as a channel.

[0029] The channel can be milled, for example. The channel can be U-shaped, for example, in the first and / or second joining partner. This means that the channel is preferably open toward an outer side of the first and / or second joining partner.

[0030] According to a further embodiment, the channel extends parallel to the first and / or second weld seam. The channel can extend over the entire length of the first and / or second weld seam.

[0031] According to a further embodiment, the cavity is or can be fluidically connected to the environment by means of at least one pilot bore or otherwise.

[0032] Gas from the environment can flow into the cavity via the pilot hole or other fluidic connection, particularly if the first weld (inner weld) is leaking (i.e., particularly during a leak test of the first weld). In other embodiments, the pilot hole can be closed and opened only for specific purposes. For example, inert gas can be introduced into the cavity via the pilot hole, for example, as part of a gas-tightness test of the welds.

[0033] According to one embodiment, the seal against the environment or the at least one pilot bore has an openable closure. This closure can be opened, for example, when inert gas is to be introduced into or refilled into the cavity.

[0034] According to a further embodiment, the cavity is filled with inert gas.

[0035] The inert gas can be helium, for example.

[0036] According to a further embodiment, a plurality of spaced-apart pilot bores are provided, each of which is connected to the cavity.

[0037] This allows, for example, helium to be introduced through one pilot hole and removed through the other, allowing helium to flow through the entire cavity or channel. This allows the helium to be guided along the inside of the first and / or second weld seam, allowing any crack or leak to be located there.

[0038] According to a further embodiment, two of the plurality of pilot bores are arranged at opposite ends of the channel.

[0039] This makes it particularly easy to test the first and / or second weld seam for leaks over its entire length.

[0040] According to a further embodiment, a plurality of channels are provided between the first and second joining partners, wherein the channels are provided fluidically separated from one another in the first and / or second joining partner.

[0041] By providing multiple, fluidically separated channels, the leak test, in which inert gas, particularly helium, flows through each channel, can be limited to one channel and thus to a section of the first and / or second joining partner. This accelerates troubleshooting.

[0042] According to a further embodiment, the channels are arranged in a direction parallel to the first and / or second weld seam.

[0043] This means that one channel can be assigned to each weld section.

[0044] According to a further embodiment, the channels extend in the direction parallel to the first and / or second weld seam.

[0045] This makes it possible to initially detect a leak using the first channel. If such a leak is detected, the search can be refined by passing inert gas through the first channel. If no crack is detected there, inert gas can be passed through the third channel.

[0046] According to a further embodiment, the joining partners are arranged in a corner joint or T-joint. For example, the joining partners can be arranged or meet at an angle of 90° to each other.

[0047] According to a further embodiment, the first and / or second weld seam is formed as a fillet weld.

[0048] According to a further aspect, a device for analyzing and / or processing a sample, in particular a lithography mask, is provided. The device comprises: a particle beam source configured to generate a particle beam; a vacuum chamber as described above in which the sample is arranged; and a detection device for detecting particles backscattered from the sample.

[0049] The particle beam source is, in particular, an electron beam or ion beam source. The detection device is, in particular, a so-called ESB detector (ESB: "Energy Selective Backscatter") and / or an SE detector (SE: "Secondary Electron"). The ESB detector is configured to detect backscattered electrons from the electron beam. To do so, the ESB detector detects electrons with energies starting at, for example, 200 eV. The ESB detector is configured to detect secondary electrons. These are electrons knocked out of the sample, in particular the lithography mask, by the electron beam with an energy of up to, for example, 50 eV.

[0050] According to yet another aspect, a method for producing and / or operating a vacuum chamber for accommodating a sample is provided. The sample is, in particular, a lithography mask. The method comprises the following steps: Forming at least one cavity in the first and / or second joining partner made of a soft magnetic material; Arranging the first and / or second joining partner in a joint, wherein the at least one cavity is fluidly connected to the joint; Creating a first weld seam that seals the joint from an interior of the vacuum chamber; Creating a second weld that seals the joint from the environment of the vacuum chamber; and Setting ambient pressure in the at least one cavity.

[0051] The cavity can be created, for example, by milling. Furthermore, a pilot hole can be provided that connects the cavity to the surrounding area.

[0052] The establishment of ambient pressure in the at least one cavity can be at least temporary. This means that the cavity is connected to the environment so that ambient pressure is established there. The cavity is then sealed with a closure. The closure can be openable.

[0053] According to a further embodiment, the cavity is filled with an inert gas, and then a leak test is carried out in the interior of the vacuum chamber and / or in its surroundings.

[0054] For example, these steps can be carried out after the vacuum chamber has been manufactured and before it is put into operation (i.e., to accommodate a sample for analysis and / or processing). If the first and second weld seams then prove to be leak-tight, the vacuum chamber can be put into operation. The leak test can, for example, involve the use of a nozzle and a detector. An inert gas, in particular helium, is sprayed through the nozzle. The inert gas is detected via the detector if a crack is present in the first or second weld seam. The nozzle and the detector are arranged on different sides of the vacuum chamber, i.e., either the detector in the interior or the nozzle in the surrounding area, or vice versa.

[0055] The aspects described for the vacuum chamber apply accordingly to the device and method described above, and vice versa.

[0056] In this case, "one" is not necessarily limited to a single element. Rather, multiple elements, such as two, three, or more, may also be included. Any other counting term used here should not be understood as implying a limitation to the exact number of elements stated. Rather, numerical deviations upwards and downwards are possible, unless otherwise stated. Furthermore, the described method steps may also be performed in a different order than the one specified, unless otherwise stated.

[0057] Further possible implementations of the invention also include combinations of features or embodiments described above or below with respect to the exemplary embodiments that are not explicitly mentioned. In this case, the person skilled in the art will also add individual aspects as improvements or additions to the respective basic form of the invention.

[0058] Further advantageous embodiments and aspects of the invention are the subject of the dependent claims and the exemplary embodiments of the invention described below. The invention will be explained in more detail below using preferred embodiments with reference to the accompanying figures. Fig. 1 shows a schematic view of a processing arrangement for checking and / or repairing a lithography mask; Fig. 2 shows in a section II from Fig. 1 a section through the vacuum chamber of the processing arrangement Fig. 1; Fig. 3 shows a flowchart of a method according to an embodiment; Fig. 4 shows different possibilities for the formation of channels; and Fig. 5 - Fig. 7 show various state-of-the-art solutions.

[0059] In the figures, identical or functionally equivalent elements have been provided with the same reference numerals where indicated. Furthermore, it should be noted that the illustrative figures are not necessarily to scale.

[0060] Fig. Figure 1 schematically shows an embodiment of a processing arrangement 100, which is embodied, for example, in the form of a scanning electron microscope. The processing arrangement 100 serves to inspect and / or repair a sample, for example, a lithography mask 10. The lithography mask 10 is intended, for example, for use in an EUV or DUV lithography system (not shown).

[0061] The processing arrangement 100 comprises an electron beam column 102. This has an electron source 104, which generates an electron beam 106. The electron beam 106 strikes the lithography mask 10. Backscattered electrons are detected by a detection device 108 of the electron beam column 102. This allows a high-resolution image of the lithography mask 10 to be generated (electron beam microscope).

[0062] The electron beam column 102 is arranged in a vacuum chamber 110. The same applies to the lithography mask 10, which is arranged on a sample table 112 below the electron beam column 102. The vacuum within the vacuum chamber 110 is generated by means of a vacuum pump 114. For example, a residual gas pressure of 10· 7 mbar to 10 -8 mbar.

[0063] The electron beam column 102 can perform electron beam-induced processing (EBIP) in conjunction with supplied process gases, which are supplied, for example, from a gas supply unit 116 from the outside via a gas line 118 into the region of a focal point of the electron beam 106. This includes, in particular, depositing material onto or etching material from the lithography mask 10. A control computer 120 of the processing arrangement 100 is, in particular, configured to suitably control the electron beam column 102, the sample stage 112, and the gas supply unit 116 for this purpose. In particular, a computer program 122 is stored on the control computer 120, which controls the processing arrangement 100 for this purpose.

[0064] Instead of the electron beam column 102, an ion beam column or another particle beam source could also be provided.

[0065] Fig. 2 shows in a section II from Fig. 1 a partial section through the vacuum chamber 110. In the partial section of the Fig. 2 shows that the vacuum chamber is composed in a partial area of ​​at least a first and a second joining partner 200, 202. The joining partners 200, 202 are formed, for example, from a plate material, such as rectangular plates. The vacuum chamber can also be formed from a tube with a lid and base (not shown). Fig. 2 they are shown in section, where the plate thickness D 200 , D 202 can be seen. The Thick D 200 , D 202are, for example, > 0.5, 1, 2, or 5 cm. The joining partners 200, 202 are made, for example, from a soft magnetic steel or other soft magnetic material, in particular metal. These form a butt joint with one another, in this example a corner joint 204. In other embodiments, a T-joint can also be formed. In particular, the joining partner 202 abuts the joining partner 200 at a right angle. The butt joint is designated by the reference numeral 206. In the butt joint, the joining partner 202 rests with its end face 208 against a broad side 210 of the joining partner 200.

[0066] A weld seam 212, which is formed, for example, as a fillet weld, connects the joining partners 200, 202 on their inner side, i.e., on the side facing an interior space 214 enclosed by the vacuum chamber 110. The weld seam 212 is also referred to herein as an inner weld seam and seals the joint 206 from the interior space 214.

[0067] Furthermore, a second weld seam 216 is provided, which connects the joining partners 200, 202 on their outer side, i.e., on the side facing an environment 218 of the vacuum chamber 110. The second weld seam 216 is also referred to herein as an outer weld seam and can also be designed as a fillet weld. The weld seams 212, 216 are preferably designed as continuous weld seams and extend across the entire component width of the joining partners 200, 202, wherein the width direction corresponds to the direction perpendicular to the plane of the paper.

[0068] In the first and / or second joining partner 200, 202 - in the exemplary embodiment in the joining partner 200 - a cavity is formed, which is manufactured here as a channel 220. The channel 220 is in cross section in Fig. 2 and extends (perpendicular to the plane of the paper) parallel to the weld seams 212, 216. In the exemplary embodiment, the channel 220 directly adjoins the joint 206 and is thus fluidly connected to it, that is. For example, an inert gas located in the cavity or channel 220 passes directly into the joint 206. In particular, a gas passes from the channel 220 via a respective contact area 222 or 224, which form part of the joint 206, to the weld seam 212 or to the weld seam 216. In the contact area 222 or 224, the end face 208 of the joining partner 202 lies directly against the broad side 210 of the joining partner 200, apart from unevennesses that lead to a microscopic volume through which gas can flow from the channel 220 to the weld seams 212, 216.In one embodiment, the cavity 220 could also be spaced apart from the joint 206 and connected to it via a fluid-conducting channel.

[0069] How to continue in Fig. 2, a pilot bore 226 is provided, which extends from an outer broad side 228 opposite the broad side 210 of the joining partner 200 to the channel 220. Gas at ambient pressure (1 bar) can flow into the channel 220 or into it via the pilot bore 226. If, for example, the inner weld seam 212 is defective, this immediately leads to a subsequent flow of ambient air when a vacuum is created in the interior space 214, so that no so-called virtual leak occurs, but rather a real one, i.e., the interior space 214 cannot be pumped out. As a result, the leak is immediately detected and can be repaired. Pumping out a virtual leak is thus reliably avoided.

[0070] In embodiments, the pilot bore can be closed and opened with a resealable closure. For example, a screw 230 can be screwed into the pilot bore 226 to seal it gas-tight. Further functions, in particular of the pilot bore or the screw 230, are described below. Fig. 3 clearly.

[0071] Fig. 3 shows in one embodiment a method for producing the vacuum chamber from the Fig. 1 and Fig. 2. In a first step S1, the cavity, in particular the channel 220, is created in the joining partner 200. For this purpose, it is milled, for example, into the broad side 210 (step S1). Subsequently, the pilot hole 226 can be drilled.

[0072] Subsequently, the joining partner 202 is arranged with its end face 208 on the width 210, in such a way that its end face 208 completely covers the channel 220 in its width direction as well as in its depth direction (corresponding to the direction perpendicular to the plane of the paper). Thus, the corner joint 204 is formed, in which the channel 220 is fluidly connected to the joint 206. This corresponds to step S2 of Fig. 3.

[0073] In a step S3, the weld seam 212 is created and in a step S4 the weld seam 216. These seal the joint in the thickness direction (see thickness D202 in Fig. 2) off.

[0074] In a step S5, an ambient pressure is established in the channel 220. This pressure is created simply by filling the channel 220 with ambient air (and then sealing it if necessary) during the manufacture of the vacuum chamber 110.

[0075] After step S5, the channel 220 is filled with inert gas in a step S6. In a step S7, a leak test is then carried out in the interior 214 of the vacuum chamber 110. For this purpose, for example, the method described in connection with Fig. 7, the detector 702 can be introduced into the interior space 214. This then detects leaks in the weld seam 212, through which inert gas from the channel 220 passes through the contact area 222 and through the weld seam 212 into the interior space 214. In this way, leak tests of the weld seam 212 can be carried out effectively.

[0076] Additionally or alternatively, the weld seam 216 may be inspected in the same manner, in which case the detector 702 is guided in the area adjacent to the weld seam 216.

[0077] If the weld seams 212, 216 prove to be sealed in steps S6 and S7, the channel 220 can, for example, be refilled with inert gas (optional). In any case, as long as inert gas is still present in the channel 220, the pilot bore 226 is sealed with the screw 230 (step S8).

[0078] The vacuum chamber 110 can then be put into operation. For this purpose, it is, for example, installed in the device 100. During operation, for example when the sample 10 (see Fig. 1) is arranged in the vacuum chamber 110 and is analyzed or processed there, inert gas is available in the channel 220 and displaces moisture or other corrosion-promoting substances, which, for example, can escape from the contact surfaces 222, 224 via cracks in the outer weld seam 216 (which form, for example, due to thermal deformation or other loads over time). In this way, corrosion is reliably avoided in the long term.

[0079] Fig. 4 shows in a plan view of the broad side 210 the joining partner 200 from Fig. 2, where Fig. 4 different embodiments for the design of the channel 220 and the pilot bore 226 are explained and shown integrated in one figure. On the right side, the pilot bore 226 is connected to the channel 220 essentially according to the Fig. 2. Furthermore, it is shown on the right-hand side that a further pilot bore 400 can be provided in addition to the pilot bore 226. The pilot bores 226 and 400 are each located at one end of the channel 220. Thus, for example, inert gas can be supplied via the bore 226 and discharged via the pilot bore 400, or vice versa.

[0080] In the lower area in Fig. Figure 4 shows an embodiment with two adjacent channels 402, 404, which can each be ventilated via pilot holes 406, 408, 410 and 412 at their respective ends. The channels 402, 404 are arranged collinearly with respect to a direction designated by R. The direction R corresponds to the course of the Fig. 4 weld seams 212, 216 not shown. This means that the channels 402, 404 each extend parallel to these weld seams.

[0081] On the left side is Fig.4 shows an embodiment with a channel having three pilot bores. In addition to the two pilot bores 416, 418 at its end, a pilot bore 420 is provided in the center. By, for example, supplying the inert gas via bore 416 and discharging it via bore 420, a segmented test or leak test can be performed. If a leak is detected in this configuration, it can be assumed that this results from a crack in a weld seam 212, 216 located in the area between the pilot bores 416, 420. The leak test is then repeated, with the inert gas being supplied via bore 420 and discharging it via bore 418. If a leak is detected here, a leak in one of the weld seams 212, 216 can be attributed to the section between the pilot bores 418 and 420.

[0082] It is important that the channels—for example, channels 402 and 404—are fluidically separated from each other, so that applying inert gas to one channel 402 does not result in the application of inert gas to the other channel 404, and vice versa. This allows for safe testing segment by segment.

[0083] Although the present invention has been described using exemplary embodiments, it can be modified in many ways. LIST OF REFERENCE SYMBOLS 10 Lithography mask 100 processing arrangement 102 electron column 104 electron source 106 electron beam 108 detector unit 110 vacuum housings 112 Sample table 114 Vacuum pump 116 Gas supply unit 118 Gas pipeline 120 tax calculators 122 Computer program product 200 joining partners 202 joining partners 204 Corner kick 206 shock 208 front side 210 Broadside 212 Weld seam 214 Surroundings 216 Weld seam 218 Surroundings 220 channel 222 Investment area 224 Investment area 226 pilot drilling 228 Broadside 400 pilot drilling 402 channel 404 channel 406 Pilot bore 408 pilot bore 410 pilot hole 412 pilot bore 414 Channel 416 pilot hole 418 pilot bore 420 pilot hole 500 steel plate 502 steel plate 504 Corner kick 506 shock 508 Weld seam 510 interior 512 surroundings 514 Area 600 weld seam 700 nozzle 702 Detector D 200 thickness D 202 thickness R direction S1 - S8 process steps

Claims

[1] Vacuum chamber (110) for receiving a sample (10), comprising: a first and a second joining partner (200, 202), each made of a soft magnetic material and forming a joint (206) with each other; a first weld seam (212) sealing the joint (206) from an interior space (214) of the vacuum chamber (110); a second weld seam (216) sealing the joint (206) from an environment (218) of the vacuum chamber (110); and at least one cavity (220) which is formed in the first and / or second joining partner (200, 202), is fluidly connected to the joint (206) and in which ambient pressure prevails. [2] Vacuum chamber according to claim 1, wherein the at least one cavity (220) is sealed from the environment (218). [3] Vacuum chamber according to claim 1 or 2, wherein the at least one cavity (220) is formed as a channel and / or extends parallel to the first and / or second weld seam (212, 216). [4] Vacuum chamber according to one of claims 1 to 3, wherein the cavity (220) is or can be fluidically connected to the environment (218) by means of at least one pilot bore (226). [5] Vacuum chamber according to one of claims 2 to 4, wherein the seal to the environment (218) or the at least one pilot bore (226) has an openable closure (230). [6] Vacuum chamber according to one of claims 1 to 5, wherein the cavity (220) is filled with an inert gas. [7] Vacuum chamber according to one of claims 4 to 6, wherein a plurality of spaced-apart pilot bores (226, 400) are provided, each of which is connected to the cavity (220). [8] Vacuum chamber according to claim 7, wherein two of the plurality of pilot bores (226, 400) are arranged at opposite ends of the channel (220). [9] Vacuum chamber according to one of claims 3 to 8, wherein a plurality of channels (402, 404) are provided between the first and second joining partners (200, 202), wherein the channels (402, 404) are provided fluidically separated from one another in the first and / or second joining partner (200, 202). [10] Vacuum chamber according to claim 9, wherein the channels (402, 404) are arranged in a row in the direction (R) parallel to the first and / or second weld seam (212, 216) and / or extend along this direction (R). [11] Vacuum chamber according to one of claims 1 to 10, wherein the joining partners (200, 202) are arranged in a corner joint (204) or T-joint to one another and / or the first and / or second weld seam (212, 216) is designed as a fillet weld. [12] Device (100) for analyzing and / or processing a sample (10), comprising: a particle beam source (104) configured to generate a particle beam (106); a vacuum chamber (110) according to one of claims 1 to 11, in which the sample (10) is arranged; and a detection device (108) for detecting particles backscattered from the sample (10). [13] Method for producing and / or operating a vacuum chamber (110) for receiving a sample (10), comprising the steps: Forming (S1) at least one cavity (220) in a first and / or second joining partner (200, 202) from a soft magnetic material; Arranging (S2) the first and second joining partners (200, 202) in a joint (206), wherein the at least one cavity (220) is fluidly connected to the joint (206); Creating (S3) a first weld seam (212) which seals the joint (206) from an interior space (214) of the vacuum chamber (110); Creating (S4) a second weld seam (216) which seals the joint (206) from an environment (218) of the vacuum chamber (110); and Setting (S5) ambient pressure in the at least one cavity (220). [14] The method of claim 13, wherein: the cavity (220) is filled with an inert gas and then a leak test is carried out in the interior (214) of the vacuum chamber (110) and / or in its surroundings (218), and / or the cavity (220) is filled with an inert gas before the sample (10) is placed in the interior (214) of the vacuum chamber (110). [15] Method according to claim 14, wherein the cavity (220) is sealed from the environment (218) of the vacuum chamber (110) by means of a closure (230) after filling with the inert gas.

Citation Information

Patent Citations

  • Apparatus and method for investigating or modifying a surface with a beam of charged particles

    EP1587128B1

  • Portable information terminal equipment, screen transiting method and data managing method

    JP1997297738A

  • Vacuum chamber

    KR1020140047893A

  • Nuclear fuel rod

    JP1997297192A

  • Welding structure of vacuum chamber

    KR1020090131435A