Method for producing a decorative element adorned with a Lichtenberg figure

By connecting a laminating layer with the decorative layer before or after burning the Lichtenberg figure, the method addresses the mechanical cohesion issue in thin decorative layers, ensuring stability and quality in automotive decorative parts.

DE102023119077B3Active Publication Date: 2024-10-24JOYSONQUIN AUTOMOTIVE SYST GMBH
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
DE102023119077
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-07-19
Publication Date
2024-10-24
Estimated Expiration
2043-07-19

AI Technical Summary

Technical Problem

The use of Lichtenberg figures in thin decorative layers for automotive applications is hindered by the formation of island-shaped areas that lose mechanical cohesion, leading to reduced stability and quality issues during processing.

Method used

A method involving a decorative layer connected with a laminating layer to ensure mechanical cohesion, either before or after the Lichtenberg figure is burned, ensuring the layer's stability and preventing island-shaped areas from detaching.

Benefits of technology

The method allows for high-quality decorative surfaces with Lichtenberg figures on thin decorative layers, maintaining mechanical stability without complex manual work, suitable for automotive applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The invention relates to a method for producing a decorative part comprising the steps of: providing a decorative layer having a first, electrically conductive surface and a second surface facing away from the first surface; bringing two or more electrodes into contact with the first surface; and applying an electrical voltage between the electrodes so that an electric current flows between the electrodes and a pattern is burned into the first surface. According to a first embodiment of the invention, the method is characterized in that the decorative layer is bonded to a laminate layer on the second surface before the electrical voltage is applied.According to a second embodiment of the invention, the method is characterized in that the decorative layer has a predetermined minimum thickness; the decorative layer is bonded to a laminating layer after the application of an electrical voltage to the first surface; and after bonding the laminating layer, the material of the decorative layer is removed from the second surface, so that the thickness of the decorative layer is reduced to a predetermined maximum thickness. The invention also provides a decorative element comprising a decorative layer, characterized in that the decorative layer has a first surface and a second surface facing away from the first surface; the decorative layer has a pattern generated by an electrical discharge on the first surface; and the first or the second surface is bonded to a laminating layer.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a method for producing a [product / service] decorated with a Lichtenberg figure decorative part as well as a decorative part that can be produced by this process. State of the art

[0002] In automotive manufacturing, decorative elements with different decorative patterns are known, which are, for example, made by means of Printed designs can be produced. However, for technical reasons, these designs are not individualized in most cases. but regularly and repeating from decorative element to decorative element. However, there is an interest in irregular, “naturally” grown decorative patterns that give the decorative element an individual character lend.

[0003] One method for producing irregular patterns on a surface consists of using an electrical discharge to burn a pattern into an electrically conductive surface. The resulting patterns are then classified according to their The discoverer, the naturalist Lichtenberg, is also referred to as Lichtenberg figures.

[0004] Lichtenberg figures can be produced, for example, on wooden surfaces. For this purpose, two or More electrodes were placed on the wood surface and subjected to an electrical voltage. Before this step The wood surface can be moistened with an electrolyte solution to increase conductivity. Provided the voltage If the voltage is high enough, a current flows between the electrodes, which, along its constantly changing path, The underlying material is decomposed by heat and discharge. This process creates channel-shaped depressions in the treated surface. These indentations form irregular, tree-like branching patterns, which are considered very decorative. These patterns are naturally unique, so that no two Lichtenberg figures are exactly alike.

[0005] In automotive manufacturing, decorative elements are used in particular for the decorative design of the interior. The decorative elements typically consist of a decorative layer and one or more components bonded to the decorative layer. connected additional layers, such as carrier and cover layers made of plastic. In the majority of cases In some cases, the decorative parts used in automotive manufacturing are narrow and long, exhibiting a large length-to-weight ratio. Width. This general format is advantageous for the use of Lichtenberg figures, as the patterns of the Lichtenberg- Figures extend along the connecting line between the two electrodes, thus forming a narrow, elongated shape. Cover the area.

[0006] One problem that hinders the use of Lichtenberg figures in such decorative elements arises However, this means that the decorative layers in question must be as thin as possible. For example, in In automotive manufacturing, wood veneers only a few millimeters thick are used for the decorative layer of a decorative element. When Lichtenberg figures are burned into such a thin decorative layer, the burned-in channels can extend across the entire thickness. the decorative layer can be penetrated. This leads to reduced stability of the decorative layer. In particular, the problem is that that the initially separated, channel-shaped depressions of the Lichtenberg figures reunite. In this process, island-shaped areas of the decorative layer are separated, which therefore no longer have any mechanical cohesion with the remaining decorative layer. This can be a hindrance when further processing the decorative layer into a decorative part. because the island-shaped areas either fall out of the decorative layer during further processing and thus impairing the quality of the decorative surface or requiring laborious manual placement. must be. Technical task

[0007] It is an object of the present invention to provide a method for producing decorative parts which for example, they can be used as decorative parts in automotive manufacturing. The decorative parts should be thin, with a The Lichtenberg figure features a decorative layer. The process should be carried out without unnecessary manual labor. and create high-quality decorative surfaces. Description of the invention

[0008] This problem is solved by a method for producing a decorative part and a decorative part according to the independent claims resolved.

[0009] The invention is based on the basic idea of ​​a decorative layer into which a Lichtenberg figure is burned or It is to be joined with a laminating layer. The laminating layer ensures the mechanical cohesion of the Decorative layer. In particular, the laminating layer connects island-shaped areas of the decorative layer, which are fired during the curing process. Lichtenberg figures can be created with the remaining decorative layer. This enables a manufacturing process that This ensures a high quality decorative surface without elaborate manual work. Manufacturing process

[0010] The invention provides two variants of a method for manufacturing a decorative part.

[0011] In a first embodiment, the invention relates to a method for producing a decorative part comprising the steps: Providing a decorative layer that consists of a first, electrically conductive surface and a second, non-conductive surface. has a surface facing away from the surface; Bringing two or more electrodes into contact with the first surface; Applying an electrical voltage between the electrodes, so that an electric current flows between them. Electrodes flow and a pattern is burned into the first surface.

[0012] The method according to the first variant is characterized in that The decorative layer is bonded to a laminating layer on the second surface before the electrical voltage is applied. becomes.

[0013] With this variant of the method, it is possible to produce a pattern in the form of a Lichtberg figure of high quality in to bake on a decorative layer, even if the decorative layer is extremely thin. This is achieved by the fact that The decorative layer is bonded to a backing layer before the electrical voltage is applied. The backing layer gives The decorative layer provides the necessary mechanical stability and prevents island-shaped areas from falling out. can form during the burning of the pattern.

[0014] In a second embodiment, the invention relates to a method for producing a decorative part comprising the steps: Providing a decorative layer that consists of a first, electrically conductive surface and a second, non-conductive surface. has a surface facing away from the surface; Contacting two or more electrodes with the first surface; and Applying an electrical voltage between the electrodes, so that an electric current flows between them. Electrodes flow and a pattern is burned into the first surface.

[0015] The method according to the second variant is characterized in that the decorative layer has a predetermined minimum thickness; The decorative layer is bonded to a laminating layer after the application of electrical voltage to the first surface. will; and After bonding the lamination layer, the material of the decorative layer is removed from the second surface, so that the thickness of the decorative layer is reduced to a predetermined maximum thickness.

[0016] With this variant of the method, it is possible to produce a high-quality pattern in the form of a Lichtberg figure in a to bake on the decorative layer while simultaneously obtaining a decorative layer of the required thickness. This is achieved by This ensures that the pattern is first burned into a decorative layer with a predetermined minimum thickness. Preferably, the minimum thickness of the decorative layer is chosen so that no damage occurs during the firing of the pattern. Island-like areas form that no longer have mechanical cohesion with the rest of the decorative layer. Following this, the material of the decorative layer is removed from the surface facing away from the pattern in order to create a to obtain a decorative layer with the desired maximum thickness. Since this process again creates island-like areas in If imperfections can form in the decorative layer that are no longer connected to the rest of the decorative layer, the decorative layer will be damaged. previously bonded to a laminating layer, which gives the decorative layer the necessary mechanical stability and the The island-shaped areas are prevented from falling out.

[0017] Both variants of the method result in a decorative part that is decorated with a Lichtenberg figure The decorative layer is bonded to a stabilizing laminate layer. (As a Lichtenberg figure) This refers to the pattern created by the electrical discharge on the first surface.

[0018] The decorative layer can be made of any material suitable for firing Lichtenberg figures. For example, the decorative layer can be made of plastic or wood, with wood being a particularly preferred material. Preferably, the decorative layer is a wood veneer, preferably a solid wood veneer.

[0019] The decorative layer has two opposing main surfaces, which within the scope of this invention are referred to as the first and The second surface is designated. These main surfaces are opposite each other and each has a opposite directions. The first surface is the main surface that is in contact with the electrodes in The pattern is then burned into the surface. The first surface of the finished decorative piece is... preferably facing the viewer and thus defines the visible side of the decorative element. The second surface is preferably turned away from the viewer and thus defines the support side of the decorative element. However, it is also possible to that Mus to burn so deeply into the decorative layer that it becomes visible on the second surface as well. In this case, the The decorative layer in the finished decorative part should also be arranged so that the second surface faces the viewer. and defines the visible side, while the first surface defines the support side.

[0020] The first and second surfaces are preferably, but not necessarily, rectangular. It is also possible to that the surfaces have different basic shapes. For example, the surfaces can be round, oval, It may be kidney-shaped, trapezoidal, or in the form of a polygon.

[0021] The decorative layer is preferably plate-shaped. This means that the decorative layer extends in length- and is greater in the lateral direction than in the depth direction. In the context of this invention, the depth direction is defined as that which The direction is designated as the one extending perpendicular to the first surface. The depth direction corresponds to the thickness of the Decorative layer.

[0022] According to the first variant of the method, the decorative layer is preferably thin. Preferably, the Decorative layer with a thickness of 100 mm or less, 50 mm or less, 20 mm or less, 10 mm or less, 5 mm or less, or 2 mm or less. The thinner the decorative layer, the lighter and more space-saving it can be. It is a decorative element. To ensure the mechanical stability of the decorative layer, the thickness of the decorative layer is... preferably at least 0.1 mm or more, 0.5 mm or more, 1 mm or more, 2 mm or more, or 5 mm or more. The decorative layer can, for example, have a thickness ranging from 0.1 mm to 100 mm, 0.5 mm to 50 mm, 1 mm to 20 mm, or 2 mm to 10 mm.

[0023] In the second variant of the process, a relatively thick decorative layer is processed first. The decorative layer Therefore, in this variant, it has a predetermined minimum thickness. The minimum thickness of the decorative layer is chosen as follows: that no island-like areas form in the decorative layer during the firing of the pattern, which do not have any mechanical resistance It has more cohesion with the rest of the decorative layer. There is a localized penetration of the decorative layer's thickness. This is possible through the fired-in pattern, provided that it does not completely separate the decorative layer from the rest of the surface. Island-shaped areas are created. Preferably, the thickness of the decorative layer is chosen so that the fired-on pattern is visible. not, i.e., not penetrating the entire thickness of the decorative layer at any point. Preferably, the The decorative layer must have a minimum thickness of at least 10 mm or more, 20 mm or more, 50 mm or more, 100 mm. or more, or 200 mm or more. The maximum thickness of the decorative layer before firing the pattern is determined by of minor importance. It should be limited to avoid removing unnecessary material. Preferably The decorative layer therefore has a thickness of 500 mm or less.

[0024] After firing the pattern and bonding it to the laminate layer, the thickness of the decorative layer is determined during the The second variant of the process reduces the thickness by removing material to a predetermined maximum thickness. The maximum thickness can, for example, be chosen so that the pattern burned into the first surface is also visible on the second. The opposite second surface is at least partially visible. Preferably, the decorative layer has, after the Removing material with a thickness of 100 mm or less, 50 mm or less, 20 mm or less, 10 mm or less, 5 mm or less, or 2 mm or less. To ensure the mechanical stability of the decorative layer, The thickness of the decorative layer after removal is preferably at least 0.1 mm or more, 0.5 mm or more, 1 mm or more, 2 mm or more, or 5 mm or more. The decorative layer can, for example, be a [missing word] after removal. Thicknesses in the range of 0.1 mm to 100 mm, 0.5 mm to 50 mm, 1 mm to 20 mm, or 2 mm to 10 mm.

[0025] The removal of material after joining the lamination layer according to the second variant of the method can for example, by sanding or planing the decorative layer from the second surface. Alternatively, the The decorative layer can also be cut or sawn into two partial layers parallel to the first surface. The one with the The first partial layer, bonded to the lamination layer, then forms the decorative element. The partial layer separated from the first surface can be used for a further round of the procedure.

[0026] According to the invention, a laminating layer is bonded to the first or second surface of the decorative part. In the case In the first variant of the process, the laminating layer is bonded to the second surface before the pattern is applied to the The first surface is fired on. According to the second variant of the process, the laminating layer is fired on with the first. Surface bonded after the pattern was burned into the first surface and before the material of the The decorative layer is removed from the second surface.

[0027] The laminating layer is preferably bonded over its entire surface to the first or second surface of the decorative part. This means that the laminating layer covers the entire surface in length and The decorative layer covers the width direction without leaving any gaps. This ensures that all, potentially Separated areas of the decorative layer are held together by the lamination layer.

[0028] The lamination layer preferably consists of an electrically insulating material. The material is preferably such that ensure that it is not damaged, deformed, or discolored as a result of electrical discharge.

[0029] The material of the laminating layer is preferably translucent. The material can be completely transparent or only partially transparent. be partially translucent or allow light to pass through. This is particularly important when the lamination layer is applied to the The first surface of the decorative layer is applied, and this surface is intended to define the visible side of the decorative part. Thus This ensures that the pattern on the first surface remains visible through the lamination layer.

[0030] However, the laminating layer can also be applied to the carrier side of the decorative part. This can, for example, This would then be the case if the laminating layer is bonded to the first surface according to the second variant of the procedure. the thickness of the decorative layer is chosen so that the burned-in pattern becomes visible on the second surface. In this case, the first surface and the laminated layer applied to it can define the substrate of the decorative element. while the second surface defines the visible side. Similarly, a method according to the first variant can be applied to the The second surface is defined by the lamination layer attached to the carrier side.

[0031] When the laminating layer is applied to the carrier side of the decorative part, it can consist of an opaque or a It should consist of a translucent material. Preferably, it should also consist of a translucent material in this case. This makes it possible to illuminate the decorative layer through the lamination layer.

[0032] The lamination layer can be made, for example, of nonwovens, woven fabrics, fibrous materials (e.g., paper) or plastic. consist of. A polyimide or a polyimide-containing composition is preferably used as the plastic. The laminating layer preferably consists of a plastic film or a fabric or nonwoven fabric on an inorganic basis, preferably made of a polyimide-based plastic film or a fiberglass fleece. The plastic film can be applied before the The decorative layer is produced, for example, by extrusion or injection molding and then applied to the decorative layer. can be applied. However, it is also possible to apply the plastic film directly to the surface by injection molding, as described below. to apply the surface of the decorative layer.

[0033] In a preferred embodiment, the laminating layer consists of an injection-molded plastic. Preferably, a polyimide or a polyimide-containing composition is used for this purpose. The plastic can for example, it can be applied directly to the surface of the decorative layer by injection molding. This has proved to be a particularly advantageous manufacturing process, as it enables the production of decorative parts with great precision. Precision and high-volume production are possible. Furthermore, applying the laminate layer by injection molding has the advantage that The molten plastic penetrates the recesses of the baked-on pattern and seals them. This results in greater mechanical reinforcement of the decorative layer and therefore greater durability of the decorative part. made possible.

[0034] The plastic can either be applied to the second surface of the [ ] according to the first variant of the method decorative layer or, according to the second variant of the process, on the first surface of the decorative layer can be applied. Even when applied to the second surface, the plastic can fill the indentations of the Seal the fired-in pattern if the pattern is fired so deeply into the decorative layer that openings to the second surface and the plastic can flow through these openings.

[0035] In a preferred embodiment of the invention, the indentations of the burned-in pattern are according to the The pattern is baked on and filled with a sealing material. This can be, as described above, the The material applied in a molten state is the laminating layer. However, it can also be an additional material. The purpose is to be used. The sealing material is preferably applied to the first surface in liquid form. The decorative layer is applied and then hardens. In the first variant of the process, the Sealing material after bonding the decorative layer to the lamination layer and after firing the pattern. applied to the first surface of the decorative layer. In the second variant of the process, the Sealing material after the pattern has been baked on, but before joining the first surface to the Laminating layer applied, provided the sealing material is not the material of the laminating layer itself is.

[0036] In particular, light-transmitting resins or plastics can be used as sealing material. Thermoplastic compositions that are in a molten state are particularly suitable. The mold is filled into the recesses of the pattern and hardens upon cooling. Inorganic materials are also used. Compounds, especially cement- or ceramic-like substances, are suitable as sealing materials. Furthermore, Metals are also used, applied in molten form. This is especially true for decorative layers made of... Tin, which is non-toxic to humans and has a relatively low melting point of 231°C, is a suitable material for wood. The sealant can be poured into channels and hardens there. It can also contain additives and / or fillers, such as... for example, particles, fibers or pigments.

[0037] After the application of the sealing material, further processing is preferably carried out, for example by sanding the first surface so that the sealing material and the surface of the decorative layer are in contact with each other become flush with the surface.

[0038] The shape of the burned-in pattern can be determined in particular by the applied voltage, the shape of the electrodes and the nature of the first surface is affected.

[0039] In principle, either direct or alternating current can be used to burn in the pattern. The applied Electrical voltage influences the shape of the pattern. A higher voltage, for example, results in deeper patterns. Broader patterns. Conversely, lower tension results in a more branched, delicate, and shallower pattern. Pattern.

[0040] Two or more electrodes are used to burn in the pattern. Preferably exactly two Electrodes were used.

[0041] The electrodes used for burning in the pattern can have different shapes, so that This results in differently shaped contact surfaces between the electrode and the surface of the decorative layer. For example, the contact area between an electrode and the surface of the decorative layer can be point-like or It must be elongated. The point-like contact surface is essentially a circular or square area. A contact surface is defined as one where the ratio of length to width is approximately 1. An elongated contact surface is defined as an area denoted as a length-to-width ratio greater than 1, in particular greater than 2, greater than 5 or greater than 10 is. An elongated contact surface can, for example, have the shape of an elongated oval or rectangle.

[0042] By combining differently shaped contact surfaces, the shape of the Lichtenberg figure can be determined. influence. For example, if an electrode with a point-shaped contact surface (a "point-shaped electrode") is used When combined with an electrode with an elongated contact surface (an "elongated electrode"), the pattern of Lichtenberg figure when applying an electrical voltage from the point-shaped electrode towards the elongated one Electrode. In this case, the elongated electrode is preferably arranged such that the longitudinal direction of the The contact area extends at a right angle to the connecting line between the two electrodes. If two point-shaped electrodes are used... When electrodes are combined, the pattern grows from each electrode in the direction of the other. Electrode. Preferably, at least one of the electrodes used has a point-shaped contact surface.

[0043] In order for a pattern to be burned into the surface of the decorative layer when electrical voltage is applied, This surface must be electrically conductive. Electrical conductivity can be achieved, in particular, by applying a coating. The electrolyte solution on the first surface is affected. Preferably, salt solutions or other solutions are used here. Aqueous electrolyte solutions are used. In a preferred embodiment, the first surface is prepared before the Contact with the electrodes, moistened with an aqueous electrolyte solution.

[0044] Following the above-described method, the decorative part can be further processed. In particular Additional layers can be bonded to the decorative element. For example, a translucent top layer can be applied. The visible side of the decorative element is applied to protect the decorative layer from external influences, especially mechanical ones. to protect against stress and / or UV radiation. Furthermore, the backing of the decorative element can be coated with a carrier layer. be connected.

[0045] In a preferred embodiment, the decorative part is added after the pattern has been fired on and the connection with the laminating layer is cut to fit the areas where the electrodes were placed on the decorative layer. remove. decorative part

[0046] The invention also provides a decorative part. The decorative part comprises a decorative layer and is therefore characterized by the fact that the decorative layer has a first surface and a second surface facing away from the first surface. surface; the decorative layer a pattern created by an electrical discharge on the first surface exhibits; and the first or second surface is bonded to a lamination layer.

[0047] The decorative part can be manufactured using the method described above.

[0048] The decorative part according to the invention is characterized in particular by a small thickness of the decorative layer. The thickness of the decorative layer is preferably 100 mm or less, 50 mm or less, 20 mm or less, 10 mm or less, 5 mm or less, or 2 mm or less.

[0049] Preferably the thickness is in a range of 0.1 mm to 100 mm, 0.5 mm to 50 mm, 1 mm to 20 mm, or 2 mm to 10 mm.

[0050] The decorative part according to the invention is in particular a decorative part for a vehicle interior. For example, it can The component in this function serves as part of the interior trim of a vehicle interior. It can, for example, be used in It can be used on motor vehicles, especially cars and trucks, trains and aircraft. The decorative part is suitable especially as part of the dashboard, door trim or roof lining of vehicle interiors. Furthermore, the component can also be used as wall cladding in buildings or as part of furniture. become. Examples of implementation

[0051] The present invention is described below with reference to exemplary embodiments in conjunction with the following The drawings are explained in more detail. The drawings show: Fig. 1: An example of a typical Lichtenberg figure Fig. 2: A schematic setup according to an embodiment of the method according to the invention. Fig. 3: A schematic setup according to a further embodiment of the method according to the invention. Fig. 4: A schematic setup according to Fig. 2 after the application of electrical voltage Fig. 5: A schematic setup according to Fig. 3 after the application of electrical voltage Fig. 6: A decorative part according to the invention Fig. 7: An intermediate step of the second variant of the method according to the invention Fig. 8: A further intermediate step of the second variant of the method according to the invention

[0052] Fig. 1 shows an example of a typical Lichtenberg figure. This corresponds to the pattern associated with the The process can be obtained according to the invention.

[0053] Fig. 2 shows a schematic setup for the method according to the invention. In this embodiment, a The decorative layer (1) is brought into contact with two electrodes (4). In this embodiment, the decorative layer (1) consists of made from a wood veneer. The electrodes (4) are placed on the first surface (6) of the decorative layer (1). The second surface of the decorative layer (1) is not shown in this example. It lies on the side facing away from the viewer. Side of the decorative layer (1). In the illustrated embodiment, both electrodes (4) have a point-shaped Contact surface with the first surface (6). Both electrodes are electrically connected to a voltage source (5). In this embodiment, the first surface (6) was treated with an aqueous solution before the electrodes (4) were attached. wetted with electrolyte solution.

[0054] Fig. 3 shows a schematic setup according to a further embodiment of the invention. Procedure. The setup corresponds to that of Fig. 2, however, instead of one of the point-shaped electrodes (4) an electrode (7) with an elongated contact surface is inserted.

[0055] Figures 4 and 5 show the two embodiments according to Figures 2 and 3 after the application of a electrical voltage. Fig. 4 corresponds to the setup according to Fig. 2, whereby two result from the electrical discharge. Lichtenberg figures (8) have formed, extending from both electrodes (4) towards the other electrode. extend. Fig. 5 corresponds to the setup according to Fig. 3. In this embodiment, only one Lichtenberg figure has formed. formed, extending from the point-like to the elongated electrode.

[0056] Fig. 6 shows a decorative part according to the invention in a top view of the first surface of the decorative layer (1), which is coated with It is decorated with two Lichtenberg figures. This decorative element can be obtained by constructing it according to Figures 2 and 4. In this embodiment, the decorative part is cut along the dividing lines (9) to separate the areas with the Remove the contact points of the two point-shaped electrodes. The layer of lamination is not shown in this illustration. It can be either with the first surface facing the viewer or the second surface facing away from the viewer. be connected.

[0057] Figures 7 and 8 illustrate the second variant of the manufacturing process according to the invention.

[0058] Fig. 7 shows a decorative layer (10) with a pattern (8) in the form of a fired-on Lichtenberg figure according to the second variant of the invention measured process. The decorative layer (10) in this case consists of a relatively thick wooden board. The thickness of the In this example, the decorative layer (10) is chosen such that the pattern (8) does not cover the entire thickness of the decorative layer (10). penetrates.

[0059] Fig. 8 shows a cross-sectional view of the decorative layer (10) according to Fig. 7 along the plane A:A after the Applying a sealant (12) and bonding the first surface with a laminating layer (11). In this example, the recesses of the pattern (8) are filled with the sealing material (12). The laminating layer (11) is with the first surface of the decorative layer (10). The first decorative layer (10) is bonded after the The lamination layer (11) is separated into two sub-layers along the dividing line (9), with the upper sub-layer having the pattern (8), which The sealing material (12) and the laminating layer (11) are included. The upper sub-layer can be manufactured so thinly, that the indentations of the pattern (8) penetrate the entire thickness of the sublayer. Through the previously connected The laminating layer (11) ensures the mechanical stability of the sublayer and thus the quality of the pattern (8). List of reference symbols 1.10 decorative layer 4 Electrode with point-shaped contact surface 5 Voltage source 6 First surface 7 Electrode with elongated contact surface 8 patterns 9 dividing line 11 layers of concealment 12 Sealing material

Claims

1. A method for producing a decorative part comprising the steps: Providing a decorative layer (1) having a first, electrically conductive surface (6) and a second, surface (6) facing away from the surface; Bringing two or more electrodes (4, 7) into contact with the first surface (6); Applying an electrical voltage between the electrodes so that an electrical current flows between the electrodes (4, 7) flows and a pattern (8) is burned into the first surface (6); characterized in that the decorative layer (1) before applying the electrical voltage on the second surface with a lamination layer (11) is connected.

2. A method for producing a decorative part comprising the steps: Providing a decorative layer (1, 10) having a first, electrically conductive surface (6) and a second, surface facing away from the surface; Bringing two or more electrodes (4, 7) into contact with the first surface (6); Applying an electrical voltage between the electrodes (4, 7) so that an electrical current flows between the electrodes (4, 7) and a pattern (8) is burned into the first surface (6); characterized in that the decorative layer (1, 10) has a predetermined minimum thickness; the decorative layer (1, 10) after applying the electrical voltage on the first surface (6) with a lamination layer (11) is connected; and after joining the lamination layer (11), the material of the decorative layer (1, 10) is removed from the second surface so that the thickness of the decorative layer (1, 10) is reduced to a predetermined maximum thickness.

3. Method according to claim 2, characterized in that the predetermined maximum thickness is selected so that the pattern (8) becomes visible on the second surface.

4. Method according to one of claims 2 and 3, characterized in that the predetermined minimum thickness of the Decorative layer (1, 10) is selected so that the firing of the pattern (8) does not result in island-shaped areas which no longer have any mechanical cohesion with the rest of the decorative layer (1, 10).

5. Method according to one of claims 1 to 4, characterized in that the lamination layer (11) consists of an electrically insulating material.

6. Method according to one of claims 1 to 5, characterized in that the lamination layer (11) consists of a made of translucent material.

7. Method according to one of claims 1 to 6, characterized in that the lamination layer (11) consists of a Plastic film or a fabric or nonwoven fabric on an inorganic basis, preferably made of a plastic film on polyimide base or a glass fiber fleece.

8. Method according to one of claims 1 to 7, characterized in that the lamination layer (11) consists of a injection-molded plastic.

9. Method according to one of claims 1 to 8, characterized in that the contact surface between the first surface (6) and a first electrode (4) is point-shaped and the contact area between the first surface (6) and a second electrode (7) is elongated.

10. Method according to one of claims 1 to 9, characterized in that the first surface (6) before the Bringing into contact with the electrodes (4, 7) is wetted with an aqueous electrolyte solution.

11. Decorative part comprising a decorative layer (1, 10), wherein the decorative layer (1, 10) has a first surface (6) and a second surface facing away from the first surface has; the decorative layer (1, 10) has a pattern (8) produced by an electrical discharge on the first surface (6); and the first surface (6) or the second surface is connected to a lamination layer (11).

Citation Information

Patent Citations

  • Method for obtaining Lichtenberg figures by utilizing electron beam irradiation

    CN109535453A

  • Wooden product superficial spark discharge fractal carving method

    CN111703245A

  • Impact device for high-energy electron beam irradiation manufacturing of Lichberg pattern

    CN114953412A

  • Method of decorating wood and wood-like products

    US4064386A

  • Method of controlling discharge of stored electric charge in plastic objects and forming Lichtenberg figures in plastic objects