Device for providing electromagnetic radiation
The use of a conversion element with phosphors embedded in a condensed metal phosphate matrix addresses overheating issues in phosphor-based systems, enabling efficient and durable high-energy radiation conversion for miniaturized applications.
Patent Information
- Application Number
- DE112013000135
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2012-06-18
- Filing Date
- 2013-06-12
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2033-06-12
AI Technical Summary
Existing phosphor-based radiation conversion systems face challenges with miniaturization due to overheating and inefficient heat dissipation, leading to potential damage and reduced efficiency, especially in applications requiring high-energy excitation radiation.
A device using a conversion element with phosphors embedded in a condensed metal phosphate matrix, which provides improved thermal conductivity and resistance to environmental factors, allowing for high-energy excitation radiation conversion without direct contact with the radiation source.
The solution enables efficient conversion of high-energy excitation radiation into desired conversion radiation with enhanced thermal stability and longevity, facilitating miniaturization and reducing the risk of phosphor damage.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[0001] The invention relates to a device for providing electromagnetic radiation. The device comprises a radiation arrangement for generating excitation radiation and at least one conversion element for generating conversion radiation. The conversion element comprises phosphors and is arranged at a distance from the radiation arrangement in a beam path of the excitation radiation.
[0002] DE 10 2010 028 776 A1 describes an optoelectronic semiconductor component with a component made of metal phosphate, which is essentially free of alkali-containing and halogen-containing components and is used in particular as an adhesive.
[0003] WO 2010 / 003 763 A1 describes a radiation-emitting device for emitting variable electromagnetic secondary radiation in a radiation direction, comprising in particular at least one radiation-emitting component which emits electromagnetic primary radiation during operation, a reflector which is arranged in the beam path of the radiation-emitting component and which has a first wavelength conversion substance for at least partially converting the primary radiation into electromagnetic conversion radiation, and a diaphragm which is variable in its orientation relative to the radiation-emitting component and to the reflector, wherein by changing the orientation of the diaphragm the secondary radiation can be changed by changing the proportion of the primary radiation which is emitted by the radiation-emitting component onto the first wavelength conversion substance and by changing the emitted conversion radiation.
[0004] DE 10 2009 003 936 A1 describes an electrical component with a light-emitting component, on whose radiation exit surface a converter ceramic is arranged for converting the wavelength of the radiation emitted by the light-emitting component. DE 10 2009 016 953 A1 describes conversion modules arranged adjacent to one another in a conversion unit in at least one arrangement direction to form a conversion arrangement for converting electrical energy into radiant energy or vice versa on a scalable scale.
[0005] Today, modern lighting systems increasingly utilize energy-efficient, high-intensity, and / or high-density radiation sources such as high-performance LEDs (light-emitting diodes), lasers, for example in the form of laser diodes, and / or superluminescent diodes. Unlike incandescent bulbs, which are thermal emitters, these radiation sources emit light in a narrowly defined spectral range, so their light is nearly monochrome or even exactly monochrome. One way to exploit additional spectral ranges is, for example, radiation conversion, in which phosphors are irradiated by LEDs and / or laser diodes, which in turn emit radiation of a different wavelength.In so-called "remote phosphor" applications, for example, a layer containing a phosphor located at a distance from a radiation source is typically illuminated by LEDs or laser diodes and in turn emits radiation of a different wavelength. For example, this technique can be used to convert light from blue LEDs into white light by adding yellow light, which is generated by exciting a layer containing a phosphor.
[0006] Furthermore, projectors are regularly used today to optically display data. Such a projector projects the data to be displayed in the form of individual still and / or moving images onto a screen, for example. It is known to generate the necessary excitation radiation in a conventional projector using a conventional discharge lamp, such as a high-pressure mercury vapor lamp. Recently, however, LARP (Laser Activated Remote Phosphor) technology has also been used. With this technology, a conversion element, which comprises or consists of phosphor and is arranged at a distance from the radiation source, is irradiated with excitation radiation, in particular an excitation beam (pump beam, pump laser beam).The excitation radiation from the excitation beam is fully or partially absorbed by the phosphor and converted into conversion radiation (emission radiation), whose wavelengths and thus spectral properties and / or color are determined by the conversion properties of the phosphor. In downconversion, the excitation radiation from the radiation source is converted by the irradiated phosphor into conversion radiation with longer wavelengths than the excitation radiation. For example, with the help of the conversion element, blue excitation radiation (blue laser light) can be converted into red or green conversion radiation (conversion light, illumination light).
[0007] The excitation radiation can introduce a high amount of energy into the conversion element, which can cause it to heat up considerably. This can lead to damage to the conversion element and / or the phosphors it contains, which can be present as a single phosphor or a phosphor mixture. Furthermore, if the phosphor is not cooled sufficiently, conversion losses occur due to reduced efficiency caused by thermal quenching. To avoid excessive heating and the associated potential damage to the conversion element or phosphor, it is known to arrange several conversion elements on a phosphor wheel (often referred to as a phosphor wheel, pump wheel, or color wheel), which is irradiated with the excitation beam while it rotates. Due to the rotation, different conversion elements and / or regions of the conversion elements are illuminated one after the other, thus distributing the introduced light energy over the entire surface.
[0008] To date, the degree of miniaturization in LARP technology has been limited due to its design, as the arrangement of the radiation source (pump laser) and the phosphor wheel requires a lot of space. However, a small installation space is desirable for various applications, for example, in the field of pico projection, i.e., small-sized mobile projectors, and / or miniaturized projection units in so-called embedded projection, where the projection unit is integrated into a mobile phone or camera, for example. The thermal connection of the conversion element is important to prevent overheating and damage.
[0009] For remote phosphor applications, thin phosphor layers such as cubic silicate minerals, orthosilicates, garnets, or nitrides are applied to the surfaces of corresponding substrates. The phosphor layers are usually mechanically fixed with binders and connected to an optical system (lenses, collimators, etc.), whereby the light coupling can occur, for example, via air or by means of an immersion medium. To ensure the best possible optical connection between the optical system and the phosphor and to avoid light losses, the most direct optical connection possible should be ensured. For remote phosphor applications, i.e. applications in which the phosphor and the radiation source, e.g.High-power laser diodes, for example, are spatially separated, a thin phosphor layer is applied to a surface, for example a substrate and / or a carrier, mechanically fixed with binders and connected to an optical system (lenses, collimators, etc.) (air, immersion, etc.).
[0010] In the aforementioned applications, the phosphors are usually excited to emit light using LEDs and / or laser diodes with high light outputs. The resulting thermal losses must be dissipated, for example via the carrier, to prevent overheating and thus thermally induced changes in the optical properties or even destruction of the phosphor. The phosphors are excited to emit light using high-power density light sources (several W / mm²), for example. The resulting high thermal losses (Stokes) lead to heat input into the phosphor layer. If these temperatures become too high, for example due to insufficient heat dissipation, this can lead to thermally induced changes in the optical properties (emission wavelength, conversion efficiency, etc.) or ultimately to the destruction of the phosphors or the layer itself.This degradation of the phosphor layer can be caused by both the phosphor and the binder. Therefore, the phosphor layer should be designed to allow optimal heat dissipation to prevent thermal destruction of the phosphors and the binder.
[0011] The phosphors, which are usually in powder form, do not form mechanically stable layers, i.e. no abrasion and / or scratch-resistant layers, without the additional use of binders such as silicones. Binders are also generally used to combine the phosphor particles into a phase which can then be applied to corresponding surfaces. When binders are used to stabilize the layer, however, these binders themselves can interact with the phosphors and thus negatively influence their optical and thermal properties, as well as their service life. In addition, the thermal conductivity of the binders often represents a limiting factor in the dissipation of heat generated in the conversion element. In addition, the binders themselves should be thermally and spectrally stable and show little to no aging properties.For this reason, the use of an inert, optically transparent, thermally and spectrally stable binder is advantageous for the production of stable and longer-lasting phosphor layers.
[0012] It is known to use silicones as binder matrices for photonic excitation (e.g., LEDs). However, these do not allow for excessively high light outputs (power densities of a few W / mm2) or require additional technological effort (e.g., color wheels to reduce the light exposure time). The known phosphor silicone mixtures are usually applied directly to metallic substrates. For example, the phosphor is suspended in organic matrices such as silicone and then screen-printed. The layers are, for example, approximately 30 µm thick. Silicone has poor thermal conductivity (λ Silikon= 0.1-0.2 W / m·K), which causes the phosphor to heat up more during operation and thus become less efficient. This is particularly problematic for high-power LEDs and laser applications.
[0013] The coating process for forming a phosphor layer is limited by the nature of the substrate materials. High-temperature processes on many plastics and metallic materials (e.g., aluminum) are unfeasible due to their melting temperatures and thermal resistance. Alternative, highly thermally conductive ceramic materials (e.g., AlN) are available, but they involve increased technological and financial effort.
[0014] Inorganic matrices with improved heat dissipation are known from various publications, such as low-melting glass from WO 2011 / 104364A1 or metal phosphates from WO 2011 / 138169 Al.
[0015] However, inorganic matrices have the disadvantage compared to organic matrices that relatively high temperatures are generally required to achieve a compact, bubble-free layer if a certain chemical stability (for example, against UV radiation and / or moisture) is required. Typical softening temperatures of common low-melting glasses are between 500°C and 600°C. At these temperatures, optoelectronic substrates such as LED chips or highly reflective substrates such as highly reflective aluminum or the phosphor to be embedded, especially nitrides, are already damaged and thus become less efficient.
[0016] Conversion elements made of a ceramic containing the phosphor or of a crystal containing the phosphor are known alternatives. In particular, the phosphor can form the ceramic or crystal. Such conversion elements can be glued to heat sinks so that the heat generated within them can be dissipated. A limiting factor for heat dissipation is the thermal conductivity of the adhesive used. Furthermore, it is beneficial for good heat dissipation if the conversion elements are made particularly thin.
[0017] In various embodiments, a device for providing electromagnetic radiation is provided that is simple and / or cost-effective to manufacture and / or that enables the provision of conversion radiation with high-energy excitation radiation. Furthermore, in various embodiments, a device for providing electromagnetic radiation is provided whose conversion element is temperature- and weather-resistant and / or has high efficiency and / or a long service life.
[0018] In various embodiments, a device for providing electromagnetic radiation is provided. The device comprises a radiation arrangement for generating excitation radiation and at least one conversion element for generating conversion radiation. The conversion element comprises a condensed metal phosphate and phosphors embedded in the condensed metal phosphate. The conversion element is arranged at a predetermined distance from the radiation arrangement in a beam path of the excitation radiation.
[0019] The conversion element, and thus the device, can be manufactured easily and / or inexpensively. The condensed metal phosphate enables the conversion element to be used to generate conversion radiation with high-energy excitation radiation. In other words, the radiation arrangement can comprise one, two, or more radiation sources that generate the excitation radiation with a high power density. Furthermore, the conversion element comprising the condensed metal phosphate is particularly temperature- and weather-resistant and has high efficiency and a long service life, since the condensed metal phosphate provides improved radiation resistance, for example, UV resistance, and heat dissipation, and the embedded phosphor is less damaged by environmental factors.
[0020] The condensed metal phosphate is a binder for the phosphor, which, for example, is in powder form, i.e., as phosphor powder, prior to binding with the metal phosphate. In other words, the metal phosphate forms a matrix for embedding the phosphor. The phosphor has a multitude of phosphor particles embedded in the matrix. The matrix can be produced from a condensed metal phosphate solution. Producing the matrix from a condensed metal phosphate solution allows the phosphor powder to be embedded at lower temperatures, with the same matrix composition, compared to a glass matrix, which can be produced, for example, by melting the raw materials. This can contribute to embedding the phosphor gently and / or causing less or no damage during embedding.
[0021] The different process temperatures become apparent when compared to glass produced via a melting process. The following process steps are carried out: - Batch production from raw materials, - Glass production by melting the mixture, - rapid cooling of the melt, if necessary by frit and if necessary production of a glass powder by grinding.
[0022] By increasing the temperature, this glass or the glass powder can be softened.
[0023] In contrast, sol-gel is a polymerization process, meaning compounds dissolved in liquids (e.g., metal phosphate) crosslink when the temperature rises, possibly releasing byproducts. The release of water is a condensation reaction. The temperatures required for crosslinking are significantly lower than the temperature required for resoftening of glass produced from the melt.
[0024] The specified distance is greater than zero, which means, for example, that the radiation source and the conversion element have no direct physical contact with each other.
[0025] The conversion element can, for example, have a conversion layer, which can be formed, for example, on a substrate. With the help of the metal phosphate, a particularly adhesive conversion layer can be created. The conversion layer can also be designed such that it is not subject to mechanical damage and / or destruction during subsequent processing steps. Furthermore, the conversion layer can be produced at moderate temperatures. For example, the temperatures can be further reduced by adding additives. The conversion element with the condensed metal phosphate can exhibit good chemical and / or optical resistance, good thermal conductivity, and / or temperature stability.This enables good quantum efficiency in the embedded phosphor, as the phosphor powder is not or only slightly damaged during embedding and / or the phosphor degenerates less during operation due to improved heat dissipation. This can contribute to high efficiency and a long lifetime, especially when applying excitation radiation with a high power density.
[0026] In various embodiments, the conversion element is arranged to be movable relative to the radiation arrangement. For example, the conversion element is arranged to be rotatable.
[0027] In various embodiments, the device comprises a phosphor wheel that is arranged to rotate about an axis and that has the conversion element. The conversion element can be arranged, for example, on an edge of the phosphor wheel and / or on a circular surface of the phosphor wheel. In addition to the conversion element, one, two, or more further conversion elements can be arranged. The conversion elements can, for example, have different phosphors.
[0028] In various embodiments, the conversion element is fixed relative to the radiation array. For example, the device can be used for a pico-projection application without a phosphor wheel, for example, in a portable electronic device, where the use of the condensed metal phosphate as a matrix for the conversion element can contribute to sufficient heat dissipation.
[0029] In various embodiments, a surface of the conversion element has a cooling structure. The cooling structure has an artificially enlarged surface of the conversion element. This can contribute to effective cooling of the conversion element.
[0030] In various embodiments, the cooling structure has grooves and / or fins. This can help to form the cooling structure effectively in a simple manner.
[0031] In various embodiments, the condensed metal phosphate is amorphous or predominantly amorphous. The fact that the metal phosphate is amorphous or predominantly amorphous can mean, for example, that the matrix itself contains no crystalline phase components or a maximum of 25 vol%, for example, a maximum of 10 vol%. The embedded crystalline phosphor is excluded from this.
[0032] In various embodiments, the condensed metal phosphate is colorless.
[0033] In various embodiments, the condensed metal phosphate is transparent to the conversion radiation and / or the excitation radiation.
[0034] In various embodiments, the condensed metal phosphate comprises aluminum phosphate, which is formed, for example, by condensation of mono-aluminum phosphate. This can contribute to oxidation-sensitive phosphors, such as nitrides, exhibiting little or no loss of efficiency after embedding in such matrices, for example, at temperatures of up to 350°C. Humidity tests have shown that these matrices react at least largely neutrally and thus exhibit good curing and / or chemical resistance.
[0035] In various embodiments, the conversion element also contains water glass as a starting material. This can contribute to embedding the phosphor powder at low temperatures and simultaneously increase chemical stability compared to a pure water glass matrix. The water glass can be present as an inorganic sol-gel, for example, as a starting material for the matrix. The water glass can, for example, contain or consist of alkali silicates.
[0036] In various embodiments, the conversion element comprises zinc-, magnesium-, and / or boron-containing additives. This can contribute to reducing the temperature required for a setting reaction during the production process of the conversion element, in particular the phosphor layer, if these elements are present as oxides and / or phosphates in the solution for producing the conversion layer or phosphor layer, i.e., in addition to the metal phosphate in the binder. For example, the temperatures can be reduced to a range between 200°C and 300°C.
[0037] In various embodiments, the radiation arrangement comprises at least one radiation source that generates the excitation radiation with a high luminance.
[0038] In various embodiments, the radiation source is a laser, a laser diode or a superluminescent diode.
[0039] In various designs, the high luminance ranges between 1 W / mm2 and 50 W / mm2.
[0040] Embodiments of the invention are illustrated in the figures and are explained in more detail below.
[0041] It shows Fig. 1 shows an embodiment of a device for providing electromagnetic radiation; Fig. 2 shows an embodiment of a device for providing electromagnetic radiation; Fig. 3 shows an embodiment of a device for providing electromagnetic radiation; Fig. 4 an embodiment of a surface structure of a conversion element; Fig. 5 an embodiment of a surface structure of a conversion element.
[0042] In the following detailed description, reference is made to the accompanying drawings, which form a part hereof, and in which is shown by way of illustration specific embodiments in which the invention may be practiced. In this regard, directional terminology such as "top," "bottom," "front," "back," "fore," "rear," etc., is used with reference to the orientation of the described figure(s). Since components of embodiments can be positioned in a number of different orientations, the directional terminology is for purposes of illustration and is in no way limiting. It is to be understood that other embodiments may be utilized and structural or logical changes may be made without departing from the scope of the present invention.It is understood that the features of the various embodiments described herein may be combined with one another unless specifically stated otherwise. The following detailed description is therefore not to be construed in a limiting sense, and the scope of the present invention is defined by the appended claims.
[0043] Throughout this description, the terms "connected," "attached," and "coupled" are used to describe both a direct and an indirect connection, a direct or indirect connection, and a direct or indirect coupling. In the figures, identical or similar elements are provided with identical reference numerals where appropriate.
[0044] In various embodiments, an electromagnetic radiation-emitting component can be an electromagnetic radiation-emitting semiconductor component and / or be designed as an electromagnetic radiation-emitting diode, as an organic electromagnetic radiation-emitting diode, as an electromagnetic radiation-emitting transistor, or as an organic electromagnetic radiation-emitting transistor. The electromagnetic radiation can be, for example, light in the visible range, UV light, and / or infrared light. In this context, the electromagnetic radiation-emitting component can be designed, for example, as a light-emitting diode (LED), as an organic light-emitting diode (OLED), as a light-emitting transistor, or as an organic light-emitting transistor.In various embodiments, the light-emitting component can be part of an integrated circuit. Furthermore, a plurality of light-emitting components can be provided, for example, housed in a common housing.
[0045] Fig. 1 Fig. 1 shows a device 10 for providing electromagnetic radiation according to various exemplary embodiments. The device 10 has a radiation arrangement 12 that generates excitation radiation 14. The radiation arrangement 12 is, for example, a radiation source or has one, two, or more radiation sources. A component that emits electromagnetic radiation is used as the radiation source, for example. The radiation source 12 can be, for example, a laser radiation source. The laser radiation source can be, for example, a laser diode. The laser diode can be a single-mode or multi-mode laser diode. For example, the laser diode can be a laser diode that emits blue laser light, which is also referred to as a blue laser diode. The power of the radiation source 12 can be, for example, 50 mW to 5 W.As an alternative to the blue laser diode, whose emission wavelengths can be, for example, in the spectral range from 400 nm to 480 nm, a UV (laser) radiation source can be used as the radiation source 12, for example with an emission wavelength between 300 nm and 400 nm.
[0046] The excitation radiation 14 is, for example, electromagnetic radiation in the visible range. The excitation radiation (pump light or pump radiation) 14 can also be, for example, ultraviolet radiation, infrared radiation, or even corpuscular radiation, such as an electron or ion beam, but the excitation radiation 14 is preferably laser radiation and / or LED light. The excitation radiation 14 is not necessarily limited to a specific spectral range; it can, for example, be pumped in the red, green, blue, and / or ultraviolet spectral range, for example by a corresponding radiation source (pump radiation source) or a combination of several radiation sources in the radiation arrangement 12. In general, the radiation sources can be designed to be operated, for example, with essentially constant power or in a pulsed manner.
[0047] The excitation radiation 14 is directed onto a conversion element 20 secured to a carrier 16. In other words, the radiation arrangement 12 illuminates or irradiates the conversion element 20 and / or the conversion element 20 is arranged in a beam path of the excitation radiation 14. The carrier 16 may also be referred to as a substrate. Furthermore, the conversion element 20 may be applied to a substrate, which may then be secured to the carrier 16. The radiation arrangement 12 is at a predetermined distance, greater than zero, from the conversion element 20 and is thus not in direct physical contact with the conversion element 20. The carrier 16 may, for example, be part of a color wheel and / or, for example, part of a projector. The device 10 may, for example, be arranged in the projector.Alternatively, the device 10 can be arranged, for example, in a motor vehicle, for example as interior lighting, headlights, or taillights, in a portable electronic device, for example a portable projector and / or a mobile phone, or in an endoscope. Furthermore, the carrier 16 can have a cooling device.
[0048] The irradiated conversion element 20, in turn, emits conversion radiation 22. Alternatively, the device 10 can have multiple radiation arrangements 12 and / or multiple conversion elements 20. The excitation radiation 14 and / or the conversion radiation 22 can also be referred to as electromagnetic radiation. To generate the conversion radiation 22, the conversion element 20 has phosphor(s). The phosphors are energetically excited with the aid of the deflected excitation beam 14. During the subsequent energetic de-excitation, the phosphors emit the conversion radiation of one or more predetermined wavelengths. Thus, a conversion of the excitation radiation 14 takes place, whereby the conversion radiation 22 is generated. During the conversion, the wavelengths of the excitation radiation 14 are shifted to shorter or longer wavelengths. The colors can be single colors or mixed colors.The individual colors can comprise, for example, green, red, or yellow light, and / or the mixed colors can be a mixture of green, red, and / or yellow light, for example, and / or can comprise, for example, white light. Blue light can also be provided, for example, by designing the conversion element 20 such that at least partially unconverted excitation radiation 14 leaves the device 10 as usable electromagnetic radiation. The individual or mixed colors can be represented using the conversion radiation 22 and / or the excitation radiation 14. For example, green, red, and yellow can be represented using blue laser light. When using UV laser light as pump light, the phosphors can also be selected to represent red, green, blue, and yellow.
[0049] The conversion element 20 comprises a matrix material (binder) comprising a condensed metal phosphate. The phosphor(s) is / are embedded in the matrix material. A phosphor can be understood as a substance that converts, with loss, electromagnetic radiation of one wavelength into electromagnetic radiation of another (longer) wavelength, for example by means of phosphorescence or fluorescence. The energy difference between absorbed electromagnetic radiation and emitted electromagnetic radiation can be converted into phonons, i.e., heat, and / or by means of emission of electromagnetic radiation with a wavelength proportional to the energy difference.
[0050] Common phosphors include garnets or nitrides, silicates, oxides, phosphates, borates, oxynitrides, sulfides, selenides, aluminates, tungstates, and halides of aluminum, silicon, magnesium, calcium, barium, strontium, zinc, cadmium, manganese, indium, tungsten, and other transition metals, or rare earth metals such as yttrium, gadolinium, or lanthanum, doped with an activator such as copper, silver, aluminum, manganese, zinc, tin, lead, cerium, terbium, titanium, antimony, or europium. In various embodiments of the invention, the phosphor is an oxidic or (oxy)nitridic phosphor, such as a garnet, orthosilicate, nitrido(alumo)silicate, nitride, or nitridorthosilicate, or a halide or halophosphate.Specific examples of suitable phosphors are strontium chloroapatite:Eu ((Sr,Ca)5(PO4)3Cl:Eu; SCAP), yttrium aluminum garnet:cerium (YAG:Ce), CaAlSiN3:Eu, or green-emitting garnet A3B5O12:Eu. A is preferably Y, Lu alone or in combination, B is preferably Al or Ga alone or in combination. Furthermore, the phosphor or phosphor mixture may contain, for example, particles with light-scattering properties and / or excipients. Examples of temporary excipients include surfactants and organic solvents. Examples of permanent additives are light-scattering particles, for example metal oxide particles, or stabilizers, for example oxide nanoparticles.
[0051] The matrix material comprises a condensed metal phosphate, for example, a condensed aluminum phosphate, from, for example, a mono-aluminum phosphate solution. The matrix material is, for example, amorphous or predominantly ammorphous, colorless, and / or transparent to the excitation radiation 14 and / or the conversion radiation 22. The condensed metal phosphate has good thermal conductivity, which is higher than that of silicone, and good UV resistance. The condensed metal phosphate is, for example, lead-free or low-lead, for example, with a proportion of less than 1 mol%. The condensed metal phosphate is generally low in alkali and / or halogen, for example, alkali- or halogen-free. The concentrations of alkali metals and halogens can therefore be negligible and / or each below 1 mol%.This means, for example, that these elements are not intentionally added and, at most, result from impurities in the raw materials used. This results in greater moisture stability. An exception is the combination of metal phosphate with alkali silicate.
[0052] The thermal expansion coefficient of the conversion layer with the matrix of metal phosphate and with the phosphor and / or optionally with additives can, for example, be greater than 5.0×10 -6 K -1 be.
[0053] The condensed metal phosphate can have phosphate as its main component, which can exist in various modifications, i.e., as polyphosphate, metaphosphate, orthophosphate, and all possible intermediates. The term phosphate also includes, for example, monophosphate such as the water-soluble Al(H2PO4)3 as well as water-insoluble polyphosphate such as [Al(PO3)3]. nDepending on the processing, metaphosphate such as (Al(PO3)3) or tertiary phosphate such as AlPO4 can be formed. A guideline is a molar ratio of phosphorus to aluminum (P / Al) of 1 to 10 as limit values.
[0054] Additives and / or components that modify the refractive index can be added to the metal phosphate. These components are, for example, inorganic. The metal phosphate can be, for example, aluminum phosphate, yttrium phosphate, alkaline earth phosphate, phosphates of the III main group and its subgroups, or other rare earth phosphates, or mixtures thereof. In particular, additives such as SiO2, e.g., in the form of Aerosil, pyrogenic Al2O3, or TiO2, etc., can also be added to the phosphate. For example, these additives are added as nanopowders; their average particle size is in the range of 1 nm to 40 nm. Ground glasses, such as tempered glass, or ground glass solder can also be added as nanopowders. These additives can increase the thermal conductivity of the conversion element 20, serve as a reflector, and / or adjust the thermal expansion coefficient.
[0055] Further optional components can be used to modify the refractive index, particularly compounds containing tellurium or bismuth. The condensed metal phosphate is moisture-resistant and can be produced, for example, at low temperatures. The proportion of added powders (phosphor and any additives) can be so high that the condensed metal phosphate primarily bonds the particles together. Some or all of the added components can be selected to chemically react with the metal phosphate, thereby modifying it. The metal phosphate is suitable for embedding phosphor powder, i.e., as a matrix for the conversion element 20.
[0056] The use of the condensed metal phosphate contributes to the high efficiency and long service life of the conversion element 20. For example, high UV resistance, high thermal conductivity, good temperature stability, and / or a high refractive index are achieved.
[0057] Such metal phosphates are produced, for example, using the well-known sol-gel process from a soluble metal phosphate or from the reaction product of a metal hydroxide with phosphoric acid, or from the reaction product of a metal salt with phosphoric acid. The solvent is first removed by drying. Subsequent treatment at elevated temperatures separates water or carbon-containing components, and the metal phosphate is then present in polymerized form. For example, aluminum, yttrium, or other rare earth phosphates are used because such phosphates exhibit high temperature and good moisture resistance. When embedding phosphors, it is important that they are not damaged by a chemical reaction with the solution or resulting reaction products, or by excessively high temperatures. The condensed metal phosphate can be in amorphous, semi-crystalline, or crystalline form.
[0058] For example, an aluminum phosphate matrix can be formed from a mono-aluminum phosphate solution by condensation at elevated temperature. Oxidation-sensitive phosphors such as nitrides, for example, exhibit no noticeable loss of efficiency after embedding in such a matrix at temperatures between 100°C and 400°C, for example, between 200°C and 350°C. Humidity tests of such conversion elements 20 have shown that these matrices react neutrally, thus indicating good setting and chemical resistance. The temperature required for the setting reaction can be further reduced if other glass-forming metal phosphates such as Zn, Mg, B, or their oxides are present in the solution. In principle, such a matrix is suitable for substrates such as glass, ceramics, or various metals.
[0059] For example, a phosphor, such as YAG:Ce or another phosphor, can be suspended in powder form in an aqueous solution of the metal phosphate and then applied to the substrate as a layer. Drying can then take place at low temperatures, such as between 80°C and 150°C, and / or at reduced ambient pressure. Curing can then occur by condensation, for example at a curing temperature that is limited, for example, by the temperature resistance of the component parts. For example, firing takes place at temperatures between 180°C and 500°C, such as between 200°C and 350°C. The solid content of phosphor can be varied depending on the desired color coordinate of the electromagnetic radiation to be provided by the device 10.It is also possible to manufacture the conversion element 20 in such a way that the excitation radiation 14 is completely converted into conversion radiation 22, apart from thermal losses. For example, the solids content of the phosphor can be selected so high that the metal phosphate used only encloses the phosphor particles with a thin layer, thereby bonding them together. Furthermore, it is possible to embed a mixture of different phosphor powders into the metal phosphate to achieve different light colors.
[0060] Fig. 2 shows an embodiment of the device 10, which largely corresponds to the Fig. 1, in contrast to the embodiment shown in Fig. In the embodiment of the device 10 shown in Figure 2, the carrier 16 is at least partially transparent to the conversion radiation 22 and / or the excitation radiation 14.
[0061] Fig. 3 shows an embodiment of the device 10, which largely corresponds to the Fig. 1, in contrast to the embodiment shown in Fig. In the embodiment of the device 10 shown in Figure 3, the carrier 16 is designed as a phosphor wheel. The phosphor wheel is rotatably mounted about an axis 24. The phosphor wheel can be rotated about the axis 24 with the aid of a drive unit (not shown). Optionally, a further conversion element 26 is arranged on the phosphor wheel. Furthermore, further conversion elements can be arranged on the phosphor wheel. The conversion elements 20, 26 can comprise identical and / or different phosphors, so that they can be used to generate conversion radiation 22 of the same or different wavelengths.
[0062] Fig. 4 shows an embodiment of a surface structure that can, for example, be present on at least one of the conversion elements 20, 26. For example, the surface structure can be a cooling structure that enlarges the surface area of the corresponding conversion element 20, 26. The surface structure is formed, for example, on a side of the corresponding conversion element 20, 26 facing away from the substrate. For example, the surface structure and / or the cooling structure has grooves 28.
[0063] Fig.5 shows an embodiment of the surface structure, which, for example, can be provided by at least one of the conversion elements 20, 26. For example, the surface structure can be the cooling structure by which the surface of the corresponding conversion element 20, 26 is enlarged. The surface structure is formed, for example, on a side of the corresponding conversion element 20, 26 facing away from the substrate. For example, the surface structure and / or the cooling structure has fins 30.
[0064] Alternatively, the corresponding conversion element 20, 26 may not have a specifically specified surface structure and / or a cooling structure.
[0065] A method for producing such a conversion element 20 may, for example, comprise the following steps: - Production or purchase of the mono-aluminium phosphate solution; - Preparation of a suspension of phosphor powder (one or different types) and mono-aluminium phosphate solution, optionally adding scattering particles and / or surfactants; - optional addition of nanopowders to adjust viscosity and / or stabilize the suspension; - Optional pretreatment of the substrate to improve wetting and / or layer adhesion. e.g., with UV radiation or plasma; - applying the layer to the substrate by a known method such as: screen or stencil printing, inkjet printing, spin coating, spraying, dipping, slurrying and / or dispensing; - Drying of the layer: for example, moderate drying, for example to avoid foaming of the layer, whereby drying temperatures can be selected depending on the solvent, the drying time and / or the layer volume; with water as the solvent, drying can be carried out, for example, at 30°C to 80°C; drying can be carried out, for example, by convection, e.g. in a drying cabinet, or in a microwave; - Curing of the layer by condensation: for example at 150°C to 500°C, for example at 200°C to 350°C, for example for amorphous or predominantly amorphous layers; the curing time can be selected depending on the layer volume and can, for example, be in the range of a few seconds to one hour, whereby curing can take place, for example, in an oxidising atmosphere; for wet layer thicknesses in the range of 50 μm, for example, 15 minutes can be sufficient; - After curing, it is optionally possible to specifically structure the layer and / or introduce the surface structure.
[0066] A grain size distribution for the phosphor powder can, for example, be a D50 between 5 µm and 50 µm, for example 5 µm to 30 µm. The mixing ratio of solution to solid can be selected depending on the grain size. For example, with decreasing grain size, increasingly more matrix solution can be used. For example, for garnet phosphors with a grain size distribution of D50 between 5 µm and 30 µm, a mixing ratio of phosphor to matrix solution of 1:0.5 to 1:3 based on the weight fraction can be selected. The conversion element 20, 26 produced in this way can be used for full or partial conversion. The molar ratio of Al to P can, for example, be in the range of 1:1 to 1:5. The proportion of additives can be so high that the matrix essentially only acts as a binder, i.e., it only sticks the particles together. In this case, the substrate can also be coated with powder, which can then, for example,by spraying the matrix solution and a subsequent temperature treatment (drying, curing).
[0067] When using the conversion element 20, 26 for a laser application (LARP, ITOS, automotive), a suspension of garnet phosphor and mono-aluminum phosphate solution can be applied, for example, by doctor blade coating, to a masked, highly reflective substrate (e.g., aluminum, as used in lighting applications). Beforehand, the substrate can optionally be irradiated with UV radiation for improved wetting. The wet film thickness can, for example, be in the range between 50 µm and 100 µm. This can then be followed by, for example, initial drying at room temperature and then drying at 80°C for, for example, 12 hours. The dried layer can then be heated at 10°C / min to, for example, 350°C, and the temperature can then be maintained for, for example, a few seconds up to an hour, for example, 15 minutes. Depending on the masking, this can be removed immediately after doctor blade coating or after initial drying.The heat treatment can be carried out in an oxidizing atmosphere, for example. The mixing ratio of phosphor to matrix solution can be 1:1 by weight, for example. The cured layer thickness can range from 40 µm to 80 µm. These layer thicknesses are suitable, for example, for ITOS applications. In the case of LARP applications, cured layer thicknesses of 10 µm to 200 µm can be used, for which correspondingly lower or higher wet layer thicknesses are produced.
[0068] When arranging the conversion element 20, 26 on a glass substrate, for example for a remote phosphor application, a suspension of nitridic phosphor in powder form and an aqueous mono-aluminum phosphate solution, which may additionally contain other phosphates or oxides such as Mg and / or Zn and / or B, can be applied to a masked soft glass substrate, for example by doctor blade coating. The substrate can optionally be irradiated with UV radiation beforehand for better wetting. The wet film thickness can, for example, be in the range between 10 µm and 50 µm. This can then be followed by initial drying, for example at room temperature, and then drying at, for example, 80°C for, for example, 12 hours. The dried layer can then be heated to 220°C, for example at 10°C / min, and the temperature can then be held for, for example, from a few seconds up to an hour, for example 15 minutes.Depending on the masking, it can be removed immediately after doctor blade coating or after initial drying. The heat treatment can be carried out in an oxidizing atmosphere, for example. The mixing ratio of phosphor to matrix solution can be 1:1 by weight, for example. The cured layer thickness can range from 30 µm to 40 m², for example. The embedded phosphor can, for example, have a quantum efficiency in the range of the original phosphor powder.
[0069] When arranging the conversion element 20, 26 on a ceramic substrate, for example, for a remote phosphor application, the substrate can be coated, for example, with a phosphor powder or a phosphor powder mixture. The dry phosphor layer can be sprayed, for example, with a mono-aluminum phosphate solution 35, so that the phosphor powder can be moistened and fixed in a subsequent thermal step.
[0070] The advantage of the described inorganic matrices containing condensed metal phosphate is that the phosphor can be embedded at moderate temperatures and without significant damage. These matrices are chemically more stable than pure water glass matrices and exhibit better thermal conductivity than organic matrices. This is particularly important for highly stressed LED and laser applications. In the case of a phosphor wheel for a LARP application, this makes it possible to operate the phosphor wheel at low speed or to use a less complex geometry for the conversion element 20, 26, for example, without a cooling structure. It is also conceivable to save phosphor by reducing the diameter of the phosphor wheel compared to a conventional phosphor wheel. This can also contribute to the progressive miniaturization of the device 10. Particularly high power densities are possible for all applications.
[0071] The matrix can be formed, for example, from a mono-aluminum phosphate solution by condensation. These solutions are inexpensive and easy to store.
[0072] Metal phosphates, for example aluminum phosphate, for example mono-aluminum phosphate or aluminum metaphosphate or polymeric aluminum phosphate and / or optional additives as oxide, phosphate and / or salt can also be added to water glass, for example, which can contribute, for example, to good weather resistance of the water glass and the conversion element 20 formed therefrom. The phosphate can then act as a hardener and can thereby contribute to defined curing and, due to ion exchange, to good chemical resistance at the same curing temperature. The aluminum phosphate and / or the additives can then be present, for example, in powder form. This is mixed as homogeneously as possible with the phosphor powder before the liquid alkali silicate, for example soda water glass, is added. The mixing ratio depends on the modulus and the type of water glass as well as on the hardener composition and hardener function.Mixing ratios of hardener to liquid alkali silicate are, for example, 1:3 to 1:8 by weight.
[0073] The pot life is often longer than with pure water glass (liquid alkali silicate) because the aluminum phosphate solution does not react with the atmosphere, as is the case with water glass (setting with CO2 from the air). As a result, the hardening and curing process is more defined, as the alkali ion from the alkali silicate is exchanged for the metal ion of the metal phosphate, resulting in uniform and simultaneous curing throughout the entire volume. This means that a polysilicic acid gel is created, the cross-linking of which is assisted by the ions contained in the metal phosphate. In the case of aluminum phosphate, this is an exchange of the alkali ion from the water glass for an aluminum ion from the hardener. The latter is then incorporated into the silicate matrix. Alkali phosphate is also produced as a filler. The exchange can be increased or even stopped by heat treatment at, for example, 300°C.which further improves weather resistance.
[0074] The mixture with water glass can, for example, be prepared according to a process with the following steps: - Mixing the metal phosphate powder with the phosphor powder and any additives; - Prepare a suspension from the powder mixture and a water glass solution; - applying the suspension containing at least one solid phosphor and at least one alkali silicate and at least one metal phosphate to a substrate surface or into a mold to produce a phosphor layer or a phosphor body; - Curing of the phosphor layer or phosphor body.
[0075] Alternatively, powdered alkali silicate can be used. In this case, it is added to the powder mixture, which is then dissolved or suspended in water.
[0076] The ratio of the volumes of alkali silicate, metal phosphate, water, and solid powder directly influences the homogeneity of the suspension (processability), the viscosity, the resulting layer thickness, the tendency to crack, the drying behavior, and the optical properties of the resulting layer (later glass content). The volume concentration ratio of liquid alkali silicate including the metal phosphate and water in such mixtures can range from approximately 1:5 to approximately 5:1, for example, from approximately 1:3 to 3:1. For example, the volume concentration ratio of liquid alkali silicate(s) including metal phosphate(s) and water is 1:3, 1:2, 1:1, 2:1, or 3:1. The ratio used can be selected depending on the target properties of the dye layer (e.g., glass content, layer thickness, strength), as well as on the phosphors themselves.In this context, “approximately” means, for example, that the corresponding numerical value may deviate by about 10% upwards or downwards.
[0077] The alkali silicate used can be, for example, sodium silicate or potassium silicate. Mixtures of the aforementioned alkali silicates are also included. The alkali silicates are compounds of the general formula M2OxnSiO2, where M is an alkali metal and n is in the range from 1 to 4. In various embodiments, the alkali silicates are used as colloidal, alkaline solutions in water, in particular sodium / potassium silicate solutions. Such aqueous solutions can be prepared by dissolving the solid alkali silicates in water at elevated temperature and pressure.
[0078] In various embodiments, the mass ratio of phosphor or phosphor mixture to the aqueous, liquid alkali silicate, i.e. the mixture of alkali silicate and water, is approximately 1:5 to approximately 5:1, for example approximately 1:3 to 3:1. Exemplary concentration ratios are 3:1, 2:1, 1:1, 1:2 or 1:3. These concentration ratios can be advantageously processed with regard to the homogeneity of the suspension, sedimentation time and layer thickness. The proportion of metal phosphate required is determined by the amount of alkali silicate and is added to the liquid portion since it dissolves and reacts. The suspension can also contain other components, for example particles with light-scattering properties and / or auxiliaries. Examples of auxiliaries include surfactants and organic solvents.The suspension can be applied to a surface of the substrate or introduced into a mold by slurrying, printing, spraying, or injection. To create a phosphor layer, the application may further include spinning and / or ultrasonic treatment.
[0079] The substrate to which the phosphor layer is applied can be, for example, the carrier 16, the phosphor wheel, a heat sink or optical component, such as a 30 collimator. The substrate can consist of various suitable materials, such as, for example, plastic, glass, ceramic or metal. Molds made of the materials mentioned can be used to form a phosphor body. The phosphor body can be, for example, a phosphor film. The phosphor layer, the phosphor film and / or the phosphor body, for example a phosphor plate, can then form the conversion element 20 or be part of the conversion element 20. The curing of the phosphor layer or the phosphor body can take place by drying and chemical reactions (for example setting by ion exchange, crosslinking, condensation).Curing or drying can take place at room temperature or at elevated temperature, for example, at 80°C to 500°C. Different curing / drying steps at different temperatures can also be combined. In one embodiment, a drying step at room temperature can be followed by a further drying step at elevated temperature, for example, 80 to 150°C. Curing / drying at elevated temperature can take place, for example, in an oven. Alternatively, the substrate or the mold and / or the phosphor layer / phosphor body can be heated using microwaves or induction techniques. During the production of a phosphor body, it can be removed from the mold after a first drying step and then further dried, optionally at elevated temperature.
[0080] The process of bonding phosphors using alkali silicates with metal phosphate allows the production of very hard, mechanically stable phosphor layers. The binder, in many cases, does not interact with the phosphors at their operating temperature, and is optically transparent, spectrally stable, and thermally stable. This allows the production of thin phosphor layers on substrate surfaces with layer thicknesses between 10 μm and 200 μm, as well as unbonded phosphor platelets or three-dimensional bodies (optical components) of larger dimensions (several mm).
[0081] In order to efficiently convert the excitation radiation 14 into conversion radiation 22 in one or more of the exemplary embodiments explained above, the scattered light component of the excitation radiation 14 can be minimized. This can be achieved, for example, by coupling light to relatively large phosphor particles. In principle, the particle sizes of the phosphors can be adjusted and selected within a certain range by appropriate processing (grinding). In practice, however, grain size distributions always exist. Within suspensions, the larger and heavier particles sediment first, the smaller and lighter ones later, so that after a certain time (depending, among other things, on the viscosity of the liquid and the particle size) a gravity-driven particle size distribution is established (small particles at the upper layer surface, larger particles at the bottom).The aqueous alkali silicate solution containing metal phosphate can, for example, be used to adjust a particle size distribution during application and curing. The phosphor layer containing the phosphor particles can then be removed from the carrier medium after drying and annealing, rotated 180°, and reapplied to a substrate with the optically more favorable coarser grain distribution facing upwards, e.g., by bonding alkali silicate with metal phosphate or pure metal phosphate.
[0082] Alternatively, the particle distribution can be influenced by ultrasonic treatment. For example, ultrasound can be used to shake coarser phosphor particles onto the coating surface.
[0083] The invention is not limited to the specified embodiments. For example, the specified embodiments can be combined. For example, the conversion element 20 may or may not have the cooling structure in any embodiment.
Claims
[1] Device (10) for providing electromagnetic radiation, with - a radiation arrangement (12) for generating excitation radiation (14), - at least one conversion element (20, 26) for generating conversion radiation (22), which comprises condensed metal phosphate and phosphors embedded in the condensed metal phosphate and which is arranged at a distance from the radiation arrangement (12) in a beam path of the excitation radiation (14), wherein the conversion element (20, 26) comprises a silicate matrix and alkali phosphate. [2] Device (10) according to claim 1, wherein the conversion element (20, 26) is arranged to be movable relative to the radiation arrangement (12). [3] Device (10) according to claim 2, which comprises a phosphor wheel which is arranged to be rotatable about an axis (24) and which comprises the conversion element (20, 26). [4] Device (10) according to claim 1, wherein the conversion element (20, 26) is fixedly arranged relative to the radiation arrangement (12). [5] Device (10) according to one of the preceding claims, wherein a surface of the conversion element has a cooling structure. [6] Device (10) according to claim 5, wherein the cooling structure comprises grooves (28) and / or fins (30). [7] Device (10) according to one of the preceding claims, wherein the condensed metal phosphate is amorphous. [8] Device (10) according to one of the preceding claims, wherein the condensed metal phosphate is colorless. [9] Device (10) according to one of the preceding claims, wherein the condensed metal phosphate is transparent to the conversion radiation (22) and / or the excitation radiation (14). [10] Device (10) according to any one of the preceding claims, wherein the condensed metal phosphate comprises aluminum phosphate formed by condensation from mono-aluminum phosphate. [11] Device (10) according to one of the preceding claims, wherein the conversion element (20, 26) comprises zinc-, magnesium- and / or boron-containing compounds. [12] Device (10) according to one of the preceding claims, wherein the radiation arrangement (12) has at least one radiation source which generates the excitation radiation (14) with a high luminance. [13] Device (10) according to claim 12, wherein the radiation source is a laser, a laser diode or a superluminescent diode. [14] Device (10) according to one of claims 12 or 13, wherein the high luminance is between 1 W / mm 2 and 50 W / mm 2 lies.
Citation Information
Patent Citations
Electrical component has light emitting element, where converter ceramics is arranged at radiation withdrawal surface of light emitting element for converting wavelength of element
DE102009003936A1
Conversion unit with multiple conversion modules, commissioning procedure of the conversion unit and an optical arrangement comprising such a conversion unit
DE102009016953A1
Optoelectronic semiconductor device
DE102010028776A1
Radiation-emitting apparatus
WO2010003763A1