Formation of high-voltage gates

By forming memory gates before high-voltage transistors in a specific sequence, the integration of split-gate memory cells with non-memory devices on a shared substrate is optimized, addressing manufacturing challenges and enhancing performance.

DE112013005992B4Active Publication Date: 2024-10-24LONGITUDE FLASH MEMORY SOLUTIONS LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
DE112013005992
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2012-12-14
Filing Date
2013-12-12
Publication Date
2024-10-24
Estimated Expiration
2033-12-12

AI Technical Summary

Technical Problem

Existing non-volatile memory technologies face challenges in integrating high-voltage gates with non-memory devices on the same substrate, requiring different production parameters, leading to inefficiencies in manufacturing and performance.

Method used

A method for manufacturing semiconductor devices with split-gate memory cells, where memory gates are formed before high-voltage transistors, allowing for efficient integration by using a sequence of etching and masking processes to ensure compatibility with both types of devices.

Benefits of technology

This approach enables efficient integration of high-voltage transistors and memory cells on the same substrate, reducing manufacturing complexity and improving performance and reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A method for fabricating a semiconductor device comprising a memory region, a first substrate region, and a second substrate region, which includes the following: Formation of a first gate in the first substrate region; Forming a selection gate (108) in the memory region; Arranging a charge-trapping dielectric (114) in the storage region and the second substrate region; Arranging a gate layer in the memory region; Removal of the charge-trapping dielectric (114) from the second substrate region; Forming a storage gate (110) on a side wall of the selection gate (108); Formation of a second gate in the second substrate region; where the memory gate (110) is formed before the second gate is formed; and where the first gate is formed before the memory gate (110) is formed.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUNDTechnical field

[0001] The embodiments described herein generally relate to non-volatile memories, such as charge trap memories. background

[0002] Non-volatile memory, such as flash memory, retains stored data even when power is removed from the memory. For example, a non-volatile memory cell stores data by storing electrical charge in an electrically isolated floating gate or in a charge-trapping layer underlying the control gate of a field-effect transistor (FET). The stored electrical charge controls the threshold of the FET and thereby controls the cell's memory state.

[0003] A non-volatile memory cell is programmed using, for example, hot carrier injection to place charge into a storage layer. High drain and gate voltages are used to facilitate the programming process, and the memory cell conducts relatively high current during programming, which may be undesirable in low-voltage or low-power applications.

[0004] A split-gate memory cell is a type of non-volatile memory cell in which a select gate is placed adjacent to a storage gate. During programming of a split-gate memory cell, the select gate is biased at a relatively low voltage, and only the storage gate is biased at a high voltage to provide the vertical electric field necessary for hot carrier injection. Since carrier acceleration occurs in the channel region, predominantly beneath the select gate, the relatively low voltage at the select gate results in more efficient carrier acceleration in the horizontal direction compared to a conventional flash memory cell. This makes hot carrier injection more efficient, with lower current and power consumption during the programming process.A split-gate memory cell can be programmed using techniques other than hot carrier injection, and depending on the technique, any advantages over the conventional flash memory cell during the programming process may vary.

[0005] Fast read time is another advantage of a split-gate memory cell. Because the select gate is in series with the memory gate, the erased state of the memory gate can be close to or in depletion mode (i.e., threshold voltage Vt less than zero volts). Even when the erased memory gate is in such depletion mode, the select gate in the off state prevents the channel from conducting significant current. With the threshold voltage of the erased state close to or below zero, the threshold voltage of the programmed state does not need to be very high and still provides a reasonable read margin between the erased and programmed states. Accordingly, the voltages applied to the select gate and the memory gate during the read operation can be less than or equal to the supply voltage.The fact that the supply voltage does not have to be pumped to a higher level therefore makes the reading process faster.

[0006] It is common practice to monolithically incorporate multiple types of field-effect devices on the same substrate as memory cells. These non-memory devices perform, for example, decoding, charge pumping, and other functions related to memory operations. The substrate may also include non-memory devices to provide functions unrelated to memory operations. Such non-memory devices, incorporated on the same substrate as the memory cells, may include transistors tailored for high-speed operations, while other transistors are tailored to handle high operating voltages. Integrating the processing of memory cells, such as a split-gate memory cell, with the processing of one or more types of non-memory transistors on the same substrate is challenging because they each require different manufacturing parameters.Accordingly, there is a need for devices and methods for integrating a memory cell and other devices on the same substrate to enable improved cost, performance, reliability, or manufacturability. JP 2011 - 103 401 A discloses a semiconductor device and a corresponding manufacturing method. SHORT OVERVIEW

[0007] It is desirable to eliminate or mitigate at least one of the problems, whether identified herein or elsewhere, or to provide an alternative to existing apparatus and methods. Embodiments described herein include methods, systems, and devices for forming high-voltage gates in computer memory.

[0008] The invention is defined in the independent claim. Dependent claims describe preferred embodiments.

[0009] One embodiment describes a method of manufacturing a semiconductor device comprising a memory region, a first substrate region, and a second substrate region. A first gate is formed in the first substrate region. A select gate is formed in the memory region. A charge-trapping dielectric is disposed in the memory region and the second substrate region. A polycrystalline silicon (poly) layer is disposed in the memory region. The charge-trapping dielectric is removed from the second substrate region. A memory gate is formed on a sidewall of the select gate. A second gate is formed in the first substrate region. In this method, the memory gate is formed before the second gate is formed and the first gate is formed before the memory gate is formed.

[0010] A semiconductor device fabricated according to the above method comprises a memory region, a first substrate region, and a second substrate region. First gates are located in the first substrate region. Second gates are located in the second substrate region. Select gates are located in the memory region. Memory gates are located in the memory region, each memory gate being formed adjacent to a corresponding select gate. In the embodiment, sidewalls of the memory gates are older than sidewalls of the second gates (i.e., they were formed previously; in particular, the memory gates are formed before the second gates are formed, and the first gates are formed before the memory gates are formed).

[0011] These and other advantages and features will become apparent in light of the following detailed description of embodiments of the invention. It should be noted that the summary and abstract sections may set forth one or more, but not all, exemplary embodiments of the present invention as contemplated by the inventor(s). It is understood that the detailed description section, and not the overview or summary section, should be used to interpret the claims. SHORT DESCRIPTION OF THE DRAWINGS / FIGURES

[0012] The accompanying drawings, which are incorporated herein and form a part of the specification, illustrate the present invention and, together with the description, serve to further explain the principles of the present invention and to enable those skilled in the art to make and use the present invention. Fig. 1 illustrates an example of a non-volatile split-gate memory cell according to one embodiment. Fig. 2 illustrates an exemplary circuit diagram of a memory cell including connections to various metal layers in a semiconductor device, according to one embodiment. Fig. 3 illustrates an exemplary semiconductor device according to an embodiment that includes both memory and peripheral circuits embedded in the same substrate. Fig. 4-13 illustrate a semiconductor device at various stages of fabrication according to one embodiment.

[0013] The features and advantages of the present invention will become more apparent from the detailed description set forth below when considered in conjunction with the drawings, in which like reference numerals identify corresponding elements throughout. In the drawings, like reference numerals generally indicate identical, functionally similar, and / or structurally similar elements. The drawing in which an element first appears is indicated by the leftmost numeral(s) in the corresponding reference numeral. DETAILED DESCRIPTION

[0014] This specification discloses one or more embodiments incorporating the features of this invention. The disclosed embodiment(s) are merely examples of the present invention. The scope of the present invention is not limited to the disclosed embodiment(s). The present invention is defined by the claims appended hereto.

[0015] The described embodiment(s) and references in the specification to "an embodiment," "an embodiment," etc., indicate that the described embodiment(s) may include a particular feature, structure, or characteristic, but not every embodiment necessarily includes that particular feature, structure, or characteristic. Furthermore, such terms do not necessarily refer to the same embodiment. Further, where a particular feature, structure, or characteristic is described in connection with one embodiment, it is to be understood that it is within the skill of one skilled in the art to effect such feature, structure, or characteristic in connection with other embodiments, whether expressly described or not.

[0016] Before describing the various embodiments in more detail, a further explanation is given regarding certain terms that may be used throughout the descriptions.

[0017] The term "etch" or "etching" is used herein to generally describe a manufacturing process of patterning a material such that at least a portion of the material remains after the etching is complete. For example, it is understood that the process of etching silicon includes the steps of patterning a capping layer (e.g., photoresist or hard mask) over the silicon and then removing the regions of silicon no longer protected by the capping layer. As such, the regions of silicon protected by the mask would remain after the etching process is complete. However, in another example, etching may also refer to a process that does not use a mask but still leaves at least a portion of the material after the etching process is complete.

[0018] The preceding description serves to distinguish the term "etching" from "removal." When etching a material, at least a portion of the material remains after the process is complete. However, "removal" is considered a broad term that can include etching.

[0019] Throughout the descriptions herein, various regions of the substrate on which the field-effect devices are fabricated are mentioned. It is understood that these regions may be present anywhere on the substrate, and further, the regions may not be mutually exclusive. That is, in some embodiments, portions of one or more regions may overlap each other. Although up to three different regions are described herein, it is understood that any number of regions may be present on the substrate and may denote areas comprising certain types of devices or materials. In general, the regions are used to conveniently describe areas of the substrate comprising similar devices and should not limit the scope and spirit of the described embodiments.

[0020] The terms "depositing" or "deposition" are used herein to describe the act of applying a layer of material to the substrate. Such terms are intended to describe any possible layer-forming technique, including, but not limited to, thermal growth, sputtering, evaporation, chemical vapor deposition, epitaxial growth, electroplating, etc.

[0021] The term "substrate," as used throughout the descriptions, is most commonly thought of as silicon. However, the substrate may also be any of a variety of semiconductor materials, such as germanium, gallium arsenide, indium phosphide, etc. In other embodiments, the substrate may be electrically non-conductive, such as a glass or sapphire wafer.

[0022] The term "poly," as used throughout the descriptions, is most commonly thought of as referring to polycrystalline silicon. Poly involves multiple small crystals as opposed to a single single crystal. Poly may be doped or may have a metal or metal silicide deposited over it.

[0023] "Poly" in this application is used as an example of a gate conductor. Other conductors may be used to form the gates, for example, metals, alloys, other doped semiconductors, or conductive materials, as will be apparent to those skilled in the art. The use of "poly" in the description of the embodiments is not intended to be limiting.

[0024] Fig. 1 illustrates an example of a non-volatile split-gate memory cell 100 according to one embodiment. The memory cell 100 is formed on a substrate 102, such as silicon. The substrate 102 is typically p-type or a p-well, while a first doped source / drain region 104 and a second doped source / drain region 106 are n-type. However, it is also possible for the substrate 102 to be n-type, while the regions 104 and 106 are p-type.

[0025] The memory cell 100 includes two gates, a select gate 108 and a store gate 110. Each gate may be a doped poly layer formed by well-known techniques, such as deposition and etching, to form the gate structure. The select gate 108 is disposed over a dielectric layer 112. The store gate 110 is disposed over a charge-trapping dielectric 114 comprising one or more dielectric layers. In one example, the charge-trapping dielectric 114 comprises a silicon nitride layer sandwiched between two silicon dioxide layers to create a three-layer stack, collectively and commonly referred to as "ONO." Other charge-trapping dielectrics may include, but are not limited to, a silicon-rich nitride film or any film comprising, but not limited to, silicon, oxygen, and nitrogen in various stoichiometries.A vertical dielectric 116 is also disposed between the select gate 108 and the memory gate 110 for electrical isolation between the two gates. In some examples, the vertical dielectric 116 and the charge-trapping dielectric 114 are the same dielectric, while other examples form one dielectric before the other (e.g., they may have different dielectric properties). As such, the vertical dielectric 116 does not need to comprise the same film structure as the charge-trapping dielectric 114. After the gates are defined, regions 104 and 106 are created by implanting dopants using, for example, an ion implantation technique. Regions 104 and 106 form the source or drain of the split-gate transistor depending on which potentials are applied to each.In split-gate transistors, for convenience, regardless of the relative bias voltages, region 104 is commonly referred to as the drain, while region 106 is commonly referred to as the source. It should be understood that this description is intended to provide a general overview of a typical split-gate architecture, and that in actual practice, many more detailed steps and layers are provided to form the final memory cell 100.

[0026] An exemplary write, read, and erase operation associated with memory cell 100 will now be described. To write a bit to memory cell 100, a positive voltage on the order of, for example, 5 volts is applied to region 106 while grounding region 104 and substrate 102. A low positive voltage on the order of, for example, 1.5 volts is applied to select gate 108, while a higher positive voltage on the order of, for example, 8 volts is applied to memory gate 110. As electrons are accelerated in a channel region between source and drain, some of them acquire sufficient energy to be injected upward and trapped in charge-trapping dielectric 114. This is known as hot electron injection.In one example of charge-trapping dielectric 114, the electrons are trapped in a nitride layer of charge-trapping dielectric 114. This nitride layer is also commonly referred to as the charge-trapping layer. The trapped charge in charge-trapping dielectric 114 stores the "high" bit in memory cell 100, even after the various supply voltages have been removed.

[0027] To "erase" the stored charge in memory cell 100 and return the state of memory cell 100 to a "low" bit, a positive voltage on the order of, for example, 5 volts is applied to region 106 while region 104 is kept floating or biased, and select gate 108 and substrate 102 are typically grounded. A high negative voltage on the order of, for example, -8 volts is applied to memory gate 110. The bias conditions between memory gate 110 and region 106 create holes through the band-to-band tunneling effect. The created holes are sufficiently excited by the strong electric field beneath memory gate 110 and are accelerated upward into charge-trapping dielectric 114. The injected holes effectively erase memory cell 100 to the "low" bit state.

[0028] To "read" the stored bit of memory cell 100, a low voltage, for example, in the range between zero and 3 volts, is applied to the select gate, the store gate, and region 104, while region 106 and substrate 102 are typically grounded. The low voltage applied to the store gate is chosen to be substantially equidistant between the threshold voltage required to turn on the transistor when it is storing a "high" bit and the threshold voltage required to turn on the transistor when it is storing a "low" bit, in order to clearly distinguish between the two states.For example, if the application of the low voltage during the "read" operation caused a significant current to flow between regions 104 and 106, the memory cell holds a "low" bit, and if the application of the low voltage during the "read" operation does not cause a significant current to flow between regions 104 and 106, the memory cell holds a "high" bit.

[0029] Fig. Figure 2 illustrates an exemplary circuit diagram of a memory cell 100 comprising connections to various metal layers in a semiconductor device. Only a single memory cell 100 is illustrated, however, as indicated by the ellipses in the X and Y directions, an array of memory cells may be connected by the various lines running in the X and Y directions. In this way, one or more memory cells 100 may be selected for reading, writing, and erasing bits based on the bit line (BL) and source line (SL) used.

[0030] An exemplary source line (SL) runs along the X-direction and is formed in a first metal layer (M1). The source line (SL) can be used to establish an electrical connection to the doped region 106 of each memory cell 100 along a row extending in the X-direction.

[0031] An exemplary bit line (BL) runs along the Y-direction and is formed in a second metal layer (M2). The bit line (BL) can be used to establish an electrical connection to the doped region 104 of each memory cell 100 along a column extending in the Y-direction.

[0032] It is understood that the Fig. 2 are merely exemplary, and the various connections could be formed in metal layers other than those shown. Furthermore, although not shown, the memory cells 100 may be arranged in an array in the Z-direction and formed in multiple stacked layers.

[0033] Fig. Figure 3 illustrates an exemplary semiconductor device that includes both memory and peripheral circuitry in the same substrate. In this example, the substrate 102 includes a core region 302 and a peripheral region 304. The core region 302 includes a plurality of memory cells 100 that may operate similarly to those previously described. It should be understood that the cross-section of Fig. 3 is merely exemplary, and that the core region 302 and the peripheral region 304 may be located in any area of ​​the substrate 102 and may be composed of various different regions. Furthermore, the core region 302 and the peripheral region 304 may exist in the same general area of ​​the substrate 102.

[0034] The peripheral region 304 may include integrated circuit components such as resistors, capacitors, inductors, etc., as well as transistors. In the illustrated embodiment, the peripheral region 304 includes a plurality of high-voltage transistors 306 and low-voltage transistors 308. In one example, the high-voltage transistors 306 are present in a different region of the substrate 102 than the low-voltage transistors 308. The high-voltage transistors 306 are capable of handling voltages as high as, for example, 20 volts, while the low-voltage transistors 308 operate at a higher speed but cannot operate at the same high voltages as the high-voltage transistors 306. In one embodiment, the low-voltage transistors 308 are configured to have a shorter gate length than the high-voltage transistors 306.The high voltage transistors 306 are typically characterized as having a thicker gate dielectric 310 than the gate dielectric of the low voltage transistors 308.

[0035] In charge-trapping memories, it is desirable to fabricate low-voltage transistors 308 and memory cells 100 from a thin layer of poly because the thin layer enables better performance. However, since semiconductor device fabrication generally occurs as a sequence of layer-deposition steps, it would be impractical to fabricate high-voltage transistors 306 from a different layer of poly than low-voltage transistors 308, forcing high-voltage transistors 306 to have the same thickness as low-voltage transistors 308. While thinness improves the performance of a low-voltage transistor 308, thinness can make high-voltage transistors 306 vulnerable to implant penetration.One way to take advantage of thin poly in both low-voltage transistors 308 and memory cells 100 without damaging high-voltage transistors 306 through implant penetration is to form the high-voltage transistors 306 before forming the low-voltage transistors 308 and memory cells 100.

[0036] Fig. 4-13 collectively illustrate a manufacturing method for a semiconductor device including memory cells and other FET devices, according to one embodiment. It should be understood that the various layers and structures are not necessarily drawn to scale and that other processing steps may be performed between those illustrated and those described herein, as will be appreciated by those skilled in the art in light of the present disclosure.

[0037] Fig. 4 illustrates a step in the manufacturing process of an intermediate semiconductor device 400. Many steps are required to create the structures on the substrate 402, such as arranging layers, covering, ablating, and the like, as will be apparent to those skilled in the art.

[0038] The semiconductor device 400 of Fig. 4 includes a substrate 402 including silicon or the like and shallow trench isolations 404 formed therein. The manufacturing process disposes a gate oxide dielectric 416 in the memory region and the second substrate region and a thicker gate dielectric in the first substrate region. In certain embodiments, the process may form semiconductor devices that are not strictly logic in the first and second substrate regions 418 and 420, as discussed below.

[0039] The process forms a first poly layer 408 on the substrate 402. The process patterns five hard mask 410 copies on the first poly layer 408. The process forms a nitride layer 412 on each oxide hard mask 410 copy. The cap layer includes a photoresist mask 414.

[0040] The region to the left of the leftmost shallow trench isolation 404A corresponds to a core (area or region) 418. The core 418 is an example of a memory region. The portion of the substrate 402 depicted to the right of the core 418 is a periphery (area or region) 420. In the periphery 420, the region between the two shallow trench isolations 404A and 404B corresponds to a region of the semiconductor device 400 that may be suitable for forming low-voltage logic. The remaining area of ​​the substrate 402 may be suitable for forming high-voltage logic. The semiconductor device 400 is an example of disposing a mask and a thick resist on a first substrate region.

[0041] Fig. 5 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 500. The process begins by removing, for example, by etching, the portions of the semiconductor device 500 that are unprotected by the photoresist mask 414, as shown generally at locations 502.

[0042] Fig. 6 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 600. The process removes the photoresist mask 414 and etches the core 418. The process places a blocking mask 602 over the periphery 420 to protect the first layer of poly 408 in the periphery 420. The process removes the nitride layers 412 and a portion of the oxide hard mask 410 in the core 418 by etching the core 418. The hard mask 410 over the first poly layer 408 in the core 418 protects the first poly layer 408 from etching to form select gates 604. Each select gate 604 may be 90 nanometers (nm) wide, but may also be from 15 nm to 100 nm wide. Other widths may also be used.

[0043] Fig. 7 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 700. The process removes the peripheral blocking mask 602. The process etches the gate oxide dielectric 416 completely, except under the gates. The process disposes an ONO charge-trapping dielectric 702 over the substrate 402. The ONO charge-trapping dielectric 702 may include a 5 nm bottom oxide, a 12.5 nm SiN layer, and an 8 nm oxide layer on top of the SiN. Other variations and combinations of thicknesses may be employed.

[0044] Fig. 8 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 800. The process places a second poly layer 802 over the entire structure 800. The process places a second periphery blocking mask 804. The process covers the second poly layer 802 in the periphery 420 and away from the core 418, creating sidewalls 806. The process performs appropriate patterning and then an N+ implantation to form, for example, source / drain regions 808 / 810.

[0045] Fig. 9 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 900. The process removes a periphery blocking mask 804 and forms a source blocking mask 904 so that portions of the second poly layer 802 can be removed, for example, by etching both the core 418 and the periphery 420. The process removes the entire second poly layer 802 in the periphery 420. The etch also removes select sidewalls 806 in the core 418. The remaining sidewalls 806 form memory gates 812. This etch is an example of removing a poly layer from a second sidewall of a select gate 604.

[0046] Fig. 10 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 1000. The process places a select gate-drain implant mask 1002. Source blocking mask 904 may be used as an element of the select gate-drain implant mask 1002. The process performs a second implant to extend the drains 808 for the select gates 604. The second implant covers the entire distance between consecutive select gates 604.

[0047] Fig. 11 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 1100. The process removes the ONO charge-trapping dielectric 702 by a wet etch over the memory region, the first gate region, and the second gate region, except beneath the memory gates and at the memory sidewall between the memory gate and the select gate, as indicated by arrows 1102. The process places a lightly doped, high-voltage drain mask 1104 over most of the substrate 402. The full hard mask stacks 412E and 410E on top of the poly 408 allow the lightly doped drains to be implanted without damaging the other elements of the semiconductor device 1100, particularly to prevent penetration of the first poly 408. The hard mask 410E may be approximately 5 nm to 70 nm thick. The hard mask 412E can be 10 nm to 70 nm thick. The regions of the first poly 408 that are not covered (ieThe first poly 408 (suitable for becoming a high-voltage transistor) is 90 nm thick. Semiconductor device 1100 is an example of a hard mask 410 that is thinner than a first gate because the first poly 408 can be formed into a high-voltage transistor 1106.

[0048] Fig. 12 illustrates a later step in the manufacturing process for forming an intermediate semiconductor device 1200. The process places a gate poly etch mask 1202 to cover the core 418 and the high-voltage region of the periphery 420. The process performs a 90 nm etch over the poly 408 in the low-voltage region of the periphery 420. The etch removes the SiON layer 412D and a portion of the hard mask 410D. An overetch would create less than approximately 24 nm of gouging in the shallow trench isolations 404. The 90 nm etch simultaneously removes a portion of the low-voltage region of the substrate 402 and the hard mask 410D. This etch patterns the low-voltage transistor 1204. The area where the low-voltage transistor 1204 is formed is an example of a second substrate region.The gate length of low-voltage transistor 1204 may be much shorter than the gate length of high-voltage transistor 1206, since low-voltage transistor 1204 may be configured to conduct a small amount of current. This processing is an example of forming a second gate, e.g., low-voltage transistor 1204, after forming memory gates 812.

[0049] Fig. Figure 13 illustrates another embodiment for replacing the steps in Fig. 12. The manufacturing process forms an intermediate semiconductor device 1300. The process removes the gate poly etch mask 1202 in the peripheral region 420. An etch patterns the low-voltage gate 1204, completely etches away the hard mask 412D and 412E, and at the same time partially removes the 410D and 410E on 1204 and 1106. The area where the high-voltage transistor 1106 is formed is an example of a first substrate region. A high-voltage transistor 1106 may be from approximately 0.1 micrometers wide to approximately 3 micrometers wide. In certain embodiments, a high-voltage transistor 1106 may be wider than 3 micrometers. The high-voltage transistor 1106 has the same thickness as the low-voltage transistor 1204. The process described above allows the high-voltage transistor 1106 to be patterned with the same thickness as the low-voltage transistor 1204 while allowing them to have different gate widths.

[0050] Following the step of Fig. 13, traditional manufacturing steps may be performed. These steps may include spacers, source and drain regions for the high-voltage transistor 1106 and the low-voltage transistor 1204. Additional steps include silicide, intermetal dielectric layers, contacts, metals, and the like.

[0051] A high-voltage transistor 1106 in the high-voltage substrate region is an example of a first logic transistor in the first substrate region. A low-voltage transistor 1204 in the low-voltage substrate region is an example of a second logic transistor in the second substrate region. One aspect of the semiconductor device 1300 of Fig. 13 is that the high-voltage transistor 1106 has the same thickness as the low-voltage transistor 1204. This common thickness can be between 40 nm and 100 nm.

[0052] Although Fig.4-13 show a specific number of memory cells 902 and transistors 1106 and 1204 being formed, other, presumably larger, numbers of these transistors may be formed according to this process.

[0053] Although embodiments have been described herein with reference to charge-trapping memories, the invention is not limited to these examples. Rather, embodiments of the invention are applicable to other types of computer memory. The invention is useful for both charge-trapping and floating-gate devices. This invention can be implemented with multi-level cells or other multi-bit technologies.

[0054] Embodiments of the present invention have been described above using functional blocks that represent the implementation of predetermined functions and their relationships. The boundaries of these functional blocks have been arbitrarily defined herein for convenience of description. Alternative boundaries may be defined as long as the predetermined functions and their relationships are implemented appropriately.

Claims

[1] A method of manufacturing a semiconductor device comprising a memory region, a first substrate region, and a second substrate region, comprising: forming a first gate in the first substrate region; forming a selection gate (108) in the memory region; disposing a charge trapping dielectric (114) in the memory region and the second substrate region; Disposing a gate layer in the memory region; removing the charge trapping dielectric (114) from the second substrate region; Forming a memory gate (110) on a sidewall of the select gate (108); forming a second gate in the second substrate region; wherein the memory gate (110) is formed before the second gate is formed; and wherein the first gate is formed before the memory gate (110) is formed. [2] The method of claim 1, further comprising disposing a hard mask (410) on the first substrate region, wherein a thickness of the hard mask (410) is thinner than a thickness of the first gate. [3] The method of claim 1, further comprising disposing a mask and a thick resist on the first substrate region. [4] The method of claim 1, further comprising disposing a lightly doped drain adjacent to the first gate in the first substrate region through a hard mask (410). [5] The method of claim 1, further comprising removing a hard mask (410) and simultaneously removing at least a portion of the second substrate region. [6] The method of claim 1, further comprising disposing a hard mask (410) on the first substrate region, the second substrate region, and the memory region. [7] The method of claim 1, further comprising forming the gate length of the first gate to be at least twice as long as the gate length of the second gate. [8] The method of claim 1, further comprising removing the gate layer from a second sidewall of the select gate (108). [9] The method of claim 1, further comprising forming the second gate having the same gate thickness as, but a different gate width than, the first gate. [10] The method of claim 1, further comprising forming the first substrate region as a high voltage substrate region and forming the second substrate region as a low voltage substrate region.

Citation Information

Patent Citations

  • Semiconductor device, and method of manufacturing the same

    JP2011103401A

  • JP002011103401A