Resin composition, process for its production and an uncrosslinked resin composition

A resin composition with a polyisobutylene backbone and silane-modified resin addresses the limitations of existing hoses by enhancing flexibility, water vapor barrier, and heat resistance, suitable for automobile air conditioner hoses.

DE112022006463T5Pending Publication Date: 2024-11-07THE YOKOHAMA RUBBER CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
DE112022006463
Authority / Receiving Office
DE · DE
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-09-29
Filing Date
2022-12-12
Publication Date
2024-11-07

AI Technical Summary

Technical Problem

Existing refrigerant transport hoses for automobile air conditioners, primarily made of rubber, face challenges with insufficient heat resistance, flexibility, and water vapor barrier properties, especially in high temperature and humidity environments, limiting their performance and installation in narrow spaces.

Method used

A resin composition comprising an elastomer with a polyisobutylene backbone and a silane-modified resin, with specific content ratios and a production method involving melt-kneading and silanol condensation catalyst addition during molding, followed by crosslinking with water or steam, to enhance flexibility, water vapor barrier properties, and heat resistance.

Benefits of technology

The resin composition achieves excellent flexibility, water vapor barrier properties, and heat resistance, suitable for refrigerant transport hoses, ensuring durability and ease of installation in confined automotive spaces.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A resin composition with excellent flexibility, water vapor barrier properties, and heat resistance is provided. The resin composition contains an elastomer with a polyisobutylene backbone and a silane-modified resin. The content of the elastomer with the polyisobutylene backbone is 30% or more and 90% or less by mass, based on the mass of the resin composition. The content of the silane-modified resin is 10% or more and 70% or less by mass, based on the mass of the resin composition. The water vapor permeability of the resin composition is 2.0 g / mm² / m². 2 ·24 h) or less. A ratio TB 100 / TB 25 a breaking strength TB 100 the resin composition at 100 °C to a breaking strength TB 25 The resin composition at 25 °C is 0.2 or more and 1.0 or less.
Need to check novelty before this filing date? Find Prior Art

Description

Technical area

[0001] The present invention relates to a resin composition, a process for producing the same, and an uncrosslinked resin composition. More specifically, the present invention relates to a resin composition with excellent flexibility, heat resistance, and water vapor barrier properties that can be used to manufacture a refrigerant transfer hose for a car air conditioner, a process for producing the same, and an uncrosslinked resin composition. State of the art

[0002] With the increasing demand for weight reduction in automobiles, efforts have been made to achieve weight reduction by producing a hose used for automobiles and made of rubber with resin with high barrier properties instead of rubber to reduce the thickness. In particular, the hose for refrigerant transport for current automotive air conditioning systems is mainly made of rubber, and if the main material can be replaced with a resin with high barrier properties, weight reduction can be achieved.

[0003] JP H04-145284 A (Patent Document 1) describes a hose for transporting a refrigerant such as Freon gas, wherein the outer tube of the hose is made of a thermoplastic elastomer containing thermoplastic polyolefin resin and EPDM or butyl rubber. Literature listPatent literature

[0004] Patent Document 1: JP H04-145284 A Brief description of the inventionTechnical problem

[0005] Car air conditioning systems and the like are installed in confined, narrow spaces within vehicles, and therefore, refrigerant transfer hoses require excellent flexibility and ease of installation even in tight spaces. The penetration of water vapor from the outside of a hose causes the moisture inside an air conditioner to freeze, and therefore the material used to form the outer tube of a refrigerant transfer hose must have excellent water vapor barrier properties. Furthermore, the refrigerant transfer hose must be robust enough to withstand long-term use in the high-temperature, high-humidity environment of an engine compartment.

[0006] However, since a thermoplastic elastomer constituting the outer tube of a resin hose described in Patent Document 1 contains thermoplastic polyolefin resin, heat resistance is not necessarily sufficient.

[0007] An object of the present invention is to provide a resin composition which can be used for producing an outer tube of a resin hose and which has excellent flexibility, water vapor barrier properties and heat resistance. Solution to the problem

[0008] One embodiment of the present invention (I) is a resin composition containing an elastomer having a polyisobutylene skeleton and a silane-modified resin. A content of the elastomer having a polyisobutylene skeleton is 30 mass % or more and 90 mass % or less based on the mass of the resin composition. A content of the silane-modified resin is 10 mass % or more and 70 mass % or less based on the mass of the resin composition. A water vapor permeability of the resin composition is 2.0 g·mm / (m 2 ·24 h) or less. A ratio of TB 100 / TB 25 a breaking strength TB 100 the resin composition at 100 °C to a breaking strength TB 25 of the resin composition at 25 °C is 0.2 or more and 1.0 or less.

[0009] One embodiment of the present invention (II) is a process for producing the resin composition of the embodiment of the present invention (I). The process comprises: preparing an uncrosslinked resin composition by melt-kneading an elastomer having a polyisobutylene backbone and a silane-modified resin; and adding a silanol condensation catalyst to the uncrosslinked resin composition during molding to mold the uncrosslinked resin composition.

[0010] One embodiment of the present invention (III) is an uncrosslinked resin composition containing an elastomer having a polyisobutylene skeleton and a silane-modified resin. The content of the elastomer having a polyisobutylene skeleton is 30 mass% or more and 90 mass% or less based on the mass of the uncrosslinked resin composition. The content of the silane-modified resin is 10 mass% or more and 70 mass% or less based on the mass of the uncrosslinked resin composition. The water vapor permeability after crosslinking of the uncrosslinked resin composition is 2.0 g·mm / (m 2 ·24 h) or less.

[0011] The present invention includes the following embodiments. [1] A resin composition containing an elastomer having a polyisobutylene backbone and a silane-modified resin, wherein a content of the elastomer having a polyisobutylene backbone is 30 mass% or more and 90 mass% or less based on the mass of the resin composition, a content of the silane-modified resin is 10 mass% or more and 70 mass% or less based on the mass of the resin composition, a water vapor permeability of the resin composition of 2.0 g·mm / (m 2 24h) or less and a ratio TB 100 / TB 25 a breaking strength TB 100 the resin composition at 100 °C to a breaking strength TB 25 the resin composition at 25 °C is 0.2 or more and 1.0 or less. [2] The resin composition according to [1], wherein the silane-modified resin is a resin obtained by modifying a polyolefin-based thermoplastic resin with a silane compound. [3] The resin composition according to [1] or [2], wherein the silane-modified resin is silane-modified polypropylene. [4] The resin composition according to any one of [1] to [3], wherein the resin composition contains a silanol condensation catalyst. [5] The resin composition according to any one of [1] to [4], wherein the elastomer having a polyisobutylene backbone is butyl rubber or modified butyl rubber. [6] The resin composition according to any one of [1] to [5], wherein the elastomer is dynamically crosslinked with a polyisobutylene backbone. [7] The resin composition according to any one of [1] to [6], wherein the resin composition contains 1 mass% or more and 4 mass% or less of an anti-aging agent based on the mass of the resin composition. [8] The resin composition according to any one of [1] to [7], wherein the resin composition has a matrix / fibril structure consisting of a matrix containing the silane-modified resin and a domain containing the elastomer having a polyisobutylene backbone dispersed in the matrix, and wherein the matrix is ​​crosslinked. [9] A process for producing the resin composition according to any one of [1] to [8], the process comprising: Producing an uncrosslinked resin composition by melt-kneading an elastomer having a polyisobutylene backbone and a silane-modified resin; and Adding a silanol condensation catalyst to an uncrosslinked resin composition during molding to mold the uncrosslinked resin composition.

[10] The method according to [9] further comprises, after the step of adding a silanol condensation catalyst to an uncrosslinked resin composition during molding to mold the uncrosslinked resin composition, preparing a crosslinked resin composition by contacting the molded uncrosslinked resin composition with water or water vapor.

[11] An uncrosslinked resin composition containing an elastomer having a polyisobutylene backbone and a silane-modified resin, wherein a content of the elastomer having a polyisobutylene backbone is 30 mass% or more and 90 mass% or less based on the mass of the uncrosslinked resin composition, a content of the silane-modified resin is 10 mass% or more and 70 mass% or less based on the mass of the uncrosslinked resin composition, and a water vapor permeability after crosslinking of the uncrosslinked resin composition of 2.0 g·mm / (m 2 24 hours) or less.

[12] The uncrosslinked resin composition according to

[11] , wherein after crosslinking of the uncrosslinked resin composition a ratio TB 100 / TB 25 a breaking strength TB 100 at 100 °C to a breaking strength TB 25 at 25 °C is 0.2 or more and 1.0 or less. Advantageous effects of the invention

[0012] The resin composition of one embodiment of the present invention has excellent flexibility, water vapor barrier properties and heat resistance. Description of embodiments

[0013] The resin composition of one embodiment of the present invention contains elastomer having a polyisobutylene backbone and a silane-modified resin.

[0014] The elastomer having a polyisobutylene backbone is not limited as long as the elastomer has a polyisobutylene backbone, but is preferably butyl rubber (IIR), modified butyl rubber, or a styrene-isobutylene-styrene block copolymer, and is more preferably butyl rubber or modified butyl rubber. The polyisobutylene backbone refers to a chemical structure formed by polymerizing a variety of isobutylenes, that is, a chemical structure represented by -[-CH2-C(CH3)2- n - (but n is an integer of 2 or more). Butyl rubber refers to an isobutylene-isoprene copolymer obtained by copolymerizing isobutylene and a small amount of isoprene and is abbreviated as IIR. Modified butyl rubber refers to butyl rubber in which a double bond, a halogen, etc., are present in an isoprene skeleton. As the modified butyl rubber, halogenated butyl rubber is preferred, brominated butyl rubber and chlorinated butyl rubber are more preferred, and brominated butyl rubber is even more preferred.

[0015] A styrene-isobutylene-styrene block copolymer is abbreviated as SIBS.

[0016] Because the resin composition contains the elastomer with a polyisobutylene backbone, the flexibility and water vapor barrier properties of the resin composition are improved. The elastomer with a polyisobutylene backbone is preferably dynamically crosslinked. Dynamic crosslinking improves durability.

[0017] The content of the elastomer with a polyisobutylene backbone is 30 mass% or more and 90 mass% or less, preferably 40 mass% or more and 89 mass% or less, and more preferably 50 mass% or more and 88 mass% or less, based on the mass of the resin composition. If the content of the elastomer with a polyisobutylene backbone is too low, flexibility cannot be ensured. If the content is too high, extrudability deteriorates.

[0018] The resin composition contains silane-modified resin. The resin composition achieves improved heat resistance because it contains silane-modified resin.

[0019] The silane-modified resin refers to a resin modified with a silane compound. The silane-modified resin is preferably a resin obtained by modifying a polyolefin-based thermoplastic resin with a silane compound, and is more preferably a crosslinkable resin having a hydrolyzable silyl group (preferably an alkoxysilyl group) obtained by modifying a polyolefin-based thermoplastic resin with a silane compound, or a crosslinked resin obtained by crosslinking the crosslinkable resin.

[0020] The silane compound is not limited, but is preferably a compound represented by formula (1). R 1 -SiR 2 n Y 3-n (1) R 1 is an ethylenically unsaturated hydrocarbon group, R 2is a hydrocarbon group, Y is a hydrolyzable organic group, and n is an integer from 0 to 2.

[0021] R 1 is preferably an ethylenically unsaturated hydrocarbon group having 2 to 10 carbons, and examples thereof include a vinyl group, a propenyl group, a butenyl group, a cyclohexenyl group, and a γ-(meth)acryloyloxypropyl group. R 2 is preferably a hydrocarbon group having 1 to 10 carbons, and examples thereof include a methyl group, an ethyl group, a propyl group, a decyl group, and a phenyl group.

[0022] Y is preferably a hydrolyzable organic group having 1 to 10 carbons, and examples thereof include an alkoxy group (e.g., a methoxy group, an ethoxy group), a formyloxy group, an acetoxy group, a propionyloxy group, an alkylamino group, and an arylamino group.

[0023] Specific examples of the silane compound include vinyltrimethoxysilane, vinyltriethoxysilane, vinyltriacetoxysilane, and γ-methacryloyloxypropyltrimethoxysilane. Of these, vinyltrimethoxysilane is preferred.

[0024] The polyolefin-based thermoplastic resin constituting the silane-modified resin is not limited, and examples include polyethylene, a copolymer of ethylene and α-olefin, polypropylene, and a copolymer of propylene and another α-olefin. Preferred are polypropylene and a copolymer of propylene and another α-olefin, and particularly preferred is polypropylene.

[0025] The hydrolyzable silyl group refers to a group that produces a silanol group (=Si-OH) by hydrolysis, and is preferably a group represented by formula (2). -SiR 2 n Y 3-n (2)

[0026] However, R 2and Y as described above.

[0027] A crosslinkable resin refers to a resin that can undergo a crosslinking reaction but is not yet crosslinked. A crosslinked resin refers to a resin formed by crosslinking a crosslinkable resin. The type of crosslinking reaction is not limited and can be crosslinked by a peroxide, but crosslinking by moisture (water crosslinking) is preferred.

[0028] The method for modifying with a silane compound is not limited, and examples include grafting and copolymerization. Grafting is a method in which a silane compound is added to a resin through a grafting reaction, and specifically, it is a reaction in which a carbon radical is generated by breaking a carbon-hydrogen bond of a polyolefin, and a silane compound having an ethylenically unsaturated hydrocarbon group is added to the carbon radical. The modification can preferably be carried out by melt-kneading resin and a silane compound of the formula (1) in the presence of a radical generator such as an organic peroxide. The copolymerization can preferably be carried out by radical copolymerization of a resin-constituting monomer and a silane compound of the formula (1).

[0029] The silane-modified resin is preferably silane-modified polypropylene. The silane-modified resin is commercially available, and a commercially available product can be used as the silane-modified resin used for one embodiment of the present invention. Examples of the commercially available silane-modified resin include "Linklon" (trade name), available from Mitsubishi Chemical Corporation.

[0030] The content of the silane-modified resin is 10 mass% or more and 70 mass% or less, preferably 11 mass% or more and 60 mass% or less, and more preferably 12 mass% or more and 50 mass% or less, based on the mass of the resin composition. If the content of the silane-modified resin is too low, extrudability deteriorates. If the content is too high, flexibility cannot be ensured.

[0031] The resin composition may contain other resins besides the silane-modified resin. Examples of resins other than the silane-modified resin include polyolefin resin and polyamide resin. Examples of the polyolefin resin include polypropylene. By blending the polypropylene with the silane-modified resin, a phase structure is formed that tends to exhibit rigidity upon heating because the viscosity of the resin component becomes stable. Furthermore, since the water vapor barrier properties of the polypropylene are good, the water vapor barrier properties of the entire composition are also good.

[0032] In a case where the resin composition contains a resin other than the silane-modified resin, the content of the resin other than the silane-modified resin is preferably 1 mass% or more and 60 mass% or less, more preferably 2 mass% or more and 55 mass% or less, and even more preferably 3 mass% or more and 50 mass% or less, based on the mass of the resin composition.

[0033] The water vapor permeability of the resin composition is 2.0 g·mm / (m 2 ·24h) or less and preferably 1.9 g·mm / (m 2 ·24 h) or less.

[0034] If the water vapor permeability is within the numerical range described above, flexibility and water vapor barrier properties can be provided in a compatible manner.

[0035] The water vapor permeability is measured at a temperature of 60 °C and a relative humidity of 95% using a water vapor permeability tester.

[0036] The resin composition has a ratio TB 100 / TB 25 the breaking strength TB 100 at 100 °C to breaking strength TB 25 at 25 °C of 0.2 or more and 1.0 or less, preferably 0.3 or more and 1.0 or less, and more preferably 0.35 or more and 1.0 or less. If the TB 100 / TB 25 is closer to 1.0, better heat resistance is achieved. By crosslinking the silane-modified resin, the TB 100 / TB 25 into the numerical range described above, and the heat resistance is improved.

[0037] The ultimate tensile strength can be measured according to the method specified in JIS K 6251 “Rubber, vulcanized or thermoplastic - Determination of tensile stress-strain properties”.

[0038] The resin composition preferably contains a silanol condensation catalyst. When the silanol condensation catalyst is included, crosslinking of the silane-modified resin is promoted. Examples of the silanol condensation catalyst include, but are not limited to, a metal salt of an organic acid, a titanate, a borate, an organic amine, an ammonium salt, a phosphonium salt, an inorganic acid, an organic acid, an ester of an inorganic acid, and a bismuth compound.

[0039] Examples of the metal salt of an organic acid include, but are not limited to, dibutyltin dilaurate, dioctyltin dilaurate, dibutyltin diacetate, dibutyltin dioctoate, stannous acetate, stannous octanoate, cobalt naphthenate, lead octylate, lead naphthenate, zinc octylate, zinc caprylate, ferrous 2-ethylhexanoate, ferrous octylate, and ferrous stearate. Examples of the titanate include, but are not limited to, tetrabutyl titanate, tetranonyl titanate, and bis(acetylacetonitrile) diisopropyl titanate. Examples of the organic amine include, but are not limited to, ethylamine, dibutylamine, hexylamine, triethanolamine, dimethylsoyamine, tetramethylguanidine, and pyridine. Examples of the ammonium salt include, but are not limited to, ammonium carbonate and tetramethylammonium hydroxide.

[0040] Examples of the phosphonium salt include, but are not limited to, tetramethylphosphonium hydroxide. Examples of the inorganic acid include, but are not limited to, sulfuric acid and hydrochloric acid. Examples of the organic acid include, but are not limited to, acetic acid, stearic acid, maleic acid, toluenesulfonic acid, and sulfonic acid such as alkylnaphthylsulfonic acid. Examples of the inorganic acid ester include, but are not limited to, a phosphoric acid ester. Examples of the bismuth compound include, but are not limited to, organic bismuth such as bismuth 2-ethylhexanoate.

[0041] The silanol condensation catalyst is preferably a metal salt of an organic acid, a sulfonic acid, or a phosphoric acid ester, and more preferably a metal carboxylate of tin, such as dioctyltin dilaurate, alkyl naphthylsulfonic acid, and ethylhexyl phosphate. One type of silanol condensation catalyst can be used alone, or two or more types of silanol condensation catalysts can be combined and used as appropriate.

[0042] The content of the silanol condensation catalyst is not particularly limited, but is preferably from 0.0001 to 0.5 parts by mass, and more preferably from 0.0001 to 0.3 parts by mass, with respect to 100 parts by mass of the silane-modified resin.

[0043] The silanol condensation catalyst is preferably used as a silanol condensation catalyst-containing base composition in which a resin and a silanol condensation catalyst are mixed. Examples of the resin that can be used for this silanol condensation catalyst-containing base composition include a polyolefin, and polyethylene, polypropylene, and a copolymer thereof are preferred. In a case where the silanol condensation catalyst is used as a silanol condensation catalyst-containing base mixture in which a resin and a silanol condensation catalyst are mixed, the content of the silanol condensation catalyst in the base mixture is preferably, but not limited to, 0.1 to 5.0 mass %. A commercially available product, for example, "PZ010" available from Mitsubishi Chemical Corporation, can be used as the silanol condensation catalyst-containing base mixture.

[0044] The resin composition preferably contains an antiaging agent. When the antiaging agent is included, extrusion moldability becomes good. Examples of the antiaging agent include, but are not limited to, a hindered phenol-based antioxidant, a phenol-based antioxidant, an amine-based antioxidant, a phosphorus-based heat stabilizer, a metal deactivator, and a sulfur-based heat-resistant stabilizer. A hindered phenol-based antioxidant is preferred, and a hindered phenol-based antioxidant having a pentaerythritol ester structure is more preferred. Specific examples of the hindered phenol-based antioxidant include IRGANOX (trade name) 1010 (pentaerythritol tetrakis[3-(3,5-ditert-butyl-4-hydroxyphenyl)propionate]), available from BASF Japan Ltd.The content of the anti-aging agent is preferably 1 mass% or more and 4 mass% or less, and more preferably 1 mass% or more and 3.5 mass% or less, based on the mass of the resin composition.

[0045] The resin composition may contain an elastomer other than the elastomer having a polyisobutylene skeleton, a resin other than the silane-modified resin, and an additive other than the silanol condensation catalyst and the antiaging agent within a range not impairing the effect of the present invention.

[0046] The resin composition can have any phase structure, but preferably has a matrix / fibril structure or a co-continuous structure, and more preferably has a matrix / fibril structure consisting of a matrix (matrix phase) containing a silane-modified resin and a domain (fibril phase) containing an elastomer with a polyisobutylene backbone dispersed in the matrix, the matrix being cross-linked. The cross-linking of the matrix contributes to heat resistance. In the case of a co-continuous structure, excellent flexibility is achieved.

[0047] The method for producing the resin composition is not limited, but preferably includes: preparing an uncrosslinked resin composition by melt-kneading an elastomer having a polyisobutylene skeleton and a silane-modified resin; and adding a silanol condensation catalyst to an uncrosslinked resin composition during molding to mold the uncrosslinked resin composition.

[0048] The production of an uncrosslinked resin composition by melt kneading an elastomer having a polyisobutylene backbone and a silane-modified resin may hereinafter also be referred to simply as the “melt kneading process”. Melt kneading is not limited, but may be carried out using a kneader, a single-screw or twin-screw extruder, or the like. The temperature during melt kneading is not limited as long as melt kneading can be carried out, but is preferably 170 to 240 °C. The time for melt kneading is not limited as long as the desired kneading material can be produced, but is preferably 2 to 10 minutes. In the melt kneading process, the elastomer with a polyisobutylene backbone and the silane-modified resin, as well as optionally various additives such as an anti-aging agent, are placed in a kneader or the like and melt-kneaded. However, the silanol condensation catalyst is preferably not added during the melt-kneading process. In a case where the silanol condensation catalyst is added during the melt-kneading process, the silane-modified resin in the resin composition gradually crosslinks when the uncrosslinked resin composition prepared by the melt-kneading process is brought into contact with water vapor in the atmosphere, and molding the resin composition after crosslinking becomes difficult. Therefore, the silanol condensation catalyst is preferably added to the uncrosslinked resin composition during molding.

[0049] The step of adding a silanol condensation catalyst to an uncrosslinked resin composition during molding to mold the uncrosslinked resin composition is also simply referred to as "silanol condensation catalyst addition and molding process." "During molding" refers to simultaneously with molding or within 6 hours before molding. Examples of molding include, but are not limited to, extrusion molding and injection molding, and extrusion molding is preferred. Extrusion molding can be performed using an extruder, but is not limited thereto, and is preferably performed using a single-screw extruder. The silanol condensation catalyst may be added to the uncrosslinked resin composition before the composition is filled into the extruder, the uncrosslinked resin composition and the silanol condensation catalyst may be filled into the extruder at the same time, or the uncrosslinked resin composition and the silanol condensation catalyst may be filled into separate filling ports of the extruder.

[0050] The silanol condensation catalyst can be added directly to the uncrosslinked resin composition, but is preferably added as a silanol condensation catalyst-containing masterbatch in which the resin and a silanol condensation catalyst are mixed. Molding conditions are not limited as long as the desired molded product can be formed.

[0051] The method for producing the resin composition preferably includes, after the step of adding a silanol condensation catalyst to an uncrosslinked resin composition during molding to mold the uncrosslinked resin composition, preparing a crosslinked resin composition by contacting the molded uncrosslinked resin composition with water or water vapor (hereinafter also simply referred to as "water contact method").

[0052] When the uncrosslinked resin composition formed by the silanol condensation catalyst addition and molding method is brought into contact with water vapor in the air, the silane-modified resin in the composition gradually crosslinks to form a crosslinked resin composition; however, if rapid preparation of a crosslinked resin composition is desired, the water contact method is preferably carried out.

[0053] Examples of the method of contacting with water or water vapor include, but are not limited to, a method of soaking in a water bath, a method of spraying with water, and a method of placing in a water vapor-containing atmosphere, but preferred is a method of placing in a water vapor-containing atmosphere. In the method of placing in a water vapor-containing atmosphere, the outer layer is allowed to stand in the air for 1 minute to 1 month, preferably 1 hour to 1 week, and more preferably 1 to 4 days at a temperature of room temperature to 200°C, preferably room temperature to 100°C, and a relative humidity of 30 to 100%, and preferably 40 to 90%. More specifically, the outer layer is preferably allowed to stand in the air for 72 hours or more at a temperature of 25°C and a relative humidity of 50%.By the water contact method, a hydrolyzable silyl group (preferably an alkoxysilyl group) in the silane-modified resin in the uncrosslinked resin composition is hydrolyzed to form a silanol group, silanol groups undergo a condensation reaction to form a siloxane bond (Si-O-Si) for crosslinking, and thus a crosslinked resin composition is obtained.

[0054] The present invention (III) relates to an uncrosslinked resin composition. An uncrosslinked resin composition of one embodiment of the present invention is an uncrosslinked resin composition containing an elastomer having a polyisobutylene skeleton and a silane-modified resin. A content of the elastomer having a polyisobutylene skeleton is 30 mass % or more and 90 mass % or less based on the mass of the uncrosslinked resin composition. A content of the silane-modified resin is 10 mass % or more and 70 mass % or less based on the mass of the uncrosslinked resin composition. A water vapor permeability after crosslinking of the uncrosslinked resin composition is 2.0 g·mm / (m 2 ·24 h) or less.

[0055] The uncrosslinked resin composition refers to a resin composition that has not yet been crosslinked. Uncrosslinked means that the resin composition has not undergone a water contact process.

[0056] The elastomer with polyisobutylene backbone, the silane-modified resin and the water vapor permeability are as described above.

[0057] The uncrosslinked resin composition crosslinks when brought into contact with water or water vapor to form a crosslinked resin composition.

[0058] The uncrosslinked resin composition after crosslinking has a ratio TB 100 / TB 25 the breaking strength TB 100 at 100 °C to breaking strength TB 25 at 25 °C of preferably 0.2 or more and 1.0 or less, more preferably 0.3 or more and 1.0 or less, and even more preferably 0.35 or more and 1.0 or less. "After crosslinking the uncrosslinked resin composition" means after the uncrosslinked resin composition is adequately crosslinked. The crosslinking conditions are not limited as long as sufficient crosslinking is allowed. For example, 1 mass% of a silanol condensation catalyst (silane crosslinking agent masterbatch PZ010, available from Mitsubishi Chemical Corporation) is added to the uncrosslinked resin composition, and the mixture is allowed to stand in air for 72 hours at a temperature of 25°C and a relative humidity of 50%. Adequate networking means that fluctuations in TB 100 of the silane-modified resin per hour of crosslinking time is within 10%, which corresponds to a steady state. Example starting materials

[0059] The starting materials used in the following examples and comparative examples are as follows. IIR: Butyl rubber “Exxon Butyl” 268, available from ExxonMobil Chemical Co. Br-IIR: Brominated butyl rubber “Exxon Bromobutyl” 2255, available from ExxonMobil Chemical Co. PP / EPDM: Thermoplastic PP / EPDM elastomer “Santoprene” (trade name) 111-35, available from ExxonMobil Japan GK Rubber crosslinking agent: Alkylphenol-formaldehyde resin “Hitanol” (trade name) 2501Y, available from Hitachi Chemical Co., Ltd. ZnO: Zinc oxide III, available from Seido Chemical Industry Co., Ltd. Silane-modified resin: Silane-modified polypropylene “Linklon” (trade name) XPM800HM, available from Mitsubishi Chemical Corporation PP: Propylene homopolymer “Prime Polypro” (trade name) J108M, available from Prime Polymer Co., Ltd. Anti-aging agent: Hindered phenol-based antioxidant “IRGANOX” (trade name) 1010, available from BASF Japan Ltd. Silanol condensation catalyst: Silane crosslinker masterbatch “Catalyst MB” PZ010, available from Mitsubishi Chemical Corporation Examples 1 to 5 and Comparative Example 1

[0060] The raw materials were charged into a twin-screw extruder (available from The Japan Steel Works, Ltd.) at the blending proportions shown in Table 1 and kneaded at 235 °C for 3 minutes. The kneaded product was continuously extruded from the twin-screw extruder in a strand-like shape, cooled with water, and then cut with a knife to obtain a pellet-shaped resin composition.

[0061] For the resulting resin composition, the water vapor permeability, flexibility, extrudability, and fracture toughness were measured and evaluated at 25 °C and 100 °C. The measurement and evaluation results are shown in Table 1. Comparison example 2

[0062] Using the PP / EPDM thermoplastic elastomer "Santoprene" (trade name) 111-35, available from ExxonMobil Japan GK, as Comparative Example 2, the water vapor permeability, flexibility, extrudability, and fracture toughness were measured and evaluated at 25 °C and 100 °C. The measurement and evaluation results are shown in Table 1.

[0063] The measurement and evaluation methods are as follows. Measurement of water vapor permeability

[0064] A sample of the resin composition to which the silanol condensation catalyst was added was formed into a film with an average thickness of 0.2 mm using a 40 mm diameter single-screw extruder (available from Pla Giken Co., Ltd.) equipped with a 550 mm wide T-shaped die, with the cylinder and die temperatures set at a temperature of 10 °C plus the melting point of the polymer component with the highest melting point in the sample composition, a chill roll temperature of 50 °C, and a take-up speed of 3 m / min.

[0065] The obtained film was crosslinked by leaving it in air at a temperature of 25 °C and a relative humidity of 50% for 72 hours and then measured at a temperature of 60 °C and a relative humidity of 95% using a water vapor transmission tester from GTR Tec Corporation.

[0066] Water vapor permeability is an indicator of water vapor barrier properties, and lower water vapor permeability indicates excellent water vapor barrier properties. Assessment of flexibility

[0067] The cross-linked film prepared for the water vapor permeability measurement, with an average thickness of 0.2 mm, was punched into a dumbbell shape according to JIS No. 3 and subjected to tensile tests at a temperature of 25 °C and a speed of 500 mm / min according to the measurement method specified in JIS K 6251 "Rubber, Vulcanized or Thermoplastic - Determination of Tensile Stress-Strain Properties." Based on the obtained stress-strain curve, a stress at 10% strain (10% modulus) was determined.

[0068] The 10% modulus is an indicator of flexibility, and a lower 10% modulus indicates greater flexibility. Flexibility is rated as passing if the 10% modulus is 10 MPa or less, and failing if the 10% modulus is above 10 MPa. Assessment of extrudability

[0069] A sample of the resin composition to which the silanol condensation catalyst was added was formed into a film with an average thickness of 0.2 mm using a 40 mm diameter single-screw extruder (available from Pla Giken Co., Ltd.) equipped with a 550 mm wide T-shaped die, with the cylinder and die temperatures set at a temperature of 10 °C plus the melting point of the polymer component with the highest melting point in the sample composition, a chill roll temperature of 50 °C, and a take-up speed of 3 m / min. The thickness of each of the films was 0.2 mm, and a case where there were no problems during molding was rated as “◯”, a case where slight dents or holes or cuts occurred at a film edge was rated as “△”, and a case where a serious dent or hole or cut occurred at a film edge was rated as “×”. Measurement of breaking strength

[0070] The film obtained during the water vapor permeability measurement, with an average thickness of 0.2 mm, was left to stand in air for 72 hours or more at a temperature of 25°C and a relative humidity of 50%, and a film of the crosslinked resin composition was prepared. The film of the crosslinked resin composition was punched into a dumbbell shape according to JIS No. 3 and subjected to tensile tests at a temperature of 25°C and a speed of 500 mm / min, and at a temperature of 100°C and a speed of 500 mm / min according to the measurement method specified in JIS K 6251 "Rubber, Vulcanized or Thermoplastic - Determination of Tensile Stress-Strain Properties." Based on the obtained stress-strain curve, the ultimate stress (breaking strength) was determined.

[0071] Using the breaking strength at 25 °C as TB 25and the breaking strength at 100 °C as TB 100 a ratio TB 100 / TB 25 calculated. The TB 100 / TB 25 is an indicator of heat resistance, and a TB 100 / TB 25 closer to 1.0 indicates superior heat resistance. Table 1-I Table 1 Example 1 Example 2 Example 3 Example 4 IIR Mass-produced parts 48 68 68 70 BR-IIR Mass-produced parts PP / EPDM Mass-produced parts Rubber crosslinking agent Mass-produced parts 1 1 1 1 ZnO Mass-produced parts Silane-modified resin Mass-produced parts 47 13 27 28 PP Mass-produced parts 13 Anti-aging agents Mass-produced parts 2 3 3 Silanol condensation catalyst Mass-produced parts 2 2 1 1 In total Mass-produced parts 100 100 100 100 Water vapor permeability: g·mm / (m 2 ·24h) 1,5 1,5 1,8 1,8 flexibility Passed Passed Passed Passed Extrusion ◯ ◯ ◯ △ availability TB 100 MPa 7,4 3,5 2,7 2,7 TB 25 MPa 17,7 9,2 6,5 6,5 TB 100 / TB 25 0,42 0,38 0,42 0,42 Table 1-II Table 1 Example 5 Comparison example 1 Comparison example 2 IIR Mass-produced parts 72 BR-IIR Mass-produced parts 69 PP / EPDM Mass-produced parts 100 Rubber crosslinking agent Mass-produced parts 1 ZnO Mass-produced parts 2 Silane-modified resin Mass-produced parts 23 PP Mass-produced parts 29 Anti-aging agents Mass-produced parts 3 Silanol condensation catalyst Mass-produced parts 1 In total Mass-produced parts 100 100 100 Water vapor permeability: g·mm / (m 2 ·24h) 1,9 1,7 14,1 flexibility Passed Passed Passed Extrudability ◯ ◯ ◯ TB 100 MPa 2,3 1,2 0,8 TB 25 MPa 5,4 8 1,7 TB 100 / TB 25 0,42 0,15 0,47 Industrial applicability

[0072] The resin composition of one embodiment of the present invention can be suitably used as a raw material for producing a molded product requiring flexibility, heat resistance, and water vapor barrier properties, such as a refrigerant transport hose. QUOTES CONTAINED IN THE DESCRIPTION

[0000] This list of documents submitted by the applicant was generated automatically and is included solely for the convenience of the reader. This list is not part of the German patent or utility model application. The DPMA assumes no liability for any errors or omissions. Cited patent literature

[0000] JP H04-145284 A [0003, 0004]

Claims

[1] Resin composition containing an elastomer with a polyisobutylene backbone and a silane-modified resin, wherein a content of the elastomer having a polyisobutylene backbone is 30 mass% or more and 90 mass% or less based on the mass of the resin composition, a content of the silane-modified resin is 10 mass% or more and 70 mass% or less based on the mass of the resin composition, a water vapor permeability of the resin composition of 2.0 g·mm / (m 2 24h) or less and a ratio TB 100 / TB 25 a breaking strength TB 100 the resin composition at 100 °C to a breaking strength TB 25 the resin composition at 25 °C is 0.2 or more and 1.0 or less. [2] The resin composition according to claim 1, wherein the silane-modified resin is a resin obtained by modifying a polyolefin-based thermoplastic resin with a silane compound. [3] The resin composition according to claim 1 or 2, wherein the silane-modified resin is silane-modified polypropylene. [4] The resin composition according to any one of claims 1 to 3, wherein the resin composition contains a silanol condensation catalyst. [5] The resin composition according to any one of claims 1 to 4, wherein the elastomer having a polyisobutylene skeleton is butyl rubber or modified butyl rubber. [6] The resin composition according to any one of claims 1 to 5, wherein the elastomer is dynamically crosslinked with a polyisobutylene backbone. [7] The resin composition according to any one of claims 1 to 6, wherein the resin composition contains 1 mass% or more and 4 mass% or less of an anti-aging agent based on the mass of the resin composition. [8] The resin composition according to any one of claims 1 to 7, wherein the resin composition has a matrix / fibril structure consisting of a matrix containing the silane-modified resin and a domain containing the elastomer having a polyisobutylene backbone dispersed in the matrix, and the matrix is crosslinked. [9] A process for producing the resin composition according to any one of claims 1 to 8, the process comprising: Producing an uncrosslinked resin composition by melt-kneading an elastomer having a polyisobutylene backbone and a silane-modified resin; and Adding a silanol condensation catalyst to an uncrosslinked resin composition during molding to mold the uncrosslinked resin composition. [10] The method of claim 9, further comprising: after the step of adding a silanol condensation catalyst to an uncrosslinked resin composition during molding to mold the uncrosslinked resin composition, preparing a crosslinked resin composition by contacting the molded uncrosslinked resin composition with water or water vapor. [11] Uncrosslinked resin composition containing an elastomer having a polyisobutylene backbone and a silane-modified resin, wherein a content of the elastomer having a polyisobutylene backbone is 30 mass% or more and 90 mass% or less based on the mass of the uncrosslinked resin composition, a content of the silane-modified resin is 10 mass% or more and 70 mass% or less based on the mass of the uncrosslinked resin composition, and a water vapor permeability after crosslinking of the uncrosslinked resin composition of 2.0 g·mm / (m 2 24 hours) or less. [12] The uncrosslinked resin composition according to claim 11, wherein after crosslinking the uncrosslinked resin composition, a ratio TB 100 / TB 25 a breaking strength TB 100 at 100 °C to a breaking strength TB 25 at 25 °C is 0.2 or more and 1.0 or less.

Citation Information

Patent Citations

  • Low permeable hose

    JP1992145284A