Austenitic heat-resistant Cr-Mn-N steel

DE202017007705U1Active Publication Date: 2024-10-31TIANJIN NEW WEISAN INDS
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE202017007705
Authority / Receiving Office
DE · DE
Patent Type
Utility models
Current Assignee / Owner
Priority Date
2016-08-26
Filing Date
2017-08-25
Publication Date
2024-10-31
Estimated Expiration
2027-08-31
Patent Text Reader

Abstract

Cr-Mn-N austenitic, heat-resistant steel, comprising, in wt%: 0.30% to 0.45% carbon, 0.80% to 1.50% silicon, 3.00% to 4.80% manganese, less than 0.02% phosphorus, less than 0.02% sulfur, 23.00% to 26.00% chromium, 6.00% to 8.00% nickel, less than 0.20% molybdenum, less than 0.30% niobium, less than 0.40% tungsten, less than 0.12% vanadium, 0.30 to 0.60% nitrogen, less than 0.08% zirconium, less than 0.08% cobalt, less than 0.08% yttrium, less than 0.10% boron, otherwise iron.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELDThis invention relates to the field of steel for automobiles, and more particularly to an austenitic, heat-resistant Cr-Mn-N steel.BACKGROUNDWith higher function and ease of automobiles, the temperature of the vehicle exhaust gas is increased due to an increase in engine speed, and the highest operating temperature of the exhaust manifold and the turbocharger connected to the engine may increase to 1050° C. or even higher. Accordingly, this requires that materials used for the turbine housing and the exhaust manifold not only have sufficient strength at high temperatures and heat resistance, but also have good dimensional stability and high ductility, as well as good thermal conductivity during their long-term operation at elevated temperature.Currently, the materials of the turbocharger housing and exhaust manifold are mainly ductile Hi-Sil-Moly iron and ductile Ni-resist iron (see CN 103898398A and CN 103898397A). The highest working temperature of the materials is below 1000°C and cannot operate normally at higher temperatures. Further, the materials have problems in working at temperatures above 1000° C., such as low thermal conductivity, a decrease in strength at high temperatures, and a high thermal expansion coefficient associated with oxidation and thermal fatigue limit. Moreover, the materials also have a disadvantage of high cost due to addition of a large amount of nickel elements. Therefore, these materials cannot meet the requirements for high performance engines.SUMMARYIn view of this, an object of the present invention is to provide an austenitic heat-resistant Cr-Mn-N steel having high strength at high temperatures, high thermal conductivity and low thermal expansion coefficient, as well as properties of high metallographic structural stability, good dimensional stability, high ductility, heat resistance, impact resistance and low manufacturing cost, in order to meet the requirements of high performance engines.In order to achieve the above object, the present invention provides the following technical overview.The present invention provides an austenitic, heat-resistant Cr-Mn-N steel comprising, in weight percent: 0.20% to 0.50% carbon, 0.50% to 2.00% silicon, 2.00% to 5.00% manganese, less than 0.04% phosphorus, less than 0.03% sulfur, 20.00% to 27.00% chromium, 6.00% to 8.00% nickel, less than 0.50% molybdenum, less than 0.60% niobium, less than 0.60% tungsten, less than 0.15% vanadium, 0.30 to 0.60% nitrogen, less than 0.08% zirconium, less than 0.10% cobalt, less than 0.10% yttrium, less than 0.20% boron, otherwise iron.The austenitic Cr-Mn-N heat resistant steel preferably comprises, in weight percent: 0.30% to 0.45% carbon; 0.80% to 1.50% silicon; 3.00% to 4.80% manganese; less than 0.02% phosphorus; less than 0.02% sulfur; 23.00% to 26.00% chromium; 6.50% to 7.00% nickel; less than 0.20% molybdenum; less than 0.30% niobium; less than 0.40% tungsten; less than 0.12% vanadium; 0.40 to 0.50% nitrogen; less than 0.08% zirconium; less than 0.08% cobalt; less than 0.08% yttrium; less than 0.10% boron, otherwise iron.In the present invention, both the manganese and nitrogen elements can facilitate austenite formation, and the nitrogen element has a 30 times greater ability to facilitate austenite formation than the nickel element. The nickel element is replaced with the manganese and nitrogen elements to facilitate austenite formation. The cost of the manganese and nitrogen elements is only 20% to 30% of the cost of the nickel element. Thus, the austenitic heat-resistant steel can be produced at a lower production cost. Moreover, the nitrogen element can also stabilize the microstructure at elevated temperatures, improve strength at elevated temperatures, improve pitting resistance, and resist stress corrosion cracking. The manganese element can act as a good desulfurization agent and a good deoxidizing agent, thus maintaining the content of sulfur and oxygen in the liquid steel at a lower level, improving the instantaneous strength at elevated temperatures, and improving the creep rupture strength and the creep performance of the material. The austenitic heat-resistant Cr-Mn-N steel provided by the present invention has properties of high temperature strength, high thermal conductivity, excellent high temperature fatigue performance, lower thermal expansion coefficient, higher metallographic structural stability, good dimensional stability, higher ductility, heat resistance, impact resistance, low production cost, etc. to thereby meet the requirements of high performance engines. Thus, the steel of the present invention can be widely used as the material of the automobile turbine casing and the exhaust manifold.There is further described a method for producing the austenitic heat-resistant Cr-Mn-N steel according to the above technical overview, comprising the steps of: (a) forming a melt by melting raw alloy materials of the elements; and (b) after a rest period, casting the melt formed in the step (a) to produce the Cr-Mn-N austenitic heat-resistant steel.Preferably, a melting temperature in step (a) is 1580-1700°C.Preferably, a rest period in step (b) is 3 to 20 minutes.Preferably, after the melt in step (b) is allowed to stand as defined in the appended claims, a slag removing process is further carried out.Preferably, a casting temperature of the Cr-Mn-N austenitic heat-resistant steel is 1550 to 1650° C.The provided method for manufacturing the austenitic heat-resistant Cr-Mn-N steel is simple. The austenitic heat-resistant Cr-Mn-N steel produced by this method has properties such as high temperature strength, high thermal conductivity, excellent fatigue performance at high temperatures, lower thermal expansion coefficient, higher stability of the metallographic structure, good dimensional stability, higher ductility, heat resistance, impact resistance, low production cost, etc., to meet the requirements of high-performance engines.DETAILED DESCRIPTIONThe present invention provides an austenitic, heat-resistant Cr-Mn-N steel comprising, in weight percent: 0.20% to 0.50% carbon, 0.50% to 2.00% silicon, 2.00% to 5.00% manganese, less than 0.04% phosphorus, less than 0.03% sulfur, 20.00% to 27.00% chromium, 6.00% to 8.00% nickel, less than 0.50% molybdenum, less than 0.60% niobium, less than 0.60% tungsten, less than 0.15% vanadium, 0.30 to 0.60% nitrogen, less than 0.08% zirconium, less than 0.10% cobalt, less than 0.10% yttrium, less than 0.20% boron, otherwise iron.In the present invention, the austenitic Cr-Mn-N heat resistant steel preferably comprises, in weight percent: 0.30% to 0.45% carbon, 0.80% to 1.50% silicon, 3.00% to 4.80% manganese, less than 0.02% phosphorus, less than 0.02% sulfur, 23.00% to 26.00% chromium, 6.50% to 7.00% nickel, less than 0.20% molybdenum, less than 0.30% niobium, less than 0.40% tungsten, less than 0.12% vanadium, 0.40 to 0.50% nitrogen, less than 0.08% zirconium, less than 0.08% cobalt, less than 0.08% yttrium, less than 0.10% boron, otherwise iron.In the present invention, both the manganese and nitrogen elements can facilitate austenite formation, and the nitrogen element has a 30 times greater ability to facilitate austenite formation than the nickel element. The cost of the manganese and nitrogen elements is only 20% to 30% of the cost of the nickel element. Thus, the austenitic heat-resistant steel can be produced at a lower production cost. Moreover, the nitrogen element can also stabilize the microstructure at elevated temperatures, improve strength at elevated temperatures, improve pitting resistance, and resist stress corrosion cracking. The manganese element can act as a good desulfurization agent and a good deoxidizing agent, thus maintaining the content of sulfur and oxygen in the liquid steel at a lower level, improving the instantaneous strength at elevated temperatures, and improving the creep rupture strength and the creep performance of the material. The austenitic heat-resistant Cr-Mn-N steel provided by the present invention has properties of high temperature strength, high thermal conductivity, excellent high temperature fatigue performance, lower thermal expansion coefficient, higher metallographic structural stability, good dimensional stability, higher ductility, heat resistance, impact resistance, low production cost, etc. to thereby meet the requirements of high performance engines. Thus, the steel of the present invention can be widely used as the material of the automobile turbine casing and the exhaust manifold.A method of manufacturing the austenitic heat-resistant Cr-Mn-N steel will be further described. The method comprises the steps of: (a) forming a melt by melting raw alloy materials of the elements; and (b) after a rest period, casting the melt formed in step (a) to produce the Cr-Mn-N austenitic heat-resistant steel;In the present invention, the source of raw alloy materials of the elements is not particularly limited, and all the goods on the market of the raw alloy materials are known and available to those skilled in the art. In the embodiments of the present invention, raw alloy materials of the elements are preferably silicon iron, manganese, ultra low carbon ferrochrome, ferroniobium, ferrotungsten, ferrovanadium, nickel plate, nitrided ferrochrome alloy, zirconium metal, yttrium metal, cobalt metal and ferroboron.In the present invention, the temperature for melting in step (a) is 1580-1700°C, more preferably 1600-1680°C, and most preferably 1630-1650°C.In the present invention, the time for melting in step (a) is preferably 0.5 to 3.0 hours, more preferably 0.6 to 2.0 hours, and most preferably 0.8 to 1.5 hours.In the present invention, the heating modes for melting the raw alloy materials are not particularly limited, and any heating mode known to those skilled in the art is available. The apparatuses for melting the raw alloy materials are not particularly limited, and any melting apparatus known to those skilled in the art may be available. In the embodiments of the present invention, the melting process is preferably carried out in a medium frequency induction furnace.After obtaining the melt, the melt is allowed to stand for several minutes and then cast for molding to obtain the austenitic heat-resistant Cr-Mn-N steel. A standing time is 3 to 20 minutes, more preferably 5 to 15 minutes, and most preferably 8 to 12 minutes.After standing, a slag removing process for the melt is preferably performed to remove the slag on the surface of the melt. The slag removing method is not particularly limited, any method for removing the slag known to those skilled in the art may be available. In the present invention, a mechanical slag removing method is preferred.According to the present invention, the melt after standing is cast for molding. A temperature for the austenitic heat-resistant Cr-Mn-N steel to be cast is 1550 to 1650° C., more preferably 1560 to 1630° C., and most preferably 1580-1620° C.In the present invention, the apparatus for the melt which is cast after being allowed to stand for molding is not particularly limited, any apparatus known to those skilled in the art is available. In the embodiments of the present invention, the method of casting the melt cast for forming is preferably performed in a ladle.In the present invention, after the casting of the melt for molding, methods of sandblasting, grinding, trimming and testing are preferably performed. Methods of sandblasting, grinding, trimming and testing are not particularly limited, and any method known to those skilled in the art is available.The provided method for manufacturing the austenitic heat-resistant Cr-Mn-N steel is simple. The austenitic heat-resistant Cr-Mn-N steel produced by this method has characteristics of high temperature strength, high thermal conductivity, excellent high temperature fatigue performance, oxidation resistance at high temperatures, lower thermal expansion coefficient, higher stability of the metallographic structure, good dimensional stability, higher ductility, heat resistance, impact resistance, low production cost, etc. to meet the requirements of high performance engines.The austenitic heat-resistant Cr-Mn-N steel of this invention will be described in detail below in combination with Examples, but these Examples should not be construed to limit the scope of the invention.Example 1I. Ingredients: Major raw materials in weight percent: fuel 0.32%, scrap steel 43.39%, chromium nitride 8.58%, ferrochrome with extremely low carbon content 34.31%, electrolytic manganese 5.15%, ferrosilicon 1.25%, and nickel plate 7.0%. Melting: A medium frequency induction furnace was used for melting. The capacity of the induction furnace can be between 0.5 tons and 3 tons. The weighed raw materials were successively fed into the medium frequency induction furnace, which was then energized and heated. After the materials were completely melted, the temperature was raised to 1580°C in the medium frequency induction furnace. Spectroscopic analysis was performed for the melt within the medium frequency induction furnace using a test strip for spectroscopic analysis. The result of the analysis is shown in the following table.% by weight0,431,204,720,0100,00825,646,720,0130,0076ElementW. WV. VN. NZrY is YB. BCo. CoFeFe% by weight0,01410,10840,49670,0520,0610,0020,0760,4472Tapping and melt processing: After the chemical composition of the melt fulfilled the requirements, liquid steel inside the furnace was heated to 1630° C. and then tapped. Before tapping, the furnace was shut down for a rest time of 8 minutes and then the slag on the surface of the liquid steel was removed. A sufficiently preheated ladle was positioned at a liquid steel outlet of the induction furnace and waited for tapping of the liquid steel. After the completion of the tapping, the slag on the surface of the liquid steel was removed and casting was expected.Casting and peeling of the box: When a casting temperature reached 1550° C., a casting process was performed. 40 minutes after completion of casting, a box detachment process was performed.V. Post-processing: After peeling off the box, sandblasting, grinding, trimming, inspecting, etc. were carried out to obtain an austenitic heat-resistant Cr-Mn-N steel.The austenitic heat-resistant Cr-Mn-N steel produced in Example 1 was tested, and the results were as follows: the tensile strength at 1050° C. was 78 MPa or higher, the yield strength was 75 MPa or higher, the thermal conductivity was 28.1 W / (m 2 ·K) or higher, the elastic modulus was 105 GPa or more, and the thermal expansion coefficient at 1100° C. was 20.0 (1 / K·10 -6); The austenitic heat-resistant Cr-Mn-N steel had properties such as excellent high-temperature strength, high thermal conductivity, and rapid thermal diffusion rate; and Ni was replaced with Mn and N, thereby greatly lowering the production cost.Example 2I. Ingredients: Major raw materials in weight percent: fuel 0.35%, scrap steel 43.29%, chromium nitride 8.65%, ultra low carbon ferrochrome 33.71%, electrolytic manganese 5.35%, ferrosilicon 1.55% and nickel plate 7.1%. Melting: A medium frequency induction furnace was used for melting. The capacity of the induction furnace can be between 0.5 tons and 3 tons. The weighed raw materials were successively fed into the medium frequency induction furnace, which was then energized and heated. After the materials were completely melted, the temperature inside the medium frequency induction furnace was raised to about 1600°C. Spectroscopic analysis was performed for the melt within the medium frequency induction furnace using a test strip for spectroscopic analysis. The result of the analysis is shown in the following table.% by weight0,501,234,760,0200,01025,406,790,0340,0015ElementW. WV. VN. NZrY is YB. BCo. CoFeFe% by weight0,00790,09660,43950,0430,0550,00180,0960,5207Tapping and melt processing: After the chemical composition of the melt fulfilled the requirements, liquid steel inside the furnace was heated to 1680°C and then tapped. Before tapping, the furnace was shut down for a rest time of 3 minutes and then the slag on the surface of the liquid steel was removed. A sufficiently preheated ladle was positioned at a liquid steel outlet of the induction furnace and waited for tapping of the liquid steel. After the completion of the tapping, the slag on the surface of the liquid steel was removed and casting was expected.Casting and peeling of the box: When a casting temperature reached 1650° C., a casting process was performed. 60 minutes after completion of casting, a box detachment process was performed.V. Post-processing: After peeling off the box, sandblasting, grinding, trimming, inspecting, etc. were performed to obtain an austenitic heat-resistant Cr-Mn-N steel.Comparative ExampleThe same raw materials were used and weighed according to their respective amounts. Comparison was made between an austenitic Cr-Ni heat-resistant steel designated as GX40CrNiSiMn25-20 in accordance with European Standard EN 10295 and the austenitic Cr-Mn-N heat-resistant steel produced in Example 2. An analysis result of the composition of the former is shown in the following table. An analysis result of the composition of the austenitic Cr-Ni heat-resistant steel designated as GX40CrNiSiMn25-20% by weight0,401,241,060,0200,01024,8519,540,031,42ElementW. WV. VN. NZrY is YB. BCo. CoFeFe% by weight-0,089---- --51,341From a comparison between the compositions of the above two materials, it is seen that the main differences are the amounts of Mn, Ni, Nb and N elements. A cost comparison between the above two 1000 kg liquid steel-based materials was shown in the following table (Number 1 stands for the austenitic Cr-Mn-N heat-resistant steel produced in Example 2, and Number 2 stands for the designated GX40CrNiSiMn25-20) heat-resistant steel.Price (RMB / kg)11,112,5570,3175,517,41,8Yield % %100%60%100%60%8,5%100%No. 1Added amount (kg)5036770-56457Cost of Raw Materials Added55546064921-97482311879No.2Add quantity1341720024-346Cost of Raw Materials Added1445233140604212-62324272PS: The alloy cost for Zr, Y, Co and B added for the material No. 1 was 580 RMB in total.From a cost standpoint [0032, the cost for the austenitic Cr-Mn-N heat-resistant steel is only 51% of the cost for the heat-resistant steel designated GX40CrNiSiMn25-20.As compared with the comparative example, the austenitic heat-resistant Cr-Mn-N steel of the present invention exhibited an increase in yield strength at room temperature by 219 MPa, an increase in tensile strength by 379 MPa, an increase in elastic modulus by 7.8% at room temperature, an increase in thermal conductivity at room temperature by 30.4%, and an increase in thermal conductivity at 1100°C by 14.4%. Specific test results are shown in Table 1. From the above property comparison, it is apparent that the property of the austenitic heat-resistant Cr-Mn-N steel of the present invention was superior to the comparative example and the production cost was greatly reduced.The above descriptions are only preferred embodiments of the present invention.References included in the specificationThis list of documents cited by the applicant has been produced in an automated manner and is only included for the better information of the reader. The list is not part of the German patent application or utility model application. The DPMA does not take any adhesion for any faults or omissions.Patent Literature citedCN 103898398 A

[0003] CN 103898397 A

[0003]

Claims

A Cr-Mn-N austenitic heat resistant steel comprising, in weight percent: 0.30% to 0.45% carbon, 0.80% to 1.50% silicon, 3.00% to 4.80% manganese, less than 0.02% phosphorus, less than 0.02% sulfur, 23.00% to 26.00% chromium, 6.00% to 8.00% nickel, less than 0.20% molybdenum, less than 0.30% niobium, less than 0.40% tungsten, less than 0.12% vanadium, 0.30 to 0.60% nitrogen, less than 0.08% zirconium, less than 0.08% cobalt, less than 0.08% yttrium, less than 0.10% boron, otherwise iron.The Cr-Mn-N austenitic heat resistant steel of claim 1, comprising, in weight percent: 0.30% to 0.45% carbon, 0.80% to 1.50% silicon, 3.00% to 4.80% manganese, less than 0.02% phosphorus, less than 0.02% sulfur, 23.00% to 26.00% chromium, 6.50% to 7.00% nickel, less than 0.20% molybdenum, less than 0.30% niobium, less than 0.40% tungsten, less than 0.12% vanadium, 0.40 to 0.50% nitrogen, less than 0.08% zirconium, less than 0.08% cobalt, less than 0.08% yttrium, less than 0.10% boron, otherwise iron.The Cr-Mn-N austenitic heat-resistant steel according to claim 1 or 2, having a working temperature of 1050°C or higher.

Citation Information

Patent Citations

  • High-silicon molybdenum-alumium ferrite heat-resisting spheroidal graphite cast iron for car turbine housings and car exhaust pipes

    CN103898397A

  • High-silicon molybdenum-chromium ferrite heat-resisting spheroidal graphite cast iron for car turbine housings and car exhaust pipes

    CN103898398A

  • CN000103898397A

  • CN000103898398A