ORDER FOR DETERMINING THE ACHIEVABLE ADHESIVE STRENGTH BEFORE THE FORMATION OF A MATERIAL-CONNECTED BOND ON A SURFACE OF A JOINTING PARTNER

DE502016016741D1Active Publication Date: 2024-10-17FRAUNHOFER GESELLSCHAFT ZUR FORDERUNG DER ANGEWANDTEN FORSCHUNG EV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502016016741
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2015-09-07
Filing Date
2016-08-31
Publication Date
2024-10-17
Estimated Expiration
2036-08-31

AI Technical Summary

Technical Problem

Current methods for determining adhesive strength, such as wedge tests and tape tests, are destructive, time-consuming, and cannot be performed during production, making it impossible to predict adhesive strength before forming a cohesive connection or coating, and they require sample destruction.

Method used

A non-destructive method using spatially resolved spectral analysis of electromagnetic radiation with detectors arranged in a row or column configuration, connected to an electronic evaluation unit, which records and evaluates wavelength-resolved intensities to create a three-dimensional data structure, allowing for data reduction and feature extraction using regression models to predict adhesive strength.

Benefits of technology

Enables rapid, non-destructive, and accurate prediction of adhesive strength, allowing for inline measurement in manufacturing processes, reducing testing time from days to milliseconds and eliminating the need for sample destruction.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to an arrangement for determining the achievable adhesive strength before forming a material-to-material bond on the surface of a joining partner. Joining partners can be joined together by adhesive bonding, welding, or soldering. Joining partners can also be joined that are both made of the same material, in particular plastics, metals, or ceramics, or where at least one joining partner is made of a polymer. In this way, joining partners made of different materials can also be examined before the material-to-material bond is established. However, the invention can also be used to determine the achievable adhesive strength of a coating applied to the surface of a component, which will also be referred to below as the joining partner, before the coating is formed.

[0002] Adhesive strength can be understood as the achievable adhesion effect.

[0003] Until now, it has been common practice to test such bond strengths using the wedge test according to DIN 65448, but also using the peel test according to ISO 4624, the angle peel test according to DIN 53282, the tensile strength test according to DIN 53288, the roller peel test according to DIN 53289, and other test methods. However, these tests only allow specimens to be tested after the bond has formed and solidified, which, like the actual testing, can take several days. This makes testing directly during production impossible. Furthermore, these methods require the specimens to be destroyed.

[0004] The adhesion strength of coatings is usually determined using a tape test. This can only be performed after the coating has formed. Therefore, a prediction is impossible. Furthermore, the coating is destroyed and the substrate is at least compromised.

[0005] For example, EP 2 138 830 A2 discloses a method for determining the influence of UV radiation on materials using IR spectroscopy.

[0006] It is therefore an object of the invention to provide possibilities for the non-destructive determination of the achievable adhesive strength before the formation of a material bond on a surface of a joining partner, which lead to results with sufficient accuracy in a significantly shorter time and can thus even be used for inline measurement in manufacturing processes.

[0007] According to the invention, this object is achieved by an arrangement having the features of claim 1. Advantageous embodiments and further developments of the invention can be realized with features specified in subordinate claims.

[0008] The inventive arrangement for determining the achievable adhesive strength before the formation of a material-to-metal bond on the surface of a joining partner comprises a plurality of detectors designed for the spatially resolved spectral analysis of electromagnetic radiation within a wavelength interval. These detectors are arranged in a row or a row and column arrangement. The detectors are connected to an electronic evaluation unit and arranged such that electromagnetic radiation emitted by a broadband radiation source impinges on the detectors either after being reflected off the surface of one of the joining partners, off a layer formed on the surface of a joining partner with which the material-to-metal bond is formed, and / or after passing through joining partners transparent to the electromagnetic radiation.The irradiation is carried out in such a way that a homogeneous intensity of electromagnetic radiation is maintained on a surface from which the electromagnetic radiation is reflected or transmitted. The surface to be detected simultaneously should therefore be irradiated with a homogeneous intensity. In broadband irradiation, electromagnetic waves within a wavelength interval are directed onto the respective surface of one of the joining partners to be examined.

[0009] The joining partner or a coating formed on the surface, onto whose surface the electromagnetic radiation is directed, is made of a material that does not absorb the respective electromagnetic radiation 100% and thus a transmission and / or reflection of at least 2% of the electromagnetic radiation is / are possible.

[0010] The electronic evaluation unit is designed in such a way that the measurement signals recorded by the detectors with spatial and wavelength resolution can be assigned to a specific wavelength range within a wavelength interval and to an individual location point within a predeterminable sub-area of ​​the irradiated surface.

[0011] The measurement and evaluation can be performed on the entire surface of the joining partner used for the material-to-material joining process, or on all joining partners. However, it is also possible to perform the measurement on one or more partial surfaces.

[0012] The totality of the wavelength-resolved intensities recorded at all locations of the respective irradiated area forms a three-dimensional data structure consisting of one wavelength-resolved and two spatially resolved dimensions (hypercube).

[0013] According to this, it should be possible to carry out data reduction for all wavelength-resolved measurement signals of the sub-area, in which meaningful features are selected and the resulting feature set is subjected to a regression procedure using a regression model stored in an electronic memory, which was determined on the basis of feature sets that were previously determined on samples whose adhesive strengths were determined using a different measuring method that preferably has a higher measuring accuracy, whereby a statement about the adhesive strength of the relevant sub-area of ​​the joint can be derived, wherein at least one sub-area is used to evaluate the adhesive strength.

[0014] A material connection of joining partners examined with the invention should belong to the same class, which should have a comparable structure or composition, as those previously examined with another measuring method.

[0015] The functional relationship between adequately selected sets of features of materially bonded joining partners and their bond strengths, which were determined using another measuring method, can be determined, for example, using linear or non-linear regression, a partial least square algorithm (PLS), a neural network, a combination of at least two of these methods or other regression methods (regression model).

[0016] The electronic memory should therefore contain the regression model created using the data sets acquired with the inventive system from samples that were subjected to data reduction and feature extraction, and whose adhesive strengths – determined using a different measurement method – were determined. Using a regression model stored in the electronic memory, the adhesive strength of a comparable sample of the same sample class with a similar structure can be determined from the data sets acquired with the inventive system.

[0017] The electronic evaluation unit performs data reduction and feature extraction from the data sets acquired with the inventive arrangement. This can involve evaluating the spectral information first, followed by the spatial information. A reverse sequence or any combination of more than two individual steps for data reduction and feature extraction is also possible.

[0018] Data reduction and feature extraction can be performed using principal component analysis (PCA), parameterization of texture information, averaging and / or standard deviation determination, and combinations thereof.

[0019] When using principal component analysis, the n intensities of the wavelengths (spectra) of all location points are transformed by a coordinate transformation into a new orthogonal coordinate system - the principal component space - in which the original data have maximum variance, and where n represents the number of measured wavelengths.

[0020] The coordinate transformation is calculated by determining the nEigenvectors (principal components) and the corresponding n eigenvalues ​​of the covariance matrix of the data set of the measured partial area. The larger the nth eigenvalue, the more the corresponding nth principal component describes the original variance, i.e. the eigenvector with the largest eigenvalue is the 1st principal component of the data set and describes the majority of the original variance of the data set. The eigenvector with the lowest eigenvalue is the nth principal component of the data set and does not describe any relevant properties of the data set. Only a certain number of principal components are taken into account - often the first three to six, which already ensure a sufficient description - for example > 95% - of the original variance of the data set.The number of principal components to be considered - and thus the dimensionality of the principal component space - can be selected based on criteria, for example, the proportion of the total variance or a scree test.

[0021] The coordinates of the spectra in the newly spanned principal component space are the so-called score values, which sufficiently characterize the corresponding location point.

[0022] With the electronic evaluation unit, data reduction and feature extraction can advantageously be carried out in such a way that the data acquired according to the invention are evaluated in the same way as the data from the samples, based on whose known adhesive strengths the regression model was created. Based on the data set acquired according to the invention, the spatially and wavelength-resolved intensities of the electromagnetic radiation, the adhesive strength of the sample is then determined using the regression model.

[0023] The evaluation of the data recorded according to the invention can preferably be carried out as follows: Variant a) Using a principal component analysis of the spectral information of all locations of the partial area, the first six principal components including the score values ​​are preferably determined. Since the data recorded according to the invention represent all locations of an examined area, the areal distribution of the score values ​​can be specified for each principal component. The different areal distributions of the score values ​​are quantified using various statistical parameters which are determined on the basis of all score values ​​of a principal component of the respective partial area. In particular, these are the variance, the interquantile distance or the mean absolute deviation. This procedure can be applied for all principal components. The adhesive strength is determined by the electronic evaluation unit on the basis of a regression model, such as e.g.B. a partial least square regression model (PLS), where the parameters may have been subjected to further prior feature extraction, preferably via another principal component analysis (PCA).

[0024] The regression model used (here PLS) was previously determined using samples of the same sample class with a comparable structure, whose bond strengths were determined using a different measuring method, whereby all steps of feature extraction were carried out analogously to the method described above.

[0025] Variant b) Using a principal component analysis of the spectral information of all recorded location points of the respective examined sub-area, one or more principal components are calculated, in particular the score values ​​of the location points per principal component, which can be specified as a distribution over the sample area. The location points can be described by various parameters of the score values ​​and represented graphically. In addition to the actual score value, this can also be achieved in particular using the parameters resulting from a texture analysis of the spatially resolved distribution of the score values. A discrete wavelet transform (DWT) is preferably used for this purpose, whereby, for example, the 'Sym2' wavelet is used to perform the calculations, followed by a calculation of further parameters, e.g. the energy signature (sum of squares) of the wavelet parameters.For further feature extraction and thus for determining the "bonding strength" feature of the partial surface, the calculated parameters determined on the examined surface of the joining partner can be determined using a regression model, in particular a linear regression model. The regression model used was previously determined using samples of the same sample class with comparable structure and properties, whose bond strengths were determined using a different measurement method. All steps of feature extraction were carried out analogously to the method described above.

[0026] Using discrete wavelet transformation, the texture of at least one image captured by the detectors, particularly recurring structures (frequencies), can be described. Wavelet transformation (WT) corresponds to digital filtering based on high-pass and low-pass frequencies, whereby the filter function (wavelet) can be variably selected and the frequency response is direction-dependent. Thus, performing WT on images or pictorial representations in vertical, horizontal, and diagonal directions produces different results. Calculations for all three directions can be performed separately. The result is determined by the low-pass information (wavelet coefficients), and the remaining information is discarded. Each pixel represents a wavelet coefficient, and all pixels together form the wavelet matrix. In addition, performing WT reduces the spatial resolution and separates information.The separation of the information means that for a number of originally m pixels after the WT there are still . m*0,5 Image points are obtained. The WT can be performed recursively multiple times. This can be done in three stages to obtain information about the fine, medium-fine, and coarse structure of the images. However, more or fewer than three stages are also possible. From the wavelet coefficients of each WT, additional parameters can be determined to describe structures of the wavelet matrix or their visual representation. Often, the root of the square sum of the coefficients of the wavelet matrix (energy), the entropy, the gray value matrix, and parameters derived from them are used.

[0027] The sample area to be examined should have a size in the range of 500 µm × 500 µm to 1500 µm × 1500 µm. Detection should be possible with a spatial resolution in the range of 0.5 µm to 1.5 µm, preferably 1 µm.

[0028] At least 30, preferably at least 100 detectors should be arranged in a row (hyperspectral camera).

[0029] At least one, preferably at least 50 detectors should be arranged in a column.

[0030] For an arrangement according to the invention, a hyperspectral camera with suitable radiation-shaping optical elements and electronic evaluation electronics can be used.

[0031] The surface should be irradiated at an angle of at least 0° to < 90° relative to the normal to the surface onto which the electromagnetic radiation impinges. When irradiating at least one joining partner that is transparent to the electromagnetic radiation, the angle to the sample normal should preferably be maintained at a minimum of 0°, i.e., the radiation should be directed as perpendicularly as possible to this surface in order to keep the reflected portion as small as possible. Irradiation and detection can also be carried out with variable angles of incidence of the electromagnetic radiation. As already stated, angles of incidence in the range of 0° to a maximum of 89° can be selected.

[0032] Detection can also be limited to linearly polarized electromagnetic radiation. In this case, an advantageous orientation of one or more polarization planes can be selected before and / or after the irradiated surface.

[0033] Particularly when using detectors that can only measure one line simultaneously spectrally and spatially resolved, the detectors and the respective joining partners that are not yet materially bonded to one another can be moved relative to one another along at least one axis and preferably at an advantageous distance from one another. With statically fixed detectors and radiation source, a sample formed with a joining partner that is not yet materially bonded can be moved along an axis. This can be achieved with a correspondingly movable table on which such a sample is arranged and can be moved in an x- and, if necessary, also in a y-direction. However, unwinding from roll to roll is also possible if the respective sample is formed from one or more flexibly deformable material(s) and is in the form of a film, for example.

[0034] The radiation source can contain elements that shape the electromagnetic radiation. In a simple design, the radiation source can be combined with a microscope. However, the radiation source can also be arranged in a hollow body, from which the electromagnetic radiation emerges diffusely and can be directed onto the surface to be irradiated. The hollow body can be a sphere or cylinder. It should be possible to irradiate a surface to be detected simultaneously and homogeneously. For a radiation source with beam-shaping optical elements, the wavelength range used should be considered when selecting the optical elements used for beam shaping.

[0035] The size of the area to be examined and the required spatial resolution can be influenced by using elements arranged upstream of the detectors that shape the electromagnetic radiation. In a simple design, the camera or detector array can be combined with a microscope or a telecentric lens.

[0036] Preferably, a diaphragm preventing the incidence of scattered electromagnetic radiation can be arranged in front of the detectors in the beam path of the electromagnetic radiation.

[0037] The radiation source can emit electromagnetic radiation whose wavelength range begins in the UV range and ends in the IR range. Radiation from the wavelength range of visible light up to the NIR range, i.e. from 250 nm to 1000 nm, is particularly preferred. Within a used wavelength range, it should be possible to use as many wavelengths within the respective interval for irradiation as possible. The limits should be determined solely by the sensitivity range of the detectors used in terms of their sensitivity / measurement accuracy of the intensities they can detect for the respective wavelengths and the optical properties of the beam guidance components. Preference should be given to using spectral ranges that exhibit the greatest variance between the spectra of the samples for determining the adhesion strength and that have the smallest possible determination error.

[0038] At least one element with which a targeted selection of the polarization of the electromagnetic radiation can be achieved can also be present or integrated in the beam path.

[0039] A sample of materially bonded joining partners can also be a multi-layer structure, preferably consisting of several layers made of different materials. The base material of the sample can be a polymer film or a thin metal or glass film to which further thin polymer, ceramic or metal layers can be applied in various combinations. The achievable adhesive strength can also be determined for more than two joining partners to be materially bonded. These can be arranged one above the other, for example in the form of a stack. As already mentioned, joining partners can be materially bonded by adhesive bonding. In this case, a suitable adhesion promoter is present between the materially bonded surfaces of the joining partners. The materially bonded connection can also be formed by welding, with or without filler material.The achievable bond strength can also be determined for a soldered joint. However, the expected bond strength of coatings, such as paint layers, plastic coatings on metal or ceramic surfaces, and coatings formed using CVD or PVD processes, can also be determined.

[0040] The detectors used, the electronic evaluation unit, and possibly also the radiation source, can constitute a so-called hyperspectral imaging system, which can be used in the arrangement according to the invention. This allows not only spectral but also texture information to be obtained for the respective detected portion of the sample.

[0041] It can be advantageous to reduce the data collected during the detection of the intensities determined at the individual locations for the individual wavelengths of a recorded wavelength range (spectrum) during the actual evaluation. This allows information relevant to determining the bond strength to be separated from information irrelevant, significantly reducing the electronic computational effort and thus the required time. The use of highly complex, cost-intensive electronic computing technology is unnecessary.

[0042] The invention allows the creation of a statistical model on the basis of which the achievable bond strength of the examined surfaces of one and / or both joining partners can be predicted in the corresponding underlying sub-area. For this purpose, the data set can be acquired using one of several optical detectors, preferably arranged in series, which enable wavelength- and spatially resolved intensities.

[0043] The achievable bond strength is influenced by the properties of the sample surfaces being examined. These properties can include particles, adsorbates, layer thicknesses, materials, surface roughness, topology, etc., as well as their distribution across the respective partial area under investigation. These sample-specific properties also cause electromagnetic radiation interacting with the sample to be reflected, scattered, or transmitted differently (spectral, intensity). The totality of a sufficient number of individual wavelength-resolved intensities (spectra) from different locations of a detected partial area of ​​a sample can thus represent information about the expected bond strength of a joining partner in the sample area under consideration.

[0044] To determine the bond strengths, the bond strength can be determined based on a measured set of characteristics using a regression model previously established with sets of characteristics with known bond strengths measured on samples of the same sample class with a comparable structure.

[0045] The measured feature sets must be subjected to data reduction and thus feature extraction. The wavelength spectra detected at the individual locations of the respective subarea can be subjected to spectral feature extraction, for example, cluster analysis or principal component analysis. The parameters used in the regression model can therefore be the number and distribution of clusters, the score values ​​of the principal components, or their distribution.

[0046] Furthermore, image compression methods for texture evaluation can be used for feature extraction. These methods involve subjecting the intensities of individual wavelengths detected at all locations of the respective subarea, or the sum or average sum of the intensities of multiple wavelengths, or the parameters determined by spectral feature reduction and / or combinations thereof to image compression. To describe the texture information of the dataset, at least one parameter should be determined using a wavelet transform or another image compression method, such as Taylor polynomials, Fourier and cosine transforms, discrete cosine transform, or the grayscale matrix method.

[0047] Based on a calibration model (regression model) created using measured data sets from samples of the same sample class with comparable structure and known adhesion strength, the adhesion strength of partial surfaces can be predicted. The measured data sets are treated for calibration and prediction using identical feature reduction steps. Examples of regression models used include multiple linear regression analysis (MLRA), principal component regression (PCR), partial least squares regression (PLS), or a neural network.

[0048] Prerequisites for sufficient determination accuracy are homogeneous illumination of the area used for detection, so that the superposition of intensity fluctuations caused by the sample with lateral fluctuations in the illumination intensity can be avoided by implementing a laterally homogeneous light field. For small sample areas, microscope optics can be advantageously used. The arrangement according to the invention can be adapted to the specific area of ​​the sample to be detected by using different optics, working distances, and magnifications.

[0049] With the invention, the achievable bond strengths of samples can be determined within a few milliseconds to minutes instead of days. A non-contact, non-destructive measurement is possible. The samples do not require any additional treatment or other preparation. It is preferably used in quality control and inline production monitoring, so that in these cases, sampling and separate determination are not necessary.

[0050] The invention will be explained in more detail below by way of example.

[0051] It shows: Figure 1 shows a wavelet transformation using the "Sym2" wavelet, and Figure 2 shows a regression model created to predict crack length in the wedge test according to DIN 65448; with which the achievable bond strength can be calculated from the crack length. Example 1

[0052] Sample sheets made of a titanium alloy, coated with around 100 nm of silicon dioxide using a plasma process, are divided into five sub-areas on a selected area of ​​2 mm x 10 mm and homogeneously irradiated using a halogen lamp as the light source. A total of 1000 × 150 optical detectors were arranged above the sample in a row-column arrangement and combined with optics (in this case a microscope) so that the entire sample area, with a width of 2 mm, could be recorded with wavelength and spatial resolution. The optical detectors were used to record the intensities of the light reflected from the sample for individual locations with wavelength resolution. A total of 150 wavelengths in the range 400 nm to 1000 nm were considered. The sample was moved perpendicular to the row arrangement of detectors in order to record the entire sample area.

[0053] The intensities recorded with the detectors for the individual location points with wavelength resolution were assigned to sub-areas of the sample, each with a size of 2 mm * 2 mm, and form a hypercube.

[0054] Subsequently, data reduction was carried out for each sub-area, using a step-by-step approach as described below: 1. Mean smoothing (moving average) of the spectra. 2. Principal component analysis of the hypercube of the sub-area. This reduces the dimensionality of the measured data set without losing important information. For this purpose, two principal components were selected to obtain two score images. Subsequently, a discrete wavelet transformation was performed for each sub-area, proceeding in the steps described below: 3. For each score image, the wavelet transformation was performed in three directions (horizontal, vertical, diagonal) and in three stages each (fine, medium, coarse structure) using the "Sym2" wavelet for all transformations = 9 transformations per score image. 4. Calculation of wavelet transformation parameters: a. Energy (sum of squares of the coefficients of the wavelet matrix) Energie = ∑ i , j p i j 2 with p(i,j), coefficient of the wavelet matrix at position (i,j). b. (Shannon) entropy Entrophy = − ∑ h ∗ log 2 h where h, values ​​of the histogram classes c. gray value matrix i. energy (measure of uniformity) ∑ i , j p i j 2 ii. Contrast (measure of variance) ∑ i , j i − j 2 p i j iii. Correlation (dependence of pixels) ∑ i , j i − μi j − μj p i j σ i σ j iv. Homogeneity (measure of monotonicity) ∑ i , j p i j 1 + i − j with p(i,j), coefficient of the wavelet matrix at position (i,j); µ expected value; and σ standard deviation.

[0055] Subsequently, the achievable adhesion strength of the sample under investigation was determined using the regression model previously created using data sets of partial areas with known adhesion strength and data treatment analogous to that described in steps 1-4 and stored in the electronic memory of the electronic evaluation unit.

Claims

1. An arrangement for determining the achievable adhesive strength before forming an integrally bonded connection at a surface of a joining partner, which arrangement comprises a broadband radiation source, a plurality of detectors and an evaluation unit, wherein the plurality of detectors are configured for a spatially resolved spectral analysis of electromagnetic radiation within a wavelength interval, are arranged in a row or a row and column arrangement, and are connected to the electronic evaluation unit and are arranged such that electromagnetic radiation emitted by the broadband radiation source impacts the detectors either after a reflection at the surface of one of the joining partners, a layer which is formed on the surface of a joining partner and with which the integrally bonded connection is formed, and / or after the irradiation of the joining partners transparent for the electromagnetic radiation, wherein the broadband radiation source is formed such that, on a surface of the joining partner from which the electromagnetic radiation is reflected or transmitted through the surface, an intensity of the electromagnetic radiation that is homogeneous laterally and in time is maintained, and the radiation is not absorbed 100%, and so an at least 2% transmission and / or reflection of the electromagnetic radiation is / are achieved and the electronic evaluation unit is formed such that the measurement signals detected by the detectors with spatial and wavelength resolution are detected within a wavelength interval for individual local points arranged on a predefinable surface of the joining partners, and measurement signals detected at several positions are in each case associated with a partial region of the detected surface (hypercube) and a data reduction is carried out for all measurement signals of the partial regions of the detected surface detected with wavelength resolution and in this process significant features are selected and on the basis of these selected features with previously determined regression model, which is stored in an electronic memory and which has been determined on the basis of the feature sets obtained in an analogous manner of joining partners connected to one another in an integrally bonded manner, the adhesive strengths of which were determined previously on samples using a different measurement method, the evaluation unit makes a prediction about a corresponding achievable adhesive strength.

2. The arrangement according to claim 1, characterized in that the electronic evaluation unit is formed such that a data reduction is achievable by feature extraction by principal component analysis, extraction of texture information, mean value formation, determination of the standard deviation and / or combinations thereof.

3. The arrangement according to any one of the preceding claims, characterized in that the respective partial region has a size in the range of 500 µm * 500 µm to 1500 µm * 1500 µm or 2 mm * 2 mm.

4. The arrangement according to any one of the preceding claims, characterized in that the surface is irradiated with at least an angle in the range of 0 ° to < 90° in relation to the normal of the surface of the irradiated joining partner.

5. The arrangement according to any one of the preceding claims, characterized in that the detection and evaluation may be carried out using at least one polarizer with at least one defined known polarization plane in relation to the plane of incidence.

6. The arrangement according to any one of the preceding claims, characterized in that the detectors and the joining partners connected in an integrally bonded manner are movable along at least one axis relative to one another and at the same time preferably at a constant distance from one another.

7. The arrangement according to any one of the preceding claims, characterized in that the radiation source has optical elements that shape the electromagnetic radiation or a radiation source that emits electromagnetic radiation diffusely onto the surface, which radiation source is arranged in particular within a hollow body and, particularly preferably in the beam path of the electromagnetic radiation, a diaphragm that avoids the incidence of scattered electromagnetic radiation is arranged in front of the detectors.

8. The arrangement according to any one of the preceding claims, characterized in that the joining partners to be connected in an integrally bonded manner form a multi-layer structure, which is preferably formed with a plurality of layers formed from different materials or substances.

9. The arrangement according to any one of the preceding claims, characterized in that the row and column arrangement of detectors with optical elements and evaluation electronics is formed with an HSI camera.