DEVICE AND METHOD FOR NON-DESTRUCTIVE TESTING OF STUD WELDING JOINTS

DE502019012233D1Active Publication Date: 2024-10-24EJOT GMBH & CO KG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502019012233
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-09-10
Filing Date
2019-08-30
Publication Date
2024-10-24
Estimated Expiration
2039-08-30

AI Technical Summary

Technical Problem

Current methods for testing stud welded connections are either destructive, unreliable, or require complex and costly procedures, often failing to detect defects until assembly or operation, which can compromise the stability and strength of the connection.

Method used

A magnetic measuring method using a device with a magnetic yoke and sensors to penetrate the welded joint, measuring changes in magnetic flux density to detect defects by comparing with reference values, optimized for cylindrical geometries and capable of spatially resolved measurements.

Benefits of technology

Provides a simple, reliable, and non-destructive means to detect defects in stud welded connections, improving sensitivity and accuracy by adapting to the geometry of the bolt and carrier plate, allowing for efficient detection of faulty connections without damaging the joint.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] A magnetic measuring method and a corresponding device are proposed, which are optimized for the simple and non-destructive testing of stud welds.

[0002] Bolt-on fasteners are used to fasten mostly cylindrical bolts to carrier plates, which are often made of sheet metal. Their applications are diverse and are found particularly in household appliances, motor vehicles, and steel and plant engineering.

[0003] For example, a car body contains approximately 500 stud welds. Bridge structures typically use several tens of thousands of shear studs.

[0004] The welded connection between the bolt and the carrier plate can be created using a laser or plasma welding process, for example, or particularly using electric resistance welding. However, joining a bolt to the carrier plate using such a welding process often results in defects such as cracks or voids, which can severely compromise the stability and strength of the connection. Faulty connections are often only discovered during final assembly or during operation and then require extensive rework.

[0005] Mechanical or thermal methods can be used to test a welded joint, but these can impair the stability of the joint due to the testing process itself.

[0006] For example, the torque test is well-known for testing stud welds, which is used as an industrial benchmark, particularly for threaded studs. However, the torque load on the studs can cause pre-damage to the welded joint.

[0007] In thermal processes, the material of the welded joint is heated, and the resulting heat distribution is measured spatially. Excessive heating can contribute to crack formation. Furthermore, such thermal tomography techniques are very complex and are typically performed in separate rooms.

[0008] An alternative is X-ray computed tomography procedures, which are both time-consuming and costly and are therefore typically only performed with a small sample.

[0009] In contrast, simple visual or acoustic tests are often not reliable enough and are difficult to automate. Both testing methods require considerable experience from the testing personnel and are also influenced by subjective assessments.

[0010] CN 2049633776 U concerns an eddy current sensor for use on rail vehicle parts.

[0011] Possibilities for detecting defects using electromagnetic means at screw holes are shown in CN 203011890 U.

[0012] The inspection of rivets is the subject of US 2008 / 0211493 A1.

[0013] A device and a method for checking riveted joints on correspondingly connected metal plates are described in CN 103868989 A.

[0014] It is therefore an object of the invention to propose a device that is as simple as possible and an efficient, reliable method for the non-destructive testing of stud welds.

[0015] According to the invention, this object is achieved with a device having the features of claim 1. This object can be achieved with the method described in claim 5. Advantageous embodiments and further developments of the invention can be realized with the features described in the subordinate claims.

[0016] The invention utilizes a magnetic field that penetrates the welded joint, whereby any defects that may form in the welded joint below and to the side of the stud alter the course of the magnetic field lines and thus the magnetic flux density. By measuring the magnetic flux density of a sample and comparing it with at least one reference or calibration value determined by measuring an ideal welded joint without defects, faulty joints can then be detected.

[0017] For the sensitivity and reliability of the process, it is important that, on the one hand, the magnetic flux penetrates the bolt and the welded joint well and, on the other hand, the magnetic field sensors, which measure the change in the magnetic flux density, are arranged as close as possible to the welded joint.

[0018] For this reason, a device is proposed that adapts as closely as possible to the specific, often cylindrical, geometry of a bolt. This is achieved by designing a magnetic yoke, for example, in the shape of a hollow cylinder, with the inner radius of the hollow cylinder selected so that it is only minimally larger than the outer diameter of the bolt, preferably a few millimeters (maximum 3 mm). For bolts with a polygonal or other shaped base, a magnetic yoke with a cavity with a correspondingly polygonal or other shaped base can be used for further optimization. The cavity can be designed to complement the outer contour of the bolt.

[0019] One or more measurements are then taken after the magnetic yoke has been placed on the bolt or the bolt has been inserted into the cavity of the magnetic yoke.

[0020] When selecting the internal dimensions of the magnetic yoke, it should be taken into account that at least one magnetic field coil still fits between the bolt and the magnetic yoke when the bolt is inserted into the cavity. Such a magnetic field coil can be permanently attached to the inner wall of the magnetic yoke and connected to an external electrical circuit. In particular, the inner diameter and height of the cavity should be selected so that the bolt to be tested can be fully inserted into the cavity.

[0021] When an electric current flows through the magnetic field coil, a magnetic field is created, which should permeate both the magnetic yoke and the stud, as well as the stud weld joint. This requires that the stud extends far enough into the hollow cylinder. To ensure this, the magnetic yoke should rest with its base on the carrier plate. However, a small gap of up to 2 mm between the magnetic yoke and the carrier plate can also be maintained, e.g., by attaching spacers.

[0022] Magnetic field sensors can rest on an annular base of the magnetic yoke and be attached, for example, by adhesive bonding. They can also be mounted internally on the inner surface or externally on the outer surface of the hollow cylinder. At least two magnetic field sensors should be arranged at opposite positions on an annular base. This allows defects that are not located centrally under the stud, but are primarily pronounced on one side of the weld joint, to be detected more efficiently than if only one magnetic field sensor or two magnetic field sensors arranged directly next to each other are used. Multiple magnetic field sensors should be arranged at equal angular distances from each other.

[0023] Alternatively, a single magnetic field sensor can be used. However, this sensor should then be guided around the bolt using rotating movements, allowing it to record multiple spatially resolved measurements. To improve measurement accuracy, measurements can also be recorded from multiple magnetic field sensors at different positions, with the different positions resulting from translational or rotating movements of the magnetic yoke around or along the bolt's longitudinal axis.

[0024] For spatially resolved spectroscopy, the carrier plate can be connected to a rotary table that is connected to a motor controller. A measurement curve is then recorded by rotating the rotary table by at least 360 degrees, with the magnetic yoke and the at least one magnetic field sensor connected to the magnetic yoke remaining fixed in the same place during the rotation, e.g., by a suspension or holder. Alternatively, the magnetic yoke and thus also the at least one magnetic field sensor can be rotated, while the carrier plate and the stud remain fixed. A measurement curve then represents the angular dependence of the magnetic flux density measured in at least one magnetic field sensor. The measurement curve of a sample under investigation can be compared with the measurement curve of a stud weld that meets the quality requirements.

[0025] For example, an average value is calculated for each measurement curve, which is derived from all measurement points within an angular range of 360 degrees. In addition, the typical standard deviation is determined for the measurement curve of a stud weld joint that meets the quality requirements. If the measurement curve of a sample under investigation deviates from the mean value of the sample under investigation by a predetermined multiple of the standard deviation in at least one angular range, it can be concluded that the stud weld joint in question is defective, and the defect can be localized by specifying the corresponding angular range.

[0026] However, standard deviations or higher moments of the statistics given by the measuring points within an angular range can also be directly compared.

[0027] To improve measurement accuracy, mean values ​​and / or standard deviations of measurement curves from several samples and / or several magnetic field sensors can also be combined.

[0028] Hall sensors are preferred for measuring a static or time-varying magnetic field. However, measuring coils, magneto-resistive, or magneto-optical sensors can also be used.

[0029] The hollow cylinder can also be closed on one side, so that the magnetic yoke consists of a hollow cylinder open on one side, with only one of the two base surfaces having an opening. The height of the hollow cylinder should then be selected so that it is greater than the maximum height of the stud above the support plate. The magnetic field sensors should be mounted on the base surface, which has an opening for inserting the stud. A hollow cylinder that is closed on one side can further increase the magnetic flux density in the stud and the weld joint.

[0030] The sensitivity of the measurement method can be improved by optimizing the design parameters of all components and advantageously positioning the fixture relative to the bolt to be tested, including the support plate. For example, the magnetic yoke can be guided or placed over the bolt by a robot arm, and the magnetic yoke can be positioned using displacement and / or position sensors. A control and evaluation device can regulate the distances to the support plate measured by the displacement and / or position sensors in such a way that the magnetic flux penetrating the magnetic field sensors is optimized.

[0031] Optimization can be achieved by conducting test measurements on defective welds and selecting the position of the magnetic yoke to achieve an optimal signal-to-noise ratio or maximize deviations from the reference value. Other parameters, such as the electrical voltage applied to the magnetic field coil or the Hall sensors, can also be optimized.

[0032] The measurement method can involve applying a static magnetic field and directly comparing the magnetic flux densities measured by at least two magnetic field sensors with reference values. A faulty connection is then characterized by deviations of at least one measured value above a predetermined tolerance. The static magnetic field can be created by selecting a permanent magnet yoke or by applying a direct current flowing through the magnetic field coil.

[0033] By applying an alternating voltage, the magnetic field coil creates a time-varying magnetic field, which induces electrical eddy currents in the stud and the weld joint. These eddy currents, in turn, generate a magnetic field that counteracts the originally applied magnetic field. The resulting effective magnetic field can then be measured in the magnetic field sensors and compared with reference values.

[0034] It should be noted that induced electrical eddy currents can lead to heating of the stud and the stud weld joint, which can impair the strength of the joint. To ensure non-destructive testing, the applied electrical voltage and frequency should be selected so that only minimal heat is generated without simultaneously reducing the sensitivity of the measurement method below a desired level.

[0035] The invention will be explained in more detail below by way of example.

[0036] Showing: Figure 1 a schematic representation of an example of a device according to the invention with a stud weld connection meeting the quality requirements. Figure 2 a section through plane AA of the experimental setup of Figure 1 . Figure 3 a schematic representation of an example of a device according to the invention with a faulty stud weld connection.

[0037] In Figure 1An example of a device for the non-destructive testing of a stud weld 3 is shown. A stud 2 is connected to a carrier plate 1 by a stud weld 3. A magnetic yoke 6, which consists of a hollow cylinder open on one side, is placed on the stud 2. Magnetic field sensors 4 are attached to a base surface of the magnetic yoke 6. Magnetic field lines of a magnetic field 7, which is generated by a magnetic field coil 5, penetrate the magnetic yoke 6, the stud 2, the stud weld 3, and the magnetic field sensors 4. The winding of the magnetic field coil 5 is closely attached to the stud 2, with the distance between the magnetic field coil 5 and the stud 2 being less than 2 mm. The magnetic field lines 7 run symmetrically with respect to the axis of symmetry of the hollow cylinder, so that the same magnetic flux density always results at the same distance from the axis of symmetry of the hollow cylinder.

[0038] In Figure 2an exemplary arrangement of the magnetization coil 5 and eight magnetic field sensors 4 is shown, wherein the eight magnetic field sensors 4 are arranged at equal angular distances from one another in a plane.

[0039] In Figure 3 is an example of a device for non-destructive testing of a faulty stud weld 3 with defect 8 and opposite Figure 1 modified magnetic field lines 7. All other elements and their reference symbols correspond to Figure 1 agree.

[0040] Defect 8 consists in the Figure 3shown example consists of a cavity which leads to an incompletely formed stud weld connection 3 and can therefore impair the strength of the connection. Since the cavity caused by the defect 8 is not penetrated by any magnetic field lines 7, the magnetic field lines 7 run asymmetrically with respect to the axis of symmetry of the hollow cylinder. This asymmetry can be detected, for example, by comparing the magnetic flux densities measured in the magnetic field sensors 4, which are mounted to the left and right of the axis of symmetry. If the difference in the magnetic flux densities is greater than a previously defined tolerance value, the stud weld connection 3 does not meet the quality requirements. Alternatively, as already described in more detail above, the entire angular dependence of the magnetic flux density can be determined by rotating the carrier plate 1 or the magnetic field sensors 4 and used to detect the defect 8.The measured values ​​recorded by the magnetic field sensors 4 represent a statistic that can be compared with a statistic resulting from the measured values ​​of a sample that meets the quality requirements. For example, the difference between the normalized standard deviations of both statistics can be calculated, and if this difference is greater than a previously defined tolerance value, a faulty stud weld can be determined. Alternative criteria for determining a faulty stud weld are described in more detail above.

Claims

1. Device for the non-destructive testing of stud welding connections (3) in which a cylindrical stud (2) is connected to a carrier plate (1) by welding, comprising a magnetic yoke (6), at least one magnetic field coil (5), and at least one magnetic field sensor (4), wherein the magnetic yoke (6) has a cavity which is formed from an open or semi-open hollow cylinder, with the inside diameter and the height of the hollow cylinder being selected such that the bolt (2) to be tested can be fully inserted into the cavity, and the at least one magnetic field sensor (4) is attached to the ring-shaped base of the magnet yoke (6), which has an opening to the cavity, or to the inner or outer lateral surface, and the at least one magnetic field coil (5) is arranged in the cavity of the magnetic yoke (6) in such a way that the magnetic field (7) generated by the magnetic field coil (5) penetrates the magnetic yoke (6), the cavity of the magnetic yoke (6) and the at least one magnetic field sensor (4).

2. Device according to claim 1, characterized in that a number of magnetic field sensors (4) are arranged at different positions and at equal and known angular distances from each other.

3. Device according to any one of the preceding claims, characterized in that the at least one magnetic field sensor (4) is a Hall effect sensor and / or a measuring coil and / or a magneto-resistive sensor and / or a magneto-optical sensor.

4. Device according to any one of the preceding claims, characterized in that the magnetic yoke (6) is a permanent magnet.

5. Method for the non-destructive testing of stud welding connections (3) by means of a device according to any one of the preceding claims, characterized in that - the magnetic yoke (6) is placed on the bolt (2) to be tested, which latter is welded to the carrier plate (1), with the bolt (2) being inserted into the hollow space of the hollow cylinder; - an electric current flows through the magnetic field coil (5), forming a magnetic field (7) which penetrates the magnetic yoke (6), the stud (2), the stud welding connection (3) and the at least one magnetic field sensor (4); and - the magnetic flux density is measured by the at least one magnetic field sensor (4) and compared with reference values.

6. Method according to the preceding claim, characterized in that the magnetic field (7) generated by the magnetic field coil (5) is a time-varying magnetic field.

7. Method according to any one of the preceding claims, characterized in that a plurality of measurement results are taken into account for comparison with a reference value, wherein the plurality of measurement results are obtained during at least one rotation of the at least one magnetic field sensor (4) about the longitudinal axis of the magnetic yoke (6), with measurements being taken both subsequent and prior to the at least one rotation, and / or the multiple measurement results are obtained from at least one translational movement of the at least one magnetic field sensor (4) along the longitudinal axis of the magnetic yoke (6), with measurements being taken both subsequent and prior to the at least one translational movement, and / or the multiple measurement results are obtained by measuring several magnetic field sensors (4), which are mounted in different positions on the magnetic yoke (6).