MANUFACTURING METHOD OF A POLISHING NUCLEAR, POLISHING NUCLEAR, ELECTROMAGNETIC ACTUATOR AND VIBRATION DAMPER

DE502021005123D1Active Publication Date: 2024-10-02SOLERO TECHNOLOGIES VILLINGEN GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502021005123
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-03-05
Filing Date
2021-03-02
Publication Date
2024-10-02
Estimated Expiration
2041-03-02

AI Technical Summary

Technical Problem

Prior art pole cores, used in electromagnetic actuators for vibration dampers, suffer from cohesive connection wear due to internal stresses and thermal expansion differences, leading to potential failure of the damper valve and vibration damper.

Method used

A manufacturing method for a pole core involving a magnetic workpiece with a groove, where non-magnetic inserts and a connecting means, such as copper, are inserted and melted to form a capillary connection, balancing material stresses and ensuring a cohesive, gas-tight seal.

Benefits of technology

The method produces a long-term stable pole core with a balanced connection, reducing the risk of failure and maintaining tightness, thus enhancing the reliability of electromagnetic actuators and vibration dampers.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a manufacturing method of a pole core having the features of patent claim 1, a pole core having the features of patent claim 10, an electromagnetic actuator having a pole core having the features of patent claim 11, and a vibration damper having such an electromagnetic actuator having the features of patent claim 12.

[0002] Pole cores are known in various designs from the prior art and are made of a magnetic material, particularly ferromagnetic metal. Such pole cores are widely used in electromagnetic actuators for conducting magnetic flux, for example, in damper valves for controlling the damping characteristics of a vibration damper. Damper valves have an outlet opening between an inlet and an outlet, which can be closed more or less. By opening or closing, the outlet opening is throttled, thus adjusting the damping behavior of a vibration damper. If the vehicle is to have a "hard" chassis, the throttling effect is increased or the outlet opening is closed more. For a "soft" chassis, the outlet opening is opened further.The opening and closing of the damper valve is carried out by an electromagnetic actuator system, which moves a valve body when an excitation coil is energized accordingly.

[0003] Damper valves should be designed to be "fall-safe" so that, for example, if the electromagnetic actuator fails, the vehicle can be operated safely with such a vibration damper.

[0004] Various pole core designs have been proposed in the prior art for this purpose. The pole core serves as a flux-conducting component and, at the same time, seals off components of the electromagnetic actuator from the medium in the vibration damper. This sealing is necessary to prevent contaminants from penetrating the components of the electromagnetic actuator and potentially disrupting the function of the electromagnetic actuator or vibration damper.

[0005] Further prior art is provided by the documents DE 43 10 719 A1 and US 2006 144 666 A1, from which a manufacturing process for a pole core is previously known.

[0006] In the past, a pole core with a flange was proposed for this purpose, which is divided into a first section and a second section by an interruption. A non-magnetic insert is arranged in the interruption and connects the first section to the second section. The insert is typically bonded to both the first and second sections by brazing and seals the interruption. A pole core designed in this way is gas-tight and liquid-tight and has proven itself in the past. However, it has been shown that the bonded connection between the first section, the insert and the second section is subject to wear due to residual stresses and different thermal expansion coefficients, and the tightness of the interruption cannot be permanently guaranteed, which can lead to premature failure of the electromagnetic actuator orof the damper valve and possibly the vibration damper.

[0007] This is where the present invention comes in.

[0008] The present invention aims to propose an improved manufacturing method for a pole core, a pole core, an improved electromagnetic actuator, and an improved vibration damper that expediently eliminates the disadvantages known from the prior art and enables the production of a long-term stable pole core while taking economic aspects into account. These objects are achieved by a manufacturing method for a pole core having the features of patent claim 1, a pole core having the features of patent claim 10, an electromagnetic actuator having the features of patent claim 11, and a vibration damper having the features of patent claim 12.

[0009] Further advantageous embodiments of the present invention are specified in the subclaims.

[0010] The inventive manufacturing method for a pole core with the features of claim 1 comprises the following process steps: Providing a magnetic workpiece having a first side and a second side, wherein the first side has a groove directed towards the second side, inserting at least two inserts and at least one connecting means into the groove, wherein the at least one connecting means is arranged between two inserts, and materially connecting the at least two inserts to one another and / or the at least two inserts to the workpiece by preferentially melting the connecting means.

[0011] The inventive manufacturing method for a pole core is based on the discovery that, when the bonding agent melts, capillary forces distribute the molten bonding agent over the contact surfaces between the workpiece and the inserts, completely wetting the contact surfaces, thereby creating an intermetallic bond between the inserts and the workpiece. With at least two inserts inserted into the groove, material stresses are partially compensated by distributing the force vectors, and a pole core with a closed and integral connection can be provided, eliminating the problems known from the prior art. Reducing the flow paths of the molten bonding agent has also proven essential.

[0012] Here and below, in the context of this invention, a magnetic workpiece is understood to mean a workpiece made of a soft magnetic material that can be easily magnetized in a magnetic field. Such a material is, for example, carbon steel, iron or so-called soft iron, steel with added silicon, a nickel-iron alloy, a nickel-cobalt alloy, or similar.

[0013] Furthermore, a preferred development of the manufacturing method provides that the at least two inserts are made of a non-magnetic material, in particular of stainless steel or rust-proof steel.

[0014] It has also proven advantageous during implementation of the manufacturing process for the at least one connecting means to comprise at least one isolated copper body that is inserted into the groove. Copper is eminently suitable for producing a material-to-material connection in the form of a closed soldered connection and, due to its material properties, has a high level of elasticity, which allows tensions due to different thermal expansions of the inserts and the workpiece to be compensated. Furthermore, copper has a low viscosity in its molten state, which is why the melt of the connecting means completely wets the inserts in the groove due to capillary forces and, after cooling, enables a resilient, brazed and material-to-material connection. The at least one isolated copper body can preferably be a copper body adapted to the shape of the groove.For example, the copper body can be a copper wire, a preformed part, or bulk material. The copper body can also be made of a copper alloy. Alternatively, instead of copper, another non-magnetic connecting material, such as silver, brass, or similar, can be used as the connecting material. Brazing, by definition, occurs in a temperature range above 723 K.

[0015] A further development of the manufacturing method provides that the groove is machined into the first side of the workpiece by a machining process, wherein the groove in the first side is preferably formed as an annular groove with a U-shaped cross-section, comprising an inner side, a base side and an outer side. The respective insert is cuboid in cross-section and can be adapted to the shape of the groove. The insert has a first surface and a second surface. In the case that the groove is an annular groove, the respective insert can also be annular, wherein the first surface corresponds to an inner circumferential surface and the second surface to an outer circumferential surface.

[0016] According to a further preferred embodiment of the manufacturing method, the first surface and / or the second surface of at least one of the two inserts is designed as a transition fit, which is why the insert in question can be pressed into the groove with a moderate pressing force. It can be advantageous if the insert only has a transition fit on the first side or the second side, while a clearance fit can be provided on the other side, thus taking into account the different thermal expansion of the materials used for the workpiece and the inserts. When the required temperature is reached, the connecting agent melts and can flow through approximately equally sized capillary gaps on both the first side and the second side. Due to capillary forces, the melt flows and is distributed throughout.

[0017] According to a further advantageous embodiment of the present manufacturing method, the workpiece is positioned during the material-to-material joining process such that at least one of the inserts is pressed into the groove by gravity. As soon as the connecting agent has liquefied upon reaching its melting temperature, at least one of the inserts can exert a compressive force on the liquefied connecting agent by gravity and displace the liquefied connecting agent between the at least two inserts, thus promoting the distribution of the molten connecting agent over the contact surfaces in the capillary gaps. The corresponding insert sinks, preferably until the at least two inserts are in abutting relationship in the groove—apart from a thin layer of the molten connecting agent.When the workpiece cools, the connecting material hardens and forms a closed, material-locking connection both between the workpiece and the inserts and preferably between the at least two inserts.

[0018] According to a preferred development of the manufacturing method, the workpiece is heated and the connecting agent is liquefied until the connecting agent is almost completely displaced by capillary transport in the groove between the inserts and the two inserts are butted against each other in the groove. Excess melt of the connecting agent can either escape from the groove or settle in a recess in the bottom. An approximately constant thickness of the connecting agent after cooling, both in the capillary gaps and between the inserts, prevents the formation of cavities or hollow spaces, which could impair the tightness of the bonded joint and promote residual stresses.

[0019] A further development of the manufacturing method provides that, after the workpiece has cooled, material is removed from the first side and / or the second side. It is particularly preferred if, after the workpiece has cooled, the first side and / or the second side are reworked using a machining process, for example, turning, milling, or grinding.

[0020] Preferably, material is removed at least in regions on the second side in order to expose an end face of one of the at least two inserts—or the bottom side of the groove—on the second side, thereby dividing the magnetic workpiece into a first section and a second section. After the at least partial removal of the second side and the exposure of at least one of the inserts, the groove forms an interruption between the first section and the second section, wherein the first section and the second section are integrally connected in the interruption by means of the at least two inserts and the connecting means.

[0021] A further aspect of the present invention relates to a pole core produced using the manufacturing method according to the invention. The pole core is preferably divided into at least two sections by an interruption, wherein at least two non-magnetic inserts are arranged in the interruption, via which the at least two sections can be connected with a material bond.

[0022] Furthermore, it is preferred if the at least two non-magnetic inserts are made of stainless steel or stainless steel and are connected by means of a brazed, integrally bonded joint, wherein copper can serve as the connecting means. The interruption is sealed gas- and liquid-tight by the inserts and the integrally bonded joint, preventing any material transport through the interruption from the first side to the second side or vice versa.

[0023] A further aspect of the present invention relates to an electromagnetic actuator with such a pole core.

[0024] A third aspect of the present invention relates to a vibration damper with such an electromagnetic actuator.

[0025] A fourth and final aspect of the present invention relates to a motor vehicle having at least one such vibration damper.

[0026] An embodiment of a pole core according to the invention is described in detail below with reference to the accompanying drawings. They show: Figure 1 shows a sectional view of a workpiece with a groove into which two inserts are pressed and which are connected to the workpiece by means of a brazed, material-locking connection in the groove, and Figure 2 shows a schematic representation of the manufacturing process of a pole core.

[0027] In the following, identical or functionally equivalent components are identified by the same reference symbols. For the sake of clarity, not all identical or functionally equivalent parts are provided with a reference number in the individual figures.

[0028] Figure 1 shows a workpiece 10 that is approximately rotationally symmetrical about a longitudinal axis XX. The workpiece 10 has a sleeve portion and a flange portion, with the flange projecting perpendicularly from the longitudinal axis XX of the sleeve portion.

[0029] The flange portion has a first side 11 and a second side 12, which are arranged spaced apart in the longitudinal axis XX on opposite sides of the flange portion.

[0030] In the flange section, from the first side 11, a groove 15 with a U-shaped cross section is arranged, which is arranged annularly around the longitudinal axis XX, preferably rotationally symmetrically thereabout, and is directed toward the second side. The groove 15 has an inner side 15a, a bottom side 15b, and an outer side 15c, with the inner side 15a and the outer side 15c being arranged parallel to the longitudinal axis XX. The bottom side 15b can be curved toward the second side 12 and can have a conical or spherical countersink.

[0031] Furthermore, the Figure 1It can be seen that two inserts 20 are inserted or pressed into the groove 15. Each insert 20 is made of a non-magnetic material, for example, stainless steel. Each insert 20 is annular with two end faces 20b, a first surface 20a formed by an inner lateral surface, and a second surface 20c formed by an outer lateral surface.

[0032] The respective insert 20 can be inserted into the groove 15 coaxially to the longitudinal axis XX, wherein the first surface 20a and the second surface 20c of the insert 20 are adapted to the inner side 15a and the outer side 15c. The inner side 15a of the groove 15 and the first surface 20a of the respective insert 20 can be designed as a transition fit and their dimensions lie within a tolerance band of ± 0.05 mm, more preferably ± 0.025 mm, and particularly more preferably ± 0.015 mm. The outer side 15c of the groove 15 and the second surface 20c of the respective insert 20 can also be designed as a transition fit and their dimensions lie within a tolerance band of ± 0.025 mm, more preferably 10.015 mm.

[0033] Figure 1shows that a further pole core section 40 made of a magnetic material can be connected to the workpiece 10. The pole core section 40 is connected to the workpiece 10 via a non-magnetic sleeve 30, preferably made of stainless steel, wherein the non-magnetic sleeve 30 can also be connected by means of the connecting means 25 through a brazed, integral connection. Preferably, the workpiece 10 can have a conical chamfer 35 on the side facing the sleeve 30.

[0034] In the groove 15, the two inserts 20 are integrally connected to the workpiece, wherein the integral connection is effected by brazing with a connecting agent 25 at temperatures above 723 K, which, according to a preferred embodiment of the manufacturing process described in more detail later, contains copper.

[0035] For this purpose, the workpiece 10 made of a magnetic material with the first side 11 and the second side 12 is firstly machined in a process step 100 according to Figure 2 provided.

[0036] Subsequently, in process step 120, the groove 15 is machined into the workpiece 10 on the first side 11 - preferably by turning or milling.

[0037] In a subsequent method step 130, at least two inserts 20 and the connecting means 25 are inserted into the groove 15, with the connecting means 25 being arranged between the two inserts 20, preferably as at least one separate body. In this state, the insert 20 last inserted or pressed into the groove 15 can protrude from the groove 15 in certain areas.

[0038] In a subsequent method step 140, the arrangement formed in method step 130 for the material-locking connection of the inserts 20 to the workpiece 10 and the inserts 20 to one another is heated until the connecting means melts.

[0039] In the case that copper is used as connecting means 25, the arrangement is heated at least to the melting temperature of copper, which is approximately 1358 K. The copper liquefies and flows due to capillary forces around the inserts 20 in the groove 15, in particular in capillary gaps between the inner side 15a and the first side 20a as well as between the outer side 15c and the second side 20c.

[0040] When heating the assembly formed in process step 130, it is advantageous if the workpiece 10 is arranged such that the groove 15 is arranged in the vertical direction such that the inserts 20 are pressed into the groove 15 by gravity. Accordingly, the Figure 1 shown workpiece 10 so that the longitudinal axis XX is aligned vertically and the groove 15 points upwards with respect to the earth's surface.

[0041] The assembly from process step 130 is heated to a temperature above the melting temperature of the connecting means 25 until the connecting means 25 between the two inserts 20 has completely melted and the two inserts 20 are in abutting relationship except for a remaining film layer of connecting means 25. A pressing force can also press the two inserts 20 into the groove 15 in the heated state of the assembly.

[0042] After cooling, both the first side 11 and the second side 12 can be mechanically reworked. To form the pole core 1 according to the invention, material is removed from the second side 12 in process step 150 in order to expose the groove 15 or the insert 20 initially inserted into the groove 15 and to divide the workpiece into two sections 16, 18. The insert 20 is preferably exposed by milling or turning, whereby the workpiece 10 is divided into the two sections 16, 18 by an interruption filled by the groove 15 and the inserts 20 arranged in the groove 15 with a material fit. The two sections 16, 18 are connected exclusively by non-magnetic material, namely the two inserts 20 and the connecting means 25. List of reference symbols

[0043] 1Pole core 10Workpiece 11First side 12Second side 15Groove 15aInside 15bBottom 15cOutside 16Sections 18Section 20Insert 20aFirst face of 20 20bEnd of 20 20czecond face of 20 21First face 22Second face 25Connecting element 30Sleeve 35Bevel 40Pole core section X-XLongitudinal axis

Claims

1. Manufacturing method for a pole core (1), comprising the following method steps: - providing a magnetic workpiece (10), having a first side (11) and a second side (12), wherein the first side (11) comprises a groove (15) oriented toward the second side (12), - inserting at least one insertion (20), as well as at least one attaching agent (25) into the groove (15), wherein the at least one attaching agent (25) is arranged between the two insertions (20), and - integrally connecting the at least two insertions (20) to each other and, optionally, the at least two insertions (20) to the workpiece (10).

2. Method in accordance with claim 1, characterized in that the integral connecting of the at least two insertions (20) to each other and / or of the at least two insertions (20) to the workpiece (10) is carried out by heating the workpiece and liquefying the attaching agent (25).

3. Method in accordance with claim 1 or 2, characterized in that the at least two insertions (20) are made of a non-magnetic material, in particular stainless steel.

4. Method in accordance with any of claims 1 to 3, characterized in that the attaching agent (25) comprises at least one isolated copper body which is inserted into the groove (15).

5. Method in accordance with any of the preceding claims, characterized in that the at least two insertions (20) comprise, on a first surface (21) and / or on a second surface (22) a transition fit (23), which is adapted to the groove (15).

6. Method in accordance with any of the preceding claims, characterized in that at least one of the two insertions (20) is inserted into the groove (15) by means of press fitting.

7. Method in accordance with any of the preceding claims, characterized in that the workpiece (10) is positioned during the integral connecting such that at least one of the two insertions (20) is pressed into the groove (15) by the force of gravity.

8. Method in accordance with any of the preceding claims, characterized in that the heating of the workpiece and the liquefying of the attaching agent (25) are continued until the attaching agent (25) in the groove (15) between the insertions (20) is melted away via capillary transport and the at least two insertions (20) lie approximately end-to-end in the groove (15).

9. Method in accordance with any of the preceding claims, characterized in that the second side is removed in order to expose at least one of the at least two insertions (20), preferably by means of a machining procedure.

10. Pole core (1), having a groove (15) which divides the pole core (1) into at least two sections (16, 18), wherein at least two non-magnetic insertions (20) are arranged in the groove (15), via which the at least two sections (16, 18) are connected to each other, and which are integrally connected to each other by means of an attaching agent (25).

11. Electromagnetic actuator having a pole core (1) in accordance with claim 10.

12. Shock absorber for a motor vehicle having an electromagnetic actuator in accordance with claim 11.

13. Motor vehicle having a shock absorber in accordance with claim 12.