PVT METHOD AND APPARATUS FOR PROCESS-PROOF PRODUCTION OF SINGLE CRYSTALS
Patent Information
- Application Number
- DE502022001983
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-09-16
- Filing Date
- 2022-09-16
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2042-09-16
AI Technical Summary
The existing PVT process for producing single-crystalline silicon carbide (SiC) crystals faces challenges in safely using reactive gases like hydrogen, which are flammable and toxic, due to the risk of explosive gas mixtures when the process chamber is damaged, and the need for complex vacuum-tight apparatuses.
A safety container surrounding the process chamber is flooded with an inert gas to prevent explosive mixtures, allowing for the use of reactive gases while maintaining a non-explosive atmosphere, even in the event of damage, and incorporating a gas sensor to interrupt gas supply if reactive gases leak into the safety container.
This solution enables the reliable and cost-effective production of SiC single crystals by preventing explosions and allowing the use of reactive gases, while also providing a cost-effective and less complex apparatus design that maintains a protective atmosphere and temperature control.
Description
Field of the invention
[0001] The invention relates to a PVT process for the reliable production of single crystals in an apparatus which has a highly heatable growth cell, a process chamber in which the growth cell is located, and a heating device surrounding the process chamber for heating the growth cell, wherein a source material and a nucleus are introduced into the growth cell, the process chamber is filled with a process gas and the growth cell is heated so that the source material is sublimated and resublimated at the nucleus. Background and general description of the invention
[0002] In industrial settings, the so-called physical vapor transport (PVT) process is considered the standard method for producing single-crystalline silicon carbide crystals (SiC crystals). The source material is usually a powder containing many different crystallites. The use of bulk crystals is also possible. An alternative process is the high-temperature chemical vapor deposition (HT-CVD) process. In the PVT process, crystal growth typically occurs within the graphite growth cell by sublimation of a SiC source material and crystallization at a predetermined SiC seed at temperatures above 2,000 °C. The driving force for crystal growth is a temperature gradient imposed on the growth cell by a heating device. Common methods for heating PVT apparatus use resistance heaters or induction heaters.With inductive heating, the growth cell (hot zone) of the vacuum-tight process chamber is surrounded by a non-conductive material, typically (quartz) glass, containing process gases required, among other things, to influence crystal growth. The process chamber can be single- or double-walled and air- or water-cooled. Typically, argon, helium, nitrogen, hydrogen, and possibly other gases for targeted doping are used as process gases. The process pressure can range from vacuum conditions to atmospheric pressure. In common processes for producing doped SiC single crystals, hydrogen is used either in low concentrations or not at all.
[0003] SiC single crystals are required for a wide range of applications in semiconductor technology due to their large band gap and high thermal conductivity.
[0004] The underlying process for producing SiC single crystals has therefore already been described in numerous documents. Reference is made to US 2011 / 0300323 A1 as an example. According to this document, an inert gas is used as the process gas, which is unproblematic from a safety perspective. Regarding the prior art, reference is also made to EP 0 811 708 A2, US 2012 / 0086001 A1, GB 772,691, DE 60 2004 001 802 T2, EP 3 760 765 A, and JP H04 193799 A.
[0005] It is a conceptual starting point and one of the objects of the present invention to enable processes, including those for the targeted incorporation of dopant substances or for the production of undoped SiC single crystals. With this starting point in mind, the present invention develops a process sequence that is reliable, with better results than in the prior art, yet still cost-effective, using a reactive gas, i.e., a flammable and / or reactive (possibly toxic) gas, e.g., hydrogen as the process gas, with concentrations of over 5% and up to 100%.
[0006] The gas molecules of the reactive gas, particularly hydrogen atoms, attach themselves to the surface of the growing single crystal, but are immediately displaced by the subsequent sublimated components of the source material. In this case, the reactive gas molecules, such as hydrogen atoms, briefly act as placeholders, allowing the creation of a crystal lattice with few defects, if not completely defect-free. Reactive gas molecules can also react with other process gases, the source material, or even the hot zone material, forming further gaseous species that enter the process gas atmosphere and can, at least temporarily, attach to the crystal. Possible reactive gases, such as silane, methane, propane, etc., supply, among other things, the elements silicon and carbon, which are incorporated into the crystal. The addition of reactive gases can overall influence the defect density (desired and / or undesired).However, the exact effect depends on a variety of parameters and their interaction. The addition of a reactive gas is intended to influence crystal growth.
[0007] The object of the present invention can therefore be seen in providing a device and a method with which improved or modified crystal growth is possible.
[0008] In a partial aspect or further development of the invention, it can be considered as an aspect of the object to provide a device and a method in which a reactive gas can be used to improve crystal growth.
[0009] In yet another aspect or development of the invention, the object may be to provide a device and a method by means of which improved crystals can be provided with little effort or cost-effectively.
[0010] However, the use of a reactive gas, including, for example, hydrogen or other reactive elements, poses a potential hazard when carrying out the process. A reactive gas can, for example, be flammable or combustible and / or toxic. In the case of hydrogen, an oxyhydrogen reaction can occur with the oxygen in the air, which is why hydrogen is referred to as a reactive gas in this description. Other examples of reactive gases currently under consideration include, in addition to hydrogen, carbon- and silicon-containing precursors or hydrocarbons and their derivatives (examples: silane, methane, propane, etc.).
[0011] Furthermore, in today's common equipment, the process chamber is typically made of quartz glass, which is inherently brittle and prone to breakage. However, quartz glass is particularly preferred because it can withstand the high temperatures of the growth cell and because it does not shield the electromagnetic field of an induction coil or the radiant heat of a resistance heater. A combination of induction and resistance heaters can also be provided. For example, an additional floor or ceiling heater can be designed as a resistance heater, while the main heater is designed as an induction heater. In principle, however, the safety requirements also apply to other materials used to provide the process chamber, and this is particularly true in the case of quartz glass.
[0012] However, if the process chamber becomes damaged or leaks, for example, if the quartz glass breaks, the hydrogen can mix with the ambient oxygen, creating an oxyhydrogen gas that is ignited by the heating device (hot components of the hot zone, typically graphite parts inside the process chamber) and explodes. Therefore, if a reactive gas is used, reliable performance of the process with the existing equipment is not possible.
[0013] A reactive gas mentioned in this description – in particular hydrogen – is not to be equated with known doping gases. Known typical doping gases are not used in the concentrations desired here and / or are neither flammable nor otherwise reactive within the meaning used in this description. Doping gases are purged around the crystal, meaning the processes take place entirely within the process chamber. For example, in this context, the process chamber can also be purged with an inert gas such as argon to directly modify the PVT process. Generally, doping gases are intended to be incorporated into the crystal or crystal structure – which is where the term "doping gas" comes from – in order to influence the physical and / or chemical properties of the crystal, for example, its electrical conductivity. In other words, molecules orComponents of a doping gas later become integral building blocks of the crystal. Such molecules or components of a doping gas remain in the crystal and can be detected there later.
[0014] In contrast, a reactive gas such as hydrogen, as a reactive component of the gas atmosphere, can influence crystal growth and dopant incorporation, but should not be incorporated into the crystal like a doping gas in order to influence the physical and chemical properties of the crystal. Due to the hazard potential of reactive gases, in particular ignition, burn-up, deflagration or even poisoning potential, reactive gases have not yet been considered for use in improving crystal growth, or at least the safety aspects described above when handling a reactive gas in this environment have not been sufficiently taken into account. Furthermore, the reactive gas to be used is not a source material in the true sense of the word. In typical PVT processes, the source material is SiC powder. In variants of the classic PVT process, such as HT-CVD, hydrogen can be used as a carrier gas, which is usually the actual source material.dR transports gaseous C- or Si-containing precursors. The gas serves as a carrier gas, i.e., a transport medium for precursors and dopants. Dopants can be solid, liquid, or gaseous elements or compounds, typically containing nitrogen, phosphorus, aluminum, boron, or vanadium.
[0015] As part of this further development and improvement, the containment vessel surrounding the process chamber was designed with the present description. Furthermore, the provision of a protective atmosphere, particularly with an inert gas, in the area between the process chamber and the vessel wall was investigated. One particular goal of the containment vessel is to prevent or prevent the formation of an explosive gas mixture in the event of damage, particularly rupture, of the process chamber.
[0016] To ensure reliable process performance, the apparatus for carrying out the process could be arranged in a vacuum cell. However, such a cell would have to be absolutely vacuum-tight and is therefore comparatively complex to manufacture because numerous feedthroughs are required to supply the apparatus with electricity, gas, and possibly cooling fluid, each of which must be vacuum-tight.
[0017] It would be advantageous, however, to present a PVT process for the reliable production of single crystals that can be carried out in an apparatus that is easy to manufacture and / or cost-effective.
[0018] The problem is solved by the invention defined in the independent claims. Dependent claims specify further developments and preferred embodiments of the invention.
[0019] To achieve the object, the invention provides that the process gas consists partly or completely of a reactive gas and that the process chamber is arranged in a containment vessel, wherein an intermediate space between a vessel wall of the containment vessel and the process chamber is flooded with a protective atmosphere, for example an inert gas, in order to displace the air therein before the sublimation of the source material is initiated.
[0020] The containment vessel should be flooded no later than when the source material sublimates, because at this point the high temperatures that can ignite the reactive gas are present. However, for safety reasons, the containment vessel should be flooded before the reactive gas is introduced into the process chamber.
[0021] Should this arrangement result in damage - in particular a breakage - of the process chamber, the reactive gas of the process chamber mixes in the protective atmosphere in the containment vessel, for example with the inert gas, to form a non-explosive gas mixture, so that an explosion cannot occur even in a hot environment.
[0022] This safety measure is particularly important when the reactive gas is flammable or prone to deflagration, such as hydrogen.
[0023] The containment vessel is particularly easy to realize if it is designed in such a way that it allows gas losses to the outside, especially to a small extent, i.e. is only approximately gas-tight. This makes the construction of the containment vessel more cost-effective, as requirements for particularly high hermeticity do not have to be taken into account and yet no undesirable reactions of the reactive gas can occur outside the process chamber. For example, the containment vessel can have a permissible leak rate greater than 0 l / min. For cost reasons, it can be advantageous and unproblematic, particularly due to the choice and geometry of the design, to allow a leak rate in the range 0 ≤ leak rate ≤ 5 l / min, or even in the range 0 ≤ leak rate ≤ 30 l / min. For example, the permissible leak rate can be greater than 2 ml / min, less preferably 5 ml / min, even less preferably 10 ml / min, even less preferably 50 ml / min or even 100 ml / min.On the other hand, it is not sensible to allow an excessively high leakage rate from the containment vessel for economic reasons and, possibly, for workplace safety reasons. For example, it may be desirable to limit the leakage rate to less than 30 l / min, preferably 10 l / min, more preferably 4 l / min, even more preferably 1 l / min, more preferably 500 ml / min, and even more preferably 150 ml / min. The goal is to achieve leakage rates in a range of 2 ml / min to 50 ml / min, preferably 10 ml / min to 20 ml / min.
[0024] To maintain the protective atmosphere, for example, inert gas can be added to compensate for gas losses and to build up and / or maintain an overpressure in the containment vessel. The overpressure prevents atmospheric oxygen from outside from entering the containment vessel. For example, a pressure regulating system can be used to maintain a relative overpressure in the containment vessel, for example in a range of 1 mbar above ambient pressure or more, preferably 3 mbar or more, more preferably 5 mbar or more, to 50 mbar above ambient pressure or less, preferably 30 mbar or less. However, a completely gas-tight containment vessel with a leak rate of 0 ml / min or a leak rate that is not measurably low is also generally included here, in which an overpressure can also be maintained in the containment vessel.
[0025] To ensure the most complete possible displacement of air from the containment vessel, the present description may further provide for a first inert gas to be admitted into the containment vessel to flood the vessel. The first inert gas may be heavier than air, so that it is admitted into the lower region of the containment vessel, displacing the air upwards. For this purpose, for example, a closable outlet at the upper end of the containment vessel may remain open until the air has escaped.
[0026] The protective atmosphere preferably comprises an inert gas, such as argon. Due to argon's high density, it collects at the bottom of the containment vessel and slowly displaces the air upwards without mixing with it. Other examples of protective atmosphere compositions that are currently commercially available include xenon, nitrogen, or carbon dioxide. In principle, the protective atmosphere can comprise any fluid, whether individually or as a mixture, that is capable of providing a protective function by neutralizing the reactive gas in the event of excessive or inadmissible escape from the process chamber and / or preventing negative effects such as deflagrations. The protective atmosphere can, for example, also exist in the liquid or solid state under normal conditions of the standard atmosphere.
[0027] Once the air has been displaced by the first inert gas, it can be replaced by another, for example, a less expensive, inert gas. The invention therefore further provides that after one or more floodings of the containment vessel with the first inert gas, this is replaced by the second inert gas, in particular nitrogen.
[0028] To ensure that the reactive gas is no longer fed into the apparatus in the event of a breach in the process chamber, the containment vessel is provided with a gas sensor capable of detecting the presence of reactive gas in the containment vessel. Furthermore, the process gas supply to the process chamber can be interrupted if the gas sensor detects the reactive gas in the containment vessel.
[0029] In a further development, the gas supply can be interrupted via an additional pressure sensor or pressure switch that monitors the pressure within the process chamber if a lower pressure is detected in the event of damage, such as a break in the quartz glass. For example, monitoring can detect a drop in absolute pressure to p ≤ 980 mbarAbs, preferably to p ≤ 950 mbarAbs, more preferably to p ≤ 920 mbarAbs. The interruption of the reactive gas supply can thus also occur independently of the detection of reactive gas, such as hydrogen, in the space between the process chamber and the cooling jacket.
[0030] An opening of the process chamber, for example, in the event of a quartz glass break, can be detected or indicated by one of the following criteria. The reactive gas / hydrogen can be detected by a gas sensor in the containment vessel. Alternatively or cumulatively, the overpressure in the containment vessel can be determined, and if the overpressure disappears, a process disturbance can be concluded (e.g., p<= approx. 2 mbarg compared to atmosphere).
[0031] Furthermore, the pressure in the process chamber can be measured, either alternatively or cumulatively. As long as this pressure remains below 950 mbarAbs (or 920 or 980), no process disturbance is detected. Exceeding the pressure threshold may indicate a process disturbance. Alternatively or cumulatively, a sudden pressure surge / pressure increase in the process chamber (pressure increase rate greater than the maximum possible pressure increase rate due to the gases being introduced) may also be detected and indicate a process disturbance—such as a quartz glass breakage. The aforementioned criteria are advantageously independent of one another and can be used individually or in conjunction with one another to shut down the process gas or hydrogen supply.
[0032] The containment vessel can advantageously provide a cooling function. The cooling function can, for example, be designed such that a cooling medium, such as water in particular, circulates around or through the containment vessel. For example, the containment vessel can have at least one cooling medium line through which the cooling medium flows. The at least one cooling medium line can be attached to the vessel wall of the containment vessel or at least connected thereto in a thermally conductive manner, if necessary with the aid of a thermally conductive paste. For example, the cooling medium line is soldered to the vessel wall. For example, the cooling medium line comprises copper, which is easy to process and / or is particularly thermally conductive.
[0033] The containment vessel can be equipped to provide temperature control of the process conditions. For example, a containment vessel designed in this way can always maintain constant temperatures—or a similar temperature range—regardless of potentially highly fluctuating ambient conditions. For example, the environment may include a daily temperature curve or seasonal temperature fluctuations, or may also be influenced by nearby thermal processes, whereby the advantageously designed containment vessel can isolate these ambient conditions from the process. Alternatively or cumulatively, the cooling function can also be influenced in response to the process parameters, in particular the temperature in the process chamber, in order to achieve temperature control of the growth process.For example, the cooling medium flow rate through the at least one cooling medium line can be varied in response to the ambient conditions and / or the process parameters in order to alter heat dissipation. In warmer ambient and / or process temperatures, for example, more cooling medium can be converted, and / or a cooler cooling medium can be used, and / or an alternative cooling medium can be introduced.
[0034] The cooling medium line can be arranged on the outside of the container wall, preferably thermally connected to the container wall or at least arranged adjacent to the container wall. The cooling medium line can then cool the container wall and ensure that the heat does not radiate into the immediate vicinity of the equipment, but is carried away by the temperature control device. The external arrangement of the cooling medium line has the advantage that fewer passages into the protective atmosphere or the interior of the protective container need to be sealed, since the cooling fluid does not penetrate into the interior. For example, the container wall can be double-walled, i.e., have an inner wall and an outer wall, whereby the cooling medium line can be arranged between the inner and outer walls of the container wall.The cooling medium line and its mountings are then concealed and protected from mechanical damage. Since the temperature control system is capable of dissipating a significant portion of the heat output from the process chamber, the outer wall of the vessel is subject to few or no restrictions regarding material selection or contact protection, as it does not become hot.
[0035] The invention further relates to an apparatus for the reliable production of single crystals according to the PVT process, which apparatus has a highly heatable growth cell for receiving a source material and a seed, a process chamber in which the growth cell is located and which has a connection to a process gas source for filling it with a process gas, and a heating device for heating the growth cell.
[0036] In order to ensure process-safe operation with a reactive gas as the process gas, the invention provides that the apparatus has a containment vessel having a vessel wall in which the process chamber is arranged, wherein the containment vessel has a connection to an inert gas source in order to be able to flood an intermediate space between the vessel wall of the containment vessel and the process chamber with an inert gas before carrying out the PVT process.
[0037] The containment vessel can be designed to allow gas to escape to the outside. It can have a pressure sensor, the pressure sensor being signal-connected to a control device, and the control device being designed to set an overpressure in the containment vessel (relative to the environment or atmosphere) based on the pressure sensor signals.
[0038] The pressure sensor can also include a pressure switch or be formed from a pressure switch. For example, the pressure sensor can be a differential pressure switch that measures the pressure difference between the inerting system in the containment vessel and the atmosphere or surroundings. If necessary, the pressure sensor can then trigger a circuit when an adjustable pressure difference is exceeded or undershot, particularly as a safety circuit or shutoff.
[0039] Based on the intended setup of the device, there is an inert gas connection in the lower section of the containment vessel and a closable outlet in its upper section. This completely displaces the air in the containment vessel upwards to the outlet, where it exits the containment vessel, by the inert gas flowing in at the lower section.
[0040] The containment vessel preferably has two inert gas connections for two different inert gases. After the first inert gas has displaced the air from the containment vessel, a less expensive fluid, such as nitrogen, can be introduced through the second inert gas connection, thus replacing the first inert gas.
[0041] The containment vessel preferably has a gas sensor that responds to a reactive gas. This allows it to be detected that a reactive gas (e.g., hydrogen) has entered the containment vessel, for example, in the event of a breach in the process chamber.
[0042] As already mentioned above, the apparatus can be used, in particular, to produce a SiC single crystal using the PVT process. For this purpose, the growth cell is equipped with silicon carbide as the source material, and the process chamber is flooded with hydrogen as a reactive gas, in addition to other process gases (e.g., argon). Short description of the characters
[0043] It shows: Fig. 1 Cross-sectional view of an apparatus according to the invention, Fig. 2 Perspective and simplified view of a partially assembled containment vessel, Fig. 3 Perspective sectional view of an embodiment of an apparatus, Fig. 4 Detail of a connection of the temperature control device of the containment vessel, Fig. 5 Segment of the vessel wall of the containment vessel with part of the temperature control device, Fig. 6 Structure of an exemplary segment of a vessel wall with temperature control device, Fig. 7 Perspective view of an embodiment of a containment vessel 8. Detailed description of the invention
[0044] In the following, the invention is described in more detail using exemplary embodiments and with reference to the figures, wherein identical and similar elements are partially provided with the same reference numerals and the features of the various exemplary embodiments can be combined with one another. Figure 1 shows a cross-sectional view of an apparatus according to the invention.
[0045] At the center of the apparatus, a growth cell 1 consisting of a hollow cylinder with a base and a lid sealing both ends is located on a stand. The growth cell 1 is made of porous graphite. A source material 2 is layered on the base. A seed 3 is located on the underside of the lid.
[0046] The growth cell 1 is arranged in a process chamber 4, which consists of a hollow cylinder closed at both ends by a floor and a ceiling. The cylindrical wall of the process chamber 4 is made of heat-resistant quartz glass and can be filled with a process gas via a process gas connection with an inlet valve 5. Since the graphite of the growth cell 1 is porous, the process gas also flows from the process chamber 4 into the growth cell 1.
[0047] A heating device 6 consists of an induction coil 7 that surrounds the process chamber 4 at the level of the growth cell. When an electric current flows through this coil, it generates an electromagnetic field that induces an electric current in the graphite of the growth cell 1, heating the growth cell 1 to temperatures of over 2,000 °C up to 2,400 °C.
[0048] The high temperatures and the required permeability for the electromagnetic field of the induction coil 7 make it necessary to manufacture at least the cylindrical wall of the process chamber 4 from a suitable, temperature-resistant material. Typically, the cylindrical wall of the process chamber 4 is made of quartz glass, which has proven particularly suitable and inexpensive to manufacture.
[0049] To produce a SiC single crystal, silicon carbide is introduced into the growth cell 1, and the process chamber 4 is flooded with a process gas consisting of up to 100% hydrogen. If the growth cell 1 is then heated by the induction coil 7, the silicon carbide sublimates and deposits itself layer by layer on the seed 3, so that a SiC single crystal grows. The hydrogen ensures that no crystal defects form in the crystal or that foreign atoms cannot become embedded at the respective growth site. The incorporation of unwanted foreign atoms regularly leads to a change in electrical conductivity, which can also occur locally and can be detrimental as a disturbance or a reduction in quality. The use of the reactive gas can also influence the process gas composition through reactions with other process gases or the hot zone (graphite components).The changed process gas composition can in turn influence the crystallinity, structure, crystal defects and doping of the SiC crystal.
[0050] For example, it has been shown that advantageous effects are achieved with a hydrogen content of 5% or more in the process gas, whereby at such low concentrations of less than 5% hydrogen in the process gas, protective measures, for example, for explosion protection, are typically not necessary. Particularly advantageous results were obtained in the range between 5% hydrogen content and approximately 40% hydrogen content, whereby an increased degree of crystal purity could be achieved in the range of 15% hydrogen content in the process gas (in particular ±5%). In principle, however, the use of a containment vessel according to the invention is also advantageous at low concentrations.
[0051] However, as described in the introduction, the use of a reactive gas such as hydrogen is problematic because in the event of a potential rupture of the wall of the process chamber 4, the reactive gas mixes with the ambient air - without the safety container according to the invention - so that, for example, an ignitable gas mixture can arise which would immediately ignite on the hot parts of the apparatus.
[0052] The process chamber 4 of the embodiment shown here is therefore surrounded by a containment vessel 8, which comprises a cylindrical vessel wall 9 surrounding the cylindrical wall of the process chamber 4, which vessel wall stands on a floor 10 and is closed at the top by a ceiling 11. The floor 10 and ceiling 11 of the containment vessel 8 adjoin the floor and ceiling of the process chamber 4.
[0053] The containment vessel 8 can simultaneously be part of the cooling concept of the apparatus. In other words, the containment vessel 8 can be integrated into the cooling concept of the apparatus. For this purpose, the cylindrical vessel wall 9 can be provided with cooling channels that are connected to a cooling system. The cooling concept can therefore provide for the containment vessel 8 to provide a cooling function for the apparatus. For example, a cooling medium, such as water, can circulate through the containment vessel 8. Alternatively, it can be provided that the containment atmosphere in the containment vessel 8 provides the cooling function. For example, the containment atmosphere can be circulated for this purpose in order to dissipate heat.Overall, the containment vessel can be equipped in such a way that the containment vessel, with its cooling function, can be used to regulate the temperature of the process conditions, ensuring that constant temperatures—or a similar temperature range—can be maintained at all times, regardless of potentially highly fluctuating ambient conditions. For example, the environment may include a daily temperature curve or seasonal temperature fluctuations, or may also be influenced by thermal processes taking place nearby.
[0054] Finally, the containment vessel 8 can be constructed in such a way that it is equipped with a conductive metal layer. The conductive metal layer can provide shielding for the process taking place inside, similar to a Faraday cage, so that, for example, alternating electromagnetic fields in the vessel wall 9 of the containment vessel 8 reach a defined end point and do not decay asymptotically, potentially to infinity. This can be advantageous if several devices are to be installed next to one another, whereby corresponding alternating fields can influence each other and mutually disrupt the process conditions. In other words, the conductive metal layer can ensure uniform process conditions even under the condition that several devices, possibly even different types, can be installed close to one another without the processes mutually disrupting each other.
[0055] Overall, it can be seen that the containment vessel 8 is capable of solving several tasks in a synergistic manner. Not only is it capable of providing the aforementioned protective atmosphere, which enables the use of a reactive gas in the process chamber, but the containment vessel 8 is also capable of shielding the process chamber from various environmental conditions such as temperature fluctuations or fluctuating electrical and / or magnetic fields, thus ensuring uniform process conditions for the process taking place in the process chamber.
[0056] In the bottom of the containment vessel 8 there is a ring line with one or more connections at an annular space 12 between the vessel wall 9 of the containment vessel 8 and the cylindrical wall of the process chamber 4 made of quartz glass. The ring line is connected to an argon source 14 and to a nitrogen source 15 via a shuttle valve 13.
[0057] A closable outlet valve 16 is located in the ceiling 11 of the containment vessel 8. A gas sensor 17 (particularly a hydrogen sensor) and a pressure sensor 18 are also provided there. A hood 20 made of a shatter-resistant plastic or sheet metal can be placed over the entire apparatus and rests on the floor of the containment vessel 8.
[0058] Furthermore, a control device 19 is provided, which is signal-connected to both sensors 17, 18 and controls the shuttle valve 13, the outlet valve 16 and the inlet valve 5 for the hydrogen supply via control lines.
[0059] The control device 19 allows the following processes to be carried out: Filling the safety container 8 with an inert gas before the process chamber 4 is filled with hydrogen: (1) The outlet valve 16 is opened. (2) The shuttle valve 13 is switched so that argon gas from the argon source 14 slowly flows into the intermediate space 12 from below, so that the intermediate space 12 is filled with argon gas from below, with the existing air being displaced through the open outlet valve 16 (or pressure relief valve or the like). (3) The outlet valve 16 and the shuttle valve 13 are closed. (4) A filling pause is observed so that any remaining air residue can settle upwards from the argon gas. (5) If necessary, repeat steps (1) to (3) once or several times. (6) Open the outlet valve 16. (7) Switch the shuttle valve 13 so that nitrogen gas slowly flows into the intermediate space 12 from below, filling the intermediate space 12 from below with the nitrogen gas from the nitrogen source 15, and displacing the existing argon gas through the open outlet valve 16. (8) Close the outlet valve 16.(9) Setting and maintaining an overpressure in the intermediate space 12 by controlled opening of the shuttle valve 13, so that despite existing and accepted leaks in the containment vessel, no air can flow into the intermediate space 12.
[0060] A sufficient overpressure is approximately 2 mbar above ambient.
[0061] In any case, steps (1) to (3) and (9) must be performed. Steps (4) and (6) to (8) are optional.
[0062] In order to be able to check whether the intermediate space 12 is sufficiently free of oxygen, an oxygen sensor can also be provided.
[0063] Behavior in case of a glass wall breakage during operation: (1) Continuous monitoring of the gas sensor 17 and (2) closing the hydrogen supply when the gas sensor 17 detects hydrogen in the gap 12.
[0064] With reference to the Figure 2A perspective view of a simplified embodiment of a partially assembled safety container 8 is shown, whereby for reasons of clarity, attachments and the process chamber 4 are not shown. Furthermore, for the sake of completeness, it should be noted that the Figure 2 The embodiment shown does not include any details for sealing the interior area 12, so that the leak rates achievable with this embodiment are comparatively high. Improved sealed containment containers 8 are presented in the embodiments of the other figures.
[0065] In Fig. 2A temperature control device 21 is arranged, at least partially, in the containment vessel 8, wherein a fluid can be fed into a coolant line 22 through connecting pieces 23. The coolant line 22 can be connected to the inner wall 44 of the containment vessel 8, for example, glued, soldered, welded, or screwed there. From the process chamber 4, heat output reaches the inner wall 44 predominantly as radiant heat, from where the heat output can be efficiently dissipated by means of the temperature control device 21. For example, liquid water can be used as the coolant. The amount of heat that can be dissipated by means of the temperature control device 21 can preferably be adjustable. For example, the amount of heat that can be dissipated can be influenced by the temperature setting for the coolant and / or the flow rate or speed, thus providing temperature control.Then, in response to sensor signals measuring the ambient temperature and / or the process temperature, the temperature control can be used to control the temperature of the process chamber 4, so that a substantially constant temperature is present in the process chamber 4 during the process sequence.
[0066] The containment vessel 8 has sight glasses 32 that bridge the interior area 12 and allow a view of the process chamber 4, for example for the purpose of process monitoring. In order to keep the direct heat radiation low, the sight glasses 32 are designed to be relatively small. Furthermore, Fig. 4 a detail of the refrigerant line 22 with line fastening 22A, connection piece 23, transition piece 23B and connection piece fastening 23A can be seen.
[0067] Fig. 3shows a sectional view of an embodiment of an apparatus 100. A process chamber 4 is partially surrounded by an induction coil 7, which is supplied with electrical power by a heating device 6. The heating device 6 is arranged partially inside and outside the containment vessel 8; for example, the power electronics can be arranged outside, so that a sealed feedthrough 62 is provided to reduce gas leaks. The induction coil 7 with parts of the electronics is located in the interior 12, i.e., in the space occupied by the containment atmosphere.
[0068] The shielding gas can be supplied through the shielding gas supply 54 on the underside of the interior 12 (several shielding gas supplies 54 may be provided if necessary). The outlet valve 16 is arranged on the top side 11, by means of which, for example, the outside air (containing oxygen) initially arranged in the protective container 8 can be released from the protective container 8, for example by admitting a shielding gas that is heavier than air. Subsequently, if a connecting line is connected to the outlet valve 16 (not shown), circulation of the shielding gas can also be provided, for example to dissipate heat from the protective container 8 or to ensure regular exchange of the shielding gas.
[0069] The coolant line 22 of the temperature control device 21 is arranged in the case shown here in the container wall 9, which is double-walled. Fig. 3In the cross-section of the containment vessel 8 with process chamber 4 shown, the interior space 12 of the containment vessel 8 for accommodating the protective atmosphere extends from the chamber wall 41 and, for example, around the process chamber 4 to the vessel wall 9, wherein the interior space 12 is sealed against the vessel wall 9 in order to keep the gas leakage rate from the interior space 12 into the environment 30 low.
[0070] Furthermore, the Fig. 3 The embodiment shown has a special feature in that the process chamber 4 is equipped with an adapter 46. In the embodiment shown, the adapter 46 has two alternative upper covers 47, 48, so that, depending on the desired process height, the upper cover 47 or the further inner upper cover 48 can be used. The covers 47, 48 can thus be used alternatively to one another if necessary.
[0071] Referring to Fig. 5, a first segment 91 of the container wall 9 of a segmented safety container 8 with a temperature control device 21 is shown, wherein the coolant line 22 is arranged in an intermediate region 122 in the container wall 9. In the case shown here, the container wall 9 comprises an inner wall 98, frame parts 92, 94, and the coolant line 22 of the temperature control device 21, which is arranged in an intermediate region 122. Frame parts 92, 94 are fastened to the first segment 91 with fastening means 97. Further fastening means 96 (e.g., screw holes) are arranged at regular intervals on the frame parts 92, 94, so that the intermediate region 122 is enclosed thereby.
[0072] Referring to Fig. 6A further embodiment of the first segment 91 with a sandwich structure is further illustrated. The coolant line 22 of the temperature control device 21 is arranged on the inner wall 98 and can be connected to the outside by means of connections 23. A frame 92, 94 surrounds or delimits the segment 91 all the way around, with an outer cover 99 being screwable onto the frame 92, 94. The outer cover 99 covers the coolant line 22 and the fastening means 97, thus protecting them from access on the one hand and from improper damage on the other. The outer cover 99 thus conceals the technical installations from direct view and access and gives the apparatus 100 an attractive appearance.
[0073] Fig. 7 Finally, an apparatus 100 is shown, mounted on the base 10, with a multi-part container wall 9, which comprises wall sections 91 and 91A. The coolant lines 22 (cf. e.g. Fig. 5 or 6) run protected behind the outer cover 99 and are connected to each other by means of compensating bends 24, so that a coolant - e.g. water - can flow through the temperature control device 21. The process chamber 4 (cf. e.g. Fig. 1 or 3 ) is surrounded on all sides by the safety atmosphere—or, depending on the design, at least above the floor 10, by the safety atmosphere. Should the process chamber 4 burst or otherwise fail and process gas escape, the process gas mixes with the protective gas stored in the interior 12 to form a harmless mixed gas.
[0074] It will be apparent to those skilled in the art that the embodiments described above are to be understood as examples and that the invention is not limited to them, but can be varied in many ways without departing from the scope of the claims. Furthermore, it is clear that the features, regardless of whether they are disclosed in the description, the claims, the figures or otherwise, also individually define essential components of the invention, even if they are described together with other features. In all figures, the same reference numerals represent the same objects, so that descriptions of objects that may only be mentioned in one or at least not with regard to all figures can also be transferred to these figures and exemplary embodiments with regard to which the object is not explicitly described in the description. List of reference symbols
[0075] 1Growth cell 2Source material 3Nucleus 4Process chamber 5Inlet valve 6Heating device 7Induction coil 8Containment vessel 9Vessel wall 10Floor 11Ceiling 12Intermediate space 13Shuttle valve 14Argon source 15Nitrogen source 16Outlet (valve) 17Gas sensor 18Pressure sensor 19Control device 20Hood 21Cooling or temperature control device 22Coolant line 22ALine fastening 23Connection piece 23AConnection holder 23BElbow 24Compensation bend 30Ambient 32Sight glass 41Process chamber wall 44Inner wall of the containment vessel 46Adapter 47Top cover of the process chamber 48Top cover of the process chamber 51Process gas supply 52Process gas discharge 54Protective gas supply 62Sealed feedthrough 91Section of the vessel wall 91AFurther section of the vessel wall 92Frame part 94Frame part 96Fastening element 97Fastening element 98Inner wall 99Outer panel 100Apparatus 122Intermediate area
Claims
1. PVT method for the process-safe production of single crystals in an apparatus which has a highly heatable growth cell (1), a process chamber (4) in which the growth cell (1) is located and a heating device (6) surrounding the process chamber (4) for heating the growth cell (1), wherein a swelling material (2) and a seed (3) being introduced into the growth cell (1), the process chamber (4) being filled with a process gas and the growth cell (1) being heated, so that the source material (2) is sublimated and resublimated at the seed (3), characterised in that the process gas consists partly or completely of a reactive gas and in that the process chamber (4) is arranged in a containment vessel (8), an intermediate chamber (12) between a container wall (9) of the containment vessel (8) and the process chamber (4) being flooded with a protective atmosphere in order to displace the air present therein before the sublimation of the source material (2) is initiated.
2. The PVT process according to claim 1, characterised in that the reactive gas comprises or consists of hydrogen, and / or in that the protective atmosphere comprises or consists of an inert gas.
3. PVT process according to claim 1 or 2, characterised in that the containment vessel (8) is constructed in such a way that it allows gas losses to the outside, and that inert gas is supplied to compensate for gas losses and to maintain an overpressure in the containment vessel (8).
4. PVT process according to claim 3, characterised in that, for flooding the containment vessel (8), a first inert gas which is heavier than air is admitted into its lower region, the air being displaced upwards, for which purpose a closable outlet at the upper end of the containment vessel (8) remains open until the air has escaped.
5. PVT process according to claim 4, characterised in that the first inert gas is argon.
6. PVT process according to claim 4 or 5, characterised in that after the containment vessel (8) has been flooded once or several times with the first inert gas, it is replaced by a second inert gas, for example nitrogen.
7. PVT process according to one of the preceding claims, characterised in that the containment vessel (8) has a gas sensor (17) which is capable of detecting the reactive gas, and in that the process gas supply to the process chamber (4) is interrupted when the gas sensor (17) detects the reactive gas in the containment vessel (8).
8. Apparatus for the process-safe production of single crystals by the PVT method, which apparatus has a highly heatable growth cell (1) for receiving a source material (2) and a seed (3), a process chamber (4) in which the growth cell (1) is located and which has a connection to a process gas source for filling it with a process gas, and a heating device (6) for heating the growth cell (1), characterised in that the apparatus has a containment vessel (8) which has a container wall (9) and in which the process chamber (4) is arranged, and in that the containment vessel (8) has a connection to a protective gas source (14, 15) in order to be able to flood an intermediate chamber (12) between the container wall (9) of the containment vessel (8) and the process chamber (4) with a protective atmosphere before the PVT process is carried out.
9. Apparatus according to claim 8, characterised in that the containment vessel (8) is constructed in such a way that it allows gas losses to the outside, that it has a pressure sensor (18) and that the pressure sensor (18) is signal-connected to a control device (19), the control device (19) being designed in such a way that an overpressure in the containment vessel (8) is set on the basis of the pressure sensor signals.
10. Apparatus according to claim 8 or 9, characterised in that, with respect to the intended installation of the apparatus, an inert gas connection is located in the lower region of the containment vessel (8) and a closable outlet is located in its upper region.
11. Apparatus according to one of claims 8 to 10, characterised in that the containment vessel has two inert gas connections for two different inert gases.
12. Apparatus according to any one of claims 8 to 11, characterised in that the containment vessel (8) comprises a gas sensor (17) which responds to a reactive gas.
13. Apparatus according to any one of claims 8 to 12, characterised in that the growth cell (1) is equipped with a silicon carbide as source material (2) and the process chamber (4) is flooded with hydrogen as reactive gas.