Cable that has a thermochromic polymer mesh layer

DE602014091224T2Active Publication Date: 2024-11-27NEXANS SA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602014091224
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2013-07-29
Filing Date
2014-07-10
Publication Date
2024-11-27
Estimated Expiration
2034-07-10

AI Technical Summary

Technical Problem

Existing temperature detection systems in electrical cables are not optimized, often deteriorating the mechanical and electrical properties of cables and can melt at high temperatures, making them ineffective for detecting abnormal heat rises.

Method used

An energy and telecommunications cable with a crosslinked polymer layer containing a thermochromic agent that irreversibly changes color at a temperature higher than the crosslinking temperature, allowing for visual detection of malfunctions without damaging the cable's mechanical or electrical properties.

Benefits of technology

The solution enables the preservation of cable properties during temperature rises, allowing for visual identification of abnormalities through color change without causing electrical losses or mechanical damage, with the thermochromic agent changing color at a temperature significantly higher than the cable's operating temperature.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to an energy and / or telecommunications cable comprising a thermochromic crosslinked polymer layer, and to a method of manufacturing said layer.

[0002] In the field of cabling, it is known to use thermochromic compositions to detect malfunctions in electrical cables, particularly those linked to overheating of the cables.

[0003] By way of example, mention may be made of document FR-2 967 258 which describes a device for detecting a rise in temperature comprising a thermochromic element capable of irreversibly changing color under the action of heat. This thermochromic element may be of the extruded rod type obtained from a polymer composition comprising an organic polymer and a thermochromic agent, this rod being independent of the cable with which it is associated.

[0004] However, the implementation of this type of device as well as its size once associated with one or more cables are not optimized. In addition, when the temperature rises too high in the vicinity of said rod, the latter can melt, resulting in its unusability.

[0005] International application WO 02 / 27733 A1 discloses an insulating material for insulating a conductor, comprising an indicator contained in the insulating material, said indicator changing optically as a function of temperature. This international application further relates to a conductor which is insulated with such an insulating material.

[0006] The aim of the present invention is to overcome the drawbacks of the techniques of the prior art by proposing in particular a cable incorporating a device for detecting a rise in temperature, which is easy to implement and which does not deteriorate the mechanical and / or electrical properties of the cable during an abnormal rise in temperature.

[0007] The present invention relates to an energy and / or telecommunications cable comprising an elongated conductive element, characterized in that the elongated conductive element is surrounded by at least one crosslinked polymer layer obtained from a crosslinkable polymer composition comprising a polymer and a thermochromic agent capable of irreversibly changing color at a reaction temperature T at under the action of a temperature increase. More particularly, said reaction temperature T at is higher than the crosslinking temperature T r of the polymer composition.

[0008] The thermochromic crosslinked layer of the invention advantageously makes it possible to preserve the mechanical and / or electrical properties of the cable during a temperature rise while making it possible to visually detect a malfunction of the cable. The thermochromic crosslinked layer of the cable of the invention thus makes it possible to detect a temperature rise, in particular to visually detect an abnormal temperature rise within the cable and / or in the cable's environment.

[0009] More particularly, the crosslinked polymer layer of the cable of the invention is a layer capable of changing color at a temperature higher than the operating temperature T of the cable.

[0010] The operating temperature T of the cable can be defined by the temperature supported by the cable, said temperature being mainly a function of the heat released by the Joule effect when the cable is in operational configuration, and / or the temperature relative to the cable's environment.

[0011] At this temperature T, the elongated conductive element, like the layer(s) surrounding said elongated conductive element (and like any other constituent element of the cable), undergoes substantially no damage likely to cause electrical losses or affect the mechanical properties of the cable.

[0012] For example, the operating temperature T of the cable is equal to 90°C for U1000 R2V type cables according to standard NF C 32-321; or 70°C for HO7V-U type cables according to standard NF C 32-201-3. Sometimes the operating temperature T of the cable can reach 120°C, or even 145°C for silicone-insulated industrial cables.

[0013] When the cable operates abnormally, for example during an electrical problem causing an abnormal rise in the operating temperature of the cable and / or during an abnormal rise in the temperature relative to the cable's environment, the temperature of the cable thus exceeds said temperature T: the temperature of the cable then becomes higher than the temperature T supported by the cable in operational configuration. The cable will thus overheat and the constituent elements of the cable may then suffer the damage mentioned above.

[0014] Thanks to the invention, this abnormal operation of the cable will be reflected by an irreversible change in color of the thermochromic element, which can thus be easily identified visually, without causing any degradation of the mechanical and / or electrical properties of the crosslinked polymer layer.

[0015] The reaction temperature T at of the thermochromic agent is the minimum temperature from which a color change occurs visually.

[0016] The reaction temperature T at of the thermochromic agent may be at least 15°C higher than the crosslinking temperature T r , and preferably at least 20°C higher than the crosslinking temperature T r .

[0017] According to a preferred embodiment, the reaction temperature T at of the thermochromic agent may be higher than the melting temperature T f or the glass transition temperature T g of the polymer. More particularly, the reaction temperature T at of the thermochromic agent may be at least 15°C higher than the melting temperature T f or the glass transition temperature T g of the polymer, and preferably at least 20°C higher than the melting temperature T f or the glass transition temperature T g of the polymer.

[0018] According to a preferred embodiment, the crosslinked polymer layer may be a layer extending continuously along the cable of the invention. It may more particularly be an extruded layer. More particularly, the reaction temperature T at of the thermochromic agent may be higher than the extrusion temperature T e of the polymer composition. In particular, the reaction temperature T at of the thermochromic agent may be at least 15°C higher than the extrusion temperature T e of the polymer composition, and preferably at least 20°C higher than the extrusion temperature T e of the polymer composition.

[0019] Thermochromic agents are well known to those skilled in the art and can be of any nature provided that they satisfy the object of the present invention.

[0020] For example, thermochromic agents can be chosen from so-called “Leuco dyes” and polydiacetylene dyes, or a mixture thereof.

[0021] A "Leuco dye" is a pigment whose molecules can have two forms, one being colorless and the other being colored. Typically, the molecular structure can be a spirolactone, such as "crystal violet lactone" which changes from colorless to intense blue under the action of temperature. Leuco dyes are reversible, so they are typically combined with a Lewis acid which stabilizes the colored form and makes the color change irreversible.

[0022] Polyacetylenes, also called polyethylene, are molecules that change color by changing their molecular configuration.

[0023] Polyacetylenes have irreversible color changes when they are in the sodium salt form, for example. In this example, the color changes irreversibly from red to blue between 55 and 65°C, then reversibly from blue to red between 70 and 100°C, then irreversibly from red to orange above 130°C. They are preferably used when you want to identify a color change at a temperature above 70°C, preferably above 90°C.

[0024] Examples of thermochromic agents include agents marketed by the company Colour-Therm, such as: the compound referenced “C” changing from black to red when the temperature is above 90°C, or the compound referenced “CT 115” changing from pink to purple when the temperature is above 120°C.

[0025] The crosslinkable polymer composition comprises at least 5% by weight of thermochromic agent.

[0026] It may further comprise less than 50% by weight of thermochromic agent, and preferably less than 20% by weight of thermochromic agent.

[0027] The polymer(s) of the invention, of the inorganic or organic type, may be homo- or co-polymers having thermoplastic and / or elastomeric properties.

[0028] Inorganic polymers can be of the polyorganosiloxane type.

[0029] Organic polymers can be of the olefin polymer type, or in other words polyolefin. More specifically, olefin polymer is a polymer of ethylene or propylene. Examples of ethylene polymers include linear low density polyethylene (LLDPE), low density polyethylene (LDPE), medium density polyethylene (MDPE), high density polyethylene (HDPE), ethylene vinyl acetate copolymers (EVA), ethylene butyl acrylate copolymers (EBA), methyl acrylate copolymers (EMA), 2-hexylethyl acrylate copolymers (2HEA), ethylene alpha olefin copolymers such as, for example, polyethylene octene (PEO), ethylene propylene copolymers (EPR), or ethylene propylene terpolymers (EPT) such as, for example, ethylene propylene diene monomer terpolymers (EPDM).

[0030] Polymers with a melting temperature T f or glass transition temperature T g , in the order of 70-90°C are preferred.

[0031] The crosslinkable polymer composition comprises at least 50% by weight of polymer, and preferably at least 80% by weight of polymer.

[0032] In a particular embodiment, the crosslinkable polymer composition may comprise at least 90% by weight of polymer(s) associated with the thermochromic agent.

[0033] The crosslinkable polymer composition may further comprise a colorant. Said colorant advantageously makes it possible to better visually highlight the color change of the thermochromic agent in the composition, in particular when the polymer used is transparent.

[0034] The coloring agent may be any type of pigment well known to those skilled in the art, added pure or in masterbatch in the composition of the invention. By way of example, mention may be made, as coloring agent, of titanium dioxide (TiO 2 ), red, yellow or orange iron oxides, carbon black, green chromium oxides.

[0035] For example, the amount of colorant in the crosslinkable polymer composition may be at most 5 parts by weight per 100 parts of polymer.

[0036] In the present invention, the term "crosslinked" means a gel content, according to ASTM D2765-01, of at least 40%, preferably at least 50%, preferably at least 60%, and particularly preferably at least 70%.

[0037] The crosslinking of the polymer composition, or more particularly of the polymer of the composition, can be carried out by any techniques well known to those skilled in the art, such as for example silane crosslinking, peroxide crosslinking, crosslinking by actinic radiation (e.g. ultraviolet), or crosslinking by electron bombardment.

[0038] For example, when the crosslinking is carried out by silane, the crosslinkable polymer composition may further comprise a silane compound and a generator of free radicals under the action of heat.

[0039] The silane compound, well known to those skilled in the art, may comprise at least one unsaturated function and at least one hydrolyzable group, preferably two hydrolyzable groups (identical or different), and particularly preferably three hydrolyzable groups (identical or different).

[0040] The hydrolyzable groups of the polymer of the invention may be alkoxysilane groups and / or carboxysilane groups, preferably alkoxysilane groups.

[0041] Examples of alkoxysilanes include vinyl trimethoxy silane, vinyltriethoxy silane, or vinyl tris(2-methoxyethoxy) silane.

[0042] The compound generating free radicals under the action of heat is intended to initiate the grafting reaction of the silane compound on the polymer and thus to graft the silane to said polymer.

[0043] The free radical generating compound may be selected from tert-butyl peroxybenzoate, 2,5-dimethyl-2,5-di(tert-butylperoxy)-3-hexyne, 2,5-dimethyl-2,5-di(tert-butylperoxy)-hexane, di-tert-butylperoxide, di(2-tert-butylperoxypropyl-(2))-benzene, O0-tert-Butyl O-2-(ethylhexyl) monoperoxycarbonate, and dicumyl peroxide, or a mixture thereof.

[0044] The polymeric composition of the invention may also comprise additives and / or fillers well known to those skilled in the art, these additives and / or these fillers making it possible, for example, to assist in the processing of the polymers, or to improve their mechanical properties, their reaction to fire, their stability to UV, their aging properties, etc.

[0045] The term "energy and / or telecommunications cable" means any electrical and / or optical cable intended for the transport of energy and / or the transmission of data. More particularly, this type of cable may comprise one or more electrical and / or optical conductor(s) (i.e. elongated conductive element(s)) surrounded by at least one crosslinked polymer layer in accordance with the invention. The crosslinked polymer layer may be an electrically insulating layer in contact or not with the electrical and / or optical conductor(s) making up the cable. It may also be a protective sheath surrounding one or more electrically insulated electrical and / or optical conductor(s).

[0046] The crosslinked layer of the invention may thus be any type of layer in a cable, extending along the elongated conductive element and surrounding said elongated conductive element. For example, it may be: an electrically insulating layer directly in physical contact with the elongated conductive element, or a layer surrounding an electrically insulating layer: in this case, the cable of the invention may further comprise an electrically insulating layer (eg a layer comprising polyvinyl chloride (PVC)), the crosslinked polymer layer then surrounding said electrically insulating layer.

[0047] In a particularly preferred embodiment, the crosslinked polymer layer may be the outermost layer of the cable.

[0048] The crosslinked polymer layer may advantageously have a thickness of at most 1 millimeter.

[0049] Another subject of the invention relates to a method of manufacturing the crosslinked polymer layer according to any one of the preceding claims, characterized in that it comprises the following steps: i. extruding the crosslinkable polymer composition to form an extruded layer, and ii. crosslinking the extruded layer obtained in step i, steps i and ii being carried out at temperatures lower than the reaction temperature Tat of the thermochromic agent.

[0050] In a particular embodiment, when the crosslinking is of the silane crosslinking type, the method may comprise the following steps, prior to step i: a. grafting a silane compound to the polymer to obtain a silane-grafted polymer, and b. mixing the thermochromic agent with the silane-grafted polymer: the crosslinkable polymer composition then comprises a silane-grafted organic polymer as the polymer of the composition of the invention.

[0051] Steps a and b are carried out at temperatures below the reaction temperature T at of the thermochromic agent.

[0052] Other characteristics and advantages of the present invention will appear in the light of the examples which follow, said examples being given for illustrative purposes and in no way limiting. Example

[0053] A crosslinkable polymer composition according to the invention was prepared under the following conditions.

[0054] In a first step, a silane compound is grafted onto a polymer of the ethylene and vinyl acetate copolymer type in the quantities mentioned in Table 1 below. The quantities indicated in Table 1 are expressed in parts by weight per 100 parts by weight of polymer(s). Table 1 Quantity EVA 100 Silane and organic peroxide compound 2

[0055] The origin of the constituents in Table 1 is as follows: EVA is a copolymer of ethylene and vinyl acetate marketed by Exxon Mobil under the reference Escorene UL 0328; the melting temperature T f of this polymer is approximately 90°C; and Silane and organic peroxide compound is a crosslinking agent coupled with a free radical generator, marketed by Evonik under the reference Silfin 59, comprising 97% by weight of Trimethoxy(vinyl)silane (VTMO) and 3% by weight of dicumyl peroxide (DCP).

[0056] The grafting step is carried out in an internal mixer at a temperature of 150°C by mixing the EVA and the silane compound. Once cooled, the mixture was ground.

[0057] This produces a silane-grafted polymer (non-crosslinked).

[0058] In a second step, the silane-grafted organic polymer is mixed with a thermochromic agent and a colorant. The quantities are mentioned in Table 2 below, and are expressed in parts by weight per 100 parts by weight of polymer(s). Table 2 Quantity Silane grafted polymer 100 Irreversible thermochromic agent 11,1 Dye 1,1

[0059] The origin of the constituents in Table 2 is as follows: Silane grafted polymer is the organic polymer obtained in the first step described above; Irreversible thermochromic agent is an ink marketed by the company Brancher under the reference “Flexo 120”; this water-based ink was dried in ambient air (25°C) for 6 days in order to dehydrate it and thus facilitate its incorporation into the silane grafted polymer matrix; the reaction temperature T at of this ink is 120°C; Colorant is titanium dioxide (TiO 2 ).

[0060] The step of mixing the constituents of Table 2 is carried out using an internal mixer at a temperature of 90°C, then using a cylinder mixer at a temperature of 90°C. The cylinder mixer improves the dispersion of the thermochromic agent and the colorant in the silane-grafted polymer matrix.

[0061] In a third step, the mixture obtained in the second step described above is extruded using a single-screw extruder at a maximum temperature of 95°C. At the extruder outlet, a layer is formed around an electric cable of the HO7VU cable type (electrical conductive wire with a diameter of 1.38 millimeters, surrounded by a PVC layer).

[0062] Once the layer has been extruded around the electric cable, the latter is placed in a pool at 63°C for 24 hours to be cold crosslinked.

[0063] The cable thus formed is capable of irreversibly changing color at a temperature of approximately 120°C (from gray to purple).

Claims

1. An energy and / or telecommunications cable comprising an elongate conductive element, the cable being characterised in that the elongate conductive element is surrounded by at least one cross-linked polymer layer obtained from a cross-linkable polymer composition comprising a polymer and a thermochromic agent that is capable of irreversibly changing colour at a reaction temperature Tat under the action of an increase in temperature, and in that the cross-linkable polymer composition comprises at least 5% by weight of the said thermochromic agent.

2. A cable according to claim 1, characterised in that the reaction temperature Tat of the thermochromic agent is higher than the cross-linking temperature Tr.

3. A cable according to any one of the preceding claims, characterised in that the reaction temperature Tat of the thermochromic agent is higher than the melting temperature Tf or the glass transition temperature Tg of the polymer.

4. A cable according to claim 3, characterised in that the reaction temperature Tat of the thermochromic agent is higher by at least 15°C than the melting temperature Tf or the glass transition temperature Tg of the polymer, and preferably higher by at least 20°C than the melting temperature Tf or the glass transition temperature Tg of the polymer.

5. A cable according to any one of the preceding claims, characterised in that the cross-linked polymer layer extends continuously along the length of the cable.

6. A cable according to any one of the preceding claims, characterised in that the cross-linked polymer layer is an extruded layer.

7. A cable according to claim 6, characterised in that the reaction temperature Tat of the thermochromic agent is higher than the extrusion temperature Te of the polymer composition.

8. A cable according to claim 7, characterised in that the reaction temperature Tat of the thermochromic agent is higher by at least 15°C than the extrusion temperature Te of the polymer composition, and preferably higher by at least 20°C than the extrusion temperature Te of the polymer composition.

9. A cable according to any one of the preceding claims, characterised in that the cross-linkable polymer composition comprises less than 50% by weight of the thermochromic agent.

10. A cable according to any one of the preceding claims, characterised in that the cross-linkable polymer composition comprises at least 50% by weight of the polymer, and preferably at least 80% by weight of the polymer.

11. A cable according to any one of the preceding claims, characterised in that the polymer is an olefin polymer.

12. A cable according to any one of the preceding claims, characterised in that the polymer is a copolymer of ethylene and vinyl acetate (EVA).

13. A cable according to any one of the preceding claims, characterised in that the cross-linked polymer layer is the outermost layer of the cable.

14. A cable according to any one of the preceding claims, characterised in that the reaction temperature Tat of the thermochromic agent is at least 15°C higher than the cross-linking temperature Tr.

15. A manufacturing method for manufacturing the cross-linked polymer layer according to any one of the preceding claims, characterised in that it comprises the following steps: i. extruding the cross-linkable polymer composition in order to form an extruded layer; and ii. cross-linking the extruded layer obtained in step i, the steps i and ii being carried out at temperatures that are lower than the reaction temperature Tat of the thermochromic agent.