Soundproofing panel for cladding a wall of a motor vehicle
Patent Information
- Application Number
- DE602017086082
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2016-07-01
- Filing Date
- 2017-03-09
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2037-03-09
AI Technical Summary
Existing acoustic protection panels for vehicles face challenges in reducing weight while maintaining sound absorption properties and air resistance, as adding heavy particles to minimize foam flakes density degrades air resistance and absorption performance.
The use of a binding agent based on two-component fibers, where the sheath is fusible at a lower temperature and the core is not, allows for a lightweight upper layer with enhanced air resistance and sound absorption by creating a network that hinders air passage without degrading insulation performance.
This approach enables a reduction in the surface mass of the upper layer while maintaining its resistance to air passage and sound absorption properties, effectively reducing costs without compromising acoustic insulation.
Description
[0001] The invention relates to an acoustic protection panel intended to cover a wall of a motor vehicle and methods for producing such a panel.
[0002] It is known from document JP-H08 / 282402 to produce an acoustic protection panel intended to cover a wall of a motor vehicle, said panel comprising, in particular so as to form a mass-spring system: a spring layer made of elastically compressible foam flakes (felt layer), intended to be turned towards the wall, a mass layer based on polyvinyl chloride (PVC).
[0003] It is also known, in particular from document EP2549474, to produce such an acoustic protection panel comprising: a lower layer of spring based on elastically compressible material, said layer being intended to be turned towards said wall, an upper layer of mass based on elastically compressible foam flakes, said flakes being bound together by a binding agent.
[0004] Advantageously, a mass-spring system requires the presence of a sealing layer between the upper and lower layers.
[0005] Such a system allows for acoustic insulation which is all the more pronounced as the upper layer has a high surface mass.
[0006] Furthermore, due to its porous nature, the upper layer allows for acoustic protection also through absorption, which gives the panel enhanced acoustic protection properties.
[0007] It is particularly known to use a bonding agent in the form of a resin introduced in liquid form to then be solidified, said resin being for example based on polyurethane.
[0008] However, the use of such a type of binder has various disadvantages explained below.
[0009] In the case of an upper layer implemented in a panel for which the absorption function is favored over the insulation function, we seek to minimize the weight of said layer in order to lighten said panel.
[0010] To do this, we could consider reducing, at iso-thickness, the density of the upper layer, so as to lower its surface mass.
[0011] However, with this approach, the upper layer sees its resistance to the passage of air deteriorate, the said layer then no longer presenting the expected acoustic absorption properties.
[0012] One aim of the invention is therefore to propose a panel having a lightweight upper layer while retaining its resistance to the passage of air, and therefore its sound absorption properties.
[0013] In this case of an upper layer implemented in a panel for which the insulation and absorption functions must be treated with the same importance, it is known, from document EP2549474, to give said layer the expected surface mass by adding a dispersion of heavy particles within the flakes, said particles being for example based on thermoplastic elastomer, in particular ethylene propylene diene monomer, loaded with mineral filler.
[0014] The addition of heavy particles mentioned above makes it possible to achieve the expected surface mass without having to resort to an overload of flakes which would have the effect of significantly increasing the thickness of the upper layer, which may be incompatible with the space available in the vehicle.
[0015] As for the absorption performance of the panel, it depends on the resistance to the passage of air in the upper layer, good absorption being achieved by a relevant choice of said resistance.
[0016] In order to reduce the cost of such a panel without modifying the mass of the upper layer, so as to maintain its insulation performance, one could consider maximizing the mass percentage of heavy particles in said layer, said particles usually having a low cost, and consequently minimizing the mass percentage of foam flakes, which are more expensive.
[0017] This cost reduction must, however, be achieved without modifying the resistance to the passage of air in the upper layer, so as not to degrade the sound absorption performance of the panel.
[0018] It is known that the intrinsic density ratio between heavy particles and foam flakes is usually very high, the ratio [intrinsic density of particles / intrinsic density of flakes] being able to be for example of the order of 50.
[0019] It should be noted here that, throughout this description, when we speak of intrinsic density, we are considering the density of an isolated flake or particle, and not the apparent density of a cluster of flakes or particles.
[0020] Taking the above ratio value as an example, this means that the addition of one volume of heavy particles must be compensated by the removal of fifty volumes of foam flakes to maintain the mass of the top layer.
[0021] However, it is observed that the resistance to the passage of air in the upper layer is essentially linked to the relative volume of flakes compared to the volume of said upper layer, the relative volume of dense particles only having a marginal effect on this parameter.
[0022] Therefore, at the same surface mass, the slightest overdose of heavy particles results in a drastic reduction in the relative volume of flakes, which leads to a consequent reduction in the resistance to the passage of air in the upper layer, with the resulting degradation in absorption performance.
[0023] Ultimately, this approach does not allow for cost reduction while maintaining the air resistance of the top layer, and therefore the sound absorption properties of the panel.
[0024] Another aim of the invention is therefore to propose a lower cost panel, while retaining the surface mass and resistance to the passage of air of the upper layer.
[0025] To this end, the invention proposes an assembly comprising an acoustic protection panel and a motor vehicle wall covered by said panel, said panel comprising, in particular so as to form a mass-spring system: a lower layer of spring based on elastically compressible material, said layer facing said wall, an upper layer of mass based on elastically compressible foam flakes, said layer being arranged on the lower layer and opposite said wall, said layer being provided with a bonding agent for said flakes which is based on bi-component fibers comprising a core, said core being fusible at high temperature or infusible, and a sheath fusible at lower temperature, said flakes being bonded by melting said sheath so as to form an agglomerated upper layer.
[0026] It is specified here that, to achieve the fusion of the sheath, one places oneself above its fusion temperature and below the possible fusion temperature of the core, the latter remaining intact and allowing the agglomerated layer to be provided with a network of fibers.
[0027] The advantage of using a two-component fibre-based binding agent is that, compared to what is observed in the case of a resin introduced in liquid form and then solidified, all composition parameters being equal, the upper layer has increased resistance to the passage of air.
[0028] The applicant has in fact noted that the bi-component fibers create veils embedded in the upper layer.
[0029] According to the applicant, the sails would hinder the passage of air, which would result in the observed increase in resistance to the passage of air.
[0030] Therefore, it is possible to reduce the surface mass of the upper layer by using bi-component fibers instead of a traditional bonding agent, while maintaining the air resistance of the upper layer.
[0031] In the case of an agglomerated top layer containing dispersed heavy particles, the advantage of using a two-component fibre-based binding agent is still that, as explained above, the air resistance of the top layer is increased by using such fibres to replace traditional binders.
[0032] Based on this observation, in order not to modify the resistance to the passage of air in the upper layer following the substitution of the resin by the bi-component fibers, it is necessary to reduce the density of said layer so that it is less of an obstacle to the passage of air, which leads to a reduction in its surface mass.
[0033] But this results in a degradation of the insulation performance of the panel.
[0034] Knowing that, as we saw above, the relative volume of heavy particles only marginally affects the resistance to the passage of air in the upper layer, it is possible to enrich the composition of the upper layer with said particles to achieve the desired surface mass so that the panel performs well in terms of sound insulation.
[0035] Other features and advantages of the invention will appear in the following description, given with reference to the attached figures, in which: there figure 1 is a schematic view in partial section of a panel of an assembly according to a first embodiment, the figure 2 is a schematic view in partial section of a panel of an assembly according to a second embodiment, the figure 3 is a schematic view in partial section of a panel of an assembly according to a third embodiment, the figure 4 is a schematic sectional view of a binder fiber, the figure 5 represents the resistivity to the passage of air of two types of agglomerated layers based on elastically compressible foam flakes, said types of layers differing from each other only by the bonding agent used which is either in the form of resin (R) or in the form of bi-component fibers (T), said resistivity being measured on a plurality of samples of different densities, the figure 6 represents the acoustic absorption in diffuse field as a function of frequency, measured in Alpha cabin, produced by two samples each comprising a lower layer based on foam and an upper layer based on foam flakes bonded together by a bonding agent, said samples differing from each other only by the bonding agent used which is either in the form of resin (R) or in the form of two-component fibers (T).
[0036] With reference to the figures, an assembly is now described comprising an acoustic protection panel 1 and a motor vehicle wall covered by said panel, said panel comprising, in particular so as to form a mass-spring system: a lower layer 2 of spring based on elastically compressible material, said layer being turned towards said wall, an upper layer 3 of mass based on flakes 4 of elastically compressible foam, said layer being arranged on the lower layer 2 and opposite said wall, said layer being provided with a bonding agent for said flakes which is based on bi-component fibers 5 comprising a core 6, said core being fusible at high temperature or infusible, and a sheath 7 fusible at lower temperature, said flakes being bonded by melting said sheath so as to form an agglomerated upper layer 3.
[0037] According to a first embodiment represented in a particular embodiment in figure 1 , the lower layer 2 is based on elastically compressible foam flakes, said flakes being bonded together by a two-component fiber-based bonding agent 5 so as to form an agglomerated lower layer 2.
[0038] Indeed, surprisingly, the applicant observed that the use of a two-component fiber-based binder 5 makes it possible to achieve a very significant reduction in the density of the lower layer 2, compared to layers based on felt or elastically compressible foam, while retaining its effectiveness as a spring in a “mass-spring” type insulation system.
[0039] According to one embodiment, the lower layer 2 may have a variable thickness which may vary from 40 mm, partly uncompressed, to 5 mm, partly highly compressed.
[0040] In particular, it is possible to compress the lower layer 2, for example at the periphery of the panel 1 or depending on space constraints around said panel in the vehicle.
[0041] According to an embodiment related to this first embodiment, the lower layer 2 has, in the uncompressed part, a density of less than 0.25, and in particular less than 0.20, such a low density being able to be achieved thanks to the use of the bi-component fibers 5, and this without harming the performance of said layer as a spring.
[0042] According to an embodiment not shown, the lower layer 2 may be covered with a protective layer on at least one of its faces, this layer being able to be of the “Spun” polyester type of 20 to 30 g / m 2< or non-woven.
[0043] Such a protective layer can in particular facilitate the shaping of the lower layer 2, in particular during a preheating step, and also protect said layer during handling of the panel 1,
[0044] According to an embodiment related to this first embodiment, the lower layer 2 has a surface mass of less than 1000 g / m 2< , and in particular less than or equal to 800 g / m 2< , which is much lower than the surface masses usually known for spring layers with a thickness of up to 40 mm.
[0045] According to an embodiment related to this first embodiment, the fibers 5 occupy between 10 and 20% by weight of the lower layer 2, and in particular between 13 and 17%, and in particular of the order of 15%.
[0046] According to one embodiment, the upper layer 3 being agglomerated, a sealing layer 8 is arranged between said upper layer and the lower layer 2.
[0047] This creates a mass-spring system with absorption properties thanks to the porosity of the upper layer 3.
[0048] According to one embodiment, the sealing layer 8 is in the form of a thermoplastic film, in particular with a thickness of less than 200 microns.
[0049] According to an embodiment not shown, the upper layer 3 is arranged on the lower layer 2 without the interposition of a sealing layer, said upper layer having a resistance to the passage of air greater than that of said lower layer.
[0050] The corresponding panel 1 then provides acoustic protection which is no longer based on a mass-spring principle which requires that a sealing layer 8 be interposed between the upper layer 3 and the lower layer 2.
[0051] Acoustic protection is then based on a principle of “bi-porosity” favoring acoustic absorption to the detriment of the insulation achieved when using a mass-spring type acoustic protection principle.
[0052] A method of producing such a panel 1 is now described, said method comprising the following steps: providing an elastically compressible lower layer 2, said layer being based on a mixture of elastically compressible foam flakes 4 mixed with two-component fibers 5, said flakes being bonded together by melting the sheath of said fibers forming a binder, heating said lower layer and placing it in a mold so as to conform it to form a spring layer, associating with it an upper layer 3, forming the mass, associated or not with a sealing layer 8 arranged between said upper and lower layers.
[0053] According to a second embodiment, represented in a particular embodiment in figure 2 , the lower layer 2 not being able to be agglomerated, a sealing layer 8 is arranged between the upper layer 3 and said lower layer.
[0054] According to an embodiment not shown attached to this second embodiment, the sealing layer 8 is in the form of a thermoplastic film, in particular with a thickness of less than 200 microns.
[0055] According to the embodiment shown in figure 2 , the lower layer 2 is based on foam - in particular polyurethane - overmolding the upper layer 3, the sealing layer 8 being produced by penetration of said foam into a fraction of the thickness of said upper layer so as to form a waterproof crust.
[0056] According to the embodiment shown, the upper layer 3 is coated, on at least its internal face, with a first non-woven fabric 9, said non-woven fabric having in particular a surface mass of between 40 and 80 g / m 2 < .
[0057] The first non-woven fabric 9 makes it possible in particular to limit the penetration of the foam into the upper layer 3 so as to retain its porous character over as large a fraction as possible of its thickness, in order to preserve its absorption properties.
[0058] In the embodiment shown, the upper layer 3 is also coated, on its external face, with a second non-woven fabric 10, said non-woven fabric, having in particular a surface mass of between 40 and 60 g / m 2 < , which has in particular the function of preventing the upper layer 3 from sticking against a tool used to pre-compress and / or thermoform it.
[0059] According to an embodiment not shown attached to this second embodiment, the upper layer 3 is arranged on the lower layer 2, which can be agglomerated, without the interposition of a sealing layer, said upper layer having a resistance to the passage of air greater than that of said lower layer.
[0060] The corresponding panel 1 then provides acoustic protection which is no longer based on a mass-spring principle which requires that the upper layer 3 be waterproof or that a sealing layer 8 be interposed between said upper layer and the lower layer 2.
[0061] Acoustic protection is then based on a principle of “bi-porosity” favoring acoustic absorption to the detriment of the insulation achieved when using a mass-spring type acoustic protection principle.
[0062] We now describe, in this case of a sealing layer 8 resulting from partial penetration of the upper layer 3 by the foam of the lower layer 2, a method of producing a panel 1, said method comprising the following steps: pouring onto a support a mixture of foam flakes 4 and two-component fibers 5, so as to form an unbound mattress, covering said mattress with a first non-woven fabric 9, hot pre-compressing the assembly so as to form a pre-bound plate, thermoforming said plate so as to produce a three-dimensional upper layer 3, placing said layer in a mold and overmolding its face provided with said first non-woven fabric with elastically compressible foam so as to form a lower layer 2 whose foam partially penetrates said upper layer, creating a sealing layer 8, demolding the panel 1 obtained.
[0063] It is also possible to provide for a second non-woven fabric 10 to be placed on the mattress on the face of said mattress opposite that receiving the first non-woven fabric 9.
[0064] As can be seen on the figure 5 , the replacement of a bonding agent in the form of resin by an agent in the form of two-component fibers 5, all other parameters remaining unchanged, leads to a significant increase in the resistivity to the passage of air of the upper layer 3, regardless of its density.
[0065] It is specified here that it is the resistivity to the passage of air (Nsm -4< ) which is expressed, and not the resistance to the passage of air (Nsm -3< ), this to free oneself from the thickness of the samples, knowing that one or the other can be used indifferently to compare two samples of the same thickness.
[0066] We now carry out, with reference to the figure 6 , a comparison, over a frequency range, of the absorption coefficient in a diffuse field, measured in an Alpha cabin, of two samples each comprising a lower layer 2 based on foam and an upper layer 3 based on foam flakes bound together by a binding agent.
[0067] The samples are similar and differ only in the bonding agent which is in the form of resin for the first sample (R) and in the form of bi-component fibers as previously described for the second sample (T).
[0068] The two samples each have a total thickness of 25 mm, with the top layer 3 having a thickness of 8 mm for each of them.
[0069] For both samples, the lower layer 2 overmoulds the upper layer 3 so as to form a sealing layer 8 produced by penetration of said foam into a fraction of the thickness of said upper layer.
[0070] It is observed, over a frequency range extending from 800 to more than 8000 Hz, that the absorption coefficient of the second sample (T) is generally higher than that of the first sample (R), and this is more particularly the case for frequencies above 4000 Hz.
[0071] There figure 6 thus illustrates the fact that the use of a binding agent in the form of two-component fibers, instead of an agent in the form of resin, leads to an improvement in the absorption properties of the upper layer 3.
[0072] Such an improvement would be explained, as previously explained, by the fact that the bi-component fibers create veils embedded in the upper layer, said veils having the effect of increasing the resistivity, or resistance, to the passage of air, and therefore the absorption properties.
[0073] According to a third embodiment, represented in a particular embodiment in figure 3 , the upper layer 3 further comprises a dispersion of heavy particles 11 of intrinsic density greater than that of the flakes, said particles being bound with the flakes 4 by fusion of the sheath 7.
[0074] Heavy particles 11 may in particular come from the grinding of scraps from the production of automotive carpets.
[0075] As such, they may in particular be based on thermoplastic elastomer - in particular ethylene propylene diene monomer - loaded with mineral filler - for example baryte or calcium carbonate - and also contain dust from fibres from the surface of said carpets.
[0076] The intrinsic density of the particles 11 can notably be between 1 and 2.5.
[0077] In particular, particles 11 may have an intrinsic density 20 to 60 times greater than that of flakes 4.
[0078] The size of the heavy particles 11 may in particular be between 5 and 10 mm, in order to allow their optimal dispersion within the upper layer 3.
[0079] According to an embodiment related to this third embodiment, the mass percentage of heavy particles 11 is between 20 and 40% of the mass of the upper layer 3.
[0080] According to an embodiment related to this third embodiment, the mass percentage of the two-component fibers 5 is between 15 and 30% of the mass of the upper layer 3.
[0081] According to an embodiment related to this third embodiment, the mass percentage of the flakes 4 is between 40 and 65% of the mass of the upper layer 3.
[0082] As shown in the figure 3 , a sealing layer 8 is arranged between the upper layer 3 and the lower layer 2.
[0083] According to an embodiment not shown attached to this third embodiment, the sealing layer 8 is in the form of a thermoplastic film, in particular with a thickness of less than 200 microns.
[0084] According to an embodiment not shown attached to this third embodiment, the lower layer 2 is agglomerated.
[0085] According to the embodiment shown in figure 3 , the lower layer 2 is based on foam - in particular polyurethane - overmolding the upper layer 3, the sealing layer 8 being produced by penetration of said foam into a fraction of the thickness of said upper layer so as to form a waterproof crust.
[0086] According to the embodiment shown, the upper layer 3 is coated, on at least its internal face, with a first non-woven fabric 9, said non-woven fabric having in particular a surface mass of between 40 and 80 g / m 2 < .
[0087] The first non-woven fabric 9 makes it possible in particular to limit the penetration of the foam into the upper layer 3 so as to retain its porous character over as large a fraction as possible of its thickness, in order to preserve its absorption properties.
[0088] According to an embodiment not shown attached to this third embodiment, the upper layer 3 is arranged on a porous lower layer 2 without the interposition of a sealing layer, said upper layer having a resistance to the passage of air greater than that of said lower layer.
[0089] The corresponding panel 1 then provides acoustic protection which is no longer based on a mass-spring principle which requires that the upper layer 3 be waterproof or that a sealing layer 8 be interposed between said upper layer and the lower layer 2.
[0090] Acoustic protection is then based on a principle of "bi-porosity" favoring acoustic absorption to the detriment of the insulation achieved when we are in a principle of mass-spring type acoustic protection.
[0091] We now describe, in this case of a sealing layer 8 resulting from partial penetration of the upper layer 3 by the foam of the lower layer 2, a method of producing a panel 1, said method comprising the following steps: pouring onto a support a mixture of foam flakes 4, bi-component fibers 5 and heavy particles 11, so as to form an unbound mattress, covering said mattress with a first non-woven fabric 9, hot pre-compressing the assembly so as to form a pre-bound plate, thermoforming said plate so as to produce a three-dimensional upper layer 3, placing said layer in a mold and overmolding its face provided with said first non-woven fabric with elastically compressible foam so as to form a lower layer 2 whose foam partially penetrates said upper layer, creating a sealing layer 8, demolding the panel 1 obtained.
[0092] According to an embodiment related to all the embodiments presented above, the flakes 4 come from recycling.
[0093] According to an embodiment related to all the embodiments presented above, the flakes 4 are based on polyurethane.
[0094] According to an embodiment related to all the embodiments presented above, the size of the flakes 4 is between 5 and 15 mm, this in order to allow their optimal dispersion within the agglomerated layer.
[0095] According to an embodiment related to all the embodiments presented above, the bi-component fibers 5 are based on polyethylene terephthalate (PET).
[0096] In particular, the core 6 may be based on polyester and the sheath 7 based on co-polyester.
[0097] According to an embodiment related to all the embodiments presented above, the fibers 5 may have a count of between 1.7 and 6 dtex, and in particular of the order of 4.4 dtex, knowing that the use of fine fibers leads to an increase in the resistance to the passage of air, and therefore to an improvement in the absorption properties of the upper layer 3.
[0098] According to an embodiment related to all the embodiments presented above, already explained for the second embodiment, the upper layer 3 can be coated, on its external face, with a second non-woven fabric 10.
[0099] The second nonwoven 10 may in particular have a surface mass of between 40 and 60 g / m 2 < , having the function of preventing the upper layer 3 from sticking against a tool used to pre-compress and / or thermoform it.
[0100] According to an embodiment related to all the embodiments presented above, the second nonwoven 10 can have a resistance to the passage of air of between 200 and 1800 Nsm -1<, so as to be resistive.
[0101] The use of such a resistive nonwoven 10 allows the use of an upper layer 3 of minimized surface mass, for example of the order of 1000 g / m 2 < , the reduction in resistance to the passage of air of said layer resulting from the minimization of its surface mass being compensated by said nonwoven which contributes to increasing the resistance to the passage of air of the assembly.
[0102] According to an embodiment related to all the embodiments presented above, the percentage by mass of the bi-component fibers 5 in the upper layer 3 is between 15 and 30% of the mass of said layer, the additional mass being provided by the flakes 4 and possibly by the heavy particles 11, as explained above.
[0103] According to an embodiment related to all the embodiments presented above, the upper layer 3 has a Young's modulus, measured in a direction corresponding to the thickness of said layer, greater than 1 MPa.
[0104] According to an embodiment applicable to all the embodiments presented above, the upper layer 3 has a surface mass of between 0.7 and 5 kg / m 2 < .
Claims
1. Assembly comprising an acoustic protection panel (1) and a motor vehicle wall (12) covered by said panel, said panel comprising, in particular to form a spring mass system: • a lower spring layer (2) made from resiliently compressible material, said layer being turned towards said wall, • an upper mass layer (3) made from flakes (4) of resiliently compressible foam, said flakes being bonded together by a bonding agent, said layer being disposed on the lower layer (2) and opposite said wall, said assembly being characterised in that said bonding agent is made from bi-component fibres (5) comprising a core (6), said core being fusible at a high temperature or non-fusible, and a sheath (7) fusible at a lower temperature, said flakes being bonded by the fusion of said sheath so as to form an agglomerated upper layer (3).
2. Assembly according to claim 1, characterised in that the upper layer (3) is disposed on the lower layer (2) without the interposition of a sealing layer, said upper layer having a resistance to the passage of air which is greater than that of said lower layer.
3. Assembly according to claim 1, characterised in that a sealing layer (8) is arranged between the upper layer (3) and the lower layer (2).
4. Assembly according to claim 3, characterised in that the sealing layer (8) is in the form of a thermoplastic film, having a thickness of less than 200 microns.
5. Assembly according to claim 3, characterised in that the lower layer (2) is made from foam moulding over the upper layer (3), the sealing layer (8) being formed by the penetration of said foam in a portion of the thickness of said upper layer so as to form a sealing crust.
6. Assembly according to any of claims 1 to 4, characterised in that the lower layer (2) is made from resiliently compressible foam flakes, said flakes being bonded together by a bonding agent made from bi-component fibres (5) so as to form an agglomerated lower layer (2).
7. Assembly according to any of claims 1 to 6, characterised in that the upper layer (3) also comprises a dispersion of heavy particles (11) with an intrinsic density greater than that of the flakes (4), said particles being bonded to said flakes by the fusion of the sheath (7) .
8. Assembly according to claim 7, characterised in that the percentage by mass of heavy particles (11) is between 20 and 40% of the mass of the upper layer (3).
9. Assembly according to any of claims 1 to 8, characterised in that the percentage by mass of bi-component fibres (5) in the upper layer (3) is between 15 and 30% of the mass of said layer.