METHOD AND DEVICE FOR WELDING USING ELECTRODES WITH COAXIAL POWER SUPPLY

DE602017086539T2Active Publication Date: 2024-12-04SIEMENS ENERGY INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602017086539
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2017-06-27
Publication Date
2024-12-04
Estimated Expiration
2037-06-27

AI Technical Summary

Technical Problem

Welding of superalloys is challenging due to their high strength and low ductility, limiting the flexibility of weld filler metal wires in achieving various alloy compositions, as existing technologies require specific filler materials for each composition.

Method used

A novel electrode with a hollow metal or metal alloy sheath surrounded by a flux coating, where the sheath conducts welding current and melts to provide base material, while the hollow core delivers additional materials via a conduit to achieve desired superalloy compositions, allowing for flexibility in forming multiple types of deposits from a single electrode.

Benefits of technology

Enables the formation of a variety of superalloy compositions by adjusting the materials delivered through the electrode's core, increasing flexibility and reducing the need for multiple electrodes, while the flux coating provides shielding and protects the weld pool from atmospheric reactions.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The present disclosure relates generally to the field of materials technology, and more particularly to methods and apparatus of welding using electrodes with coaxial power feed.BACKGROUND

[0002] Welding of superalloys presents a variety of technical challenges because of the high strength (and corresponding low ductility) that these alloys are optimized to achieve. One challenge involves the weld filler metal wires, which are typically fabricated to provide a specific / particular alloy deposit, i.e., a desired deposit composition for a specific superalloy, for routine processing via arc welding (e.g., GTAW, PAW, GMAW etc.) or for beam (e.g., laser) processing with wire (e.g., LBW). Such specificity limits any flexibility of trying to achieve a variety of compositions of superalloy deposits. Prior art is disclosed by US35132288A, US1161366A and US4683368.SUMMARY

[0003] It should be appreciated that the present inventor has recognized the above limitations of prior art weld filler metal wires and electrodes, and now discloses a new electrode for use in a weld operation. The object is met by an apparatus of claim 1 and a method of claim 10. Preferred emodiments are disclosed in the dependent claims

[0004] According to the invention, an electrode for use in a welding operation is included in an apparatus of welding. The electrode comprises a metal cylinder defining a hollow core therebetween. The hollow core provides a conduit for delivering one or more materials therebetween via a delivery means. The cylinder may be formed of pure metals or metal alloys for forming a desired superalloy material composition, while materials delivered via the conduit comprises a balance of composition resulting deposit achieves the desired superalloy composition as a result of at least the combination of the cylinder materials and core delivered materials. It should be appreciated that the pure metal or metal alloy of the cylinder be of a material that is readily extruded (e.g., plastically shaped) into its cylindrical form. According to the invention the electrode further comprises a flux material surrounding the cylinder. The flux material may also contribute to the desired superalloy composition as a result of the weld operation. The delivery means may be a carrier assist gas or a mechanical assembly operably connected to the electrode for delivering the one or more materials to a delivery end of the electrode.BRIEF DESCRIPTION OF THE DRAWINGS

[0005] Fig. 1 is a schematic illustration of an electrode in accordance with the disclosure provided herein; Fig. 2 is a further schematic illustration of the electrode of Fig. 1, and in accordance with the disclosure provided herein; Fig. 3 illustrates a block diagram of a welding method in accordance with the disclosure provided herein. DETAILED DESCRIPTION

[0006] The present inventor has developed a novel method and apparatus for depositing a variety of difficult to deposit alloys. The method involves a variation of a shielded metal arc welding (SMAW) process, which is also referred to as stick welding or coated electrode welding. The novel process involves the use of an electrode consisting of a hollow metal or metal alloy sheath / core which is surrounded by a shielding means, i.e., an adherent coating flux. In operation, the metal alloy of the hollow sheath / core conducts welding current while the flux coating provides shielding. During the welding operation, the hollow metal sheath / core melts off and provides, e.g., the base material for the deposit, e.g., a pure nickel or alloyed nickle, iron etc., while the filler material delivered via the hollow core provides, e.g., the remaining materials required for forming the desired deposit. The flux coating melts during the weld operation, releases shielding gases, and provides a slag (first molten and then solid) to protect the molten deposit from atmospheric reactions. It should be appreciated that the flux may also contribute to the deposit's chemistry and may act to remove impurities from the molten pool.

[0007] It should be appreciated that the inventor's novel electrode now provides the flexibility for forming a variety of deposit superalloy compositions from a single electrode. For example, for a nickel based superalloy, an electrode comprising a pure nickel metal cylinder can be used to form any nickel based deposit superalloy composition, as the remaining or balance compositional constituents for forming the desired deposit composition may now be delivered via the hollow core of the electrode. Said another way, it is now possible to form, e.g., multiple types of nickel deposits, by changing the materials delivered through the electrode hollow core to form the desired deposit instead of changing the electrode. The electrode may include and be applied to other materials, in addition to the superalloys referenced herein, e.g., stainless steels, oxide dispersion strengthened alloys, etc., where the metal cylinder would be formed of the, e.g., iron, while the remaining constituents for forming stainless steel deposits are provided via the hollow core.

[0008] Referring now to the drawings wherein the showings are for purposes of illustrating embodiments of the subject matter herein only and not for limiting the same, Fig. 1 is a schematic illustration of one exemplary embodiment of a welding apparatus including electrode 100.

[0009] The electrode 100 is a SMAW electrode 100 and includes a cylinder 105, i.e., a metal cylinder or tube, defining a hollow core 110 therebetween for establishing an electrical current during a weld operation. The core 110 may be cylindrically shaped defining an interior (i.e., a core interior) adapted or sized to provide a conduit for delivery of materials 150, i.e. erg- , a stream of powdered feed materials (e.g., metal alloy powder and / or other constituents) and a material delivery means, e.g., a carrier (assist) gas or rotary system, therebetween.

[0010] The metal cylinder 105 may be formed of a ductile material, such as elemental metals, e.g., iron, nickel, cobalt, aluminum, or extrudable metal alloy materials including a subset of elements of a composition contributing to define a desired, e.g., superalloy, material, e.g., nickel or nickel alloy (e.g., CM247, Inconel 718, Inconel 939, Haynes 282, ER NiCr-3...). In operation, the conduit 110, i.e., the hollow cored portion of the electrode 100, may facilitate the delivery of a balance of the compositional constituents, e.g., Cr, Mo, Ti, Al, W, Mo, C, Ta, etc., in a powder form and with the carrier gas. It should be appreciated that the combination of the cylinder material and the core delivered materials results, after possible anticipated volatile losses, in achieving the deposited superalloy composition.

[0011] The carrier (assist) gas may be any known type of arc welding assist gas, e.g., argon, helium, hydrogen, carbon dioxide, oxygen, nitrogen, etc. or blends thereof, and may be optionally required depending upon what embodiment of the electrode 100 is provided. The feed rate of powder with assist gas may be regulated in concert with, e.g., the burn-off rate of the electrode 100 to achieve the desired superalloy deposit composition. The inventor has identified increased and potentially unlimited flexibility in this approach to lean or enrich the core powder feed rate or to regulate core powder composition to modulate deposit composition.

[0012] With continued reference to the figures, the electrode 100 further includes a shielding means 120 to provide shielding from, e.g., atmospheric reactions when an arc is established between the end of the electrode and substrate to be welded. According to the invention, the shielding means is an adherent flux coating 120 which surrounds the metal alloy cored portion 110 of the electrode 100. The flux coating 120 Provides shielding, i.e., during the SMAW operation and protection from, e.g., atmospheric reactions when an arc is established between the end of the electrode and substrate to be welded.

[0013] The flux coating 120 may be a full flux coating such that it is capable of providing complete shielding, e.g., during the SMAW operation shielding, without any further assistance, e.g., from another shielding source. Additionally or alternatively, the flux coating 120 may be a reduced flux coating, which may require an additional shielding means to assist with the shielding function. Additionally, the shielding means may be flux material projected or delivered through the conduit 110. The conduit delivered flux may be provided along with any hollow core feed materials, e.g., either mixed therewith and simultaneously fed or as conglomerate particles.

[0014] In a further example, not forming part of the present invention, the shielding means 120 may be an assist gas which may be fed around or through the conduit 110 to provide additional shielding, e.g., at the point of welding. The additional shielding means may be provided with any of the flux coatings (full or reduced). Additionally, an auxiliary shielding gas may also be provided, e.g., at the point of welding, to provide additional shielding, e.g., at an outer surface of the metal alloy tubular core wire 100. In yet a further embodiment, additional powdered flux may also be projected or delivered through the conduit 110 to assist in shielding as the additional shielding means.

[0015] With continued reference to the figures, and now Fig. 2, a further embodiment of the apparatus including the electrode 100 is provided. In the embodiment of Fig. 2, the delivery means for delivering materials through the hollow core 110 may be a mechanical assembly 200 to mechanically deliver the feed materials (e.g., powder) through the conduit 110. In one embodiment, the mechanical assembly 200 may be a rotary screw or auger 200 (Fig. 2) which may be operationally configured to control the flow and / or throughput of materials through the core 110.

[0016] The auger 200 may be configured to retract or be withdrawn axially relative to the electrode 100 and at a burn-off rate of the electrode 100. Additionally or alternatively, the electrode 100 may move or be projected over, e.g. a fixed auger during the weld operation.

[0017] Delivery of the feed materials (i.e., powder) via the auger 200 may be determined by the speed of rotation of the auger 200, and size (depth) and interval of auger threading (flutings). Additionally or alternatively, the auger delivery end, i.e., the end where the powder is being delivered via the auger 200, should be at or reside in the proximity of the welding end of the electrode 100 (e.g., ARC of Fig. 2).

[0018] In yet another exemplary embodiment, the delivery means may be one or more acoustic or ultrasonic waves projected from an acoustic or ultrasonic device or system. The ultrasonic system may be configured, e.g., to generate and / or impose ultrasonic waves to the electrode 100 to enhance delivery of the materials through the conduit 110. The waves may be directed towards the electrode 100 or towards the materials within the conduit 110 for directionally controlling the flow and throughput of materials within the conduit 110 and through the electrode 100.

[0019] It should be appreciated that the mechanical delivery means may be used with the carrier assist gas or in lieu of any gas assisted propulsion of core feed materials through the electrode 100. Any combination of delivery means may be used for delivering the core feed materials via the conduit 110.

[0020] With continued reference to the figures, and now Fig. 3, a welding technique (method) 1000 utilizing embodiments of the electrode 100 is provided. It should be appreciated that any steps disclosed herein are not required to be performed in any particular order, and are hereby provided for exemplary purposes. For example, steps for delivering the materials via the hollow core 110 may occur prior to forming the weld pool, while forming the weld pool, or once the weld pool has been formed.

[0021] The method 1000 includes melting the electrode 100 to form a deposit of, e.g., a material composition, e.g., a superalloy material composition on a superalloy substrate (1010). It should be appreciated that during the weld process, the electrode 100 is handled, i.e., via an electrode holder 300, also known as a stinger 300. According to the invention, the stinger 300 defines an interior or opening having at least a portion thereof sized or adapted to facilitate the feeding of materials 150 and / or the delivery means 200 (e.g., propulsion gas, auger) therethrough. For example, fig. 2 shows an embodiment of the stinger 300 with an interior 310 adapted to receive the auger 200 therethrough for delivery of the feed materials 150 at the delivery end of the electrode 100 near the point of welding.

[0022] The electrode 100 is held by the stinger 300 opposite the delivery end of the feed materials 150, i.e., opposite the welding end. Portions of any electrode coatings, i.e., flux coating 200 , is removed or stripped (SC , fig. 1) in order for the stinger 300 to hold the electrode 100 (e.g., the metal cylinder 105 ) and to thereby establish a welding current connection during the welding operation.

[0023] During the welding process the electrode 100 is consumed at the point of welding, i.e. it is melted and becomes part of a weld pool, as does the flux coating 120 . To form the weld pool, the substrate is melted, via an electric arc.

[0024] The metal cylinder 105 may comprise pure metals for forming, e.g., the desired superalloy material deposit composition. The core feed materials 150 comprising a balance of compositional constituents for forming the desired superalloy material deposit are delivered through the conduit 110, e.g., via the delivery means, at a delivery end of the electrode proximate to or at the point of welding (1020 ). Upon consumption of the metal cylinder, the core delivered materials, and the flux coating, the combination of the melted cylinder 105 and delivered materials 150 result in the deposit achieving the desired superalloy material composition.

[0025] It should be appreciated that in operation, the flux coating 120 upon consumption generates a shielding gas that shields the weld pool and surrounding heated area and protects the substrate from atmospheric contamination. The flux also enters the weld pool and forms a slag on the surface of the weld pool which may remain on a weld bead when the weld pool solidifies into a weld bead. While present in the volume of the weld pool, it should be appreciated that the flux may also deoxidize and / or remove impurities present in the weld pool. While present on the surface, the slag may also help shape the weld pool during solidification. The flux coating 120 may be neutral, i.e., may have virtually no effect on deposit composition, or alternatively, the flux may be active, i.e., making additions to the deposit composition or compensating for volatile losses during processing, e.g., the weld operation.

[0026] Additionally or alternatively, the method 1000 may include removing any slag resulting from melting of the flux coating 120 via any means for removing slag from a surface of a substrate known in the art and chosen with sound judgment (1030 ).

[0027] After slag removal, if needed, the method 1000 may include steps for finishing the substrate or component and preparing the component to be used in operation (1040 ). In this step 1040, and upon removal of any slag, the finishing and preparation steps may include heat treating the component, e.g., via a furnace, e.g., a high heat vacuum furnace. Additionally or alternatively, and prior to or after heat treatment, the component may be finished or machined to reduce undesired structures from the surface of the substrate, e.g., via a chip-removing method (e.g., using abrasive blasting media), and / or a grinding method. Additionally or alternatively, the finishing steps may include non-destructive testing methods to test the integrity of the component.

[0028] It should be noted that the term "comprising" does not exclude other elements or steps and the use of articles "a" or "an" does not exclude a plurality.

Claims

1. An apparatus of welding including an electrode (100) comprising: a metal cylinder (105) defining a weld end and a hollow interior (110), powdered feed materials (150) positioned in the hollow interior (110) and movable with respect to the metal cylinder towards the weld end of the electrode, a delivery means operable to move the powdered feed materials with respect to the metal cylinder, and an adherent flux coating (120) surrounding the metal cylinder (105), and using an electrode holder (300) defining an interior or opening having at least a portion thereof sized or adapted to facilitate the feeding of the powdered feed materials (150) and / or the delivery means therethrough, wherein the electrode (100) is held by the electrode holder (300) opposite the weld end, wherein portions of the flux coating (200) are removed or stripped in order for the electrode holder (300) to hold the metal cylinder (105) and to thereby establish a welding current connection during the welding operation.

2. The apparatus of claim 1, wherein the metal cylinder (150) comprises a ductile material wherein the ductile material comprises one or more of iron, nickel, cobalt, aluminum, titanium.

3. The apparatus of claim 2, wherein the ductile material comprises extrudable metal alloy materials including a subset of elements of a composition contributing to define a desired superalloy material composition, and wherein the powdered feed materials delivered via the conduit comprises a balance of compositional constituents defining the desired superalloy material composition.

4. The apparatus of any of claims 1 to 3, wherein the delivery means is a carrier gas.

5. The apparatus of claim 4, wherein the carrier gas is selected from one or more of argon, helium, hydrogen, carbon dioxide, oxygen, nitrogen, or blends thereof.

6. The apparatus of claim 1, wherein the delivery means comprises a mechanical assembly that includes an auger.

7. The apparatus of claim6, wherein the auger is configured to retract axially relative to the electrode at a burn-off rate of the electrode.

8. The apparatus of claim 6, wherein the auger is fixed and the electrode is adapted to project over the auger in operation.

9. The apparatus of any of claims 1 to 3, wherein the delivery means is an acoustic or ultrasonic system configured to deliver acoustic or ultrasonic waves to facilitate delivery of the powdered feed materials to the weld end.

10. A shielded metal arc welding method using an apparatus according to any of claims 1 to 9 comprising: melting a substrate and the electrode to form a deposit material composition.