Double-sheet thermoforming process for a hollow body and hollow body by derivation
The double-sheet thermoforming process for poly-aryl-ether-ketones achieves crystallized hollow bodies with improved adhesion and structural integrity by using pseudo-amorphous compositions that coalesce and crystallize without intermediate layers, addressing the need for additional adhesion in existing processes.
Patent Information
- Application Number
- FR2021010778
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-10-12
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-10-12
AI Technical Summary
Existing double-sheet thermoforming processes for poly-aryl-ether-ketones require an additional intermediate layer for adhesion, which complicates the manufacturing of high-performance crystallized hollow bodies.
A double-sheet thermoforming process using sheets composed of pseudo-amorphous poly-aryl-ether-ketone compositions that remain in an amorphous state until contact, allowing for direct coalescence and subsequent crystallization without an intermediate layer, utilizing specific viscosity and crystallization time ranges to achieve a crystallized hollow body.
The process enables the production of high-quality, crystallized hollow bodies with improved adhesion and structural integrity, eliminating the need for additional adhesion layers and enhancing manufacturing efficiency.
Smart Images

Figure 00000032_0000 
Figure 00000032_0001
Abstract
Description
Title of the invention: Double-sheet thermoforming method for a hollow body and hollow body derived therefrom Technical field
[0001] The invention relates to the field of double-sheet thermoforming processes for a hollow body.
[0002] More specifically, the invention relates to such methods using sheets based on poly-aryl-ether-ketone(s). Prior art
[0003] Poly-aryl-ether-ketones are well-known high-performance technical polymers. They can be used for applications requiring temperature and / or mechanical or even chemical constraints. They can also be used for applications requiring excellent fire resistance and low emissions of smoke or toxic gases. Finally, they have good biocompatibility. These polymers are found in fields as varied as aeronautics and space, offshore drilling, automotive, railway, marine, wind power, sports, construction, electronics and even medical implants.
[0004] Double-sheet thermoforming processes for thermoplastics are also known from the prior art. They make it possible in particular to produce hollow rigid articles.
[0005] A double-sheet thermoforming process involves thermoforming two sheets to form two halves of an article and welding these halves together to obtain a hollow article.
[0006] Two methods are known in particular.
[0007] According to a first method, two thermoplastic polymer sheets are placed in a clamping frame and heated simultaneously. When the sheets have reached the forming temperature, i.e. are sufficiently softened, air is forced between the sheets and / or a vacuum is applied to the outer part of the sheets, pressing them against two halves of molds which can be closed and pressed against each other allowing a pinching effect.
[0008] According to a second method, the two sheets are sequentially thermoformed in their respective mold halves. The two mold halves are then closed and pressed against each other, allowing the pinching effect.
[0009] An example of implementation with thermoplastic polymers having a high deflection temperature (HHDT) is described in US patent 5,114,767 A2. HHDT polymers include, within the meaning of this technique, polyetherimides, polyamideimides, polyimides, polysulfones, polyether sulfone, polyphenyl sulfone, polyetheretherketone, polyetherketoneketone, polyaryl sulfone, aromatic polyamides, polyaryl sulfones and polyphenyl ether / polystyrene blends.
[0010] Two layers of HHDT thermoplastic polymer, such as one of those mentioned above, are first heated above their deflection temperature and placed between two mold halves heated to a temperature below said deflection temperature. A layer of a low deflection temperature (LHDT) polymer is interposed between the two layers of HHDT thermoplastic polymer. The two mold halves are then closed against each other, the adhesion between the two layers of HHDT polymer being ensured by the presence of the LHDT polymer. Finally, a hollow body is formed by injecting gas into the mold.
[0011] This technique has the disadvantage of requiring the addition of an adhesion layer between the two layers intended to mainly form the hollow body.
[0012] There is currently a need to use poly-aryl-ether-ketones in thermoforming processes in order to manufacture high performance crystallized hollow bodies.
[0013] The present invention provides a double-sheet thermoforming process comprising at least two sheets of poly-aryl-ether-ketone(s) capable of crystallizing without requiring an additional intermediate layer. Summary of the invention
[0014] The invention relates to a double-sheet thermoforming method for manufacturing a hollow body. The method comprises:
[0015] - the provision of two sheets comprising at least one face consisting of a pseudo-amorphous composition based on poly-aryl-ether-ketone(s);
[0016] - a step of softening the two sheets at a softening temperature, so as to form softened leaves,
[0017] the softening temperature being greater than or equal to the glass transition temperature of each pseudo-amorphous composition;
[0018] - a step of forming the softened sheets so as to form sheets thermoformed;
[0019] - a step of bringing into contact and coalescing at least one contact zone of said softened leaf faces, and / or
[0020] sheets being formed or already formed,
[0021] so as to form an intermediate body, the contact zones being heated to a contacting temperature, each contact zone remaining in an essentially amorphous state at least until contacting; and,
[0022] - a step of crystallization of the composition at a mold temperature, for form a hollow crystallized body,
[0023] the crystallization step being implemented essentially after the contacting and coalescence step, and preferably essentially after the forming step.
[0024] Advantageously, the composition may have a viscosity at 380°C, at 1 Hz, as measured by a parallel plane rheometer, ranging from 200 Pa.s to 8000 Pa.s, preferably from 500 Pa.s to 5000 Pa.s, and more preferably from 750 Pa.s to 4500 Pa.s.
[0025] Advantageously, the isothermal half-crystallization time at the contact temperature of the composition may be at least 3 seconds, preferably at least 5 seconds, and most preferably at least 8 seconds; and / or at most 30 minutes, preferably at most 10 minutes, still preferably at most 5 minutes, and most preferably at most 2 minutes.
[0026] According to certain embodiments, the poly-aryl-ether-ketone(s) may be a poly-ether-ketone-ketone. It may preferably be a homopolymer or a copolymer essentially consisting of, or consisting of, at least one isophthalic repeating unit (I), having the chemical formula:
[0027] [Chem.l]
[0028] and in the case of the copolymer, of a terephthalic repeating unit (T), having for chemical formula:
[0029] [Chem.2] =.. O ..___„ O *..........4 / ....... G .......4 4................4 '.................*
[0030] the molar percentage of T units relative to the sum of the T and I units being from 0% to 5% or from 35% to 78%, preferably from 45% to 75%, and extremely preferably from 48% to 52% or from 65% to 74%.
[0031] According to certain embodiments, the poly-aryl-ether-ketone(s) may be a copolymer essentially consisting of, or consisting of, a repeating unit of formula:
[0032] [Chem.3]
[0033] (III);
[0034] and a repeating pattern of formula:
[0035] [Chem.4] ° / —°—\* (IV);
[0036] the molar percentage in unit (III) relative to the sum of units (III) and (IV) being: 0% to 99%, preferably 5% to 95%, more preferably 10% to 50% and most preferably 20% to 40%.
[0037] According to certain embodiments, the poly-aryl-ether-ketone(s) may be a copolymer essentially consisting of, or consisting of, a repeating unit having the formula:
[0038] [Chem.5] .____ ____ O —C h— o—( S—o——* (in);
[0039] and a repeating pattern having the formula:
[0040] [Chem.6] (V);
[0041] the molar percentage in unit (III) relative to the sum of units (III) and (V) being from 0% to 99% and preferably from 0% to 95%.
[0042] According to certain embodiments, the composition may comprise at least one other thermoplastic polymer other than a poly-aryl-ether-ketone and / or may comprise at least one filler and / or may comprise at least one additive.
[0043] According to certain embodiments, the composition may consist of the poly-aryl-ether-ketone(s), optionally one or more other thermoplastic polymer(s) other than a poly-aryl-ether-ketone, optionally one or more fillers, and optionally one or more additives.
[0044] According to certain embodiments, each sheet may be constituted, independently or not of one another, of a pseudo-amorphous composition based on poly-aryl-ether-ketone(s).
[0045] Advantageously, the two sheets may have, independently or not of one another, a thickness of 200 microns to 20 millimeters, preferably a thickness of 500 microns to 10 millimeters.
[0046] Advantageously, the crystallization step can be carried out up to an average crystallinity level in the thickness strictly greater than 7%, as measured by WAXS, during the crystallization step; preferably up to a crystallinity level greater than or equal to 10%, or greater than or equal to 15%, or greater than or equal to 20%, or even greater than or equal to 25%.
[0047] Advantageously, the softening step can be carried out with a softening temperature having a value strictly greater than Tg and less than or equal to (Tg+80)°C, and preferably having a value ranging from (Tg + 10)°C to (Tg+75)°C.
[0048] Advantageously, the crystallization step can be carried out at a mold temperature close to the temperature at which the composition has a minimum isothermal half-crystallization time.
[0049] Advantageously, the difference between the mold temperature and the softening temperature is less than or equal to 50°C, and preferably greater than or equal to 15°C.
[0050] According to certain embodiments, the contacting and coalescence step is implemented with a pinch pressure having a value ranging from 1 bar to 50 bars, preferably with a pinch pressure having a value ranging from 5 bars to 40 bars, and more preferably with a pinch pressure having a value ranging from 7 bars to 30 bars.
[0051] The invention also relates to a hollow body comprising at least one internal surface consisting of a crystallized composition based on poly-aryl-ether-ketone(s), capable of being obtained by a process as described above.
[0052] The present invention is based on the use by the inventors of sheets comprising at least one face consisting of a pseudo-amorphous composition based on poly-aryl-ether-ketone(s) for a double-sheet thermoforming process for manufacturing a hollow body. The use of such sheets can in particular be implemented in a process such as those described above. These sheets allow for good quality heat sealing at the contact zone between the sheets, since the composition of each sheet remains in an essentially amorphous state until the compositions come into contact and coalescence. The composition of each sheet is nevertheless crystallizable and crystallizes after the compositions come into contact and coalescence. The inventors were thus able to exploit the particularly advantageous crystallization kinetics of pseudo-amorphous poly-aryl-ether-ketone(s) to implement a hollow body crystallized from sheets of pseudo-amorphous composition(s) based on poly-aryl-ether-ketone(s), without the need for an intermediate adhesive layer. Figures
[0053] [Fig.l] is a diagram of a double-sheet thermoforming device.
[0054] [Fig.2] is a block diagram representing the main steps of a double-sheet thermoforming process according to a first embodiment and for which the device according to [Fig.l] is particularly suitable. Detailed description of the invention Definitions
[0055] The term "glass transition temperature", noted Tg, is understood to mean the temperature at which a polymer, at least partially amorphous, passes from a rubbery state to a glassy state, or vice versa, as measured by differential scanning calorimetry (DSC) according to standard NF ISO 11357-2:2020, in second heating using a heating rate of 20°C / min.
[0056] In the present invention, when reference is made to a glass transition temperature, this is more particularly, unless otherwise indicated, the glass transition temperature at half-step height as defined in this standard. The compositions based on PAEK(s) in the present invention may optionally have several glass transition steps in the DSC analysis, in particular due, where appropriate, to the presence of several different immiscible polymers. In this case, the term glass transition temperature means the highest glass transition temperature corresponding to the glass transition step of the PAEK or the mixture of PAEKs.
[0057] The term "melting temperature", denoted Tf, is understood to mean the temperature at which an at least partially crystallized polymer passes into the viscous liquid state, as measured by differential scanning calorimetry (DSC) according to standard NF EN ISO 11357-3:2018, on first heating, using a heating rate of 20°C / min. In the present invention, when reference is made to a melting temperature, it is more particularly, unless otherwise indicated, the peak melting temperature as defined in this standard. The compositions based on PAEK(s) in the present invention may possibly have several melting peaks in the DSC analysis, in particular due to and / or for a given polymer to the presence of different crystalline forms. In this case, the term melting temperature means the melting temperature corresponding to the highest melting peak in temperature.
[0058] The term “pseudo-amorphous” polymer, or “pseudo-amorphous” composition, is understood to mean a polymer, or a composition, which is present at a temperature below its glass transition temperature in essentially amorphous form. The polymer, or the composition, is nevertheless capable of crystallizing once brought to a temperature above its glass transition temperature for a sufficient period of time. For the purposes of the invention, a “pseudo-amorphous” polymer, or a “pseudo-amorphous” composition, has a crystallinity level of 0% to 7% at 25°C.
[0059] The “crystallinity rate” can be measured by WAXS. For example, the analysis can be carried out by wide angle X-ray scattering (WAXS), on a Nano-inXider® type device with the following conditions:
[0060] - Wavelength: main Kal line of copper (1.54 Angstroms).
[0061] - Generator power: 50 kV - 0.6 mA.
[0062] - Observation mode: transmission.
[0063] - Counting time: 10 minutes.
[0064] A spectrum of the scattered intensity as a function of the diffraction angle is thus obtained. This spectrum makes it possible to identify the presence of crystals, when peaks are visible on the spectrum in addition to the amorphous halo.
[0065] In the spectrum, the area of the crystalline peaks (denoted AC) and the area of the amorphous halo (denoted AH) can be measured. The mass proportion of crystalline PEKK in the PEKK is then estimated by the ratio (AC) / (AC +AH).
[0066] The term “isothermal half-crystallization time”, noted “11 / 2” at a measurement temperature, means the time required to reach a relative crystallinity of 0.5 for isothermal crystallization at the measurement temperature, as defined according to ISO 11357-7:2015.
[0067] According to this standard, the isothermal crystallization conditions are implemented by a first step of melting a test piece then cooling as quickly as possible to the chosen measurement temperature so that crystallization begins after the end of the cooling step. The time at which the isothermal step ends, i.e. the time required to obtain a complete crystallization curve, depends on the crystallization rate. In the absence of clarity of the DSC curve, this time is set at five times the time required to reach the maximum crystallization rate.
[0068] The term "polymer blend" is understood to mean a macroscopically homogeneous polymer composition. The term encompasses blends of compatible and / or miscible polymers, the blend having a glass transition temperature intermediate to those of its polymers considered individually. The term also encompasses such compositions composed of phases immiscible with each other and dispersed at the micrometric scale.
[0069] The term "copolymer" means a polymer resulting from the copolymerization of at least two chemically different types of monomer, called comonomers. A copolymer is therefore formed from at least two repeating units. It can also be formed from three or more repeating units.
[0070] The acronym "PAEK" corresponds to the notation "poly-aryl-ether-ketone", "PAEKs" to "poly-aryl-ether-ketones" and "PAEK(s)" to "poly-aryl-ether-ketone or poly-aryl-ether-ketones".
[0071] In all the ranges set out in this application, the terminals are included unless otherwise stated.
[0072] Pseudo-amorphous composition based on poly-aryl-ether-ketone(s)
[0073] The composition based on poly-aryl-ether-ketone(s) in sheet form for the process according to the invention is pseudo-amorphous.
[0074] It is the essentially amorphous character of the composition which allows good coalescence of the peripheral zones of the sheets brought into contact in the double-sheet thermoforming process. This is why the at least one poly-aryl-ether-ketone, respectively the composition comprising it, advantageously has a crystallinity rate of less than or equal to 5.0%, or less than or equal to 3.0%, or even less than or equal to 1.0%, and ideally of approximately 0%.
[0075] The composition must have a crystallization rate at a temperature between Tf and Tg sufficiently slow, so as to be able to form sheets in the pseudo-amorphous state.
[0076] The composition must also have a crystallization rate between Tf and Tg sufficiently slow so as to remain in an essentially amorphous state during the softening step and until the contacting step.
[0077] Conversely, the composition must have a crystallization rate between Tf and Tg sufficiently fast so as to be able to crystallize within a reasonable time scale after the contacting and coalescence step.
[0078] Advantageously, the isothermal half-crystallization time of the composition at the softening temperature and / or at the contact temperature may be at least 3 seconds and at most 30 minutes.
[0079] The isothermal half-crystallization time of the composition at the softening temperature and / or at the contact temperature may preferably be at least 5 seconds, and more preferably at least 8 seconds.
[0080] The isothermal half-crystallization time of the composition at the softening temperature and / or at the contact temperature may preferably be at most 10 minutes, more preferably at most 5 minutes, and extremely preferably at most 2 minutes.
[0081] Advantageously, the viscosity of the composition at 380°C and 1 Hz, as measured with a 25 mm diameter parallel plane rheometer, under nitrogen flushing, has a value of 200 Pa.s to 8000 Pa.s, preferably of 500 Pa.s to 5000 Pa.s, and more preferably of 750 Pa.s to 4500 Pa.s.
[0082] These viscosity ranges are particularly advantageous for making it possible to obtain a sheet having good strength and a substantially uniform thickness during extrusion of the sheet, reasonable resistance to fining during the step of forming the softened sheets, and finally to allow good coalescence during the step of bringing the two sheets into contact and coalescing with each other.
[0083] The composition may in particular have a viscosity having a value of: 750 Pa.s to 1200 Pa.s, or from 1200 Pa.s to 1600 Pa.s, or from 1600 Pa.s to 2000 Pa.s, or from 2000 Pa.s to 2400 Pa.s, or from 2400 Pa.s to 2800 Pa.s, or from 2800 Pa.s to 3200 Pa.s, or from 3200 Pa.s to 3600 Pa.s, or from 3600 Pa.s to 4000 Pa.s, or from 4000 Pa.s to 4250 Pa.s, or from 4250 Pa.s to 4500 Pa.s.
[0084] The composition preferably has a glass transition temperature Tg greater than or equal to 125°C, more preferably greater than or equal to 145°C, and extremely preferably greater than or equal to 150°C.
[0085] The composition preferably has a melting temperature Tf greater than or equal to 250°C, and more preferably greater than or equal to 270°C. The composition may in particular have a melting temperature greater than or equal to 280°C, or greater than or equal to 290°C, or greater than or equal to 300°C, or greater than or equal to 310°C, or greater than or equal to 320°C, or even greater than or equal to 330°C.
[0086] The composition comprises at least 50% by weight of at least one poly-aryl-ether-ketone. It is indifferently designated in the remainder of the application as a composition based on poly-aryl-ether-ketone(s).
[0087] A poly-aryl-ether-ketone (PAEK) comprises the units of the following formulas: (-Ar-X-) and (-Ah-Y-),
[0088] in which:
[0089] - Ar and An each denote a divalent aromatic radical;
[0090] - Ar and Ari may preferably be chosen from 1,3-phenylene, 1,4- phenylene, 1,1'-divalent biphenylene in 3,3' positions, 1,1'-divalent biphenyl in 3,4' positions, 1,4-naphthylene, 1,5-naphthylene and 2,6-naphthylene;
[0091] - X denotes an electron-withdrawing group; it may preferably be chosen from: carbonyl group and sulfonyl group,
[0092] - Y denotes a group chosen from an oxygen atom, a sulfur atom, a alkylene group, such as -(CH)2- and isopropylidene.
[0093] In these X and Y units, at least 50%, preferably at least 70% and more particularly at least 80% of the X groups are a carbonyl group, and at least 50%, preferably at least 70% and more particularly at least 80% of the Y groups represent an oxygen atom.
[0094] According to a preferred embodiment, 100% of the X groups denote a carbonyl group and 100% of the Y groups represent an oxygen atom.
[0095] The weight of PAEK or, where appropriate, the sum of the weights of the PAEKs of the composition may represent at least 60%, or at least 70%, or at least 80%, or at least 85%, or at least 90%, or at least 92.5%, or at least 95%, or at least 99%, or at least 99.9% or 100% of the total weight of the composition.
[0096] In certain embodiments the composition consists essentially of PAEK(s), i.e. it comprises from 90% to 99.9% of the total weight of the composition in PAEK(s).
[0097] In certain embodiments, the composition is made up of PAEK(s), i.e., it is made up of at least 99.9%, ideally 100%, of the total weight of the composition in PAEK(s).
[0098] Advantageously, the PAEK(s) may be chosen from:
[0099] - a polyether-ketone-ketone, also called PEKK; a PEKK comprises a / unit(s) of formula: -Ph-O-Ph-C(O)-Ph-C(O)-;
[0100] - a poly-ether-ether-ketone, also called PEEK; a PEEK comprises one or more motif(s) of formula: -Ph-O-Ph-O-Ph-C(O)-;
[0101] - a poly-ether-ketone, also called PEK; a PEK comprises one or more units of formula: -Ph-O-Ph-C(O)-;
[0102] - a poly-ether-ether-ketone-ketone, also called PEEKK; a PEEKK comprises one or more units of formula: -Ph-O-Ph-O-Ph-C(O)- Ph-C(O)-;
[0103] - a poly-ether-ether-ether-ketone, also called PEEEK; a PEEEK comprises one or more units of formula: -Ph-O-Ph-O-Ph-O- Ph-C(O)-;
[0104] - a poly-ether-diphenyl-ether-ketone also called PEDEK; a PEDEK comprises one or more units of formula: a PEDEK comprises one or more units of formula -Ph-O-Ph-Ph-O-Ph-C(O)-;
[0105] - their mixtures; and,
[0106] - copolymers comprising at least two of the above-mentioned units,
[0107] in which: Ph represents a phenylene group and -C(O)- a group carbonyl, each of the phenylenes being able independently to be of ortho (1-2), meta (1-3) or para (1-4) type, preferentially being of meta or para type.
[0108] Furthermore, defects, end groups and / or monomers may be incorporated in very small amounts into the polymers as described in the list above, without having an impact on their performance.
[0109] According to certain embodiments, the composition comprises, is essentially composed of, or even consists of, a poly-ether-ketone-ketone polymer comprising:
[0110] a terephthalic unit and an isophthalic unit, the terephthalic unit having the formula: [YES] [Chem.7] (i);
[0112] the isophthalic unit having the formula:
[0113] [Chem.8] (II).
[0114] For a polymer of a given family, such as the PEKK family, the term "comprises one or more units" means that this / these unit(s) have a total molar proportion of at least 50% in the polymer. This / these unit(s) may represent a molar proportion of at least 60%, or at least 70%, or at least 80%, or at least 85%, or at least 90%, or at least 92.5%, or at least 95%, or at least 99%, or at least 99.9% in the polymer. The term "essentially consisting of unit(s)" means that the unit(s) represent(s) a molar proportion of 95% to 99.9% in the copolymer. Finally, "consisting of unit(s)" means that 171st unit(s) represent a molar proportion of at least 99.9% in the polymer.
[0115] Preferably, the polyether-ketone-ketone is essentially made up of, or even made up of: isophthalic “I” and terephthalic “T” units.
[0116] Preferably, the poly-ether-ketone-ketone is, where appropriate, a random copolymer.
[0117]
[0118]
[0119]
[0120]
[0121]
[0122]
[0123] The choice of the molar proportion of T units relative to the sum of T and I units is one of the factors that allows the adjustment of the crystallization rate properties of polyether-ketone-ketones. A given molar proportion of T units relative to the sum of T and I units can be obtained by adjusting the respective concentrations of the reactants during the polymerization, in a manner known per se. The molar proportion of T units relative to the sum of the T and I units of PEKK(s) may in particular vary from: 0 to 5%; or from 5 to 10%; or from 10 to 15%; or from 15 to 20%; or from 20 to 25%; or from 25 to 30%; or from 30 to 35%; or from 35 to 40%; or from 40 to 45%; or from 45 to 48%, or from 48% to 51%, or from 51% to 54%, or from 54% to 58%, or from 58% to 62%, or from 62% to 65%, or from 65 to 68%; or from 68% to 73% or from 73% to 75%; or from 75 to 78%; or from 78 to 80%; or from 80 to 85%. According to particular embodiments, the polyether-ketone-ketone is essentially constituted, or even constituted, of “T” and “I” units, with a molar proportion of T units relative to the sum of the T and I units ranging from 0% to 5% or from 35% to 78%. Indeed, for this range of molar proportions, a polyether-ketone-ketone has an appropriate crystallization speed allowing on the one hand to be obtained in essentially amorphous form by means of sufficiently rapid cooling and to crystallize sufficiently quickly once heated above its glass transition temperature. These molar proportions of T units relative to the sum of the T and I units are therefore particularly suitable for compositions essentially constituted, or even constituted, of a single polyether-ketone-ketone.The molar proportion of T units relative to the sum of the T and I units may preferably be from 0% to 5% or from 35% to 78%, preferably from 45% to 75% and more preferably from 48% to 52% or from 65% to 74%. The molar proportion of T units relative to the sum of the T and I units may in particular be approximately 50% or approximately 70%. The composition preferably does not consist of a polyether-ether-ketone homopolymer consisting of a single repeating unit of formula: [Chem.9] (III). Indeed, this polymer crystallizes very rapidly when heated above its Tg, which makes it very difficult to form thick pseudo-amorphous sheets and which also makes it very difficult to form such sheets in an essentially amorphous state. Furthermore, due to its very rapid crystallization, this polymer does not allow good coalescence between sheets and results in poor adhesion properties at the contact zone.
[0124] Based on this observation, it may nevertheless be envisaged to reduce the crystallization rate of the above homopolymer in various ways.
[0125] A first aspect is the introduction of a certain number of defects into the structure of the homopolymer consisting of the unit of formula (III), i.e. a modification of its chemical structure.
[0126] The composition may comprise, be essentially composed of, or even be composed of, a polymer comprising a unit of formula:
[0127] [Chem. 10]
[0128] and a unit of formula:
[0129] [Chem. 11] (IV).
[0130] Preferably, the polymer is essentially made up of, or even made up of: units of formula (III) and (IV).
[0131] Preferably, the polymer is, where appropriate, a random copolymer.
[0132] The molar proportion of unit (III) relative to the sum of units (III) and (IV) may range from 0% to 99%, preferably from 5% to 95%, more preferably from 10% to 50% and most preferably from 20% to 40%.
[0133] According to certain variants, the composition may comprise, be essentially constituted of, or even constituted of, a polymer comprising, being essentially constituted of, or even constituted of:
[0134] a unit of formula:
[0135] [Chem. 12] (III);
[0136] and a unit of formula:
[0137] [Chem. 13] (IVa).
[0138] Preferably, the polymer is essentially made up of, or even made up of: units of formula (III) and (IVa).
[0139] Preferably, the polymer is, where appropriate, a random copolymer.
[0140] The molar proportion of unit (III) relative to the sum of units (III) and (IVa) can range from 0% to 99%, and preferably from 5% to 95%.
[0141] The composition may comprise, be essentially constituted, or even constituted, of a polymer comprising a unit of formula:
[0142] [Chem. 14] (V).
[0145] Preferably, the polymer is essentially made up of, or even made up of, units of formula (III) and (V).
[0146] Preferably, the polymer is, where appropriate, a random copolymer.
[0147] The molar proportion of unit (III) relative to the sum of units (III) and (V) can range from 0% to 99%, preferably from 0% to 95%.
[0148] According to certain variants, the composition may comprise, be essentially constituted of, or even constituted of, a polymer comprising, being essentially constituted of, or even constituted of:
[0149] a unit of formula:
[0150] [Chem. 16] (III),
[0151] and a unit of formula:
[0152] [Chem. 17] (Go).
[0153] Preferably, the polymer is essentially made up of, or even made up of, units of formula (III) and (Va).
[0154] Preferably, the polymer is, where appropriate, a random copolymer.
[0155] The molar proportion of unit (III) relative to the sum of units (III) and (Va) can range from 0% to 99%, and preferably from 0% to 95%.
[0156] A second aspect for reducing the crystallization of a homopolymer consisting of the repeating unit of formula (III) is to mix it with another PAEK which takes longer to crystallize. This other PAEK may in particular be a PEKK essentially consisting, preferably consisting, of unit I and / or unit T or even a copolymer comprising the repeating unit of formula (III), in particular those presented above.
[0157] A third aspect for reducing the crystallization rate of a PEEK homopolymer consisting of the repeating unit of formula (III) is to blend it with another polymer other than a PAEK, in particular an amorphous polymer. An amorphous polymer compatible with many PAEKs, in particular with a PEKK or a PEEK, is for example a polyetherimide.
[0158] A fourth aspect, not developed in detail here, for reducing the crystallization of a PEEK homopolymer consisting of the repeating unit of formula (III) would be the addition of an additive acting as a crystallization rate modulating agent.
[0159] According to certain particular embodiments, the composition is in particular essentially constituted, or constituted, of a single PAEK chosen from:
[0160] - a PEKK, in particular being essentially constituted, or constituted of the units I and T, as described above;
[0161] - a polymer essentially consisting of, or consisting of, units of formula (III) and (IV), as described above; and,
[0162] - a polymer essentially consisting of, or consisting of, units of formula (III) and (V), as described above.
[0163] According to certain embodiments, the composition comprises, consists essentially of, or consists of a single PAEK, of substantially homogeneous composition and / or viscosity.
[0164] According to certain embodiments, the composition comprises, is essentially made up of, or is made up of, several different PAEKs, i.e. in particular having a different chemical composition and / or a different viscosity.
[0165] According to certain particular embodiments, the composition comprises at least two PAEKs of different chemical composition, more particularly:
[0166] - a PEKK, in particular being essentially constituted, or constituted of the patterns I and T, as described above, and in addition to this PEKK,
[0167] - at least one of the following polymers: PEK, PEEKEK, PEEK, in particular a polymer essentially consisting of, or consisting of units of formula (III) and (V) as described above, PEEKK, PEKEKK, PEEEK, PEDEK, or a polymer essentially consisting of, or consisting of units of formula (III) and (IV) as described above, with a content of less than 50% by weight of the total weight of the composition, preferably less than or equal to 30% by weight of the composition.
[0168] According to certain particular embodiments, the composition comprises a mixture of several PAEKs, the PAEKs being a copolymer of PAEK with different molar proportions in repeating units. In particular, the composition may comprise a mixture of copolymers of PEKKs having a different molar ratio in “T-type” units relative to the sum of the “T-type” and “I-type” units.
[0169] According to certain particular embodiments, the composition may also comprise a mixture of several PAEKs, the PAEKs being a copolymer of PAEK with different viscosities.
[0170] Finally, the composition may also comprise a mixture of PAEK copolymers, the PAEKs being a copolymer of PAEK with different molar proportions in repeating units and different viscosities.
[0171] According to certain embodiments, the composition may further comprise one or more other polymers not belonging to the PAEK family, in particular other thermoplastic polymers.
[0172] According to certain embodiments, the composition may comprise a mixture of PAEK(s) with at least one fluoropolymer, such as the fluoropolymers described in application EP 2,767,986 and US 9,543,058. The fluoropolymer may preferably be chosen from the list consisting of: a polytetrafluoroethylene (PTFE), a poly(vinyl fluoride) (PVF), a poly(vinyl fluoride) (PVDF), a polychlorotrifluoroethylene (PCTFE), a perfluoroalkoxy polymer, a perfluoroalkoxy-alkane copolymer (PFA), a fluorinated ethylene-propylene copolymer (FEP), a poly(ethylene-co-tetrafluoroethylene) (ETFE), polyethylenechlorotrifluoroethylene (ECTFE), a perfluorinated elastomer (FFKM), a perfluoropoly ether (PFPE), and a mixture thereof.
[0173] Since fluoropolymers are generally immiscible with PAEKs, the composition is, in these embodiments, advantageously a dispersion of fluoropolymer particles in said at least one PAEK.
[0174] According to certain embodiments, the composition comprises a mixture of PAEK(s) and a polyetherimide (PEI), a silicone-polyimide copolymer or a polysiloxane / polyimide block copolymer (such as a polyetherimide / polydimethylsiloxane (PEI / PDMS)), such as the polymers described in applications EP 0 323 142 and US 8 013 251.
[0175] According to certain embodiments, the composition may comprise alternatively to the aforementioned thermoplastics or in addition to them: a polyphenylene sulfone (PPSU), a polysulfone (PSU), a polycarbonate (PC), a polyphenylene ether (PPE), a poly(phenylene sulfide) (PPS), a poly(ethylene terephthalate) (PET), a polyamide (PA), a polybenzimidizole (PBI), a poly(amide-imide) (PAI), a poly(ether sulfone) (PES), a poly(aryl sulfone), a poly(ether imide sulfone), a polyphenylene, a polybenzoxazole, a polybenzothiazole, or a mixture thereof.
[0176] According to certain particular embodiments, the composition is essentially made up, or made up of a mixture of:
[0177] - PAEK chosen from: a PEKK, in particular being essentially made up of, or consisting of units I and T, as described above; a polymer consisting essentially of, or consisting of, units of formula (III) and (IV), as described above; and a polymer consisting essentially of, or consisting of units of formula (III) and (V), as described above;
[0178] - with another polymer chosen from the list consisting of:
[0179] FEP, PFA, FFKM, PEI, PEI / PDMS, PES, PSU, PPSU, PPS, PPE and their mixture.
[0180] The composition may in particular be essentially made up of, or made up of, a mixture of:
[0181] - PEKK, essentially consisting of, or consisting of, the I and T units, wherein
[0182] the molar proportion of T units relative to the sum of T and I units ranges from 45% to 75%;
[0183] - with another polymer chosen from the list consisting of: FEP, PFA, FFKM, PEI, PEVPDMS, PES, PSU, PPSU, PPS, PPE and their mixture.
[0184] According to certain embodiments, the composition may further comprise fillers and / or additives.
[0185] Among the fillers, let us mention fillers of the mainly reinforcing type, in fibrous or non-fibrous form. Non-fibrous fillers can in particular be titanium dioxide, talc or calcium carbonate. Fibrous fillers can in particular be glass fibers and carbon fibers, ground or not.
[0186] Among the fillers, let us mention fillers of the mainly thermally conductive type, and in particular fillers which can be chosen from the list consisting of: ceramics, such as boron nitride or aluminum oxide, metals, such as copper, stainless steel, aluminum, gold, silver, carbon fillers, such as carbon black, carbon nanotubes, graphite, mineral fillers, such as hematite, or their mixture.
[0187] The composition may thus comprise less than 50% by weight of fillers, preferably less than 40% by weight of fillers and even more preferably less than 25% by weight of fillers, relative to the total weight of the composition.
[0188] Among the additives, mention may be made of stabilizing agents (light, in particular UV, and heat such as, for example, phosphate salts), optical brighteners, dyes, pigments, flow agents, additives for adjusting the viscosity of the composition in the molten state, additives for adjusting the crystallization rates of the composition, additives for adjusting the heat capacity of the composition, or a combination of these additives. The composition may thus comprise less than 10% by weight, preferably less than 5% by weight, and even more preferably less than 1% by weight of additive(s) relative to the total weight of the composition.
[0189] Sheet comprising the composition on at least one of its faces
[0190] A sheet is a three-dimensional article that is typically flat or substantially planar and has a thickness that is significantly less than both its length and its width. A sheet may in particular have a thickness less than 10%, or less than 5%, of both its length and its width.
[0191] The sheet may be non-porous, porous, microporous, etc., depending on the intended application and use.
[0192] According to certain embodiments, the sheet may be made of the pseudo-amorphous composition based on polyaryl ether ketone(s).
[0193] According to certain embodiments, the sheet may be formed by a multiplicity of layers, i.e. at least two layers, each layer being able to have independently of one another a different chemical composition or not. In this embodiment, the composition based on poly-aryl-ether-ketone(s) is then used to form a layer at the periphery of the multiplicity of layers, i.e. on at least one of the two faces of the sheet.
[0194] According to some embodiments, each sheet may be made of two layers. An advantageous example of a bi-layer sheet is a sheet made of a first layer of PEKK consisting of T:I repeat units and having a T:I molar ratio of about 70:30 and a second layer of PEKK consisting of T:I repeat units and having a T:I molar ratio of about 60:40, the PEKK having a T:I ratio being advantageously used to constitute the inner face of a sheet.
[0195] The thickness of the sheet can be measured, for example, using a standard micrometer.
[0196] The sheet, or where appropriate the layer consisting of the composition based on poly-aryl-ether-ketone(s), may in particular have a thickness ranging from 200 microns to 20.00 millimeters. Preferably the sheet has a thickness ranging from 500 microns to 10.00 millimeters.
[0197] According to particular embodiments, the sheet, or where appropriate the layer consisting of the composition based on poly-aryl-ether-ketone(s), has a thickness equal to a value ranging from 500 microns to 1000 microns, or has a value ranging from 1.00 millimeter to 2.00 millimeters, or has a value ranging from 2.00 millimeters to 3.00 millimeters, or has a value ranging from 3.00 millimeters to 4.00 millimeters, or has a value ranging from 4.00 millimeters to 5.00 millimeters, or has a value ranging from 6.00 millimeters to 7.00 millimeters, or has a value ranging from 8.00 millimeters to 9.00 millimeters, or has a value ranging from 9.00 millimeters to 10.00 millimeters.
[0198] Generally speaking, the sheet thickness is substantially uniform, that is to say that its thickness can vary from one place to another on the sheet by at most approximately 10%, preferably by at most approximately 5%.
[0199] The sheet, or where appropriate the layer made of the composition based on poly-aryl-ether-ketone(s), can be manufactured by methods known per se comprising:
[0200] - a step of heating the composition based on poly-aryl-ether-ketone(s) to a suitable temperature above its melting temperature, to provide a molten resin composition;
[0201] - a step of forming the molten resin composition into a sheet; and
[0202] - a step of quenching the sheet at a speed sufficiently fast to obtain a sheet in a pseudo-amorphous state.
[0203] In some embodiments, the sheets used in the present invention may be manufactured by melt extrusion. The extrusion temperature will depend on the melting temperature of the polymer (which, in the case of PEKK, is influenced by its T:I ratio) as well as its melt viscosity. For example, when the ratio of T:I isomers in PEKK is 70:30 or 50:50, the preferred extrusion temperature is between about 350°C and about 380°C. Generally, extrusion temperatures of about 5°C to about 70°C, or about 10°C to about 50°C, above the melting temperature of the composition are suitable temperatures.
[0204] The extruded sheet is transported from the die directly onto polished metal or textured rolls, commonly referred to as "chill rolls" because the surface temperature of these rolls is maintained below the melting temperature of the polymer. A stream of air or other gas may also be directed toward the extruded sheet to aid in cooling. The rate at which the sheet is cooled (referred to as the quench rate) and solidified is an important aspect in achieving a pseudo-amorphous sheet structure. The quench rate is largely determined by the temperature of the chill rolls, the thickness of the sheet, and the line speed. It must be fast enough to achieve the sheet in a pseudo-amorphous state. Double-sheet thermoforming process
[0205] [Fig.l] schematically shows a device 1 adapted for a double-sheet thermoforming process according to the invention, in particular for the process described by the block diagram of [Fig.2].
[0206] With reference to [Fig.l], the device 1 comprises a frame 20 comprising clamping means 21 capable of fixing two sheets 10 thereto. The two sheets 10 are initially substantially parallel to each other and separated by an inter-sheet space 60.
[0207] The sheets 10 each comprise an internal face 11 consisting of a pseudo-amorphous composition based on poly-aryl-ether-ketone(s). The internal faces 11 of the two sheets 10 face each other and are capable of being brought into contact, at least partially, with each other at a contact zone 12 during the contacting and coalescence step.
[0208] The device 1 also comprises two mold halves 30 comprising walls 31, the shape of which is adapted to the desired final shape of the hollow body to be manufactured.
[0209] Each mold half 30 may be, independently of one another, flat, positively shaped, or negatively shaped.
[0210] According to advantageous embodiments, one of the two mold halves is of negative shape. The other mold half can then be a plate, of positive shape, or negatively shaped. The other half of the mold may be a plate or negatively shaped.
[0211] The mold halves 30 can be moved (direction of the arrows) from an open position ([Fig. 1 ]), away from each other, to a closed position (not shown), so that the walls 31 form a cavity.
[0212] The external faces 13 of the two sheets 10 face their respective half of the mold 30. They are capable of being brought into contact at a pinching zone 14 with parts 32 of the half-molds 30 intended to ensure closure by pinching. The parts 32 of the half-molds 30 may be flat or, on the contrary, have a shape making it possible to increase the contact surface at the pinching zone 14.
[0213] Each mold half 30 may comprise perforations 33 allowing gases to escape during, at least, the forming step. These perforations 33 may advantageously be connected to a gas outlet tube 40 through which the vacuum may be drawn in order to allow, at least in part, the forming of the sheets 10. Alternatively and / or in addition, the forming of the sheets may be carried out, at least in part, by injection of pressurized gas, by means of a gas inlet tube 50 which may be inserted, at least temporarily, at the inter-sheet space 60. The gas may optionally be heated so that the sheets 10 maintain a temperature sufficiently close to the softening temperature during the forming step.
[0214] Each sheet can be heated on its external face 13 and / or on its internal face 11 using a heating means by radiation, convection or conduction, making it possible to ensure softening. The heating can be carried out for example using infrared lamps and / or by blowing hot air and / or in an oven. The heating means are arranged so that each sheet softens as uniformly as possible.
[0215] According to one embodiment, shown in [Fig.l], a heating means 70 may be arranged at the inter-sheet space 60, thus making it possible to heat the internal face 11 of the two sheets 10 during the softening step. In addition (not shown in the diagram of [Fig.l]), additional heating means may be used, at least temporarily, to heat the external faces of the sheets 10. This may in particular be necessary in the case where the sheet has a very significant thickness.
[0216] Also in addition (not shown in the diagram of [Fig.l]), additional heating means may be used so as to heat, in embodiments where the contacting temperature is higher than the softening temperature, the contact zones 12 of at least one or both sheets 10. According to certain embodiments, this additional heating mode can be implemented by conduction by bringing the part of the half-mold 32 into contact with the pinching zone 14 of one of the two sheets 10 for a sufficient duration. These additional heating means are arranged in such a way that the pinching zones 14 have the most uniform temperature possible.
[0217] The device according to [Fig.l] is particularly suitable for implementing a double-sheet thermoforming process 100 according to a process whose block diagram is presented in [Fig.2].
[0218] With reference to [Fig.2], the method 100 comprises the provision of two sheets 10 comprising at least one face 11 consisting of a pseudo-amorphous composition based on poly-aryl-ether-ketone(s).
[0219] The method 100 comprises a step 105 of softening each of the sheets at a softening temperature, so as to form softened sheets 110.
[0220] The softening temperature may otherwise be referred to as the “thermoforming temperature.”
[0221] The softening temperature is greater than or equal to the glass transition temperature of each pseudo-amorphous composition.
[0222] According to the embodiments where the composition of the sheets is different, the softening temperature may be different for each sheet. Conversely, according to the embodiments where the composition of the sheets is similar, the softening temperature of each sheet may be similar.
[0223] The softening temperature can be measured using a thermocouple near the inner face 11 of a sheet 10 (outside the contact zone 12).
[0224] The softening temperature generally has a value strictly greater than Tg and less than or equal to (Tg+80)°C. The softening temperature may preferably be from (Tg+10)°C to (Tg+75)°C.
[0225] According to certain embodiments, the softening temperature may be from (Tg+15)°C to (Tg+65)°C or from (Tg+20)°C to (Tg+60)°C.
[0226] Advantageously, the softening temperature is substantially uniform over the entire internal face 11 of each sheet 10, except possibly at the contact zones 12 and neighboring zones, if a contact temperature different from the softening temperature is imposed.
[0227] For example, for PEKK consisting essentially of, or consisting of, repeating units T and I and having a T:I molar ratio equal to approximately 70%, the softening temperature may be from 175°C to 225°C. In the case where the softening temperature is equal to the contacting temperature of the contacting zones, a temperature of 195°C to 215°C may advantageously be chosen.
[0228] When the sheets 10 have reached their softening temperature, the heating element 70 can be removed from the inter-sheet space 60.
[0229] The method 100 comprises a step 115 of forming the softened sheets 110. The forming can in particular be carried out by blowing a pressurized gas onto the internal faces 11 and / or by sucking air onto the external faces 13.
[0230] For example, a pressure of 1 to 6 bars, preferably 1.2 to 5 bars, can be exerted on the internal faces 11 and / or a vacuum of 0.001 to 0.9 bar, preferably 0.05 to 0.85 bar, can be exerted on the external faces 13.
[0231] The method 100 comprises a step of bringing into contact and coalescing 125 at least one contact zone 12 of said faces 11 of the softened sheets so as to form an intermediate body 130. For the step of bringing into contact and coalescing, the contact zones 12 are heated to a contacting temperature, each contact zone 12 remaining in an essentially amorphous state at least until contacting. The contact step is implemented by bringing the half-molds 30 together so that the parts of the half-mold 32 first come into contact with the sheets 10 at the pinching zones 14, then bring the two sheets 10 into contact at their contact zone 12. The coalescence of the two sheets 10 is made possible by the fact that the composition of the internal faces 11 constituting them is in an essentially amorphous state at the time the contact zones 12 are brought into contact.
[0232] The contact temperature can be measured using a thermocouple near a contact area 12 of a sheet 10.
[0233] The contact temperature is generally greater than or equal to the softening temperature.
[0234] The contact temperature is generally less than or equal to the mold temperature.
[0235] According to some embodiments, the contact temperature may be equal to about the softening temperature.
[0236] According to some embodiments, the contact temperature may be equal to approximately the mold temperature.
[0237] According to certain embodiments, the contact temperature may be a few degrees or a few tens of degrees higher than the softening temperature.
[0238] The contact temperature may in particular be at least 5°C, or at least 10°C, or at least 15°C higher than the softening temperature.
[0239] The contact temperature may in particular be at most 75°C, or at most 60°C, or at most 50°C, or at most 45°C, or at most 40°C, or at most 35°C, or not more than 30°C, or not more than 25°C or not more than 20°C above the softening temperature.
[0240] According to certain embodiments, the contact temperature may be a few degrees or a few tens of degrees lower than the mold temperature. These embodiments may in particular be implemented when the part 32 of a half-mold 30 is placed in contact for a sufficient time with the pinching zone 14 before the step of contact and coalescence of the contact zones 12 of the sheets 10.
[0241] The contact temperature may in particular be at most 5°C, or at most 10°C, or at most 15°C lower than the mold temperature.
[0242] In order to facilitate the coalescence of the contact zones 12, a pinching pressure can be exerted on the two half-molds 30. According to certain embodiments, the pinching pressure is from 1 bar to 50 bars. The pinching pressure can preferably be from 5 bars to 40 bars and even more preferably be from 7 to 30 bars. The pinching pressure can be adapted by providing an air gap between the two half-molds.
[0243] The method 100 finally comprises a crystallization step 135 of the composition based on poly-aryl-ether-ketone(s) at a mold temperature, so as to form a crystallized hollow body after the contacting and coalescence step 115 and after the forming step 125, to form a crystallized hollow body 140.
[0244] The mold can be brought to the mold temperature, preferably as uniform as possible, using suitable mold heating means, for example electric heating devices.
[0245] The mold temperature may advantageously be a temperature close to the temperature at which the composition has a minimum isothermal half-crystallization time.
[0246] According to certain embodiments, the mold temperature may be close to (Tg + Tf) / 2. The mold temperature is preferably not greater than 35°C, or not greater than 25°C, or not greater than 15°C, or not greater than 10°C above (Tg + Tf) / 2. The mold temperature is preferably not less than 45°C, or 35°C, or 25°C, or 20°C below (Tg + Tf) / 2.
[0247] For example, for PEKK consisting essentially of, or consisting of, repeating units T and I and having a T:I molar ratio equal to approximately 70%, the mold temperature may be from 210°C to 270°C, and preferably from 220°C to 260°C, and more preferably from 225°C to 255°C.
[0248] Advantageously, the difference between the softening temperature and the mold temperature can be less than or equal to 60°C, so as to avoid any warping. The difference between the softening temperature and the mold temperature may be less than or equal to 50°C, or less than or equal to 40°C.
[0249] Also advantageously, the difference between the softening temperature and the mold temperature may be greater than or equal to 15°C, or greater than or equal to 20°C, or even greater than or equal to 25°C.
[0250] The duration of the crystallization step may depend on the thickness of the sheets, the mold temperature, the shape of the mold and the desired crystallization rate. For example, for PEKK consisting essentially of, or consisting of, repeating units T and I and having a T:I molar ratio equal to about 70%, this duration may be from 1 minute to 30 minutes, preferably from 2 minutes to 15 minutes, and more preferably from 3 minutes to 10 minutes.
[0251] According to certain embodiments, the sufficiently long heating of the contact zone makes it possible to achieve an average crystallinity rate strictly greater than 7%, as measured by WAXS. Preferably, it makes it possible to achieve a crystallinity rate greater than or equal to 10%, or greater than or equal to 15%, or greater than or equal to 20%, or even greater than or equal to 25%.
[0252] Although the block diagram of [Fig.2] represents sequential type steps, some of these steps may in practice overlap and / or take place simultaneously, or even in a different order.
[0253] According to certain embodiments, the forming step 115 of the sheets 10 may be initiated before the contacting and coalescing step 125 by initiating an air blow and / or a vacuum suction before the contact zones 12 have been brought into contact. According to these embodiments, the forming step 115 may be implemented so as to be completed before, at the same time as, or after the contacting and coalescing step.
[0254] According to particular embodiments, the forming step 115 can end before the contacting and coalescence step 125. This is the case in particular when the sheets are formed one by one and then brought into contact with each other.
[0255] According to some embodiments, the forming step 115 may be completed at approximately the same time as the contacting and coalescing step 125.
[0256] According to certain embodiments (not shown in [Fig.2]), the forming step can be implemented essentially after the contacting and coalescence step.
[0257] Although the crystallization step may, to some extent, be initiated before the end of the contacting step and / or before the end of the forming step, it is essential for the implementation of the invention that the composition be in an essentially amorphous state for the contacting and coalescence of the contact zones. sheets. It is also advantageous if the forming step is carried out with a predominantly amorphous composition. Examples Example 1
[0258] A hollow body was manufactured using a device as shown diagrammatically in [Fig.l] according to a process following the block diagram of [Fig.2].
[0259] Two amorphous sheets 2.3 millimeters thick made of a polyetherketoneketone consisting of T and I units with a molar ratio of 70:30 and a viscosity at 380°C, at 1Hz, of 3906Pa.s are used.
[0260] The inner face of the sheets is heated to a softening temperature of 210°C for the softening step. No additional heating means are used to heat the inter-sheet contact areas.
[0261] The two half-molds are closed with a pinching pressure of 10 bars.
[0262] The two sheets are thermoformed and held for approximately 5 minutes in a mold heated to a temperature of 240°C. The mold is then opened by removing one of the two half-molds and the hot hollow body is cooled by a jet of air.
[0263] The hollow body thus obtained is opaque in appearance, that is to say crystallized. Example 2
[0264] A hollow body was made with the same sheets as those used in Example 1.
[0265] The inner face of the sheets is heated to a softening temperature of 200°C for the softening step. The contact zones are brought to a temperature of 220°C.
[0266] The two half-molds are closed with a pinching pressure of 10 bars.
[0267] The two sheets are thermoformed and held for approximately 5 minutes in a mold heated to a temperature of 240°C. The mold is then opened by removing one of the two half-molds and the hot hollow body is cooled by a jet of air.
[0268] The hollow body thus obtained is opaque in appearance, that is to say crystallized.
Claims
Claims
1. A method (100) of double-sheet thermoforming for manufacturing a hollow body (140), said method comprising: - providing two sheets (10) comprising at least one face (11) made of a pseudo-amorphous composition based on poly-aryl-ether-ketone(s), the pseudo-amorphous composition having a crystallinity rate of 0% to 7%, as measured by WAXS; - a step of softening (105) the two sheets (10) at a softening temperature, so as to form softened sheets (110); the softening temperature being greater than or equal to the glass transition temperature of each pseudo-amorphous composition; - a step of forming (115) the softened sheets (110) so as to form thermoformed sheets (120);- a step of bringing into contact and coalescence (125) of at least one contact zone (12) of said faces (11) of the softened sheets, and / or of the sheets being formed or already formed, so as to form an intermediate body (130), the contact zones (12) being heated to a contacting temperature, each contact zone remaining in an essentially amorphous state at least until contacting, the step of bringing into contact and coalescence being implemented with a pinching pressure having a value ranging from 1 bar to 50 bars;and, - a crystallization step (135) of the composition at a mold temperature, to form a crystallized hollow body (140), the crystallized hollow body having an average crystallinity rate strictly greater than 7%, as measured by WAXS, the crystallization step (135) being implemented essentially after the contacting and coalescence step (125), and preferably essentially after the forming step (115).;
2. A double-sheet thermoforming method according to claim 1, wherein said composition has a viscosity at 380°C, at 1Hz, as measured by a parallel plane rheometer, ranging from 200 Pa.s to 8000 Pa.s, preferably from 500 Pa.s to 5000 Pa.s, and more preferably from 750 Pa.s to 4500 Pa.s.
3.
4. Thermoforming method according to any one of claims 1 and 2, wherein the isothermal half-crystallization time at the contact temperature is at least 3 seconds, preferably at least 5 seconds, and most preferably at least 8 seconds; and / or wherein the isothermal half-crystallization time at the contact temperature is at most 30 minutes, preferably at most 10 minutes, more preferably at most 5 minutes, and most preferably at most 2 minutes. Double-sheet thermoforming process according to any one of the preceding claims, in which the at least one poly-aryl-ether-ketone is a poly-ether-ketone-ketone, preferably a homopolymer or a copolymer essentially consisting of, or consisting of, at least one isophthalic repeating unit (I), having the chemical formula: [Chem. 18] and in the case of the copolymer, a terephthalic repeating unit (T), having the chemical formula: [Chem. 19]
5. the molar percentage of T units relative to the sum of the T and I units being from 0% to 5% or from 35% to 78%, preferably from 45% to 75%, and more preferably from 48% to 52% or from 65% to 74%. A double-sheet thermoforming process according to any one of claims 1 to 3, wherein the at least one poly-aryl-ether-ketone is a copolymer essentially consisting of, or consisting of, a repeating unit of chemical formula: and a repeating motif of chemical formula: [Chem.21]
6. (IV); the molar percentage in unit (III) relative to the sum of units (III) and (IV) being: 0% to 99%, preferably 5% to 95%, more preferably 10% to 50% and most preferably 20% to 40%. Double-sheet thermoforming process according to any one of claims 1 to 3, in which the at least one poly-aryl-ether-cetone is a copolymer essentially consisting of, or consisting of, a repeating unit having the formula: [Chem.22] (iii); and a repeating motif having the formula: [Chem.23]
7. (V); the molar percentage in unit (III) relative to the sum of units (III) and (V) being from 0% to 99% and preferably from 0% to 95%. Double-sheet thermoforming method according to any one of the preceding claims, in which the composition consists of polyaryl ether ketone(s), optionally other thermoplastic polymer(s) other than a polyaryl ether ketone, optionally filler(s), and optionally additive(s).
8. Double-sheet thermoforming method according to any one of the preceding claims, in which each sheet is made, independently or not of one another, of a pseudo-amorphous composition based on polyaryl ether ketone(s).
9. Double-sheet thermoforming method according to any one of the preceding claims, in which the two sheets have, independently or not of one another, a thickness of 200 microns to 20 millimeters, preferably a thickness of 500 microns to 10 millimeters.
10. Double-sheet thermoforming method according to any one of the preceding claims, in which the crystallization step is carried out up to an average crystallinity rate in the thickness greater than or equal to 10%, as measured by WAXS, during the crystallization step; preferably up to an average crystallinity rate greater than or equal to 15%, or greater than or equal to 20%, or even greater than or equal to 25%.
11. Double-sheet thermoforming method according to any one of the preceding claims, in which the softening step (105) is carried out at a softening temperature having a value strictly greater than Tg and less than or equal to (Tg+80)°C, and preferably having a value ranging from (Tg+10)°C to (Tg+75)°C.
12. A double-sheet thermoforming method according to any one of the preceding claims, wherein the crystallization step is carried out at a mold temperature close to the temperature at which the composition has a minimum isothermal half-crystallization time.
13. A double-sheet thermoforming method according to any one of the preceding claims, wherein the difference between the mold temperature and the softening temperature is less than or equal to 60°C, and / or greater than or equal to 15°C.
14. A double-sheet thermoforming method according to any one of the preceding claims, wherein the contacting and coalescing step is carried out with a pinch pressure having a value ranging from 5 bar to 40 bar, and in a manner
15. preferred with a pinch pressure ranging from 7 bars to 30 bars. Hollow body comprising at least one internal surface consisting of a crystallized composition based on polyaryl ether ketone(s), capable of being obtained by a process according to any one of claims 1 to 14.